Low noise amplifier and preparation method thereof
By depositing the second polysilicon gate on the polysilicon gate of the low-noise amplifier and forming a thick metal silicide layer, the problem of large gate resistance is solved, performance is improved and device reliability is ensured.
Patent Information
- Application Number
- CN202410958883.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-15
AI Technical Summary
The gate resistance of existing low-noise amplifiers is large, which affects its performance. The traditional method of reducing gate resistance has high requirements and is difficult to control, making it easy to damage the active area.
By depositing a second polysilicon gate on the polysilicon gate, it is higher than the side wall structure, and forming a thicker metal silicide layer in the self-aligning silicide process, increasing the on-resistance and reducing the polysilicon Gate resistance while avoiding affecting the conduction of the active region.
It effectively reduces the gate resistance of the low-noise amplifier, improves performance, and ensures the reliability of the device, avoiding the leakage increase problem caused by the metal silicide layer on the source and drain regions surfaces penetrating the PN junction.
Smart Images

Figure CN118969616A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor manufacturing technology, and in particular to a low noise amplifier and a method for preparing the same. Background Art
[0002] The core performance of a low noise amplifier (LNA) includes parameters such as cutoff frequency Ft, transconductance and gain Gm&Gain, and minimum noise factor NFmin. The calculation formula of the minimum noise factor NFmin is: It can be seen that the minimum noise factor NFmin is proportional to the gate resistance Rg, where ω is the transistor vibration frequency, T is the temperature, and γ int is the thermal noise, g ds0 is the conductance when Vds = 0. Further, the gate resistance Rg is usually the parallel resistance of the resistance of the polysilicon gate and the on-resistance of the metal silicide, wherein the resistance of the polysilicon gate with a smaller resistance value is dominant.
[0003] Reducing the gate resistance Rg of a single low noise amplifier LNA tube is very beneficial to reducing the minimum noise factor Nfmin and thus improving the performance of the LNA.
[0004] At present, a traditional method for reducing the gate resistance Rg of a single LNA tube is to expose the top of the polysilicon gate by etching a certain thickness of the side wall (Spacer) on the side of the polysilicon gate, so that the metal silicide layer on the top of the polysilicon gate prepared by the subsequent self-aligned silicide process is thicker, thereby appropriately reducing the resistance Rg. However, this method has high requirements for the etching process, the exposed top morphology of the polysilicon gate is difficult to control, and it is easy to damage the active area. Summary of the invention
[0005] The present application provides a low noise amplifier and a preparation method thereof, which can solve the problem that the gate resistance Rg of the noise amplifier LNA is too large and affects the performance of the LNA.
[0006] On the one hand, an embodiment of the present application provides a method for preparing a low noise amplifier, comprising:
[0007] A semiconductor structure is provided, the semiconductor structure at least comprising: a substrate, a well region, a source region, a drain region, a first polysilicon gate and a sidewall structure, the well region is located in the substrate, the source region and the drain region are spaced apart in the well region, the first polysilicon gate is located on the substrate between the source region and the drain region, and the sidewall structure is located on both sides of the first polysilicon gate;
[0008] forming a hard mask layer, wherein the hard mask layer covers the substrate surface, the sidewall structure and the first polysilicon gate;
[0009] Etching the hard mask layer on the first polysilicon gate to expose the first polysilicon gate;
[0010] Depositing a second polysilicon gate on the first polysilicon gate by a selective epitaxial process, wherein the upper surface of the second polysilicon gate exceeds the top of the sidewall structure by a certain height;
[0011] etching the hard mask layer on the substrate; and
[0012] A metal silicide layer is formed on the first polysilicon gate, the surface of the source region and the surface of the drain region through a self-aligned silicide process, wherein the thickness of the metal silicide layer on the first polysilicon gate is greater than the thickness of the metal silicide layer on the source region and the drain region.
[0013] Optionally, in the method for preparing the low noise amplifier, the step of forming a metal silicide layer on the first polysilicon gate, the surface of the source region and the surface of the drain region by a self-aligned silicide process includes:
[0014] Depositing a metal material on the surface of the second polysilicon gate, the surface of the source region, and the surface of the drain region, the metal material reacts with the second polysilicon gate, the source region, and the drain region respectively;
[0015] A high temperature annealing process is performed on the semiconductor structure after the metal material is deposited.
