Film-forming agent composition as well as preparation method and application thereof

By using film-forming agent compositions such as acrylic (ester) copolymers, serratonium chloride hydropyroxene and trimethylsilyloxy silicate in sunscreen cosmetics, the sunscreen index, friction resistance and water resistance of sunscreen cosmetics are solved. The sexual deficiencies have achieved better skin feeling and sun protection.

CN118948674APending Publication Date: 2024-11-15GUANGZHOU HUANYA COSMETIC SCI & TECH CO LTD

Patent Information

Application Number
CN202410990163.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing sunscreen cosmetics have challenges in improving sunscreen index, friction resistance, film formation and waterproofing and sweat resistance, resulting in poor skin feeling and difficulty in ensuring stability.

Method used

A film-forming agent composition is adopted, including acrylic (ester) copolymer, pyroxene, trimethylsilyloxy silicate and other film-forming synergists, to form a uniform protective film and improve the sun protection effect. and water resistance, and enhance the stability and dispersion of the film by poly C10-30 alkanol acrylate.

Benefits of technology

It significantly improves the sun protection index, enhances the anti-water and anti-friction effects, ensures the softness and durability of the skin and the sun protection effect, and makes the skin feel refreshed and not sticky.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004958642650000061
    Figure BDA0004958642650000061
  • Figure BDA0004958642650000071
    Figure BDA0004958642650000071
  • Figure BDA0004958642650000072
    Figure BDA0004958642650000072
Patent Text Reader

Abstract

The invention discloses a film-forming agent composition as well as a preparation method and application thereof, and relates to the technical field of cosmetics. The film-forming agent composition disclosed by the invention is prepared from an acrylic acid (ester) copolymer, selammonium chloride hectorite and a film-forming synergist, the film forming synergist is prepared from at least one of trimethylsiloxy silicate ester and poly (C10-30 alkanol acrylate). The acrylic acid (ester) copolymer, the Slassine chloride hectorite and the film-forming synergist have a synergistic effect, so that the sunscreen index, the water-resistant effect and the friction-resistant effect of the product can be effectively improved, and the sunscreen effect is improved after the product encounters water.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of cosmetics, and in particular to a film-forming agent composition, a preparation method and an application thereof. Background Art

[0002] Ultraviolet rays are the main cause of exogenous skin aging. Excessive exposure can cause skin sunburn, tanning, and aging. In order to reduce the damage of ultraviolet rays to the skin, a variety of sunscreen cosmetics have been developed. Summer outdoor activities, water sports and other usage scenarios require sunscreen cosmetics to have high sun protection, anti-friction, film-forming, and waterproof and sweat-resistant functions to achieve long-term protection of the skin.

[0003] In the related art, the sun protection index is generally increased by increasing the amount of sunscreen added, but this will also make it difficult to ensure the skin feel and stability of sunscreen cosmetics. If the film-forming agent is not selected well, it will also cause problems such as sticky skin feel. In addition, if the film-forming and waterproof capabilities of sunscreen cosmetics are not good, its ultraviolet protection effect will be greatly reduced. Therefore, it is more important to provide a film-forming agent composition that has enhanced sunscreen ability and good anti-friction, film-forming, waterproof and anti-sweat effects. Summary of the invention

[0004] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention provides a film-forming agent composition, which can effectively improve the sunscreen effect, friction resistance, film formation and water resistance and sweat resistance of sunscreen cosmetics.

[0005] The present invention also provides a method for preparing the film-forming agent composition.

[0006] The present invention also provides application of the film-forming agent composition in preparing sunscreen cosmetics.

[0007] The present invention also provides a sunscreen cosmetic comprising the film-forming agent composition.

[0008] A film-forming agent composition according to the first embodiment of the present invention comprises: an acrylic acid (ester) copolymer, stearalkonium hectorite and a film-forming synergist;

[0009] The film-forming synergist includes at least one of trimethylsiloxysilicate and poly C10-30 alkyl acrylate.

