Sodium-cooled fast reactor tin-bismuth alloy filling method

Through the combination of heating device and injection tube, the precise filling and filling of sodium-cooled fast-load tin bismuth alloy is achieved, solving the problem of filling and filling quality control, and improving sealing performance and safety.

CN118989281APending Publication Date: 2024-11-22CFHI DALIAN HYDROGENANT REACTOR +1
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202411089291.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing sodium-cooled fast reactor tin bismuth alloy filling process is difficult to control the filling quality, resulting in poor sealing performance and gas leakage problems, affecting the safe operation of the nuclear reactor.

Method used

The combination of heating device and injection tube is adopted to melt the tin bismuth alloy through the heating device and stably inject it into the alloy tank through the injection tube, achieving precise control and stability of the filling process and ensuring sealing performance.

Benefits of technology

It improves the filling efficiency and quality, improves the stability and reliability of the processing technology, and ensures the safe operation of the sodium-cooled fast reactor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118989281A_ABST
    Figure CN118989281A_ABST
Patent Text Reader

Abstract

The invention provides a sodium-cooled fast reactor tin-bismuth alloy filling method, and relates to the technical field of sodium-cooled fast reactors. The mode that the heating device and the injection pipe are matched is adopted, convenient filling of the sodium-cooled fast reactor tin-bismuth alloy is achieved, after the tin-bismuth alloy is heated and melted through the heating device, the tin-bismuth alloy is stably injected into the alloy groove through the injection pipe, accurate control and stability of the filling process are achieved, and the filling efficiency is improved. Therefore, the sealing performance of the sodium-cooled fast reactor can be improved, potential safety hazards such as gas leakage are effectively prevented, and the safe operation of the fast reactor is finally guaranteed. By means of the method, the filling efficiency and quality are improved, the stability and reliability of the machining technology are improved, and a powerful guarantee is provided for long-term safe operation of the fast reactor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of sodium-cooled fast reactors, and in particular to a method for filling a sodium-cooled fast reactor with tin-bismuth alloy. Background Art

[0002] With the replacement of domestic nuclear power products, the fourth generation of nuclear reactors represented by sodium-cooled fast reactors have gradually become the focus of development. Sodium-cooled fast reactors use liquid sodium metal as a coolant, and fast neutrons cause nuclear fission and maintain chain reactions. Rotating shield plugs (referred to as cocks) replace traditional top cover components to achieve support guidance, shielding, sealing, and motion positioning. The rotatable seals at the cock annular gap are mostly sealed with tin-bismuth alloys. As an important sealing medium, tin-bismuth alloy is in a solidified state when the whole reactor is in operation and in a molten state when the material is replaced. Therefore, the filling quality of tin-bismuth alloy has an important influence on the sealing performance of sodium-cooled fast reactors.

[0003] At present, the filling of tin-bismuth alloy generally adopts the process of melting, stirring and pouring outside the reactor, that is, the tin-bismuth alloy is melted and poured into the alloy tank of the sodium-cooled fast reactor. However, when pouring the molten tin-bismuth alloy into the alloy tank, it may be affected by factors such as pouring speed and force, resulting in fluctuations in the filling quality, making it difficult to control the filling quality, and environmental factors may also affect the precise control of the filling process, thereby leading to problems such as poor sealing performance of the fast reactor or gas leakage, affecting the safe operation of the sodium-cooled fast reactor. Summary of the invention

[0004] The problem to be solved by the present invention is how to conveniently fill the tin-bismuth alloy and ensure good sealing performance of the tin-bismuth alloy.

[0005] In order to solve the above problems, the present invention provides a sodium-cooled fast reactor tin-bismuth alloy filling method, based on a sodium-cooled fast reactor tin-bismuth alloy filling device, the device comprises a heating device and an injection pipe, one end of the injection pipe is connected to the heating device, and the other end is used to extend into the alloy tank of the sodium-cooled fast reactor;

[0006] When it is necessary to inject tin-bismuth alloy into the alloy tank, the method comprises:

[0007] placing a tin-bismuth alloy block in the heating device and sealing the heating device;

[0008] Turning on the heating device to heat and melt the tin-bismuth alloy block into a liquid tin-bismuth alloy;

[0009] When the injection condition is met, the liquid tin-bismuth alloy is injected into the alloy tank using the injection pipe.

[0010] Optionally, placing the tin-bismuth alloy block in the heating device comprises:

[0011] Obtaining a placement plan for the tin-bismuth alloy blocks according to the size of the tin-bismuth alloy blocks, the size of the inner wall of the heating device, and the mass of the tin-bismuth alloy to be filled;

[0012] The tin-bismuth alloy blocks are stacked in the heating device according to the placement plan.

[0013] Optionally, the injection conditions include: the outlet temperature of the heating device, the temperature of the injection pipe and the temperature of the alloy tank reach respective first target values, and the alloy tank is under inert gas protection.

