Semiconductor device bit line forming method, semiconductor device
By forming a fin-structured bit line contact layer and conductive layer on the semiconductor device, increasing the contact surface and optimizing the bit line contact structure, the problem of high bit line contact resistance of the semiconductor device is solved, the data reading and writing performance is improved, and the process is simplified process.
Patent Information
- Application Number
- CN201811184657.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-10-11
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2038-10-11
AI Technical Summary
Existing semiconductor devices have high bit line contact resistance, which affects the data reading and writing performance of memory cells.
By forming a fin-structured bit line contact layer and a conductive layer on the semiconductor substrate, the number of contact surfaces between the bit line and the semiconductor substrate is increased, and the bit line contact structure is optimized through selective etching of the mask layer to reduce contact resistance.
The data reading and writing performance of the memory cell is improved, the bit line contact resistance is reduced, the process flow is simple, and the practicality is high.
Smart Images

Figure CN111048467B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a method for forming a bit line of a semiconductor device and a semiconductor device. Background Art
[0002] With the development of semiconductor technology, the size of semiconductor devices is getting smaller and smaller. In the existing semiconductor manufacturing method, the contact area of the bit line formed also decreases as the size of the device decreases, which usually leads to a higher contact resistance in the bit line contact area, making it difficult for the memory cell to read and write data normally, affecting the performance of the semiconductor device.
[0003] Therefore, it is necessary to propose a new method for forming a bit line of a semiconductor device.
[0004] It should be noted that the information disclosed in the above background technology section is only used to enhance the understanding of the background of the present disclosure, and therefore may include information that does not constitute the prior art known to ordinary technicians in the field. Summary of the invention
[0005] The purpose of the present disclosure is to provide a method for forming a bit line of a semiconductor device and a semiconductor device, thereby overcoming the problem of high contact resistance of the bit line of the existing semiconductor device at least to a certain extent.
[0006] Other features and advantages of the present disclosure will become apparent from the following detailed description, or may be learned in part by the practice of the present disclosure.
[0007] According to one aspect of the present disclosure, a method for forming a bit line of a semiconductor device is provided, comprising: providing a semiconductor substrate, the semiconductor substrate comprising an active area, a shallow trench isolation structure, a buried word line and a groove above the buried word line; depositing an isolation layer, the isolation layer filling the groove and covering the upper surface of the semiconductor substrate; selectively etching the isolation layer using a first mask layer having an active area pattern so that the thickness of the isolation layer remaining in the groove is less than the depth of the groove; depositing a bit line contact layer, the bit line contact layer filling the upper surface groove of the isolation layer; depositing a bit line conductive layer; selectively etching the bit line conductive layer and the bit line contact layer using a second mask layer having a bit line pattern, the cross-sectional width of the second mask layer along any active area being greater than the cross-sectional spacing between two buried word lines in the active area along the active area.
[0008] In an exemplary embodiment of the present disclosure, a cross section of the second mask layer along any active region is aligned with a center of a cross section of a middle region of two buried word lines in the active region along the active region.
[0009] In an exemplary embodiment of the present disclosure, after depositing the bit line conductive layer, the method further includes: depositing an insulating layer; selectively etching the bit line conductive layer and the bit line contact layer using a second mask layer having a bit line pattern includes: selectively etching the insulating layer, the bit line conductive layer and the bit line contact layer using a second mask layer having a bit line pattern.
[0010] In an exemplary embodiment of the present disclosure, after selectively etching the bit line conductive layer and the bit line contact layer using a second mask layer having a bit line pattern, the method further includes: depositing a dielectric layer, the dielectric layer filling the upper surface gaps of the isolation layer and covering the upper surface of the semiconductor substrate; and forming a storage node contact plug in the dielectric layer.
[0011] In an exemplary embodiment of the present disclosure, before depositing the dielectric layer, the method further comprises: forming a barrier layer on the upper surface of the semiconductor substrate, the upper surface of the isolation layer, the sidewalls of the bit line conductive layer and the sidewalls of the bit line contact layer.
[0012] In an exemplary embodiment of the present disclosure, the material of the isolation layer is silicon nitride or silicon oxynitride, the material of the bit line contact layer is polysilicon, and the material of the bit line conductive layer includes one or more of tungsten, titanium tungsten, and titanium nitride.
[0013] In an exemplary embodiment of the present disclosure, the material of the insulating layer includes one or more of silicon dioxide, silicon nitride, and silicon oxynitride.