[0016] Optionally, in the method for preparing the low noise amplifier, a certain thickness of the second polysilicon gate is consumed during the process of forming the metal silicide layer.
[0017] Optionally, in the method for preparing the low noise amplifier, the thickness of the metal silicide layer is
[0018]
[0019] Optionally, in the method for preparing the low noise amplifier, in the process of depositing the second polysilicon gate on the first polysilicon gate through a selective epitaxial process, the flow rate of the silicon source gas introduced is 10sccm~100sccm, and the process temperature is 500℃~1200℃.
[0020] Optionally, in the method for preparing the low noise amplifier, the thickness of the second polysilicon gate is
[0021] Optionally, in the method for preparing the low noise amplifier, the upper surface of the first polysilicon gate is flush with the top of the sidewall structure.
[0022] Optionally, in the method for preparing the low noise amplifier, after etching the hard mask layer on the substrate and before forming a metal silicide layer on the first polysilicon gate, the surface of the source region and the surface of the drain region by a self-aligned silicide process, the method for preparing the low noise amplifier further includes:
[0023] The semiconductor structure is pre-cleaned by a wet cleaning process after etching the hard mask layer on the substrate.
[0024] Optionally, in the method for preparing the low noise amplifier, the step of forming a hard mask layer includes:
[0025] forming a silicon oxide layer, wherein the silicon oxide layer covers the substrate surface, the sidewall structure and the first polysilicon gate;
[0026] A silicon nitride layer is formed, wherein the silicon nitride layer covers the silicon oxide layer.
[0027] On the other hand, an embodiment of the present application further provides a low noise amplifier, including:
[0028] A substrate, a well region, a source region, a drain region, a first polysilicon gate and a sidewall structure, wherein the well region is located in the substrate, the source region and the drain region are spaced apart in the well region, the first polysilicon gate is located on the substrate between the source region and the drain region, and the sidewall structure is located on both sides of the first polysilicon gate;
[0029] A metal silicide layer, wherein the metal silicide layer is located on the first polysilicon gate, on the surface of the source region and on the surface of the drain region, wherein the metal silicide layer on the first polysilicon gate exceeds a certain height from the top of the sidewall structure, and the thickness of the metal silicide layer on the first polysilicon gate is greater than the thickness of the metal silicide layer on the source region and the drain region.
[0030] The technical solution of this application has at least the following advantages:
[0031] After preparing the first polysilicon gate, the present application continues to prepare the second polysilicon gate on the first polysilicon gate through a selective epitaxial process, so that the second polysilicon gate is higher than the sidewall structure, exposing more polysilicon gate (second polysilicon gate) material, so that a thicker metal silicide layer is subsequently prepared on top of the first polysilicon gate through a self-aligned silicide process, thereby increasing the on-resistance of the metal silicide and reducing the resistance of the polysilicon gate, thereby reducing the gate resistance of the low-noise amplifier and improving the performance of the low-noise amplifier.
