Additive manufacturing high-temperature alloy powder recycling tool

By designing additive manufacturing high-temperature alloy powder recycling tooling, using hydraulic presses and vacuum heat treatment technology, the molding and remelting of waste powder of high-temperature alloy powder is solved, and effective utilization of resources and reduction of production costs are achieved.

CN222058827UActive Publication Date: 2024-11-26INST OF METAL RESEARCH - CHINESE ACAD OF SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420728136.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-10
Publication Date
2024-11-26
Estimated Expiration
2034-04-10

AI Technical Summary

Technical Problem

Due to the high hardness and large surface area of ​​waste powder of high temperature alloy powder, it is difficult to press and form at room temperature, and it is easy to increase oxygen under high temperature conditions, resulting in difficulty in secondary remelting powder, resulting in waste of resources and high production costs.

Method used

An additive manufacturing high-temperature alloy powder recycling tool is designed, including cover plate, sleeve, upper and lower pad plate, which provides initial pressure through a hydraulic press and sintered in a vacuum heat treatment furnace to form an annular powder pressing ingot, solving the problem of The problem of powder forming and remelting.

Benefits of technology

Effective press forming and secondary remelting recovery of high-temperature alloy powders are realized, which reduces production costs and ensures the quality of finished products and the reuse of resources.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222058827U_ABST
    Figure CN222058827U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of additive manufacturing high-temperature alloy powder recovery and powder metallurgy, in particular to an additive manufacturing high-temperature alloy powder recovery tool, which consists of a cover plate, a sleeve, an upper base plate and a lower base plate, and is structurally characterized in that the cover plate is arranged at the top of the sleeve, and a plurality of positioning screws are arranged in the center of the cover plate; the edge of the cover plate and the outer edge of the top of the sleeve are fixed together through a plurality of fastening screws. The milling flat is arranged at the bottom of the outer side of the sleeve, so that screw fastening and loosening operation can be conveniently carried out after the tool is fixed; a lower base plate is arranged at the bottom in the sleeve; according to the device, the additive manufacturing high-temperature alloy waste powder can be pressed and formed, so that secondary remelting recovery of the waste powder is realized, and the production cost of the additive manufacturing high-temperature alloy powder is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of additive manufacturing high-temperature alloy powder recovery and powder metallurgy, and in particular to an additive manufacturing high-temperature alloy powder recovery tool. Background Art

[0002] High-temperature alloys are usually based on iron, cobalt and nickel, and have excellent high-temperature mechanical properties by adding a large amount of alloying elements. Therefore, they are widely used in the manufacture of hot end components of aircraft engines. According to the molding process, high-temperature alloys can be divided into deformed high-temperature alloys, cast high-temperature alloys and powder high-temperature alloys. Powder high-temperature alloys mainly refer to high-temperature alloys produced and prepared by powder metallurgy. They have the advantages of uniform structure, fine grains and no macro-segregation, and are widely used in additive manufacturing and other fields. At present, there are two main methods for manufacturing powder high-temperature alloys: gas atomization powder making and plasma rotating electrode powder making. Among them, gas atomization powder making technology has become the most commonly used powder making technology due to its advantages of high production efficiency, low production cost and controllable powder particle size.

[0003] Additive manufacturing technology has particle size requirements for the required powder raw materials: the powder particle size range required for selective laser melting (SLM) is (15-53) μm. Too large a powder size will lead to incomplete melting of the powder during the laser scanning process, which will cause metallurgical defects in the printed parts; the powder particle size range required for electron beam selective melting is (60-150) μm. In addition to the requirements for powder composition, morphology, fluidity, etc., the overall powder yield of domestic aerosol powder making generally does not exceed 50%. With the continuous development of additive manufacturing technology, the amount of waste powder obtained in the production process is increasing, resulting in a huge waste of resources. For waste powders that meet the requirements, they can be used as raw materials for secondary remelting and powder spraying, thereby realizing the reuse of resources.

