Battery

By setting grooves on the outer surface of the battery case and welding, the problems of high welding cost and low stability of the battery ear are solved, and the effect of reducing manufacturing costs and improving the cleanliness of the welding area is achieved.

CN222072038UActive Publication Date: 2024-11-26ZHUHAI COSMX BATTERY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420651791.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-29
Publication Date
2024-11-26
Estimated Expiration
2034-03-29

AI Technical Summary

Technical Problem

The existing battery ear welding structure is high, and it is impossible to detect false welding and missed welding, and the process stability is low.

Method used

The outer surface of the battery case is provided with grooves, and the pole ears are welded toward one side surface of the inner side of the casing through the bottom of the groove to form a soldering printing, reducing the shell thickness of the welding area, and realizing the shell outside the casing Welding with the extreme ears improves the cleanliness and stability of the welding area.

Benefits of technology

It reduces the cost of battery manufacturing, improves the cleanliness and stability of the welding area, and can detect false and missed welding in a timely manner, improving the stability of the battery process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222072038U_ABST
    Figure CN222072038U_ABST
Patent Text Reader

Abstract

The utility model provides a battery, and relates to the technical field of batteries. The battery comprises a shell and a battery cell located in the shell, a first groove is formed in the outer side of the shell wall of the shell, the battery cell is provided with a first tab, and the first tab is opposite to the first groove; the first tab is welded with the inner side of the shell wall of the shell to form a first welding mark; the first welding mark is positioned in the first groove, so that the thickness of the shell in the welding area is reduced, the welding of the shell and the tab is realized outside the shell, the production and manufacturing cost is reduced, the cleanliness of the welding area is improved, the conditions of insufficient welding and missing welding can be found in time, and the risk of welding failure of the shell and the tab is reduced; and the stability of the battery manufacturing process is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of battery technology, and in particular to a battery. Background Art

[0002] Batteries are widely used in various power supply devices, including consumer electronics, new energy vehicles, and energy storage devices. Batteries have different sizes and structures depending on the application scenario, and the battery shell can be made of different materials.

[0003] In the related art, metal-packaged batteries have good safety. The tabs of the battery cells in the metal-packaged batteries need to be welded to the metal shell. Since the tabs are connected to the inner surface of the shell, the shell and the tabs need to be welded from the inside of the shell, that is, from one side of the tabs.

[0004] However, the current battery tab welding structure has a high cost, and is unable to detect cold welds and leaking welds, resulting in low process stability. Utility Model Content

[0005] In view of the above problems, an embodiment of the present application provides a battery to solve the technical problems that the current battery tab welding structure has high cost, cannot detect cold solder joints and leaking solder joints, and has low process stability.

[0006] In order to achieve the above-mentioned purpose, the present application provides a battery, which includes a shell and a battery cell located in the shell, the outer side of the shell wall of the shell is provided with a first groove, the battery cell has a first pole ear, and the first pole ear is opposite to the first groove; the first pole ear is welded to the inner side of the shell wall of the shell to form a first weld mark; the first weld mark is located in the first groove.

[0007] The battery provided in the embodiment of the present application is provided with a groove on the outer surface of the shell, and is welded to the pole ear through the bottom of the groove on one side surface facing the inside of the shell, thereby reducing the shell thickness in the welding area, so that the welding of the shell and the pole ear is realized outside the shell, reducing the production and manufacturing cost, and improving the cleanliness of the welding area. It is possible to detect cold welding and leaking welding in time, reducing the risk of welding failure between the shell and the pole ear, and improving the stability of the battery process.

[0008] In some embodiments, a ratio of an area of ​​the first weld mark to an area of ​​a bottom of the first groove is greater than or equal to 15% and less than or equal to 45%.

[0009] In some embodiments, the first weld print includes a plurality of weld segments; the plurality of weld segments are sequentially connected end to end; or,

[0010] The first weld mark is spiral; or,

[0011] The first weld print includes a plurality of welding segments; the plurality of welding segments are arranged at intervals.

[0012] In some embodiments, the battery may further include a sealing member, a second groove is provided on the outer side of the shell wall of the shell, a liquid injection hole is provided in the second groove, and the sealing member seals the liquid injection hole; the sealing member is connected to the groove wall of the second groove.