[0014] According to one aspect of the present disclosure, there is provided a semiconductor device, comprising: a semiconductor substrate, in which a plurality of active areas arranged in an array and shallow trench isolation structures between the active areas are arranged; a buried word line, located in the semiconductor substrate and intersecting with the array of the active areas; a groove, located above the buried word line; an isolation layer, partially filling the groove and covering the buried word line; a bit line contact layer, the bottom of which is a fin structure, located above the area between the buried word lines in each of the active areas, and the two bottom corners of the bit line contact layer are respectively located in two grooves in the same active area; a bit line conductive layer, the top view projection of which is a strip, the bit line conductive layer covers the upper surface of the bit line contact layer and intersects with the array of the active areas.
[0015] In an exemplary embodiment of the present disclosure, the method further includes: an insulating layer covering an upper surface of the bit line conductive layer.
[0016] In an exemplary embodiment of the present disclosure, the device further includes: a dielectric layer filling the upper surface of the semiconductor device and having an upper surface flush with the bit line conductive layer.
[0017] The exemplary embodiments of the present disclosure have the following beneficial effects:
[0018] On the one hand, the structure of the bit line contact in the existing semiconductor device is changed, and the number of contact surfaces between the bit line contact layer and the semiconductor substrate is increased by side contact, fin structure, etc., thereby increasing the area of the bit line contact, reducing the contact resistance, and improving the data reading and writing performance of the storage unit. On the other hand, this exemplary embodiment controls the cross-sectional width of the second mask layer and selectively etches the bit line contact layer through the second mask layer to achieve structural improvement of the bit line contact, with a simple process flow and high practicality.
[0019] It is to be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present disclosure. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The accompanying drawings herein are incorporated into the specification and constitute a part of the specification, illustrate embodiments consistent with the present disclosure, and together with the specification are used to explain the principles of the present disclosure. Obviously, the accompanying drawings described below are only some embodiments of the present disclosure, and for ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without creative work.
[0021] Figure 1 A flowchart showing a method for forming a bit line of a semiconductor device in this exemplary embodiment;
[0022] Figures 2 to 17 A flowchart showing a method for forming a bit line of a semiconductor device in this exemplary embodiment is shown;
[0023] Fig.18 and Fig.19 A sub-flow chart showing a method for forming a bit line of a semiconductor device in this exemplary embodiment;
[0024] Figure 20 to Figure 22 A sub-flow chart showing another method for forming a bit line of a semiconductor device in this exemplary embodiment;
[0025] Fig.23 and Fig.24 A schematic structural diagram of a semiconductor device in this exemplary embodiment is shown;
[0026] Fig.25 A schematic structural diagram of another semiconductor device in this exemplary embodiment is shown. DETAILED DESCRIPTION
[0027] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the examples set forth herein; rather, these embodiments are provided so that the disclosure will be more comprehensive and complete and to fully convey the concepts of the example embodiments to those skilled in the art. The described features, structures, or characteristics may be combined in any suitable manner in one or more embodiments.
[0028] The exemplary embodiment of the present disclosure first provides a method for forming a bit line of a semiconductor device, referring to Figure 1 and Figure 2 to Figure 17 As shown, the method may include the following steps S110 to S160:
[0029] Step S110, reference Figure 2 and Figure 3 , a semiconductor substrate 101 is provided, the semiconductor substrate 101 includes an active area 102 , a shallow trench isolation structure 104 , a buried word line 103 and a groove 105 above the buried word line 103 .
[0030] Figure 2 is a top view of the semiconductor substrate 101, and a side view is made in the AA′ and BB′ directions, respectively, Figure 3 The semiconductor substrate 101 may be a p-type silicon substrate, an n-type silicon substrate, a silicon germanium substrate, etc. The active regions 102 are usually arranged in an array in the semiconductor substrate 101 and separated by a shallow trench isolation structure 104; a source and a drain may be pre-formed in the active region 102, or the positions of the source and the drain may be pre-defined, and in the process of forming the bit line in this embodiment, the source and the drain are formed at the corresponding positions of the semiconductor substrate 101 by an ion implantation process.
[0031] The buried word line 103 may intersect with the active area 102, and generally includes a word line conductive layer and a gate electrode layer. The gate electrode layer is located in the area where the buried word line 103 intersects with the active area 102, and may be made of polysilicon. The word line conductive layer is located above the gate electrode layer, and may be made of tungsten. An adhesion layer formed of a conductive material such as titanium nitride or titanium may be added between the two, and this is not particularly limited in this embodiment. When forming the buried word line 103, a buried word line hole may be formed first, and then the materials of the gate electrode layer and the word line conductive layer may be filled therein. The buried word line hole may be incompletely filled, or may be etched back after filling, thereby leaving a groove of a certain depth in the buried word line hole, so that an isolation material may be filled in the groove later to isolate the buried word line 103 from the structure above.
