A licker-in roller with ultra-wear-resistant nano coating

By spraying the nanoprotective layer of metal cermet composite coating on the burr roller, the problems of unstable rotation and roller surface wear during high-speed operation are solved, the service life is extended and the wear resistance is improved, and more efficient production and Reduced costs.

CN111378918BActive Publication Date: 2024-11-22SHANGHAI INFOMAN NANOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010250478.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-04-01
Publication Date
2024-11-22
Estimated Expiration
2040-04-01

AI Technical Summary

Technical Problem

The existing burr rollers rotate unsteadily and have large vibrations when running at high speed, and the roller surface is fatigued and worn due to changes in temperature fields, and the service life is short. The existing solutions such as surfacing wear-resistant materials and micron coatings are difficult to effectively solve the problem. .

Method used

Using nanoprotective layers, including nano-bottom layer and ceramic surface layer of metal cermet composite coating, is sprayed on the roller body through supersonic nanothermal spraying equipment to form a wear-resistant and impact-resistant coating with a thickness of 150-200μm, which improves the The bonding force and wear resistance of the roller surface and the substrate.

Benefits of technology

The service life of the burr roller is significantly improved to 6-8 months, reducing production costs, improving working efficiency, improving the quality of the plate and belt and the wear resistance of the roller body, eliminating the vibration problems during high-speed operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111378918B_ABST
    Figure CN111378918B_ABST
Patent Text Reader

Abstract

The present invention discloses a super wear-resistant nano coating for a burr roller, wherein a nano protective layer is coated on the surface of the burr roller, wherein the nano protective layer is a metal ceramic composite coating, wherein the metal ceramic composite coating comprises a nano bottom layer and a nano ceramic surface layer, wherein the nano bottom layer and the nano ceramic surface layer are sprayed sequentially from the bottom layer to the surface layer. The super wear-resistant nano coating for a burr roller provided by the present invention has a wear-resistant and scratch-resistant nano coating composite material, wherein the composite material has both good physical properties and chemical stability, can improve the bonding ability between the coating and the substrate, and has both mechanical load and impact resistance, and the service life is increased from the original 2 months to more than 6-8 months, which is much longer than the service life of the burr roller in the prior art, effectively improving the unit operation rate and product quality, reducing maintenance costs, and providing reliable guarantee for customers to reduce costs and increase efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of equipment in the steel industry, and in particular to a super wear-resistant nano coating of a licker-in roller. Background Art

[0002] The current hairpin rollers are not stable enough during high-speed operation, and the vibration critical point is low and the vibration is large. It is difficult for the hairpin rollers to achieve the purpose of high-speed operation. In the actual production process, due to the uneven temperature field in the working environment of the hairpin rollers, stress is generated. As the rollers rotate, the temperature field changes periodically, and the stress also changes accordingly. The roller surface temperature is high and the fatigue strength decreases, which causes the roller surface to crack due to fatigue. At the same time, the hairpin rollers are subjected to mechanical stress during the pickling of the strips, and the roller surface is severely worn, which not only affects the quality of the strips, but also seriously affects the service life of the hairpin rollers. The service life of the hairpin rollers in the existing technical state is 2 months. The current solution is to build up the wear-resistant material on the roller surface to improve the wear resistance of the roller surface, or to use micron material to spray the wear-resistant layer to increase the service life of the roller. Both methods cannot solve the problems of roller surface wear, cracking, and the reduction of roughness leading to the slipping of the strip. The welding layer and the sprayed micron coating are easy to peel off. Summary of the invention

[0003] The object of the present invention is to provide a super wear-resistant nano coating for a burring roller to solve one or more of the above-mentioned problems in the prior art.

[0004] According to the ultra-wear-resistant nano coating of a hair pressing and lickering roller of the present invention, a nano protective layer is coated on the surface of the hair pressing and lickering roller, and the nano protective layer is a metal-ceramic composite coating, and the metal-ceramic composite coating includes a nano bottom layer and a nano ceramic surface layer, and the nano bottom layer and the nano ceramic surface layer are sprayed sequentially from the bottom layer to the surface layer.