[0010] The film-forming agent composition according to the embodiment of the present invention has at least the following beneficial effects:

[0011] Acrylic acid (ester) copolymer is an oil-soluble polymer that can form a uniform protective film on the skin surface and has a water-resistant effect. Stearalkonium hectorite has excellent film-forming properties and can form a uniform and smooth film on the skin surface, giving the skin a soft and smooth feeling. This film not only helps prevent water loss, but also protects the skin from the external environment; the oil droplets in the oil phase are covered by stearalkonium hectorite, which reduces the contact with the water phase, prevents re-emulsification, and makes the sunscreen cosmetics effectively water-resistant. Stearalkonium hectorite also has thickening and suspension effects, which helps powders (such as physical sunscreens such as titanium dioxide and zinc oxide) to disperse and improve the sunscreen effect. Trimethylsiloxysilicate can form a waterproof film on the skin surface, effectively preventing water loss and maintaining the softness of the skin. At the same time, this ingredient also has excellent application performance, which can increase the smoothness of cosmetics, reduce the dryness of the skin, and make sunscreen cosmetics easier to apply evenly. Poly C10-30 alkyl acrylate has good film-forming properties and can form a uniform and thick film. It can also improve the dispersibility of color powders, etc., enhance the sunscreen effect, and has excellent stability and viscosity adjustment capabilities, which can help sunscreen cosmetics maintain a stable texture and lasting feel.

[0012] The acrylic acid (ester) copolymer, stearalkonium hectorite, and film-forming synergist in the film-forming composition of the embodiment have a synergistic effect with each other, which can effectively improve the sun protection index, water resistance and anti-friction effect of the product, and the sun protection effect is improved after contact with water. Compared with the sunscreen cosmetics without the film-forming composition of the present invention, the SPF value can be increased by 50.8% to 77.0% after adding the film-forming composition of the present invention; compared with before the water bath, after the 25°C water bath for 40 minutes, the SPF value of the sunscreen cosmetics added with the film-forming composition of the present invention can be increased by 3.2% to 18.0%; after the friction treatment, the equivalent film thickness residual rate of the sunscreen cosmetics added with the film-forming composition of the present invention reaches more than 85%.

[0013] According to some embodiments of the present invention, the film-forming agent composition comprises, in parts by weight:

[0014] 0.2 to 5 parts of acrylic acid (ester) copolymer,

[0015] 0.025-1.5 parts of stearalkonium hectorite,

[0016] 0-6 parts of trimethylsiloxysilicate,

[0017] Poly C10-30 alkyl acrylate 0-5 parts.

[0018] According to some embodiments of the present invention, the film-forming agent composition comprises, in parts by weight:

[0019] 0.4 to 2.0 parts of acrylic acid (ester) copolymer,

[0020] 0.1 to 1.7 parts of stearalkonium hectorite,

[0021] 0.1 to 6.5 parts of trimethylsiloxysilicate,

[0022] Poly C10-30 alkyl acrylate 0 to 3 parts.

[0023] According to some embodiments of the present invention, the film-forming agent composition comprises, in parts by weight:

[0024] 0.4 to 2.0 parts of acrylic acid (ester) copolymer,

[0025] 0.1 to 1.7 parts of stearalkonium hectorite,

[0026] 0.8 to 6.5 parts of trimethylsiloxysilicate,

[0027] Poly C10-30 alkyl acrylate 0 to 1.5 parts.

[0028] According to some embodiments of the present invention, the film-forming agent composition comprises, in parts by weight:

[0029] 0.4 to 0.6 parts of acrylic acid (ester) copolymer,

[0030] 1.3-1.7 parts of stearalkonium hectorite,

[0031] 5.5 to 6.5 parts of trimethylsiloxysilicate.

[0032] According to some embodiments of the present invention, the film-forming agent composition comprises, in parts by weight:

[0033] 0.8 to 2.0 parts of acrylic acid (ester) copolymer,

[0034] 0.1-0.6 parts of stearalkonium hectorite,

[0035] 0.8 to 1.5 parts of trimethylsiloxysilicate,

[0036] 0.8 to 1.5 parts of poly C10-30 alkyl acrylate.

[0037] According to some embodiments of the present invention, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.005-7.5): (0-30): (0-25).

[0038] According to some embodiments of the present invention, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.005-3.5): (0-15): (0-25).

[0039] According to some embodiments of the present invention, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.08-3.2): (0.1-13): (0-1.5).

[0040] According to some embodiments of the present invention, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.08-3.2): (0.5-13): (0-1.2).

[0041] According to some embodiments of the present invention, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1:(2.8-3.2):(11-13):0.

[0042] According to some embodiments of the present invention, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.08-0.5): (0.5-1.2): (0.5-1.2).

