Method for synergistic graded conversion and resource utilization of sludge and biomass

Through the mixed pyrolysis gasification technology of sludge and biomass, the pyrolysis of sludge is catalyzed by alkali metal potassium in biomass, the problems of low pyrolysis gas quality and unstable coke in the existing technology are solved, and high efficiency is achieved , stable resource utilization of sludge and biomass.

CN119040026APending Publication Date: 2024-11-29HEFEI GENERAL MACHINERY RES INST

Patent Information

Application Number
CN202411255885.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-09
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The existing copyrolysis technology of sludge and biomass has problems such as low pyrolysis gas quality, unstable components, inability to directly utilize coke powder, and the generation of low melting point particles, making it difficult to achieve the generation of high-quality pyrolysis gas and coke.

Method used

By drying, drying, crushing and sieving the sludge and biomass respectively to a particle size between 75 and 97 μm, mixing and forming, pyrolysis and gasification is carried out in a fixed bed reactor, and alkali metal potassium in the biomass is catalyzed Sludge pyrolysis produces high-quality molded coke, and improves carbon conversion and gas quality through the gasification process of molded coke.

Benefits of technology

Improve the pyrolysis efficiency and pyrolysis gas yield of sludge, generate high-quality, stable components and molded coke, reduce the generation of low-melting fine particles, alleviate the ash accumulation and pollution problems of equipment, and broaden the coke Range of use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119040026A_ABST
    Figure CN119040026A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of organic solid waste pyrolysis, in particular to a method for synergistic graded conversion and resource utilization of sludge and biomass. The method comprises the following steps: firstly, respectively drying and crushing collected sludge and biomass, then uniformly mixing according to a set mass ratio, putting the mixture into a mold to be pressed into briquette fuel, and then putting the briquette fuel into a fixed bed reactor to be pyrolyzed to obtain pyrolysis gas and briquette coke. The sludge and the biomass are mixed to prepare the briquette fuel, alkali metal potassium rich in the biomass is effectively utilized to catalyze sludge pyrolysis, the pyrolysis efficiency of the sludge and the pyrolysis gas yield are improved, a large amount of briquette coke is generated, and high value-added utilization of the sludge and the biomass is achieved; and the carbon conversion rate and the fuel gas quality are also improved by graded pyrolysis and gasification of the sludge and the biomass briquette. The invention provides a new approach method for sludge pyrolysis gasification, and has a wide application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of organic solid waste pyrolysis, and in particular to a method for coordinated graded conversion and resource utilization of sludge and biomass. Background Art

[0002] With the development of my country's social economy, the output of organic solid waste has increased rapidly. As a derivative of sewage treatment, the output of sludge has exceeded 60 million tons / year. Improper treatment of large amounts of organic solid waste will not only cause secondary pollution, but also waste resources. Therefore, achieving high-value, reduced, and harmless disposal of sludge is a major demand for meeting the construction of ecological civilization and sustainable development.

[0003] At present, conventional sludge and biomass disposal methods include sanitary landfill, building material utilization, land utilization and incineration, but these disposal methods also lead to soil hardening and alkalization, poor quality of building materials, heavy metal pollution, air pollution and other problems. While absorbing and reducing the volume of sludge and biomass, pyrolysis gasification technology not only eliminates the harm of pathogens to the environment, but also makes full use of the large amount of carbon and hydrogen resources in the raw materials to obtain diversified products, and realizes the reduction, resource utilization and harmless utilization of sludge and biomass. It is a technology with broad prospects. However, sludge has high moisture content, high ash content and low reaction activity. The yield of pyrolysis gas and tar is low when it is pyrolyzed and gasified alone, and the quality of coke is low, which is difficult to use later.

[0004] my country has abundant biomass resources, totaling about 436 million tons of standard coal per year. Biomass has a high content of alkali metal potassium and good pyrolysis and gasification reaction activity, but biomass particles have low viscosity and are difficult to form, resulting in loose and fragile coke, which is difficult to transport and use. At the same time, alkali metals are also easily released in large quantities, leading to problems such as equipment dust accumulation, slagging corrosion, and atmospheric pollutant (particulate matter) emissions.

[0005] At present, there are technologies for the co-pyrolysis of sludge and biomass, see patents CN106433713A, CN112923371A, CN109135785A, etc. However, these public sludge-biomass co-pyrolysis technologies, although they can improve the sludge pyrolysis efficiency, still have problems such as low pyrolysis gas quality, unstable components, simple mixed pyrolysis of two fuels resulting in coke in powder form that cannot be directly used, and the generation of low melting point particles.

