Method for uncovering press-fit type aluminum base with high thermal conductivity
By filling slots in the aluminum base with high-temperature-resistant gaskets, and combining the direct lamination method of thermosetting adhesive and high thermal conductivity PP, the problem of glue overflow in the existing technology is solved, and the high thermal conductivity and mechanical strength of the aluminum substrate are achieved. Improved to avoid short circuits and dimensional deviations.
Patent Information
- Application Number
- CN202411026492.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-10-15
AI Technical Summary
In the existing technology, when NFPP or high thermal conductivity PP is used to make a radiator, it is easy to cause glue to overflow from the crimping hole, which is difficult to remove, affects the hole diameter, and leads to short circuit problems. The thick aluminum base makes manual polishing difficult and may burn out the circuit. Or damage the solder mask layer.
The grooving process before lamination is used to dig out the area on the aluminum base and fill it with high-temperature-resistant gaskets, and use thermosetting glue and high thermal conductivity PP for direct lamination. The laser burns the four corners of the thermosetting glue to expose the crimping holes to avoid the impact of glue overflow. aperture, and ensure conduction without damaging the solder mask layer.
It effectively avoids the size deviation and short circuit of the crimping hole, ensures the normal conduction and heat dissipation performance of the aluminum substrate, and improves the mechanical strength and reliability.
Smart Images

Figure CN118785631A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum bases, and in particular to a method for uncovering a pressed aluminum base with high thermal conductivity. Background Art
[0002] Thermal management has a significant and huge impact on the overall performance, reliability and cost of a project. As one of the main technologies for thermal management, aluminum block heat dissipation technology has been widely used. Aluminum heat sinks have been playing a leading role for many years, which is the result of the right choice. For example, it is cheap, low in density, easy to process and form, and has good hardness. Another important point is that the heat sink made of it is very close to pure copper products in terms of heat dissipation performance. Then the device acts directly on the aluminum base and dissipates heat directly, which is more effective.
[0003] However, the existing technology generally uses NFPP or high thermal conductivity PP to make heat sinks for transferring heat from press-fit devices, which mainly have the following problems: Using NFPP: The glue flow is not good, which may lead to glue shortage, board explosion and delamination, and the process is long and the cost is high. At the same time, the thermal conductivity of NFPP is poor; Use high thermal conductivity PP: When slotting and pressing first, PP overflows seriously, resulting in glue accumulation at the crimping hole, which cannot be removed, affecting the hole diameter and causing abnormal crimping holes; pressing first and then slotting, it is necessary to mechanically control the depth of the aluminum base and then laser burn the PP. The disadvantages of this method are: The slot size is too small, the mechanical gong is easy to deviate, resulting in dimensional deviation; PP overflow glue, when removing the cover in a very small area of 3*3mm, adheres to the surface of the PTH hole and is extremely difficult to handle; Since the thickness of the aluminum base is 2.0mm, the height difference is too large, and it is impossible to manually polish the surface of the PTH hole. Even if it is laser burned, it cannot be cleaned up, and it may burn the circuit or copper, or damage the solder mask and PAD surface. Summary of the invention
[0004] The main purpose of the present invention is to propose a method for uncovering a pressed aluminum base with high thermal conductivity, aiming to solve the technical problems that the existing heat sink used to transmit heat from the crimped device has poor heat dissipation effect and easily causes glue overflow on the crimping hole, which is difficult to remove and causes a short circuit.
[0005] To achieve the above object, the present invention provides a method for removing a pressed aluminum-based cover with high thermal conductivity, comprising the following steps: S100: On the thick copper FR-4 board, L1-L4 layers are pressed normally from top to bottom to make a complete 4-layer board process and obtain a 4-layer hard board; S200: Slot the aluminum base opening, dig out a 3*3mm area, obtain a slotted aluminum base, and fill the slot with a high-temperature resistant gasket; S300: The bottom of the L4 layer is filled with thermosetting adhesive and high thermal conductivity PP as required, and directly pressed with the slotted aluminum base; S400: After the pressing is completed, the high-temperature gasket is taken out, the PP is heat-conducted in the groove by mechanical gong, and then the four corners of the thermosetting adhesive are burned by laser. Then the thermosetting adhesive is taken out to expose the pressing holes to obtain the aluminum substrate.
[0006] Optionally, in step S100, the L1 and L4 layers include 0.5 oz copper foil respectively, and the L2 and L3 layers include 3 oz copper foil respectively.
[0007] Optionally, in step S100, four layers of prepreg are provided between layers L1 and L2, and between layers L3 and L4, respectively.
[0008] Optionally, in step S100, a core layer is provided between layers L2 and L3, and the core layer does not contain copper.
[0009] Optionally, in step S100, the 4-layer board process includes surface treatment, solder mask characters, and open and short circuit detection.
[0010] Optionally, in step S200, a pre-pressing grooving process is used to dig out all openings and fill them with high temperature resistant gaskets.
[0011] Optionally, in step S200, the thickness of the aluminum base is 2.0 mm.
[0012] Optionally, in step S200, the crimping hole is a plated-through hole, namely, a PTH hole.
