A production process and rotary hearth furnace technology, applied in the field of metallurgy, can solve the problems of increased processing burden, increased production cost, increased processing capacity or power consumption, etc., achieve good promotion and application prospects, solve high production costs, increase production costs Effect

Active Publication Date: 2016-04-27
PANGANG GRP PANZHIHUA STEEL & VANADIUM
View PDF1 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Since the preparation process of carbon-containing pellets requires an additional binder, if the binder is an inorganic type, it will increase the production cost of the pellets and increase the processing burden of the subsequent process, resulting in unnecessary processing capacity or power consumption. increase; if the organic type adhesive is used, the cost will increase even more due to the influence of its overall higher price

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

example 1

[0032] The water content of the iron concentrate is 7.9wt%, the water content of the high-temperature asphalt powder is 5.0wt%, and the proportion of the high-temperature asphalt powder whose particle size is below 40 mesh accounts for 25.5wt%. The iron concentrate and high-temperature asphalt powder are batched according to the ratio of 96.9wt% and 3.1wt%, and mixed on the roller mixer for 5 minutes, and then the resulting mixture enters the storage bin of the ball briquetting machine. After testing, the water content of the mixture at this time is 7.8wt%, and the temperature is 32°C. The waste heat flue gas of 602°C is passed into the mixture from the bottom of the storage bin for 3 minutes, and the water content of the mixture is 6.4wt%. , The temperature is 91°C, and then the balls are pressed, and the drop strength of the carbon-containing pellets obtained by pressing is ≥6 times / 50cm, which meets the requirements of subsequent transportation.

example 2

[0034] The water content of the iron concentrate is 2.3wt%, the water content of the high-temperature asphalt powder is 1.8wt%, and the proportion of the high-temperature asphalt powder whose particle size is below 40 mesh accounts for 60.8wt%. The iron concentrate, high-temperature pitch powder, and anthracite powder are batched according to the ratio of 81wt%, 5wt%, and 14wt%, and mixed on the roller mixer for 8 minutes, and then the resulting mixture enters the storage bin of the pelletizing machine. After testing, the water content of the mixture at this time is 1.8wt%, and the temperature is 48°C. Water vapor is passed into the mixture from the bottom of the storage bin for 4 minutes. At this time, the water content of the mixture is 5.1wt%, and the temperature is 99°C. , and then start to press the balls, and the drop strength of the carbon-containing pellets obtained by pressing is ≥8 times / 50cm, which meets the requirements for subsequent transportation.

[0035] The p...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
softening pointaaaaaaaaaa
densityaaaaaaaaaa
Login to view more

Abstract

The invention discloses a pelletizing method of pellets for a direct reduction production process of a rotary hearth furnace. The pelletizing method comprises the following steps: controlling the water content of high-temperature asphalt powder to be not more than 5wt%, controlling the water content of iron ore concentrate to be not more than 8wt%, and uniformly mixing the high-temperature asphalt powder, the iron ore concentrate and a carbon-containing supplementary reducing agent to obtain a mixture, wherein the mixing amount of the high-temperature asphalt powder is not lower than 3wt% of the total amount of the mixture, and the mixing amount of the carbon-containing supplementary reducing agent accounts for 0-25wt% of the total amount of the mixture; pelletizing the mixture to obtain the pellets, wherein the water content of the mixture is controlled at 5-6.5wt%, and the temperature of the mixture is 90-130 DEG C. By adopting the pelletizing method disclosed by the invention, the problem of high preparation and production cost of a traditional pelletizing process is solved, the pelletizing method can be used for simultaneously assisting in solving the process defect that ash and other impurities are introduced when an inorganic adhesive is adopted for pelletizing, and the pelletizing method further has good popularization and application prospect.

Description

technical field [0001] The invention belongs to the technical field of metallurgy, and more specifically relates to a pelletizing method for pellets used in a rotary hearth furnace direct reduction production process. Background technique [0002] With the increasing shortage of resources, especially the scarcity of high-quality iron-containing raw materials and coking coal, the survival and development of traditional blast furnace smelting iron and steel enterprises have been greatly challenged. However, the non-blast furnace ironmaking technology with less resource constraints, greater flexibility, and short process has attracted more and more attention. The attention and application of it to the production of direct reduction of iron ore has achieved rapid development. [0003] In actual production, iron concentrate resources including vanadium-titanium magnetite are directly reduced by rotary hearth furnace. However, due to the overall low grade of iron concentrate in m...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): C22B1/244
Inventor 刘功国秦洁何绍刚
Owner PANGANG GRP PANZHIHUA STEEL & VANADIUM
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products