Protruding structure and dispensing plate roller

By designing a raised structure on the dot-coated plate roller, increasing the contact area between the bump and the slurry, the problem of insufficient liquid volume of the plate roller is solved, the coating thickness and coverage rate are improved, and the cost of replacing the anilox roller is reduced. And improves the adhesion of the battery separator.

CN222093794UActive Publication Date: 2024-12-03HEBEI GELLEC NEW ENERGY MATERIAL SCI&TECHNOLOY CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202322825238.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-20
Publication Date
2024-12-03
Estimated Expiration
2033-10-20

AI Technical Summary

Technical Problem

In the existing dot coating process, the liquid volume of the plate roller is difficult to effectively control, resulting in the coating point height being unable to rise, the thickness and coverage being small, which cannot meet the requirements of the battery separator.

Method used

A dot coating roller with a raised structure is designed. The projected area of ​​the bumps along the height direction accounts for 13.24 to 35.54% of the surface area, the number of small bumps is 5 to 10, and the dimensions are 0.1 to 0.2mm width and 0.1 to 0.25mm. The height is hemispherical, rectangular or elliptical, and the adjacent spacing is 0.1 to 0.35 mm. The liquid-carrying capacity is improved by increasing the contact area between the bumps and the slurry.

Benefits of technology

The liquid volume of the dot coating roller is increased, the problems of low thickness and coverage are solved, the coating height and coating volume are increased, the cost of replacing the anilox roller is reduced, and the adhesion of the battery separator is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222093794U_ABST
    Figure CN222093794U_ABST
Patent Text Reader

Abstract

The utility model discloses a convex structure and a point coating plate roller, convex points on the surface of the point coating plate roller are convex structures, each convex structure comprises a convex part, and a small convex point or a plurality of distributed small convex points are formed at the top end of each convex part. According to the point coating plate roller, the problem that the liquid carrying amount of the point coating plate roller is small in the coating process is solved, the liquid carrying amount of the point coating plate roller is increased, the liquid carrying amount is not increased by selecting a deeper anilox roller any more, and the cost for replacing the anilox roller is reduced. Under the condition that the coating coverage rate of the salient points is not increased, the height of a coating formed by the point coating plate roller is increased, and the coating amount is increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of batteries, and in particular relates to a convex structure and a dot coating roller. Background Art

[0002] With the increasing application of new energy, the demand for new ion batteries is also increasing day by day, and the requirements for various battery characteristics are also getting higher and higher. For example, in the field of new energy vehicle companies, the requirements for battery life, charge and discharge times, capacity, fast charging, low-temperature working environment, etc. are becoming more and more stringent. As an important component of ion batteries, the requirements for diaphragms are also getting higher and higher. The performance of diaphragms determines the interface structure and internal resistance of the battery, and directly affects the battery's capacity, cycle and safety performance. Excellent performance diaphragms play an important role in improving the overall performance of batteries. The main function of the diaphragm is to separate the positive and negative electrodes of the battery to prevent the two electrodes from contacting and short-circuiting. In addition, it also has the function of allowing electrolyte ions to pass through.

[0003] As for the diaphragm production process, roller coating and spray coating are currently commonly used. Compared with roller coating, spray coating can reduce the coating coverage, reduce the impact on the air permeability of the diaphragm, save slurry, and at the same time improve the physical properties of the diaphragm. However, due to process limitations, spray coating has inherent defects such as uncertain spray point shape, difficult thickness control, and poor coverage. Therefore, a new production process is needed that can not only retain the advantages of spraying, but also improve its inherent defects. This new process is the spot coating process. The spot coating process can accurately control the coating coverage, the coating points are arranged in a matrix, and the shape of the points is approximately circular. The thickness can also be accurately controlled by parameters such as the plate roller, anilox roller, and slurry, which can better meet the battery's requirements for the diaphragm.

