Iron mold sand coating and self-hardening resin sand composite casting mold device of wind power main shaft

Through the iron sand-covered and self-hardened resin sand composite casting device, the problems of high production cost and low mechanical performance of wind power spindle castings are solved, and low-cost and high-performance wind power spindle castings are realized, which improves the yield strength of castings and Low temperature impact toughness.

CN222094656UActive Publication Date: 2024-12-03浙江省机电设计研究院有限公司 +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420436598.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-07
Publication Date
2024-12-03
Estimated Expiration
2034-03-07

AI Technical Summary

Technical Problem

The existing wind power spindle castings have high production costs, complex operation and low mechanical properties, and are not suitable for harsh environments.

Method used

The iron-type sand-covered and self-hardened resin sand composite casting device is adopted. The iron-type sand-covered and self-hardened resin sand composite casting model is matched and cooperated with each other to form a complete wind power spindle composite casting model, and the design control of the sand-covered layer is used. The cooling speed and structure of the iron are improved by the density and mechanical properties of the castings.

Benefits of technology

The production of wind power spindle castings with low production costs, easy operation, dense casting structure and good comprehensive performance is achieved, which improves the yield strength and low-temperature impact toughness of castings, reduces the mechanical processing allowance, and simplifies the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222094656U_ABST
    Figure CN222094656U_ABST
Patent Text Reader

Abstract

The utility model relates to an iron mold sand-lined and self-hardening resin sand composite casting mold device of a wind power main shaft, and belongs to the technical field of casting wind power generation. The device disclosed by the utility model comprises a self-hardening resin sand upper box sand box, a self-hardening resin sand bottom box sand box, an iron mold sand-lined casting mold for a side surface cavity of a shaft body of the wind power main shaft, and self-hardening resin sand casting molds for the bottom, the top and the surface of an inner cavity of the wind power main shaft, and the iron mold sand-lined casting mold and the self-hardening resin sand casting molds are matched with each other to be assembled. The self-hardening resin sand casting mold is provided with a self-hardening resin sand upper box casting mold and a self-hardening resin sand bottom box casting mold, and the self-hardening resin sand upper box casting mold and the self-hardening resin sand bottom box casting mold are located in the self-hardening resin sand upper box sand box and the self-hardening resin sand bottom box sand box respectively. The casting mold is reasonable in structural design, safe, reliable, low in production cost, convenient to operate, more compact in casting product structure, better in comprehensive performance and capable of meeting use requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a casting device, in particular to an iron mold covered with sand and self-hardening resin sand composite casting device for a wind power main shaft, and belongs to the technical field of casting wind power generation. Background Art

[0002] Wind power generation technology is a green and sustainable new energy technology, and is currently being vigorously developed in my country. The operating environment of wind turbines is relatively harsh, so the mechanical properties of the load-bearing components in the main engine are required to be high. Among them, the main shaft of the wind turbine (hereinafter referred to as the wind turbine main shaft), which is the main load-bearing component, is usually forged from forged steel and machined after heat treatment, and its production cost is very high.

[0003] In recent years, in order to reduce the production cost of wind turbine main shafts, wind turbine main shafts have gradually begun to use ductile iron castings instead of forgings. Ductile iron main shaft castings are currently mainly produced by self-hardening sand casting or metal mold casting. The self-hardening sand casting process for producing wind turbine main shafts has the disadvantages of complex production operations, high labor intensity, low molten iron utilization, many casting defects, and relatively low performance of the main shaft; the metal mold casting process for casting wind turbine main shafts has the disadvantages of poor surface quality, large machining allowance during mechanical processing, and relatively low low-temperature impact toughness in its mechanical properties, which is not conducive to the application of wind turbine mainframes under harsh environmental conditions.

[0004] Therefore, developing a wind turbine main shaft casting production process with low production cost, easy operation, dense casting product structure and good comprehensive performance has become an important part of reducing the manufacturing cost of wind power equipment and achieving lightweight, high-quality and sustainable development of wind power equipment. Utility Model Content

[0005] The purpose of the utility model is to overcome the above-mentioned shortcomings in the prior art and to provide an iron mold covered with sand and self-hardening resin sand composite casting device for a wind turbine main shaft which has a reasonable structural design, is safe and reliable, has a low production cost, is easy to operate, has a denser casting product structure, and has better comprehensive performance.