[0043] The method for preparing the above-mentioned film-forming agent composition according to the second aspect of the present invention comprises the following steps:

[0044] The acrylic acid (ester) copolymer, stearalkonium hectorite and a film-forming synergist are mixed to obtain the film-forming agent composition.

[0045] According to some embodiments of the present invention, when the film-forming synergist includes the trimethylsiloxysilicate, the preparation method includes the following steps:

[0046] The solution containing trimethylsiloxysilicate and a volatile solvent is mixed with the remaining combination, and the volatile solvent is removed to obtain the film-forming agent composition.

[0047] According to some embodiments of the present invention, the volatile solvent includes isododecane, undecane / tridecane (7:3), and cyclopentasiloxane.

[0048] According to the third aspect of the present invention, the film-forming agent composition is used in the preparation of sunscreen cosmetics.

[0049] A sunscreen cosmetic according to a fourth aspect of the present invention comprises the film-forming agent composition as described in the first aspect of the present invention. Since the sunscreen cosmetic adopts all the technical solutions of the film-forming agent composition of the above embodiment, it at least has all the beneficial effects brought by the technical solutions of the above embodiment. Moreover, the sunscreen cosmetic containing the above film-forming agent composition has a refreshing and non-greasy feel.

[0050] According to some embodiments of the present invention, the dosage form of the sunscreen cosmetic is selected from cream, mousse, gel, emulsion or spray.

[0051] According to some embodiments of the present invention, the sunscreen cosmetic further comprises a sunscreen and excipients acceptable in the cosmetics field.

[0052] According to some embodiments of the present invention, the mass percentage of the film-forming agent composition in the sunscreen cosmetic is 0.3% to 18%. For example, it can be 0.3%, 0.5%, 0.8%, 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, 4%, 4.5%, 5%, 5.5%, 6%, 6.5%, 7%, 7.5%, 8%, 8.5%, 9%, 9.5%, 10%, 11%, 12%, 13%, 14%, 15%, 16%, 17% or 18%.

[0053] According to some embodiments of the present invention, the sunscreen includes a combination of at least two of titanium dioxide, zinc oxide, ethylhexyl methoxycinnamate, isopentyl p-methoxycinnamate, bis-ethylhexyloxyphenol methoxyphenyl triazine, diethylaminohydroxybenzoyl hexyl benzoate, diethylhexyl butyramido triazone, ethylhexyl triazone, phenylbenzimidazole sulfonic acid, methylene bis-benzotriazolyl tetramethylbutylphenol, butyl methoxydibenzoylmethane, polysilicone-15, octocrylene, homosalate, ethylhexyl salicylate, disodium phenyl dibenzimidazole tetrasulfonate, terephthalylidene dicamphor sulfonic acid, and drometrizole trisiloxane.

[0054] According to some embodiments of the present invention, the auxiliary material includes at least one of an emulsifier, a moisturizing oil, a skin feel regulator, a polyol and an additive.

[0055] According to some embodiments of the present invention, the emulsifier includes at least one of lauryl PEG-9 polydimethylsiloxyethyl dimethicone, cetyl PEG / PPG-10 / 1 dimethicone, PEG-10 dimethicone, and polyglyceryl-2 dipolyhydroxystearate.

[0056] According to some embodiments of the present invention, the emollient oil includes at least one of dibutyl adipate, coconut oil caprylate / caprate, polydimethylsiloxane, octyl polymethicone, dicaprylyl carbonate, isononyl isononanoate, phenyl trimethicone, isododecane, isohexadecane, propylheptyl octanoate, undecane / tridecane (7:3), and butyl octanol salicylate.

[0057] According to some embodiments of the present invention, the skin feel regulator includes at least one of silica, vinyl dimethicone / polymethylsiloxane silsesquioxane crosspolymer, and polymethylsilsesquioxane.

[0058] According to some embodiments of the present invention, the polyol includes at least one of glycerol, butanediol, 1,3-propylene glycol, and 1,2-hexanediol.

[0059] According to some embodiments of the present invention, the additive includes at least one of a colorant, a chelating agent, a thickener, a stabilizer, a dispersant, a moisturizer, a pH adjuster, an antioxidant, a fragrance, a skin protectant, and a preservative.

[0060] According to some embodiments of the present invention, the chelating agent includes at least one of disodium EDTA and tetrasodium EDTA.

[0061] According to some embodiments of the present invention, the thickener includes at least one of xanthan gum and sodium polyacrylate.

