A method for hydrogenation conversion of wide distillation range Fischer-Tropsch wax
By using molecular sieve catalysts of specific grain sizes in the hydrogenation isomerical cracking process, the problem in the prior art is solved that it is difficult to meet the pour point and viscosity index requirements of light and heavy base oil components in Fischer-Tropsch synthetic waxes simultaneously. , achieve high efficiency and high yield of lubricating oil base oil with low pour point and high viscosity index.
Patent Information
- Application Number
- CN202111346680.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-15
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-11-15
AI Technical Summary
When using traditional hydrogenation isomerial dewaxing catalysts, it is difficult to meet the pour point and viscosity index requirements of light and heavy base oil components in wide distillation Fischer-Tropsch synthetic wax at the same time, and the process economy is poor.
Using a hydroisomerative cracking process based on combining molecular sieve catalysts with specific grain sizes, the light in the broad distillation raw materials can be highly selectively converted through steps such as hydropreparation, hydroisomerization-cracking and hydrorefining. and medium-quality components, and light and medium-quality base oil components are formed by subsequent hydrocracking.
A lubricating oil base oil with low pour point and high viscosity index is achieved at a high yield, which avoids excessive cracking of the whole fraction, reduces the generation of by-products, and improves the yield and performance of base oil products.
Smart Images

Figure CN116120966B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for hydrogenation conversion of Fischer-Tropsch synthesis products, and in particular to a method for producing a base oil-based product by hydrogenation conversion using wide-distillation range Fischer-Tropsch synthesis wax as a raw material. Background Art
[0002] Fischer-Tropsch wax is the main product of the Fischer-Tropsch synthesis reaction of synthesis gas (CO and H2). It is mainly composed of long-chain alkanes, which can be further hydrogenated to produce liquid fuels and chemicals. The main components of Fischer-Tropsch wax are straight-chain alkanes, which contain almost no sulfur, nitrogen and aromatics. It is a high-quality raw material for high-grade lubricant base oil. The technical key to converting Fischer-Tropsch wax products into high-grade lubricant base oil is to improve the low-temperature flow properties of the oil while maintaining a high viscosity index, that is, to lower the freezing point, which can be achieved through hydrocracking and hydroisomerization reactions.
[0003] In the field of lubricating base oil produced by hydrogenation and reforming of Fischer-Tropsch wax, many relevant patents have been published at home and abroad. For example, US5834522 discloses a method for producing lubricating base oil using Fischer-Tropsch synthesis products as raw materials, wherein the Fischer-Tropsch synthesis products are hydrogenated and isomerized in a hydrogenation and isomerization reaction zone, and the generated oil is separated by distillation, and then the distillation bottoms are dewaxed to obtain oil and non-oil fractions. US5882505 discloses a method for producing lubricating base oil by converting Fischer-Tropsch synthesis wax with a boiling point greater than 370°C using a countercurrent reactor, wherein the raw material is contacted with a hydrogenation and isomerization catalyst in a fixed bed reactor, and the product after the reaction is contacted with a hydrogenation and dewaxing catalyst in at least one fixed bed reactor to obtain the target product, wherein the hydrogenation and isomerization reaction products flow in the opposite direction to the hydrogen-containing gas. CN1688674 discloses a multi-step method for preparing a heavy lubricating oil base from Fischer-Tropsch wax, which comprises hydrodewaxing the wax in a first hydrodewaxing step to obtain an isomerization product of a partially dewaxed heavy base oil fraction, and then hydrodewaxing the heavy lubricating oil fraction in one or more successive hydrodewaxing steps to remove hydrocarbons below the heavy lubricating oil fraction to obtain a heavy lubricating oil base. CN1703488 discloses a method for preparing fuel and lubricating oil base from Fischer-Tropsch wax, which comprises (1) hydrodewaxing the Fischer-Tropsch wax to prepare an isomerization product comprising a fuel and a partially hydrodewaxed base oil fraction, (2) separating the two fractions, (3) separating the partially hydrodewaxed base oil fraction into a heavy fraction and a lower boiling point fraction, and (4) further hydrodewaxing the lower boiling point fraction and the heavy fraction to prepare a lubricating oil base including a heavy lubricating oil base. CN101230290 discloses a method for producing solvent oil, lubricating oil base oil and heavy wax from Fischer-Tropsch wax, wherein the whole fraction product obtained by converting the wax in the hydrorefining zone is fractionated to obtain a light fraction of solvent oil, and then the base oil fraction segment product is separated and then subjected to hydroisomerization conversion, and the remaining heavy fraction is directly subjected to hydrorefining to obtain decolorized wax. US7198710 discloses a method for producing a high viscosity index lubricating oil base oil from Fischer-Tropsch wax, wherein the Fischer-Tropsch wax is first fractionated to obtain a light component and a heavy component, and then hydroisomerization dewaxing is performed to reduce the pour point of the raw material, and a light lubricating oil base oil with a pour point that meets the requirements can be obtained. When the heavy component is hydroisomerized dewaxed, since the pour point is unqualified, the solvent dewaxing method is used to further reduce the pour point of the heavy component, and finally a heavy lubricating oil base oil product with a pour point that meets the requirements is obtained.
[0004] In the above process, the disadvantage of using the traditional hydroisomerization dewaxing catalyst in the hydrodewaxing operation unit is that when the full-fraction or wide-fraction Fischer-Tropsch wax is used as the feed, it is difficult to make the light and heavy base components meet the requirements of pour point and viscosity index at the same time. When the heavy base oil component has a qualified pour point, the viscosity index loss of the light base oil component is large, and it is difficult to produce API III light lubricating base oil products with a viscosity index>120; and when the light base oil component has a qualified viscosity index, the heavy component cannot be used as a lubricating base oil product with a qualified pour point. When the traditional hydrocracking catalyst is used, whether the full-fraction or wide-fraction Fischer-Tropsch wax is used as the feed, the light and heavy base oil products can mostly meet the requirements of pour point and viscosity index at the same time, but the process produces a large amount of cracking products, and the yield of light and heavy base oils is too low, which seriously affects the process economy. Summary of the invention
[0005] In view of the deficiencies of the prior art, the present invention provides a method for hydrogenation conversion of wide-range Fischer-Tropsch wax, which can produce low-pour point, high-viscosity index lubricating base oil with high yield through hydrogenation pretreatment-hydroisomerization-hydrofining-fractionation process. The core technology of the invention is based on the combination of molecular sieve catalyst hydroisomerization cracking process with specific crystal size, so that light and medium components in wide-range raw materials can be highly selectively converted into isomerized products, and heavy components can continue to be hydrocracking to generate light and medium base oil components after high-selectivity isomerization, thereby avoiding excessive cracking of all fractions at the same time, reducing the generation of gaseous hydrocarbons and gasoline and diesel fraction by-products, and achieving simultaneous improvement of base oil product yield and performance.