[0006] The technical solution adopted by the utility model to solve the above problems is: the iron mold covered sand and self-hardening resin sand composite casting device of the wind turbine main shaft includes a self-hardening resin sand upper box sand box and a self-hardening resin sand bottom box sand box, which is characterized by: it also includes an iron mold covered sand casting mold for the side cavity of the wind turbine main shaft body and a self-hardening resin sand casting mold for the bottom, top, and inner cavity cavity surface of the wind turbine main shaft, the iron mold covered sand casting mold and the self-hardening resin sand casting mold are matched with each other, and the self-hardening resin sand casting mold is provided with a self-hardening resin sand upper box casting mold and a self-hardening resin sand bottom box casting mold. The self-hardening resin sand bottom box casting mold, the self-hardening resin sand upper box casting mold and the self-hardening resin sand bottom box casting mold are respectively located in the self-hardening resin sand upper box sand box and the self-hardening resin sand bottom box sand box; the tooling for the sand-covered molding of the iron mold in the iron mold sand-covered casting mold comprises a model, a mold plate, an iron mold, a sand-shooting plate, a sand-shooting head, a positioning pin, a sand-shooting hole, a positioning pin hole and a coated sand; the iron mold and the model are molded together by the positioning pins at the mold plate and the positioning pin holes at the iron mold; the coated sand in the sand-shooting head is shot into the gap between the iron mold and the model through the sand-shooting holes on the sand-shooting plate to form a sand-covered layer.

[0007] Preferably, the iron mold of the utility model comprises a skirt sand-covered layer groove and a mesh groove, the upper and lower parting surfaces of the iron mold are both provided with a skirt sand-covered layer groove, and the mesh groove is arranged in the inner cavity of the iron mold of the wind turbine main shaft.

[0008] Preferably, the width of the skirt sand-coating groove of the utility model is 80-120 mm and the thickness is 20-25 mm, so as to prevent the molten iron from leaking out from the parting surface under static pressure during pouring, thereby causing major production safety accidents and damaging the iron mold.

[0009] Preferably, the spacing of the mesh grooves of the utility model is between 250-400mm, the width of the mesh grooves is 20-30mm, and the height is 10-15mm; this prevents the sand coating from cracking or detaching from the inner cavity of the iron mold during the cooling process after sand coating molding, causing surface defects of the casting during pouring.

[0010] Preferably, the iron mold of the utility model further comprises upper and lower skirt edges of the iron mold, and the width of the upper and lower skirt edges of the iron mold is 200-250mm and the height is 80mm.

[0011] Preferably, the iron mold of the utility model also includes an iron mold wall thickness, and the iron mold wall thickness is 120-180mm; so as to meet the solidification cooling speed of molten iron, and the requirements of iron mold rigidity and strength.

[0012] Preferably, the iron mold covered with sand casting mold of the utility model is a through-type casting mold, which is composed of a plurality of sections of iron mold covered with sand casting molds.

[0013] Preferably, the utility model further comprises a movable spindle-shaped positioning pin, and the multi-section iron mold covered sand casting mold is positioned by the movable spindle-shaped positioning pin and is stacked on the self-hardening resin sand casting mold and the iron mold covered sand casting mold in sequence.

[0014] Preferably, the self-hardening resin sand upper box sand box and the self-hardening resin sand bottom box sand box of the utility model are both provided with upper and lower skirts of the sand box, reinforcing ribs and sand hanging ribs, and the upper and lower skirts of the sand box in the self-hardening resin sand upper box sand box and the self-hardening resin sand bottom box sand box match the upper and lower skirts of the iron mold in the iron mold.

[0015] Preferably, the sand covering layer of the utility model adopts heat-cured coated sand, and the surface layer of the sand covering layer adopts a refractory technical structure.