[0062] According to some embodiments of the present invention, the stabilizer includes at least one of sodium chloride and magnesium sulfate.

[0063] According to some embodiments of the present invention, the dispersant includes at least one of polyhydroxystearic acid, polyglyceryl-3 polydimethylsilyl hydroxyethyl polydimethylsiloxane, and lauryl polyglyceryl-3 polydimethylsiloxyethyl polydimethylsiloxane.

[0064] According to some embodiments of the present invention, the moisturizing agent includes at least one of sodium hyaluronate and hydrolyzed sodium hyaluronate.

[0065] According to some embodiments of the present invention, the pH adjuster includes at least one of aminomethyl propanol and tromethamine.

[0066] According to some embodiments of the present invention, the antioxidant includes at least one of p-hydroxyacetophenone, pentaerythritol tetrakis (di-tert-butyl hydroxyhydrocinnamate), tocopherol (vitamin E), and tocopherol acetate.

[0067] According to some embodiments of the present invention, the skin protectant includes at least one of ascorbyl tetraisopalmitate, tetrahydromethylpyrimidine carboxylic acid, allantoin, and panthenol.

[0068] According to some embodiments of the present invention, the preservative includes at least one of phenoxyethanol, sodium benzoate, and potassium sorbate.

[0069] According to some embodiments of the present invention, the sunscreen cosmetic comprises the following components in percentage by mass: 0.3% to 18% of the above-mentioned film-forming agent composition, 15.0% to 30.0% of sunscreen agent, 1.5% to 6.0% of emulsifier, 2.0% to 42.0% of moisturizing oil, 0.5% to 5.0% of skin feel regulator, 2.0% to 15.0% of polyol and 0.5% to 15.0% of additives; the balance is water.

[0070] According to some embodiments of the present invention, the additive includes at least one of a chelating agent, a humectant, a dispersant, an antioxidant, a stabilizer, and a fragrance.

[0071] According to some embodiments of the present invention, based on the total mass of the sunscreen cosmetic, the sunscreen cosmetic includes the following components in mass percentage: the content of the chelating agent is 0.01% to 0.2%; the content of the moisturizing agent is 0.02% to 2%; the content of the dispersant is 0.1% to 3.0%; the content of the antioxidant is 0.02% to 5%; the content of the stabilizer is 0.2% to 2%; and the content of the fragrance is 0.02% to 0.5%.

[0072] According to some embodiments of the present invention, the method for preparing the sunscreen cosmetic comprises the following steps:

[0073] The components are mixed to obtain the sunscreen cosmetic.

[0074] Other features and advantages of the present invention will be set forth in the description which follows, and in part will be apparent from the description, or may be learned by practice of the present invention. DETAILED DESCRIPTION

[0075] The following will be combined with the embodiments to clearly and completely describe the concept of the present invention and the technical effects produced, so as to fully understand the purpose, characteristics and effects of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, other embodiments obtained by those skilled in the art without creative work are all within the scope of protection of the present invention.

[0076] If the specific conditions are not specified in the examples, the experiments were carried out under conventional conditions or conditions recommended by the manufacturer. If the manufacturers of the reagents or instruments are not specified, they are all conventional products that can be purchased commercially.

[0077] When a numerical range is disclosed herein, the above range is considered to be continuous and includes the minimum and maximum values ​​of the range, as well as every value between such minimum and maximum values. Further, when a range refers to an integer, every integer between the minimum and maximum values ​​of the range is included. In addition, when multiple ranges are provided to describe features or characteristics, the ranges can be combined. In other words, unless otherwise indicated, all ranges disclosed herein should be understood to include any and all subranges included therein.

[0078] "Parts by mass" refers to the basic unit of measurement for expressing the mass ratio of multiple components. 1 part can represent any unit mass, such as 1g or 2.689g. If we say that the mass of component A is a parts and the mass of component B is b parts, it means the ratio of the mass of component A to the mass of component B is a:b. Alternatively, it means that the mass of component A is aK and the mass of component B is bK (K is an arbitrary number, indicating a multiple factor). It should not be misunderstood that, unlike the mass parts, the sum of the mass of all components is not limited to 100 parts.

[0079] "And / or" is used to indicate that one or both of the stated situations may occur, for example, A and / or B includes (A and B) and (A or B).