[0032] Furthermore, the present application prepares the second polysilicon gate through a selective epitaxial process to make it higher than the sidewall structure, exposing more polysilicon gate material. In the subsequent self-aligned silicide process, only the metal silicide layer on the top of the first polysilicon gate will be thickened, and the metal silicide layer on the surface of the source region and the drain region will not be thickened, that is, only the gate resistance of the device will be reduced, and the on-resistance of the active area will not be affected, thereby avoiding the situation where the metal silicide layer on the surface of the source region and the drain region penetrates the PN junction and causes an increase in leakage, thereby ensuring the reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0034] Figure 1 is a flow chart of a method for preparing a low noise amplifier according to an embodiment of the present invention;
[0035] Figure 2-Figure 7 is a schematic diagram of a semiconductor structure in each process step of preparing a low noise amplifier according to an embodiment of the present invention;
[0036] The reference numerals are described as follows:
[0037] 10-substrate, 11-well region, 12-source region, 13-drain region, 14-lightly doped drain region, 20-gate oxide layer, 30-first polysilicon gate, 40-sidewall structure, 41-sidewall one, 42-sidewall two, 50-hard mask layer, 60-second polysilicon gate, 70-metal silicide layer. DETAILED DESCRIPTION
[0038] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0039] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0040] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0041] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0042] The present invention provides a method for preparing a low noise amplifier. Figure 1 , Figure 1 : is a flow chart of a method for preparing a low noise amplifier according to an embodiment of the present invention, wherein the method for preparing the low noise amplifier comprises:
[0043] Step S1: providing a semiconductor structure, the semiconductor structure at least comprising: a substrate, a well region, a source region, a drain region, a first polysilicon gate and a sidewall structure, the well region is located in the substrate, the source region and the drain region are spaced apart in the well region, the first polysilicon gate is located on the substrate between the source region and the drain region, and the sidewall structure is located on both sides of the first polysilicon gate;
[0044] Step S2: forming a hard mask layer, wherein the hard mask layer covers the substrate surface, the sidewall structure and the first polysilicon gate;
[0045] Step S3: etching the hard mask layer on the first polysilicon gate to expose the first polysilicon gate;
[0046] Step S4: depositing a second polysilicon gate on the first polysilicon gate by a selective epitaxial process, wherein the upper surface of the second polysilicon gate exceeds the top of the sidewall structure by a certain height;
[0047] Step S5: etching the hard mask layer on the substrate; and
[0048] Step S6: Forming a metal silicide layer on the first polysilicon gate, the surface of the source region and the surface of the drain region through a self-aligned silicide process, wherein the thickness of the metal silicide layer on the first polysilicon gate is greater than the thickness of the metal silicide layer on the source region and the drain region.
[0049] Specifically, refer to Figure 2-Figure 7 , Figure 2-Figure 7 It is a schematic diagram of the semiconductor structure in each process step of preparing a low noise amplifier according to an embodiment of the present invention.
[0050] First, perform step S1: refer to Figure 2 , Figure 2 It is a schematic diagram of a semiconductor structure after forming film layers such as a substrate, a well region, a source region, a drain region, a first polysilicon gate and a sidewall structure according to an embodiment of the present application. A semiconductor structure is provided, and the semiconductor structure at least includes: a substrate 10, a well region 11, a source region 12, a drain region 13, a first polysilicon gate 30 and a sidewall structure 40, the well region 11 is located in the substrate 10, the source region 12 and the drain region 13 are spaced apart in the well region 11, the first polysilicon gate 30 is located on the substrate 10 between the source region 12 and the drain region 14, and the sidewall structure 40 is located on both sides of the first polysilicon gate 30.
[0051] Preferably, before executing step S2, the manufacturing process of the low noise amplifier may further include the steps of: forming a gate oxide layer 20 and a plurality of lightly doped drain regions 14. The gate oxide layer 20 is located between the substrate 10 and the first polysilicon gate 30, and the process of preparing the gate oxide layer 20 is before the process of preparing the first polysilicon gate 30; the plurality of lightly doped drain regions 14 are located in the well region 11 between the source region 12 and the drain region 14, and the process of preparing the lightly doped drain region 14 may be before the process of preparing the sidewall structure 40.
[0052] In this embodiment, the sidewall structure 40 may include: an L-shaped sidewall 1 41 and a fan-shaped sidewall 2 42. The sidewall 1 41 may be made of silicon dioxide, and the sidewall 2 42 may be made of silicon nitride.
[0053] Preferably, the upper surface of the first polysilicon gate 30 is flush with the top of the spacer structure 40 .
[0054] Furthermore, after forming the sidewall structure 40, the preparation process of the low noise amplifier may also include: a step of forming an ion heavily doped region (not shown) on the surface of the source region 12 and the drain region 13, the ion heavily doped region on the surface of the source region 12 serving as the source of the device, and the ion heavily doped region on the surface of the drain region 13 serving as the drain of the device.
[0055] In this embodiment, the conductivity type of the doped ions in the well region 11 is P type; the conductivity type of the doped ions in the source region 12 and the drain region 14 is N type; the conductivity type of the doped ions in the lightly doped drain region 14 is N type; the conductivity type of the doped ions in the heavily doped ion region on the surface of the source region 12 is N type (N+); the conductivity type of the doped ions in the heavily doped ion region on the surface of the drain region 13 is N type (N+).