[0016] Compared with the prior art, the utility model has the following advantages and effects: (1) The overall structural design is reasonable, safe and reliable. The rapid cooling conditions of the iron mold covered with sand casting are utilized to greatly refine the grain structure and metallographic structure morphology of the wind turbine main shaft, which is beneficial to improving the mechanical properties of the wind turbine main shaft; (2) Through the high rigidity of the iron mold covered with sand casting, the graphitization expansion of ductile iron during the solidification process can be utilized to make the internal structure of the wind turbine main shaft more compact, and a higher molten iron yield can be achieved in the wind turbine main shaft casting production; (3) The inner cavity, bottom and top of the main shaft are made of self-hardening resin sand, which can meet the requirements of the wind turbine main shaft for the drum-shaped structure of the inner cavity, while meeting the process requirements in the production process of the wind turbine main shaft, and ensuring the compactness of the structure of the top of the wind turbine main shaft; (4) Compared with the metal mold, the iron mold covered with sand is used to form the wind turbine casting mold. The outer side casting mold can adjust the cooling conditions of the molten iron during the solidification process by adjusting the thickness of the sand coating layer, and will not produce the strong chilling effect in the metal mold casting process. The surface quality of its outer surface is much better than that of metal mold casting, which can greatly reduce the machining allowance of the outer surface, greatly improve the yield strength of the wind turbine main shaft casting, and prevent the wind turbine main shaft from brittle fracture during use; (5) Compared with the self-hardening resin sand casting wind turbine main shaft, the utility model casting production of the wind turbine main shaft has: its metallographic structure is denser, the graphite morphology is more round and fine, and its comprehensive mechanical properties are better; (6) The iron mold sand-coated casting mold of the wind turbine main shaft is made by sand-coated molding equipment, and equipped with corresponding mechanical equipment. The production process has low labor intensity, simple process control, good product consistency, and can realize mass production of wind turbine main shafts. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a structural schematic diagram of a wind turbine main shaft casting according to an embodiment of the utility model.

[0018] Figure 2 It is a schematic diagram of a composite casting device for casting a main shaft of a wind turbine generator according to an embodiment of the utility model.

[0019] Figure 3 It is a schematic diagram of sand-coated molding of an iron mold in a composite casting device for casting a wind turbine main shaft according to an embodiment of the utility model.

[0020] Figure 4It is a schematic structural diagram of an iron mold in a composite casting device for casting a wind turbine main shaft according to an embodiment of the utility model.

[0021] Figure 5 yes Figure 4 Schematic diagram of the cross-sectional structure of AA.

[0022] Figure 6 This is a schematic diagram of the self-hardening resin sand box structure in the composite casting device for casting the wind turbine main shaft in the embodiment of the utility model Figure 1 .

[0023] Figure 7 This is a schematic diagram of the self-hardening resin sand box structure in the composite casting device for casting the wind turbine main shaft in the embodiment of the utility model Figure 2 .

[0024] Figure 8 yes Figure 7 Schematic diagram of the cross-sectional structure of BB.

[0025] Fig. 9 It is a structural schematic diagram of a movable spindle-shaped positioning pin in an embodiment of the utility model.

[0026] Fig.10 The production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (resin sand bottom box and main shaft inner cavity) is shown in FIG. Figure 1 .

[0027] Fig.11 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (the flange iron mold and the resin sand bottom box are combined and locked) Figure 2 .

[0028] Fig.12 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (the various iron molds are closed and locked) is shown in FIG. Figure 3 .

[0029] Fig.13 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (the upper resin sand box and the uppermost iron mold are combined and locked) Figure 4 .

[0030] Fig.14 The production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (molten iron fills the composite casting mold) is shown in FIG. Figure 5 .

[0031] Fig.15 The production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (after the molten iron in the casting is completely solidified, the fastening bolts between the composite castings are loosened) Figure 6 .

[0032] Fig.16 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (the resin sand upper box is lifted off the main shaft and the lower casting mold) Figure 7 .

[0033] Fig.17 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (the air outlet channel is separated from the main shaft) Figure 8 .

