Heat-resistant asphalt pavement structure suitable for high temperature
By using asphalt layer and structural reinforcement mesh frame structure mixed with ceramic powder in asphalt pavement, combined with vertical and cross-seam joint design, the problems of ruts and pavement cracks at high temperatures are solved, the fatigue resistance and overall performance of the pavement are improved, and the road surface is realized. The dual benefits of economic costs and environmental protection.
Patent Information
- Application Number
- CN202420467217.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-12
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-03-12
AI Technical Summary
Existing asphalt pavement is prone to ruts and road cracks in high temperature environments, resulting in road damage, mainly due to the high road surface temperature, low asphalt bonding and insufficient integrity and fatigue resistance of the pavement structure.
The soil base, base layer and deformation-resistant surface layer structure are sequentially spread from bottom to top. The deformation-resistant surface layer is an asphalt layer mixed with ceramic powder, which is connected through the grid frame structure of the structural steel mesh, combining fine aggregate and The ceramic particles of coarse aggregate enhance the integrity and fatigue resistance of the pavement, and strengthen the pavement structure through the design of longitudinal oblique seams and transverse flat seams.
It effectively improves the resistance to permanent deformation and fatigue of the road surface, reduces the occurrence of ruts under high temperatures, reduces economic costs and protects the environment, and enhances the overall stability and wear resistance of the road surface.
Smart Images

Figure CN222065060U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of asphalt pavement structures, and in particular relates to a heat-resistant asphalt pavement structure suitable for high temperatures. Background Art
[0002] In recent years, the social economy has developed rapidly and the urban transportation network has become increasingly mature, but the occurrence of road diseases has not decreased. Analyzing the causes of road diseases, rutting and pavement cracking are the main factors of road damage. The rutting and pavement cracking are mainly caused by the excessively high road surface temperature, the low adhesion of asphalt, and the integrity and fatigue resistance of the pavement structure.
[0003] Ceramic waste powder can be crushed into powder and added to asphalt cementitious materials as a modifier. Ceramic waste powder has a positive effect on high temperature performance and can improve the ability of asphalt cementitious materials to resist permanent deformation. By improving the pavement structure of the base and surface layers and the combination design between the structures, the integrity and fatigue resistance of the pavement structure can be effectively improved and the generation of road rutting can be reduced. Utility Model Content
[0004] In view of the above problems existing in the prior art, the purpose of the utility model is to provide a heat-resistant asphalt pavement structure suitable for high temperatures, which can improve the road surface's resistance to permanent deformation and fatigue resistance and is suitable for high temperature environments.
[0005] The utility model provides the following technical solutions: a heat-resistant asphalt pavement structure suitable for high temperatures, comprising a soil base, a base layer and an anti-deformation surface layer paved in sequence from bottom to top; the anti-deformation surface layer is an asphalt layer mixed with ceramic powder, which comprises a lower layer, a middle layer and an upper layer in sequence from bottom to top, a structural steel mesh 1 is arranged between the lower layer and the base layer, a structural steel mesh 2 is arranged between the lower layer and the middle layer, and between the middle layer and the upper layer, and the structural steel mesh 1 is connected to the structural steel mesh 2 to ensure that the entire asphalt pavement is connected into a whole.
[0006] Furthermore, the structural steel mesh 1 and the structural steel mesh 2 are connected by tying the steel bars to form an integral grid frame structure.
[0007] Furthermore, the structural steel mesh 1 and the structural steel mesh 2, and the adjacent structural steel meshes 2 are staggered in vertical arrangement.
[0008] Furthermore, the ceramic powder includes fine aggregate and coarse aggregate, the fine aggregate is ceramic particles with a particle size range of less than 4.75 mm, and the coarse aggregate is ceramic particles with a particle size range of 4.75-9.50 mm.
[0009] Furthermore, the base layer is a layered structure.
[0010] Furthermore, the longitudinal joints on the base layer and the anti-deformation surface layer adopt an oblique joint structure, and the transverse joints adopt a flat joint structure.
[0011] Furthermore, the structural steel mesh 1 and the structural steel mesh 2 are both double-glued metal mesh surfaces.