[0006] Therefore, there is an urgent need for a sludge pyrolysis gasification method that can produce high-quality pyrolysis gas and coke and reduce the generation of particulate matter. Summary of the invention

[0007] In order to solve the above problems, the present invention provides a method for the coordinated graded conversion and resource utilization of sludge and biomass.

[0008] The present invention adopts the following technical solutions:

[0009] A method for synergistic graded conversion and resource utilization of sludge and biomass, comprising the following steps:

[0010] S1. The collected sludge and biomass are respectively aired and dried, and then crushed and sieved to a particle size between 75 and 97 μm; the sludge is municipal sludge, and the biomass is straw; in the municipal sludge, the sum of the silicon and aluminum contents in the municipal sludge ash mass proportion is greater than 40wt%, and the phosphorus content in the municipal sludge ash mass proportion is greater than 10wt%, and the silicon, aluminum and phosphorus are calculated as high-valent oxides (SiO2, Al2O3, P2O5).

[0011] S2. The sieved sludge and biomass are uniformly mixed according to a set mass ratio, placed in a mold, and pressed into a molded fuel, wherein the sludge accounts for 30wt% to 70wt% of the total mass of the sludge and biomass;

[0012] S3. The molded fuel is placed in a fixed bed reactor for pyrolysis and gasification to obtain pyrolysis gas and molded coke.

[0013] Preferably, the drying is carried out at 105° C. for at least 12 hours.

[0014] Preferably, the pressing pressure is 2 MPa and the pressing time is 2 min.

[0015] Preferably, the pyrolysis and gasification procedure is: argon atmosphere, argon flow rate 60 ml / min, heating to 1000° C. at a rate of 10° C. / min, and then cooling to room temperature at a rate of 45° C. / min.

[0016] Preferably, the molded coke is used for gasification and gas production, and the steps are: placing the molded coke in a fixed bed reactor, first stabilizing it at room temperature and argon atmosphere for 10 minutes, with the argon flow rate set to 60 mL / min, then heating it to 1000°C at a rate of 10°C / min, and maintaining the gas flow rate at 60 mL / min; when the temperature rises to 1000°C, switching the argon to a carbon dioxide atmosphere and keeping it warm for 120 minutes, with the carbon dioxide flow rate maintained at 60 mL / min, so that the molded coke is fully gasified; finally, reducing the temperature to room temperature at a rate of 45°C / min to prepare synthesis gas and ash.

[0017] The beneficial effects of the present invention are:

[0018] The present invention mixes sludge with biomass to prepare briquette fuel, effectively utilizing the alkali metal potassium rich in biomass to catalyze the pyrolysis of sludge, improving the pyrolysis efficiency and pyrolysis gas yield of sludge, and generating a large amount of briquette coke, thus realizing the high added value utilization of sludge and biomass. The graded pyrolysis and gasification of sludge and biomass briquette fuel also improves the carbon conversion rate and gas quality. Specifically:

[0019] 1) The method for preparing molded fuel by mixing sludge and biomass provided by the present invention can give full play to the advantages of the two fuels. On the one hand, it effectively utilizes the alkali metal potassium rich in the biomass to catalyze the pyrolysis of the sludge to improve the pyrolysis efficiency and pyrolysis gas yield of the sludge during the pyrolysis process, and increase the output of high-quality, component-stable synthesis gas and molded coke. On the other hand, it strengthens the fixation of potassium in the biomass by phosphates and ash rich in silicon and aluminum in the sludge. During the pyrolysis and gasification process of molded fuel, the release of alkali metals into the gas phase needs to overcome diffusion resistance. The phosphates and silicon-aluminum-containing ash in the sludge effectively inhibit the release of alkali metal potassium, thereby reducing the generation of low-melting-point fine particles, alleviating the dust and slagging phenomenon of equipment, reducing corrosion to equipment and the generation of pollutants, and reducing environmental pollution.

[0020] 2) Compared with direct pyrolysis or continuous pyrolysis gasification of unformed sludge and biomass mixed fuel, the method of the present invention separates pyrolysis and gasification, which can not only improve the efficiency of the pyrolysis stage, produce pyrolysis gas with higher content of CH4, CO, and H2 and stable components, but also generate a large amount of formed coke with a certain strength. The gas production rate (CH4 and CO production rate) of the regasification of formed coke is also higher than the gasification rate of the gasification stage in continuous pyrolysis gasification, and the effect is better. In addition, in addition to being used for gasification, formed coke can also be used for ironmaking or preparation of carbon materials, etc., which broadens the scope of use of pyrolytic coke, and formed coke has more advantages in transportation and utilization. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a comparison chart of the pyrolysis gas components after changing the sludge and straw mixing molding method in Example 2 of the present invention (red, molded fuel) and Comparative Example 1 (green, ordinary mixing), in which (a) is the CO production, (b) is the H2 production, and (c) is the CH4 production.