[0013] Optionally, in step S300, the thickness of the thermosetting adhesive is 0.025 mm*2.
[0014] Optionally, in step S300, the high temperature resistant gasket is silicone rubber or ceramic fiber paper.
[0015] The technical solution of the present invention has the following beneficial effects: the technical solution of the present invention uses a grooving process before pressing to dig out all the openings of the aluminum base, thereby avoiding the situation where the mechanical gong is easily deviated when pressing first and then grooving, resulting in dimensional deviation; by using thermosetting adhesive, it can prevent PP overflow from affecting the aperture of the crimping hole, and prevent direct adhesion to the copper sheet, thereby ensuring the normal conduction of the crimping hole, and does not damage the solder mask layer and the PAD surface, effectively dissipating heat while effectively avoiding short circuits. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.
[0017] Figure 1 A flowchart of a method for uncovering a press-fit aluminum-based product with high thermal conductivity according to an embodiment of the present invention; Figure 2 This is a schematic diagram of the structure of the aluminum substrate L1-L4 layers according to an embodiment of the present invention; Figure 3 This is a schematic diagram of aluminum-based slotting according to an embodiment of the present invention; Figure 4 FIG. 1 is a schematic diagram of the overall structure of an aluminum substrate according to an embodiment of the present invention.
[0018] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0020] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0021] In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0022] The invention provides a press-fit aluminum-based uncovering method with high thermal conductivity.
[0023] like Figures 1 to 4 As shown, in one embodiment of the present invention, the method for uncovering the pressed aluminum base with high thermal conductivity comprises the following steps: S100: On the thick copper FR-4 board, L1-L4 layers are pressed normally from top to bottom to make a complete 4-layer board process and obtain a 4-layer hard board; S200: Slot the aluminum base opening, dig out a 3*3mm area, obtain a slotted aluminum base, and fill the slot with a high-temperature resistant gasket; S300: The bottom of the L4 layer is filled with thermosetting adhesive and high thermal conductivity PP as required, and directly pressed with the slotted aluminum base; S400: After the pressing is completed, the high temperature gasket is removed, the PP is mechanically gonged in the groove for heat conduction, and then the four corners of the thermosetting adhesive are burned by laser. Then the thermosetting adhesive is removed to expose the pressing holes to obtain the aluminum substrate, thereby effectively Specifically, in step S100, the L1 and L4 layers each include 0.5 oz copper foil, which has good conductivity and good versatility, and the L2 and L3 layers each include 3 oz copper foil, i.e., 105 μm, which can withstand a larger current or high voltage.
[0024] Specifically, in step S100, four layers of prepreg are provided between L1 and L2, and between L3 and L4, respectively. The prepreg is used as a bonding material and interlayer insulation for the inner conductive patterns of the multi-layer printed circuit board, and can also play a good role in heat insulation.
[0025] Specifically, in step S100, a core layer is provided between the L2 and L3 layers, and the core layer does not contain copper. Since it does not contain copper foil, although its conductivity is poor, it has good mechanical strength and insulation performance, and has a lower manufacturing cost and a higher cost performance.
[0026] Specifically, in step S100, the 4-layer board process includes surface treatment, solder mask characters, and open and short circuit detection, which can effectively solve the problem of short circuit caused by components directly acting on the aluminum substrate.
[0027] Specifically, in step S200, a grooving process is used before lamination to dig out all the openings of the aluminum base and fill them with high-temperature resistant gaskets to ensure smooth lamination. The high-temperature resistant gaskets are silicone rubber or ceramic fiber paper, which is convenient for direct removal after lamination.
[0028] Specifically, in step S200, the thickness of the aluminum substrate is 2.0 mm, which is not only light and flexible, but also corrosion-resistant, has a long service life, and has good thermal insulation performance.
[0029] Specifically, in Example 1 of the present invention, the thickness of the thermosetting adhesive is 0.025mm*2. During actual use, the thermosetting adhesive has the characteristics of fast curing and high strength, and can avoid overflow of high thermal conductivity PP. When the cover is removed in an extremely small area of 3*3mm, the surface of the crimping hole is clean, the aperture of the crimping hole will not be affected, and the high thermal conductivity PP will not be directly bonded to the copper sheet, thereby ensuring normal conduction of the crimping hole and not damaging the solder mask and the PAD surface. While effectively dissipating heat, the aluminum substrate and the thick copper plate FR-4 are bonded and pressed together to effectively avoid short circuits. In particular, when there are requirements for the thickness of the aluminum substrate, the required dielectric thickness can be met by using thermosetting adhesive and high thermal conductivity PP.
[0030] The specific principles of the present invention are as follows: Lamination is the process of bonding insulating materials, copper foil and prepreg into a whole under a certain temperature and pressure. This process has a crucial impact on the performance of the circuit board.