[0013] In some embodiments, the sealing member is welded to the groove wall of the second groove to form a second weld mark.

[0014] In some embodiments, the thickness dimension of the sealing member is greater than the depth dimension of the second groove.

[0015] In some embodiments, the ratio of the thickness of the sealing member to the depth of the second groove is greater than or equal to 10 and less than or equal to 100.

[0016] In some embodiments, the first groove and the second groove are located on the same side of the housing, and a groove depth of the first groove is greater than a groove depth of the second groove.

[0017] In some embodiments, the spacing between adjacent sides of the first groove and the second groove is greater than or equal to 1 mm.

[0018] In some embodiments, the ratio of the width of the sealing member to the width of the second groove is greater than or equal to 30% and less than or equal to 80%.

[0019] In some embodiments, a ratio of a distance between a center of the first weld mark and a center of the second weld mark to a distance between a center of the first groove and a center of the second groove is greater than or equal to 0.8 and less than or equal to 1.2.

[0020] In some embodiments, the sealing member includes a portion recessed into the liquid injection hole and a portion connected to the shell.

[0021] In some embodiments, the sealing member may include a first conductive layer, an insulating rubber layer and a second conductive layer. The first conductive layer is arranged around the injection hole and welded to the second groove. The second conductive layer is located on the side of the first conductive layer away from the shell. The insulating rubber layer is bonded between the first conductive layer and the second conductive layer.

[0022] In some embodiments, the sealing member includes an adhesive layer and a metal layer, the adhesive layer is bonded to the groove wall of the second groove, and the metal layer is connected to a side of the adhesive layer facing away from the shell.

[0023] In some embodiments, the circumferential edge of the shell has a skirt; the projection of the upper surface of the first weld mark in the shell thickness direction is lower than the edge of the skirt; and / or the projection of the upper surface of the second weld mark in the shell thickness direction is lower than the edge of the skirt.

[0024] In some embodiments, the battery may further include a pole, the battery cell has a second pole ear, the shell wall of the shell is provided with a through hole, the pole is passed through the through hole and is at least partially located inside the shell; the second pole ear is welded to the pole.

[0025] The present application provides a battery, which includes a shell and a battery cell located in the shell, wherein a first groove is provided on the outer side of a shell wall of the shell, and the battery cell has a first pole ear, and the first pole ear is opposite to the first groove; the first pole ear is welded to the inner side of the shell wall of the shell and forms a first weld mark; the first weld mark is located in the first groove, thereby reducing the shell thickness in the welding area, so that the welding of the shell and the pole ear is achieved outside the shell, reducing the production and manufacturing cost, and improving the cleanliness of the welding area, so that cold welding and leaking welding can be discovered in time, reducing the risk of welding failure between the shell and the pole ear, and improving the stability of the battery process.

[0026] In addition to the technical problems solved by the present application, the technical features that constitute the technical solutions, and the beneficial effects brought about by the technical features of these technical solutions described above, other technical problems that can be solved by the battery provided by the present application, other technical features included in the technical solutions, and the beneficial effects brought about by these technical features will be further described in detail in the specific implementation methods. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, a brief introduction will be given below to the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0028] Figure 1 A schematic diagram of the structure of a battery provided in an embodiment of the present application;

[0029] Figure 2 An exploded view of a battery provided in an embodiment of the present application;

[0030] Figure 3 A schematic diagram of a first structure of a first weld print of a battery provided in an embodiment of the present application;

[0031] Figure 4 A schematic diagram of a second structure of the first weld print of a battery provided in an embodiment of the present application;

[0032] Figure 5 A third structural schematic diagram of the first weld print of the battery provided in an embodiment of the present application;

[0033] Figure 6 A side view of a battery provided in an embodiment of the present application;

[0034] Figure 7 for Figure 6 Cross-sectional view in CC direction;

[0035] Figure 8 A partial cross-sectional view of the position of the first groove of the battery provided in an embodiment of the present application;

[0036] Fig. 9 A schematic diagram of a first structure of a sealing member of a battery provided in an embodiment of the present application;

[0037] Fig.10 A cross-sectional view of a first structure of a sealing member of a battery provided in an embodiment of the present application;

[0038] Fig.11 A schematic diagram of a second structure of a sealing member of a battery provided in an embodiment of the present application;

[0039] Fig.12 A cross-sectional view of a second structure of a sealing member of a battery provided in an embodiment of the present application.

