A micro groove heat pipe extrusion die
By adopting detachable and connected die core and separate rear die design in micro-tree hot tube extrusion molds, the problem of difficult and cost of mold processing is solved, and the easy maintenance of the mold and the improvement of production efficiency is achieved. It is suitable for Made a shell of a micro heat pipe.
Patent Information
- Application Number
- CN202011003082.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-22
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-09-22
AI Technical Summary
The existing micro-trench hot-tube extrusion molds have problems such as easy damage to the core structure, difficult processing and high manufacturing cost. Especially when manufacturing the tube and shell of the micro-heat pipe, traditional milling processes and electric spark processing methods are difficult to meet the requirements. This results in long manufacturing cycles and high costs.
A micro-trench hot tube extrusion mold was designed, using a detachable connection structure between the die core and the front die, and processing it through a separate rear die body and die pad, reducing the processing difficulty and manufacturing cost of the mold. Structures such as welding chambers, working belts and hollow knives are used to achieve molding and shaping of extruded products.
It realizes easy replacement and maintenance of die cores, reduces the difficulty and cost of mold manufacturing, improves the scope of application and production efficiency of micro-tree hot tube extrusion molds, solves the problems of mold processing difficulties and high costs, and simplifies manufacturing process.
Smart Images

Figure CN111940534B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of mechanical devices, and in particular to a micro-sized groove heat pipe extrusion die. Background Art
[0002] As a highly efficient heat transfer element, micro heat pipes are widely used in thermal control fields such as aerospace and solar energy. For example, micro heat pipes made of aluminum alloy micro grooves are key components for solving the heat dissipation problem of high heat flux density components on satellites and other spacecraft in space environments. The groove microstructure of the liquid wick on the tube shell is at the sub-millimeter scale, which poses a severe challenge to the processing and manufacturing of the tube shell. To date, extrusion technology, especially split-flow hot extrusion, is one of the main forming processes for manufacturing heat pipe shells and other hollow profiles.
[0003] However, the existing micro-grooved heat pipe extrusion dies used for the production of micro-heat pipes often have problems such as easy damage to the core structure and complex and difficult processing of the mold, which seriously restricts the application of extrusion in the field of heat pipe manufacturing. These problems are specifically reflected in the following two aspects: First, the core structure of the micro-heat pipe has a small diameter and is extremely easy to be damaged due to poor strength and rigidity; the existing one-piece core structure not only has high processing costs, but also causes the entire mold to be scrapped after the core structure is damaged; second, the typical outer dimensions of a micro-heat pipe are usually below 4 mm, which makes the depth-to-width ratio of the die hole structure of the micro-grooved heat pipe extrusion die very large, that is, the cross-sectional size of the die hole structure is small and the depth is large, which poses a severe challenge to mold processing. The traditional milling process is difficult to meet the manufacturing requirements of the micro-grooved heat pipe extrusion die used to produce micro-heat pipes, and the currently widely used electric spark machining method will greatly increase the production cost, resulting in the mold having problems such as difficult processing, high manufacturing cost and long manufacturing cycle. Summary of the invention
[0004] The problem solved by the invention is how to make the mold core easy to replace and reduce the processing difficulty and manufacturing cost of the mold.
[0005] In order to solve the above problems, the present invention provides a micro-grooved heat pipe extrusion die, comprising a die core and a front die, a rear die body and a die pad that are detachably connected in sequence; a welding chamber is provided at the connection between the rear die body and the front die, a working belt connected to the welding chamber is provided on the rear die body, and an empty knife is provided at the connection between the rear die body and the die pad, one end of the working belt away from the welding chamber is connected to one end of the empty knife, and the other end of the empty knife passes through the die core; a mounting hole that passes through the front die is provided on the front die, and the mounting hole is connected to the welding chamber; the die core is suitable for being inserted into the mounting hole and detachably connected to the mounting hole, and one end of the die core toward the die pad extends into the working belt through the welding chamber.
