High-temperature-resistant microphone stay wire

By alternately setting single-layer and multi-layer Mail film sections on the Maila line and hot melting is carried out, the existing Maila line has been solved, and the problem of insufficient proportion of high-temperature welding communication surface and cumbersome peeling is achieved, and high-efficiency hot melt welding and resistance are achieved Abrasive, suitable for a wide range of high-frequency inductors and medical equipment.

CN222106282UActive Publication Date: 2024-12-03DONGGUAN QINYUANJIN WIRE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420534806.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-19
Publication Date
2024-12-03
Estimated Expiration
2034-03-19

AI Technical Summary

Technical Problem

The hot melt welding communication surface of existing Maila wires with copper joints under high temperature conditions account for less than 80%, and the peeling process is cumbersome and difficult to replace, which affects its widespread use in its application fields.

Method used

Design a high-temperature resistant mela line, which alternately arranges single-layer and multi-layer mela film segments along the length direction, and is fixed as single-layer mela film segments at both ends, and is formed by spiral winding and hot melting of PET film to ensure welding. The communication surface reaches more than 80%, and smooth connection is achieved through the transition section.

Benefits of technology

It realizes efficient hot melt welding between the Maila wire and the copper joint, avoids the peeling process, enhances wear resistance and service life, and ensures the effectiveness of the conductive contact surface above 80%.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222106282U_ABST
    Figure CN222106282U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of leads, in particular to a high-temperature-resistant Mylar stay wire, which comprises a wire core formed by twisting a plurality of enameled wires into a bundle, a Mylar film layer is wrapped outside the wire core, and along the length direction of the Mylar stay wire, the Mylar film layer is alternately divided into a single-layer Mylar film section and a multi-layer Mylar film section; the two ends of the Mylar line are both single-layer Mylar film sections. According to the Mylar film, the Mylar film layers of the Mylar stay wire are alternately divided into the single-layer Mylar film sections and the multi-layer Mylar film sections along the length direction of the Mylar stay wire, and the single-layer Mylar film sections are arranged at the two ends of the Mylar stay wire, so that when the Mylar film is subjected to hot melting welding with a copper joint, the Mylar film can meet the requirement of hot melting welding, and when the Mylar film is used, the Mylar film can meet the requirement of hot melting welding. The multi-layer mylar film section is thick and cannot be damaged due to friction caused by contact with other objects, and the single-layer mylar film section is thin and cannot be easily abraded due to contact with other objects, so that good performance is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of conductors, in particular to a high-temperature resistant Mylar wire. Background Art

[0002] Adding one or two layers of Mylar film (PET film) on the outside of LITZ wire and enameled stranded wire can increase the insulation voltage of the wire and also serve as a shield. This type of wire is called Mylar wire and is widely used in high-frequency inductors, transformers, converters, communication equipment, medical equipment and other fields.

[0003] The carbonized portion of the Mylar film after hot melting will affect the contact area ratio between the copper joint and the conductor. Except for a very thin single-layer Mylar film, the conductive contact area of ​​the remaining Mylar wires and the copper joints directly hot-melt welded (hot-melt welding without removing the Mylar film) is less than 80%. Therefore, some processes prohibit direct hot-melt welding of the Mylar wire. However, stripping the Mylar wire is more troublesome, and other wiring harnesses cannot replace the Mylar wire well. For this reason, the utility model provides a high-temperature resistant Mylar wire that can be directly hot-melt welded. Utility Model Content

[0004] The utility model aims to solve the shortcomings in the prior art and provides a high temperature resistant Mylar wire.

[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0006] A high temperature resistant Mylar wire, comprising a wire core formed by twisting a plurality of enameled wires into a bundle, wherein the outer side of the wire core is wrapped with a Mylar film layer, and along the length direction of the Mylar wire, the Mylar film layer is alternately single-layer Mylar film segments and multi-layer Mylar film segments;

[0007] Both ends of the Mylar wire are single-layer Mylar film segments.

