Direct current electric arc material melting furnace system
The DC electric arc furnace system addresses the challenge of achieving high melting temperatures and processing difficult materials by stabilizing AC current to DC and adjusting current strength, enabling efficient melting of materials like auto catalysts and other challenging substances.
Patent Information
- Application Number
- PCT/EP2024/058718
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-11
- Filing Date
- 2024-03-28
- Publication Date
- 2024-10-17
AI Technical Summary
Direct current electric arc furnaces (LELK) face limitations in achieving melting temperatures above 2000 °C without a vacuum environment and struggle with difficult-to-melt materials like auto catalysts with high dielectric resistance.
The system includes a DC electric arc furnace with a current converter, lead-lag compensator, switchboard, step-down transformer, and control panel, which stabilizes AC current to DC, allowing for adjustable electrode configurations and increased current strength up to 4000 A, enabling melting temperatures above 2000 °C and efficient processing of challenging materials.
This configuration allows for efficient melting of materials like auto catalysts and other difficult-to-process substances, achieving higher temperatures and improving operational efficiency by directly proportional current strength adjustment, ensuring stable and efficient melting processes without damaging electrodes or the furnace chamber.
Smart Images

Figure 000011 
Figure 000012 
Figure 00000010_0000
Abstract
Description
[0001] Direct current electric arc material melting furnace system
[0002]
[0001] The invention relates to a system (S) comprising a DC electric arc furnace LELK, a method for melting and / or smelting materials, a computer-implemented method, as well as the use of such a system (S) for melting and / or smelting materials.
[0003] Background of the art
[0004]
[0002] Electric arc furnaces (ELK) are furnaces that use an electric arc to melt materials. They are used for melting steel, hard-melting metals, metal shavings, and for processing low-dispersed materials. In electric arc furnaces, metal raw materials are directly exposed to the electric arc. Thus, the current in the furnace flows through the charged material. Two types of electric arc furnaces are known - direct current electric arc furnaces (LELK) and alternating current electric arc furnaces (MELK). [1]
[0005]
[0003] LELKs are more efficient than alternating current electric arc furnaces (MELKs) because they have a lower noise level, they do not cause current surges in the network, and they also create a lower level of gas formation during the melting of materials. Depending on the technical performance, LELK can be 10-15% more economical compared to MELK. LELK can be further divided into two subtypes: steel melting and ore thermal furnaces, where the former are intended for melting different types of steel, while the latter are intended for melting ore materials and various slags. [2]
[0006]
[0004] LELK's melting capacities can be from 1 ton to 400 tons. LELK are also used for various laboratory needs, including dentistry, the melting volume of such furnaces can be up to a few tens of grams. The working temperature of industrial LELKs can reach 1800 °C, while the working temperature of small furnaces suitable for laboratories can be up to 3000 °C. LELK differs from induction furnaces in that the material to be melted is exposed to the direct effect of an electric arc, and the current flow through the material to be melted.
[0007]
[0005] Known MELKs have three lifting electrodes connected to a three-phase connection, the disadvantage of these furnaces is the formation of cold zones, which means that the material to be melted is heated unevenly and additional heat, including chemical energy, is required to eliminate the cold zones, or for compensation. The operation of MELK is based on the fact that its operation regulation system is based on maintaining a consistent - stable, current, and voltage level.
[0008]
[0006] Vacuum electric arc furnaces (VELK) and spark discharge plasma melting furnaces (DPKK) are also known. VELK and DPKK are intended for providing particularly clean castings, or for melting other chemically active metals, such as titanium. This type of furnace is used for scientific research, as well as for the production of parts needed for military aviation. [3]
[0009]
[0007] Known LELKs are designed with a single upper electrode, which is made of graphite and acts as a cathode. Current flows from anode to cathode, and anode configurations, and types can vary. Alternating current is converted into direct current with the help of a transformer, thyristors serve as current rectifiers. Such a device has high stability of the electric arc, reduced noise level by 20 dB, lower waste and gas emissions, as well as 15-20 % lower maintenance costs of the device. [4]
[0010]
[0008] The disadvantages of the known LELKs are the need for high voltages exceeding 440 V, as well as the inability to provide melting temperatures of industrial LELK materials above 2000 °C without a vacuum environment.
[0011]
[0009] Therefore, it is still an urgent question of how to improve the functionality of LELK, which would make it possible to work with difficult-to-melt materials (for example, auto catalysts) as well as new types of materials that have a high dielectric resistance exceeding 104Q.