[0012] By adopting the above technology, compared with the prior art, the beneficial effects of the utility model are as follows:
[0013] 1) In the utility model, based on the layer structure of the asphalt surface mixed with ceramic powder, the surface layer is designed in layers, and a grid frame structure composed of a structural steel mesh 1, a structural steel mesh 2 and binding steel bars is set, so that a stable overall structure is formed between each surface layer of the road surface and between the surface layer and the base layer, which can improve the overall deformation resistance and fatigue resistance of the road surface and avoid rutting at high temperatures;
[0014] 2) In the present invention, by selecting the particle size of the ceramic powder, the compactness of the surface layer can be increased to a greater extent, and the overall anti-deformation ability of the road surface can be further improved; and waste ceramics can be used for grinding, which can effectively reduce economic costs and protect the environment;
[0015] 3) In the present invention, the first structural steel mesh and the second structural steel mesh are staggered so that the steel mesh and the steel mesh formed by the steel bars form a whole, thereby ensuring the stability of the mechanical properties of the overall steel mesh structure and enhancing the fatigue resistance and wear resistance of the road surface;
[0016] 4) In the utility model, the longitudinal joints adopt an oblique joint structure, and the transverse joints adopt a flat joint structure, so that the parts between the joints are connected into a whole through the structural form of the joints, and the pavement structure performance is more stable;
[0017] 5) In the present invention, when the longitudinal joint adopts an oblique joint structure, the force is decomposed into two directions, the horizontal direction and the vertical direction, so that the connection is strengthened in the horizontal direction and the force is ensured in the vertical direction. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a cross-sectional schematic diagram of the asphalt road of the utility model;
[0019] Figure 2 It is a schematic diagram of the structure of the structural steel mesh 1 / structural steel mesh 2 of the utility model. DETAILED DESCRIPTION
[0020] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments of the specification. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.
[0021] On the contrary, the present invention covers any substitution, modification, equivalent method and scheme made on the essence and scope of the present invention as defined by the claims. Further, in order to make the public have a better understanding of the present invention, some specific details are described in detail in the following detailed description of the present invention. Those skilled in the art can fully understand the present invention without the description of these details.
[0022] See also Figure 1-2 A heat-resistant asphalt pavement structure suitable for high temperatures includes a soil base 1, a base layer 2 and an anti-deformation surface layer 3 which are paved in sequence from bottom to top.
[0023] The base layer 2 includes a lower base layer, a middle base layer and an upper base layer from bottom to top. The anti-deformation surface layer 3 is an asphalt layer mixed with ceramic powder, which includes a lower layer, a middle surface layer and an upper surface layer from bottom to top.
[0024] Specifically, a structural steel mesh 1 4 is provided between the lower layer and the upper base layer, a structural steel mesh 2 5 is provided between the lower layer and the middle surface layer, and between the middle surface layer and the upper layer.
[0025] After the asphalt pavement base layer 2 is paved, the structural steel mesh 4 is placed, and the bundling steel bars 3 that fix the structural steel mesh 4 and the structural steel mesh 2 5 are pre-placed at the bundling place of the structural steel mesh 4, and then the asphalt mixture mixed with waste ceramics is continued to be paved in the middle of the asphalt surface layer, and then the structural steel mesh 2 5 is placed, and the bundling steel bars 3 are bound to the structural steel mesh 2 5 to complete the bundling of the grid frame structure, and the asphalt surface layer is continued to be paved until the road surface is completed.
[0026] Among them, the structural steel mesh 1 4 and the structural steel mesh 2 5 are both made of 8*10cm double-glued metal mesh.
[0027] Specifically, the adjacent structural steel meshes 2 5 and the structural steel meshes 2 5 and 1 4 are staggered.
[0028] Specifically, the ceramic powder includes fine aggregate and coarse aggregate, the fine aggregate is ceramic particles with a particle size range of less than 4.75 mm, and the coarse aggregate is ceramic particles with a particle size range of 4.75-9.50 mm.
[0029] Specifically, the longitudinal joints on the base layer 2 and the anti-deformation surface layer 3 adopt an oblique joint structure, and the transverse joints adopt a flat joint structure.