[0031] Thermosetting adhesive: Thermosetting adhesive is a special adhesive that cures quickly and completes the bonding process by heating. The bonding process is completed by chemical cross-linking. Thermosetting adhesive has the performance characteristics of fast curing, high mechanical strength after curing, heat resistance, cold resistance, and good chemical resistance, and will not have volatilization loss, deterioration, and aging. Thermosetting adhesive does not melt when heated, but cures through chemical reactions, so its properties are irreversible after curing. This makes thermosetting adhesive perform well in bonding situations that require long-term durability. Polypropylene, referred to as PP, is a polymer formed by the addition polymerization of propylene. It is a white waxy material with a transparent and light appearance. Its chemical formula is (C3H6)n, its density is 0.89-0.91g / cm3, it is flammable, its melting point is 164-170℃, it softens at about 155℃, and its operating temperature range is -30-140℃. It is resistant to corrosion by acids, alkalis, salt solutions and various organic solvents below 80℃, and it can decompose under high temperature and oxidation. Polypropylene is a thermoplastic synthetic resin with excellent performance. It is a colorless, translucent, thermoplastic, lightweight general-purpose plastic with chemical resistance, heat resistance, electrical insulation, high-strength mechanical properties and good high-wear-resistant processing properties.
[0032] FR-4 is one of the commonly used substrates for PCBs. It is a code for a flame-resistant material grade, which means that the resin material must be able to extinguish itself after burning. FR-4 is not a material name, but a material grade.
[0033] FR-4 is generally divided into: FR-4 rigid board, common board thickness 0.8-3.2mm; FR-4 thin board, the common board thickness is less than 0.78mm.
[0034] Oz itself is a unit of weight. The conversion formula between ounce and gram (g) is: 1oz ≈ 28.35g. The thickness of the copper foil of the copper clad laminate is measured by the weight of the single-sided copper foil. The commonly used thicknesses in China are: 0.5 OZ (18um), 1 OZ (35um), 2 OZ (70um), 3 OZ (105um), 4 OZ (140um), 5 OZ (175um). Among them, 1 OZ means that the weight of 1 square meter of copper foil is 35 grams.
[0035] Specifically, compared with the prior art, the advantages and positive effects of the present invention lie in that the technical solution of the present invention specifically uses a grooving process before pressing, digging out all openings, i.e., crimping holes, and using a method of uncovering and directly pressing, combined with the use of thermosetting adhesive, the normal conduction of the crimping holes is ensured without affecting the appearance. The aluminum substrate FR-4 has many layers and a thick board, thereby effectively improving the mechanical strength and chemical stability of the product, increasing its durability and reliability, and can effectively solve the problem of components directly acting on the aluminum substrate to dissipate heat without short-circuiting.
[0036] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the inventive concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.
Claims
1. A method for uncovering a pressed aluminum base with high thermal conductivity, characterized in that: The following steps are involved: S100: On the thick copper FR-4 board, L1-L4 layers are pressed normally from top to bottom to make a complete 4-layer board process and obtain a 4-layer hard board; S200: Slot the aluminum base opening, dig out a 3*3mm area, obtain a slotted aluminum base, and fill the slot with a high-temperature resistant gasket; S300: The bottom of the L4 layer is filled with thermosetting adhesive and high thermal conductivity PP as required, and directly pressed with the slotted aluminum base; S400: After the pressing is completed, the high-temperature gasket is taken out, the PP is heat-conducted in the groove by mechanical gong, and then the four corners of the thermosetting adhesive are burned by laser, and then the thermosetting adhesive is taken out to expose the pressing holes to obtain the aluminum substrate.
2. The method for uncovering a pressed aluminum base with high thermal conductivity according to claim 1, characterized in that: In the step S100, the L1 and L4 layers each include 0.5 oz copper foil, and the L2 and L3 layers each include 3 oz copper foil.
3. The method for uncovering a pressed aluminum base with high thermal conductivity according to claim 1, characterized in that: In the step S100, four layers of prepreg are respectively arranged between the layers L1 and L2, and between the layers L3 and L4.
4. The method for uncovering a pressed aluminum-based cover having high thermal conductivity according to claim 1, characterized in that: In the step S100, a core layer is provided between the L2 and L3 layers, and the core layer does not contain copper.
5. The method for uncovering a pressed aluminum base with high thermal conductivity according to claim 1, characterized in that: In step S100, the 4-layer board process includes surface treatment, solder mask characters, and open and short circuit detection.
6. The method for uncovering a pressed aluminum base with high thermal conductivity according to claim 1, characterized in that: In the step S200, a pre-pressing grooving process is used to dig out all the openings of the aluminum base and fill them with high temperature resistant gaskets.
7. The method for uncovering a pressed aluminum base with high thermal conductivity according to claim 1, characterized in that: In the step S200, the thickness of the aluminum base is 2.0 mm.
8. The method for uncovering a pressed aluminum-based cover with high thermal conductivity according to claim 1, characterized in that: In the step S200, the crimping hole is a plated-through hole, namely, a PTH hole.
9. The method for uncovering a pressed aluminum base with high thermal conductivity according to claim 1, characterized in that: In the step S300, the thickness of the thermosetting adhesive is 0.025 mm*2.
10. The method for uncovering a pressed aluminum-based cover with high thermal conductivity according to claim 1, characterized in that: In step S300, the high temperature resistant gasket is silicone rubber or ceramic fiber paper.