[0040] Description of reference numerals:

[0041] 10-Battery;

[0042] 100-shell; 101-first groove; 1011-first weld mark; 102-second groove; 1021-second weld mark; 110-main body; 120-cover plate; 130-liquid injection hole; 140-skirt; 150-explosion-proof groove;

[0043] 200-battery cell; 210-first pole ear; 220-second pole ear;

[0044] 300-sealing member; 310-first conductive layer; 320-insulating rubber layer; 330-second conductive layer;

[0045] 400-Pole. DETAILED DESCRIPTION

[0046] In order to make the purpose, technical solutions and advantages of this application clearer, the technical solutions in the embodiments of this application will be clearly and completely described below in conjunction with the drawings in the embodiments of this application. Obviously, the described embodiments are part of the embodiments of this application, not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0047] Batteries are widely used in various power supply devices, including consumer electronics, new energy vehicles, and energy storage devices. Batteries have different sizes and structures depending on the application scenario, and the battery shell can be made of different materials. At present, metal-packaged batteries have good safety. The tabs of the battery cells in metal-packaged batteries need to be welded to the metal shell. Since the tabs are connected to the inner surface of the shell, the shell and the tabs need to be welded from the inside of the shell, that is, from the tab side.

[0048] However, the current battery tab welding operation is performed on the tab side, resulting in higher manufacturing and time costs for the battery. At the same time, during the battery preparation process, the welding condition of the tab cannot be directly confirmed. Therefore, cold solder joints and leaking solder joints cannot be detected, and the process stability is low.

[0049] The present application provides a battery, which reduces the shell thickness in the welding area by arranging a groove on the outer surface of the shell and welding the side surface of the bottom of the groove toward the inside of the shell to the pole ear, so that the welding of the shell and the pole ear is achieved outside the shell, reducing the production and manufacturing cost, and improving the cleanliness of the welding area. It is possible to detect cold welding and leaking welding in time, reducing the risk of welding failure between the shell and the pole ear, and improving the stability of the battery process.

[0050] The battery of the embodiment of the present application is described below in conjunction with the accompanying drawings. It should be noted that the battery provided in the embodiment of the present application can be a secondary battery, that is, the battery in the embodiment of the present application can be charged and discharged and recycled, and the specific type of the battery can include but is not limited to lithium batteries, lithium cobalt oxide batteries, lithium iron phosphate batteries, ternary batteries, etc., and the battery and the scene in which the battery can be used include but are not limited to electronic products, communication equipment, transportation, etc., such as mobile phones, computers, new energy vehicles and other products, and the embodiment of the present application does not specifically limit this.

[0051] Figure 1 A schematic diagram of the structure of a battery provided in an embodiment of the present application, Figure 2 An exploded diagram of a battery provided in an embodiment of the present application, Figure 3 A schematic diagram of a first structure of a first weld mark of a battery provided in an embodiment of the present application.

[0052] Please refer to Figures 1 to 3 An embodiment of the present application provides a battery 10, which includes a shell 100 and a battery cell 200. The battery cell 200 is located inside the shell 100, and the battery cell 200 has a first pole ear 210. A first groove 101 is provided on the outer side of the shell wall of the shell 100, and the first pole ear 210 is opposite to the first groove 101. The first pole ear 210 is welded to the inner side of the shell wall of the shell 100.

[0053] The shell wall of the housing 100 is thinner at the position of the first groove 101 than at other positions of the housing 100, and the position where the first pole tab 210 is welded to the inner wall of the housing 100 is located below the first groove 101, that is, the first pole tab 210 is welded to the surface of the bottom wall of the first groove 101 facing the inner side of the housing 100, so when the pole tab is welded to the housing 100, the welding can be performed on the outside of the housing 100, that is, on the side where the first groove 101 is located. The welding of the first pole tab 210 and the housing 100 can form a first weld mark 1011, and the first weld mark 1011 is located in the first groove 101.