[0006] The wide-range Fischer-Tropsch wax hydrogenation conversion method of the present invention mainly comprises: the wide-range Fischer-Tropsch wax first enters a hydrogenation pretreatment reaction zone to complete the hydrogenation saturation and hydrogenation deoxygenation of non-alkane components in the raw material; the obtained hydrogenation pretreatment oil enters a hydrogenation isomerization reaction zone to complete the hydrogenation isomerization-cracking of the hydrogenation pretreatment oil on a combined molecular sieve catalyst with a specific grain size; the obtained hydroisomerization cracking oil enters a hydrorefining reaction zone for further treatment to obtain a crude product; the crude product is fractionated in a normal / vacuum tower to obtain base oil, diesel, gasoline and other products.
[0007] The technical solution of the present invention includes the following implementation steps:
[0008] 1) The wide distillation range fraction of Fischer-Tropsch wax is mixed with hydrogen and enters the hydrogenation pretreatment reaction zone. On the bed containing the hydrogenation pretreatment catalyst, the temperature is 150-450°C, the hydrogen partial pressure is 3-18MPa, and the raw oil volume space velocity is 0.3-5h -1 , under the condition of hydrogen-to-oil ratio of 200:1-2000:1, the non-alkane components in the feedstock are hydrogenated and saturated and hydrodeoxygenated to obtain hydrogenation pretreated oil;
[0009] 2) The hydrotreated oil obtained in step 1) enters the hydroisomerization-cracking reaction zone, and the reaction temperature is 250-400°C, the hydrogen partial pressure is 2-20MPa, and the feed oil volume space velocity is 0.3-5h -1 , under the condition of hydrogen-oil ratio of 200:1-2000:1, carrying out hydroisomerization reaction to complete the hydroisomerization and hydrocracking reaction of the hydrotreatment pretreated oil to obtain hydroisomerization cracked oil;
[0010] 3) The hydroisomerized cracked oil obtained in step 2) enters the hydrotreating reaction zone. On the hydrotreating catalyst, the reaction temperature is 180-320°C, the hydrogen partial pressure is 2-20MPa, and the raw oil volume space velocity is 0.3-5h -1 , under the condition of hydrogen-oil ratio of 200:1-2000:1, further hydrogenation saturation of hydroisomerized cracking oil is completed to obtain a crude product;
[0011] 4) The crude product obtained in step 3) enters a normal / vacuum tower for fractionation to obtain gasoline, diesel, base oil and other products;
[0012] Among them, the combined catalyst with a specific grain size in the step 2) is: a catalyst A prepared by using a molecular sieve with an AEL structure and a grain size of 10 nm to 500 nm as a carrier and loaded with platinum, palladium and / or iridium, and a catalyst B prepared by using a molecular sieve with a TON structure and a grain size of 500 nm to 10 μm as a carrier and loaded with platinum, palladium and / or iridium in a certain proportion.
[0013] The method described herein, wherein the Fischer-Tropsch wax wide distillation range fraction raw material in step 1) refers to a Fischer-Tropsch wax fraction having an initial distillation point not higher than 240°C and not lower than 180°C and a final distillation point not lower than 700°C and not higher than 730°C.
[0014] The method described herein, wherein the content of normal alkanes in the Fischer-Tropsch wax wide distillation range fraction raw material in step 1) is not less than 90 wt%.
[0015] In the method, the hydrogenation pretreatment catalyst in step 1) is composed of a heat-resistant inorganic oxide as a carrier and a transition metal and a non-metallic additive.
[0016] The method described above, wherein the heat-resistant inorganic oxide in the hydrogenation pretreatment catalyst in step 1) is aluminum oxide, silicon oxide and / or an amorphous composite of the two.
[0017] The method described, wherein the transition metal loading component in the hydrogenation pretreatment catalyst in step 1) is composed of one or more metals selected from cobalt, nickel, molybdenum and tungsten, and one or more non-metallic additives selected from nitrogen, phosphorus, sulfur or boron.
[0018] The method, wherein the transition metal loaded on the hydrogenation pretreatment catalyst in step 1) is one or more of cobalt, nickel, molybdenum and tungsten, and the mass content thereof is 10-28wt%.
[0019] In the method, the non-metallic additive supported on the hydrogenation pretreatment catalyst in step 1) is one or more of nitrogen, phosphorus, sulfur or boron, and its mass content is 2-8wt%.
[0020] The method, wherein the preferred hydrogenation pretreatment reaction conditions in step 1) are: temperature 180-320°C, hydrogen partial pressure 5-12MPa, feed oil volume space velocity 0.5-3h -1 , the hydrogen-to-oil ratio is 200:1-1600:1.
[0021] In the method, the hydro-pretreated oil obtained in step 1) is not subjected to atmospheric and vacuum distillation, but directly enters the subsequent hydro-isomerization-cracking reaction zone to continue the reaction.
[0022] The method, wherein the catalysts A and B in step 2) are catalysts using a ten-membered ring molecular sieve carrier and loaded with platinum, palladium and / or iridium metal components.
[0023] The method, wherein the catalyst A in step 2) is a catalyst using a molecular sieve having an AEL structure as a carrier and loaded with platinum, palladium and / or iridium metal components.
[0024] The method, wherein the mass content of active metal on catalyst A in step 2) is 0.3-0.6wt%.
[0025] The method, wherein the catalyst B in step 2) is a catalyst using a molecular sieve having a TON structure as a carrier and loaded with platinum, palladium and / or iridium metal components.
[0026] The method, wherein in step 2), the mass content of active metal on catalyst B is 0.4-0.8wt%.
[0027] In the method, the particle size of the AEL structure molecular sieve carrier used in the catalyst A in step 2) is 20nm to 200nm.