[0080] Example

[0081] This example provides 8 film-forming agent compositions. The formulas are shown in Table 1 in parts by weight.

[0082] Table 1

[0083]

[0084] The steps for preparing the film-forming agent compositions of Examples 3, 4, 6, 7, and 8 are as follows:

[0085] (1) dissolving trimethylsiloxysilicate in isododecane and placing it in an emulsifying pot, and heating it to 80° C.;

[0086] (2) adding poly (C10-30 alkyl acrylate), stearalkonium chloride hectorite and acrylic acid (ester) copolymer to the emulsifying pot and stirring evenly;

[0087] (3) Continue stirring to volatilize the isododecane to obtain a film-forming agent composition.

[0088] The steps for preparing the film-forming agent composition of Examples 1, 2, and 5 are as follows:

[0089] (1) Adding poly (C10-30 alkyl acrylate), stearalkonium hectorite and acrylic acid (ester) copolymer into an emulsifying pot and heating to 80° C.;

[0090] (2) Continue stirring to evenly disperse the raw materials to obtain a film-forming agent composition.

[0091] Comparative Example

[0092] This example provides 7 film-forming agent compositions. The formulas are shown in Table 2 in parts by weight.

[0093] Table 2

[0094]

[0095] The preparation method of the film-forming agent composition of Comparative Example 3 is the same as that of Examples 1, 2 and 5.

[0096] The preparation method of the film-forming agent composition of Comparative Example 4 is the same as that of Examples 3, 4, 6, 7 and 8.

[0097] The steps for preparing the film-forming agent composition of Comparative Example 5 are as follows:

[0098] (1) adding hydrogenated polycyclopentadiene / isododecane, stearalkonium hectorite and acrylic acid (ester) copolymer into an emulsifying pot and heating to 80° C.;

[0099] (2) Continue stirring to volatilize the isododecane to obtain a film-forming agent composition.

[0100] Application Examples 1 to 8

[0101] This application example provides 8 kinds of sunscreen creams. The formulas are shown in Table 3.

[0102] Table 3

[0103]

[0104]

[0105]

[0106] The steps of preparing the sunscreen cream of Application Examples 1 to 8 are as follows:

[0107] (1) preliminarily dissolving p-hydroxyacetophenone by heating with 1,2-hexanediol to obtain a p-hydroxyacetophenone solution; dissolving trimethylsiloxysilicate in phase D by using isododecane until it becomes transparent to obtain a trimethylsiloxysilicate solution;

[0108] (2) Add the remaining components of phase A into a water phase pot, stir and disperse them evenly at 80° C., add p-hydroxyacetophenone solution before emulsification and stir evenly to obtain a phase A mixture;

[0109] (3) Mix phase B with octyl polymethylsiloxane, isononyl isononanoate and an appropriate amount of polydimethylsiloxane in phase C, and grind evenly through a colloid mill for 3 times to obtain a phase B mixture;

[0110] (4) Add the phase B mixture, the remaining phase C components and the phase D components into an emulsifying pot, heat to 80°C, and stir to disperse evenly;

[0111] (5) Slowly and evenly add the phase A mixture into the emulsifier and stir for 15 minutes;

[0112] (6) Cool down to 45°C, add the E phase components into the emulsifier, and stir and homogenize for 3 minutes.

[0113] (7) Degassing by vacuuming at 37° C., discharging the product, and allowing the product to stand to obtain a sunscreen cream.

[0114] Application Comparative Example 1

[0115] This application example provides a sunscreen cream, which is basically the same as application example 4, except that 2.6% of the film-forming agent composition of example 4 is replaced by 0.1% of the film-forming agent composition of comparative example 1 and 2.5% of deionized water.

[0116] Application Comparative Example 2

[0117] This application example provides a sunscreen cream, which is basically the same as application example 4, except that 2.6% of the film-forming agent composition in example 4 is replaced by 2.6% of deionized water.

[0118] Application Comparative Example 3

[0119] This application example provides a sunscreen cream, which is basically the same as application example 4, except that 2.6% of the film-forming agent composition of example 4 is replaced by 1.6% of the film-forming agent composition of comparative example 3 and 1% of deionized water.

[0120] Application Comparative Example 4

[0121] This application example provides a sunscreen cream, which is basically the same as application example 4, except that 2.6% of the film-forming agent composition of example 4 is replaced by 1% of the film-forming agent composition of comparative example 4 and 1.6% of deionized water.

