Neodymium iron boron powder charging device
By designing a NdFeB powder charging device with a compartment cotton and a vacuum environment, the problem of temperature instability in the production of NdFeB magnets is solved, and the stable control of powder temperature and the consistency of product performance is achieved.
Patent Information
- Application Number
- CN202420558223.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-21
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-03-21
AI Technical Summary
During the production process of traditional neodymium iron boron magnets, the temperature of the neodymium iron boron powder charging device is unstable, which affects the consistency of product performance.
A neodymium iron boron powder charging device including the outer tank body and the inner tank body is designed. The inner tank body is equipped with a partition cotton to form a vacuum environment. It uses non-magnetic stainless steel alloy material, and the angle is designed to prevent powder. Material accumulation, inflation and deflation valves control powder flow.
Effectively maintain the powder within the optimal temperature range, reduce temperature fluctuations, and improve product consistency.
Smart Images

Figure CN222088401U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of NdFeB magnets, in particular to a NdFeB powder charging device. Background Art
[0002] The traditional production process of NdFeB magnets includes smelting process, airflow grinding process, molding process, sintering process, etc. After the airflow grinding process is completed, the NdFeB powder in the powder loading device is placed into the mold according to the powder weight required by the process, and then pressed into NdFeB magnet blocks, and the same production action is repeated many times. In the actual production process, the powder loading weight of the NdFeB powder loading device is about 400kg, and the unit weight of the molding production is about 600g-800g / mold. The time used to press 1 mold is 1min. In this way, it takes about 10 hours to produce each can of product. The optimal temperature of NdFeB powder is 16℃-25℃. Long-term production will cause the powder temperature in the loading device to change with the change of the external temperature. Temperature is an important factor affecting product performance, which in turn affects product consistency. Utility Model Content
[0003] In view of this, the purpose of the utility model is to provide a NdFeB powder charging device, which can maintain a stable optimum temperature during the molding process.
[0004] In order to achieve the above purpose, the technical solution adopted by the utility model is:
[0005] A NdFeB powder charging device, comprising:
[0006] A tank body, the tank body comprising an outer tank body and an inner tank body arranged inside the outer tank body, a first accommodating cavity is formed between the outer tank body and the inner tank body, an interlayer of cotton is arranged in the first accommodating cavity, a second accommodating cavity is formed inside the inner tank body, and the second accommodating cavity is used to accommodate NdFeB powder;
[0007] A vacuum ball valve is provided on the outer tank body and is communicated with the first accommodating chamber.
[0008] The above-mentioned NdFeB powder charging device, wherein a manual butterfly valve is provided at the upper end of the tank body.
[0009] In the above-mentioned NdFeB powder charging device, the tank body is provided with an inflation valve and an deflation valve, and both the inflation valve and the deflation valve are communicated with the second accommodating chamber.
[0010] The above-mentioned NdFeB powder charging device, wherein the tank body comprises:
[0011] Base;
[0012] A lower structure in an arc shape provided on the base;
[0013] A cylindrical middle structure connected to the lower structure;
[0014] and a conical upper structure connected to the middle structure.
[0015] In the above-mentioned NdFeB powder charging device, there is an angle between the upper structure and the middle structure, and the angle is 130° to 150°.
[0016] In the above-mentioned NdFeB powder charging device, the height of the upper structure is 1 / 3 of the height of the tank body.
[0017] In the above-mentioned NdFeB powder charging device, the outer tank body and the inner tank body are both made of non-magnetic stainless steel alloy.
[0018] In the above-mentioned NdFeB powder charging device, the thickness of the outer tank body and the inner tank body is 2-5 mm.
[0019] In the above-mentioned NdFeB powder charging device, the thickness of the interlayer cotton is 2-5 mm.
[0020] In the above-mentioned NdFeB powder charging device, the first containing chamber is in a vacuum state, and the oxygen content in the first containing chamber is less than 30 ppm.