[0028] The method, wherein the grain size of the TON structure molecular sieve carrier used in the catalyst B in step 2) is 800nm to 5μm.
[0029] The method described herein, wherein the molecular sieve having an AEL structure is one or more of SAPO-11, MeAPO-11 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Cd or Ni).
[0030] The method described herein comprises the following steps: wherein the mass percentage of Me in the molecular sieve MeAPO-11 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Cd or Ni) having an AEL structure is 0.5 to 1.5 wt%.
[0031] The method described, wherein the molecular sieve having a TON structure is one or more of ZSM-22, Me-ZSM-22 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Fe, Cd or Ni, etc.), Theta-1, KZ-2, ISI-1 and NU-10, etc.
[0032] The method described herein, wherein the molecular sieve having a TON structure is Me-ZSM-22 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Fe, Cd or Ni, etc.), and the mass percentage of Me is 0.2 to 2.0 wt%.
[0033] The method, wherein the total acid content of the molecular sieve carrier with an AEL structure is 200 to 800 μmol (Pyridine) / g, and the total acid content is measured and calculated using pyridine adsorption infrared spectroscopy.
[0034] The method described herein, wherein the external surface acid amount of the molecular sieve carrier having an AEL structure is 100 to 300 μmol (2,6-Di-tert-butylpyridine) / g, and the external surface acid amount is measured and calculated using 2,6-di-tert-butylpyridine adsorption infrared spectroscopy.
[0035] The method, wherein the total acid content of the molecular sieve carrier having a TON structure is 100-600 μmol (Pyridine) / g, and the total acid content is measured and calculated using pyridine adsorption infrared spectroscopy.
[0036] The method described, wherein the external surface acid amount of the molecular sieve carrier with a TON structure is 0 to 100 μmol (2,6-Di-tert-butylpyridine) / g, and the external surface acid amount is tested and calculated using 2,6-di-tert-butylpyridine adsorption infrared spectroscopy.
[0037] The method, wherein in step 2), the combination of catalysts A and B is A on top and B on the bottom, with a volume ratio of 1:10-10:1.
[0038] The method, wherein in step 2), the volume ratio of catalyst A to catalyst B is 1:6-6:1.
[0039] The method, wherein in step 2), the volume ratio of catalyst A to catalyst B is 1:3-3:1.
[0040] The method, wherein the conditions for the hydroisomerization reaction in step 2) are: temperature of 250-400°C, hydrogen partial pressure of 2-15 MPa, and feed oil volume space velocity of 0.5-3 h -1 , the hydrogen-to-oil ratio is 200:1-1600:1.
[0041] The method, wherein the preferred hydroisomerization reaction conditions in step 2) are: temperature 280-380°C, hydrogen partial pressure 2.5-8MPa, feed oil volume space velocity 0.5-1.5h -1 , the hydrogen-to-oil ratio is 200:1-800:1.
[0042] The method, wherein the hydrotreating catalyst in step 3) is composed of a heat-resistant inorganic oxide as a carrier and a metal component supported on the carrier.
[0043] The method described above, wherein the heat-resistant inorganic oxide in the hydrorefining catalyst of step 3) is aluminum oxide, silicon oxide and / or an amorphous composite of the two.
[0044] The method described above, wherein the metal component in the hydrorefining catalyst in step 3) is composed of one or more metals selected from platinum, palladium and iridium, and one or more additives selected from cobalt, nickel, molybdenum and tungsten.
[0045] The method, wherein the mass content of active metals platinum, palladium and iridium in the hydrogenation refining catalyst in step 3) is 0.2-0.5wt%, and the mass content of the auxiliary agent is 0.5-3wt%.
[0046] The method, wherein the hydrofining reaction conditions in step 3) are: temperature 180-320°C, hydrogen partial pressure 2-15MPa, raw oil volume space velocity 0.5-3h -1 , the hydrogen-to-oil ratio is 200:1-1600:1.
[0047] The method, wherein the crude product obtained in step 3) enters the normal and vacuum towers in sequence for fractionation to obtain products such as gasoline, kerosene, diesel and base oil.
[0048] The method, wherein the atmospheric and vacuum distillation towers in step 4) are well-known operations in the art, usually including one or more flash distillation, atmospheric distillation, and vacuum distillation tower operation units to achieve separation of products in different distillation ranges.
[0049] Compared with the existing methods, the Fischer-Tropsch wax hydrogenation conversion method provided by the present invention has the following advantages: wide-range Fischer-Tropsch wax can be converted into lubricating oil base oil products with high selectivity; the process conditions are simple, and there is no need to circulate the products of hydrogenation isomerization-cracking, and the target product can be obtained in one pass; the base oil product prepared by this method has a high yield and excellent performance.
[0050] Compared with the prior art, the method of the invention can obtain a base oil with a low pour point and a high viscosity index at a higher yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 Brief process flow chart DETAILED DESCRIPTION
[0052] The present invention is further described below in conjunction with specific embodiments, but it should be pointed out that the present invention is not limited thereto.
[0053] The information and preparation methods of the pre-hydrogenation catalyst, hydroisomerization catalyst and hydrofining catalyst used in the embodiments of the present invention are as follows:
[0054] 1. Hydrogenation pretreatment catalyst T1
[0055] The hydrogenation pretreatment catalyst T1 is prepared by a conventional impregnation method. The catalyst is composed of a heat-resistant inorganic oxide aluminum oxide and / or silicon oxide as a carrier, one or more metals of cobalt, nickel, molybdenum and tungsten loaded on the carrier, and one or more additives selected from nitrogen, phosphorus, sulfur or boron. Based on the weight percentage of the catalyst, the content of cobalt, nickel, molybdenum and tungsten is 25wt%, the content of nitrogen, phosphorus, sulfur and boron is 5wt%, and the rest is aluminum oxide and / or silicon oxide.
[0056] 2. Hydroisomerization-cracking catalysts A and B, etc.