[0032] Step S120, reference Figure 4 , an isolation layer 106 is deposited, and the isolation layer 106 fills the groove and covers the upper surface of the semiconductor substrate 101.
[0033] Among them, the isolation layer 106 can be used to isolate the buried word line from other structures subsequently formed above, and can be made of isolation materials such as silicon dioxide, borophosphosilicate glass, etc.; in an exemplary embodiment, the material of the isolation layer 106 can be silicon nitride or silicon oxynitride. These two materials have good insulation properties, and the silicon-nitrogen bonds therein are conducive to selective etching in subsequent steps.
[0034] The isolation layer 106 may be deposited by a CVD (Chemical Vapor Deposition) process. During the deposition process, the grooves above the buried word lines are first filled, and then the entire upper surface of the semiconductor substrate 101 is covered to form a complete isolation layer 106. In an exemplary embodiment, after the isolation layer 106 is deposited, the upper surface of the isolation layer 106 may be planarized by a CMP (Chemical Mechanical Polishing) process to obtain a flat film layer.
[0035] Step S130, reference Figures 5 to 8 The isolation layer 106 is selectively etched using the first mask layer 107 having the active area pattern, so that the thickness of the isolation layer 106 remaining in the groove is smaller than the depth of the groove.
[0036] The active area pattern can be Figure 5 As shown, a pattern of the first mask layer 107 exposing the active area 102 is formed along the direction of the active area 102. During the etching process, the isolation layer 106 above the active area 102 is removed, and the isolation layer 106 above the shallow trench isolation structure 104 is retained; the semiconductor substrate 101 can be used as an etching stop layer, and a certain degree of over-etching can be performed to etch a portion of the isolation layer 106 in the groove, leaving a shallow groove with a smaller depth. Note that in this process, the isolation layer 106 in the groove needs to be over-etched to a certain extent, but it cannot be completely etched, which will affect the isolation protection of the buried word line 103.
[0037] In an exemplary embodiment, a groove with a greater depth may be reserved in advance above the buried word line 103 , and the depth of over-etching may be controlled within a larger range in step S130 to control the thickness of the remaining isolation layer 106 .
[0038] In an exemplary embodiment, when the material of the isolation layer 106 is silicon nitride, tetrafluoromethane and oxygen can be used as etching gases in step S130 to perform dry etching, which has a better etching effect on silicon nitride and a poorer etching effect on silicon dioxide for silicon substrates or shallow trench isolation. The isolation layer 106 can be effectively removed, and the surface structure of the semiconductor substrate 101 can be retained.
[0039] Step S140, reference Fig. 9 and Fig.10 , a bit line contact layer 108 is deposited, and the bit line contact layer 108 fills the upper surface trench of the isolation layer 106 .
[0040] Refer to the above Figure 7 and Figure 8 As shown, after the isolation layer 106 is selectively etched in step S130, the isolation layer 106 above the shallow trench isolation structure 104 between the active areas 102 is retained, so that more trenches appear on the upper surface of the isolation layer 106, that is, trenches along the direction of the active area 102. In step S140, the bit line contact layer 108 can be deposited to fill the above-mentioned trenches. In other words, the bit line contact layer 108 can fill the remaining grooves above the buried word line 103 and cover the upper surface of the active area 102.
[0041] It should be noted that the upper surface of the bit line contact layer 108 can be flush with the upper surface of the insulating layer, and the deposition process conditions can be controlled to obtain a bit line contact layer 108 of appropriate thickness; or a certain degree of over-deposition can be performed, and then the excess bit line contact layer 108 can be removed through a CMP process to obtain a flat upper surface of the bit line contact layer 108 and the isolation layer 106, and the CMP process can use the isolation layer 106 as the termination layer.
[0042] The bit line contact layer 108 may be formed of a conductive material, for example, metal tungsten, titanium, aluminum, etc. may be deposited using a PVD (Physical Vapor Deposition) process; in an exemplary embodiment, the material of the bit line contact layer 108 may also be polysilicon, which has good conductivity and good contact performance with the semiconductor substrate 101.
[0043] Step S150, reference Fig.11 and Fig.12 , a bit line conductive layer 109 is deposited.