[0034] Fig.18 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (each iron mold hangs the main shaft) Figure 9 .

[0035] Fig.19 The schematic diagram of the production process of casting a wind turbine main shaft by a composite casting device according to an embodiment of the present invention (the main shaft is lifted off the resin sand bottom box) Figure 10 .

[0036] In the figure: iron mold covered sand casting mold T1, self-hardening resin sand casting mold Z2, self-hardening resin sand upper box sand box Z3, self-hardening resin sand bottom box sand box Z4, hanging shaft 5, movable spindle-shaped positioning pin 6, fastening bolt 7, fastening bolt hole 8, sand covering layer air outlet 9;

[0037] Iron mold coated sand casting mold T1: model 11, pattern plate 12, iron mold 13, sand shooting plate 14, sand shooting head 15, positioning pin 16, sand shooting hole 17, positioning pin hole 18, coated sand 19;

[0038] Iron mold 13: iron mold upper and lower skirts 131, skirt sand layer grooves 132, iron mold wall thickness 133, mesh grooves 134;

[0039] Self-hardening resin sand casting mold Z2: self-hardening resin sand upper box casting mold Z2-1, self-hardening resin sand bottom box casting mold Z2-2;

[0040] Self-hardening resin sand upper box sand box Z3, self-hardening resin sand bottom box sand box Z4: sand box upper and lower skirts 34-1, reinforcing ribs 34-2, and sand hanging ribs 34-3. DETAILED DESCRIPTION

[0041] The present invention will be further described in detail below with reference to the accompanying drawings and through examples. The following examples are provided to explain the present invention, but the present invention is not limited to the following examples.

[0042] Example

[0043] See also Figures 1 to 19In this embodiment, a process of casting a wind turbine main shaft by using an iron mold coated with sand and a self-hardening resin sand composite mold is adopted. The bottom, top, and inner cavity surface of the wind turbine main shaft are formed by a self-hardening resin sand mold Z2, and the side surface cavity of the wind turbine main shaft is formed by an iron mold coated with sand mold T1. A complete wind turbine main shaft composite mold is formed by assembling the above-mentioned mold boxes, and then molten iron is poured. After solidification and cooling, the wind turbine main shaft casting is produced by casting.

[0044] The iron mold covered with sand and self-hardening resin sand composite casting device of the wind turbine main shaft in this embodiment includes an iron mold covered with sand casting mold T1, a self-hardening resin sand casting mold Z2 (a self-hardening resin sand upper box casting mold Z2-1 and a self-hardening resin sand bottom box casting mold Z2-2), a self-hardening resin sand upper box sand box Z3, a self-hardening resin sand bottom box sand box Z4, an iron mold, fastening bolts 7 between the iron molds and between the sand box and the iron mold, a movable spindle-shaped positioning pin 6 between the iron molds, and a movable spindle-shaped positioning pin 6 between the sand box and the iron mold.

[0045] See also Figure 2 As shown, the casting mold in the iron mold covered with sand and self-hardening resin sand composite casting device of the wind turbine main shaft of this embodiment mainly consists of two parts, namely, the iron mold covered with sand casting mold T1 and the self-hardening resin sand casting mold Z2; among them, the iron mold covered with sand casting mold T1 is a through-type casting mold, which is composed of multiple sections of iron mold covered with sand casting molds T1.

[0046] For the tooling of the iron mold covered with sand in the iron mold covered with sand casting T1, see Figure 3 As shown, the tooling for sand-coating the iron mold in the iron mold sand-coated casting T1 includes a model 11, a mold plate 12, an iron mold 13, a sand-shooting plate 14, a sand-shooting head 15, a positioning pin 16, a sand-shooting hole 17, a positioning pin hole 18 and a coated sand 19. The sand-coating molding process is the same as the sand-coating molding process of the ordinary iron mold. The sand-coating layer of the iron mold adopts heat-cured coating sand 19. The heated iron mold 13 and the model 11 are molded together through the mold plate 12, the positioning pin 16 and the iron mold 13, and the positioning pin hole 18. Then, the coated sand 19 in the sand-shooting head 15 is injected into the gap between the iron mold 13 and the model 11 through the sand-shooting hole 17 on the sand-shooting plate 14 with compressed air to form a sand-coating layer. After curing and demolding, the production of the wind turbine main shaft iron mold sand-coated casting T1 is completed; the sand-coating layer is provided with a sand-coating layer vent 9.

