Preparation equipment of silicon monoxide / carbon composite material

By connecting the reaction zone and the deposition and coating zone in the silicon oxide/carbon composite preparation equipment, a one-step preparation of silicon oxide/carbon composite materials is achieved, and the problems of cumbersome production processes, long cycles and high energy consumption in the existing technology are solved. , improves the economical and production efficiency of materials.

CN222082436UActive Publication Date: 2024-11-29HUANXIN DIBO (ANHUI) NEW ENERGY R&D CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420237550.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-31
Publication Date
2024-11-29
Estimated Expiration
2034-01-31

AI Technical Summary

Technical Problem

In the prior art, the two-step method is generally used to produce silicon oxide/carbon composite materials, which leads to problems such as cumbersome production processes, long cycles, high energy consumption and high cost.

Method used

Design a preparation equipment for silicon oxide/carbon composite materials, and realize the preparation of SiO and SiO@C composite materials through the uniting reaction zone and the deposition and coating zone. Silicon and silicon dioxide under negative pressure and heating conditions Co-deposition with carbon elements simplifies process flow and reduces energy consumption.

Benefits of technology

The simplified preparation process of SiO@C composite materials is realized, shortening production cycles, reducing energy consumption and cost, and improving the economics of the materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222082436U_ABST
    Figure CN222082436U_ABST
Patent Text Reader

Abstract

The utility model provides preparation equipment of a silicon monoxide / carbon composite material, which comprises a reaction area and a deposition coating area which are communicated with each other, and during reaction, the reaction area and the deposition coating area are in a negative pressure heating state; during reaction, silicon and silicon dioxide are contained in the reaction area, generated silicon monoxide enters the reaction area, and the silicon monoxide and the carbon element are co-deposited to obtain the silicon monoxide / carbon composite material. According to the preparation equipment of the silicon monoxide / carbon composite material, integration of preparation of SiO and preparation of the SiO (at) C composite material is realized through the reaction region and the deposition coating region which are arranged in a communicating manner, and the SiO (at) C composite material serving as a negative electrode is directly obtained from silicon / silicon oxide. The whole process can be realized only through one-time feeding operation, and only the temperature of the reaction area and the temperature of the deposition coating area need to be controlled at the same time, so that the economical efficiency of the SiO-C composite material is improved from multiple aspects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of preparation of composite materials of silicon monoxide (SiO) and carbon, in particular to equipment for preparing the silicon monoxide / carbon composite material. Background Art

[0002] In recent years, lithium-ion batteries have become the preferred power source for 3C products, electric vehicle batteries, power tool batteries, energy storage batteries, etc. due to their excellent charge and discharge cycle performance. At present, the negative electrode material in commercial lithium-ion batteries is mainly graphite materials, and the theoretical capacity of graphite materials is 372mAh / g, which limits the further improvement of the energy density of lithium-ion batteries. Therefore, SiO with higher specific capacity (about 1400mA / g) has entered people's field of vision. However, due to its high cost, the progress of introducing it into batteries is still relatively slow.

[0003] Currently practical SiO-based negative electrode materials usually have a composite component of SiO@C (silicon dioxide and carbon) to improve the service life of the SiO negative electrode. However, the method for producing SiO@C composite materials under the prior art generally adopts a two-step method, that is, first synthesizing SiO based on silicon and silicon oxide, and then realizing carbon coating of SiO based on different processes to form the final SiO@C composite material with a carbon-coated structure. Common carbon coating processes have been disclosed in invention patent applications such as CN111653739B and CN111689500A, that is, mixing and granulating materials based on SiO and C, and then calcining at high temperature. The main problem with similar two-step production methods is that the production process is relatively cumbersome, resulting in a long production cycle, high energy consumption, and high costs. Utility Model Content

[0004] Aiming at the problem that the existing SiO@C composite materials used for battery negative electrodes are mainly produced by a two-step process, which has complicated processes and high costs, the utility model provides a preparation device for a silicon oxide / carbon composite material which can realize the preparation of SiO and SiO@C materials in one step.

[0005] The technical solution of the utility model provides a preparation device for silicon monoxide / carbon composite material, comprising a reaction zone and a deposition coating zone which are interconnected. During the reaction, the reaction zone and the deposition coating zone are in a negative pressure heating state;

[0006] During the reaction, silicon and silicon dioxide are placed in the reaction zone, and silicon oxide is generated and enters the reaction zone. The internal silicon oxide is co-deposited with carbon elements to obtain a silicon oxide / carbon composite material.

[0007] Preferably, the deposition coating area is provided with a gas inlet, and during the reaction, the gas inlet provides a carbon source.

[0008] Preferably, the carbon source is a single substance or a mixture of carbon-containing organic gases.

