A preparation method of folic acid-coupled gold nanorod/polypyrrole/ferric oxide multifunctional composite nano-diagnosis and treatment agent
A technology of ferric tetroxide and gold nanorods, which can be used in preparations for in vivo experiments, medical preparations containing active ingredients, and drug combinations, etc., can solve the problems of low immunity and lack of targeting of patients, and achieve Conducive to mass production, good imaging effect, and strong tumor targeting effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0040] (1) prepare the gold nanorod solution that sodium lauryl sulfate is stable;
[0041] (2) Add 0.373g ferric chloride to 10mL 8% polyvinyl alcohol solution, heat and stir thoroughly;
[0042] (3) Add 1 mL of the gold nanorod solution prepared in step (1) to the polymer solution prepared in step (2), ultrasonically disperse, and stir evenly;
[0043] (4) Add 70 μL of pyrrole monomer dropwise to the mixed solution prepared in step (3) after ice-bathing, stir for 10 minutes, quickly place it in a refrigerator at 4°C, and keep it for 12 hours. The solution turns black, and the mixture containing Suspension of gold nanorods / polypyrrole nanoparticles;
[0044] (5) Measure 2 mL of the suspension of gold nanorods / polypyrrole nanoparticles prepared in step (4), dilute with 12 mL of ionized water and 1.6 mL of ethanol, raise the temperature to 60 ° C, and quickly add 0.8 mL of the suspension under nitrogen protection After reacting for 25 minutes, 0.8 mL of ammonia solution was a...
Embodiment 2
[0049] (1) prepare the gold nanorod solution that sodium lauryl sulfate is stable;
[0050] (2) Add 180mg of ferric chloride into 10mL of 8% polyvinyl alcohol solution, heat and stir thoroughly;
[0051] (3) Add 2 mL of the gold nanorod solution prepared in step (1) to the polymer solution prepared in step (2), ultrasonically disperse, and stir evenly;
[0052] (4) Add 100 μL of pyrrole monomer dropwise to the mixed solution prepared in step (3) after ice-bathing, stir for 10 minutes, quickly place it in a refrigerator at 4°C, and keep it for 12 hours. The solution turns black, and the mixture containing Suspension of gold nanorods / polypyrrole nanoparticles;
[0053] (5) Measure 5 mL of the gold nanorod / polypyrrole nanoparticle suspension prepared in step (4), dilute it with 16 mL of ionized water and 2 mL of ethanol, raise the temperature to 70 ° C, and quickly add 1.2 mL of Ammonia solution, after reacting for 25 minutes, add 1.2 mL of ammonia solution again, and continue ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com