A crude oil nucleophilic deconstruction aid and its preparation method and application
By using crude oil nucleophilic deconstruction additives composed of metal detergents, polymer ashless dispersants, etc. in the crude oil pretreatment process, the problem of low electrodesalting efficiency of crude oil is solved, and the effective removal of moisture and salt in crude oil is achieved, which improves the improvement of Process stability and product quality.
Patent Information
- Application Number
- CN202310259183.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-17
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2043-03-17
AI Technical Summary
The low electrodesalting efficiency in the crude oil pretreatment process leads to high moisture and salt content in the crude oil, affecting the long-term stable operation of the production process and product quality.
The crude oil nucleophilic deconstruction additive consisting of metal detergent, polymer ashless dispersant, polyol ethylene-propylene copolymer and fatty alcohol ethylene-propylene copolymer is used to decompose the rubber groups in crude oil through its good solubility and dispersion properties. , improve the removal rate of salt and water.
The efficiency of the crude oil electrodesalting process is significantly improved, the moisture and salt content in the crude oil is reduced, and the quality of crude oil after pretreatment and the long-term stable operation of the subsequent processing process is ensured.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of additives in a petroleum refining process, and in particular to a crude oil nucleophilic deconstruction auxiliary agent and a preparation method and application thereof. Background Art
[0002] With the deterioration of the quality of crude oil processed by domestic refineries, the content of high molecular weight and high boiling point colloids, asphaltene, water, salt, mechanical impurities, etc. in crude oil has increased significantly, and the asphaltene content is as high as 15% or more. Salt, water, mechanical impurities, etc. will form lumps in the process of electrical desalting of crude oil, which greatly reduces the efficiency of electrical desalting in the crude oil pretreatment process. The salt content of crude oil after desalting is high, the oil content of drainage is large and difficult to handle, and the amount of sludge generated in the electrical desalting tank is large, and backwashing is difficult, which affects the long-term stable operation of the production process and product quality to a certain extent, and has an extremely adverse effect on the pretreatment process (electrical desalting process) of crude oil and subsequent processing technology. In view of this situation, the existing solution is to improve the electrical desalting equipment and optimize the process parameters, but it is difficult to solve the problem fundamentally. The water content and salt content in the treated crude oil are still high and fail to meet the standards.
[0003] Patent document 202110032526.8 discloses a lubricating oil composition, in which a metal detergent and an ashless dispersant are added to a mineral oil lubricating oil. The metal detergent is at least one of calcium alkyl salicylate and magnesium alkyl salicylate, and at least one of calcium alkylbenzene sulfonate, magnesium alkylbenzene sulfonate, calcium petroleum sulfonate, and magnesium petroleum sulfonate, with a content of 1.5 to 3.0. The ashless dispersant is at least one of polymer succinimide, polyisobutylene monosuccinimide, and polyisobutylene bissuccinimide, with a content of 3.0 to 5.0%. Patent document 202111475767.6 also discloses a lubricating oil composition, which also contains a metal detergent and an ashless dispersant. In addition to the molecular structure and performance indicators being different from the above patents, the lubricating oil base oil used is not a mineral oil type, but a synthetic fatty acid polyol ester and / or fatty alcohol polyester. The calcium-based detergents in terms of calcium element are calcium alkyl sulfonates and calcium alkylbenzene sulfonates with a content of no more than 3000ppm, and the boron-modified dispersants in terms of boron element are succinimide-based dispersants with a content of no more than 1000ppm. The above patents only disclose two lubricating oil compositions, namely, the composition after adding detergents and dispersants and other additives to mineral oil base oil and synthetic ester base oil, respectively, and the main properties of lubricating oil, etc., and do not involve the application of the corresponding additives in the pretreatment process of oil refining or other occasions, and the two do not belong to the same field and direction. Patent document 201110381854.5 A method for preparing a high-value-loss lubricating oil metal detergent dispersant discloses a specific preparation method of detergent dispersants such as high-alkalinity petroleum sulfonates, alkyl sulfonates, alkylbenzene sulfonates, etc. as lubricating oil additives, and also does not involve detergent dispersants that can be used in oil refining processes, especially in the electro-desalting process of crude oil pretreatment or other scenarios.