[0054] It is understandable that since the welding operation between the first pole tab 210 and the shell 100 is performed outside the shell 100, the manufacturing cost and time cost in the production process can be reduced, and the production efficiency can be improved. And since the first weld mark 1011 formed is located in the first groove 101, that is, the first weld mark 1011 is located outside the shell 100, the welding condition of the shell 100 and the first pole tab 210 can be clearly seen outside the shell 100, so as to accurately judge whether there is a cold weld or a leaky weld between the shell 100 and the first pole tab 210, so as to ensure the stability of the battery 10 process.

[0055] It should be noted that in the battery 10 provided in the embodiment of the present application, the thickness of the shell 100 in the welding area is reduced by setting the first groove 101 on the outer surface of the shell 100, and the first pole ear 210 is welded through the side surface of the bottom of the first groove 101 facing the inside of the shell 100, thereby avoiding the occurrence of cold welding and leaking welding. In addition, the first groove 101 can improve the cleanliness of the welding area, reduce the risk of welding failure between the shell 100 and the pole ear, and thus improve the stability of the battery 10 process.

[0056] In the embodiment of the present application, the first groove 101 on the outer surface of the shell 100 can also provide positioning for the welding operation between the shell 100 and the first pole tab 210 , thereby ensuring the accuracy of the welding position of the first pole tab 210 and improving the welding accuracy between the first pole tab 210 and the shell 100 .

[0057] In addition, since the position of the first groove 101 reduces the thickness of the shell 100, that is, the thickness of the shell 100 with the first groove 101 is less than the thickness of other positions of the shell 100, the height of the first weld mark 1011 set in the groove is also reduced, avoiding the first weld mark 1011 from exceeding the size boundary of the shell 100. In this way, a larger accommodating space is provided for the installation of components such as the external circuit board of the battery 10, and the design of the external protection plate can be simplified.

[0058] In some embodiments, the housing 100 may be made of a conductive metal material, including but not limited to aluminum, iron and other metals or alloys. The embodiment of the present application does not specifically limit the type of metal material used.

[0059] Exemplarily, the battery cell 200 of the battery 10 may include a positive electrode tab and a negative electrode tab, and the first electrode tab 210 may be a negative electrode tab.

[0060] Figure 6 A side view of a battery provided in an embodiment of the present application, Figure 7 for Figure 6 Cross-sectional view in CC direction, Figure 8 A partial cross-sectional view of the position of the first groove of the battery provided in an embodiment of the present application.

[0061] Please continue to refer to Figures 6 to 8 , and combined with Figures 1 to 3 In some embodiments, the ratio of the area of ​​the first weld mark 1011 to the bottom area of ​​the first groove 101 is greater than or equal to 15% and less than or equal to 45%. This arrangement improves the welding efficiency between the housing 100 and the first tab 210 while ensuring that the first tab 210 and the housing 100 have good welding strength and welding reliability.

[0062] Exemplarily, the area of ​​the first weld mark 1011 is S1, the bottom area of ​​the first groove 101 is S2, and the specific values ​​of the ratio of S1 to S2 include but are not limited to 15%, 16%, 20%, 25%, 30%, 35%, 40%, 44%, 45%, etc., which are not specifically limited to the embodiments of the present application.

[0063] In some embodiments, the shape of the first groove 101 can be square, circular, elliptical, trapezoidal or other shapes, as long as the first electrode tab 210 and the shell 100 can form a reliable welding relationship, and the embodiments of the present application do not make specific limitations on this.

[0064] Figure 4 A second structural schematic diagram of the first weld print of the battery provided in the embodiment of the present application, Figure 5 A third structural schematic diagram of the first weld mark of a battery provided in an embodiment of the present application.

[0065] For example, Figure 3 As shown, combined with Figure 1 and Figure 2 The first weld mark 1011 may include a plurality of weld segments disposed at intervals, and the plurality of weld segments disposed at intervals are connected end to end, thereby improving the welding reliability between the housing 100 and the first electrode tab 210 .

[0066] For example, Figure 4 As shown, combined with Figure 1 and Figure 2 The first weld mark 1011 may be spiral-shaped, and the spiral weld mark may extend along the length direction of the first groove 101 and form a plurality of spiral centers, thereby improving the welding reliability between the shell 100 and the first electrode tab 210 .

[0067] For example, Figure 5 As shown, combined with Figure 1 and Figure 2 The first weld mark 1011 may include a plurality of weld marks arranged at intervals, the plurality of weld marks arranged at intervals are parallel to each other, and the plurality of weld marks arranged at intervals extend along the length direction of the first groove 101 , thereby improving the welding reliability between the shell 100 and the first pole ear 210 .