[0008] As a further description of the above technical solution:

[0009] A transition section is arranged along the length direction of the Mylar wire and between the single-layer Mylar film section and the multi-layer Mylar film section.

[0010] As a further description of the above technical solution:

[0011] The Mylar film layer is formed by spirally winding a PET film on a wire core and then hot-melting the film.

[0012] As a further description of the above technical solution:

[0013] The multi-layer Mylar film segment is a 2-4-layer PET film spirally wound on a wire core and then heat-melted.

[0014] As a further description of the above technical solution:

[0015] The thickness of the PET film is 0.02 mm-0.03 mm.

[0016] As a further description of the above technical solution:

[0017] The length of the single-layer Mylar film segment is 2 cm-5 cm.

[0018] As a further description of the above technical solution:

[0019] The length of the multi-layer Mylar film segment is 5 cm-8 cm.

[0020] The utility model has the following beneficial effects:

[0021] 1. Compared with the prior art, the high temperature resistant Mylar wire is provided with Mylar film layers alternately divided into single-layer Mylar film segments and multi-layer Mylar film segments along the length direction of the Mylar wire, and both ends of the Mylar wire are single-layer Mylar film segments, so that when hot-melt welding is performed with the copper joint, the Mylar film can meet the requirements of hot-melt welding.

[0022] 2. Compared with the prior art, the high temperature resistant Mylar wire has a Mylar film layer that is alternately divided into single-layer Mylar film segments and multi-layer Mylar film segments along the length direction of the Mylar wire. When the multi-layer Mylar film segment is used, it is thicker and will not be damaged by friction with other objects, while the single-layer Mylar film segment is thinner and is not easy to be worn by other objects, thereby having good performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a three-dimensional schematic diagram of a high temperature resistant Mylar wire proposed by the utility model;

[0024] Figure 2 This is a cross-sectional schematic diagram of a high temperature resistant Mylar wire proposed by the utility model;

[0025] Figure 3 The utility model provides a three-dimensional schematic diagram of a wire cutter specially used for high-temperature resistant Mylar wire.

[0026] Legend:

[0027] 101, single-layer Mylar film section; 102, multi-layer Mylar film section; 103, transition section; a, enameled wire; b, Mylar film layer; 2, clamp body; 2a, first tooth plate; 2b, second tooth plate. DETAILED DESCRIPTION

[0028] Reference Figure 1-Figure 2The utility model provides a high-temperature resistant Mylar wire, comprising a wire core formed by twisting a plurality of enameled wires a into a bundle, the outer side of the wire core is wrapped with a Mylar film layer b, the Mylar film layer b (PET film) has excellent insulation and high-temperature resistance, and also plays a shielding role, so that the formed Mylar wire has excellent performance, along the length direction of the Mylar wire, the Mylar film layer b is alternately single-layer Mylar film segment 101 and multi-layer Mylar film segment 102, and both ends of the Mylar wire are single-layer Mylar film segments 101.

[0029] When the high temperature resistant Mylar wire of the utility model is hot-melt welded with a copper joint, since both ends of the Mylar wire are single-layer Mylar film sections, the Mylar film can meet the requirements of hot-melt welding.

[0030] like Figure 3 As shown in the figure, it is a three-dimensional schematic diagram of a wire cutter specially used for high-temperature resistant Mylar wire of the utility model, wherein the jaws of the pliers body 2 are relatively wide, which is basically equivalent to the length of the multi-layer Mylar film segment 102, and the first tooth plate 2a and the second tooth plate 2b are fixedly arranged on the inner side of the jaws of the pliers body 2. When the high-temperature resistant Mylar wire is interrupted in the middle, the first tooth plate 2a and the second tooth plate 2b correspond to two interruption positions, which can just cut off one of the multi-layer Mylar film segments 102, and both ends of the remaining high-temperature resistant Mylar wire are still single-layer Mylar film segments 101.

[0031] In one embodiment, a transition section 103 is provided along the length direction of the Mylar wire and between the single-layer Mylar film section 101 and the multi-layer Mylar film section 102 , that is, the single-layer Mylar film section 101 and the multi-layer Mylar film section 102 are smoothly connected.

