Gold ore grinding and floating technological process

By extending the flotation and selection time, increasing the medium- ore remilling process, and optimizing the pharmaceutical combination, the problems of low efficiency of ore dressing equipment and waste of resources have been solved, the gold ore dressing indicators have been improved and the comprehensive utilization of resources have been significantly improved, and concentrate has been significantly improved Grade and productivity.

CN119034953APending Publication Date: 2024-11-29HENAN ZHONGKUANG ENERGY CO LTD SONGXIAN SHISHUDI GOLD MINE

Patent Information

Application Number
CN202411236002.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The existing ore dressing production equipment has reduced efficiency due to long-term use, reduced quality of the raw ore, unstable control of the gold content of tailings, resulting in waste of resources and difficulty in adapting to new demands, affecting the comprehensive utilization and competitive strength of the mine.

Method used

A gold ore grinding process flow is proposed, including extending flotation and selection time, increasing the medium ore remilling process flow, adopting a closed circuit remilling system combining cyclone and vertical mill to optimize the flotation agent combination and improve the refinement Mineral grade and reduce the running tail loss of gold carrier minerals during closed circuit cycles.

Benefits of technology

Effectively reduce metal loss in tailings, improve concentrate grade, improve resource utilization and economic benefits, extend equipment service life, and improve production continuity and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119034953A_ABST
    Figure CN119034953A_ABST
Patent Text Reader

Abstract

The invention discloses a gold ore grinding and floating technological process which comprises the following steps that raw ore is crushed to form crushed ore, the crushed ore is put into a ball mill to be crushed, the crushed ore enters a vibrating screen to be screened, the screened ore is put into an ore pulp pool, and the ore pulp pool is fed into a first-section cyclone through a slurry pump to be separated; the separated overflowed mineral aggregate enters a roughing stirring tank to be stirred and then is subjected to roughing and four times of scavenging, and the rough scavenging volume is 112 m; and middlings obtained after roughing and scavenging enter a middling pond and are fed into a concentration stirring tank through a foam pump. The original two-stage grading of a grader and a cyclone is changed into one-stage grading of the cyclone, so that the cyclic load of the two-stage grading is reduced, the grading efficiency is improved, one grading device is standby and the other grading device is used without stopping production and overhauling every year, and the production continuity is ensured; in the flotation operation, the original rough scavenging volume is expanded from 80m to 112m, and the flotation time is prolonged, so that the condition of metal loss in tailings is effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of mining, in particular to a gold ore grinding and flotation process. Background Art

[0002] In view of the fact that the existing mineral processing equipment has been in operation for many years, and the characteristics of the mine ore have changed to varying degrees, the production process has encountered several challenges and limitations. The main manifestations are that the quality of the ore has gradually declined, the quality of the concentrate is low, and it is difficult to maintain it above 20g / t; the gold content in the tailings is not stable, sometimes as high as 0.3g / t, resulting in waste of resources; in addition, due to the long service life of the equipment, some facilities have become aged, the work efficiency has been reduced, and it is difficult to adapt to the current new needs. In order to solve the current problems and shortcomings of the mine, improve the comprehensive utilization of mine resources, and enhance the overall competitiveness of the mine under the new economic situation, we propose a gold ore grinding and flotation process. Summary of the invention

[0003] The technical problem to be solved by the present invention is to overcome the existing defects, provide a gold ore grinding and flotation process, prolong the flotation time, thereby effectively reducing the metal loss in the tailings; prolong the concentration time, and improve the concentrate grade; add a process flow of re-grinding the middlings, which can improve the dissociation degree of the gold carrier mineral monomers, improve the concentrate grade, and prevent the loss of gold carrier mineral conjoined bodies during the closed-loop circulation process, so that the gold ore dressing index is greatly improved, resulting in good economic and social benefits, and can effectively solve the problems in the background technology.

[0004] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a gold ore grinding and flotation process, comprising the following steps: crushing the raw ore to form crushed ore, putting it into a ball mill for crushing, the crushed ore entering a vibrating screen for screening, putting the screened ore into a slurry pool, and sending it into a cyclone for separation through a slurry pump, the overflowed ore after separation enters a roughing stirring tank for stirring, and then undergoes roughing and four scavenging, and the roughing scavenging volume is 112m³; the intermediate ore obtained after roughing and scavenging is concentrated into the intermediate ore pool, and is sent into a closed-circuit grinding system composed of a cyclone group and a vertical mill through a foam pump (the cyclone plays the role of pre-grading and checking grading), and the returned sand enters the vertical mill for regrinding, and the overflow enters the concentration stirring tank, and then the concentrate is output after three concentrations.