[0122] Application Comparative Example 5

[0123] This application example provides a sunscreen cream, which is basically the same as application example 4, except that 2.6% of the film-forming agent composition of example 4 and 0.43% of isododecane are replaced with 3.03% of the film-forming agent composition of comparative example 5.

[0124] Application Comparative Example 6

[0125] This application example provides a sunscreen cream, which is basically the same as application example 6, except that 1.65% of the film-forming agent composition of example 6 is replaced by 1% of the film-forming agent composition of comparative example 6 and 0.65% of deionized water.

[0126] Application Comparative Example 7

[0127] This application example provides a sunscreen cream, which is basically the same as application example 7, except that 3.45% of the film-forming agent composition of example 7 is replaced by 1% of the film-forming agent composition of comparative example 7 and 2.45% of deionized water.

[0128] Test Example 1

[0129] The test was conducted with reference to the method of human skin patch test in the "Technical Specification for Safety of Cosmetics" (2015 Edition). 30 volunteers aged 18 to 60 who met the test requirements were selected as subjects (including 10 males and 20 females). The sunscreen creams of Application Examples 1 to 8 were used as test substances, and patch tests were conducted to detect their potential to cause adverse reactions to human skin. The test substance was added to the patch tester in an amount of 0.020 to 0.025 g. The control well was a blank control (no substance was placed). The patch tester with the test substance was applied to the back of the subject with a hypoallergenic tape, and gently pressed with the palm of the hand to apply it evenly to the skin for 24 hours. The test site was marked for observation. Observe the skin reaction according to the skin adverse reaction grading standard shown in Table 4 at 30 minutes (after the indentation disappears), 24 hours and 48 hours after removing the test substance patch tester, and record the observation results.

[0130] The test results are shown in Table 5.

[0131] Table 4

[0132]

[0133] Table 5

[0134]

[0135]

[0136]

[0137] The sunscreen creams of application examples 1 to 8 do not cause any allergic or irritating effects on the skin. The sunscreen creams of the present invention are mild and safe and do not irritate the skin.

[0138] Test Example 2

[0139] Use a 1 mL disposable syringe to draw the sunscreen creams of application examples 1 to 8 and the sunscreen creams of application comparative examples 1 to 7 respectively, and apply them evenly on the PMMA plate. The loading amount is 1.3 mg / cm 2 Place it horizontally in a place without direct light at room temperature for 15 minutes to balance and dry, then use Labsphere UV2000S instrument to test the transmittance of the sunscreen sample in the 290-400nm ultraviolet band, and use the instrument software to analyze the results and calculate the SPF in vitro (Abbreviated as SPF).

[0140]

[0141] Where, E(λ) is the erythema effect coefficient (CIE-1987); I(λ) is the irradiation intensity of the UV light source of the instrument used for SPF testing; A0(λ) is the average monochromatic absorbance of each sample plate before UV irradiation; dλ is the wavelength step size (1nm).

[0142] The results are shown in Table 6.

[0143] Table 6

[0144] sample SPF sample SPF Application Example 1 108 Application Comparative Example 1 73 Application Example 2 92 Application Comparative Example 2 61 Application Example 3 100 Application Comparative Example 3 84 Application Example 4 94 Application Comparative Example 4 71 Application Example 5 93 Application Comparative Example 5 88 Application Example 6 94 Application Comparative Example 6 80 Application Example 7 102 Application Comparative Example 7 74 Application Example 8 106

[0145] Compared with the comparative example 2 without adding the film-forming agent composition, the SPF of the application example 1 is increased by 77.0%.

[0146] Compared with the comparative example 2 without adding the film-forming agent composition, the SPF of the application example 2 is increased by 50.8%.

[0147] Compared with the comparative example 2 without adding the film-forming agent composition, the SPF of the application example 3 is increased by 63.9%.

[0148] Compared with Application Example 2 without adding a film-forming agent composition, Application Example 4 has an SPF value increased by 54.1%; Application Example 1, compared with Application Example 4, only contains the corresponding stearalkonium hectorite, and the SPF value is reduced by 22.3%. Application Example 3, compared with Application Example 4, only contains the corresponding acrylic acid (ester) copolymer and stearalkonium hectorite, and the SPF value is reduced by 10.6%. Application Example 4, compared with Application Example 4, only contains the corresponding trimethylsiloxysilicate, and the SPF value is reduced by 24.5%. Application Example 5, compared with Application Example 4, replaces the trimethylsiloxysilicate in the film-forming agent composition with a corresponding content of hydrogenated polycyclopentadiene, and the SPF value is reduced by 6.4%.