[0004] Therefore, it is of great significance to provide a new crude oil additive, in which the above-mentioned metal detergent and ash-free dispersant are applied, so as to solve the technical problems in the crude oil pretreatment electrical desalting process. Summary of the invention
[0005] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a crude oil nucleophilic deconstruction aid, which has good solubility and dispersibility for micelles formed by colloids, asphaltene, water, water-soluble salts, organic chlorine, mechanical impurities, etc. in crude oil, and has good removal performance for chloride ions in crude oil, providing support for the long-term stable operation of the crude oil desalting and dehydration pretreatment process and subsequent processing technology.
[0006] In order to achieve the above object, the present invention adopts the following technical solution:
[0007] In a first aspect, the present invention provides a crude oil nucleophilic deconstruction aid, which consists of component A and component B; wherein component A consists of a metal detergent, a polymer ashless dispersant, a polyol ethylene-propylene copolymer, and a fatty alcohol ethylene-propylene copolymer; and component B is a solvent.
[0008] As a further preferred embodiment of the technical solution of the present invention, the metal detergent is a highly basic petroleum sulfonate or an alkyl salicylate; further preferably, the highly basic petroleum sulfonate or the highly basic alkyl salicylate has a base value in the range of 150 to 400 mgKOH / g; further preferably, the petroleum sulfonate is one or more of barium petroleum sulfonate, calcium petroleum sulfonate, and magnesium petroleum sulfonate; and the alkyl salicylate is one or more of calcium alkyl salicylate, barium alkyl salicylate, and magnesium alkyl salicylate.
[0009] As a further preferred embodiment of the technical solution of the present invention, the polymer ashless dispersant is polyisobutylene succinimide; further preferred, the polymer ashless dispersant is one or more of polyisobutylene monosuccinimide, polyisobutylene bissuccinimide, and polyisobutylene polysuccinimide; further preferred, the molecular weight of polyisobutylene is 500 to 5000, preferably 1200 to 5000.
[0010] As a further preferred embodiment of the technical solution of the present invention, the ethylene-propylene copolymer in the polyol ethylene-propylene copolymer and the fatty alcohol ethylene-propylene copolymer is an ethylene oxide propylene oxide copolymer; and the polymerization method is random or block copolymerization.
[0011] As a further preferred embodiment of the technical solution of the present invention, the polyol is one or more of 2,3-propylene glycol, glycerol, pentaerythritol, trimethylolpropane and sorbitan.
[0012] As a further preferred embodiment of the technical solution of the present invention, the fatty alcohol is a monohydric fatty alcohol, preferably, the carbon number of the fatty alcohol is C2 to C 30 More preferably, the carbon number of the fatty alcohol is C4 to C 18 .
[0013] As a further preferred embodiment of the technical solution of the present invention, in terms of mass percentage, the content of the metal detergent in component A is 10% to 80%; the content of the polymer ashless dispersant is 10% to 60%; the content of the polyol ethylene-propylene copolymer is 5% to 50%; and the content of the fatty alcohol ethylene-propylene copolymer is 5% to 30%.
[0014] More preferably, in terms of mass percentage, the content of metal detergent in component A is 40% to 60%; the content of polymer ashless dispersant is 15% to 40%; the content of polyol ethylene-propylene copolymer is 10% to 30%; and the content of fatty alcohol ethylene-propylene copolymer is 10% to 20%.
[0015] In the above technical scheme, the metal detergent has the properties of cleaning, solubilization and dispersion, which is beneficial to the separation of salts and organic matter; the high molecular ashless dispersant is polyisobutylene succinimide, which has good dispersing and solubilizing properties for the micelles formed by colloids, asphaltene and other components in heavy oil, making it easier for the salts wrapped in the colloids and asphaltene to migrate to the outside; the functions of the polyol ethylene-propylene copolymer and the fatty alcohol ethylene-propylene copolymer are dispersion, solubilization and demulsification, making it easier for the oil and water to separate, reducing the water content in the oil and thus increasing the salt removal rate.
[0016] As a further preferred embodiment of the technical solution of the present invention, the solvent of component B is one or more of toluene, xylene, straight-run kerosene, straight-run diesel, solvent oil, commercial kerosene, and commercial diesel.