[0014] Optionally, the device further comprises: a first stop valve, a second stop valve and a vent valve, wherein the first stop valve is arranged on the injection pipe and is used to connect the heating device and the alloy tank, the second stop valve and the vent valve are both arranged on the heating device, the second stop valve is used to connect the heating device and the inert gas pipeline, and the vent valve is used to connect the heating device and the outside air;

[0015] The step of injecting the liquid tin-bismuth alloy into the alloy tank by using the injection pipe comprises:

[0016] The second stop valve is opened, the vent valve is closed, the outlet pressure of the inert gas pipeline is adjusted, and when the internal pressure of the heating device reaches the first target pressure, the first stop valve is opened.

[0017] Optionally, the step of injecting the liquid tin-bismuth alloy into the alloy tank using the injection pipe further comprises:

[0018] The height of the liquid level in the alloy tank is obtained, and when the liquid level reaches a target height, the first stop valve, the heating device and the second stop valve are closed.

[0019] Optionally, before starting the heating device, the method further comprises:

[0020] The second stop valve and the vent valve are opened to purge the interior of the heating device with inert gas.

[0021] Optionally, when it is necessary to take out the tin-bismuth alloy from the alloy tank, the method includes:

[0022] Turning on the heater of the alloy tank to melt the tin-bismuth alloy in the alloy tank into liquid tin-bismuth alloy, and turning on the heating device at the same time;

[0023] When the extraction condition is met, the liquid tin-bismuth alloy in the alloy tank is extracted into the heating device using the injection pipe.

[0024] Optionally, the device further comprises a third stop valve, which is arranged on the heating device and is used to connect the heating device with the vacuum pump;

[0025] The extraction conditions include: the outlet temperature of the heating device, the injection pipe temperature and the alloy tank temperature have reached their respective second target values, and the third stop valve has been opened.

[0026] Optionally, the step of extracting the liquid tin-bismuth alloy in the alloy tank into the heating device by using the injection pipe comprises:

[0027] The power supply of the vacuum pump is turned on, and when the internal pressure of the heating device reaches the second target pressure, the first stop valve is opened.

[0028] Optionally, the device further comprises: an injection pipe heater, the injection pipe heater being at least partially disposed on the injection pipe;

[0029] Before injecting the liquid tin-bismuth alloy in the heating device into the alloy tank, and / or before extracting the liquid tin-bismuth alloy in the alloy tank into the heating device, the method further includes:

[0030] The injection pipe heater is turned on to heat the injection pipe.

[0031] The beneficial effects of the present invention are:

[0032] The present invention adopts a heating device and an injection tube to realize convenient filling of the sodium-cooled fast reactor tin-bismuth alloy. After the tin-bismuth alloy is heated and melted by the heating device, it is stably injected into the alloy tank through the injection tube, realizing precise control and stability of the filling process, thereby ensuring that the sealing performance of the sodium-cooled fast reactor is improved, effectively preventing safety hazards such as gas leakage, and ultimately ensuring the safe operation of the fast reactor. Through this method, not only the filling efficiency and quality are improved, but also the stability and reliability of the processing technology are improved, providing a strong guarantee for the long-term safe operation of the fast reactor. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 It is a schematic structural diagram of a tin-bismuth alloy filling device for a sodium-cooled fast reactor according to an embodiment of the present invention;

[0034] Figure 2 It is a partial schematic diagram of the alloy groove and the mechanical compression sealing structure in the embodiment of the present invention;

[0035] Figure 3 This is a schematic diagram of the installation position of the heating device in an embodiment of the present invention;

[0036] Figure 4 This is a schematic diagram of the height position of the alloy groove in an embodiment of the present invention;

[0037] Figure 5 Schematic diagram of the installation position of the small plug tin-bismuth alloy tank and the heating device in the embodiment of the present invention.

[0038] Description of reference numerals:

[0039] 1. Heating device; 2. Injection pipe; 3. First stop valve; 4. Second stop valve; 5. Vent valve; 6. Pressure gauge interface; 7. Pressure gauge; 8. Sealing cover; 9. Injection pipe heater; 10. Power supply of injection pipe heater; 11. Support seat; 12. Alloy groove; 13. Mechanical compression sealing structure; 14. Large plug; 15. Medium plug; 16. Small plug; 17. Large plug tin-bismuth alloy groove; 1701. Notch position of large plug tin-bismuth alloy groove; 1702. Bottom position of large plug tin-bismuth alloy groove; 18. Medium plug tin-bismuth alloy groove; 1801. Notch position of medium plug tin-bismuth alloy groove; 1802. Bottom position of medium plug tin-bismuth alloy groove; 19. Small plug tin-bismuth alloy groove 12; 1901. Notch position of small plug tin-bismuth alloy groove; 1902. Bottom position of small plug tin-bismuth alloy groove. DETAILED DESCRIPTION

[0040] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0041] A sodium-cooled fast reactor tin-bismuth alloy filling method according to an embodiment of the present invention is based on a sodium-cooled fast reactor tin-bismuth alloy filling device, the device comprising a heating device 1 and an injection pipe 2, one end of the injection pipe 2 is connected to the heating device 1, and the other end is used to extend into an alloy tank 12 of the sodium-cooled fast reactor;

[0042] When it is necessary to inject tin-bismuth alloy into the alloy tank 12, the method includes:

[0043] Placing a tin-bismuth alloy block in the heating device 1 and sealing the heating device 1;

[0044] Turning on the heating device 1 to heat and melt the tin-bismuth alloy block into a liquid tin-bismuth alloy;

[0045] When the injection condition is met, the liquid tin-bismuth alloy is injected into the alloy tank 12 using the injection pipe 2 .