[0012] The summary of the invention
[0013]
[0010] The proposed invention is a system (S) that comprises an electric arc direct current furnace LELK (1), a DC current converter or current converter (2), a lead-lag compensator (3), a switchboard (4), a step-down transformer ( 5), direct current (DC) power line (6), control panel (7), control cables (8), power supply (9) and alternating current (AC) power line (15). FIG.l.
[0014] [Oi l] In this invention, the term "useful power P" is active power and is expressed in units of W.
[0015] The term "reactive power Q" - power that is not used in work and is expressed in VAR units.
[0016] The term "materials" - automobile or auto catalysts, Li-ion and other types of batteries and accumulators, FeW and NiW compounds, dielectrics, carbon filters, oxides and hydroxides of various metals, electronic scrap.
[0017] The term “cos ” - phase angle between current (I) and voltage (U).
[0018] The term “AC” - alternating current.
[0019] The term “DC” - direct current.
[0020]
[0012] The LELK (1) included in the system (S) comprises at least one first electrode (10a, 10b) and optionally at least one-second electrode (11), where at least one first electrode (10a, 10b) and optionally at least one- second electrode (11 ) is placed perpendicular to the base of the bath (13). The first electrode (10a, 10b) may be positioned opposite the second electrode (11) and the first electrodes (10a, 10b) may be positioned parallel to each other and; where at least part of at least one first electrode (10a, 10b) is configured to be arranged at a material to be melted.
[0021] Likewise, LELK (1) includes thermal insulation material (12), a bath for material loading (13), and a body (14). Various thermally resistant materials, such as MgO bricks, can be used as heat insulation materials (12). The LELK (1) can also comprise a lid that can be closed and opened to ensure the supply of meltable material. In LELK (1) thermal melting of materials and ore takes place. The LELK (1) bath for loading materials (13) can be replaced and is made of heat-resistant material (ceramics), such as magnesite bricks, or any other heat-resistant material. The LELK (1) can be equipped with a discharge hole (16) designed for the discharge of molten material. LELK (1) can optionally be equipped with a cooling system, where water can be used as a cooling medium.
[0022]
[0013] At least one first electrode (10a, 10b) and at least one- second electrode (11) can be made of different materials, but preferably of graphite, they must provide a dielectric conductivity of at least 20 A / cm2, preferably 25 A / cm2. The height of at least one first (10a, 10b) and of at least one-second electrode (11) can be adjusted both mechanically and automatically, this can happen both during and before melting.
[0023]
[0014] The power supply (9) can be of any range depending on the locally available connection types and standards, but the best is AC 6 - 12 kV / 0.38 - 0.44 kV, the power supply (9) provides the power supply to the step-down transformer (5). The power and parameters of the electric supply (9) can be different, according to the intended production of LELK (1). A step-down transformer (5) provides power to the LELK system (S) via the AC power line (15) and is connected to the switchboard (4). A step-down transformer (5) ensures the reduction of the incoming voltage. A switchboard (4) is a device that supplies electricity to oil, water, and other auxiliary systems. The switchboard (4) is connected to the lead-lag compensator (3) via the AC power line (15).
[0024]
[0015] The AC power line (15) operates in the 380-440V range.
[0025]
[0016] The lead-lag compensator (3) includes at least one capacitor (3a), as well as at least one inductive coil (3b) and a computer (3c).
[0026]
[0017] The current converter (2) is connected to the lead-lag compensator (3) through the AC power line (15), where the lead-lag compensator (3) stabilizes the AC current supplied to the current converter (2) through the AC power line ( 15) keeping cos(|) in the range of 0.95 to 0.99.
[0018] The current converter (2) converts alternating current to direct current and provides a direct current supply to at least one first electrode (10a, 10b) and optionally to at least one-second electrode (11) via a DC power line (6).
[0019] When the current converter (2) opens the thyristors and supplies DC current to at least one first electrode (10a, 10b) or optionally at least one-second electrode (11) via the DC power line (6), the computer (3c) analyzes and adjusts current on the AC power line (15), when coscp is not in the range of 0.95 to 0.99, the computer (3c) turns on at least one capacitor (3a) and at least one inductor (3b), thus removing reactive power and higher harmonics in the AC power line (15).