[0005] As a preferred technical solution of the present invention, the mineral materials remaining on the screen after screening by the vibrating screen are returned to the ball mill for further crushing.

[0006] As a preferred technical solution of the present invention, the underflow ore material separated by a cyclone is put into a ball mill for further crushing.

[0007] As a preferred technical solution of the present invention, the ore after roughing can directly enter the intermediate ore pool through a pipeline.

[0008] As a preferred technical solution of the present invention, the roughed ore can be directly output through a pipeline and combined with the concentrated product as the final product.

[0009] As a preferred technical solution of the present invention, the middling ore in the middling ore pool is sent to the second-stage cyclone through the middling ore pipeline after regrinding by a foam pump for re-separation, and the separated overflow ore is sent to the concentration stirring tank, and the concentrate is output after three concentrations; the separated underflow is sent to the vertical mill for regrinding and then returned to the middling ore pool, and then sent to the concentration stirring tank through a foam pump, and the concentrate is output after three concentrations.

[0010] As a preferred technical solution of the present invention, the slurry pump, foam pump and first-stage cyclone are all in one-in-use and one-in-reserve, and the second-stage cyclone is in three-in-use and one-in-reserve.

[0011] As a preferred technical solution of the present invention, intermediate ore spare pipelines are arranged between the roughing equipment and the primary scavenging equipment, between the primary scavenging equipment and the secondary scavenging equipment, between the secondary scavenging equipment and the tertiary scavenging equipment, and between the tertiary scavenging equipment and the quaternary scavenging equipment.

[0012] As a preferred technical solution of the present invention, the reagents for rough selection are 50 g / t of kerosene and 100 g / t of butyl ammonium black powder; the reagents for the first scavenging selection are 17 g / t of kerosene and 34 g / t of butyl ammonium black powder; the reagents for the second scavenging selection are 6 g / t of kerosene and 11 g / t of butyl ammonium black powder; the reagents for the third scavenging selection are 3 g / t of kerosene and 5 g / t of butyl ammonium black powder.

[0013] As a preferred technical solution of the present invention, the reagents for rough selection are 50 g / t of sodium sulfide, 20 g / t of butyl xanthate, and 100 g / t of butyl ammonium black medicine; the reagents for primary scavenging selection are 30 g / t of sodium sulfide, 10 g / t of butyl xanthate, and 50 g / t of butyl ammonium black medicine; the reagents for secondary scavenging selection are 15 g / t of sodium sulfide, 5 g / t of butyl xanthate, and 25 g / t of butyl ammonium black medicine.

[0014] Compared with the prior art, the invention has the following beneficial effects: the original two-stage classification of the classifier + cyclone is changed to one-stage classification of the cyclone, so as to reduce the circulation load of the two-stage classification and improve the classification efficiency, and the classification equipment is kept in one standby and one in use without annual shutdown and maintenance, so as to ensure the continuity of production; in the flotation operation, the original rough scavenging volume is expanded from 80m³ to 112m³, so as to extend the flotation time, thereby effectively reducing the loss of metal in the tailings; in the concentration operation, the original two concentrations are changed to three concentrations, so as to extend the concentration time and improve the concentrate grade; the process flow of regrinding the middling ore is added, and the closed-circuit regrinding process combined with the vertical mill and the cyclone can be adopted, so as to improve the dissociation degree of the gold carrier mineral monomer, improve the concentrate grade, and prevent the loss of the gold carrier mineral conjoined body in the closed-circuit circulation process; in the flotation reagent system, the combination ratio of the flotation reagent is optimized, so as to improve the flotation performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the process flow of the present invention; Figure 2 It is a schematic diagram of the process flow of the present invention; Figure 3 It is a schematic diagram of the small closed-circuit test process of the present invention; Figure 4 It is a schematic diagram of the small closed-circuit test process of the present invention. DETAILED DESCRIPTION

[0016] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0017] See also Figure 1-4 The present invention provides a technical solution: a gold ore grinding and flotation process, comprising the following steps: crushing the raw ore to form crushed ore, putting it into a ball mill for crushing, the crushed ore entering a vibrating screen for screening, putting the screened ore into a slurry pool, and sending it into a cyclone for separation through a slurry pump, changing the existing two-stage classification of a classifier + a cyclone into a one-stage classification of a cyclone, reducing the circulating load of the two-stage classification, improving the classification efficiency, and keeping one backup and one use of the classification equipment without annual shutdown for maintenance, thereby ensuring production continuity.