[0017] As a further preferred embodiment of the technical solution of the present invention, the mass ratio of component A to component B is 90:10 to 30:70; further preferably, the mass ratio of component A to component B is 70:30 to 50:50.
[0018] In a second aspect, the present invention also provides a method for preparing the above-mentioned crude oil nucleophilic deconstruction auxiliary agent, comprising the following steps:
[0019] (1) synthesizing polyol ethylene oxide propylene oxide copolyether and fatty alcohol ethylene oxide propylene oxide copolyether by using polyol, fatty alcohol, ethylene oxide and propylene oxide;
[0020] (2) adding a metal detergent, a polymer ashless dispersant, and the polyol ethylene oxide propylene oxide copolyether and fatty alcohol ethylene oxide propylene oxide copolyether obtained in step (1) into a solvent, and stirring evenly to obtain the crude oil nucleophilic deconstruction aid.
[0021] It can be understood that in the above technical scheme, in step (1), the polyol ethylene oxide propylene oxide copolyether is synthesized using polyol, ethylene oxide and propylene oxide; the fatty alcohol ethylene oxide propylene oxide copolyether is synthesized using fatty alcohol, ethylene oxide and propylene oxide; and the polymerization method is random or block copolymerization.
[0022] As a further preferred embodiment of the technical solution of the present invention, the synthesis conditions of polyol ethylene oxide propylene oxide copolyether are as follows: the molar mass ratio of polyol, ethylene oxide and propylene oxide is 1: (3-8): (4-9), the reaction temperature is 130-155°C, the reaction pressure is 0.3-0.55 MPa, the molar mass ratio of polyol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1: (3-7): (4-8), the molecular weight of the polymer is 4000-8000, and the reaction is terminated.
[0023] As a further preferred embodiment of the technical solution of the present invention, the synthesis conditions of fatty alcohol ethylene oxide propylene oxide copolyether are as follows: the molar mass ratio of fatty alcohol, ethylene oxide and propylene oxide is 1: (3-8): (4-9), the reaction temperature is 130-155° C., the reaction pressure is 0.3-0.55 MPa, the molar mass ratio of fatty alcohol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1: (3-7): (4-8), the molecular weight of the polymer is 4000-8000, and the reaction is terminated.
[0024] In a third aspect, the present invention claims protection for the use of the above-mentioned crude oil nucleophilic deconstruction aid in the electrical desalting process of crude oil pretreatment.
[0025] As a preferred technical solution of the present invention, in specific application, the concentration of the crude oil nucleophilic deconstruction aid in the crude oil is 1 to 100 ppm; more preferably, the concentration of the crude oil nucleophilic deconstruction aid in the crude oil is 5 to 30 ppm.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] 1. Nucleophilic additives are substances that can provide anions, or atoms or groups with lone electron pairs. The applicant has found that they have good solubility and dispersibility for micelles formed by colloids, asphaltene, water, water-soluble salts, organic chlorine, mechanical impurities, etc. in crude oil, and have good removal performance for chloride ions in crude oil, providing support for the long-term stable operation of crude oil desalting and dehydration pretreatment processes and subsequent processing processes; therefore, by adding nucleophilic deconstruction additives to the crude oil pretreatment process, the content of water, water-soluble salts, organic chlorine, mechanical impurities, etc. in the crude oil can meet the requirements of atmospheric pressure reduction and other post-processing processes after being treated by the crude oil electric desalting process.
[0028] 2. The crude oil nucleophilic deconstruction aid of the present invention is composed of a high alkalinity detergent, a polymer ashless dispersant, a polyol ethylene-propylene copolymer and a fatty alcohol ethylene-propylene copolymer dispersant, etc., so as to effectively prevent or reduce the tendency of colloids, asphaltene and other components in the crude oil, as well as water, inorganic salts, mechanical impurities and the like contained in the crude oil to condense and nucleate; or the micelles or other impurities formed in the crude oil can be dispersed and dissolved in the crude oil through the effects of cleaning, dispersing, solubilizing, and increasing flow, thereby improving the quality and processability of the crude oil after pretreatment, ensuring the long-term stable operation of the device at full load, and improving the quality of related products.