[0046] This embodiment adopts the method of cooperating the heating device 1 and the injection tube 2 to realize the convenient filling of the sodium-cooled fast reactor tin-bismuth alloy. After the tin-bismuth alloy is heated and melted by the heating device 1, it is stably injected into the alloy tank 12 through the injection tube 2, realizing the precise control and stability of the filling process, so as to ensure that the sealing performance of the sodium-cooled fast reactor is improved, effectively prevent safety hazards such as gas leakage, and finally ensure the safe operation of the fast reactor. Through this method, not only the filling efficiency and quality are improved, but also the stability and reliability of the processing technology are improved, providing a strong guarantee for the long-term safe operation of the fast reactor.

[0047] Optionally, placing the tin-bismuth alloy block in the heating device 1 comprises:

[0048] Obtaining a placement plan for the tin-bismuth alloy blocks according to the size of the tin-bismuth alloy blocks, the size of the inner wall of the heating device 1 and the mass of the tin-bismuth alloy to be filled;

[0049] The tin-bismuth alloy blocks are stacked in the heating device 1 according to the placement plan.

[0050] The mass of the tin-bismuth alloy to be filled refers to the total amount of the tin-bismuth alloy to be filled, and the tin-bismuth alloy block is formed by melting and casting the tin alloy and the bismuth alloy according to a certain ratio. It can be understood that before carrying out this method, the tin-bismuth alloy block needs to be manufactured first.

[0051] In this optional embodiment, the placement of the tin-bismuth alloy blocks in the heating device 1 is first determined based on the size of the tin-bismuth alloy blocks, the size of the heating device 1, and the size of each tin-bismuth alloy block, so as to select the best placement method, such as even and compact placement, which can ensure that the tin-bismuth alloy blocks can be completely melted at one time, thereby improving the melting efficiency and reducing the cost. At the same time, placing the tin-bismuth alloy blocks in the heating device 1 according to the best placement scheme can effectively utilize the volume of the heating device 1, ensure heating uniformity, improve operating efficiency, and further improve the accuracy and stability of the tin-bismuth alloy filling process.

[0052] Optionally, the size of the tin-bismuth alloy block can be determined according to the size of the inner wall of the container of the heating device 1. For example, if the heating device 1 is a rectangular parallelepiped, the tin-bismuth alloy block is designed to be a rectangular parallelepiped structure. In this way, it can be ensured that the important tin-bismuth alloy block required can be melted all at once.

[0053] Optionally, the method further comprises: performing a chemical test on the manufactured tin-bismuth alloy block. The chemical test is used to determine the proportion, melting point, and solidification point of the tin-bismuth alloy, thereby determining the process parameters for melting the tin-bismuth alloy based on these parameters; the chemical test is also used to determine the density of the tin-bismuth alloy, thereby determining the required weight of the tin-bismuth alloy based on the density parameter.

[0054] Optionally, the injection conditions include: the outlet temperature of the heating device 1, the temperature of the injection pipe 2 and the temperature of the alloy tank 12 respectively reach respective first target values, and the alloy tank 12 is under inert gas protection.

[0055] In this optional embodiment, by setting corresponding injection conditions, including temperature control and inert gas protection, the injection stability can be improved, the alloy quality can be guaranteed, and the operation safety can be improved, providing a reliable technical guarantee for the subsequent filling process. It can be understood that one end of the injection pipe 2 is inserted into the interior of the heating device 1, and the other end is inserted into the interior of the alloy tank 12. The heating device 1 is provided with a connecting pipe, and the injection pipe 2 passes through the connecting pipe to enter the heating device 1. The outlet temperature of the heating device 1 refers to the temperature of the outlet connected to the injection pipe 2, that is, the outlet of the connecting pipe.

[0056] Specifically, the outlet temperature of the heating device 1 reaches the set target temperature to ensure that the tin-bismuth alloy is fully melted and maintained within a suitable temperature range, which is beneficial to the subsequent injection process. When the temperature of the injection pipe 2 and the temperature of the alloy tank 12 are also maintained within a suitable temperature range, the melted tin-bismuth alloy can be prevented from cooling and solidifying, thereby affecting the injection process. In addition, placing the alloy tank 12 in an inert gas protection can effectively prevent the occurrence of oxidation, pollution and other problems, thereby ensuring the quality of the injected alloy.