[0047] The iron type 13 structure of the wind turbine main shaft includes an iron type upper and lower skirts 131, a skirt sand layer groove 132, an iron type wall thickness 133 and a mesh groove 134; see Figure 4-Figure 5As shown, its structure is an upper and lower through-type, that is, the upper and lower planes of each iron mold are in contact with the parting surfaces of other iron molds or self-hardening resin sand casting molds; the upper and lower parting surfaces of each iron mold need to be made with skirts that are the same as the parting surfaces of the iron mold or self-hardening resin sand box that are in contact with the combined box; the upper and lower parting surfaces of each iron mold are provided with positioning pin holes for other iron molds or self-hardening resin sand casting molds; each parting point of the iron mold is provided with a fastening screw hole structure at the corresponding position of the parting point of the iron mold in contact with it, or the parting surface of the self-hardening resin sand casting mold in contact with it;

[0048] The anti-sand detachment mesh grooves 134 of the inner cavity of the wind turbine main shaft iron mold have a spacing of 250-400mm, a groove width of 20-30mm, and a height of 10-15mm, which prevents the sand coating layer from cracking or detaching from the inner cavity of the iron mold during the cooling process after the sand coating molding, causing surface defects of the casting during pouring.

[0049] The upper and lower parting surfaces of the iron mold need to be made into a skirt sand-covered groove 132 with a width of 80-120mm and a thickness of 20-25mm to prevent the molten iron from leaking from the parting surface under static pressure during pouring, causing major production safety accidents and damaging the iron mold.

[0050] Four hanging shafts 5 are arranged outside the iron mold for lifting, turning over, closing and unpacking of the iron mold; multiple horizontal and vertical reinforcing ribs can be made on the outer side of the iron mold to strengthen the rigidity of the iron mold and the strength of the sand box; according to the weight of the wind turbine main shaft, the wall thickness of the iron mold is controlled at 120-180mm to meet the solidification cooling speed of the molten iron, as well as the rigidity and strength of the iron mold; the width of the upper and lower skirts 131 of the iron mold is controlled at 200-250mm, and the height is about 80mm.

[0051] The self-hardening resin sand upper box sand box Z3 and the self-hardening resin sand bottom box sand box Z4 are both provided with upper and lower skirts 34-1, reinforcing ribs 34-2 and sand hanging ribs 34-3. The upper and lower skirts 34-1 of the self-hardening resin sand upper box sand box Z3 and the self-hardening resin sand bottom box sand box Z4 match the upper and lower skirts 131 of the iron mold in the iron mold 13.

[0052] The production of self-hardening resin sand casting mold Z2 is similar to that of ordinary self-hardening resin sand casting mold. Its sand box structure is similar to that of ordinary self-hardening resin sand. However, at the junction with the iron mold parting surface, a skirt structure, a positioning pin and a positioning pin hole structure that are consistent with the position and structure of the iron mold are required, and a fastening screw hole 8 structure is made at the corresponding position of the iron mold at the parting surface of the iron mold covered sand casting mold that contacts it, see Figure 6-Figure 8 The self-hardening resin sand model and sand box can be used to produce the self-hardening resin sand casting Z2 required for the wind turbine main shaft casting (see Figure 2 As shown), the production process is similar to that of ordinary self-hardening resin sand casting molds.