[0005] In some embodiments, the grade of the metal-ceramic composite coating is INF-8235.

[0006] In some embodiments, the metal-ceramic composite coating has a thickness of 150-200 μm.

[0007] In some embodiments, the thickness of the nano-bottom layer is 30-50 μm, and the thickness of the nano-ceramic surface layer is 150-200 μm.

[0008] In some embodiments, a supersonic nano thermal spraying device is used to spray the nano protective layer on the roller body, and the spraying speed is 500-2500 m / s.

[0009] In some embodiments, the burr roller includes an outer roller body, an inner roller body and a rotating shaft. The inner roller body is hollow and is arranged on the inner circumferential wall of the outer roller body. The rotating shaft is inserted into the inner roller body, and the surface of the outer roller body is provided with a wear-resistant nano coating.

[0010] In some embodiments, the outer roller body is a hollow roller body, two inner ring grooves are opened on the inner circumferential wall of the outer roller body, a block bar is provided between the two inner ring grooves, and the two inner ring grooves are arranged in parallel; an outer ring groove is opened on the outer circumferential wall of the inner roller body, and an annular cavity is formed between the outer ring groove and the inner ring groove.

[0011] In some embodiments, the widths of the two inner annular grooves are equal, a plurality of rollers are placed in the inner annular grooves, and the rollers are arranged in the axial direction of the outer roller body.

[0012] In some embodiments, the rollers can roll in the annular cavity.

[0013] In some embodiments, the inner roller body abuts against the retaining ring body, and the retaining ring body also abuts against the end of the roller. The cross-section of the retaining ring body is "L"-shaped, and the side edges of the retaining ring body and the side edges of the inner roller body are clamped with each other.

[0014] The present invention provides a super wear-resistant nano coating for a hairpin roller, which is a nano-ceramic composite coating that is wear-resistant, impact-resistant and has high bonding strength. The nano coating material has both good physical properties and chemical stability, which can improve the bonding ability between the coating and the substrate, while improving the wear resistance and scratch resistance of the hairpin roller surface, and has both mechanical load and impact resistance. The service life of the hairpin roller can reach 6-8 months, which is much longer than the service life of the hairpin roller in the prior art, so that the hairpin roller can continue to work for a long time, thereby reducing production costs, improving work efficiency, and improving the defects of the prior art. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic structural diagram of the combination of an outer roller body and an inner roller body of a licker-in roller according to an embodiment of the present invention;

[0016] Figure 2 It is a structural schematic diagram of a ring body of a licker-in roller according to an embodiment of the present invention;

[0017] Figure 3 It is a structural schematic diagram of a roller body of a licker-in roller according to an embodiment of the present invention;

[0018] Figure 4 The present invention is a schematic structural diagram of a licker-in roller according to an embodiment of the present invention. DETAILED DESCRIPTION

[0019] The present invention will be further described in detail below in conjunction with the accompanying drawings.

[0020] like Figure 1 As shown in the figure, a super wear-resistant nano coating for a hair pressing and pricking roller is coated with a nano protective layer on the surface of the hair pressing and pricking roller. The nano protective layer is a metal-ceramic composite coating. The metal-ceramic composite coating includes a nano bottom layer and a nano ceramic surface layer. The nano bottom layer and the nano ceramic surface layer are sprayed from the bottom layer to the surface layer in sequence.

[0021] The nano protective layer is a metal-ceramic composite coating, which includes a nano bottom layer and a nano ceramic surface layer, and the nano bottom layer and the nano ceramic surface layer are formed by spraying from the bottom layer to the surface layer in sequence.

[0022] The base layer of the metal-ceramic composite coating is INF-8235-1, and the surface layer of the metal-ceramic composite coating is INF-8235-2.

[0023] The thickness of the nano protective layer is 150~250μm, wherein the nano bottom layer is a nano Ni-based material, and the nano ceramic layer is a ceramic-based composite layer; the thickness of the nano bottom layer is 30~50μm, and the thickness of the nano ceramic surface layer is 150-200μm. At this thickness of the nano protective layer, the entire burr roller has the effects of wear resistance, scratch resistance and impact resistance.