[0057] Optionally, the device further comprises: a first stop valve 3, a second stop valve 4 and a vent valve 5, wherein the first stop valve 3 is arranged on the injection pipe 2, and is used to connect the heating device 1 and the alloy tank 12, the second stop valve 4 and the vent valve 5 are both arranged on the heating device 1, the second stop valve 4 is used to connect the heating device 1 with the inert gas pipeline, and the vent valve 5 is used to connect the heating device 1 with the outside air;

[0058] The step of injecting the liquid tin-bismuth alloy into the alloy tank 12 by using the injection pipe 2 comprises:

[0059] The second stop valve 4 is opened, the vent valve 5 is closed, and the outlet pressure of the inert gas pipeline is adjusted. When the internal pressure of the heating device 1 reaches the first target pressure, the first stop valve 3 is opened.

[0060] like Figure 1As shown, the device includes a heating device 1 and related valves arranged on the heating device 1, such as the second stop valve 4 and the vent valve 5 in this embodiment. When the second stop valve 4 is opened, the heating device 1 can be connected to the inert gas pipeline, and the inert gas can be introduced into the heating device 1 to remove the air in the heating device 1 to avoid adverse effects on the heating of the tin-bismuth alloy block. The vent valve 5 is connected to the outside air and can also be called an exhaust valve. When the vent valve 5 is opened, the heating device 1 is connected to the outside, and when the vent valve 5 is closed, the heating device 1 is isolated from the outside air. Therefore, by opening and closing the second stop valve 4 and the vent valve 5, the pressure inside the heating device 1 can be adjusted, so that a certain pressure difference is generated between the heating device 1 and the alloy tank 12, so that the pressure difference can be used to realize the flow of the tin-bismuth alloy between the heating device 1 and the alloy tank 12. Compared with the method of pouring the tin-bismuth alloy into the alloy tank 12 after melting it outside the pile, this method is more convenient to operate on the one hand, and the pressure in the heating device 1 can be adjusted only by opening and closing the valve, so that the tin-bismuth alloy can automatically flow into the alloy tank 12. On the other hand, it can also improve the injection quality and stability of the tin-bismuth alloy.

[0061] Optionally, the step of injecting the liquid tin-bismuth alloy into the alloy tank 12 using the injection pipe 2 further includes:

[0062] The liquid level in the alloy tank 12 is obtained, and when the liquid level reaches a target height, the first stop valve 3, the heating device 1 and the second stop valve 4 are closed.

[0063] In this optional embodiment, by real-time monitoring of the liquid level in the alloy tank 12, the filling status of the liquid tin-bismuth alloy is timely known. When the liquid level in the alloy tank 12 reaches the target height, the first stop valve 3 is closed to stop the injection, ensuring that the injection amount meets the design requirements, avoiding over-injection or under-injection, and improving the accuracy of the filling. Turning off the heating device 1 and no longer needing to continue heating can effectively avoid the occurrence of overheating, save energy, and reduce costs. Close the second stop valve 4 to stop the inert gas purge.

[0064] Optionally, before starting the heating device 1, the method further comprises:

[0065] The second stop valve 4 and the vent valve 5 are opened to purge the interior of the heating device 1 with inert gas.

[0066] In this optional embodiment, the air can be exhausted by purging the inside of the heating device 1 with an inert gas, and an inert gas (such as argon or nitrogen) can be introduced to establish an inert gas protection environment, which can effectively reduce the effects of oxygen and water vapor in the air on the oxidation and corrosion of the alloy, thereby ensuring the quality and stability of the alloy. In addition, the purging of the inert gas can also ensure that the environment inside the heating device 1 is pure, eliminate possible pollutants and impurities, thereby improving the heating effect of the heating device 1 on the alloy, ensuring that the alloy receives appropriate temperature and protection during the melting process, and improving production quality and efficiency.

[0067] Optionally, when it is necessary to take out the tin-bismuth alloy from the alloy tank 12, the method includes:

[0068] Turning on the heater of the alloy tank 12 to melt the tin-bismuth alloy in the alloy tank 12 into liquid tin-bismuth alloy, and turning on the heating device 1 at the same time;

[0069] When the extraction condition is met, the liquid tin-bismuth alloy in the alloy tank 12 is extracted into the heating device 1 by using the injection pipe 2 .

[0070] The existing process of off-pile melting, stirring, and pouring injection cannot be used to extract the tin-bismuth alloy when replacing the tin-bismuth alloy, which increases the complexity of the maintenance and replacement process and reduces the operating efficiency.

[0071] In this optional embodiment, when the conditions for extracting the tin-bismuth alloy from the alloy tank 12 are met, it can be directly extracted into the heating device 1. Before extraction, the purpose of heating the alloy tank 12 is to melt the tin-bismuth alloy into a liquid state, because the tin-bismuth alloy is in a solid state when the full stack is in operation, so it needs to be heated to a molten state first. Before extraction, the heating device 1 is also heated to ensure that the extracted liquid tin-bismuth alloy will not cool and solidify, so as to keep the tin-bismuth alloy flowing in the heating device 1.