[0006] Optionally, the mold core includes a positioning portion, a connecting portion and a shaping portion, and the positioning portion, the connecting portion and the shaping portion are sequentially connected in the direction from the front mold to the rear mold body; the mounting hole includes a first accommodating hole suitable for accommodating the positioning portion and a second accommodating hole suitable for accommodating the connecting portion, and the hole wall of the first accommodating hole is suitable for limiting the rotation of the positioning portion around the axis of the positioning portion; the connection between the connecting portion and the shaping portion is located in the welding chamber, and the shaping portion extends into the working belt at one end away from the connecting portion.
[0007] Optionally, the shaping portion is coaxially arranged with the working belt, and an annular gap is provided between a side wall of one end of the shaping portion extending into the working belt and an inner wall of the working belt.
[0008] Optionally, the positioning portion, the connecting portion and the shaping portion are all coaxially arranged, and the cross-sectional area of the connecting portion is larger than the cross-sectional area of the shaping portion and smaller than the cross-sectional area of the positioning portion.
[0009] Optionally, a prismatic structure and / or a groove structure is provided on the side wall of one end of the shaping portion extending into the working belt, and the extending direction of the prismatic structure and / or the groove structure is parallel to the axis of the shaping portion.
[0010] Optionally, the empty knife includes a first empty knife and a second empty knife which are connected, wherein one end of the first empty knife away from the second empty knife is connected to the working belt, and one end of the second empty knife away from the first empty knife passes through the mold pad and is connected to the outside world; and a cross-sectional area of the first empty knife is larger than a cross-sectional area of the working belt and smaller than a cross-sectional area of the second empty knife.
[0011] Optionally, the welding chamber is arranged on a side of the rear mold body facing the front mold.
[0012] Optionally, the front mold is provided with a plurality of diversion holes penetrating the front mold, and the plurality of diversion holes are all connected to the welding chamber and are arranged at intervals around the mounting hole.
[0013] Optionally, the front mold and the rear mold body are respectively provided with one of a positioning groove and a positioning platform, and the positioning platform is plug-fitted with the positioning groove.
[0014] Optionally, the micro-miniature groove heat pipe extrusion die also includes a positioning piece, and the micro-miniature groove heat pipe extrusion die is suitable for being assembled in a die base of an extruder, and the positioning piece is arranged on the outer side wall of the rear die body, and / or, is arranged on the outer side wall of the die pad, and is used to limit the micro-miniature groove heat pipe extrusion die from rotating around the axis of the micro-miniature groove heat pipe extrusion die in the die base.
[0015] Compared with the prior art, the present invention has the following beneficial effects: by setting a mold core and a mounting hole, a detachable connection between the mold core and the front mold is achieved, so that the mold core is easy to replace. On the one hand, the mold core and the front mold are suitable for separate manufacturing and molding, which reduces the manufacturing difficulty and cost of the mold core and the front mold and facilitates the later maintenance and replacement of the mold core; on the other hand, the front mold is suitable for assembling mold cores of different specifications through the mounting holes to produce extruded products of different specifications, thereby improving the application scope of the micro-grooved heat pipe extrusion mold and reducing the use cost of the micro-grooved heat pipe extrusion mold. By setting a detachably connected rear mold body and mold pad, corresponding hole-groove structures can be processed on the rear mold body and the mold pad respectively. In this way, compared with the integrated rear mold, the separate rear mold (detachably connected rear mold body and mold pad) greatly reduces the processing difficulty and processing cost of the rear mold, shortens the manufacturing cycle of the rear mold, and makes the hole-groove structures on the rear mold body and the mold pad after thickness reduction easy to process, and its processing technology can choose relatively economical and efficient milling, fast wire cutting and other processes, further reducing the manufacturing cost of the rear mold, thereby greatly reducing the processing difficulty and processing cost of the micro-groove heat pipe extrusion mold, shortening the manufacturing cycle of the micro-groove heat pipe extrusion mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 An exploded view of the structure of a micro-groove heat pipe extrusion die in an embodiment of the present invention;
[0017] Figure 2 This is a schematic diagram of the structure of a micro-groove heat pipe extrusion die in an embodiment of the present invention;
[0018] Figure 3 A schematic structural diagram of a micro-grooved heat pipe extrusion die from another perspective in an embodiment of the present invention;
[0019] Figure 4 for Figure 3 Sectional view at AA in the middle;
[0020] Figure 5 for Figure 4 A partial enlarged view of point C in the middle;
[0021] Figure 6 A structural schematic diagram of a micro-grooved heat pipe extrusion die from another perspective in an embodiment of the present invention;
[0022] Figure 7 for Figure 6 Sectional view at the middle BB.