[0018] The overflowed ore after separation enters the roughing mixing tank for mixing. After roughing and four sweeping, the roughing volume is expanded from 80m³ to 112m³, which prolongs the flotation time and effectively reduces the loss of metal in the tailings.

[0019] The middlings obtained after roughing and scavenging enter the middling pool, and are sent to the concentration stirring tank through a foam pump. After three concentrations, the concentrate is output. The original two concentrations are changed to three concentrations, which prolongs the concentration time and improves the concentrate grade.

[0020] According to the preferred technical solution, the middlings in the middling pool are sent to the second-stage cyclone through the middling pipeline after regrinding by a foam pump for re-separation, and the separated overflow ore is sent to the concentration stirring tank, and the concentrate is output after three concentrations; the separated underflow is sent to the vertical mill for regrinding and then returned to the middling pool, and then sent to the concentration stirring tank through a foam pump, and the concentrate is output after three concentrations. By increasing the process flow of regrinding the middlings and adopting a closed-circuit regrinding process combined with a vertical mill and a cyclone, the dissociation degree of the gold carrier mineral monomer can be improved, the concentrate grade can be improved, and the loss of the gold carrier mineral conjoints in the closed-circuit circulation process can be prevented.

[0021] A further preferred technical solution is that the ore after roughing can directly enter the middling pool through a pipeline. Specifically, when the roughing product meets the sales needs, the roughing middling and the concentrated product can be combined as the final product, and the middlings from the other four scavengings can be combined and re-ground before being concentrated. This can effectively reduce the burden of subsequent scavenging operations and improve the recovery rate.

[0022] When the grade of the scavenging product is low, the roughing medium can be selected for regrinding, and the medium ores from the other four scavenging operations can be returned sequentially according to the conventional process, or some of the products can be combined for regrinding and some can be returned sequentially, thus ensuring the quality of the final product.

[0023] If the regrinding equipment needs to be repaired, a process can be adopted in which all operations are returned in full sequence, so that production will not be stopped due to equipment maintenance.

[0024] The traditional flotation process is one roughing and four scavenging. The original plan is to re-grind the roughing medium, and return the other four scavenging medium in sequence according to the conventional process. The significance of re-grinding the medium and then entering the fine is mainly to improve the grade (quality) of the concentrate (i.e. the final product). In order to maximize the recovery rate on the basis of improving the concentrate grade, it is possible to consider the feasibility of gathering all the medium together for re-grinding, so that each flotation operation can increase the amount of foam (i.e. the medium) scraped as much as possible. After many discussions and experiments, it was finally decided to use a three-way connection in the flow pipeline of the medium in each flotation operation, so that it can be switched according to the actual situation in production, mainly according to specific production needs and product quality, using a set of equipment to switch multiple processes, and realize the selection of multiple flotation processes with a set of equipment. Specifically, it can: ① The roughing medium is regrinded, and the medium ores from the other four sweepings are returned sequentially according to the normal process; ② The roughing medium is combined with the selected products as the final product, and the medium ores from the other four sweepings are combined and regrinded before being selected; ③ The products of some operations are combined and regrinded, and some operations are returned sequentially; ④ All operations are returned sequentially.

[0025] A further preferred technical solution is that when the rough selected ore meets the sales requirements, it can also be directly output through the concentrate (optional) pipeline as the final product.

[0026] The preferred technical solution is to set intermediate ore spare pipelines between the roughing equipment and the primary scavenging equipment, between the primary scavenging equipment and the secondary scavenging equipment, between the secondary scavenging equipment and the tertiary scavenging equipment, and between the tertiary scavenging equipment and the fourth scavenging equipment. After each scavenging, it can be selected whether to perform ore selection in sequence or return to the previous equipment for multiple scavenging according to the quality of the product after scavenging, thereby realizing the selection of multiple flotation processes with one set of equipment.