[0004] For gas atomization powder making equipment, different equipment structures also put forward different requirements for the size and shape of the powder spraying ingot. Therefore, the waste powder should generally be pressed and formed according to the equipment structure before the secondary remelting and powder spraying. However, due to the high hardness of high-temperature alloy powder, it is extremely difficult to press and form at room temperature. At the same time, due to the large specific surface area of ​​high-temperature alloy powder, it is very easy to increase oxygen under high temperature conditions, which may have an adverse effect on subsequent use. Therefore, solving the problem of pressing and forming waste powder so that it can match gas atomization powder making equipment is of great significance for realizing the remelting and recycling of waste powder and reducing the production cost of high-temperature alloy powder for additive manufacturing. Utility Model Content

[0005] In order to solve the shortcomings and deficiencies of the prior art, the utility model provides a high-temperature alloy powder recovery tool for additive manufacturing. The technical solution of the utility model is:

[0006] A tool for recovering high-temperature alloy powder for additive manufacturing, comprising a cover plate, a sleeve, an upper pad and a lower pad, and the specific structure is: the cover plate is placed on the top of the sleeve, a plurality of positioning screws are arranged in the center of the cover plate, and the edge of the cover plate is fixed to the outer edge of the top of the sleeve by a plurality of fastening screws; a milling flat is arranged on the bottom of the outer side of the sleeve to facilitate screw tightening and loosening operations after the tool is fixed; a lower pad is placed on the bottom of the inner side of the sleeve, and an upper pad is placed inside the sleeve.

[0007] The above-mentioned additive manufacturing high-temperature alloy powder recovery tooling, a preferred embodiment of which is that a plurality of top holes are provided at the bottom of the sleeve.

[0008] The above-mentioned additive manufacturing high-temperature alloy powder recovery tooling has a preferred embodiment in which 4 to 6 positioning screws are provided and 4 to 6 fastening screws are provided.

[0009] The above-mentioned additive manufacturing high-temperature alloy powder recovery tooling has a preferred embodiment that, in order to obtain annular powder pressed ingots, the upper pad and the lower pad are provided with circular holes of the same diameter, and a sleeve center column is arranged in the sleeve and passes through the circular holes of the upper pad and the lower pad.

[0010] A preferred embodiment of the above-mentioned additive manufacturing high-temperature alloy powder recovery tool is that the material of the tool is a metal material or a ceramic material.

[0011] The method for using the additive manufacturing high-temperature alloy powder recovery tooling comprises the following steps:

[0012] (1) Place the lower plate into the sleeve, and then place the powder into the upper part of the lower plate in the sleeve; the amount of powder placed is generally 2 to 5 kg;

[0013] (2) Smooth the upper surface of the powder, then install the upper pad so that it lies flat on the top of the powder;

[0014] (3) Use a hydraulic press and a pressing tooling to press the upper plate to provide initial pressure for powder pre-pressing. The initial pressure is generally controlled within the range of 3 to 100 MPa. After compaction, the pressing tooling can be removed.

[0015] (4) Install the tooling cover and tighten the fixing screws;

[0016] (5) Tighten the positioning screws to ensure that the upper pad remains in a fixed position during subsequent production;

[0017] (6) The tooling and the waste powder therein are transferred into a vacuum heat treatment furnace, and then vacuumed to a vacuum degree of <0.1 Pa, and the powder is sintered under a suitable sintering process. The sintering process can be selected as a direct heating method or a staged heating method;

[0018] (7) As the furnace cools to room temperature, open the cover plate and the upper pad in turn and take out the powder sintered ingot. If the sintered ingot cannot be taken out, it can be pushed out through the bottom top hole through the lower pad using screws and other tools.

[0019] The advantages and beneficial effects of the utility model are:

[0020] The utility model can press and shape waste powder of high-temperature alloy for additive manufacturing, thereby realizing secondary remelting and recycling of waste powder, thereby reducing the production cost of high-temperature alloy powder for additive manufacturing;

[0021] The utility model is suitable for the pressing and molding of high-temperature alloy powders in most additive manufacturing processes, has strong practicability and high economic value. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 This is a schematic diagram of the high-temperature alloy powder recovery tooling for additive manufacturing of the utility model;

[0023] Figure 2 This is a cross-sectional view of the high-temperature alloy powder recovery tooling for additive manufacturing of the utility model;

[0024] Figure 3 It is a schematic diagram of the supporting tooling for pressing;

[0025] In the figure: 1-positioning screw; 2-fastening screw; 3-cover plate; 4-sleeve; 5-upper pad; 6-lower pad; 7-milling flat; 8-top hole; 9-middle column of the sleeve. DETAILED DESCRIPTION

[0026] The specific implementation of the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments of the specification.