[0022] Figure 2 The following are comparison diagrams of segmented pyrolysis and gasification products and continuous pyrolysis and gasification products of Examples 1-3 and Comparative Examples 1-3 of the present invention at different sludge and straw ratios. (a) is a comparison diagram of segmented pyrolysis and gasification products and continuous pyrolysis and gasification products when the sludge ratio is 30wt% and the straw ratio is 70wt%; (b) is a comparison diagram of segmented pyrolysis and gasification products and continuous pyrolysis and gasification products when the sludge ratio is 50wt% and the straw ratio is 50wt%; (c) is a comparison diagram of segmented pyrolysis and gasification products and continuous pyrolysis and gasification products when the sludge ratio is 70wt% and the straw ratio is 30wt%. DETAILED DESCRIPTION

[0023] The technical solution of the present invention is described in more detail below in conjunction with the embodiments.

[0024] As shown in Table 1 and Table 2 below, the sludge used in this experiment is municipal sludge, which has the characteristics of high silicon, high aluminum and high phosphorus; the biomass is straw, which is high potassium biomass.

[0025] Table 1 Industrial analysis and elemental analysis of municipal sludge and straw

[0026]

[0027]

[0028] M-moisture; A-ash; V-volatile matter; FC-fixed carbon; St-total sulfur

[0029] Table 2 Ash chemical composition of municipal sludge and straw

[0030]

[0031] Example 1

[0032] A method for synergistic graded conversion and resource utilization of sludge and biomass, comprising the following steps:

[0033] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0034] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0035] S2. First, the sludge particles and biomass particles are artificially and evenly mixed in a mass ratio of 3:7 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing; then a certain amount of the fully mixed fuel is put into a mold, and after vibrating and flattening the material, the mold is placed in a tablet press and pressed at a pressure of 2 MPa for 2 minutes to prepare a cylindrical solid fuel with a diameter of about 25 mm.

[0036] S3. Put the prepared solid particle fuel into a crucible and then into a fixed bed reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. After the temperature rises to 1000℃, it is lowered to room temperature at a rate of 45℃ / min to prepare cylindrical coke and pyrolysis gas.

[0037] The pyrolysis gas obtained in step S3 is collected into a gas bag, and the gas composition is detected by a mass spectrometer.

[0038] The cylindrical coke obtained in step S3 is collected and placed in a fixed bed reactor. It is first stabilized at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60 mL / min. Then the temperature is raised to 1000°C at a rate of 10°C / min, and the gas flow rate is maintained at 60 mL / min. When the temperature rises to 1000°C, the argon gas is switched to a carbon dioxide atmosphere and the temperature is kept constant for 120 minutes, and the carbon dioxide flow rate is maintained at 60 mL / min to fully gasify the coke. Finally, it is reduced to room temperature at a rate of 45°C / min to prepare synthesis gas and ash.

[0039] The synthesis gas is collected using a gas bag, and the gas composition is detected using a mass spectrometer.

[0040] Example 2

[0041] A method for synergistic graded conversion and resource utilization of sludge and biomass, comprising the following steps:

[0042] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0043] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0044] S2. First, sludge particles and biomass particles are artificially and evenly mixed in a mass ratio of 1:1 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing; then a certain amount of the fully mixed fuel is put into a mold, and after vibrating and flattening the material, the mold is placed in a tablet press and pressed at a pressure of 2 MPa for 2 minutes to prepare a cylindrical solid fuel with a diameter of about 25 mm.

[0045] S3. Put the prepared solid particle fuel into a crucible and then into a fixed bed reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. When the temperature rises to 1000℃, reduce it to room temperature at a rate of 45℃ / min, and prepare cylindrical coke and pyrolysis gas.

[0046] The pyrolysis gas obtained in step S3 is collected into a gas bag, and the gas composition is detected by a mass spectrometer.