[0068] Fig. 9 A schematic diagram of a first structure of a battery sealing member provided in an embodiment of the present application, Fig.10 A cross-sectional view of a first structure of a sealing member for a battery provided in an embodiment of the present application.

[0069] Please refer to Fig. 9 and Fig.10 , and combined with Figure 1 , Figure 2 , Figure 6 and Figure 7 In the embodiment of the present application, the housing 100 may be provided with an injection hole 130, and the battery 10 may inject electrolyte into the housing 100 through the injection hole 130, and the battery cell 200 is immersed in the electrolyte. The battery 10 may also include a sealing member 300, and after the electrolyte is injected, the injection hole 130 is sealed by the sealing member 300 to ensure that the injection hole 130 has good sealing. The specific connection method and corresponding structure of the sealing member 300 on the housing 100 are described in detail below.

[0070] In some embodiments, a second groove 102 may be provided on the outer side of the shell wall of the shell 100 , the injection hole 130 may be provided in the second groove 102 , and the sealing member 300 is at least partially located in the second groove 102 to seal the injection hole 130 .

[0071] The sealing member 300 is connected to the groove wall of the second groove 102 , including but not limited to bonding, welding, etc.

[0072] Exemplarily, the sealing member 300 is welded to the groove wall of the second groove 102, and a second weld mark 1021 is formed. When the sealing member 300 is welded to the housing 100, the welding operation can be performed outside the housing 100, and the formed second weld mark 1021 is located on the upper surface of the sealing member 300. In this way, the welding strength and welding reliability of the sealing member 300 and the housing 100 can be improved.

[0073] In addition, the second groove 102 can be provided to locate the welding position of the sealing member 300 , thereby improving the welding position accuracy of the sealing member 300 , and further improving the reliability of the sealing of the sealing member 300 to the injection hole 130 .

[0074] It should be noted that after the electrolyte is injected into the shell 100, the second groove 102 can be made on the outer wall of the shell 100 by laser, so that the residual crystals of the electrolyte can be removed when the second groove 102 is formed, ensuring the cleanliness of the welding position of the sealing member 300 when sealing the injection hole 130, and avoiding poor sealing. In addition, the problem of electrolyte overflow during the welding process is avoided, the packaging reliability of the sealing member 300 to the shell 100 is improved, and the consistency of the appearance of the shell 100 is ensured.

[0075] In some embodiments, the thickness of the sealing member 300 is greater than the depth of the second groove 102. In this way, at least part of the sealing member 300 can be accommodated by the second groove 102, thereby improving the sealing reliability of the sealing member 300 and avoiding interference between the sealing member 300 and components such as the protective plate outside the housing 100.

[0076] In some embodiments, the ratio of the thickness of the sealing member 300 to the depth of the second groove 102 is greater than or equal to 10 and less than or equal to 100.

[0077] Exemplarily, the thickness dimension of the sealing member 300 is H1, the depth dimension of the second groove 102 is H2, and the specific ratio of H1 to H2 can be 10, 11, 20, 30, 50, 70, 90, 99, 100, etc., which is not specifically limited in the embodiments of the present application.

[0078] In some embodiments, the first groove 101 and the second groove 102 are located on the same side of the housing 100, and the groove depth of the first groove 101 is greater than the groove depth of the second groove 102. Such an arrangement can improve the welding strength between the housing 100 and the tab.

[0079] It can be understood that the thickness of the shell 100 at the position of the first groove 101 is smaller than the thickness of the shell 100 at the position of the second groove 102 .

[0080] In some embodiments, the spacing between the adjacent sides of the first groove 101 and the second groove 102 is greater than or equal to 1 mm. This arrangement can prevent the first weld mark 1011 formed by welding the second electrode tab 220 from interfering with the second weld mark 1021 formed by welding the sealing member 300, so that the first weld mark 1011 and the second weld mark 1021 overlap during the welding process, thereby avoiding heat accumulation on the surface of the housing 100.

[0081] For example, the specific value of the spacing dimension between adjacent sides of the first groove 101 and the second groove 102 can be 1 mm, 1.1 mm, 2 mm, 5 mm, 10 mm, 20 mm, etc., which is not specifically limited in the embodiment of the present application.