[0053] See also Figure 9-Figure 19 As shown, the production process of composite casting of wind turbine main shaft in this embodiment is as follows: first, the multi-section iron mold coated sand casting mold T1, self-hardening resin sand bottom box casting mold Z2-2, self-hardening resin sand upper box casting mold Z2-1 and self-hardening resin sand casting mold Z2 on the surface of the inner cavity required for the wind turbine main shaft casting are respectively produced, and then each section of the iron mold coated sand casting mold T1 is positioned by a movable spindle-shaped positioning pin 6, and is stacked on the self-hardening resin sand casting mold Z2 and the iron mold coated sand casting mold T1 in sequence, and finally is positioned by the movable spindle-shaped positioning pin 6, and the self-hardening resin sand upper box cover is placed on the topmost iron mold coated sand casting mold T1, completing the box assembling process of the composite casting of the iron mold coated sand and self-hardening resin sand of the wind turbine main shaft, and then the self-hardening resin sand upper box casting mold Z2-1 and the iron mold coated sand casting mold are positioned. The sand casting mold T1, the iron mold covered with sand casting mold T1 and the iron mold covered with sand casting mold T1, and the iron mold covered with sand casting mold T1 and the self-hardening resin sand bottom box casting mold Z2-2 are locked one by one with fastening bolts 7 (cooperating with fastening bolt holes 8), and finally a complete composite casting mold is formed, and then molten iron is poured into the casting mold. When the molten iron forming the wind turbine main shaft casting in the composite casting mold is completely solidified and cooled to about 400°C, the casting mold is unpacked, and the self-hardening resin sand upper box sand box Z3 and each iron mold are successively lifted off from the wind turbine main shaft casting, and then the wind turbine main shaft casting is lifted off from the self-hardening resin sand bottom box sand box Z4, completing the production of a wind turbine main shaft casting; the lifted iron mold can be cleaned, and the residual heat of the iron mold can be used to carry out the next round of sand covering molding on the iron mold.

[0054] The process principle of the iron mold sand-coated and self-hardening resin sand composite casting device for casting the wind turbine main shaft in this embodiment is as follows: At present, the weight of the wind turbine main shaft is 15-25 tons, which is a large ductile iron casting, and the material is mainly QT500-14, and the low-temperature impact toughness is about 7 joules at -20°C. The casting of ductile iron wind turbine main shaft is currently mainly self-hardening resin sand casting or metal mold casting. At present, both of these two casting production methods have certain shortcomings in producing wind turbine ductile iron main shafts: for self-hardening resin sand casting wind turbine main shafts, due to the slow cooling rate of molten iron during the production process, the graphite morphology and grain size in its metallographic structure have certain deficiencies, affecting its mechanical properties, especially in terms of yield strength and low-temperature impact toughness; at the same time, slow cooling also prolongs the time of the production process, and the production efficiency is not high; the casting process is labor-intensive, time-consuming, and the process is cumbersome; at the same time, the wind turbine main shaft adopts self-hardening resin sand molding, and the rigidity of the outer surface of the casting is relatively low. During the solidification process of ductile iron, the ability to use graphitization expansion to self-compensate for shrinkage is poor, and large risers are required for shrinkage compensation. The molten iron recovery rate in production is low and the production cost is high. For the use of metal molds to cast wind turbine main shafts, the mold has high rigidity and the cooling speed of the molten iron after pouring is fast, which is conducive to the self-compensation effect of ductile iron in the solidification process; however, due to the strong chilling effect of the metal mold, in the production of as-cast ductile iron castings, enhanced inoculation treatment is required, otherwise certain carbides will be produced during the production process, which will seriously deteriorate the mechanical properties of the wind turbine main shaft castings. Therefore, the material of the wind turbine main shaft cast by metal molds is often high-silicon solid-solution ductile iron. This high-silicon solid-solution ductile iron is not good for wind turbine main shaft castings with low-temperature impact requirements. In actual production, its chemical composition and spheroidizing inoculation treatment need to be strictly controlled. , improper control can easily cause major failures such as spindle breakage during use; in the process of metal mold casting, the molten iron is in direct contact with the metal mold. In order to ensure that the molten iron will not adhere to the metal mold during pouring and the subsequent solidification and cooling process, a thick layer of refractory coating must be applied to the inner cavity of the metal mold before pouring. This layer of coating is the main reason for the poor surface quality and large machining allowance of the current metal mold casting wind turbine main shaft; at the same time, due to the frequent contact between the metal mold and the molten iron, the life of the metal mold is very short. Generally, it can only be scrapped after about 20 uses, resulting in high mold costs during the production process, increasing the production cost of the wind turbine main shaft. Iron mold sand casting is achieved by covering the iron mold with a layer of coated sand. The heat conduction speed of the iron mold sand casting is between the sand mold and the metal mold, and the heat conduction speed is controllable and adjustable.The heat conduction rate of this part can be controlled by adjusting the thickness of the sand coating, so that the molten iron in this part solidifies and cools at an appropriate cooling rate, thereby meeting the internal metallographic organizational requirements of the wind turbine main shaft and obtaining round, fine graphite nodule organization, grain organization, and matrix organization requirements, thereby greatly improving the comprehensive mechanical properties of the main shaft casting, especially the yield strength and low-temperature impact toughness of the casting; the casting formed by the iron mold sand coating has good rigidity, and can make full use of the self-compensation effect of the graphitization expansion of ductile iron, which can improve the molten iron recovery rate in casting production and the density of the internal organization of the casting; the sand coating layer formed in the iron mold sand coating casting adopts compressed air sand shooting molding, and the sand coating layer has a dense organization, high strength, and a smooth surface. The produced casting has good surface roughness and high dimensional accuracy, which can greatly reduce the processing allowance of the wind turbine main shaft casting.