[0056] Then, execute step S2: refer to Figure 3 , Figure 3 It is a schematic diagram of the semiconductor structure after forming a hard mask layer according to an embodiment of the present application, wherein a hard mask layer 50 is formed, and the hard mask layer 50 covers the surface of the substrate 10 (the source region 12 and the drain region 14 ), the sidewall structure 40 and the first polysilicon gate 30 .
[0057] Preferably, the step of forming the hard mask layer 50 may specifically include:
[0058] S2.1: forming a silicon oxide layer, wherein the silicon oxide layer covers the surface of the substrate 10, the sidewall structure 40 and the first polysilicon gate 30;
[0059] S2.2: forming a silicon nitride layer, wherein the silicon nitride layer covers the silicon oxide layer.
[0060] Next, execute step S3: refer to Figure 4 , Figure 4 This is a schematic diagram of the semiconductor structure after etching the hard mask layer on the first polysilicon gate according to an embodiment of the present application. Using the patterned first photoresist layer as a mask (not shown), a dry etching process is adopted to etch the hard mask layer 50 on the first polysilicon gate 30 to expose the first polysilicon gate 30.
[0061] Further, step S4 is performed: refer to Figure 5 , Figure 5 It is a schematic diagram of the semiconductor structure after the second polysilicon gate is formed in an embodiment of the present application. Through a selective epitaxial process, a second polysilicon gate 60 is deposited on the first polysilicon gate 30, and the upper surface of the second polysilicon gate 60 exceeds the top of the sidewall structure 40 by a certain height.
[0062] In the present application, the first polysilicon gate 30 and the second polysilicon gate 60 together constitute the gate of a low noise amplifier (transistor).
[0063] Preferably, in the process of depositing the second polysilicon gate 60 on the first polysilicon gate 30 by the selective epitaxial process, the flow rate of the introduced silicon source gas is 10 sccm-100 sccm, and the process temperature is 500° C.-1200° C.
[0064] Preferably, the thickness of the second polysilicon gate 60 is
[0065] Next, execute step S5: refer to Figure 6 , Figure 6 It is a schematic diagram of a semiconductor structure after etching the hard mask layer on the substrate according to an embodiment of the present application, wherein the hard mask layer 50 on the surface of the substrate 10 (the source region 12 and the drain region 14) is etched.
[0066] Furthermore, after etching the hard mask layer on the substrate and before forming a metal silicide layer on the first polysilicon gate, the surface of the source region and the surface of the drain region by a self-aligned silicide process, the method for preparing the low noise amplifier may further include: performing a pre-cleaning treatment on the semiconductor structure after etching the hard mask layer on the substrate by a wet cleaning process to remove Figure 6 The natural oxide layer on the surface of the semiconductor structure shown provides a second polysilicon gate surface not covered by the natural oxide layer and the surfaces of the source region 12 and the drain region 14 not covered by the natural oxide layer for preparing the metal silicide layer in step S6.
[0067] In this embodiment, an HF solution may be used to perform a pre-cleaning treatment on the semiconductor structure after etching the hard mask layer on the substrate.
[0068] Finally, execute step S6: reference Figure 7 , Figure 7 1 is a schematic diagram of a semiconductor structure after a metal silicide layer is formed in an embodiment of the present application. A metal silicide layer 70 is formed on the first polysilicon gate 30, on the surface of the source region 12, and on the surface of the drain region 13 through a self-aligned silicide process, wherein the thickness of the metal silicide layer 70 on the first polysilicon gate 30 is greater than the thickness of the metal silicide layer 60 on the source region 12 and the drain region 13.