[0030] The construction process of asphalt in this embodiment is as follows:
[0031] S1. Ceramic collection: There are a lot of waste ceramics available for collection in ceramic factories. During the collection process, they are recycled in the form of layered milling;
[0032] S2, grinding the waste ceramics into crushed slag powder, grinding the recycled waste ceramics into powder;
[0033] S3, recycled aggregate and screening particle size, screening the waste ceramics ground into powder, separating the powder into coarse and fine materials, and screening the ceramic particles;
[0034] S4. Mixing the asphalt mixture, and mixing the coarse aggregate and fine aggregate in order according to the proportion;
[0035] S5, layered paving. The content of ceramic particles in each surface layer is different, so it needs to be paved in layers, and each layer needs to be compacted separately to ensure the density of the road surface;
[0036] S6. For construction joint treatment, use bevel joints for longitudinal construction joints and flat joints for transverse joints.
[0037] The ceramic particles used in this embodiment are derived from waste ceramic factories. The recycling of waste ceramics can not only effectively reduce economic costs but also protect the environment. The road surface designed by this patent can reduce the temperature of road surfaces in summer and improve the driving experience.
[0038] In this embodiment, when collecting waste ceramics, the milling method used is a mechanical form. In the process of recycling old materials, milling is a common way to recycle waste. In the recycling step of old materials, milling is performed at a speed of 20m / min.
[0039] In this embodiment, the recycled aggregate and the sieved particle size are verified by the Marshall test to determine the particle size range of the waste ceramic particles. The waste ceramics ground into powder are sieved, and the powder is divided into coarse material and fine material. Ceramic particles with a particle size range of 4.75-9.50 mm are sieved out, of which ceramic particles smaller than 4.75 mm are used as fine aggregate, and those in the particle size range of 4.75-9.5 mm are used as coarse aggregate. The coarse and fine aggregates are then stored separately so that the ratio of coarse and fine aggregates is appropriate during the grading design process.
[0040] In this embodiment, the mixture ratio of different surface layers of the road surface is:
[0041] The lower layer has ordinary asphalt and 20% of ceramic particles as aggregate; or modified asphalt and 40% of ceramic particles as aggregate;
[0042] The middle surface layer has 40% aggregate of common asphalt and ceramic particles; or 50% aggregate of modified asphalt and ceramic particles;
[0043] The upper layer has ordinary asphalt and 20% aggregate of ceramic particles. The mesh frame structure steel mesh 4 is located at the contact between the asphalt surface layer and the base layer, and the structural steel mesh 2 5 is located between the asphalt surface layers. The steel meshes between the two use the same bundling method and are placed in an upper and lower offset manner. After the asphalt pavement base layer is paved, the steel mesh 1 is placed, and the bundling steel bars 6 that fix the structural steel mesh 4 and the structural steel mesh 2 5 are pre-placed at the bundling place of the structural steel mesh 1 4, and then the asphalt mixture mixed with waste ceramics is continued to be paved in the middle of the asphalt surface layer, and then the structural steel mesh 2 5 is placed, and the bundling steel bars 6 are bound to the structural steel mesh 2 5 to complete the bundling of the grid frame structure, and the asphalt surface layer is continued to be paved until the road surface is completed.
[0044] In this embodiment, the asphalt mixture mixing process is as follows:
[0045] First, ordinary asphalt is mixed and stirred for 5 to 10 seconds, and then 4.75-9.5mm coarse aggregate and fine aggregate are added in sequence according to the proportion, and the stirring time is 10-15 seconds; a more specific form of the step of heating and stirring the mixture is that the mixture without ceramic particles is first heated at a high position separately, and the heating temperature is 80-130 degrees Celsius. The temperature used in this embodiment is 115 degrees Celsius. Then, according to the bonding curve of asphalt, the adding temperature of ceramic particles is determined to be between 190-220 degrees Celsius, and the temperature is determined to be 200 degrees Celsius in the example.