[0029] 3. The various components of the present invention are not simply superimposed and combined, but are scientifically and rigorously configured, and the various components work synergistically; the metal detergent has the properties of cleaning, solubilization and dispersion, which is beneficial to the separation of salts and organic matter; the high molecular ashless dispersant is polyisobutylene succinimide, which has good dispersing and solubilizing properties for the micelles formed by colloids, asphaltene and other components in heavy oil, making it easier for the salts wrapped in the colloids and asphaltene to migrate to the outside; the functions of the polyol ethylene-propylene copolymer and the fatty alcohol ethylene-propylene copolymer are dispersion, solubilization and demulsification, making it easier for the oil and water to separate, reducing the water content in the oil and thus increasing the salt removal rate.
[0030] 4. The present invention creatively combines metal detergents and ash-free dispersants with polyol ethylene-propylene copolymers and fatty alcohol ethylene-propylene copolymers, and applies them to the electrical desalting process of crude oil pretreatment and achieves good technical effects. The method provided by the present invention is simple and easy to implement, economical and practical, and can be widely promoted and applied to the electrical desalting process of crude oil. DETAILED DESCRIPTION
[0031] In order to make the purpose, technical solution and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with the embodiments. Of course, the specific embodiments described here are only used to explain the present invention and are not used to limit the present invention.
[0032] Although the steps in the present invention are arranged with numbers, they are not used to limit the order of the steps. Unless the order of the steps is clearly stated or the execution of a certain step requires other steps as a basis, the relative order of the steps can be adjusted. It is understood that the term "and / or" used in this article involves and covers any and all possible combinations of one or more of the associated listed items.
[0033] It should be noted that, for those embodiments in which specific conditions are not specified, conventional conditions or conditions recommended by the manufacturer are used; for those reagents or instruments used without indicating the manufacturer, they are all conventional products that can be purchased commercially; at the same time, it should be emphasized that the electrical desalting performance of crude oil can be measured using conventional analytical instruments and experimental equipment, which is an existing mature process mastered by those skilled in the art, and the present invention does not make a detailed description of the process.
[0034] Example 1
[0035] A crude oil nucleophilic deconstruction aid is composed of 60% of component A and 40% of component B by mass percentage; component A is composed of 30% of high-basic calcium petroleum sulfonate, 50% of polyisobutylene monosuccinimide, 10% of propylene oxide copolyether of glycerol ethylene oxide and 10% of lauryl alcohol ethylene oxide and propylene oxide copolyether; component B is a xylene solvent.
[0036] This embodiment also provides a method for preparing the crude oil nucleophilic deconstruction auxiliary agent, comprising the following steps:
[0037] (1) synthesizing glycerol ethylene oxide propylene oxide copolyether by using glycerol, ethylene oxide and propylene oxide; wherein the molar mass ratio of glycerol, ethylene oxide and propylene oxide is 1:6:7, the reaction temperature is 135° C., the reaction pressure is 0.45 MPa, the molar mass ratio of glycerol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1:5:6, the molecular weight of the polymer is 6000-8000, and the reaction is terminated;
[0038] (2) synthesizing lauryl alcohol, ethylene oxide and propylene oxide copolyether by using lauryl alcohol, ethylene oxide and propylene oxide; wherein the molar mass ratio of lauryl alcohol, ethylene oxide and propylene oxide is 1:6:7, the reaction temperature is 135°C, the reaction pressure is 0.45 MPa, the molar mass ratio of lauryl alcohol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1:5:6, the molecular weight of the polymer is 6000-8000, and the reaction is completed;
[0039] (3) In a synthesis kettle, first add a measured amount of xylene solvent, then add high alkalinity petroleum calcium sulfonate, polyisobutylene monosuccinimide, and the synthesized propylene oxide copolyether and lauryl alcohol ethylene oxide copolyether in sequence at a temperature of 25° C., and stir for 60 minutes to obtain the crude oil nucleophilic deconstruction aid.
[0040] Example 2
[0041] A crude oil nucleophilic deconstruction aid, which consists of 50% component A and 50% component B by mass percentage; wherein component A consists of 20% calcium alkyl salicylate, 50% polyisobutylene polysuccinimide, 15% pentaerythritol ethylene oxide propylene oxide copolyether and 15% octadecyl alcohol ethylene oxide propylene oxide copolyether; component B is a toluene solvent.