[0020] The task of the current converter (2) is to ensure the operation of the LELK (1) by regulating it according to the current strength (I) from 0.1 A to 4000 A, preferably from 0.1 A to 2000 A, and even better from 0, 1 A to 1700 A.
[0027]
[0021] The function of the lead-lag compensator (3) is to ensure that the coscp value on the AC power line (15) is equal to at least 0.95 or tends to the value 1. The closer the coscp parameter is to the value 1, the more efficient the LELK ( 1) operation [5], a coscp value of 0.01 is equivalent to 1% efficiency in terms of useful power (P). Using the AC power line (15) the lead-lag compensator (3) is connected to the current converter (2). The current converter (2) is a device that can optionally include at least one current transformer (2a). Current converter (2) with the help of thyristor rectifiers and transformer (2a) converts alternating current into direct current and also maintains a stable current strength (I). Current converter (2) can be 6 pulses, 12 pulses, etc. With the help of the DC power line (6), the current converter (2) provides the required local direct current supply to at least one first electrode (10a, 10b) and optionally to at least one-second electrode (11).
[0028]
[0022] Using control cables (8) the control panel (7) is connected to the current converter (2), and lead-lag compensator (3). The control panel (7) is a device that provides monitoring and control of the LELK (1), current converter (2), current transformer (2a) included in it, lead-lag compensator (3), and computer (3c) included in it. The control panel (7) can be connected to a switchboard (4) and a step-down transformer (5). The power supply to the lead-lag compensator (3) can also be provided without a step-down transformer (5) and switchboard (4).
[0029]
[0023] Depending on the desired direction of electrolysis, the connections of the first electrodes (10a, 10b) and the second electrode (11) of LELK (1) can be of the following types: in the first case, only two first electrodes (10a, 10b) work; where independently of each other, one is the anode and the other the cathode, while the second electrode (11) is disconnected or absent; in the second case, both first electrodes (10a, 10b) act as cathodes and the second electrode (11) acts as anode; in the third case, only one first electrode (10a, 10b) works as a cathode and a second electrode (11) works as an anode. The first electrodes (10a, 10b) and the second electrode (11) can be replaced.
[0030]
[0024] In previously known LELK models, the lead-lag compensator (3) is not used, and the LELK adjustment after setting the current strength (I) is not performed. By adjusting the operation of the LELK according to the current (I), it is possible to ensure the working temperature of the LELK of different sizes above 2000 °C without a vacuum environment. Also, it allows to the restoration of melting processes interrupted for various reasons at any time without damaging the electrodes or the furnace chamber. Such proposed system (S) and its principles of operation allow to melt of auto catalysts, Li-ion and other types of batteries and accumulators, FeW and NiW compounds, dielectrics, carbon filters, ores of various compositions, oxides, and hydroxides of various metals, electronic scrap. Such a system (S) can be in different execution and variation versions, as well as include LELK (1) of different volumes and shapes with different numbers of electrodes.
[0031]
[0025] For example, using system (S) for melting and / or smelting materials, work can be started with a current of 0.1 A, which can be increased gradually, according to the thermal properties of the material to be melted, up to 610 A and above, in such a way that coscp is equal to at least 0 .95 or .99. The closer the parameter coscp is to 1, the more efficient the operation of the system
[0032] (5). Such adjustment of the system (S) according to the current strength ensures a directly proportional increase in the temperature of the LELK (1) depending on the set current strength, where the higher the current strength (I), the higher the temperature of the material to be melted.
[0026] A method for melting and / or smelting materials, wherein the method comprises the following steps:
[0033] - providing material to be melted;
[0034] - inserting material to be melted in the system (S) LELK (1);
[0035] - setting the current strength in the current converter (2), in the range from 0.1 A to 4000 A using the control panel (7);
[0036] - setting the lead-lag compensator (3) so that cos(|) is in the range from 0.95 to 0.99;
[0037] - melting the material for a time sufficient to convert the material into molten material. For example, from 1 minute to 50 hours, preferably from 30 minutes to 10 hours.