[0046] In the layered paving step of this embodiment, after the mixture is mixed, it is necessary to use a grader to carry out paving operations. The paving operation should be carried out continuously. According to the paving operation volume of the mixture, two unloading vehicles are equipped at the construction site to avoid the phenomenon of untimely supply of the mixture. At the same time, the specific paving area is determined in combination with the paving thickness and the compacted dry density, and the post-unloading distance is controlled. For the graded crushed stone subbase operation, the paving thickness is 18cm each time, and the cross-sectional length should be controlled within 15cm. During the paving process, when encountering larger gravel, it should be cleaned out of the mixture in time. When segregation problems are found in the mixture, manual methods should be adopted in time to deal with it; during the paving process, the initial pressure, repeated pressure, and final pressure must be considered; the flatness of the three compactions, and it should be noted that the roller cannot be parked at will.
[0047] In the construction joint step of this embodiment, in order to ensure the construction quality of the highway pavement cushion layer, joint and U-turn processing are required. First, after completing the rolling operation, the cushion layer flatness should be inspected, which can be achieved using a 3m long ruler. If it is found that the cushion layer flatness is not up to standard, the structure here needs to be cleaned up. During the rolling operation, when rolling a new section, the roller should be parked on the compacted section and go deep into the working section for about 15cm before rolling, thereby achieving effective treatment of the transverse construction joint. Secondly, when the cushion layer rolling meets the requirements and then turns around, it is necessary to first cover it with tarpaulin or a relatively thick plastic sheet with a length of about 10m, and then 10cm of soil or gravel can be directly spread on the position and then turn around. In the highway pavement structure, the cushion layer is located between the base and the roadbed, and plays a transitional role in the entire pavement structure, which has a greater impact on the road traffic situation. If you want to ensure the safe driving of vehicles and reduce the occurrence of pavement disease problems, you must do a good job in the construction of the pavement cushion layer.
[0048] Specifically, the asphalt surface layer aggregate can be divided into an upper layer made of a mixture of granite aggregate and ceramic particles; the middle layer and the lower layer are made of a mixture of marble aggregate and ceramic particles. The granite used as aggregate is relatively hard and not easy to weather for road paving; the crusher is rolled by a crusher because it can strictly control the particle size of the crushed stone to ensure the quality of the coarse aggregate.
[0049] Specifically, the upper layer uses SBS modified asphalt and the lower layer uses road petroleum asphalt.
[0050] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A heat-resistant asphalt pavement structure suitable for high temperatures, characterized in that: The invention comprises a soil base (1), a base layer (2) and an anti-deformation surface layer (3) which are spread in sequence from bottom to top; the anti-deformation surface layer (3) is an asphalt layer mixed with ceramic powder, which comprises a lower layer, a middle layer and an upper layer in sequence from bottom to top; a structural steel mesh 1 (4) is arranged between the lower layer and the base layer (2); a structural steel mesh 2 (5) is arranged between the lower layer and the middle layer, and between the middle layer and the upper layer; the structural steel mesh 1 (4) is connected to the structural steel mesh 2 (5) to ensure that the entire asphalt pavement is connected into a whole.
2. A heat-resistant asphalt pavement structure suitable for high temperatures according to claim 1, characterized in that: The structural steel mesh 1 (4) and the structural steel mesh 2 (5) are connected by binding steel bars (6) to form an integral grid frame structure.
3. The heat-resistant asphalt pavement structure suitable for high temperature according to claim 2, characterized in that: The first structural steel mesh (4) and the second structural steel mesh (5) and the adjacent second structural steel meshes (5) are arranged in an up-down staggered manner.
4. The heat-resistant asphalt pavement structure suitable for high temperature according to claim 1, characterized in that: The base layer (2) is a layered structure.
5. The heat-resistant asphalt pavement structure suitable for high temperature according to claim 4, characterized in that: The longitudinal joints on the base layer (2) and the anti-deformation surface layer (3) adopt an oblique joint structure, and the transverse joints adopt a flat joint structure.
6. The heat-resistant asphalt pavement structure suitable for high temperature according to claim 1, characterized in that: The structural steel mesh 1 (4) and the structural steel mesh 2 (5) are both double-glued metal mesh surfaces.