[0082] In some embodiments, the ratio of the width of the sealing member 300 to the width of the second groove 102 is greater than or equal to 30% and less than or equal to 80%. In this way, the sealing member 300 can be ensured to completely seal the injection hole 130, improve the sealing reliability, and improve the welding strength and welding reliability between the sealing member 300 and the housing 100.

[0083] Exemplarily, the specific values ​​of the ratio of the width dimension of the sealing member 300 to the width dimension of the second groove 102 include but are not limited to 30%, 31%, 40%, 50%, 60%, 70%, 79%, 80%, etc., which are not specifically limited in the embodiments of the present application.

[0084] In some embodiments, the ratio of the distance between the center of the first weld mark 1011 and the center of the second weld mark 1021 to the distance between the center of the first groove 101 and the center of the second groove 102 is greater than or equal to 0.8 and less than or equal to 1.2. In this way, it can be ensured that when forming the first weld mark 1011 and the second weld mark 1021, the two welding processes will not affect each other, thereby ensuring the welding reliability between the first electrode tab 210 and the sealing member 300 and the housing 100, and improving the convenience of process implementation.

[0085] For example, the distance D1 between the center of the first weld mark 1011 and the center of the second weld mark 1021, the distance D2 between the center of the first groove 101 and the center of the second groove 102, and the ratio of D1 to D2 can be 0.8, 0.81, 0.9, 1.0, 1.1, 1.19, 1.2, etc., which is not specifically limited in the embodiments of the present application.

[0086] It should be noted that the sealing member 300 in the embodiment of the present application may be a single-layer metal sheet structure. Alternatively, the sealing member 300 may be a multi-layer composite sheet structure. The multi-layer structure of the sealing member 300 is exemplarily described below.

[0087] In some embodiments, Fig.10 As shown, the sealing member 300 includes a portion recessed into the injection hole 130 and a portion connected to the housing 100. Exemplarily, the sealing member 300 is a single-layer metal sheet, and the area of ​​the single-layer metal sheet opposite to the injection hole 130 is recessed into the injection hole 130. This arrangement ensures that the injection hole 130 has good sealing performance.

[0088] Fig.11A schematic diagram of a second structure of a sealing member of a battery provided in an embodiment of the present application, Fig.12 A cross-sectional view of a second structure of a sealing member of a battery provided in an embodiment of the present application.

[0089] Please refer to Fig.11 and Fig.12 , and combined with Figure 1 , Figure 2 , Figure 6 and Figure 7 In some embodiments, the sealing member 300 may include a first conductive layer 310, an insulating rubber layer 320 and a second conductive layer 330. The first conductive layer 310 is arranged around the injection hole 130 and is welded to the second groove 102. The second conductive layer 330 is located on the side of the first conductive layer 310 away from the shell 100, and the insulating rubber layer 320 is bonded between the first conductive layer 310 and the second conductive layer 330.

[0090] It is understandable that the insulating adhesive layer 320 may be a hot melt adhesive film layer, and when the pressure inside the housing 100 of the battery 10 needs to be released at high temperature, the meltable insulating adhesive layer 320 is used to release the pressure. While ensuring that the injection hole 130 has good sealing, when the pressure inside the battery 10 needs to be released, the insulating adhesive layer 320 can melt at high temperature so that the pressure can be released from the injection hole 130, and at normal temperature, the first conductive layer 310 and the second conductive layer 330 are located on both sides of the insulating adhesive layer 320, and cooperate to have good strength and stability to improve the sealing reliability of the injection hole 130.

[0091] In other embodiments, the sealing member 300 may be a two-layer structure. The sealing member 300 may include an adhesive layer and a metal layer, wherein the adhesive layer is bonded to the groove wall of the second groove 102, and the metal layer is connected to the side of the adhesive layer away from the housing 100. While ensuring that the injection hole 130 has good sealing, when the pressure inside the battery 10 needs to be released, the adhesive layer can melt at a high temperature so that the pressure can be released from the injection hole 130.

[0092] In addition, an explosion-proof groove 150 may be provided on the surface of the shell 100, and the explosion-proof groove 150 is used to realize the pressure relief function of the shell 100. The multi-layer composite structure at the position of the sealing member 300 can assist the explosion-proof groove 150 in pressure relief.

