Cleaning solution for battery injection liquid crystal substance

The crystals on the surface of the lithium battery liquid injection equipment are soaked through a mixed solution of multiple solvents, which solves the problem of poor cleaning effect in the prior art, and achieves efficient removal of crystals, ensuring liquid injection sealing and quality. Reduced loss of quality cost.

CN118995346APending Publication Date: 2024-11-22ZHENGZHOU BAK BATTERY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410923292.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the prior art, the DMC solvent used to clean the liquid injection crystals of lithium batteries have poor effect, resulting in residual crystals on the surface of the equipment, affecting the liquid injection sealing and quality, and causing loss of quality cost.

Method used

Using a mixed solution of dimethyl carbonate (DMC), vinyl carbonate (EC), organic carbonate or propionate, the crystals on the surface of the equipment are soaked, and the crystals are removed by using their chemical reactions, temperature and soaking time. Adjustable.

Benefits of technology

It significantly improves the cleaning efficiency of crystals, reduces the residual on the surface of the equipment, ensures the sealing and quality of the liquid injection, and avoids the occurrence of poor batch liquid injection.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a cleaning solution for a battery injection crystal substance, which comprises the following components in percentage by mass: 10-90% of dimethyl carbonate, 10-90% of ethylene carbonate and the balance of auxiliaries, 2%-60% of ethylene carbonate; the balance is an auxiliary agent; and the auxiliary agent is at least one of organic carbonic ester and propionate. The auxiliary agent can be pure organic carbonic ester or propionate, and can also be a mixture of the organic carbonic ester and the propionate. According to the invention, a plurality of solvents are mixed to prepare the cleaning solution capable of more effectively cleaning the crystal substances, and the liquid injection equipment is soaked in the cleaning solution to fully react, so that the crystal substances can be quickly and effectively removed. Batch liquid injection adverse accidents caused by crystallization of a production line are avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of battery liquid injection crystallization treatment, and in particular relates to a cleaning solution for battery liquid injection crystallization. Background Art

[0002] During the production of lithium batteries, electrolyte needs to be injected into the battery cells. The electrolyte is usually a solution that is easy to crystallize. When the production line runs for a long time, crystals are easily generated on the surface of the injection tray, hopper, sealing plug and other related equipment in the injection equipment. However, the injection crystals are difficult to clean. The commonly used cleaning method is to use DMC solvent to clean the crystals. This method has a poor cleaning effect on the crystals, and most of the crystals will still remain on the surface of the equipment. When the equipment is in long-term operation, the residual crystals will cause the injection seal to be loose, resulting in poor batch injection and extremely high quality cost losses. Summary of the invention

[0003] In view of the deficiencies described in the above-mentioned prior art, the present invention provides a cleaning solution for battery injection crystals, which is prepared by mixing multiple solvents to obtain a cleaning solution capable of soaking and effectively removing crystals.

[0004] The technical solution adopted by the present invention is: A cleaning solution for battery injection crystals, comprising dimethyl carbonate (DMC), ethylene carbonate (EC) and an auxiliary agent, wherein the mass percentage of dimethyl carbonate (DMC) is 10%-90%; the mass percentage of ethylene carbonate (EC) is 2%-60%; the balance is the auxiliary agent; and the auxiliary agent is at least one of an organic carbonate and a propionate. That is, the auxiliary agent can be either a simple organic carbonate or a propionate, or a mixture of organic carbonate and propionate.

[0005] As a preferred embodiment of the present invention, dimethyl carbonate (DMC), ethylene carbonate (EC) and the auxiliary agent are mixed at room temperature according to mass percentage.

[0006] As a preferred embodiment of the present invention, the organic carbonate includes at least one of propylene carbonate (PC), ethyl methyl carbonate (EMC), and diethyl carbonate (DEC). The organic acid ester can be a single carbonate or a mixture of multiple different carbonates.

[0007] As a preferred embodiment of the present invention, the propionate ester includes at least one of methyl propionate (MP), ethyl propionate (EP) and propyl propionate (PP). The propionate ester can be a single propionate ester or a mixture of multiple different propionates.