[0027] The preferred technical solution is that the remaining ore on the screen after vibrating screen screening is returned to the ball mill for re-crushing, and the bottom flow ore after a cyclone separation is put into the ball mill for re-crushing, both of which can improve the comprehensive utilization rate of mining resources and further improve product grade and total output.

[0028] The preferred technical solution is that the slurry pump, foam pump and first-stage cyclone are all equipped with one in use and one in reserve, and the second-stage cyclone is equipped with one in use and one in reserve. When maintenance is needed, it only needs to be switched to the spare equipment without stopping production, thus ensuring production continuity and improving work efficiency.

[0029] Preferably, a slurry pipeline is provided between the primary concentrating equipment and the roughing equipment, for discharging the slurry generated during the concentrating process as tailings through the roughing and scavenging equipment and corresponding pipelines.

[0030] As a specific embodiment of the present invention: the results of the process mineralogy research on gold ore in a certain mining area show that the main metal sulfide of the gold mine in this area is pyrite, followed by chalcopyrite, a small amount of galena, bornite, sphalerite, and trace amounts of other sulfides; non-metallic minerals are mainly quartz and feldspar, followed by biotite, dolomite and calcite; pyrite is the main gold-bearing mineral, and gold mainly exists in the form of leaching gold. Secondly, in the sulfide-encapsulated gold, carbonate and oxide gold and silicate gold account for a small proportion, and it is appropriate to use flotation technology to recover gold. After many flotation tests, the research results show that butyl ammonium black medicine is an excellent collector for the flotation of the gold mine. With butyl ammonium black medicine as the main collector, whether it is used alone or in combination with butyl xanthate or kerosene, the flotation effect is significantly better than that with butyl xanthate as the main collector.

[0031] Optional technical solutions, such as Figure 3 As shown, the reagents for roughing are 50g / t kerosene and 100g / t butyl ammonium black powder; the reagents for the first scavenging are 17g / t kerosene and 34g / t butyl ammonium black powder; the reagents for the second scavenging are 6g / t kerosene and 11g / t butyl ammonium black powder; the reagents for the third scavenging are 3g / t kerosene and 5g / t butyl ammonium black powder. By adopting this reagent system, when the gold grade of the feed ore is 1.28g / t, a flotation concentrate with a gold grade of 25.04g / t and a recovery rate of 80.55% can be obtained.

[0032] Optional technical solutions, such as Figure 4 As shown, the reagents for roughing are 50 g / t sodium sulfide, 20 g / t butyl xanthate, and 100 g / t butyl ammonium black powder; the reagents for primary scavenging are 30 g / t sodium sulfide, 10 g / t butyl xanthate, and 50 g / t butyl ammonium black powder; the reagents for secondary scavenging are 15 g / t sodium sulfide, 5 g / t butyl xanthate, and 25 g / t butyl ammonium black powder. By adopting this reagent system, when the feed gold grade is 1.30 g / t, a gold concentrate with a gold grade of 27.59 g / t and a recovery rate of 81.52% can be obtained.

[0033] This application has created a new reagent system suitable for the flotation of low-grade gold ores. Combined with the new gold grinding and flotation process, it has completely solved the problems and shortcomings that have existed in mine dressing plants for many years, such as outdated equipment, low degree of automation, poor production stability, low dressing efficiency, and high energy consumption.

[0034] Through the transformation of mineral processing technology, the smelting cost of flotation concentrate has been significantly reduced, and the consumption of flotation reagents has been reduced to a certain extent, reducing the unit cost of mineral processing. Before the technical transformation, the average gold grade of the product was 24g / t and the recovery rate was 83%; after the technical transformation, the average gold grade of the product was 35 g / t-40g / t, and the recovery rate was about 86%. The gold concentrate grade was increased by more than 10g / t and the gold recovery rate was increased by about 3 percentage points compared with before the technical transformation; after conversion, the smelting and processing costs of gold concentrate products can be saved by 4.5 million yuan / year, and the additional gold is about 8.4 kilograms (equivalent to an output value of 4 million yuan), and the average annual saving of reagent costs is about 140,000 yuan / year.