[0057] Hydroisomerization-cracking catalyst A is prepared by impregnation, electrostatic adsorption or ion exchange. The catalyst uses a molecular sieve carrier with an AEL structure, which is one or more of SAPO-11, MeAPO-11 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Cd or Ni), and the molecular sieve has a particle size of 20nm to 200nm, a total acid content of 200 to 800μmol (Pyridine) / g, and an external surface acid content of 100 to 300μmol (2,6-Di-tert-butylpyridine) / g. Based on the weight percentage of the catalyst, the content of platinum, palladium and / or iridium is 0.5wt%, and the rest is the molecular sieve of the above-mentioned AEL structure.
[0058] Hydroisomerization-cracking catalyst B is prepared by impregnation, electrostatic adsorption or ion exchange. The catalyst uses a molecular sieve carrier with a TON structure, which is one or more of ZSM-22, Me-ZSM-22 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Fe, Cd or Ni, etc.), Theta-1, KZ-2, ISI-1 and NU-10, etc. The molecular sieve has a particle size of 800nm to 5μm, a total acid content of 100 to 600μmol (Pyridine) / g, and an external surface acid content of 0 to 100μmol (2,6-Di-tert-butylpyridine) / g. Based on the weight percentage of the catalyst, the content of platinum, palladium and / or iridium is 0.5wt%, and the rest is the molecular sieve of the above-mentioned TON structure.
[0059] Hydroisomerization-cracking catalyst C is prepared by impregnation, electrostatic adsorption or ion exchange. The catalyst uses a molecular sieve carrier with a TON structure, which is one or more of ZSM-22, Me-ZSM-22 (Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Fe, Cd or Ni, etc.), Theta-1, KZ-2, ISI-1 and NU-10, etc. The molecular sieve has a particle size of 20nm to 200nm, a total acid content of 300 to 800μmol (Pyridine) / g, and an external surface acid content of 100 to 300μmol (2,6-Di-tert-butylpyridine) / g. Based on the weight percentage of the catalyst, the content of platinum, palladium and / or iridium is 0.5wt%, and the rest is the molecular sieve of the above-mentioned TON structure.
[0060] Industrial catalyst D, the carrier is SAPO-11 molecular sieve, which belongs to AEL structure, the particle size of the molecular sieve is 600nm, the total acid content is 850μmol (Pyridine) / g, and the external surface acid content is 330μmol (2,6-Di-tert-butylpyridine) / g. Based on the weight percentage of the catalyst, the content of platinum, palladium and / or iridium is 0.5wt%, and the rest is the above-mentioned SAPO-11 molecular sieve.
[0061] Industrial catalyst E, the carrier is ZSM-22 molecular sieve, which belongs to TON structure, the particle size of the molecular sieve is 600nm, the total acid content is 700μmol (Pyridine) / g, and the external surface acid content is 240μmol (2,6-Di-tert-butylpyridine) / g. Based on the weight percentage of the catalyst, the content of platinum, palladium and / or iridium is 0.5wt%, and the rest is the above ZSM-22 molecular sieve.
[0062] Other catalyst characteristics are described in detail in the comparative examples.
[0063] 3. Hydrorefining catalyst T2
[0064] The hydrofining catalyst T2 is prepared by a conventional impregnation method. The catalyst is composed of a heat-resistant inorganic oxide aluminum oxide and / or silicon oxide as a carrier, one or more metals of platinum, palladium and iridium loaded on the carrier, and one or more additives selected from cobalt, nickel, molybdenum and tungsten. Based on the weight percentage of the catalyst, the content of platinum, palladium and / or iridium is 0.25wt%, the content of cobalt, nickel, molybdenum and tungsten is 1.5wt%, and the rest is aluminum oxide and / or silicon oxide.
[0065] Test of total acidity of samples (pyridine adsorption infrared (Py-IR) test): Weigh 10-20 mg of sample and press it into a circular self-supporting sheet with a diameter of 13 mm, and put it into the in-situ infrared cell. Pre-treat it at 350℃ for 30 minutes, cool it to room temperature and record the blank sample spectrum. After pyridine is adsorbed, heat it to 150℃ and vacuum it for 30 minutes, cool it to room temperature and record the spectrum of pyridine adsorption. Calculate the total acidity of the sample based on the characteristic peak area.
[0066] Sample external surface acidity test (2,6-di-tert-butylpyridine adsorption infrared (DTBPy-IR) test): Weigh 10-20 mg of sample and press it into a circular self-supporting sheet with a diameter of 13 mm, and place it in an in-situ infrared cell. First, vacuum pre-treat at 350°C for 30 minutes, cool to 150°C and record the blank sample spectrum. After adsorbing 2,6-di-tert-butylpyridine (2,6-Di-tert-butylpyridine), vacuum for 30 minutes and record the spectrum of 2,6-di-tert-butylpyridine adsorption. After that, heat to 300°C and vacuum for 30 minutes, cool to 150°C and record the spectrum of 2,6-di-tert-butylpyridine adsorption. Calculate the total acidity of the sample based on the characteristic peak area.
[0067] The embodiments of the present invention use a wide distillation range Fischer-Tropsch wax as a raw material, and its properties are shown in Table 1.
[0068] The brief process flow chart of the present invention is as follows Figure 1 shown.