[0008] As a preferred embodiment of the present invention, the equipment with battery injection crystals is completely immersed in a cleaning solution to allow the cleaning solution and the crystals to fully react. The immersion time is 0.1h-10h. During the immersion, the temperature of the cleaning solution is set at 10-60°C to complete the cleaning of the crystals on the surface of the injection equipment.

[0009] The present invention prepares a cleaning solution that can more effectively clean crystals by mixing multiple solvents, and the crystals can be quickly and effectively removed by immersing the injection equipment in the cleaning solution for full reaction, thereby avoiding batch injection accidents caused by crystallization on the production line. DETAILED DESCRIPTION

[0010] Example 1 Mix 8 kg of DMC, 1 kg of EC, and 1 kg of EMC at room temperature to prepare a cleaning solution for injection crystals. Soak 5 g of crystals on the surface of the injection equipment collected from the production line in the cleaning solution. Allow the crystals to fully react with the solution at 20°C for 3 hours. Filter the solution, weigh the residual crystals, and confirm the cleaning effect of the solution on the crystals.

[0011] Example 2 Mix 6 kg of DMC, 3 kg of EC, and 1 kg of PC at room temperature to prepare a cleaning solution for injection crystals. Soak 5 g of crystals on the surface of the injection equipment collected from the production line in the cleaning solution. Allow the crystals to fully react with the solution at 40°C for 1 hour. Filter the solution, weigh the residual crystals, and confirm the cleaning effect of the solution on the crystals.

[0012] Example 3 Mix 4 Kg of DMC, 5 Kg of EC, 0.5 Kg of DEC, and 0.5 Kg of EP at room temperature to prepare a cleaning solution for injection crystals. Soak 5 g of crystals on the surface of the injection equipment collected from the production line in the cleaning solution. Allow the crystals to fully react with the solution at 30°C for 2 hours. Filter the solution, weigh the residual crystals, and confirm the cleaning effect of the solution on the crystals.

[0013] Comparative Example Take 10 kg of DMC and 5 g of crystals collected from the surface of the injection equipment in the production line and immerse them in the cleaning solution at room temperature. Allow the crystals to fully react with the solution for 1 hour at 25°C. Filter the solution and weigh the remaining crystals to confirm the cleaning effect of the solution on the crystals.

[0014] The cleaning effects of Examples 1-3 and Comparative Examples on crystals are shown in Table 1: Table 1 Example 1 Example 2 Example 3 Comparative Example Residual weight g 0.15 0.03 0.05 1.5 Crystal cleaning efficiency 97% 99.40% 99% 70% It can be seen intuitively from Table 1 that the cleaning efficiency of the crystals is higher when the cleaning solution of the present invention is used.

[0015] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0016] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A cleaning solution for battery injection crystals, characterized in that: The invention comprises dimethyl carbonate, ethylene carbonate and an auxiliary agent, wherein the mass percentage of dimethyl carbonate is 10%-90%; the mass percentage of ethylene carbonate is 2%-60%; the balance is the auxiliary agent; and the auxiliary agent is at least one of organic carbonate and propionate.

2. The cleaning solution for battery injection crystals according to claim 1, characterized in that: Dimethyl carbonate, ethylene carbonate and an auxiliary agent are mixed at room temperature according to mass percentage.

3. The cleaning solution for battery injection crystals according to claim 1 or 2, characterized in that: The organic carbonate includes at least one of propylene carbonate, ethyl methyl carbonate and diethyl carbonate.

4. The cleaning solution for battery injection crystals according to claim 3, characterized in that: The propionate ester includes at least one of methyl propionate, ethyl propionate and propyl propionate.

5. The cleaning solution for battery injection crystals according to claim 4, characterized in that: Completely immerse the device with battery injection crystals in the cleaning solution for 0.1h-10h; during immersion, keep the temperature of the cleaning solution at 10-60°C.