[0072] Optionally, the device further comprises a third stop valve, which is arranged on the heating device 1 and is used to connect the heating device 1 with the vacuum pump;

[0073] The extraction conditions include: the outlet temperature of the heating device 1 , the temperature of the injection pipe 2 , and the temperature of the alloy tank 12 have reached their respective second target values, and the third stop valve has been opened.

[0074] In this optional embodiment, by opening the third stop valve and connecting the vacuum pump, the heating device 1 can be evacuated to a negative pressure using the vacuum pump while ensuring that the temperature in the heating device 1 reaches a predetermined target value, so that a pressure difference is generated between the heating device 1 and the alloy tank 12. The tin-bismuth alloy in the alloy tank 12 can be extracted into the heating device 1 for heat preservation using the pressure difference, and the operation is simple and convenient.

[0075] It should be noted that since the heating device is connected to the vacuum pump and the inert gas pipeline in different scenarios, the third stop valve and the second stop valve can also share one valve. Therefore, when the tin-bismuth alloy is filled into the alloy tank, the valve is connected to the inert gas pipeline, and when the tin-bismuth alloy in the alloy tank is extracted, the valve is connected to the vacuum pump, thereby simplifying the device structure.

[0076] Optionally, the step of extracting the liquid tin-bismuth alloy in the alloy tank 12 into the heating device 1 by using the injection pipe 2 includes:

[0077] The power supply of the vacuum pump is turned on, and when the internal pressure of the heating device 1 reaches the second target pressure, the first stop valve 3 is opened.

[0078] In this optional embodiment, since the third stop valve is opened, that is, the heating device 1 is connected to the vacuum pump, the power of the vacuum pump is turned on at this time to evacuate the heating device 1, so that the interior of the heating device 1 is in a negative pressure state, and when the internal pressure of the heating device 1 reaches a certain value, the first stop valve 3 for connecting the heating device 1 and the alloy tank 12 is opened to extract the tin-bismuth alloy that has been heated and melted in the alloy tank 12 into the heating device 1 under the action of the pressure difference, thereby realizing the extraction of the tin-bismuth alloy, so as to facilitate the replacement of the tin-bismuth alloy medium in the sodium-cooled fast reactor.

[0079] Optionally, the device further comprises: an injection pipe heater 9, wherein the injection pipe heater 9 is at least partially disposed on the injection pipe 2;

[0080] Before injecting the liquid tin-bismuth alloy in the heating device 1 into the alloy tank 12, and / or before extracting the liquid tin-bismuth alloy in the alloy tank 12 into the heating device 1, the method further includes:

[0081] The injection pipe heater 9 is turned on to heat the injection pipe 2 .

[0082] In this optional embodiment, the injection tube heater 9 is used to heat the injection tube 2 so that the temperature inside the injection tube 2 is not lower than the melting point of the tin-bismuth alloy, thereby preventing the tin-bismuth alloy from solidifying when flowing from the heating device 1 to the alloy tank 12 or from the alloy tank 12 to the heating device 1 through the inflow tube, thereby hindering the injection or extraction of the tin-bismuth alloy or causing fluctuations.

[0083] Optionally, after heating and melting the tin-bismuth alloy block to form a liquid tin-bismuth alloy, the process further includes: removing impurities from the liquid tin-bismuth alloy, thereby ensuring that the tin-bismuth alloy injected into the alloy tank 12 has a higher purity.

[0084] Optionally, the specific steps of removing impurities include: turning off the power switch of the heating device 1, opening the sealing cover 8 of the heating device 1, removing impurities from the liquid tin-bismuth alloy, and then closing the sealing cover 8 and turning on the power switch of the heating device 1 for insulation treatment.

[0085] Optionally, the alloy tank 12 is a tank body for holding the tin-bismuth alloy to be filled. To ensure the quality of the tin-bismuth alloy filling, it needs to be cleaned before filling, and special cleaning tools and vacuum cleaner nozzles (adapted to the special structure of the tank body) are manufactured. The method of first adsorbing impurities, wiping with white cloth and then adsorbing impurities is adopted to remove attached foreign matter and impurities to prevent the tin-bismuth alloy from being integrated into the tin-bismuth alloy after filling, affecting its sealing performance. After cleaning, a special cover plate is installed to isolate foreign matter from the outside and to insulate. When the tin-bismuth alloy is injected, it is in liquid state, that is, the temperature of the alloy tank 12 tank body must be ensured not to be lower than the melting point of the tin-bismuth alloy to avoid abnormal solidification of the tin-bismuth alloy and the generation of excess impurities. During the tin-bismuth alloy injection stage, the tank body electric heater must be turned on to ensure the tank body temperature.

[0086] Optionally, the end of the injection pipe 2 extending into the alloy tank 12 has a preset distance from the bottom surface of the alloy tank 12 .

[0087] Optionally, the preset distance is 10 mm.

[0088] The setting of the preset distance can ensure that the tin-bismuth alloy flowing out of the injection tube 2 can be stably injected into the alloy tank 12, and avoid large fluctuations of the tin-bismuth alloy in the alloy tank 12. The distance of 10 mm can ensure that the tin-bismuth alloy can flow out of the injection tube 2 smoothly, and will not cause large fluctuations of the liquid in the alloy tank 12, thereby affecting the detection accuracy of the liquid level in the alloy tank 12.