[0042] This embodiment also provides a method for preparing the crude oil nucleophilic deconstruction auxiliary agent, comprising the following steps:
[0043] (1) using pentaerythritol, ethylene oxide and propylene oxide to synthesize pentaerythritol ethylene oxide propylene oxide copolyether; wherein the molar mass ratio of pentaerythritol, ethylene oxide and propylene oxide is 1:6:7, the reaction temperature is 135°C, the reaction pressure is 0.45 MPa, the molar mass ratio of pentaerythritol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1:5:6, the molecular weight of the polymer is 6000-8000, and the reaction is terminated;
[0044] (2) using octadecyl alcohol, ethylene oxide and propylene oxide to synthesize octadecyl alcohol ethylene oxide propylene oxide copolyether; wherein the molar mass ratio of octadecyl alcohol, ethylene oxide and propylene oxide is 1:6:7, the reaction temperature is 135° C., the reaction pressure is 0.45 MPa, the molar mass ratio of octadecyl alcohol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1:5:6, the molecular weight of the polymer is 6000-8000, and the reaction is completed;
[0045] (3) In a synthesis kettle, first add a measured amount of toluene solvent, then add alkyl salicylate calcium, polyisobutylene polysuccinimide, and the synthesized pentaerythritol ethylene oxide propylene oxide copolyether and octadecyl alcohol ethylene oxide propylene oxide copolyether in sequence at a temperature of 25° C., and stir for 60 minutes to obtain the crude oil nucleophilic deconstruction aid.
[0046] Example 3
[0047] A crude oil nucleophilic deconstruction auxiliary agent is composed of 40% component A and 60% component B by mass percentage; component A is composed of 10% of a mixture of highly basic petroleum calcium sulfonate and alkyl calcium salicylate (petroleum calcium sulfonate and alkyl calcium salicylate each account for 50%), 50% of polyisobutylene bissuccinimide, 30% of trimethylolpropane ethylene oxide propylene oxide copolyether and 10% of octanol ethylene oxide propylene oxide copolyether; component B is solvent oil.
[0048] This embodiment also provides a method for preparing the crude oil nucleophilic deconstruction auxiliary agent, comprising the following steps:
[0049] (1) synthesizing trimethylolpropane, ethylene oxide and propylene oxide trimethylolpropane ethylene oxide propylene oxide copolyether by using trimethylolpropane, ethylene oxide and propylene oxide; wherein the molar mass ratio of trimethylolpropane, ethylene oxide and propylene oxide is 1:6:7, the reaction temperature is 135° C., the reaction pressure is 0.45 MPa, the molar mass ratio of trimethylolpropane, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1:5:6, the molecular weight of the polymer is 6000-8000, and the reaction is terminated;
[0050] (2) synthesizing octanol, ethylene oxide and propylene oxide copolyether by using octanol, ethylene oxide and propylene oxide; wherein the molar mass ratio of octanol, ethylene oxide and propylene oxide is 1:6:7, the reaction temperature is 135° C., the reaction pressure is 0.45 MPa, the molar mass ratio of octanol, ethylene oxide and propylene oxide monomers in the polymer after the reaction is controlled to be 1:5:6, the molecular weight of the polymer is 6000-8000, and the reaction is terminated;
[0051] (3) In a synthesis reactor, first add a measured amount of solvent oil solvent, then add a mixture of high-alkalinity petroleum calcium sulfonate and alkyl calcium salicylate, polyisobutylene bissuccinimide, and the synthesized trimethylolpropane ethylene oxide propylene oxide copolyether and octanol ethylene oxide propylene oxide copolyether in sequence at a temperature of 25° C., and stir for 60 minutes to obtain the crude oil nucleophilic deconstruction aid.
[0052] Application Example 1
[0053] A crude oil 1 was not added with a nucleophilic deconstruction aid, and its salt concentration was 7.2 mg / L (in terms of NaCl), and its water content was 1.2%. After electrical desalination, its salt concentration was 3.5 mg / L (in terms of NaCl), and its water content was 1.2%. After adding 10 ppm of the crude oil nucleophilic deconstruction aid prepared in Example 1, its salt concentration after electrical desalination was only 1.8 mg / L (in terms of NaCl), and its water content was 0.2%.