[0069] Preferably, the step of forming the metal silicide layer 70 on the first polysilicon gate 30, the surface of the source region 12 and the surface of the drain region 13 by a self-aligned silicide process may specifically include:
[0070] Step S6.1: by depositing a refractory metal material on the surface of the second polysilicon gate 60, the surface of the source region and the surface of the drain region, the refractory metal material reacts with the second polysilicon gate 60, the source region on the substrate surface and the drain region on the substrate surface respectively. In this embodiment, the refractory metal material includes: a stacked NiPt layer and a TiN layer;
[0071] Step S6.2: performing a first high-temperature annealing process on the semiconductor structure after the refractory metal material is deposited, so as to form an initial metal silicide layer on the first polysilicon gate 30, the surface of the source region 12 and the surface of the drain region 13, the process temperature is 300°C, and the duration is 25s; wherein the NiPt layer in the refractory metal material reacts with the second polysilicon gate 60 to generate an initial metal silicide layer TiSi2; similarly, the NiPt layer in the refractory metal material reacts with the source region of a portion of the thickness of the substrate surface to generate an initial metal silicide layer TiSi2, and the NiPt layer in the refractory metal material reacts with the drain region of a portion of the thickness of the substrate surface to generate an initial metal silicide layer TiSi2;
[0072] Step S6.3: using the SPM solution and the SC1 solution to clean the semiconductor structure after the first high temperature annealing process;
[0073] Step S6.4: performing a second high temperature annealing process on the semiconductor structure after the cleaning process, with a process temperature of 410° C. and a duration of 30 seconds, to transform the initial metal silicide layer TiSi2 into TiSi.
[0074] It is worth noting that in the process of forming the metal silicide layer 70, during the first high-temperature annealing process, the refractory metal material reacts with the second polysilicon gate 60 to generate TiSi2. Similarly, the NiPt layer in the refractory metal material reacts with the source region of the substrate surface with a thickness of part and generates an initial metal silicide layer TiSi2; the NiPt layer in the refractory metal material reacts with the drain region of the substrate surface with a thickness of part and generates an initial metal silicide layer TiSi2. During the second high-temperature annealing, TiSi2 is transformed into TiSi, so the final metal silicide layer 70 includes from bottom to top: TiSi, TiN layer. Further, in this embodiment, the second polysilicon gate 60 is completely reacted and consumed in step S6, so the final metal silicide layer 70 covers the first polysilicon gate 30. Among them, the metal silicide layer 70 has a high resistivity.
[0075] Based on the material properties of the second polysilicon gate 60, the second polysilicon gate 60 reacts with NiPt faster, and the second polysilicon gate 60 is located at a higher position (at the top of the first polysilicon gate 30), and the metal silicide generation reaction is more complete. Therefore, the thickness of the metal silicide layer 70 finally generated by the reaction on the first polysilicon gate 30 will be greater than the thickness of the metal silicide layer 70 generated by the reaction on the source region 12 and the drain region 13.
[0076] Preferably, the thickness of the metal silicide layer 70 on the first polysilicon gate 30 is The thickness of the metal silicide layer 70 on the source region 12 and the drain region 13 is
[0077] In the present application, after preparing the first polysilicon gate, the second polysilicon gate is continuously prepared on the first polysilicon gate by a selective epitaxial process, so that the second polysilicon gate is higher than the sidewall structure, and more polysilicon gate (second polysilicon gate) material is exposed, so that a thicker metal silicide layer is subsequently prepared on the top of the first polysilicon gate by a self-aligned silicide process, increasing the on-resistance of the metal silicide and reducing the resistance of the polysilicon gate, thereby reducing the gate resistance of the low-noise amplifier and improving the performance of the low-noise amplifier. Further, the present application prepares the second polysilicon gate by a selective epitaxial process so that it is higher than the sidewall structure, exposing more polysilicon gate material. In the subsequent self-aligned silicide process, only the metal silicide layer on the top of the first polysilicon gate is thickened, and the metal silicide layer on the surface of the source region and the drain region is not thickened, that is, only the gate resistance of the device is reduced, and the on-resistance of the active region is not affected, and the metal silicide layer on the surface of the source region and the drain region is prevented from penetrating the PN junction to increase the leakage, thereby ensuring the reliability of the device.
[0078] Based on the same inventive concept, the present application also provides a low noise amplifier, referring to Figure 7 , the low noise amplifier comprises:
[0079] A substrate 10, a well region 11, a source region 12, a drain region 13, a first polysilicon gate 30 and a sidewall structure 40, wherein the well region 11 is located in the substrate 10, the source region 12 and the drain region 13 are arranged in the well region 11 at intervals, the first polysilicon gate 30 is located on the substrate 10 between the source region 12 and the drain region 13, and the sidewall structure 40 is located on both sides of the first polysilicon gate 30;
[0080] A metal silicide layer 70, wherein the metal silicide layer 70 is located on the first polysilicon gate 30, on the surface of the source region 12, and on the surface of the drain region 13, wherein the metal silicide layer 70 located on the first polysilicon gate 30 exceeds a certain height from the top of the sidewall structure 40, and the thickness of the metal silicide layer 70 on the first polysilicon gate 30 is greater than the thickness of the metal silicide layer 70 on the source region 12 and the drain region 13.