[0069] 1) The Fischer-Tropsch wax wide distillation range fraction raw material and hydrogen are mixed and enter the hydrogenation pretreatment reaction zone, react on a bed layer equipped with a hydrogenation pretreatment catalyst, complete the hydrogenation saturation and hydrodeoxygenation of non-alkane components in the raw material, and obtain the hydrogenation pretreatment oil;
[0070] 2) the hydrotreated oil obtained in step 1) enters the hydroisomerization-cracking reaction zone, and undergoes a hydroisomerization reaction on a combined catalyst having a specific crystal size, thereby completing the hydroisomerization and hydrocracking reactions of the hydrotreated oil to obtain a hydroisomerized cracked oil;
[0071] 3) The hydroisomerized cracked oil obtained in step 2) enters the hydrotreating reaction zone, and further hydrogenation saturation of the hydroisomerized cracked oil is completed on the hydrotreating catalyst to obtain a crude product;
[0072] 4) The crude product obtained in step 3) enters an atmospheric pressure tower and / or a vacuum tower for fractionation to obtain gasoline, diesel, and lubricating oil base oil;
[0073] Example 1
[0074] The hydrogenation pretreatment reactor uses a hydrogenation pretreatment catalyst T1, which is 15wt% Ni-6wt% Mo-4wt% W-5wt% P / Al2O3. The reaction conditions are 220°C, 6MPa (hydrogen pressure, the same below), and a space velocity of 1.5h -1 (Volume space velocity of crude oil, the same below), hydrogen-to-oil ratio 700;
[0075] The hydroisomerization-cracking reactor uses hydroisomerization catalysts A and B. Catalyst A uses SAPO-11 molecular sieve as a carrier, the molecular sieve grain size is 120 nm, the total acid content is 650 μmol (Pyridine) / g, the external surface acid content is 230 μmol (2,6-Di-tert-butylpyridine) / g, and 0.5 wt% Pd is loaded on catalyst A, that is, 0.5 wt% Pd / SAPO-11; catalyst B uses ZSM-22 molecular sieve as a carrier, the molecular sieve grain size is 2.3 μm, the total acid content is 300 μmol (Pyridine) / g, the external surface acid content is 20 μmol (2,6-Di-tert-butylpyridine) / g, and 0.5 wt% Pt is loaded on catalyst B, that is, 0.5 wt% Pt / ZSM-22. The two were loaded in the following manner: A on top and B on the bottom, with a loading volume ratio of 1:1. During the reaction, the raw materials flowed from A to B. The reaction conditions were 336°C, 8 MPa (hydrogen pressure, the same below), and a space velocity of 0.7 h -1 (Volume space velocity of crude oil, the same below), hydrogen-to-oil ratio 600;
[0076] The hydrotreating reactor uses a hydrotreating catalyst T2, which is 0.25wt% Pt-1.5wt% Co / SiO2. The reaction conditions are 230°C, 8MPa (hydrogen pressure, the same below), and a space velocity of 1.5h -1(Volume space velocity of raw oil, the same below), hydrogen to oil ratio is 600. The product yields obtained after the raw materials are converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0077] Example 2
[0078] The hydrogenation pretreatment reactor uses a hydrogenation pretreatment catalyst T1, which is 14wt% Ni-7wt% Mo-4wt% W-4wt% P-1wt% B / Al2O3. The reaction conditions are 250°C, 5MPa, and a space velocity of 3.0h -1 , hydrogen-to-oil ratio is 800; the hydroisomerization-cracking reactor adopts hydroisomerization catalysts A and B, catalyst A adopts SAPO-11 molecular sieve as a carrier, the molecular sieve grain size is 100nm, the total acid amount is 600μmol (Pyridine) / g, the external surface acid amount is 260μmol (2,6-Di-tert-butylpyridine) / g, and 0.5wt% Pt is loaded on catalyst A, that is, 0.5wt% Pt / SAPO-11; catalyst B adopts ZSM-22 molecular sieve as a carrier, the molecular sieve grain size is 2.5μm, the total acid amount is 260μmol (Pyridine) / g, the external surface acid amount is 30μmol (2,6-Di-tert-butylpyridine) / g, and 0.5wt% Pd is loaded on catalyst B, that is, 0.5wt% Pd / ZSM-22. The two were loaded in the following manner: A on top and B on the bottom, with a loading volume ratio of 3:1. During the reaction, the raw materials flowed from A to B. The reaction conditions were 357°C, 10 MPa, and a space velocity of 0.8 h -1 , hydrogen-to-oil ratio 500; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 210℃, 10MPa, space velocity 1.0h -1 , hydrogen to oil ratio 800. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0079] Example 3
[0080] The hydrogenation pretreatment reactor uses a hydrogenation pretreatment catalyst T1, which is 16wt% Ni-4wt% Mo-5wt% W-5wt% B / Al2O3, and the reaction conditions are 260℃, 7MPa, and a space velocity of 3.0h -1, hydrogen-to-oil ratio 600; the hydroisomerization-cracking reactor uses hydroisomerization catalysts A and B, catalyst A uses SAPO-11 molecular sieve as a carrier, the molecular sieve particle size is 80nm, the total acid content is 580μmol (Pyridine) / g, the external surface acid content is 240μmol (2,6-Di-tert-butylpyridine) / g, and catalyst A is loaded with 0.4wt% Pt-0.1wt% Pd, that is, 0.4wt% Pt-0. 1wt% Pd / SAPO-11; Catalyst B uses ZSM-22 molecular sieve as carrier, the molecular sieve particle size is 3.5μm, the total acid content is 360μmol (Pyridine) / g, the external surface acid content is 40μmol (2,6-Di-tert-butylpyridine) / g, and the catalyst B is loaded with 0.25wt% Pd-0.25wt% Pt, that is, 0.25wt% Pd-0.25wt% Pt / ZSM-22. The two are loaded in A on top and B on the bottom, with a loading volume ratio of 1:3. During the reaction, the raw materials flow from A to B, and the reaction conditions are 325℃, 9MPa, and an air velocity of 1.0h -1 , hydrogen-to-oil ratio 700; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% Co / SiO2, the reaction conditions are 220℃, 9MPa, space velocity 1.2h -1 , hydrogen to oil ratio 700. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0081] Example 4