[0055] The side cavity of the wind turbine main shaft in the casting device of this embodiment adopts an iron mold covered with sand casting mold T1, and the iron mold covered with sand casting mold T1 is formed by compressed air injection molding. The iron mold covered with sand casting mold can fully utilize the process characteristics of iron mold covered with sand casting, so that the heat in the molten iron poured into the casting mold is conducted to the iron mold and absorbed at a faster speed through the sand coating layer, and then further radiated to the atmosphere, so that the molten iron solidifies faster. At the same time, there is a sand coating layer between the molten iron and the iron mold, and the molten iron and the sand coating layer will not produce a strong chilling effect to cause the generation of carbides, affecting the mechanical properties of the wind turbine main shaft; it can greatly reduce the silicon content in the chemical composition of the molten iron and improve the low-temperature impact toughness of the wind turbine main shaft casting.

[0056] The iron mold sand-coated casting molding method of the wind turbine main shaft in this embodiment adopts compressed air injection molding, and the surface of the sand coating layer is compact, smooth and high in strength. All the processes in the molding process, such as mold closing, sand-coated sand-shot molding, curing, and straight demolding, are completed by a special mechanical device, which can realize batch mechanized molding. The inner cavity of the main shaft is molded by self-hardening resin sand, which can form a drum-shaped or other special-shaped inner cavity, which is convenient for the subsequent cleaning of the casting; the upper box casting of the main shaft is molded by self-hardening resin sand, which is conducive to the shrinkage compensation of molten iron; the bottom box casting is molded by self-hardening resin sand, which is conducive to the discharge and arrangement of the casting using a bottom pouring system.

[0057] The composite casting mode of the iron mold covered sand casting mold T1 and the self-hardening resin sand casting mold Z2 in this embodiment satisfies the process requirements of molten iron pouring, solidification, cooling, cleaning, etc. during the casting of ductile iron wind turbine main shaft, and realizes the riser-free casting production of wind turbine main shaft casting, low production cost and short production cycle; the wind turbine main shaft casting has a dense internal structure, good comprehensive mechanical properties, high surface roughness and dimensional accuracy.

[0058] Through the above description, those skilled in the art can already implement it.

[0059] In addition, it should be noted that the shapes and names of the parts and components of the specific embodiments described in this specification may be different, and the above content described in this specification is only an example of the structure of the utility model. All equivalent changes or simple changes made based on the structure, features and principles described in the patent concept of the utility model are included in the protection scope of the utility model patent. Technicians in the technical field of the utility model can make various modifications or supplements to the specific embodiments described or replace them in a similar manner, as long as they do not deviate from the structure of the utility model or exceed the scope defined by the claims, they should all fall within the protection scope of the utility model.