[0023] Description of reference numerals:
[0024] 1-front mold, 11-mounting hole, 111-first accommodating hole, 112-second accommodating hole, 12-diverter hole, 13-positioning platform; 2-rear mold, 21-rear mold body, 22-mold pad, 23-welding chamber, 24-working belt, 25-empty knife, 251-first empty knife, 252-second empty knife, 26-positioning groove; 3-mold core, 31-positioning part, 32-connecting part, 33-forming part; 4-positioning piece. DETAILED DESCRIPTION
[0025] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0026] It should be noted that, in the coordinate axis X-axis provided herein, the positive direction of the X-axis represents the front, and the reverse direction of the X-axis represents the rear. At the same time, it should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein.
[0027] Combination Figure 1-Figure 7 As shown, an embodiment of the present invention provides a micro-groove heat pipe extrusion die, comprising a die core 3 and a front die 1, a rear die body 21 and a die pad 22 which are detachably connected in sequence; a welding chamber 23 is provided at the connection between the rear die body 21 and the front die 1, a working belt 24 connected to the welding chamber 23 is provided on the rear die body 21, and an empty knife 25 is provided at the connection between the rear die body 21 and the die pad 22, an end of the working belt 24 away from the welding chamber 23 is connected to one end of the empty knife 25, and the other end of the empty knife 25 passes through the die core 3; a mounting hole 11 passing through the front die 1 is provided on the front die 1, and the mounting hole 11 is connected to the welding chamber 23; the die core 3 is suitable for being inserted into the mounting hole 11 and detachably connected to the mounting hole 11, and one end of the die core 3 facing the die pad 22 extends into the working belt 24 through the welding chamber 23.
[0028] The micro-groove heat pipe extrusion die comprises a detachably connected front die 1 and a rear die 2, the rear die 2 comprises a detachably connected rear die body 21 and a die pad 22, and the front die 1, the rear die body 21 and the die pad 22 are Figure 1The two molds are detachably connected in the reverse direction of the middle X-axis (for example, detachably connected by fasteners such as cylindrical pins), so as to facilitate the independent manufacturing and molding of the rear mold body 21 and the mold cushion 22 of the front mold 1 and the rear mold 2. The welding chamber 23 is arranged at the connection between the front mold 1 and the rear mold body 21, and the welding chamber 23 can be arranged on the side of the front mold 1 facing the rear mold body 21, or on the side of the rear mold body 21 facing the front mold 1, or the welding chamber 23 can be arranged on both the front mold 1 and the rear mold body 21 (that is, the welding chamber 23 is surrounded when the front mold 1 and the rear mold body 21 are connected). The front mold 1 is provided with a mounting hole 11 and a diverter hole 12 which penetrate the front mold 1, and the mounting hole 11 and the diverter hole 12 are both connected to the welding chamber 23, wherein the mounting hole 11 is used to assemble the mold core 3, and the diverter hole 12 is used to accommodate the plastically flowing billet (i.e., the material used to produce the extruded product) and guide the billet to the welding chamber 23; specifically, the front mold 1 is provided with a diverter hole 12, and the diverter hole 12 is connected to the welding chamber 23, so that the billet extruded on the side of the front mold 1 away from the rear mold 2 can flow plastically through the diverter hole 12 and gather in the welding chamber 23. The working belt 24 and the empty knife 25 are both cylindrical hole structures, which are used to connect the welding chamber 23 and the outside world (the outside of the micro-groove heat pipe extrusion mold); specifically, the working belt 24 is arranged on the rear mold body 21 and is connected to the welding chamber 23, and the empty knife 25 is arranged at the connection between the rear mold body 21 and the die pad 22. The empty knife 25 can be arranged only on the die pad 22, or the empty knife 25 can be arranged on both the rear mold body 21 and the die pad 22 (that is, the two ends of the empty knife 25 extend to the rear mold body 21 and the die pad 22 respectively); and the front end of the empty knife 25 (that is, the empty knife 25 is located at Figure 7 The end of the idle knife 25 in the positive direction of the X axis) is connected to the end of the working belt 24 away from the welding chamber 23, and the rear end of the idle knife 25 (that is, the idle knife 25 is located at Figure 4 The end in the opposite direction of the X-axis) passes through the die pad 22 and is connected to the outside world (the outside of the micro-groove heat pipe extrusion die).