[0082] The hydrogenation pretreatment reactor uses a hydrogenation pretreatment catalyst T1, which is 13wt% Ni-5wt% Mo-7wt% W-5wt% N / Al2O3, and the reaction conditions are 270℃, 8MPa, and a space velocity of 3.0h -1, hydrogen-to-oil ratio of 500; the hydroisomerization-cracking reactor uses hydroisomerization catalysts A and B, catalyst A uses SAPO-11 molecular sieve as a carrier, the molecular sieve particle size is 60nm, the total acid content is 700μmol (Pyridine) / g, the external surface acid content is 280μmol (2,6-Di-tert-butylpyridine) / g, and catalyst A is loaded with 0.3wt% Pt-0.2wt% Pd, that is, 0.3wt% Pt- 0.2wt% Pd / SAPO-11; Catalyst B uses ZSM-22 molecular sieve as carrier, the molecular sieve particle size is 5.0μm, the total acid content is 380μmol (Pyridine) / g, the external surface acid content is 50μmol (2,6-Di-tert-butylpyridine) / g, and the catalyst B is loaded with 0.3wt% Pd-0.2wt% Pt, that is, 0.3wt% Pd-0.2wt% Pt / ZSM-22. The two are loaded in A on top and B on the bottom, with a loading volume ratio of 1:5. During the reaction, the raw materials flow from A to B, and the reaction conditions are 320℃, 6MPa, and an air velocity of 0.9h -1 , hydrogen-to-oil ratio 550; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 260℃, 12MPa, space velocity 2.5h -1 , hydrogen to oil ratio 500. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0083] Comparative Example 1
[0084] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 15wt% Ni-6wt% Mo-4wt% W-5wt% P / Al2O3. The reaction conditions are 220°C, 6MPa, and a space velocity of 1.5h -1 , hydrogen-to-oil ratio 700; the hydroisomerization-cracking reactor uses hydroisomerization catalyst A, catalyst A uses SAPO-11 molecular sieve as a carrier, the molecular sieve particle size is 120nm, the total acid content is 650μmol (Pyridine) / g, the external surface acid content is 230μmol (2,6-Di-tert-butylpyridine) / g, and 0.5wt% Pd is loaded on catalyst A, that is, 0.5wt% Pd / SAPO-11; the reaction conditions are 356℃, 8MPa, and the space velocity is 0.7h -1 , hydrogen-to-oil ratio 600; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% Co / SiO2, the reaction conditions are 230℃, 8MPa, space velocity 1.5h -1, hydrogen to oil ratio 600. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0085] Comparative Example 2
[0086] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 14wt% Ni-7wt% Mo-4wt% W-4wt% P-1wt% B / Al2O3. The reaction conditions are 250°C, 5MPa, and a space velocity of 3.0h -1 , hydrogen-to-oil ratio is 800; the hydroisomerization-cracking reactor uses hydroisomerization catalysts B and A, catalyst A uses SAPO-11 molecular sieve as a carrier, the molecular sieve grain size is 100nm, the total acid content is 600μmol (Pyridine) / g, the external surface acid content is 260μmol (2,6-Di-tert-butylpyridine) / g, and 0.5wt% Pt is loaded on catalyst A, that is, 0.5wt% Pt / SAPO-11; catalyst B uses ZSM-22 molecular sieve as a carrier, the molecular sieve grain size is 2.5μm, the total acid content is 260μmol (Pyridine) / g, the external surface acid content is 30μmol (2,6-Di-tert-butylpyridine) / g, and 0.5wt% Pd is loaded on catalyst B, that is, 0.5wt% Pd / ZSM-22. The two were loaded in the manner of B on top and A on the bottom, with a loading volume ratio of 3:1. During the reaction, the raw materials flowed from B to A. The reaction conditions were 357°C, 10 MPa, and a space velocity of 0.8 h -1 , hydrogen-to-oil ratio 500; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 210℃, 10MPa, space velocity 1.0h -1 , hydrogen to oil ratio 800. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0087] Comparative Example 3
[0088] A process similar to that of this embodiment is used. The hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 16wt% Ni-4wt% Mo-5wt% W-5wt% B / Al2O3. The reaction conditions are 260°C, 7MPa, and a space velocity of 3.5h -1, hydrogen-to-oil ratio is 600; the hydroisomerization-cracking reactor uses hydroisomerization catalysts D and C, the carrier used by catalyst D is SAPO-11 molecular sieve, the molecular sieve grain size is 600nm, the total acid content is 850μmol (Pyridine) / g, the external surface acid content is 330μmol (2,6-Di-tert-butylpyridine) / g, and the D catalyst is loaded with 0.5wt% Pd, that is, 0.5wt% Pd / SAPO-11-D; the carrier used by catalyst C is ZSM-22 molecular sieve, the molecular sieve grain size is 100nm, the total acid content is 500μmol (Pyridine) / g, the external surface acid content is 200μmol (2,6-Di-tert-butylpyridine) / g, and the catalyst C is loaded with 0.5wt% Pt, that is, 0.5wt% Pt / ZSM-22-C. The two were filled in a D-up and C-down manner, with a filling volume ratio of 1:3. During the reaction, the raw materials flowed from D to C. The reaction conditions were 325°C, 9MPa, and a space velocity of 1.0h -1 , hydrogen-to-oil ratio 700; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% Co / SiO2, the reaction conditions are 220℃, 9MPa, space velocity 1.2h -1 , hydrogen to oil ratio 700. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0089] Comparative Example 4
[0090] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 13wt% Ni-5wt% Mo-7wt% W-5wt% N / Al2O3. The reaction conditions are 270°C, 8MPa, and a space velocity of 4.0h -1, hydrogen-to-oil ratio of 500; the hydroisomerization-cracking reactor uses hydroisomerization catalysts D and E, the carrier used by catalyst D is SAPO-11 molecular sieve, the molecular sieve grain size is 600nm, the total acid content is 850μmol (Pyridine) / g, the external surface acid content is 330μmol (2,6-Di-tert-butylpyridine) / g, and the D catalyst is loaded with 0.5wt% Pd, that is, 0.5wt% Pd / SAPO-11-D; the carrier used by catalyst E is ZSM-22 molecular sieve, the molecular sieve grain size is 600nm, the total acid content is 700μmol (Pyridine) / g, the external surface acid content is 240μmol (2,6-Di-tert-butylpyridine) / g, and the catalyst E is loaded with 0.5wt% Pt, that is, 0.5wt% Pt / ZSM-22-E. The loading method of the two is D on top and E on the bottom, with a loading volume ratio of 1:5. During the reaction, the raw materials flow from D to E. The reaction conditions are 320℃, 6MPa, and a space velocity of 0.9h -1 , hydrogen-to-oil ratio 550; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 260℃, 12MPa, space velocity 2.5h -1 , hydrogen to oil ratio 500. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0091] Comparative Example 5