[0149] Compared with the comparative example 2 without adding the film-forming agent composition, the SPF of the application example 5 is increased by 52.5%.

[0150] Compared with Application Example 2 without adding a film-forming agent composition, Application Example 6 has an SPF value increased by 54.1%; Compared with Application Example 6, Application Comparative Example 6 only contains the corresponding acrylic (ester) copolymer in the film-forming agent composition, and the SPF value is reduced by 14.9%.

[0151] Compared with Application Example 2 without adding a film-forming agent composition, Application Example 7 has an SPF value increased by 67.2%; Compared with Application Example 7, Application Comparative Example 7, which only contains the corresponding poly C10-30 alkanol acrylate in the film-forming agent composition, has an SPF value reduced by 27.5%.

[0152] Compared with the comparative example 2 without adding the film-forming agent composition, the SPF of the application example 8 is increased by 73.8%.

[0153] Test Example 3

[0154] (1) Use a 1 mL disposable syringe to draw the sample to be tested and apply it evenly on the PMMA plate. The application amount is 1.3 mg / cm 2 ; Place it horizontally in a place without direct light at room temperature for equilibrium drying for 15 minutes, then use the LabsphereUV2000S instrument to test the transmittance of the sunscreen sample in the 290-400nm ultraviolet band, and use the instrument software to analyze the results and calculate the SPF.

[0155] (2) Place the substrate with the sample in an electric constant temperature oscillating water bath at 25°C and an oscillation frequency of 50 times / min for 40 minutes, shake off the water droplets, maintain constant temperature and humidity, dry, and then test the SPF. Compare the changes in the sun protection index before and after the water bath.

[0156] The results are shown in Table 7.

[0157] Table 7

[0158]

[0159]

[0160] From the results in Table 7, it can be seen that the SPF value of the sunscreen cream prepared by the film-forming agent composition of the present invention after water bathing is increased by 3.2%-18.0% compared with that before water bathing, that is, the sunscreen effect is improved after contacting with water. Compared with the application examples 1-8, the SPF values ​​of the comparative examples 1-7 after water bathing are all reduced to varying degrees compared with those before water bathing, and there is no effect of increasing the SPF value after contacting with water.

[0161] Combined with the results in Table 6 above, it is shown that the components of the film-forming agent composition of the present invention have a synergistic effect, which can effectively improve the SPF value and water resistance, and the SPF value can be further improved after contacting water.

[0162] Test Example 4

[0163] The tested sunscreen samples were charged at 1.3 mg / cm 2 Spread the amount of coating on the test substrate, place it horizontally at room temperature without direct light and dry it for 15 minutes, then use Labsphere UV2000S instrument to detect and calculate the SPF value as the baseline SPF value (SPF BEF). Apply a 200-gram weight pressure on the cylindrical device (3 cm long, 1.5 cm in diameter), then roll the cylinder to the left and right once on the tested sunscreen sample film to simulate the friction process, and finally test the SPF value of the sunscreen sample film after friction (SPF AFT). Calculate the equivalent film thickness residual rate:

[0164] Equivalent film thickness residual rate = (Lg (SPF AFT) / Lg (SPF BEF)) * 100%.

[0165] The results are shown in Table 8.

[0166] Table 8

[0167] sample Equivalent film thickness residual rate after friction (%) Application Example 2 90.2 Application Example 4 86.1 Application Example 7 88.5 Application Comparative Example 1 73.1 Application Comparative Example 4 78.2 Application Comparative Example 6 68.4 Application Comparative Example 7 76.6

[0168] Application Example 2 contains a film-forming composition of acrylic acid (ester) copolymer, stearalkonium hectorite, and poly C10-30 alkyl acrylate, Application Example 4 contains a film-forming composition of acrylic acid (ester) copolymer, stearalkonium hectorite, and trimethylsiloxy silicate, Application Example 7 contains a film-forming composition of acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxy silicate, and poly C10-30 alkyl acrylate, Application Comparative Examples 1, 4, 6, and 7 contain only stearalkonium hectorite, trimethylsiloxy silicate, acrylic acid (ester) copolymer, and poly C10-30 alkyl acrylate in the film-forming composition, respectively, and the equivalent film thickness residual rate after friction is significantly lower than that of Application Examples 2, 4, and 7. This indicates that the film-forming composition of the present invention has the effect of improving the friction resistance of sunscreen cosmetics.