[0047] Furthermore, the cylindrical coke formed in step S3 is placed in a fixed bed reactor. First, it is stabilized at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60 mL / min. Then, the temperature is raised to 1000°C at a rate of 10°C / min, and the gas flow rate is maintained at 60 mL / min. When the temperature rises to 1000°C, the argon gas is switched to a carbon dioxide atmosphere and kept warm for 120 minutes, and the carbon dioxide flow rate is maintained at 60 mL / min, so that the coke is fully gasified. Finally, it is reduced to room temperature at a rate of 45°C / min to prepare synthesis gas and ash.

[0048] The synthesis gas is collected and the gas composition is detected by a mass spectrometer.

[0049] Example 3

[0050] A method for synergistic graded conversion and resource utilization of sludge and biomass, comprising the following steps:

[0051] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0052] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0053] S2. First, the sludge particles and biomass particles are artificially and evenly mixed in a mass ratio of 7:3 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing; then a certain amount of the fully mixed fuel is put into a mold, and after vibrating and flattening the material, the mold is placed in a tablet press and pressed at a pressure of 2 MPa for 2 minutes to prepare a cylindrical solid fuel with a diameter of about 25 mm.

[0054] S3. Put the prepared solid particle fuel into a crucible and then into a fixed bed reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. After the temperature rises to 1000℃, it is lowered to room temperature at a rate of 45℃ / min to prepare cylindrical coke and pyrolysis gas.

[0055] The pyrolysis gas obtained in step S3 is collected into a gas bag, and the gas composition is detected by a mass spectrometer.

[0056] The cylindrical coke obtained in step S3 is collected and placed in a fixed bed reactor. It is first stabilized at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60 mL / min. Then the temperature is raised to 1000°C at a rate of 10°C / min, and the gas flow rate is maintained at 60 mL / min. When the temperature rises to 1000°C, the argon gas is switched to a carbon dioxide atmosphere and the temperature is kept constant for 120 minutes, and the carbon dioxide flow rate is maintained at 60 mL / min to fully gasify the coke. Finally, it is reduced to room temperature at a rate of 45°C / min to prepare synthesis gas and ash.

[0057] The synthesis gas is collected using a gas bag, and the gas composition is detected using a mass spectrometer.

[0058] Comparative Example 1

[0059] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0060] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0061] S2. First, the sludge particles and biomass particles are evenly mixed manually in a mass ratio of 1:1 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing.

[0062] S3. Take a certain amount of fully mixed fuel and put it into a crucible, and then put it into a thermogravimetric reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. When the temperature rises to 1000℃, it is lowered to room temperature at a rate of 45℃ / min to prepare cylindrical coke and pyrolysis gas.

[0063] The pyrolysis gas obtained in step S3 is collected into a gas bag, and the gas composition is detected by a mass spectrometer.

[0064] Comparative Example 2

[0065] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0066] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0067] S2. First, the sludge particles and biomass particles are artificially and evenly mixed in a mass ratio of 3:7 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing; then a certain amount of the fully mixed fuel is put into a mold, and after vibrating and flattening the material, the mold is placed in a tablet press and pressed at a pressure of 2 MPa for 2 minutes to prepare a cylindrical solid fuel with a diameter of about 25 mm.

[0068] S3. Put the prepared solid particle fuel into a crucible and then into a fixed bed reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. When the temperature rises to 1000℃, switch the argon to a carbon dioxide atmosphere and keep it warm for 120 minutes, and maintain the carbon dioxide flow rate at 60mL / min to fully gasify the coke. Finally, reduce it to room temperature at a rate of 45℃ / min to prepare synthesis gas and ash.

[0069] The synthesis gas is collected and the gas composition is detected by a mass spectrometer.

[0070] Comparative Example 3

[0071] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0072] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0073] S2. First, sludge particles and biomass particles are artificially and evenly mixed in a mass ratio of 1:1 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing; then a certain amount of the fully mixed fuel is put into a mold, and after vibrating and flattening the material, the mold is placed in a tablet press and pressed at a pressure of 2 MPa for 2 minutes to prepare a cylindrical solid fuel with a diameter of about 25 mm.

[0074] S3. Put the prepared solid particle fuel into a crucible and then into a fixed bed reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. When the temperature rises to 1000℃, switch the argon to a carbon dioxide atmosphere and keep it warm for 120 minutes, and maintain the carbon dioxide flow rate at 60mL / min to fully gasify the coke. Finally, reduce it to room temperature at a rate of 45℃ / min to prepare synthesis gas and ash.

[0075] The synthesis gas is collected and the gas composition is detected by a mass spectrometer.