[0032] In one embodiment, the Mylar film layer b is formed by spirally winding a PET film on a wire core and then hot-melting it. During production, a conveying mechanism for moving the wire core and a rotating structure for winding the PET film are used. By reasonably and periodically controlling the moving speed of the conveying mechanism or the rotating speed of the wound PET film, a single layer can be wound on one section of the wire core and multiple layers can be wound on another section. Finally, the PET film is tightly connected to the wire core through hot melting.

[0033] In one embodiment, the multi-layer Mylar film segment 102 is formed by 2-4 layers of PET film spirally wound on a wire core and then hot-melted, and the single-layer Mylar film segment 101 is formed by a single layer of PET film spirally wound on a wire core and then hot-melted, so that the multi-layer Mylar film segment is thicker and will not be damaged by friction caused by contact with other objects, while the single-layer Mylar film segment is thinner and is not easily worn by contact with other objects, thereby having good performance.

[0034] In one embodiment, the thickness of the PET film is 0.02mm-0.03mm, so that the single-layer Mylar film segment 101 can meet the conditions for direct hot-melt welding with the copper joint, thereby avoiding the problem of peeling the Mylar wire during welding. The conductive contact area of ​​the direct hot-melt welding (hot-melt welding without peeling the Mylar film) is basically guaranteed to be above 80%. After hot-melt welding, various evaluations and tests are carried out, and it can be put into production and use normally.

[0035] In one embodiment, the length of the single-layer Mylar film segment 101 is 2 cm-5 cm, and the length of the single-layer Mylar film segment 101 is consistent with the joint length required for copper joint welding.

[0036] In one embodiment, the length of the multi-layer Mylar film segment 102 is 5 cm-8 cm.

[0037] Both ends of the Mylar wire are single-layer Mylar film segments 101, which means that its length is a discontinuous length, which must satisfy: the length of the high temperature resistant Mylar wire = the length of the single-layer Mylar film segment 101 + (the length of the single-layer Mylar film segment 101 + the multi-layer Mylar film segment 102) * N, where N is a positive integer.

[0038] Generally, the length of the high temperature resistant Mylar wire cannot fully meet the needs of use. It can be used in the form of a redundant part of the length. The redundant length is less than the sum of the length of the single-layer Mylar film segment 101 and the length of the multi-layer Mylar film segment 102, that is, generally less than 13 cm, which will not cause the problem of excessive redundancy.

[0039] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A high temperature resistant Mylar wire, comprising a wire core formed by twisting a plurality of enameled wires (a) into a bundle, wherein the outer side of the wire core is wrapped with a Mylar film layer (b), characterized in that: Along the length direction of the Mylar wire, the Mylar film layer (b) is alternately a single-layer Mylar film segment (101) and a multi-layer Mylar film segment (102); Both ends of the Mylar wire are single-layer Mylar film segments (101).

2. The high temperature resistant Mylar wire according to claim 1, characterized in that: A transition section (103) is provided along the length direction of the Mylar wire and between the single-layer Mylar film section (101) and the multi-layer Mylar film section (102).

3. A high temperature resistant Mylar wire according to claim 1 or 2, characterized in that: The Mylar film layer (b) is formed by spirally winding a PET film on a wire core and then hot-melting it.

4. The high temperature resistant Mylar wire according to claim 3, characterized in that: The multi-layer Mylar film segment (102) is a 2-4-layer PET film spirally wound on a wire core and then heat-melted.

5. The high temperature resistant Mylar wire according to claim 3, characterized in that: The thickness of the PET film is 0.02 mm-0.03 mm.

6. The high temperature resistant Mylar wire according to claim 1, characterized in that: The length of the single-layer Mylar film segment (101) is 2 cm-5 cm.

7. The high temperature resistant Mylar wire according to claim 1, characterized in that: The length of the multi-layer Mylar film segment (102) is 5 cm-8 cm.