[0024] The nano protective layer is sprayed on the roller body 1 by using a supersonic nano thermal spraying device, and the spraying speed is 500-2500m / s

[0025] The microhardness of the prepared nano coating reaches HV900-1100, the roller surface roughness is Ra5-6, the bonding force between the coating and the substrate is above 80Mpa, and the service life is more than 6-8 months.

[0026] The present invention provides a cold-rolled burr-in roller with a wear-resistant and scratch-resistant nano-coating, which has a wear-resistant, scratch-resistant and impact-resistant nano-coating composite material. The composite material has both good physical properties and chemical stability, can improve the bonding ability of the coating and the substrate, and at the same time improves the wear resistance and scratch resistance of the surface of the burr-in roller, and has both mechanical load and impact resistance. The service life is increased from the original 2 months to more than 6-8 months, which is much longer than the service life of the cold-rolled burr-in roller in the prior art, effectively improves the unit operation rate and product quality, reduces maintenance costs, and provides reliable guarantee for customers to reduce costs and increase efficiency.

[0027] A method for preparing a wear-resistant and roughness-resistant nano-coating:

[0028] The steps include:

[0029] (1) Cleaning and degreasing: the roller body 1 is immersed in a non-ionic surfactant solution with a mass concentration of 5% to 10% for cleaning, then ultrasonically cleaned in acetone, and ventilated and dried;

[0030] (2) Sandblasting: Use first-grade brown corundum to roughen the roller surface;

[0031] (3) Preparation of the bottom layer: Using supersonic flame spraying equipment, the molten bottom layer nanomaterial is sprayed onto the roller surface of the burring roller at a rate of 500-2500 m / s, and the coating thickness is 30-50 μm;

[0032] (4) Surface layer preparation: Using supersonic flame spraying equipment, the molten surface layer nanomaterial is sprayed onto the roller surface of the burring roller at a rate of 500-2500 m / s, and the coating thickness is 150-200 um.

[0033] like Figure 1~2 As shown in the figure, a burr-pressing roller with a super wear-resistant nano coating comprises a roller body 1 and shaft bases 2 arranged at both ends of the roller body 1. The surface of the roller body 1 is coated with a nano protective layer, and the wear resistance of the surface layer of the roller body 1 can be greatly improved through the nano protective layer, and the anti-scratch ability can also be improved;

[0034] The roller body 1 includes an outer roller body 11, a hollow roller body middle part 12 and hollow roller body ends 13 located at both ends of the roller body middle part 12. The roller body middle part 12 and the roller body ends 13 are both arranged inside the outer roller body 11, and the diameter of the roller body ends 13 is larger than the diameter of the roller body middle part 12. The two ends of the roller body are widened, which can solve the defect of the unstable pressure roller in high-speed operation.

[0035] The outer roller body 1 is a hollow roller body, and two inner ring grooves 101 are provided on the inner peripheral wall of the outer roller body 1, and a block bar 102 is provided between the two inner ring grooves 101, and the two inner ring grooves 101 are arranged in parallel; an outer ring groove 201 is provided on the outer peripheral wall of the inner roller body 2, and an annular cavity is formed between the outer ring groove 201 and the inner ring groove 101. By providing the inner ring groove 101 on the outer roller body 1 and the outer ring groove 201 on the inner roller body 2, the rotation effect of the roller body as a whole is better.

[0036] The widths of the two inner ring grooves 101 are equal, and a plurality of rollers 13 are placed in the inner ring grooves 101, and the rollers 13 are arranged in the axial direction of the outer roller body 1. The rollers 13 are installed to increase the rolling of the inner roller body 2 and the outer roller body 1.

[0037] The rollers 13 can roll in the annular cavity.

[0038] The inner roller body 2 is in contact with the retaining ring body 202, which is also in contact with the end of the roller 13. The retaining ring body 202 has an L-shaped cross section, and the side of the retaining ring body 202 is engaged with the side of the inner roller body 2. Installing the retaining ring body 202 facilitates the disassembly of the outer roller body 1 and the inner roller body 2.