[0009] Preferably, the deposition coating zone is provided with a gas outlet, and the gas outlet is connected to an external negative pressure device to maintain a negative pressure environment of the reaction zone and the deposition coating zone system.

[0010] Preferably, the reaction zone further includes a material holding zone and a transition zone, the material holding zone contains silicon powder and silicon dioxide powder, the transition zone connects the material holding zone and the deposition coating zone, and during the reaction, silicon dioxide vapor enters the deposition coating zone from the transition zone.

[0011] Preferably, the material holding area comprises a first reaction area and a second reaction area which are separated from each other, the first reaction area and the second reaction area are respectively connected to the deposition coating area, and the first reaction area and the second reaction area are respectively used to hold silicon powder and silicon dioxide powder.

[0012] The preparation equipment of silicon monoxide / carbon composite material of the utility model realizes the integration of the preparation of SiO and the preparation of SiO@C composite material by connecting the reaction zone and the deposition coating zone, and realizes the direct acquisition of SiO@C composite material as the negative electrode from silicon / silicon oxide. The whole process can be realized by only one feeding operation, and it is only necessary to control the temperature of the reaction zone and the deposition coating zone at the same time, which simplifies the preparation process of the terminal product SiO@C composite material, compresses the production cycle of the whole process, and realizes the integration of the two-step reaction, reduces the heating process and reduces the reaction energy consumption, and improves the economy of SiO@C composite material from many aspects. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a schematic structural diagram of a preparation device for silicon dioxide / carbon composite material of the utility model;

[0014] Figure 2 It is a structural schematic diagram of another embodiment of the preparation equipment of silicon monoxide / carbon composite material of the utility model.

[0015] In the figure,

[0016] 1: reaction zone 2: deposition and coating zone 21: gas outlet 22: gas inlet 11: material holding zone 12: transition zone 1A: first reaction zone 1B: second reaction zone DETAILED DESCRIPTION

[0017] The following is a detailed description of the present invention in conjunction with the accompanying drawings and specific embodiments. In this specification, the size ratios in the drawings do not represent the actual size ratios, but are only used to reflect the relative position relationship and connection relationship between the components. Components with the same name or the same number represent similar or identical structures and are only for illustrative purposes.

[0018] The preparation equipment of silicon oxide / carbon composite material of the utility model mainly realizes the integration of SiO preparation and SiO@C composite material preparation, and realizes obtaining SiO@C composite material from silicon / silicon oxide in one step in the same device. Its main technical scheme is to prepare silicon oxide by converting silicon-silicon oxide in the same device, and add a carbon source to provide copper element when depositing silicon oxide, so that carbon element is deposited and coated on the surface of silicon oxide when depositing silicon oxide.

[0019] Specifically, Figure 1 It is a structural schematic diagram of a preparation device for silicon dioxide / carbon composite materials. It includes a reaction zone 1 and a deposition coating zone 2, and the reaction zone 1 is connected to the deposition coating zone 2. The reaction zone 1 and the deposition coating zone 2 are sealed during the reaction and maintain the required negative pressure state, which is usually achieved by an external vacuum pumping device. During the reaction, the reaction zone 1 and the deposition coating zone 2 are under negative pressure and at a certain temperature. A mixed powder of Si and SiO is placed in the reaction zone 1 to generate SiO. Under high temperature conditions, SiO evaporates into the deposition coating zone 2 and can be deposited in the deposition coating zone 2 due to the temperature difference. In addition to the air outlet 21 for vacuuming, the deposition coating zone 2 also has an air inlet 22 for air intake. One of the functions of the air outlet 21 is to prepare and maintain the vacuum environment of the reaction zone 1 and the deposition coating zone 2 system. The function of the air inlet 22 is to introduce specific gas components into the reaction system. For example, a carbon source can be introduced during the reaction process, or an inert gas can be introduced through the air inlet 22 during the preparation of the experiment or at the end of the experiment to ensure the reaction environment and reaction products. The function of the air outlet 21 is to discharge the air in the reaction zone 1 and the deposition coating zone 2 system so that the system can maintain a certain negative pressure state. When the reaction is in progress, the air inlet 22 is also used to provide a carbon source, which is a carbon-containing organic gas, such as methane, ethylene, acetylene, etc. In the negative pressure vacuum and heating state of the deposition coating zone 2, the carbon source will crack to obtain a carbon element, and the SiO vapor obtained from the reaction zone 1 will enter the deposition coating zone 2. SiO and the cracked C element are mixed and deposited in the deposition coating zone 2, directly forming a SiO@C composite material with a uniform C coating structure. The reaction zone 1 generally includes a material holding zone 11 and a transition zone 12, wherein the transition zone 12 connects the material holding zone 11 and the deposition coating zone 2, and silicon and / or silicon oxide is placed in the material holding zone 11. Generally, after the temperature in the material holding zone 11 during the reaction is reached, the steam can enter the deposition coating zone 2 through the transition zone 12.