[0038]
[0027] A computer-implemented method for melting and / or smelting materials in the system (S), comprising the following steps:
[0039] - determining the current target value of the material to be melted, where the current target value is the value that provides the necessary temperature for melting the intended material;
[0040] - sending a signal with the current target value from the control panel (7) to the current converter (2);
[0041] - turning on the current converter (2) and setting the current target value on the DC power line
[0042] (6) in the range from 0.1 A to 4000 A and for at least one first electrode (10a, 10b) and optionally for at least one- second electrode (11); - using the computer (3c), analyze whether the cos(|) on the AC power line (15) is in the range of 0.95 to 0.99;
[0043] - recommend turning on at least one capacitor (3a) and at least one inductive coil (3b) at the same time, if the cos(|) value is not in the range from 0.95 to 0.99;
[0044] - monitoring current target values using the control panel (7) on the DC power line (6) and at least one first electrode (10a, 10b) and optionally at least one-second electrode (11), as well as cos(|) monitoring on the AC power line (15 ). As well as optionally monitoring the switching on of at least one capacitor (3 a) and at least one inductive coil (3b) in the lead-lag compensator (3).
[0045]
[0028] System (S) can be used for melting and / or smelting various materials, especially difficult- to-melt ones, such as auto catalysts.
[0046]
[0029] The invention is explained with the following drawings:
[0047] FIG.l Scheme of the LELK system (S).;
[0048] FIG.2 LELK system (S) operating mode with six 150 kVA current peaks in a 20 ms time interval; FIG.3 Average percentage composition distribution before melting;
[0049] FIG.4 Melting and / or smelting process and extraction of precious metals.
[0050] Examples
[0051]
[0030] The following examples are intended to illustrate some preferred embodiments of the invention and are not, however, limiting.
[0052]
[0031] In the experiment, the two first electrodes (10a, 10b) and one- second electrode (11) of graphite, with a diameter of 100 mm and a dielectric conductivity of 25 A / cm2, were used. For starting the LELK and for current flow between the first electrodes (10a, 10b), crushed graphite, which was initially deposited on the melting material, was used to provide current flow between the two first electrodes (10a, 10b). As the temperature of the melting materials increases, their dielectric resistance decreases. For the experimental LELK system (S), a current converter (2) from the manufacturer ABB model DCS 800 was used.
[0053]
[0032] Experimental LELK current measurements were made with a Fluke 190-204 SCOPEMETER, where the current strength (I) depends on the opening angle of the thyristors. FIG. 2 shows that the system (S) has six 150 kVA current peaks in a 20 ms time interval in operating mode.
[0054]
[0033] Within the framework of the experimental part, twenty melts have been carried out, in which used auto catalysts were used as raw materials. The processing of these materials is important, especially for the separation and extraction of precious metals - platinum, palladium, and rhodium. Each experimental melt was made using 1000 kg of raw material - auto catalysts. Precious metals are collected using commonly known methods, for example with a collector. Before each melt, a quantitative material analysis was performed to determine the percentage composition of the material to be melted. The obtained data were collected and their average percentage distribution of material composition is shown in FIG. 3.
[0055] According to the obtained data, it can be seen that the mentioned precious metals make up a total of 0.237% or 2.37 kg of the total 1000 kg of raw material. The average distribution of precious metals is as follows: Pt - 0.126%, Pd - 0.085%, and Rh - 0.026%.
[0056] The system (S) described in the invention was used for melting and / or smelting the auto catalysts sent for recycling.
[0057]
[0034] The smelting process and extraction of precious metals were carried out in the following set current (I) range: 5A to 1000A. FIG. 4. It can be seen that the current parameter (I) set at the start of the melting process, which is equal to 5A, corresponds to the temperature parameter of the melting material, t °C, which is equal to 25 °C. On the other hand, the set current strength (I) of 1000 A corresponds to the temperature of the material to be melted, t °C, which is equal to 1700 °C.
[0058]
[0035] When smelting auto catalysts and extracting precious metals, additives Na2O, Na2COs, CaO, CaCOs, or Ca(OH)2 can be used during smelting, the amount of which can be added as needed depending on the processes taking place during smelting.
[0059]
[0036] As a result of experiments, it has been proven that the temperature (t, °C) of the material to be melted increased with the increase of the set current (I) parameter. So, when melting materials with the system (S), the temperature of the materials is not related to the holding time but depends on the current (I), where the higher the current (I), the higher the temperature (t, °C) of the material to be melted.
[0060]
[0037] In order to be able to determine how efficiently precious metals were extracted from auto catalysts sent for recycling after smelting, a quantitative analysis of the obtained slag and determination of the amount of precious metals was performed. Averaged over twenty smeltings, it was determined that platinum, palladium, and rhodium totaled an average of 2.8 grams per metric ton of slag. This means that, on average, 2370-2.8=2367.2 g of precious metals were obtained from each 1 metric ton of auto catalyst melt.
