Corrosion-resistant glass film
By setting the first and second openings on the glass film and setting bumps on the release film, the problem of viscosity failure caused by dust pollution on the glue surface is solved, and the service life of the glass film is extended and its resistance is maintained. Corrosion characteristics.
Patent Information
- Application Number
- CN202420692954.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-07
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-07
AI Technical Summary
Before the existing glass film is used, the glue surface is easily contaminated by dust, causing viscosity failure, reducing protection and service life, and thus affecting its corrosion resistance and moisture resistance.
A corrosion-resistant glass film is designed, and the bottom surface is fixedly installed with EVA colloid, and a first opening and closing port is arranged to penetrate through the top surface of the glass film to the colloid surface, and a corresponding second opening and closing port and a pressure are provided on the release film. The marks are convenient for tearing off the edges before use to avoid dust adhesion. The release film is assisted by bumps.
Through this design, dust affects viscosity effectively, extends the service life of the glass film and maintains its corrosion resistance.
Smart Images

Figure CN222064409U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of glass films, in particular to a corrosion-resistant glass film. Background Art
[0002] Glass film refers to a kind of film in the home building materials market. It has various colors, is energy-saving and environmentally friendly, and is mainly used to decorate indoor and outdoor glass. This kind of glass film can not only change the monotonous and transparent image of ordinary glass, add beauty to indoor and outdoor, but also insulate and block cold, explosion-proof and earthquake-resistant, and add safety insurance to the room. The most basic composition of glass film is: polyester substrate (PET), one side is coated with an anti-scratch layer (HC), and the other side is an installation glue layer and protective film. Glass film is usually synthesized by a single or multi-layer PET interlayer, with thicknesses of: 2MIL (0.05mm), 4MIL (0.10mm), 7MIL (0.18mm), 11MIL (0.28mm), 14MIL (0.36mm), etc. Considering safety and ease of construction, the thickness of the film substrate should be above 2MIL. PET is a material with strong durability, strong moisture resistance, high and low temperature resistance. It is clear and transparent, and has been processed by various processes such as metallization coating, magnetron sputtering, and interlayer synthesis to become a film with different characteristics. Professional membrane manufacturers usually use their own patented adhesives for interlayer synthesis and installation of adhesive layers, mainly pressure-sensitive adhesives and water-activated adhesives.
[0003] Before the existing glass film is used, the adhesive surface will be affixed with release paper to protect the unused adhesive surface from damage and cannot be used. However, dust is easily attached to the edge of the release paper and the adhesive surface of the glass film. If the dust sticks to the area for a long time, the adhesion will fail. The adhesion failure means that the protectiveness is reduced, which will cause dust to move closer to the used surface of the glass film, thereby reducing the service life and further reducing its corrosion resistance, moisture resistance, durability and other properties. For this reason, we propose a corrosion-resistant glass film. Utility Model Content
[0004] In view of the above problems, the utility model provides a corrosion-resistant glass film, which has the effect of maintaining the corrosion-resistant property during use.
[0005] The technical solution of the utility model is:
[0006] A corrosion-resistant glass film comprises a glass film body, a colloid is fixedly mounted on the bottom surface of the glass film body, a release film is arranged below the glass film body, the release film and the colloid are glued together, a first opening and closing opening is arranged on the surface of the glass film body along the inner side of the edge, and the first opening and closing opening passes through the top surface of the glass film body and extends to the surface of the colloid.
[0007] In a further technical solution, bumps are fixedly mounted at the four corners of the release film.
[0008] In a further technical solution, a second opening and closing opening opposite to the first opening and closing opening is formed on the surface of the release film.
[0009] In a further technical solution, a first indentation is provided on the surface of the glass film body, and a second indentation is provided on the surface of the release film opposite to the first indentation, and the first indentation is located at the opening center of the first opening and closing mouth, and the second indentation is located at the opening center of the second opening and closing mouth.
[0010] In a further technical solution, the material of the colloid is EVA.
[0011] The beneficial effects of the utility model are:
[0012] By setting the first opening and closing mouth, dust can be adhered to the edge where the glass film body and the release film are connected, resulting in reduced viscosity. When in use, if dust adheres to the edge of the glass film body and the colloid, the surface between the edge of the glass film body and the first opening and closing mouth can be directly torn off along the opening of the first opening and closing mouth before use. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a schematic diagram of the overall structure of an embodiment of the utility model;
[0014] Figure 2 This is a schematic diagram of the structure of the glass film body and the colloid in the embodiment of the utility model;
[0015] Figure 3 It is a schematic structural diagram of a release film according to an embodiment of the utility model.