[0076] Comparative Example 4

[0077] S1. Spread the collected sludge evenly in a container and put it in a blast drying oven for drying at 105°C for 12 hours. Then put the sludge in a grinder and grind it quickly for 30 seconds. After taking it out, use a 160-200 mesh sieve to sieve it into particles with a diameter of about 75-97 microns;

[0078] Similarly, the collected biomass was evenly spread in a container and placed in a forced air drying oven for 12 hours at 105°C. The biomass was then placed in a grinder and rapidly ground for 30 seconds, and after being taken out, it was sieved using a 160-200 mesh sieve into particles with a diameter of about 75-97 microns.

[0079] S2. First, the sludge particles and biomass particles are artificially and evenly mixed in a mass ratio of 7:3 and placed in a closed container to obtain fuel, and then a vortex mixer is used to oscillate and mix for 3 minutes to improve the uniformity of the fuel mixing; then a certain amount of the fully mixed fuel is put into a mold, and after vibrating and flattening the material, the mold is placed in a tablet press and pressed at a pressure of 2 MPa for 2 minutes to prepare a cylindrical solid fuel with a diameter of about 25 mm.

[0080] S3. Put the prepared solid particle fuel into a crucible and then into a fixed bed reactor. First, stabilize it at room temperature and argon atmosphere for 10 minutes, and the argon flow rate is set to 60mL / min. Then, heat it to 1000℃ at a rate of 10℃ / min, and keep the gas flow rate at 60mL / min. When the temperature rises to 1000℃, switch the argon to a carbon dioxide atmosphere and keep it warm for 120 minutes, and maintain the carbon dioxide flow rate at 60mL / min to fully gasify the coke. Finally, reduce it to room temperature at a rate of 45℃ / min to prepare synthesis gas and ash.

[0081] The synthesis gas is collected and the gas composition is detected by a mass spectrometer.

[0082] Figure 1 The pyrolysis gas composition comparison diagram of Example 2 (red, molding and mixing) of the present invention and Comparative Example 1 (green, ordinary mixing) after changing the sludge and straw mixing molding method, in which (a) is the CO production, (b) is the H2 production, and (c) is the CH4 production. It can be seen from the figure that pyrolysis after molding sludge and straw can significantly increase the production of CO, H2, and CH4 in the pyrolysis gas.

[0083] Figure 2 The following is a comparison chart of the products of staged pyrolysis and gasification (formed coke and then gasification) and continuous pyrolysis and gasification at different sludge and straw ratios in Examples 1-3 of the present invention and Comparative Examples 1-3. It can be seen from the figure that in a CO2 gasification atmosphere, the staged pyrolysis and gasification process of sludge and straw with different mixing ratios first pyrolyzing and then gasifying can stably increase the production of CH4 and CO.

[0084] The above implementation modes are only used to illustrate the technical solutions of the present invention, but not to limit the present invention. Although the present invention has been described in detail with reference to the above implementation modes, those skilled in the art should understand that any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for the coordinated hierarchical conversion and resource utilization of sludge and biomass, characterized in that: The following steps are involved: S1. The collected sludge and biomass are respectively dried and crushed and sieved to a particle size between 75 and 97 μm, wherein the sludge is municipal sludge and the biomass is straw; S2. The sieved sludge and biomass are uniformly mixed according to a set mass ratio, placed in a mold, and pressed into a molded fuel, wherein the sludge accounts for 30wt% to 70wt% of the total mass of the sludge and biomass; S3. The molded fuel is placed in a fixed bed reactor for pyrolysis and gasification to obtain pyrolysis gas and molded coke.

2. The method for synergistic graded conversion and resource utilization of sludge and biomass according to claim 1, characterized in that: The drying is carried out at 105° C. for at least 12 hours.

3. The method for synergistic graded conversion and resource utilization of sludge and biomass according to claim 1, characterized in that: The pressing pressure is 2 MPa, the pressing time is 2 min, and the solid fuel is pressed into a cylindrical shape with a diameter of 25 mm.

4. The method for synergistic graded conversion and resource utilization of sludge and biomass according to claim 1, characterized in that: The pyrolysis and gasification procedure is: argon atmosphere, argon flow rate 60 ml / min, heating to 1000° C. at a rate of 10° C. / min, and then cooling to room temperature at a rate of 45° C. / min.

Citation Information

Patent Citations

  • Sludge pyrolysis method adopting biomass adding

    CN106433713A

  • Method for treating activated sludge by co-pyrolysis of sludge and biomass

    CN109135785A

  • Sludge coupling biomass pyrolysis gasification device and method

    CN112923371A

Cited By

  • Method for mitigating alkali metal volatilization during biomass gasification

    WO2026208848A1