[0029] The rear end of the mold core 3 (i.e., the end of the mold core 3 facing the rear mold 2, which is also the end of the mold core 3 located at Figure 1The end in the opposite direction of the X-axis in the middle) extends into the working belt 24, and the inner wall of the working belt 24 and the side wall of the rear end of the mold core 3 form a channel of a certain shape (i.e., the shape of the cross section of the extruded product) for the molding and shaping of the extruded product; in this way, after the blank flows into the welding chamber 23 through the diversion hole 12, the blank is continuously gathered in the welding chamber 23, and the static pressure it is subjected to is continuously increased, so that the blank is extruded and formed from between the rear end of the mold core 3 and the working belt 24 through the welding chamber 23, and is separated from the micro-groove heat pipe extrusion mold through the empty knife 25, and finally an extruded product is obtained. Moreover, the mold core 3 is suitable for being inserted into the mounting hole 11 provided on the front mold 1, and the mold core 3 and the mounting hole 11 are suitable for plug-in fit (or clearance fit) to realize the assembly of the mold core 3 on the front mold 1, thereby ensuring the stability of the mold core 3 when the micro-grooved heat pipe extrusion mold is working, so as to obtain an extruded product that meets composite requirements; moreover, the mold core 3 and the mounting hole 11 are detachably connected, that is, the mold core 3 and the front mold 1 are detachably connected, so that the mold core 3 is easy to replace.
[0030] By providing the mold core 3 and the mounting hole 11, a detachable connection between the mold core 3 and the front mold 1 is achieved, so that the mold core 3 is easy to replace. On the one hand, the mold core 3 and the front mold 1 are suitable for separate manufacturing and molding, which reduces the manufacturing difficulty and cost of the mold core 3 and the front mold 1 and facilitates the later maintenance and replacement of the mold core 3; on the other hand, the front mold 1 is suitable for assembling mold cores 3 of different specifications through the mounting hole 11 to produce extruded products of different specifications, thereby improving the application range of the micro-grooved heat pipe extrusion mold and reducing the use cost of the micro-grooved heat pipe extrusion mold. By setting a detachably connected rear mold body 21 and a mold pad 22, corresponding hole-groove structures can be processed on the rear mold body 21 and the mold pad 22 respectively. In this way, compared with the integrated rear mold 2, the separate rear mold 2 (detachably connected rear mold body 21 and mold pad 22) greatly reduces the processing difficulty and processing cost of the rear mold 2, shortens the manufacturing cycle of the rear mold 2, and makes the hole-groove structures on the rear mold body 21 and the mold pad 22 after thickness reduction easy to process, and its processing technology can choose relatively economical and efficient milling, fast wire cutting and other processes, further reducing the manufacturing cost of the rear mold 2, thereby greatly reducing the processing difficulty and processing cost of the micro-groove heat pipe extrusion mold, shortening the manufacturing cycle of the micro-groove heat pipe extrusion mold.