[0092] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 13wt% Ni-5wt% Mo-7wt% W-5wt% N / Al2O3. The reaction conditions are 270°C, 8MPa, and a space velocity of 4.0h -1, hydrogen-to-oil ratio of 500; the hydroisomerization-cracking reactor uses hydroisomerization catalysts F and G, catalyst F uses a molecular sieve carrier with an ATO structure, which is CoAPO-31 (the heteroatom Co content is 1.5wt%), the molecular sieve grain size is 100nm, the total acid content is 420μmol (Pyridine) / g, the external surface acid content is 180μmol (2,6-Di-tert-butylpyridine) / g, and the total content of loaded metal is 0.4wt% Pt; catalyst G uses a molecular sieve carrier with a FER structure, which is Fe-ZSM-35 (the heteroatom Fe content is 2.0wt%), the molecular sieve grain size is 2.0μm, the total acid content is 280μmol (Pyridine) / g, the external surface acid content is 50μmol (2,6-Di-tert-butylpyridine) / g, and the content of loaded metal is 0.4wt% Pd. The two were filled in the manner of F on top and G on the bottom, with a filling volume ratio of 1:5. During the reaction, the raw materials flowed from F to G. The reaction conditions were 320°C, 6MPa, and a space velocity of 0.9h -1 , hydrogen-to-oil ratio 550; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 260℃, 12MPa, space velocity 2.5h -1 , hydrogen to oil ratio 500. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0093] Comparative Example 6
[0094] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 13wt% Ni-5wt% Mo-7wt% W-5wt% N / Al2O3. The reaction conditions are 270°C, 8MPa, and a space velocity of 4.0h -1, hydrogen-to-oil ratio of 500; the hydroisomerization-cracking reactor uses hydroisomerization catalysts H and I, catalyst H uses a heteroatom aluminum phosphate molecular sieve carrier with an AEL structure, which is ZnAPO-11 (the heteroatom Zn content is 1.0wt%), the molecular sieve has a grain size of 80nm, a total acid amount of 500μmol (Pyridine) / g, an external surface acid amount of 150μmol (2,6-Di-tert-butylpyridine) / g, and a metal loading of 0.5wt% Pt; catalyst I uses a heteroatom aluminum silicate molecular sieve carrier with an MTT structure, which is Ni-ZSM-23 (the heteroatom Ni content is 1.5wt%), the molecular sieve has a grain size of 1μm, a total acid amount of 300μmol (Pyridine) / g, an external surface acid amount of 60μmol (2,6-Di-tert-butylpyridine) / g, and a metal loading of 0.4wt% Pd. The two were loaded in a H-up and I-down manner, with a loading volume ratio of 1:5. During the reaction, the raw materials flowed from H to I. The reaction conditions were 320°C, 6MPa, and a space velocity of 0.9h -1 , hydrogen-to-oil ratio 550; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 260℃, 12MPa, space velocity 2.5h -1 , hydrogen to oil ratio 500. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0095] Comparative Example 7
[0096] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 13wt% Ni-5wt% Mo-7wt% W-5wt% N / Al2O3. The reaction conditions are 270°C, 8MPa, and a space velocity of 4.0h -1, hydrogen-to-oil ratio of 500; the hydroisomerization-cracking reactor uses hydroisomerization catalysts J and K. Catalyst J uses a molecular sieve carrier with an AFI structure, which is SAPO-5. The molecular sieve has a grain size of 50nm, a total acid content of 780μmol (Pyridine) / g, an external surface acid content of 280μmol (2,6-Di-tert-butylpyridine) / g, and a precious metal content of 0.4wt% Pd; Catalyst K uses a molecular sieve carrier with an *MRE structure, which is ZSM-48. The molecular sieve has a grain size of 4.5μm, a total acid content of 560μmol (Pyridine) / g, an external surface acid content of 80μmol (2,6-Di-tert-butylpyridine) / g, and a precious metal content of 0.3wt% Pt. The loading method of the two is J on top and K on the bottom, with a loading volume ratio of 1:5. During the reaction, the raw materials flow from J to K. The reaction conditions are 320℃, 6MPa, and space velocity 0.9h -1 , hydrogen-to-oil ratio 550; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 260℃, 12MPa, space velocity 2.5h -1 , hydrogen to oil ratio 500. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0097] Comparative Example 8
[0098] A process similar to that of this embodiment is used. A hydrogenation pretreatment catalyst T1 is used in the hydrogenation pretreatment reactor. The catalyst T1 is 13wt% Ni-5wt% Mo-7wt% W-5wt% N / Al2O3. The reaction conditions are 270°C, 8MPa, and a space velocity of 4.0h -1 , hydrogen-to-oil ratio of 500; the hydroisomerization-cracking reactor uses hydroisomerization catalysts L and M. Catalyst L uses a molecular sieve carrier with an AFO structure, which is SAPO-41. The molecular sieve has a particle size of 350nm, a total acid content of 600μmol (Pyridine) / g, an external surface acid content of 260μmol (2,6-Di-tert-butylpyridine) / g, and a metal loading of 0.5wt% Pt; Catalyst M uses a molecular sieve carrier with an MTW structure, which is ZSM-12. The molecular sieve has a particle size of 4.5μm, a total acid content of 450μmol (Pyridine) / g, an external surface acid content of 120μmol (2,6-Di-tert-butylpyridine) / g, and a metal loading of 0.5wt% Pd. The loading method of the two is L on top and M on the bottom, with a loading volume ratio of 1:5. During the reaction, the raw materials flow from L to M. The reaction conditions are 320℃, 6MPa, and space velocity 0.9h -1, hydrogen-to-oil ratio 550; the hydrotreating reactor uses hydrotreating catalyst T2, catalyst T2 is 0.25wt% Pt-1.5wt% W / SiO2, the reaction conditions are 260℃, 12MPa, space velocity 2.5h -1 , hydrogen to oil ratio 500. The product yields obtained after the raw materials were converted and fractionated through the reaction process are shown in Table 2, and the properties of the base oil products are shown in Table 3.
[0099] As shown in Table 2, compared with the comparative example, the base oil yield is significantly improved by the method of the present invention, the yield of light hydrocarbons and diesel with lower value byproducts is significantly reduced, and the heavy wax remaining in the product is less, and the wide-range Fischer-Tropsch wax component is completely and efficiently converted. At the same time, as shown in Table 3, compared with the comparative example, the base oil obtained by the method of the present invention has a higher viscosity index and a lower pour point.