[0039] In the above, by increasing the width at both ends of the outer roller body 1, it is possible to ensure that the roller can remain stable and eliminate vibration during high-speed operation, thereby achieving the purpose of making the critical point outside the process speed. The operating speed of the roller can be increased to 12,000 to 18,000 rpm.

[0040] Among them, Figure 4 As shown in , the roller body diameter is 60-450mm, the diameter of the roller body end 13 is 10mm larger than the diameter of the roller body middle part 12, the roller body coating thickness is 150-200um, and the outer end surface of the roller body end (13) is provided with a connecting cylinder 14, and the connecting cylinder 14 is surrounded by a mounting base 15, and the mounting base (15) is provided with a plurality of mounting screw holes. In this embodiment, the two ends of the outer roller body 1 are widened, and the diameter of the roller body end 13 is 10mm larger than the diameter of the roller body middle part 12, which can solve the defect of the unstable pressure roller in high-speed operation.

[0041] Screw holes are also provided at positions corresponding to the mounting screw holes of the shaft base 4, and the shaft base 4 and the roller end 13 are fixedly connected by screws. The screws are installed and fixed along the axis direction, with good fixing effect, stable and convenient installation.

[0042] like Figure 3 As shown in the figure, the outer roller body 1 is provided with a ring body 5 at intervals, and the diameter of the ring body 5 is slightly larger than the diameter of the outer roller body 11. The function of the ring body 5 is to make the silk thread easy to be formed on the pressure roller, so as to become a silk cake.

[0043] The central axis of the outer roller body 1, the roller body middle part 12, the roller body end 13 and the shaft base 4 are located on the same straight line. The purpose of this design is to ensure the stability and stability of the roller speed under the same axis.

[0044] The ultra-wear-resistant nano coating of the burr-in roller provided by the present invention can eliminate the critical point and vibration of the roller during high-speed rotation by adjusting the width of the inner cavity at both ends of the sleeve, thereby achieving the purpose of stable rotation.

[0045] The above is only a preferred embodiment of the present invention. It should be pointed out that a person skilled in the art can make several similar modifications and improvements without departing from the creative concept of the present invention, and these are also considered to be within the scope of invention protection.

Claims

1. A licker-in roller with a super wear-resistant nano coating, characterized in that: The burring roller comprises a roller body and an axis base arranged at both ends of the roller body, the roller body has a diameter of 60-450㎜, the diameter of the roller body end is 10㎜ larger than the diameter of the middle part of the roller body, the roller body comprises an outer roller body, an inner roller body and a rotating shaft, the inner roller body is hollow, the inner roller body is arranged on the inner peripheral wall of the outer roller body, the rotating shaft is inserted into the inner roller body, the surface of the outer roller body is provided with a wear-resistant nano coating, the outer roller body is a hollow roller body, two inner ring grooves are opened on the inner peripheral wall of the outer roller body, a block bar is arranged between the two inner ring grooves, and the two inner ring grooves are arranged in parallel; an outer ring groove is opened on the outer peripheral wall of the inner roller body, an annular cavity is formed between the outer ring groove and the inner ring groove, the width of the two inner ring grooves is equal, a plurality of rollers are placed in the inner ring groove, the rollers can roll in the annular cavity, and the rollers are arranged in the axial direction of the outer roller body, The inner roller body is in contact with the retaining ring body, and the retaining ring body is also in contact with the end of the roller. The cross-section of the retaining ring body is "L"-shaped, and the side of the retaining ring body is clamped with the side of the inner roller body. The outer roller body is provided with a ring body at an interval, and the diameter of the ring body is slightly larger than the diameter of the outer roller body. A supersonic nano thermal spraying device is used to spray a nano protective layer on the outer roller body, and the spraying speed is 500-2500m / s. The nano protective layer is a metal-ceramic composite coating, and the metal-ceramic composite coating includes a nano bottom layer and a nano ceramic surface layer. The nano bottom layer and the nano ceramic surface layer are sprayed from the bottom layer to the surface layer in sequence. The thickness of the nano bottom layer is 30-50μm, and the thickness of the nano ceramic surface layer is 150-200μm. The nano bottom layer is a nano Ni-based material, and the nano ceramic surface layer is a ceramic-based composite layer.