[0004] After all, the spot coating process is a new coating method, and many aspects are still imperfect. For example, the relationship between the coverage rate and the equipment parameters is not fixed, the thickness cannot be achieved by adjusting the equipment parameters, the liquid carrying capacity depends entirely on the tension to transfer, it is highly dependent on the slurry, and the production materials of the plate roller are highly required. The most urgent problem to be solved now is that the amount of liquid on the plate roller cannot be effectively controlled. The convex points of the plate roller are in contact with the anilox roller, and the slurry is transferred to the convex points of the plate roller by the tension difference of the slurry on the material, and then transferred to the diaphragm. However, during the debugging process, it is often the case that the plate roller carries less liquid, and the height of the coating point cannot be raised, resulting in a small thickness and a small coating amount that does not meet the requirements. Summary of the invention

[0005] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a protrusion structure.

[0006] Another purpose of the utility model is to provide a dot coating roller.

[0007] The purpose of the utility model is achieved through the following technical solutions.

[0008] A convex structure comprises: a convex, a small convex point or a plurality of distributed small convex points are formed on the top of the convex.

[0009] In the above technical solution, the number of the small protrusions is 5 to 10.

[0010] In the above technical solution, the projection area formed by the small protrusions distributed on the top of the protrusions after being projected along the height direction of the protrusions is 13.24-35.54% of the projection area formed by the protrusions after being projected along the height direction of the protrusions.

[0011] In the above technical solution, the size of the small protrusions is: a width of 0.1 to 0.2 mm and a height of 0.1 to 0.25 mm.

[0012] In the above technical solution, the small protrusions are in the shape of a hemisphere, a cuboid, an ellipsoid or a cone.

[0013] In the above technical solution, when a plurality of distributed small protrusions are formed on the top of the protrusion, the spacing between adjacent small protrusions is 0.1 to 0.35 mm.

[0014] In the above technical solution, the length of the protrusion is 1.5 to 3 mm, and the width of the protrusion is 0.6 to 1 mm.

[0015] In the above technical solution, the protrusion includes a cylinder and a hemisphere with a diameter the same as that of the cylinder. The hemisphere is connected to the top of the cylinder and is formed integrally with the cylinder.

[0016] In the above technical solution, the protrusion is a first cylinder, a truncated cone and a second cylinder integrally formed from bottom to top, and the first cylinder, the truncated cone and the second cylinder are coaxially arranged.

[0017] A dot coating roller, wherein the convex structures are uniformly distributed on the surface of the dot coating roller as convex points on the surface of the dot coating roller.

[0018] In the above technical solution, the projection area formed by projecting the convex points along the height direction of the convex points is 28.26-50.24% of the surface area of ​​the dot coating roller.

[0019] In the above technical solution, the spacing between adjacent protrusions is 0.5 to 1.2 mm.

[0020] A dot coating method comprises: using the dot coating roller to perform coating.

[0021] Compared with the prior art, the utility model has the following beneficial effects:

[0022] 1. The convex structure of the utility model solves the problem of the small amount of liquid carried by the spot coating roller during the coating process. The utility model improves the liquid carrying capacity of the spot coating roller by improving the shape of the convex points on the spot coating roller. Since the materials of the anilox roller and the spot coating roller are different, the tensions on the slurry are different. The liquid carrying capacity of the spot coating roller on the slurry is transferred by the different tensions of the anilox roller and the spot coating roller on the same slurry. During the transfer process, if the density of the convex points distributed on the surface of the spot coating roller remains unchanged, the shape of the convex point surface of the spot coating roller will affect the liquid carrying capacity. The utility model increases the surface area of ​​the convex points in contact with the slurry, and increases the contact area to achieve slurry transfer under a constant surface tension;

[0023] 2. The convex structure of the utility model can ensure the amount of liquid on the dot coating roller, thus solving the problems of small coating thickness, small coverage and small coating amount caused by small amount of liquid;

[0024] 3. The utility model increases the amount of liquid carried by the dot coating roller, and no longer relies on selecting a deeper anilox roller to increase the amount of liquid carried, thereby reducing the cost of replacing the anilox roller.

[0025] 4. It is possible to increase the height of the coating formed by the dot coating roller and increase the coating amount without increasing the convex dot coating coverage. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 is a side view of the convex point in Comparative Example 1;

[0027] Figure 2 A top view of the convex point in Comparative Example 1;

[0028] Figure 3 It is a side view of the convex point in comparative example 2;

[0029] Figure 4 It is a top view of the convex point in comparative example 2;

[0030] Figure 5 is a side view of the raised structure;

[0031] Figure 6 is a top view of the raised structure;

[0032] Figure 7 It is a partial schematic diagram of the dot coating roller.