[0100] Table 1 Properties of wide range Fischer-Tropsch wax feedstock oil
[0101]
[0102]
[0103] Table 2 Product yield
[0104]
[0105] Table 3 Base oil product properties
[0106]
Claims
1. A method for hydrogenating and converting wide-range Fischer-Tropsch wax, characterized in that: It includes the following steps: 1) The wide distillation range fraction of Fischer-Tropsch wax is mixed with hydrogen and enters the hydrogenation pretreatment reaction zone. On the bed containing the hydrogenation pretreatment catalyst, the temperature is 150-450°C, the hydrogen partial pressure is 3-18MPa, and the raw oil volume space velocity is 0.3-5h -1 , under the condition of hydrogen-to-oil ratio of 200:1-2000:1, the non-alkane components in the feedstock are hydrogenated and saturated and hydrodeoxygenated to obtain hydrogenation pretreated oil; 2) The hydrotreated oil obtained in step 1) enters the hydroisomerization-cracking reaction zone. On a combined catalyst with a specific crystal size, the reaction temperature is 250-400°C, the hydrogen partial pressure is 2-20 MPa, and the feed oil volume space velocity is 0.3-5 h -1 , under the condition of hydrogen-oil ratio of 200:1-2000:1, carrying out hydroisomerization reaction to complete the hydroisomerization and hydrocracking reaction of the hydrotreatment pretreated oil to obtain hydroisomerization cracked oil; 3) The hydroisomerized cracked oil obtained in step 2) enters the hydrotreating reaction zone. On the hydrotreating catalyst, the reaction temperature is 180-320°C, the hydrogen partial pressure is 2-20 MPa, and the raw oil volume space velocity is 0.3-5 h -1 , under the condition of hydrogen-oil ratio of 200:1-2000:1, further hydrogenation saturation of hydroisomerized cracking oil is completed to obtain a crude product; 4) The crude product obtained in step 3) enters an atmospheric pressure tower and / or a vacuum tower for fractionation to obtain gasoline, diesel, and lubricating oil base oil; The combined catalyst with a specific crystal size in step 2) is composed of a catalyst A prepared by using a molecular sieve with a crystal size of 10 nm to 500 nm and an AEL structure as a carrier and loading one or more of the active metals platinum, palladium or iridium, and a catalyst B prepared by using a molecular sieve with a crystal size of 500 nm to 10 μm and a TON structure as a carrier and loading one or more of the active metals platinum, palladium or iridium; The molecular sieve with AEL structure is one or two of SAPO-11 and MeAPO-11, wherein Me = one or more of Zn, Mg, Mn, Co, Cr, Cu, Cd or Ni, and the mass content of Me is 0.5-1.5wt%; the molecular sieve with TON structure is one or more of ZSM-22, Me-ZSM-22, Theta-1, KZ-2, ISI-1 and NU-10, wherein Me in Me-ZSM-22 = one or more of Zn, Mg, Mn, Co, Cr, Cu, Fe, Cd or Ni, and the mass content of Me is 0.2-2.0wt%; The mass content of active metals loaded in catalyst A is 0.3-0.6wt%, and the mass content of active metals loaded in catalyst B is 0.4-0.7wt%; In the combined catalyst with a specific crystal size, the total acid amount of the AEL structure molecular sieve carrier used in catalyst A is 200-800 μmol pyridine / g, and the external surface acid amount is 100-300 μmol 2,6-di-tert-butylpyridine / g; the total acid amount of the TON structure molecular sieve carrier used in catalyst B is 100-600 μmol pyridine / g, and the external surface acid amount is 0-100 μmol 2,6-di-tert-butylpyridine / g; The Fischer-Tropsch wax wide distillation range fraction raw material refers to a Fischer-Tropsch wax fraction with an initial distillation point of not higher than 240°C and not lower than 180°C, a final distillation point of not lower than 700°C and not higher than 730°C, and the normal alkane content in the Fischer-Tropsch wax fraction is not lower than 90wt%.
2. The method according to claim 1, characterized in that In the combined catalyst with a specific grain size, the grain size of the AEL structure molecular sieve carrier used in catalyst A is 20nm~200nm; the grain size of the TON structure molecular sieve carrier used in catalyst B is 800nm~5μm.
3. The method according to claim 1, characterized in that: In the step 2), the combination of catalysts A and B is A on top and B on the bottom. When used for hydroisomerization-cracking reaction, the raw materials flow through A and B in sequence, and the volume ratio of catalysts A and B is 1:10-10:
1.
4. The method according to claim 3, characterized in that The volume ratio of catalyst A and catalyst B is 1:6-6:
1.
5. The method according to claim 1, characterized in that The reaction conditions of the hydrogenation pretreatment in step 1) are: temperature 180-320°C, hydrogen partial pressure 5-12MPa, raw oil volume space velocity 0.5-3h -1 , hydrogen-to-oil ratio is 200:1-1600:1; The hydrogenation pretreatment catalyst is composed of one or more of the active metals cobalt, nickel, molybdenum and tungsten supported by alumina and / or silicon oxide, and one or more non-metallic additives selected from nitrogen, phosphorus, sulfur or boron. The mass content of the active metal in the catalyst is 10-28wt%, and the mass content of the additive is 2-8wt%.
6. The method according to claim 1, characterized in that The conditions for the hydroisomerization reaction in step 2) are: temperature of 250-400°C, hydrogen partial pressure of 2-15 MPa, and feed oil volume space velocity of 0.5-3 h -1 , the hydrogen-to-oil ratio is 200:1-1600:
1.
7. The method according to claim 1, characterized in that The conditions for the hydrofining reaction in step 3) are: temperature 180-320°C, hydrogen partial pressure 2-15MPa, and feed oil volume space velocity 0.5-3h -1 , hydrogen-to-oil ratio is 200:1-1600:1; The hydrotreating catalyst is composed of one or more active metals selected from platinum, palladium and iridium supported on alumina and / or silicon oxide, and one or more additives selected from cobalt, nickel, molybdenum and tungsten. The mass content of the active metal in the catalyst is 0.2-0.5wt%, and the mass content of the additive is 0.5-3wt%.
8. The method according to claim 1, characterized in that The crude product obtained in step 3) is sequentially distilled into normal and vacuum towers to obtain gasoline, diesel and lubricating oil base oil products.
Citation Information
Patent Citations
Hydroisomerization treatment process for feeds from the fisher-tropsch process
US5834522A
Conversion of fisher-tropsch waxes to lubricants by countercurrent processing
US5882505A
Isomerization / dehazing process for base oils from Fischer-Tropsch wax
US7198710B2
Lubricating oil base oil prepared by hydrogenation of Fischer-Tropsch synthetic wax and preparation method thereof
CN112126464A