[0044] The bit line conductive layer 109 may cover the upper surface of the entire device structure, specifically, cover the upper surfaces of the bit line contact layer 108 and the isolation layer 106 .
[0045] In an exemplary embodiment, the material of the bit line conductive layer 109 may include one or more of tungsten, titanium tungsten, and titanium nitride. When multiple materials are included, the bit line conductive layer 109 may be formed by depositing the multiple materials simultaneously, and the various material components are uniformly distributed in the bit line conductive layer 109.
[0046] In an exemplary embodiment, the material of the bit line conductive layer 109 and the bit line contact layer 108 can be the same, for example, both can be tungsten. Usually, before depositing the bit line contact layer 108, an adhesion layer can be formed first. The adhesion layer is generally a titanium nitride layer. Then, the deposition of the bit line conductive layer 109 and the bit line contact layer 108 can be completed by one deposition, and excess tungsten is deposited to cover the upper surface of the isolation layer 106.
[0047] Step S160, reference Figures 13 to 17 The bit line conductive layer 109 and the bit line contact layer 108 are selectively etched using a second mask layer 110 having a bit line pattern, wherein the cross-sectional width of the second mask layer 110 along any active area 102 is greater than the cross-sectional spacing between two buried word lines 103 in the active area 102 along the active area 102 .
[0048] like Fig.13 and Fig.15 As shown, the second mask layer 110 defines a bit line pattern, intersecting with the active area 102, and the intersecting area is the area where the bit line contacts. The second mask layer 110 covers the bit line area and exposes the area outside the bit line. Fig.14 As shown, the cross-sectional width of the second mask layer 110 along the active area 102 is H, and the cross-sectional spacing between the two buried word lines 103 in the active area 102 along the active area 102 is h, and H>h. During the etching process, only the bit line conductive layer 109 and the bit line contact layer 108 below the second mask layer 110 are retained, wherein, in the shallow grooves above the two buried word lines 103 in the same active area 102, the bit line contact layer 108 in at least one shallow groove is partially retained, Fig.16 and Fig.17 It is shown that the bit line contact layer 108 is partially retained in two shallow grooves at the same time. In other cases, it can also be only partially retained in the shallow groove on the left or the shallow groove on the right. In addition to contacting the upper side of the semiconductor substrate 101, the bit line contact layer 108 also forms at least one side contact, thereby increasing the area of the bit line contact and reducing the contact resistance.
[0049] In an exemplary embodiment, the cross section of the second mask layer 110 along any active region 102 can be aligned with the center of the cross section of the middle region of the two buried word lines 103 in the active region 102 along the active region 102, that is, the cross section of the second mask layer 110 exceeds the boundary of the middle region of the buried word line 103 on both sides. After selective etching using the second mask layer 110, the following can be formed: Fig.17 The bottom is a bit line contact layer 108 of a fin structure, which is equivalent to forming contact with the semiconductor substrate 101 on three sides, which can further increase the area of the bit line contact and reduce the contact resistance.
[0050] It should be noted that the materials of the first mask layer 107 and the second mask layer 110 may be the same or different. Generally, the first mask layer 107 and the second mask layer 110 may be formed by stacking a bottom anti-reflection coating (BARC) and a photoresist layer (PR). In some embodiments, in order to further protect the structure below the first mask layer 107 or the second mask layer 110 from being etched, a hard mask layer of silicon oxide or silicon nitride may be added above the photoresist layer. This exemplary embodiment does not specifically limit this.
[0051] Based on the above description, in this exemplary embodiment, on the one hand, the structure of the bit line contact in the existing semiconductor device is changed, and the number of contact surfaces between the bit line contact layer 108 and the semiconductor substrate 101 is increased by side contact, fin structure, etc., thereby increasing the area of the bit line contact, reducing the contact resistance, and improving the data reading and writing performance of the storage unit. On the other hand, this exemplary embodiment controls the cross-sectional width of the second mask layer 110 and selectively etches the bit line contact layer 108 through the second mask layer 110 to achieve the structural improvement of the bit line contact, and the process flow is simple and the practicability is high.
[0052] In an exemplary embodiment, after step S150, the method for forming a bit line of a semiconductor device may further include the following steps:
[0053] refer to Fig.18 , depositing an insulating layer 111;
[0054] Accordingly, step S160 can be implemented by the following steps:
[0055] The insulating layer, the bit line conductive layer 109 and the bit line contact layer 108 are selectively etched using the second mask layer 110 having the bit line pattern; Fig.19 The structure shown.