[0061] References
[0062] [1] Hurtta Matti, Direct current electric arc furnace WO2021094646, 2021
[0063] [2] / JYFOBA5I IIETb nOCTOJJHHOFO TOKA; https: / / toledo.su / catalog / plavilnye-pechi /
[0064] [3] DjieKTpo^yroBaa newt - Electric arc furnace; https: / / ru.wikibrief.org / wiki / Electric_arc_furnace
[0065] [4] DC Electric Arc Furnace; https: / / www.ispatguru.com / dc-electric-arc-furnace /
[0066] [5] Resonance; https: / / en.wikipedia.org / wiki / Resonance
Claims
Claims1. System (S) comprising:- a direct current electric arc furnace LELK (1), comprising at least one first electrode (10a, 10b) and optionally at least one- second electrode (11);- wherein at least a part of the at least one first electrode (10a, 10b) is configured to be arranged at a material to be melted;- power converter (2), for converting AC current supplied via an AC power line (15) to DC current for providing the DC current via a DC power line (6) to the at least one first electrode (10a, 10b) and optionally to the at least one second electrode (11);- power converter (2) is connected to the lead-lag compensator (3) via the AC power line (15);- wherein the lead-lag compensator (3) stabilizes the AC current supplied to the power converter (2) via the AC power line (15) by holding cos(j> in the range of 0,95 to 0,99, wherein cos(j> is the phase angle between current and voltage;- wherein power converter (2) is configured to regulate the DC current provided to the at least one first electrode (10a, 10b) and optionally to the at least one-second electrode (11) to a set current,- wherein the set current has a value in the range of 0.1 A to 4000 A.
2. The system (S) according to claim 1, wherein the AC power line (15) is operated in the range of 380 to 440 V.
3. The system (S) according to claim 1 or 2, wherein the lead-lag compensator (3) comprises at least one capacitor (3a), at least one inductive coil (3b) and a computer (3c).
4. The system (S) according to claims 1 to 3, further comprising a switchboard (4) which is connected to the lead-lag compensator (3) via an AC power line (15).
5. The system (S) according to claims 1 to 4 further comprises a step-down transformer (5) which ensures a reduction of the incoming voltage and is connected to the switchboard (4) via an AC power line (15).
6. The system (S) according to claims 1 to 5 further comprises a heat-resistant bath (13) for melting materials.
7. The system (S) according to claim 6 further comprises a discharge hole (16) for draining the molten material.
8. The system (S) according to claims 1 to 7, wherein the set current value is in the range of 0.1 A to 2000 A, preferably 0.1 A to 1700 A.
9. The system (S) according to claims 1 to 8 further contains the cooling system of the DC electric arc furnace LELK (1).
10. A method for melting and / or smelting materials, where the method comprises the following steps:- providing a meltable material;- placing the meltable material in the systems’ (S) according to claims 1 to 9 the direct current electric arc furnace LELK (1);- setting the current strength in the current converter (2), in the range from 0.1 A to 4000 A, using the control panel (7);- setting the lead-lag compensator (3) to have cos(j> is in the range from 0.95 to 0.99;- melting the material for a time sufficient to convert the material into molten material.
11. A computer- implemented method for melting and / or smelting materials in a system (S) according to any one of claims 1 to 9, comprising the following steps:- determining the current target value of the material to be melted;- sending a signal with the current target value from the control panel (7) to the current converter (2);- switching on the current converter (2) and setting current target values in the range of 0.1 A to 4000 A for at least one first electrode (10a, 10b) and optionally for at least one- second electrode (11) using the DC power line (6);- analyzing using the computer (3c) whether the cos(j> on the AC power line (15) is in the range of O.95 to O.99;- recommending turning on at least one capacitor (3a) and at least one inductive coil (3b) at the same time, if the cos(|) value is not in the range from 0.95 to 0.99;- monitoring, using the control panel (7), the current target value on the DC power line (6) and at least one first electrode (10a, 10b) and optionally at least one-second electrode (11), and cos(j> on the AC power line (15).
12. Use of the system (S) according to any of claims 1 to 9 for melting and / or smelting materials.
Citation Information
Patent Citations
Direct current electric arc furnace
WO2021094646A1
Flicker compensating apparatus for DC arc furnace
EP0483405B1
Method for stabilizing a power supply network against reactive load fluctuations, and a power factor compensation device