[0021] Due to the adoption of the above technology, the utility model has the following positive effects compared with the prior art:
[0022] The use of the powder charging device of the utility model can reduce the low product performance caused by the local temperature increase of the magnet, maintain the temperature of the powder at the optimal temperature, reduce the temperature fluctuation, and improve the consistency of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a schematic diagram of the NdFeB powder charging device of the utility model.
[0024] Figure 2 It is an enlarged schematic diagram of the tank body of the NdFeB powder charging device of the utility model.
[0025] In the attached figure: 1. outer tank body; 2. inner tank body; 3. interlayer cotton; 4. vacuum ball valve; 5. manual butterfly valve; 61. base; 62. lower structure; 63. middle structure; 64. upper structure; 7. copper quick-connect 8mm connector. DETAILED DESCRIPTION
[0026] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0027] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by terms such as “upper”, “lower”, “left”, “right”, “inside”, “outside”, “front”, “back”, “lateral” and “vertical” are based on the directions or positional relationships shown in the accompanying drawings and are only for the convenience of describing the present invention. They do not indicate or imply that the device or component referred to must have a specific direction and therefore should not be understood as a limitation on the present invention.
[0028] It should be specially explained that the terms “horizontal” and “vertical” in the present invention are used to illustrate a rough positional relationship, rather than a strict “horizontal plane” or “vertical plane”.
[0029] See also Figure 1 to Figure 2 As shown, a preferred embodiment of a NdFeB powder loading device is shown, comprising: a tank body and a vacuum ball valve 4, the tank body comprising an outer tank body 1 and an inner tank body 2 arranged inside the outer tank body 1, a first accommodating chamber is formed between the outer tank body 1 and the inner tank body 2, an interlayer cotton 3 is arranged in the first accommodating chamber, a second accommodating chamber is formed inside the inner tank body 2, and the second accommodating chamber is used to accommodate NdFeB powder; the vacuum ball valve 4 is arranged on the outer tank body 1, and the vacuum ball valve 4 is connected to the first accommodating chamber.
[0030] Among them, the structure of the outer tank body 1, the interlayer cotton 3, and the inner tank body 2 can reduce the low product performance caused by the local temperature increase of the magnet, maintain the temperature of the powder at the optimal temperature, reduce temperature fluctuations, and improve product consistency.
[0031] Preferably, the inner wall of the inner tank body 1 is smooth without welds, and the surface roughness Ra is less than or equal to 1.6 μm. Surface roughness Ra refers to the unevenness of the small spacing and tiny peaks and valleys of the machined surface. This is conducive to reducing the friction between the inner surface of the inner tank body 1 of the NdFeB powder loading device and the magnet powder to be pressed and formed, which is conducive to smooth feeding of the magnetic powder.
[0032] Furthermore, as a preferred embodiment, a manual butterfly valve 5 is provided at the upper end of the tank body.
[0033] Furthermore, as a preferred embodiment, an inflation valve and an deflation valve are provided on the tank body, and both the inflation valve and the deflation valve are communicated with the second accommodating chamber.
[0034] Specifically, the inflation valve and the deflation valve use a copper quick-insert 8mm connector 7 .
[0035] Further, as a preferred embodiment, the tank body includes: a base 61; an arc-shaped lower structure 62 arranged on the base 61; a cylindrical middle structure 63 connected to the lower structure 62; and a conical upper structure 64 connected to the middle structure 63.
[0036] Furthermore, as a preferred embodiment, there is an angle between the upper structure 64 and the middle structure 63, and the angle is 130° to 150°, especially 145°, to prevent powder accumulation and facilitate material unloading.
[0037] Further, as a preferred embodiment, the height of the upper structure 64 is 1 / 3 of the height of the tank body.
[0038] Furthermore, as a preferred embodiment, both the outer tank body 1 and the inner tank body 2 are made of non-magnetic stainless steel alloy, preferably stainless steel 316 steel layer.
[0039] Further, as a preferred embodiment, the thickness of the outer tank body 1 and the inner tank body 2 is 2-5 mm, preferably 3-5 mm.
[0040] Further, as a preferred embodiment, the thickness of the interlayer cotton 3 is 2-5 mm, preferably 3-5 mm.