[0020] Figure 2It is a specific embodiment of the preparation equipment of silicon dioxide / carbon composite material. The reaction zone 1 can be further divided into a first reaction zone 1A and a second reaction zone 1B, and the first reaction zone 1A and the second reaction zone 1B are both connected to the deposition coating zone 2. The first reaction zone 1A and the second reaction zone 1B are respectively used to contain Si powder and SiO2 powder. After heating, the steam is gathered in the deposition coating zone 2 and fully reacted in the deposition coating zone 2 to obtain SiO vapor. At the same time, the carbon element obtained by the cracking of the carbon source entering the air inlet 22 is deposited in the deposition coating zone 2 together with the SiO in the deposition coating zone 2 to obtain the desired SiO@C composite material product. After Si and SiO are separated and stored, it can be ensured that Si vapor and SiO vapor converge in the deposition coating zone 2 in a controlled manner, thereby ensuring that SiO can be generated and deposited in the deposition coating zone 2 in a directional manner, thereby improving the conversion rate of the product.

[0021] In the specific reaction control process, after the Si powder and SiO2 powder are placed in the first reaction zone 1A and the second reaction zone 1B, the system is sealed, and the vacuum is started through the gas outlet 21 and the vacuum degree of the system is maintained, and the first reaction zone 1A, the second reaction zone 1B and the transition section between the first reaction zone 1A and the second reaction zone 1B are heated at the same time. When the first reaction zone 1A and the second reaction zone 1B are heated, the deposition coating zone 2 is opened for heating, and the temperature of the first reaction zone 1A and the second reaction zone 1B is maintained at above 1300°C, and the temperature in the deposition coating zone 2 is maintained at above 700°C. The gas inlet 22 is opened, and the carbon source is input from the gas inlet 22 into the deposition coating zone 2, and the gas flow rate is kept basically stable. After keeping the temperature for 12 hours, the carbon source input of the gas inlet 22 is closed, and after all temperatures are lowered to room temperature and the pressure of the system is restored, the deposition coating zone 2 is opened to collect and obtain the SiO@C composite material. Preferably, during the heating process, the heating start time of the deposition coating zone 2 can be slightly later than the heating timing of the reaction zone 1. Usually, the heating operation of the deposition coating zone 2 can be started after the temperature of the reaction zone 1 rises to 900°C, so that the reaction zone 1 and the deposition coating zone 2 in the system reach the temperature required for the reaction basically synchronously.

[0022] The above content is only a description of the preferred implementation mode of the utility model, and does not limit the scope of the utility model. Without departing from the design spirit of the utility model, various modifications and improvements made to the technical solution of the utility model by ordinary technicians in this field should fall within the protection scope determined by the claims of the utility model.

Claims

1. A preparation device for a silicon oxide / carbon composite material, characterized in that: It comprises a reaction zone (1) and a deposition coating zone (2) which are interconnected. During the reaction, the reaction zone (1) and the deposition coating zone (2) are in a negative pressure heating state; During the reaction, silicon and silicon dioxide are placed in the reaction zone (1), and silicon dioxide is generated and enters the reaction zone (1). The silicon dioxide is co-deposited with carbon to obtain a silicon dioxide / carbon composite material.

2. The preparation equipment of silicon dioxide / carbon composite material according to claim 1, characterized in that: The deposition coating area (2) is provided with a gas inlet (22), and during the reaction, the gas inlet (22) provides a carbon source.

3. The preparation equipment of silicon dioxide / carbon composite material according to claim 2, characterized in that: The carbon source is a single substance or a mixture of carbon-containing organic gases.

4. The preparation equipment of silicon dioxide / carbon composite material according to claim 1, characterized in that: The deposition coating zone (2) is provided with a gas outlet (21), and the gas outlet (21) is connected to an external negative pressure device to maintain a negative pressure environment of the reaction zone (1) and the deposition coating zone (2) system.

5. The preparation equipment of silicon dioxide / carbon composite material according to claim 1, characterized in that: The reaction zone (1) further comprises a material holding zone (11) and a transition zone (12); silicon powder and silicon dioxide powder are held in the material holding zone (11); the transition zone (12) connects the material holding zone (11) and the deposition coating zone (2); during the reaction, silicon dioxide vapor enters the deposition coating zone (2) from the transition zone (12).

6. The preparation equipment of silicon dioxide / carbon composite material according to claim 5, characterized in that: The material holding area (11) comprises a first reaction area (1A) and a second reaction area (1B) which are separated from each other, the first reaction area (1A) and the second reaction area (1B) are respectively connected to the deposition coating area (2), and the first reaction area (1A) and the second reaction area (1B) are respectively used to hold silicon powder and silicon dioxide powder.