[0033] Among them, 1: bulge, 2: small bulge, 3: bulge, 4: second cylinder, 5: frustum, 6: first cylinder. DETAILED DESCRIPTION

[0034] The technical solution of the present utility model is further described below in conjunction with specific embodiments.

[0035] The thickness increment is: on the same roll of base film, use coating rollers at different points to coat the same slurry. After coating, use the same thickness gauge to measure ten sets of thickness data and take the average value of the ten sets of thickness data. The difference between the average value and the base film thickness is the thickness increment.

[0036] The coating amount is: cut the battery separator into 3 groups, the area (specification) of each group of battery separator after cutting is 40mm*60mm, weigh them, take the average weight of the 3 groups of battery separators, divide the average weight by the area (40mm*60mm), and calculate the weight per square meter of the battery separator. Similarly, calculate the weight per square meter of the base membrane. The weight per square meter of the battery separator minus the weight per square meter of the base membrane is the coating amount.

[0037] In the following embodiments, the base film is a PE plastic film.

[0038] Example 1

[0039] like Figures 5 to 7 As shown, a dot coating roller comprises a cylindrical cavity surrounded by a plane, a plurality of convex points 3 are uniformly distributed on the surface of the cylindrical cavity, each convex point 3 is a convex structure, a projection area formed by projecting the convex point along the convex point height direction is 28.26% of the surface area of ​​the dot coating roller, and a spacing between every two adjacent convex points is 0.8 mm, wherein each convex structure comprises: a convex 1, 5 distributed small convex points 2 are formed at the top of the convex, a projection area formed by projecting the small convex points distributed at the top of the convex along the convex point height direction is 20.24% of the projection area formed by projecting the convex points along the convex point height direction, the shape of the small convex points is an ellipsoid, each small convex point has a width of 0.1 mm and a height of 0.2 mm, and the 5 small convex points are arranged along a cross, that is, there are 3 small convex points in a horizontal column and 3 small convex points in a vertical column (the intersection of the horizontal column and the vertical column is provided with a same small convex point), and the spacing between every two adjacent small convex points in the horizontal and vertical directions is 0.1 mm.

[0040] In this embodiment, the protrusion includes: a hemisphere and a cylinder. The bottom end of the cylinder is used to connect with the surface of the dot coating roller. The hemisphere is connected to the top of the cylinder and is integrally formed with the cylinder. The height of the protrusion is 2 mm, the diameter of the cylinder is 1 mm, and the height of the cylinder is 1.5 mm.

[0041] Example 2

[0042] A dot coating roller is basically the same as that in Example 1, except that the protrusion in this example is a first cylinder 6, a truncated cone 5, and a second cylinder 4 which are integrally formed from bottom to top, the first cylinder, the truncated cone, and the second cylinder are coaxially arranged, the diameters of the first cylinder and the second cylinder are 1 mm and 0.6 mm, respectively, and the heights of the first cylinder and the second cylinder are 1.5 mm and 1.5 mm, respectively. The diameter of the upper surface of the truncated cone is 0.6 mm, the diameter of the lower surface of the truncated cone is 1 mm, and the height of the truncated cone is 0.3 mm.

[0043] Comparative Example 1

[0044] like Figure 1 , 2 As shown in FIG. 7 , a dot coating roller is basically the same as the dot coating roller in Example 1, with the only difference being that the convex points of the dot coating roller in this comparative example are the convex points in Example 1 (ie, the convex points in this comparative example do not include small convex points).

[0045] Comparative Example 2

[0046] A dot coating roller, such as Figures 3-4 As shown, it is basically the same as the dot coating roller in Example 2, with the only difference being that the convex points of the dot coating roller in this comparative example are the convex points in Example 2 (ie, the convex points in this comparative example do not include small convex points).