[0169] Test Example 5

[0170] 10 female volunteers aged 25 to 35 who met the test requirements were selected for skin feel test evaluation. After using the test samples, the skin feel was evaluated and the average of the evaluation results was calculated.

[0171] Test scoring rules: 5 points. Score according to the stickiness of the sample when applied: 5 points - very sticky; 4 points - sticky; 3 points - a little sticky; 2 points - basically not sticky; 1 point - not sticky at all (the minimum scoring interval is 0.5 points).

[0172] The results are shown in Table 9.

[0173] Table 9

[0174] sample Sticky feeling Application Example 1 2.05 Application Example 2 1.65 Application Example 3 1.95 Application Example 4 1.50 Application Example 5 1.40 Application Example 6 1.25 Application Example 7 1.15 Application Example 8 1.25

[0175] After testing, the sunscreen cream of the present invention has a refreshing and non-greasy feel on the skin.

[0176] The embodiments of the present invention are described in detail above in conjunction with the embodiments, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the relevant technical field without departing from the purpose of the present invention.

Claims

1. A film-forming agent composition, characterized in that include: Acrylic acid (ester) copolymer, stearalkonium hectorite and film-forming synergist; The film-forming synergist includes at least one of trimethylsiloxysilicate and poly C10-30 alkyl acrylate.

2. The film-forming agent composition according to claim 1, characterized in that The mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.005-7.5): (0-30): (0-25); Preferably, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.005-3.5): (0-15): (0-25); Preferably, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.08-3.2): (0.1-13): (0-1.5).

3. The film-forming agent composition according to claim 1, characterized in that The mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly C10-30 alkyl acrylate is 1: (0.08-0.5): (0.5-1.2): (0.5-1.2); Or, the mass ratio of the acrylic acid (ester) copolymer, stearalkonium hectorite, trimethylsiloxysilicate, and poly (C10-30 alkyl acrylate) is 1:(2.8-3.2):(11-13):

0.

4. The method for preparing the film-forming agent composition according to any one of claims 1 to 3, characterized in that: The following steps are involved: The acrylic acid (ester) copolymer, stearalkonium hectorite and a film-forming synergist are mixed to obtain the film-forming agent composition.

5. Use of the film-forming agent composition according to any one of claims 1 to 3 in the preparation of sunscreen cosmetics.

6. A sunscreen cosmetic, characterized in that: include: The film-forming agent composition according to any one of claims 1 to 3.

7. The sunscreen cosmetic according to claim 6, characterized in that: The mass percentage of the film-forming agent composition in the sunscreen cosmetic is 0.3% to 18%.

8. The sunscreen cosmetic according to claim 6, characterized in that: The sunscreen cosmetic further comprises a sunscreen agent and auxiliary materials acceptable in the cosmetics field.

9. The sunscreen cosmetic according to claim 8, characterized in that: The sunscreen agent includes a combination of at least two of titanium dioxide, zinc oxide, ethylhexyl methoxycinnamate, isoamyl p-methoxycinnamate, bis-ethylhexyloxyphenol methoxyphenyl triazine, diethylaminohydroxybenzoyl hexyl benzoate, diethylhexyl butyramido triazone, ethylhexyl triazone, phenylbenzimidazole sulfonic acid, methylene bis-benzotriazolyl tetramethylbutylphenol, butyl methoxydibenzoylmethane, polysilicone-15, octocrylene, homosalate, ethylhexyl salicylate, disodium phenyl dibenzimidazole tetrasulfonate, terephthalylidene dicamphor sulfonic acid, and drometrizole trisiloxane; And / or, the auxiliary materials include at least one of an emulsifier, a moisturizing oil, a skin feel regulator, a polyol and an additive.

10. The sunscreen cosmetic according to claim 6, characterized in that: The dosage form of the sunscreen cosmetic is selected from cream, mousse, gel, emulsion or spray.

Citation Information

Patent Citations

  • Rapid-film-forming durable anti-rubbing type high-power sunscreen liquid and preparation method thereof

    CN117643549A

Cited By

  • Permeation blocking composition for reducing transdermal penetration of sunscreen

    CN120267560A