[0089] Optionally, the device further comprises a support seat 11 (also referred to as a support seat), which is arranged at the bottom of the heating device 1. The arrangement of the support seat 11 can be used to adjust the height of the heating device 1 so that the injection pipe 2 led out from the heating device 1 is at a suitable distance from the alloy tank 12, thereby ensuring smooth injection of the tin-bismuth alloy in the injection pipe 2.

[0090] Optionally, the heating device 1 is further provided with a pressure gauge interface 6 , which is used to connect a pressure gauge 7 , and the pressure gauge 7 is used to detect the internal pressure of the heating device 1 .

[0091] The present invention is further described below by way of examples.

[0092] Example 1

[0093] This embodiment provides a sodium-cooled fast reactor tin-bismuth alloy filling method, including tin-bismuth alloy block manufacturing test, tin-bismuth alloy heating device 1 function test, product component removal and temporary fixation, heating device 1 installation and fixation, alloy tank 12 cleaning and preheating, tin-bismuth alloy block melting, argon protection, tin-bismuth alloy injection, impurity cleaning and vacuum extraction. Each step is described below.

[0094] The tin-bismuth alloy heating device 1 refers to a tin-bismuth alloy external heating melting device, which has the functions of melting, injecting and extracting tin-bismuth alloy. The main structure is as follows Figure 1 As shown. To ensure good functionality during the melting of tin-bismuth alloy, a no-load heating test is conducted in advance to master the basic operating steps and heating time of the equipment. To ensure good sealing during the injection and extraction of tin-bismuth alloy, a sealing test is conducted under working pressure in advance to find defective parts and repair them in time.

[0095] The product components refer to the components that affect the filling of the tin-bismuth alloy. It can be understood that according to the product structure, there is a mechanical compression sealing structure 13 at the position where the tin-bismuth alloy is to be filled (alloy groove 12), which is a mechanical structure to isolate the external environment. The alloy groove 12 and the mechanical sealing structure are respectively as follows: Figure 2 As shown in the solid rectangular frame. Before filling the tin-bismuth alloy, the mechanical compression sealing structure 13 and the parts that affect its disassembly and assembly need to be completely removed, the non-annular structural parts are moved away from the working area, the annular structural parts cannot be lifted away from the working area due to interference with other product parts, and the manufacturing support tool is temporarily fixed by lifting it from the installation position. It should be understood that when filling the tin-bismuth alloy, the mechanical compression sealing structure 13 needs to be removed and fixed to expose the opening position of the tin-bismuth alloy slot 12 so that the injection tube 2 can extend into the tin-bismuth alloy slot 12.

[0096] like Figure 3As shown, the sodium-cooled fast reactor has three cocks, namely a large cock 14, a middle cock 15, and a small cock 16. The cocks are sealed with tin-bismuth alloy, and accordingly, there are three tin-bismuth alloy grooves 12, namely a large cock tin-bismuth alloy groove 17 (the arrow in the figure indicates a full circle of circumference), a middle cock tin-bismuth alloy groove 18 (the arrow in the figure indicates a full circle of circumference), and a small cock tin-bismuth alloy groove 19 (the arrow in the figure indicates a full circle of circumference). Since the positions of the three tin-bismuth alloy grooves 12 are different, the installation and fixation of the heating device 1 must be considered to be able to meet the filling of the tin-bismuth alloy in the three tin-bismuth alloy grooves 12 at the large, medium and small plugs, and the size of the heating device 1 and the structure of the items installed on the plug are comprehensively considered, that is, the base of the heating device 1 can be installed on the plug and support the heating device 1 reliably and stably, and the heating device 1 can achieve the injection tube 2 extending into the tin-bismuth alloy groove 12 at this position and 10 mm above the bottom of the groove. This distance can ensure that the tin-bismuth alloy can be stably injected into the alloy groove 12. The installation position of the heating device 1 is determined by comprehensively considering the above two conditions, and the middle plug is rotated to a specific angle in advance to ensure that the heating device 1 can melt all the filling at one time during the filling process of the tin-bismuth alloy. Figure 3 At the same time, the heights of the three tin-bismuth alloy grooves 12 are inconsistent, as shown in FIG. Figure 4 As shown, a special support is designed and manufactured, installed at the bottom of the heating device 1, and the installation height of the heating device 1 is adjusted to meet the requirements of filling and extracting and replacing the tin-bismuth alloy in the three tin-bismuth alloy slots 12. Figure 4 In the figure, the slot openings and slot bottom positions of three alloy slots 12 are shown, namely the slot opening position 1901 of the small plug tin-bismuth alloy slot and the slot bottom position 1902 of the small plug tin-bismuth alloy slot, the slot position 1801 of the middle plug tin-bismuth alloy slot and the slot bottom position 1802 of the middle plug tin-bismuth alloy slot, and the slot opening position 1701 of the large plug tin-bismuth alloy slot and the slot bottom position 1702 of the large plug tin-bismuth alloy slot.