[0081] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.
Claims
1. A method for preparing a low noise amplifier, characterized in that: include: A semiconductor structure is provided, the semiconductor structure at least comprising: a substrate, a well region, a source region, a drain region, a first polysilicon gate and a sidewall structure, the well region is located in the substrate, the source region and the drain region are spaced apart in the well region, the first polysilicon gate is located on the substrate between the source region and the drain region, and the sidewall structure is located on both sides of the first polysilicon gate; forming a hard mask layer, wherein the hard mask layer covers the substrate surface, the sidewall structure and the first polysilicon gate; Etching the hard mask layer on the first polysilicon gate to expose the first polysilicon gate; Depositing a second polysilicon gate on the first polysilicon gate by a selective epitaxial process, wherein the upper surface of the second polysilicon gate exceeds the top of the sidewall structure by a certain height; etching the hard mask layer on the substrate; and A metal silicide layer is formed on the first polysilicon gate, the surface of the source region and the surface of the drain region through a self-aligned silicide process, wherein the thickness of the metal silicide layer on the first polysilicon gate is greater than the thickness of the metal silicide layer on the source region and the drain region.
2. The method for preparing a low noise amplifier according to claim 1, characterized in that: The step of forming a metal silicide layer on the first polysilicon gate, the surface of the source region and the surface of the drain region by a self-aligned silicide process comprises: Depositing a metal material on the surface of the second polysilicon gate, the surface of the source region, and the surface of the drain region, the metal material reacts with the second polysilicon gate, the source region, and the drain region respectively; A high temperature annealing process is performed on the semiconductor structure after the metal material is deposited.
3. The method for preparing a low noise amplifier according to claim 1, characterized in that: In the process of forming the metal silicide layer, a certain thickness of the second polysilicon gate is consumed.
4. The method for preparing a low noise amplifier according to claim 1, characterized in that: The thickness of the metal silicide layer is 5. The method for preparing a low noise amplifier according to claim 1, characterized in that: In the process of depositing the second polysilicon gate on the first polysilicon gate by the selective epitaxial process, the flow rate of the introduced silicon source gas is 10 sccm-100 sccm, and the process temperature is 500°C-1200°C.
6. The method for preparing a low noise amplifier according to claim 1, characterized in that: The thickness of the second polysilicon gate is 7. The method for preparing a low noise amplifier according to claim 1, characterized in that: The upper surface of the first polysilicon gate is flush with the top of the sidewall structure.
8. The method for preparing a low noise amplifier according to claim 1, characterized in that: After etching the hard mask layer on the substrate and before forming a metal silicide layer on the first polysilicon gate, the surface of the source region and the surface of the drain region by a self-aligned silicide process, the method for preparing the low noise amplifier further includes: The semiconductor structure is pre-cleaned by a wet cleaning process after etching the hard mask layer on the substrate.
9. The method for preparing a low noise amplifier according to claim 1, characterized in that: The steps of forming the hard mask layer include: forming a silicon oxide layer, wherein the silicon oxide layer covers the substrate surface, the sidewall structure and the first polysilicon gate; A silicon nitride layer is formed, wherein the silicon nitride layer covers the silicon oxide layer.
10. A low noise amplifier, characterized in that: include: A substrate, a well region, a source region, a drain region, a first polysilicon gate and a sidewall structure, wherein the well region is located in the substrate, the source region and the drain region are spaced apart in the well region, the first polysilicon gate is located on the substrate between the source region and the drain region, and the sidewall structure is located on both sides of the first polysilicon gate; A metal silicide layer, wherein the metal silicide layer is located on the first polysilicon gate, on the surface of the source region and on the surface of the drain region, wherein the metal silicide layer on the first polysilicon gate exceeds a certain height from the top of the sidewall structure, and the thickness of the metal silicide layer on the first polysilicon gate is greater than the thickness of the metal silicide layer on the source region and the drain region.