[0035] The undisclosed parts in the present invention are all prior art, and their specific structures, materials and working principles are not described in detail. Although the embodiments of the present invention have been shown and described, it is understood by those skilled in the art that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principles and spirit of the present invention, and the scope of the present invention is defined by the attached claims and their equivalents.

Claims

1. A gold ore grinding and flotation process, characterized in that: The following steps are involved: The raw ore is crushed into crushed ore, which is then put into the ball mill for crushing. The crushed ore enters the vibrating screen for screening, and the screened ore is put into the slurry pool, and is sent to a cyclone for separation through a slurry pump. The overflowed ore after separation enters the roughing stirring tank for stirring, and then undergoes roughing and four scavenging. The roughing and scavenging volume is 112m³; the middling ore obtained after roughing and scavenging enters the middling ore pool, and is sent to the concentrating stirring tank through a foam pump, and then the concentrate is output after three concentrating.

2. A gold ore grinding and flotation process according to claim 1, characterized in that: The remaining ore on the vibrating screen after screening is returned to the ball mill for further crushing.

3. A gold ore grinding and flotation process according to claim 2, characterized in that: The underflow ore material separated by the first stage cyclone is put into the ball mill for further crushing.

4. A gold ore grinding and flotation process according to claim 3, characterized in that: The roughed ore can be directly fed into the intermediate ore pool through a pipeline.

5. The gold ore grinding and flotation process according to claim 3 is characterized by: The roughed ore can be directly output through a pipeline and combined with the selected product as the final product.

6. A gold ore grinding and flotation process according to claim 4 or 5, characterized in that: The middlings in the middling pool are sent to the second-stage cyclone through a foam pump and a middling pipeline after regrinding for re-separation, and the separated overflow ore is sent to a concentration stirring tank, and the concentrate is output after three concentrations; The separated underflow is sent to the vertical mill for regrinding and then returned to the intermediate ore pool. It is then sent to the concentration mixing tank through a foam pump and the concentrate is output after three concentrations.

7. A gold ore grinding and flotation process according to claim 6, characterized in that: The slurry pump, foam pump and first-stage cyclone are all equipped with one in use and one in reserve, and the second-stage cyclone is equipped with three in use and one in reserve.

8. The gold ore grinding and flotation process according to claim 1 is characterized by: A mid-ore spare pipeline is arranged between the roughing equipment and the primary scavenging equipment, between the primary scavenging equipment and the secondary scavenging equipment, between the secondary scavenging equipment and the tertiary scavenging equipment, and between the tertiary scavenging equipment and the fourth scavenging equipment.

9. The gold ore grinding and flotation process according to claim 1, characterized in that: The reagents for rough selection are 50g / t kerosene and 100g / t butyl ammonium black powder; the reagents for the first scavenging selection are 17g / t kerosene and 34g / t butyl ammonium black powder; the reagents for the second scavenging selection are 6g / t kerosene and 11g / t butyl ammonium black powder; the reagents for the third scavenging selection are 3g / t kerosene and 5g / t butyl ammonium black powder.

10. The gold ore grinding and flotation process according to claim 1, characterized in that: The reagents used in the roughing selection are 50 g / t of sodium sulfide, 20 g / t of butyl xanthate, and 100 g / t of butyl ammonium black powder; the reagents used in the first scavenging selection are 30 g / t of sodium sulfide, 10 g / t of butyl xanthate, and 50 g / t of butyl ammonium black powder; the reagents used in the second scavenging selection are 15 g / t of sodium sulfide, 5 g / t of butyl xanthate, and 25 g / t of butyl ammonium black powder.

Citation Information

Patent Citations

  • Open-circuit method for improving refractory gold ore concentrate quality and recovery rate

    CN101028613A

  • Flotation method for high-grade low-sulfide-content gold-bearing ore

    CN110711647A

  • Gold ore tailing multi-stage screening and gradient magnetic separation resource utilization system and method

    CN113856889A

  • Flotation method for improving beneficiation index of low-grade high-mud-content refractory gold ore

    CN117884250A

Cited By

  • Gold ore flotation full-process intelligent monitoring and optimal control method and system

    CN120276349A