[0093] Exemplarily, the insulating rubber layer 320 has good corrosion resistance to prevent corrosion by the electrolyte. Exemplarily, the materials that can be used for the insulating rubber layer 320 include, but are not limited to, polystyrene, polypropylene, polyethylene, polyester, polyvinyl chloride, polyimide, acrylonitrile-butadiene-styrene plastic, polycarbonate, polyamide, acid-modified resin, polyethylene, polyhydroxyacetylethylenediamine, modified polyolefin resin, polyolefin, polyvinyl chloride, fluororubber, other polyolefins and copolymers thereof, epoxy acrylate and polyurethane acrylate, etc., which are not specifically limited in the embodiments of the present application.

[0094] In some embodiments, the circumferential edge of the housing 100 has a skirt 140, and the projection of the upper surface of the first weld mark 1011 in the thickness direction of the housing 100 is lower than the edge of the skirt 140. This arrangement can ensure that the first weld mark 1011 does not exceed the size boundary of the housing 100, thereby increasing the space available for subsequent assembly of the battery 10.

[0095] In some embodiments, the projection of the upper surface of the second weld mark 1021 in the thickness direction of the housing 100 is lower than the edge of the skirt 140. This arrangement ensures that the second weld mark 1021 does not exceed the size boundary of the housing 100, thereby increasing the space available for subsequent assembly of the battery 10.

[0096] The thickness direction of the shell 100 is Figure 6 The X direction in .

[0097] In some embodiments, the battery 10 may further include a pole 400, the battery cell 200 has a second pole ear 220, the shell wall of the shell 100 is provided with a through hole, the pole 400 is passed through the through hole and is at least partially located inside the shell 100; the pole 400 is provided with a welding hole, the second pole ear 220 is opposite to the welding hole and is welded to the pole 400.

[0098] It can be understood that the pole 400 includes a column and a flange, the column is inserted into the through hole, and the flange is located outside the shell 100. The protective plate outside the shell 100 can be welded to the flange of the pole 400, and the second pole ear 220 inside the shell 100 can be welded to the column, and the weld mark is located on the welding hole. In this way, no other connecting parts are required, which reduces the production cost and improves the overall energy density of the battery 10.

[0099] Exemplarily, the electrode post 400 may be a positive electrode post, and the second electrode tab 220 may be a positive electrode tab.

[0100] It should be noted that the shell 100 of the battery 10 provided in the embodiment of the present application may include a main body 110 and a cover plate 120 , and the main body 110 and the cover plate 120 are covered and welded to each other, thereby enclosing a closed space for accommodating the battery cell 200 .

[0101] The following is an exemplary description of the assembly process of the battery cell 200 in the battery 10 .

[0102] Step 1: Fix the positive electrode ear to the pole 400 on the shell 100 by laser welding, and fix the negative electrode ear of the battery cell 200 to the negative pole on the shell 100 by laser welding. Then place the battery cell 200 in the shell 100.

[0103] Step 2: Fix the negative electrode ear to the shell 100 by a clamp, and the negative electrode ear is located at the projection position of the first groove 101 perpendicular to the shell wall; and electrically connect the shell 100 and the second electrode ear 220 by laser welding or resistance welding.

[0104] Step 3: Fix the main body 110 and the cover plate 120 of the housing 100 after assembling the battery cell 200 by a clamp, and assemble the two together by laser welding.

[0105] Step 4: Place the assembled battery cell 200 in an oven and bake it at a certain temperature for a certain period of time to remove moisture from the battery cell 200.

[0106] Step 5: inject a certain amount of electrolyte into the battery cell 200 through the injection hole 130 , and then seal the injection hole 130 with the sealing member 300 .

[0107] The embodiment of the present application provides a battery 10, which includes a shell 100 and a battery cell 200 located in the shell 100, the shell wall of the shell 100 is provided with a first groove 101, and the battery cell 200 has a first pole ear 210, and the first pole ear 210 is opposite to the first groove 101; the first pole ear 210 is welded to the inner side of the shell wall of the shell 100, and a first weld mark 1011 is formed; the first weld mark 1011 is located in the first groove 101, thereby reducing the thickness of the shell 100 in the welding area, so that the welding of the shell 100 and the pole ear is realized outside the shell 100, reducing the production manufacturing cost, and improving the cleanliness of the welding area, so that the situation of cold welding and leaking welding can be discovered in time, reducing the risk of welding failure between the shell 100 and the pole ear, and improving the stability of the battery 10 process.