[0041] Furthermore, as a preferred embodiment, the first containing chamber is in a vacuum state, and the oxygen content in the first containing chamber is less than 30 ppm.
[0042] Example 1
[0043] This embodiment adopts the above structure, wherein the thickness of the outer tank body 1 and the inner tank body 1 is 4 mm, the thickness of the interlayer cotton 3 is 4 mm, the material of the outer tank body 1 and the inner tank body 1 is 316 stainless steel, the oxygen content in the first containing chamber is 18 ppm, and the inner surface roughness of the inner tank body 1 is 1.6 μm.
[0044] The magnetic powder prepared by the apparatus of this embodiment was pressed and sintered. The results are shown in Table 1.
[0045] Example 2
[0046] This embodiment adopts the above structure, wherein the thickness of the outer tank body 1 and the inner tank body 1 is 5 mm, the thickness of the interlayer cotton 3 is 5 mm, the material of the outer tank body 1 and the inner tank body 1 is 316 stainless steel, the oxygen content in the first containing chamber is 12 ppm, and the inner surface roughness of the inner tank body 1 is 1.4 μm.
[0047] The magnetic powder prepared by the apparatus of this embodiment was pressed and sintered. The results are shown in Table 1.
[0048] Comparative Example 1
[0049] This ratio uses a single-layer tank body with a thickness of 4mm and no insulation layer.
[0050] The magnetic powder prepared by the comparative example device was pressed and sintered. The results are shown in Table 1.
[0051] Table 1
[0052]
[0053] According to Table 1, it can be seen that the product using the NdFeB powder charging device provided by the utility model has very low discreteness in various performance parameters and has good consistency; on the contrary, the product using the prior art device provided by Comparative Example 1 has very high discreteness in various performance parameters and poor product consistency.
[0054] The above description is only a preferred embodiment of the present invention, and does not limit the implementation mode and protection scope of the present invention. For those skilled in the art, it should be aware that all solutions obtained by equivalent substitutions and obvious changes made using the description and illustrations of the present invention should be included in the protection scope of the present invention.
Claims
1. A NdFeB powder charging device, characterized in that: include: A tank body, the tank body comprising an outer tank body and an inner tank body arranged inside the outer tank body, a first accommodating cavity is formed between the outer tank body and the inner tank body, an interlayer of cotton is arranged in the first accommodating cavity, a second accommodating cavity is formed inside the inner tank body, and the second accommodating cavity is used to accommodate NdFeB powder; A vacuum ball valve is provided on the outer tank body and is communicated with the first accommodating chamber.
2. The NdFeB powder charging device according to claim 1, characterized in that: A manual butterfly valve is arranged at the upper end of the tank body.
3. The NdFeB powder charging device according to claim 1, characterized in that: The tank body is provided with an inflation valve and an deflation valve, and both the inflation valve and the deflation valve are communicated with the second accommodating chamber.
4. The NdFeB powder charging device according to claim 1, characterized in that: The tank body comprises: Base; A lower structure in an arc shape provided on the base; A cylindrical middle structure connected to the lower structure; and a conical upper structure connected to the middle structure.
5. The NdFeB powder charging device according to claim 4, characterized in that: An included angle is formed between the upper structure and the middle structure, and the included angle is 130° to 150°.
6. The NdFeB powder charging device according to claim 4, characterized in that: The height of the upper structure is 1 / 3 of the height of the tank body.
7. The NdFeB powder charging device according to claim 1, characterized in that: The outer tank body and the inner tank body are both made of non-magnetic stainless steel alloy.
8. The NdFeB powder charging device according to claim 1, characterized in that: The thickness of the outer tank body and the inner tank body is 2-5 mm.
9. The NdFeB powder charging device according to claim 1, characterized in that: The thickness of the interlayer cotton is 2-5 mm.
10. The NdFeB powder charging device according to claim 1, characterized in that: The first containing chamber is in a vacuum state, and the oxygen content in the first containing chamber is less than 30 ppm.