[0097] Taking the filling of the small plug tin-bismuth alloy tank 19 as an example, the installation diagram of the heating device 1 is as follows: Figure 5 As shown, it can be seen that a replaceable support is provided at the bottom of the heating device 1 to adjust the installation height of the heating device 1. By adjusting the support to a suitable height, the installation of the heating device 1 can not only meet the requirements of installing the heating device 1 on the cock, but also meet the requirements that the injection pipe 2 led out from the heating device 1 can penetrate into the alloy tank 12 and be about 10mm away from the bottom of the tank.

[0098] The melting of the tin-bismuth alloy block refers to placing the rectangular tin-bismuth alloy block into the heating device 1 and melting it into a liquid tin-bismuth alloy. The layout diagram of the tin-bismuth alloy block for one melting is calculated and drawn according to the size of the tin-bismuth alloy block, the inner wall size of the heating device 1 and the mass of the tin-bismuth alloy to be filled. After the alloy blocks are stacked according to the layout diagram, the heating device 1 is closed, the inert gas pipeline is connected, preferably the argon cylinder connection pipeline, the argon gas is purged in the heating device 1, the air in the heating device 1 is discharged, the outlet pressure of the argon cylinder and the opening size of the vent valve 5 on the heating device 1 are adjusted to ensure continuous argon purging, the power switch of the heating device 1 is turned on to heat and melt the tin-bismuth alloy, and the thermocouple on the heating device 1 is kept warm for a sufficient time after reaching the target temperature, the power of the heating device 1 is turned off, the flange cover of the heating device 1 (i.e., the sealing cover 8) is opened, and impurities on the liquid surface of the tin-bismuth alloy are removed using a special tool, the flange cover is closed again, the power of the heating device 1 is turned on to continue to keep warm, and the power 1010 of the injection pipe heater is turned on simultaneously to preheat the injection pipe 2.

[0099] Argon filling protection refers to the use of argon gas to isolate the molten tin-bismuth alloy from contact with air during the tin-bismuth alloy filling process. Before the tin-bismuth alloy is melted, argon gas is purged in the heating device 1 to displace the air in the device. During the melting stage, the output pressure of the gas cylinder is adjusted and argon gas is continuously purged in the heating device 1 to prevent air from being sucked back into the heating device 1 due to high temperature. Before the tin-bismuth alloy is injected into the tin-bismuth alloy tank 12, argon gas is purged in the tank body to displace the air in the tank body. During the injection stage, the output pressure of the gas cylinder is adjusted and argon gas is continuously purged in the tank body to prevent air from entering the alloy tank 12.

[0100] Injecting tin-bismuth alloy means injecting tin-bismuth alloy into the large, medium and small stopcock tin-bismuth alloy tanks respectively. When the outlet temperature of the heating device 1, the temperature of the injection pipe 2 and the tank body temperature of the tin-bismuth alloy tank 12 reach the target value, the tank body is notified that the argon protection has been completed, and the conditions for injecting tin-bismuth alloy are met. Adjust the outlet pressure of the argon gas bottle connected to the heating device 1, close the vent valve 5, increase the pressure in the container of the heating device 1, and after reaching the target pressure, open the first stop valve 3, and inject tin-bismuth alloy into the tank body through the pressure difference. During the injection process, observe the pressure of the pressure gauge 7 on the heating device 1, adjust the outlet pressure of the argon gas bottle to adjust the injection speed, and use a special metal liquid level gauge to measure the injection height. After the injection liquid level meets the requirements, close the first stop valve 3, turn off the power supply of the heating device 1, close the valve of the argon gas bottle, and stop the injection.

[0101] Impurity cleaning refers to the removal of impurities on the surface of the alloy liquid after the tin-bismuth alloy is injected into the alloy tank 12. After the injection is stopped, the cover plates above the tank body are opened in turn, the surface state of the alloy is checked, and the impurities are removed using a special tool (a colander adapted to the structure and size of the tank body). After the inspection is correct, the cover plate is reinstalled. After all inspections are completed, the power supply of the tank body electric heater is turned off until the tank body cools down naturally. During this period, the argon protection in the tank body is not turned off.

[0102] Vacuum extraction is the process of taking out the tin-bismuth alloy that has been injected into the tank body. When the tin-bismuth alloy is taken out and re-injected according to actual needs, vacuum extraction is required. Specifically, the heating device 1 is installed in a suitable position, the third stop valve is opened, so that the vacuum pump is connected to the heating device 1, the power supply of the heating device 1 is turned on to heat the container of the heating device 1, the injection tube heater 9 is turned on to heat the injection tube 2, and the power supply of the tank body electric heater is turned on to heat the alloy in the tank body. When the above temperature reaches the target value, the vacuum pump power supply is turned on, the pressure in the heating device 1 is pumped to negative pressure, the first stop valve 3 is opened, and the alloy in the tank body is pressed into the heating device 1 under the action of the pressure difference, and then the tin-bismuth alloy in the heating device 1 is injected into a special collection container for storage with reference to the tin-bismuth alloy injection technology.