[0108] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, or it can be an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0109] In the description of the present application, it should be understood that the terms "upper", "lower", "front", "back", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0110] The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of this application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the application described herein can be implemented in an order other than those illustrated or described herein.

[0111] In addition, the terms "comprises," "comprising," and "having," and any variations thereof, are intended to cover non-exclusive inclusions. For example, a process, method, system, product, or apparatus that includes a series of steps or elements is not necessarily limited to those steps or elements explicitly listed, but may include other steps or elements not explicitly listed or inherent to such process, method, product, or apparatus.

[0112] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. A battery, characterized in that: It includes a shell and a battery cell located in the shell, the outer side of the shell wall of the shell is provided with a first groove, the battery cell has a first pole ear, and the first pole ear is opposite to the first groove; the first pole ear is welded to the inner side of the shell wall of the shell to form a first weld mark; the first weld mark is located in the first groove.

2. The battery according to claim 1, characterized in that The ratio of the area of ​​the first weld mark to the bottom area of ​​the first groove is greater than or equal to 15% and less than or equal to 45%.

3. The battery according to claim 1 or 2, characterized in that: The first weld print includes a plurality of weld segments; the plurality of weld segments are sequentially connected end to end; or, The first weld mark is spiral; or The first weld mark includes a plurality of welding segments; the plurality of welding segments are arranged at intervals.

4. The battery according to claim 1 or 2, characterized in that: It also includes a sealing member. A second groove is provided on the outer side of the shell wall of the shell. A liquid injection hole is provided in the second groove. The sealing member seals the liquid injection hole. The sealing member is connected to the groove wall of the second groove.

5. The battery according to claim 4, characterized in that The sealing member is welded to the groove wall of the second groove to form a second weld mark.

6. The battery according to claim 4, characterized in that The thickness of the sealing member is greater than the depth of the second groove.

7. The battery according to claim 6, characterized in that The ratio of the thickness of the sealing member to the depth of the second groove is greater than or equal to 10 and less than or equal to 100.

8. The battery according to claim 4, characterized in that The first groove and the second groove are located on the same side of the housing.

9. The battery according to claim 8, characterized in that The groove depth of the first groove is greater than the groove depth of the second groove.

10. The battery according to claim 4, characterized in that The distance between adjacent sides of the first groove and the second groove is greater than or equal to 1 mm.

11. The battery according to claim 4, characterized in that The ratio of the width of the sealing member to the width of the second groove is greater than or equal to 30% and less than or equal to 80%.

12. The battery according to claim 5, characterized in that A ratio of a distance between a center of the first weld mark and a center of the second weld mark to a distance between a center of the first groove and a center of the second groove is greater than or equal to 0.8 and less than or equal to 1.

2.

13. The battery according to claim 5, characterized in that The sealing member includes a portion recessed into the liquid injection hole and a portion connected to the shell.

14. The battery according to claim 5, characterized in that The sealing member includes a first conductive layer, an insulating rubber layer and a second conductive layer. The first conductive layer is arranged around the injection hole and welded to the second groove. The second conductive layer is located on the side of the first conductive layer away from the shell. The insulating rubber layer is bonded between the first conductive layer and the second conductive layer.

15. The battery according to claim 4, characterized in that The sealing member comprises an adhesive layer and a metal layer, the adhesive layer is bonded to the groove wall of the second groove, and the metal layer is connected to a side of the adhesive layer away from the shell.

16. The battery according to claim 5, characterized in that The circumferential edge of the shell has a skirt; the projection of the upper surface of the first weld mark in the thickness direction of the shell is lower than the edge of the skirt; and / or the projection of the upper surface of the second weld mark in the thickness direction of the shell is lower than the edge of the skirt.

17. The battery according to claim 1 or 2, characterized in that: It also includes a pole, the battery core has a second pole ear, the shell wall of the shell is provided with a through hole, the pole is passed through the through hole and is at least partially located inside the shell; the second pole ear is welded to the pole.