[0054] Application Example 2
[0055] Crude oil 2 was not added with a nucleophilic deconstruction aid, and its salt concentration was 14.5 mg / L (in terms of NaCl). After electro-desalting, its salt concentration was 4.7 mg / L (in terms of NaCl), and its water content was 1.0%. Crude oil 2 was added with 20 ppm of the nucleophilic deconstruction aid prepared in Example 2, and its salt concentration after electro-desalting was only 1.5 mg / L (in terms of NaCl), and its water content was 0.1%.
[0056] Application Example 3
[0057] Crude oil 3 was not added with nucleophilic deconstruction aid, and its salt concentration was 21.6 mg / L (in terms of NaCl), and its water content was 0.6%. After electrical desalination, its salt concentration was 5.6 mg / L (in terms of NaCl), and its water content was 0.3%. After adding 20 ppm of the crude oil nucleophilic deconstruction aid prepared in Example 3, its salt concentration after electrical desalination was only 2.7 mg / L (in terms of NaCl), and its water content was 0.1%.
[0058] Finally, it should be noted that the above embodiments do not limit the present invention in any form; those skilled in the art can make some modifications and improvements based on the present invention; therefore, any changes, modifications, substitutions, combinations, and simplifications made without departing from the essential content and principles of the present invention should be equivalent replacement methods and are within the scope of protection required by the present invention.
Claims
1. Application of a crude oil nucleophilic deconstruction aid in an electrical desalting process for crude oil pretreatment, characterized in that: The concentration of the crude oil nucleophilic deconstruction aid in the crude oil is 1 to 100 ppm; The crude oil nucleophilic deconstruction aid is composed of component A and component B; component A is composed of a metal detergent, a polymer ashless dispersant, a polyol ethylene-propylene copolymer, and a fatty alcohol ethylene-propylene copolymer; component B is a solvent; The metal detergent is a highly basic petroleum sulfonate or an alkyl salicylate; the polymer ashless dispersant is polyisobutylene succinimide; The preparation of the crude oil nucleophilic deconstruction auxiliary agent comprises the following steps: (1) synthesizing polyol ethylene oxide propylene oxide copolyether and fatty alcohol ethylene oxide propylene oxide copolyether by using polyol, fatty alcohol, ethylene oxide and propylene oxide; (2) adding a metal detergent, a polymer ashless dispersant, and the polyol ethylene oxide propylene oxide copolyether and the fatty alcohol ethylene oxide propylene oxide copolyether obtained in step (1) to a solvent, and stirring them evenly to obtain the crude oil nucleophilic deconstruction aid; The polyol ethylene-propylene copolymer is the polyol ethylene oxide propylene oxide copolyether in step (1), and the fatty alcohol ethylene-propylene copolymer is the fatty alcohol ethylene oxide propylene oxide copolyether in step (1).
2. The use according to claim 1, characterized in that: The ethylene-propylene copolymer in the polyol ethylene-propylene copolymer and the fatty alcohol ethylene-propylene copolymer is an ethylene oxide-propylene oxide copolymer.
3. The use according to claim 2, characterized in that: The polyol is one or more of 2,3-propylene glycol, glycerol, pentaerythritol, trimethylolpropane and sorbitan; the carbon number of the fatty alcohol is C2 to C30.
4. The use according to claim 3, characterized in that: Calculated by mass ratio, the content of metal detergent in component A is 10% to 80%; the content of high molecular ashless dispersant is 10% to 60%; the content of polyol ethylene-propylene copolymer is 5% to 50%; and the content of fatty alcohol ethylene-propylene copolymer is 5% to 30%.
5. The use according to claim 1, characterized in that: The solvent is one or more of toluene, xylene, straight-run kerosene, straight-run diesel, solvent oil, commercial kerosene, and commercial diesel.
6. The use according to claim 5, characterized in that: The mass ratio of component A to component B is 90:10 to 30:70.
Citation Information
Patent Citations
Preparation method of high base number lubricating oil metal cleaning dispersant
CN103130635A
Lubricating oil composition
CN114591777A
Lubricating oil composition
CN114752427A
Crude oil desalting composition and method of use thereof
CN101205482A
Method for removing metals from crude oil
CN103146421A