[0031] In order to further understand the advantages of the micro-grooved heat pipe extrusion die provided by the present invention, the following is an example of the micro-grooved heat pipe extrusion die being used to produce the shell of a micro-heat pipe; as a highly efficient heat transfer element, the micro-heat pipe is mainly composed of a shell, a liquid wick, and a working medium; compared with the traditional copper metal with excellent heat transfer performance, the micro-heat pipe is widely used in thermal control fields such as aerospace and solar energy due to its high heat transfer coefficient, low thermal resistance, and fast thermal response speed. For example, the micro-heat pipe of the aluminum alloy micro-grooved heat pipe is a key component to solve the heat dissipation problem of high heat flux density components on satellites and other spacecraft in the space environment. The groove microstructure of the liquid wick on the shell is at a sub-millimeter scale (typical size is 0.3mm), which poses a severe challenge to the processing and manufacturing of the shell. So far, extrusion technology, especially split-flow hot extrusion, is one of the main forming processes for manufacturing the shell and other hollow profiles of micro heat pipes. It has the advantages of high production efficiency, low cost, excellent product performance, and near-net forming. However, the existing micro-grooved heat pipe extrusion dies used to produce micro heat pipes have problems such as easy damage to the core structure and complex and difficult processing of the mold, which seriously restricts the application of extrusion in the field of heat pipe manufacturing. These problems are specifically reflected in the following two aspects: First, the core structure of the micro heat pipe has a small diameter and is easily damaged due to poor strength and stiffness; the existing integrated core structure not only has high processing costs, but also has problems such as easy damage to the core structure after damage. Will cause the entire mold to be scrapped; second, the typical external dimensions of a micro heat pipe are usually below 4 mm, which makes the depth-to-width ratio of the mold hole structure (i.e., the mounting hole 11, the diverter hole 12, the working belt 24, the empty knife 25 and other structures) of the micro groove heat pipe extrusion mold very large, that is, the cross-sectional size of the mold hole structure is small and the depth is large, which poses a severe challenge to mold processing. The traditional milling process is difficult to meet the manufacturing requirements of the micro groove heat pipe extrusion mold used to produce micro heat pipes, and the currently widely used electric spark machining method will greatly increase the production cost, resulting in the problems of difficult processing, high manufacturing cost and long manufacturing cycle of the rear mold 2.In view of the above problem one, the present invention provides a detachably connected mold core 3 and front mold 1 to achieve a detachable connection between the mold core 3 and the front mold 1, thereby making the mold core 3 easy to replace, reducing the manufacturing difficulty and cost of the mold core 3 and the front mold 1, greatly facilitating the later maintenance and replacement of the mold core 3, thereby greatly reducing the production cost of the tube shell of the micro heat pipe; In view of the above problem two, the present invention provides a separated design rear mold 2, that is, by providing a detachably connected rear mold body 21 and a mold pad 22, so that the corresponding The hole-groove structure (die hole structure) of the rear die 2 is provided, so as to reduce the processing difficulty and processing cost of the rear die 2, shorten the manufacturing cycle of the rear die 2, and make the hole-groove structure (die hole structure) on the rear die body 21 and the die pad 22 after the thickness is reduced easy to process and its processing technology can choose relatively economical and efficient milling, fast wire cutting and other processes, further reducing the processing difficulty and manufacturing cost of the rear die 2, further shortening the manufacturing cycle of the rear die 2, thereby reducing the manufacturing cost and difficulty of the micro-groove heat pipe extrusion die for producing the tube shell of the micro heat pipe. In this way, when the micro-groove heat pipe extrusion die of the present invention is used to produce micro heat pipes (such as micro-groove heat pipes), it can break through the technical bottleneck of batch precision manufacturing of the tube shell of the micro heat pipe in the prior art (i.e., the above-mentioned problem one and problem two), and improve the performance of the tube shell of the micro heat pipe.
[0032] Optionally, combined Figure 1-Figure 5 As shown, the mold core 3 includes a positioning portion 31, a connecting portion 32 and a shaping portion 33, and the positioning portion 31, the connecting portion 32 and the shaping portion 33 are connected in sequence in the direction from the front mold 1 to the rear mold body 21; the mounting hole 11 includes a first accommodating hole 111 suitable for accommodating the positioning portion 31 and a second accommodating hole 112 suitable for accommodating the connecting portion 32, and the hole wall of the first accommodating hole 111 is suitable for limiting the rotation of the positioning portion 31 around the axis of the positioning portion 31; the connection between the connecting portion 32 and the shaping portion 33 is located in the welding chamber 23, and the shaping portion 33 extends to the working belt 24 at one end away from the connecting portion 32.