[0047] A polyvinylidene fluoride (PVDF) slurry with a viscosity of 300cp is coated on a base film using a dot coating roller to obtain a battery separator, wherein the dot coating roller is one of Examples 1 to 2 and Comparative Examples 1 to 2, the thickness of the base film is 12 μm, the width of the base film is 1000 mm, the coating target (coating) thickness is 4 μm, and the coating length is 3000 m.

[0048] The effects of coating 10 times with the point coating roller in comparative example 1 and the point coating roller in embodiment 1 are compared, as shown in Table 1:

[0049] Table 1

[0050]

[0051] It can be seen from the data in Table 1 that the thickness increment and coating amount obtained by using the dot coating roller of Example 1 are greater than those obtained by using the dot coating roller of Comparative Example 1.

[0052] The effects of coating 10 times with the point coating roller in comparative example 2 and the point coating roller in example 2 are compared:

[0053] Table 2

[0054]

[0055]

[0056] It can be seen from the data in Table 2 that the thickness increment and coating amount obtained by using the dot coating roller of Example 2 are greater than those obtained by using the dot coating roller of Comparative Example 2.

[0057] The battery separators prepared in Examples 1-2 and Comparative Examples 1-2 were subjected to a test of the adhesion of the electrodes (the positive electrode electrode is aluminum foil, and the negative electrode electrode is carbon sheet) in the battery separator characteristics: the battery separators prepared in Examples 1-2 and Comparative Examples 1-2 were each cut into ten samples with a length of 10 cm and a width of 1 cm, and hot pressed at a pressure of 1200 kg and 60°C for 2 seconds to test their adhesion to the positive and negative electrode electrodes.

[0058] Table 3

[0059]

[0060] It can be seen from the data in Table 3 that, compared with the protrusions in Comparative Examples 1 and 2, the protrusion structure of the utility model not only increases the coating thickness and coating amount, but also increases the bonding force between the battery diaphragm and the electrode, which can greatly enhance the performance of the diaphragm.

[0061] The above is an exemplary description of the present invention. It should be noted that, without departing from the core of the present invention, any simple deformation, modification or other equivalent replacement that can be done by other technical personnel in this field without expending creative labor falls within the protection scope of the present invention.

Claims

1. A protrusion structure, characterized in that: include: A protrusion (1) is provided with a small protrusion (2) or a plurality of distributed small protrusions (2) formed at the top of the protrusion (1), wherein the small protrusions (2) are in the shape of a hemisphere, a cuboid, an ellipsoid or a cone, and the number of the small protrusions (2) is 5 to 10.

2. The protrusion structure according to claim 1, characterized in that: The projection area formed by the small protrusions (2) distributed at the top of the protrusion (1) after being projected along the height direction of the protrusion (1) is 13.24-35.54% of the projection area formed by the protrusion (1) after being projected along the height direction of the protrusion (1).

3. The protrusion structure according to claim 1, characterized in that: The dimensions of the small protrusions (2) are: a width of 0.1 to 0.2 mm and a height of 0.1 to 0.25 mm.

4. The protrusion structure according to claim 1, characterized in that: When a plurality of distributed small protrusions (2) are formed on the top of the protrusion (1), the spacing between adjacent small protrusions (2) is 0.1 to 0.35 mm.

5. The protrusion structure according to claim 1, characterized in that: The length of the protrusion (1) is 1.5 to 3 mm, and the width of the protrusion (1) is 0.6 to 1 mm.

6. The protrusion structure according to claim 1, characterized in that: The protrusion (1) comprises a cylinder and a hemisphere with the same diameter as the cylinder. The hemisphere is connected to the top of the cylinder and is formed integrally with the cylinder.

7. The protrusion structure according to claim 1, characterized in that: The protrusion (1) is a first cylinder (6), a truncated cone (5) and a second cylinder (4) which are integrally formed from bottom to top, and the first cylinder (6), the truncated cone (5) and the second cylinder (4) are coaxially arranged.

8. A dot coating roller, characterized in that: The raised structures described in any one of claims 1 to 7 are uniformly distributed on the surface of the dot coating roller as raised dots (3) on the surface of the dot coating roller.

Citation Information

Cited By

  • Protruding structure and dispensing method

    CN117861935A