[0027] Example 1

[0028] A tool for recovering high-temperature alloy powder for additive manufacturing, comprising a cover plate 3, a sleeve 4, an upper pad 5, a lower pad 6 and a sleeve center column 9, and the specific structure is: the cover plate 3 is placed on the top of the sleeve 4, 4 positioning screws 1 are arranged in the center of the cover plate 3, and the edge of the cover plate 3 is fixed to the outer edge of the top of the sleeve 4 by 4 fastening screws 2; a milling flat 7 is arranged on the bottom of the outer side of the sleeve 4 to facilitate screw tightening and loosening operations after the tool is fixed; a lower pad 6 is placed on the bottom of the sleeve 4, and an upper pad 5 is placed in the sleeve; two top holes 8 are arranged at the bottom of the sleeve, and circular holes of the same diameter are opened on the upper pad 5 and the lower pad 6, a sleeve center column 9 is arranged in the sleeve 4 and passes through the circular holes of the upper pad 5 and the lower pad 6, and the material of the tool is 304 stainless steel.

[0029] Select additive manufacturing high temperature alloy powder K4169, the powder weight is 8.5kg, use the above-mentioned tooling for secondary powder pressing, each powder loading amount is 4.25kg, and the use method includes the following steps:

[0030] (1) Place the lower plate 6 into the sleeve 4, and then place the powder into the upper part of the lower plate 6 in the sleeve 4;

[0031] (2) Smooth the upper surface of the powder, and then install the upper pad 5 so that it lies flat on the top of the powder;

[0032] (3) Using a pressing tooling to press the upper pad 5, providing an initial pressure for the powder pre-pressing molding, the initial pressure is selected to be 10 MPa, and the pressing tooling can be removed after compaction;

[0033] (4) Install the tooling cover 3 and tighten the fixing screws 2;

[0034] (5) Tighten the positioning screw 1 to ensure that the upper pad remains in a fixed position during subsequent production;

[0035] (6) The tooling and the waste powder inside it are transferred into a vacuum heat treatment furnace, and then vacuumed. When the vacuum degree reaches 0.087 Pa, the temperature is raised to sinter the powder. The sintering process is 750°C for 4 hours and then cooled with the furnace;

[0036] (7) After the furnace cools to room temperature, open the cover plate 3 and the upper pad 5 in sequence and take out the powder sintered ingot.

[0037] After sintering, the powder sintered ingot was taken out. The appearance and color of the sintered ingot were consistent with the original waste powder. The O and N content results of the sintered ingot and the original powder are shown in Table 1. There was no obvious increase in oxygen and nitrogen after the powder was sintered into an ingot.

[0038] Table 1 Results of O and N contents of sintered ingots and original powders

[0039]

[0040]

Claims

1. An additive manufacturing high temperature alloy powder recovery tool, characterized in that: It consists of a cover plate, a sleeve, an upper pad and a lower pad, and the specific structure is: the cover plate is placed on the top of the sleeve, a plurality of positioning screws are provided in the center of the cover plate, and the edge of the cover plate is fixed to the outer edge of the top of the sleeve by a plurality of fastening screws; a milling flat is provided on the bottom of the outer side of the sleeve; a lower pad is placed on the bottom of the inner side of the sleeve, and an upper pad is placed inside the sleeve.

2. The additive manufacturing high-temperature alloy powder recovery tool according to claim 1, characterized in that: The bottom of the sleeve is provided with a plurality of top holes.

3. The additive manufacturing high-temperature alloy powder recovery tool according to claim 1, characterized in that: The number of the positioning screws is 4 to 6, and the number of the fastening screws is 4 to 6.

4. The additive manufacturing high-temperature alloy powder recovery tool according to claim 1, characterized in that: The upper pad and the lower pad are provided with circular holes of the same diameter, and a sleeve center column is arranged in the sleeve and passes through the circular holes of the upper pad and the lower pad.