[0033] In the direction from the front mold 1 to the rear mold body 21 (i.e. Figure 1The positioning portion 31, the connecting portion 32 and the shaping portion 33 of the mold core 3 are connected in sequence, and the positioning portion 31, the connecting portion 32 and the shaping portion 33 are preferably formed in one piece to improve the structural strength of the mold core 3, thereby improving the stability and reliability of the micro-groove heat pipe extrusion mold during operation. The mounting hole 11 includes a first receiving hole 111 and a first receiving hole 112 that are connected. The end of the first receiving hole 111 away from the first receiving hole 112 is connected to the outside world, which is convenient for the mold core 3 to be inserted into the mounting hole 11 from the first receiving hole 111 when installing and replacing the mold core 3. The end of the first receiving hole 112 away from the first receiving hole 111 is connected to the welding chamber 23, so that the shaping portion 33 can be inserted into the working belt 24 through the welding chamber 23. The first accommodating hole 111 and the first accommodating hole 112 are respectively adapted to the positioning portion 31 and the connecting portion 32 to ensure the stability of the mold core 3 when connected to the front mold 1; moreover, the hole wall of the first accommodating hole 111 is suitable for constraining the freedom of rotation of the mold core 3 around its axis, that is, the hole wall of the first accommodating hole 111 is suitable for limiting the rotation of the positioning portion 31 around the axis of the positioning portion 31 to prevent the mold core 3 from rotating around its own axis and affecting the molding of the extruded product, and further improves the stability of the mold core 3 when connected to the front mold 1.
[0034] Furthermore, the cross-section of the positioning portion 31 (i.e., the surface exposed when the positioning portion 31 is cut by a plane perpendicular to the axis of the mold core 3) is a non-circular shape such as a polygon, an ellipse, or a waist shape, and the first accommodating hole 111 is adapted to the shape of the positioning portion 31, so as to achieve the limiting effect of the hole wall of the first accommodating hole 111 on the rotation of the positioning portion 31 around the axis of the positioning portion 31.
[0035] Optionally, combined Figure 1-Figure 7 As shown, the shaping portion 33 is coaxially arranged with the working belt 24 , and an annular gap is provided between the side wall of one end of the shaping portion 33 extending into the working belt 24 and the inner wall of the working belt 24 .
[0036] There is an annular gap between the side wall of the shaping portion 33 extending into the working belt 24 (i.e., the end of the shaping portion 33 away from the connecting portion 32, which is also the rear end of the shaping portion 33) and the inner wall of the working belt 24, so that the inner wall of the working belt 24 and the rear end of the shaping portion 33 (i.e., the shaping portion 33 is located at the rear end of the shaping portion 33) are not connected. Figure 1 The side wall of the molding part 33 (the end opposite to the X-axis) is surrounded by a ring-shaped channel to produce extruded products such as micro-grooved heat pipes. The axis of the molding part 33 and the axis of the working belt 24 are located on the same straight line to ensure that the rear end of the molding part 33 is stably located in the middle position of the working belt 24 to ensure that the wall thickness of the extruded products such as tubes produced by the micro-grooved heat pipe extrusion die is uniform.
[0037] Furthermore, the shaping portion 33 may be a cylindrical structure such as a cylindrical shape, an elliptical cylindrical shape, a column shape, etc., and the working belt 24 may also be a cylindrical structure, and the cylindrical structures of the shaping portion 33 and the working belt 24 may be the same or different. In one embodiment of the present invention, the cross section of the working belt 24 is a rounded rectangular shape (i.e., the corners of the rectangle are rounded), which, on the one hand, facilitates the demolding of the extruded product; on the other hand, facilitates the processing and forming of the working belt 24 on the rear mold body 21 (for example, by milling, fast wire cutting, etc.).
[0038] Furthermore, the gap between the side wall at the rear end of the shaping portion 33 and the inner wall of the working belt 24 can also be other shapes, so that the micro-groove heat pipe extrusion die is suitable for producing extruded products such as profiles.