Claims

1. A composite casting device of iron mold covered with sand and self-hardening resin sand for a wind turbine main shaft, comprising a self-hardening resin sand upper box sand box (Z3) and a self-hardening resin sand bottom box sand box (Z4), characterized in that: It also includes an iron mold coated sand casting mold (T1) for the side cavity of the wind turbine main shaft and a self-hardening resin sand casting mold (Z2) for the bottom, top, and inner cavity surface of the wind turbine main shaft, wherein the iron mold coated sand casting mold (T1) and the self-hardening resin sand casting mold (Z2) are matched with each other, and the self-hardening resin sand casting mold (Z2) is provided with a self-hardening resin sand upper box casting mold (Z2-1) and a self-hardening resin sand bottom box casting mold (Z2-2), and the self-hardening resin sand upper box casting mold (Z2-1) and the self-hardening resin sand bottom box casting mold (Z2-2) are respectively located in the self-hardening resin sand upper box sand box (Z3) and the self-hardening resin sand bottom box sand box (Z4); The tooling for sand-coated molding of the iron mold in the iron mold sand-coated casting mold (T1) comprises a model (11), a mold plate (12), an iron mold (13), a sand-shooting plate (14), a sand-shooting head (15), a positioning pin (16), a sand-shooting hole (17), a positioning pin hole (18) and a coating sand (19); the iron mold (13) and the model (11) are molded together through the positioning pin (16) at the mold plate (12) and the positioning pin hole (18) at the iron mold (13); the coating sand (19) in the sand-shooting head (15) is shot into the gap between the iron mold (13) and the model (11) through the sand-shooting hole (17) on the sand-shooting plate (14) to form a coating sand layer.

2. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 1 is characterized in that: The iron mold (13) comprises a skirt sand-covered layer groove (132) and a mesh groove (134); the upper and lower parting surfaces of the iron mold are both provided with a skirt sand-covered layer groove (132); and the mesh groove (134) is arranged in the inner cavity of the iron mold (13) of the wind turbine main shaft.

3. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 2 is characterized in that: The skirt sand-covered groove (132) has a width of 80-120 mm and a thickness of 20-25 mm.

4. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 2 is characterized in that: The spacing between the mesh grooves (134) is between 250 and 400 mm, the width of the mesh grooves (134) is between 20 and 30 mm, and the height is between 10 and 15 mm.

5. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 2 is characterized in that: The iron mold (13) further comprises an upper iron mold skirt and a lower iron mold skirt (131), wherein the width of the upper iron mold skirt and the lower iron mold skirt (131) are 200-250 mm and the height is 80 mm.

6. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 2 is characterized in that: The iron mold (13) further comprises an iron mold wall thickness (133), and the iron mold wall thickness (133) is 120-180 mm.

7. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 1 is characterized in that: The iron mold covered with sand casting mold (T1) is a through casting mold, which is composed of a plurality of sections of iron mold covered with sand casting molds (T1).

8. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 7 is characterized in that: It also includes a movable spindle-shaped positioning pin (6), and the multi-section iron mold covered sand casting mold (T1) is positioned by the movable spindle-shaped positioning pin (6) and is stacked on the self-hardening resin sand casting mold (Z2) and the iron mold covered sand casting mold (T1) in sequence.

9. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 5 is characterized in that: The self-hardening resin sand upper flask (Z3) and the self-hardening resin sand bottom flask (Z4) are both provided with flask upper and lower skirts (34-1), reinforcing ribs (34-2) and sand hanging ribs (34-3); the flask upper and lower skirts (34-1) in the self-hardening resin sand upper flask (Z3) and the self-hardening resin sand bottom flask (Z4) match the iron mold upper and lower skirts (131) in the iron mold (13).

10. The iron mold sand-coated and self-hardening resin sand composite casting device for the wind turbine main shaft according to claim 1, characterized in that: The sand coating layer is made of thermally cured coated sand (19).

Citation Information

Cited By

  • Iron mold sand coating and self-hardening resin sand composite casting mold device of wind power main shaft and production method thereof