[0016] Description of reference numerals:
[0017] 1. Glass film body; 2. Release film; 3. Colloid; 4. First opening and closing mouth; 5. First indentation; 6. Second opening and closing mouth; 7. Second indentation; 8. Bump. DETAILED DESCRIPTION
[0018] The embodiments of the present utility model will be further described below in conjunction with the accompanying drawings. Example
[0019] like Figure 1-Figure 3 As shown, a corrosion-resistant glass film includes a glass film body 1, an EVA colloid 3 is fixedly installed on the bottom surface of the glass film body 1, a release film 2 is provided under the glass film body 1, the release film 2 and the colloid 3 are glued together, and a first opening and closing mouth 4 is provided on the surface of the glass film body 1 along the inner side of the edge, and the first opening and closing mouth 4 passes through the top surface of the glass film body 1 and extends to the surface of the colloid 3.
[0020] The working principle of the above technical solution is as follows:
[0021] Before the glass film body 1 is used, the release film 2 is always adhered to the surface of the colloid 3 and is cut flush with the edge of the glass film body 1. When dust enters the edges of the glass film body 1 and the release film 2, the portion outside the first opening and closing opening 4 on the surface of the glass film body 1 will be affected by the dust, resulting in reduced adhesion. When using the glass film body 1, the outer edge of the glass film body 1 can be directly torn off along the first opening and closing opening 4, and then proceed.
[0022] In another embodiment, if Figure 1 and Figure 3 As shown, bumps 8 are fixedly installed at the four corners of the release film 2 . By providing the bumps 8 , the release film 2 can be easily torn off from the surface of the glass film body 1 .
[0023] When tearing off the release film 2 , just pull the protrusion 8 from one of the protrusions 8 in the opposite direction of the glass film body 1 .
[0024] In another embodiment, if Figure 1 and Figure 3 As shown, a second opening and closing opening 6 opposite to the first opening and closing opening 4 is provided on the surface of the release film 2. By providing the second opening and closing opening 6, when the edge of the glass film body 1 needs to be torn off, the release film 2 can be torn off at the same time, which is convenient for use. A first indentation 5 is provided on the surface of the glass film body 1, and a second indentation 7 opposite to the first indentation 5 is provided on the surface of the release film 2. The first indentation 5 is located at the opening center of the first opening and closing opening 4, and the second indentation 7 is located at the opening center of the second opening and closing opening 6. By providing the first indentation 5 and the second indentation 7, the edges of the glass film body 1 and the release film 2 can be easily torn off.
[0025] When tearing off the glass film body 1 and the edge of the release film 2 , just cut along the folds of the first indentation 5 and the second indentation 7 .
[0026] The above embodiments only express the specific implementation methods of the utility model, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the utility model. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the utility model, which all belong to the protection scope of the utility model.
Claims
1. A corrosion-resistant glass film, comprising a glass film body (1), characterized in that: A colloid (3) is fixedly mounted on the bottom surface of the glass film body (1), a release film (2) is provided below the glass film body (1), the release film (2) and the colloid (3) are glued together, and a first opening (4) is provided on the surface of the glass film body (1) along the inner side of the edge, and the first opening (4) passes through the top surface of the glass film body (1) and extends to the surface of the colloid (3).
2. The corrosion-resistant glass film according to claim 1, characterized in that: Bumps (8) are fixedly mounted at the four corners of the release film (2).
3. The corrosion-resistant glass film according to claim 1, characterized in that: The surface of the release film (2) is provided with a second opening (6) opposite to the first opening (4).
4. The corrosion-resistant glass film according to claim 1, characterized in that: The surface of the glass film body (1) is provided with a first indentation (5), and the surface of the release film (2) is provided with a second indentation (7) opposite to the first indentation (5), and the first indentation (5) is located at the opening center of the first opening and closing opening (4), and the second indentation (7) is located at the opening center of the second opening and closing opening (6).
5. The corrosion-resistant glass film according to claim 1, characterized in that: The material of the colloid (3) is EVA.