[0056] The insulating layer 111 covers the upper surface of the bit line conductive layer 109. Usually, in the subsequent process, a capacitor structure will also be formed, so the insulating layer 111 can insulate and isolate the bit line structure. After the insulating layer is deposited, the insulating layer 111 needs to be etched in step S160. Depending on the actual situation, step-by-step etching or one-step etching can be used.
[0057] In an exemplary embodiment, the material of the insulating layer 111 may include one or more of silicon dioxide, silicon nitride, and silicon oxynitride, all of which have good insulation and isolation properties. When the insulating layer 111 includes multiple material components, it may be a stack of multiple single-component film layers.
[0058] In an exemplary embodiment, after step S160, the method for forming a bit line of a semiconductor device may further include the following steps:
[0059] refer to Fig. 20 , depositing a dielectric layer 112 , the dielectric layer 112 fills the upper surface gap of the isolation layer 106 and covers the upper surface of the semiconductor substrate 101 ;
[0060] refer to Fig.21 , a storage node contact plug 113 is formed in the dielectric layer 112 .
[0061] The dielectric layer 112 may be a silicon dioxide layer or a composite layer of a silicon nitride / silicon dioxide / silicon nitride structure. The dielectric layer 112 may be used to form an inter-level dielectric (ILD) structure and play a certain role in fixing and protecting the bit line structure. The storage node contact plug 113 is used to form a contact between the semiconductor substrate 101 and the capacitor element formed above in the subsequent process. Conductive materials such as polysilicon, titanium nitride, titanium, tungsten, etc. may be used. The storage node contact plug 113 of a stacked structure may also be formed by these materials. This embodiment does not specifically limit this.
[0062] For further reference, Fig. 22 Before depositing the dielectric layer 112, a barrier layer 114 may be formed on the upper surface of the semiconductor substrate 101, the upper surface of the isolation layer 106, the sidewalls of the bit line conductive layer 109, and the sidewalls of the bit line contact layer 108. The material of the barrier layer 114 may include one or more of silicon dioxide, silicon nitride, and silicon oxynitride. The barrier layer 114 may further play an insulating and isolating role. In an exemplary embodiment, the barrier layer 114 may be formed by an ALD (Atomic layer deposition) process, which is conducive to controlling the thickness and uniformity of the barrier layer 114.
[0063] The exemplary embodiments of the present disclosure also provide a semiconductor device. The structure of the semiconductor device can refer to Fig.23 and Fig.24As shown, it includes: a semiconductor substrate 101, in which a plurality of active areas 102 and shallow trench isolation structures 104 are arranged between the active areas 102; buried word lines 103, located in the semiconductor substrate 101 and intersecting with the active areas 102; grooves 105, located above the buried word lines 103; an isolation layer 106, partially filling the grooves 105 and covering the buried word lines 103; a bit line contact layer 108, the bottom of which is a fin structure, located above the area between the buried word lines 103 in each active area 102, and the two bottom corners of the bit line contact layer 106 are respectively located in two grooves 105 in the same active area 102; a bit line conductive layer 109, the top view projection of which is a strip, covers the upper surface of the bit line contact layer 108, and intersects with the array of active areas 102.
[0064] Based on the structure of the semiconductor device, on the one hand, the structure of the bit line contact in the existing semiconductor device is changed, and the number of contact surfaces between the bit line contact layer and the semiconductor substrate is increased by side contact, fin structure, etc., thereby increasing the area of the bit line contact, reducing the contact resistance, and improving the data reading and writing performance of the storage unit. On the other hand, the semiconductor device of this exemplary embodiment can be formed by the method in the above embodiment, and its process flow is simple and has high practicality.
[0065] In an exemplary embodiment, referring to the above Fig.19 As shown, the semiconductor device may further include an insulating layer 111 covering an upper surface of the bit line conductive layer 109 .
[0066] In an exemplary embodiment, referring to the above Fig. 20 As shown, the semiconductor device further includes a dielectric layer 112 filling the upper surface of the semiconductor device and having an upper surface flush with the bit line conductive layer 109 .
[0067] In an exemplary embodiment, referring to the above Fig.21 As shown, the semiconductor device further includes a storage node contact plug 113 located in the dielectric layer 112 .
[0068] In an exemplary embodiment, referring to the above Fig. 22 As shown, the semiconductor device further includes a barrier layer 114 , which covers the upper surface of the semiconductor substrate 101 , the upper surface of the isolation layer 106 , the sidewalls of the bit line conductive layer 109 , and the sidewalls of the bit line contact layer 108 .