[0103] Although the present invention is disclosed as above, the protection scope of the present invention is not limited thereto. Those skilled in the art may make various changes and modifications without departing from the spirit and scope of the present invention, and these changes and modifications will fall within the protection scope of the present invention.

Claims

1. A method for filling a sodium-cooled fast reactor with tin-bismuth alloy, characterized in that: A tin-bismuth alloy filling device for a sodium-cooled fast reactor, the device comprising a heating device (1) and an injection pipe (2), one end of the injection pipe (2) being connected to the heating device (1), and the other end being used to extend into an alloy tank (12) of a sodium-cooled fast reactor; When it is necessary to inject tin-bismuth alloy into the alloy tank (12), the method comprises: Placing a tin-bismuth alloy block in the heating device (1), and sealing the heating device (1); Turning on the heating device (1) to heat and melt the tin-bismuth alloy block into a liquid tin-bismuth alloy; When the injection conditions are met, the liquid tin-bismuth alloy is injected into the alloy tank (12) using the injection pipe (2).

2. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 1, characterized in that: Placing the tin-bismuth alloy block in the heating device (1) comprises: Obtaining a placement plan for the tin-bismuth alloy blocks according to the size of the tin-bismuth alloy blocks, the size of the inner wall of the heating device (1) and the mass of the tin-bismuth alloy to be filled; The tin-bismuth alloy blocks are stacked in the heating device (1) according to the placement plan.

3. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 1, characterized in that: The injection conditions include: the outlet temperature of the heating device (1), the temperature of the injection pipe (2) and the temperature of the alloy tank (12) respectively reach their respective first target values, and the alloy tank (12) is protected by an inert gas.

4. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 1, characterized in that: The device further comprises: a first stop valve (3), a second stop valve (4) and a vent valve (5); the first stop valve (3) is arranged on the injection pipe (2) and is used to connect the heating device (1) and the alloy tank (12); the second stop valve (4) and the vent valve (5) are both arranged on the heating device (1); the second stop valve (4) is used to connect the heating device (1) and the inert gas pipeline; the vent valve (5) is used to connect the heating device (1) and the outside air; The step of injecting the liquid tin-bismuth alloy into the alloy tank (12) using the injection pipe (2) comprises: The second stop valve (4) is opened, the vent valve (5) is closed, the outlet pressure of the inert gas pipeline is adjusted, and when the internal pressure of the heating device (1) reaches the first target pressure, the first stop valve (3) is opened.

5. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 4, characterized in that: The step of injecting the liquid tin-bismuth alloy into the alloy tank (12) using the injection pipe (2) further comprises: The height of the liquid level in the alloy tank (12) is obtained, and when the liquid level reaches a target height, the first stop valve (3), the heating device (1) and the second stop valve (4) are closed.

6. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 4, characterized in that: Before starting the heating device (1), the method further comprises: The second stop valve (4) and the vent valve (5) are opened to purge the interior of the heating device (1) with an inert gas.

7. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 4, characterized in that: When it is necessary to take out the tin-bismuth alloy from the alloy tank (12), the method comprises: Turning on the heater of the alloy tank (12) to melt the tin-bismuth alloy in the alloy tank (12) into liquid tin-bismuth alloy, and turning on the heating device (1) at the same time; When the extraction conditions are met, the liquid tin-bismuth alloy in the alloy tank (12) is extracted into the heating device (1) using the injection pipe (2).

8. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 7, characterized in that: The device further comprises a third stop valve, which is arranged on the heating device (1) and is used to connect the heating device (1) with the vacuum pump; The extraction conditions include: the outlet temperature of the heating device (1), the temperature of the injection pipe (2) and the temperature of the alloy tank (12) have reached their respective second target values, and the third stop valve has been opened.

9. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 8, characterized in that: The method of using the injection pipe (2) to extract the liquid tin-bismuth alloy in the alloy tank (12) into the heating device (1) comprises: The power supply of the vacuum pump is turned on, and when the internal pressure of the heating device (1) reaches the second target pressure, the first stop valve (3) is opened.

10. The method for filling tin-bismuth alloy for sodium-cooled fast reactor according to claim 7, characterized in that: The device further comprises: an injection pipe heater (9), wherein the injection pipe heater (9) is at least partially arranged on the injection pipe (2); Before the liquid tin-bismuth alloy in the heating device (1) is injected into the alloy tank (12), and / or before the liquid tin-bismuth alloy in the alloy tank (12) is extracted into the heating device (1), the method further comprises: The injection pipe heater (9) is turned on to heat the injection pipe (2).

Citation Information

Cited By

  • Three-cock assembly suitable for reactor and control rod driving cock suitable for three-cock assembly

    CN119724652A

  • Cock assembly for reactor

    CN119724653A

  • Stopcock assembly for a reactor

    CN119724653B

  • Machining method and machining device for lubricating guide pipe

    CN120306955A