[0069] In an exemplary embodiment, the structure of the semiconductor device can refer to Fig.25 As shown, the bit line structure includes a fin-type bit line contact layer 108 and a bit line conductive layer 109, and a barrier layer 114 is formed on the outer wall; the upper surface gap of the semiconductor device is filled with a dielectric layer 112, and a storage node contact plug 113 is also provided in the dielectric layer 112.
[0070] Those skilled in the art will readily appreciate other embodiments of the present disclosure after considering the specification and practicing the invention disclosed herein. This application is intended to cover any variations, uses, or adaptations of the present disclosure that follow the general principles of the present disclosure and include common knowledge or customary technical means in the art that are not disclosed in the present disclosure. The specification and examples are to be regarded as exemplary only, and the true scope and spirit of the present disclosure are indicated by the claims.
[0071] It should be understood that the present disclosure is not limited to the exact structures that have been described above and shown in the drawings, and that various modifications and changes may be made without departing from the scope thereof. The scope of the present disclosure is limited only by the appended claims.
Claims
1. A method for forming a bit line of a semiconductor device, characterized in that: include: Providing a semiconductor substrate, the semiconductor substrate comprising an active area, a shallow trench isolation structure, a buried word line, and a groove above the buried word line; Depositing an isolation layer, wherein the isolation layer fills the groove and covers the upper surface of the semiconductor substrate; Selectively etching the isolation layer using the first mask layer having the active area pattern so that the thickness of the isolation layer remaining in the groove is smaller than the depth of the groove; Depositing a bit line contact layer, wherein the bit line contact layer fills the upper surface groove of the isolation layer; depositing a bit line conductive layer; The bit line conductive layer and the bit line contact layer are selectively etched using a second mask layer having a bit line pattern, wherein a cross-sectional width of the second mask layer along any of the active regions is greater than a cross-sectional spacing between two buried word lines in the active region along the active region; forming a barrier layer on the upper surface of the semiconductor substrate, the upper surface of the isolation layer, the sidewalls of the bit line conductive layer, and the sidewalls of the bit line contact layer; Depositing a dielectric layer on the barrier layer, wherein the dielectric layer fills the upper surface gap of the isolation layer and covers the upper surface of the semiconductor substrate; Storage node contact plugs are formed in the dielectric layer.
2. The method according to claim 1, characterized in that A cross section of the second mask layer along any of the active regions is aligned with a center of a cross section of a middle region of two buried word lines in the active region along the active region.
3. The method according to claim 1, characterized in that After depositing the bit line conductive layer, the method further comprises: Depositing an insulating layer; The selective etching of the bit line conductive layer and the bit line contact layer by using the second mask layer having the bit line pattern comprises: The insulating layer, the bit line conductive layer and the bit line contact layer are selectively etched using a second mask layer having a bit line pattern.
4. The method according to claim 1, characterized in that The material of the isolation layer is silicon nitride or silicon oxynitride, the material of the bit line contact layer is polysilicon, and the material of the bit line conductive layer includes one or more of tungsten, titanium tungsten, and titanium nitride.
5. The method according to claim 3, characterized in that: The material of the insulating layer includes one or more of silicon dioxide, silicon nitride, and silicon oxynitride.
6. A semiconductor device, characterized in that: include: A semiconductor substrate, wherein a plurality of active areas arranged in an array and shallow trench isolation structures between the active areas are disposed in the semiconductor substrate; a buried word line located within the semiconductor substrate and intersecting the array of active areas; a groove located above the buried word line; an isolation layer partially filling the groove and covering the buried word line; A bit line contact layer, the bottom of which is a fin structure, is located above the area between the buried word lines in each of the active regions, and two bottom corners of the bit line contact layer are respectively located in two grooves in the same active region; A bit line conductive layer, the top view projection of which is in the shape of a strip, the bit line conductive layer covers the upper surface of the bit line contact layer and intersects with the array of active areas; a barrier layer, located on the upper surface of the semiconductor substrate, the upper surface of the isolation layer, the sidewall of the bit line conductive layer, and the sidewall of the bit line contact layer; a dielectric layer disposed on the barrier layer; The storage node contact plug is located in the dielectric layer.
7. The semiconductor device according to claim 6, characterized in that Also includes: An insulating layer covers the upper surface of the bit line conductive layer.
8. The semiconductor device according to claim 6, characterized in that Also includes: A dielectric layer fills the upper surface of the semiconductor device and has an upper surface flush with the bit line conductive layer.