[0039] Optionally, combined Figure 1-Figure 7 As shown, the positioning portion 31 , the connecting portion 32 and the shaping portion 33 are all coaxially arranged, and the cross-sectional area of the connecting portion 32 is larger than the cross-sectional area of the shaping portion 33 and smaller than the cross-sectional area of the positioning portion 31 .
[0040] The axes of the positioning portion 31 , the connecting portion 32 and the shaping portion 33 are located on the same straight line, so as to facilitate the manufacturing and molding of the mold core 3 and to facilitate the installation of the mold core 3 into the installation hole 11 . The cross-sectional area of the connecting portion 32 (i.e., the area of the surface exposed when the connecting portion 32 is cut by a plane perpendicular to the axis of the core 3) is smaller than the cross-sectional area of the positioning portion 31 (i.e., the area of the surface exposed when the positioning portion 31 is cut by a plane perpendicular to the axis of the core 3), so that the positioning portion 31 limits the connecting portion 32 and the shaping portion 33, so as to limit the movement of the core 3 toward the die pad 22 after the core 3 is assembled into the mounting hole 11; since the shaping portion 33 needs to be adapted to the working belt 24 to produce extruded products with composite requirements, when the cross-sectional area of the extruded product is small, the cross-sectional area of the shaping portion 33 usually also needs to be set smaller, and the connecting portion 32 with a cross-sectional area larger than the cross-sectional area of the shaping portion 33 (i.e., the cross-sectional area of the connecting portion 32 is larger than the cross-sectional area of the shaping portion 33) is set to improve the overall structural strength of the core 3, so as to avoid the shaping portion 33 having a low structural strength and being easy to damage.
[0041] Further, in the direction from the connecting portion 32 to the shaping portion 33 (i.e. Figure 1 The connection part 32 and the shaping part 33 have a smooth transition at the connection part, that is, the connection part 32 and the shaping part 33 are in a truncated cone or prism structure, so as to improve the structural strength of the connection part 32 and the shaping part 33 at the connection part, thereby improving the structural strength of the shaping part 33 and improving the stability and reliability of the mold core 3 when the micro-groove heat pipe extrusion mold is in operation.
[0042] Optionally, a prismatic structure and / or a groove structure is provided on the side wall of one end of the shaping portion 33 extending into the working belt 24 , and the extending direction of the prismatic structure and / or the groove structure is parallel to the axis of the shaping portion 33 .
[0043] In this embodiment, when the micro-grooved heat pipe extrusion die is used to produce a tube material such as a micro-grooved heat pipe whose inner surface has a liquid-absorbing core with a groove microstructure, a groove structure is provided on the side wall of one end of the shaping portion 33 extending into the working belt 24 (i.e., the side surface of the rear end of the shaping portion 33 facing the inner wall of the working belt 24), and / or a prismatic structure is convexly provided; and the groove structure (prismatic structure) extends along the axial direction of the shaping portion 33 so that the groove structure (prismatic structure) cooperates with the inner wall of the working belt 24, thereby enabling the micro-grooved heat pipe extrusion die to produce a tube material (such as a micro-grooved heat pipe) with a liquid-absorbing core with a groove microstructure.
[0044] The groove structure (rib-shaped structure) can be arranged on the inner wall of the working belt 24, or on the side wall of one end of the shaping portion 33 extending into the working belt 24, both of which can make the micro-grooved heat pipe extrusion die suitable for producing micro-grooved heat pipes and other pipes. In this embodiment, it is preferred that the groove structure (rib-shaped structure) is arranged on the side wall of one end of the shaping portion 33 extending into the working belt 24, so as to reduce the difficulty of molding the working belt on the rear mold body 21 and the difficulty of manufacturing the rear mold body 21.
[0045] Furthermore, based on the fact that the groove structure (prismatic structure) extends along the axial direction of the shaping portion 33, it is preferred that a plurality of groove structures (prismatic structures) are spaced apart on the side wall of one end of the shaping portion 33 extending into the working belt 24, that is, a plurality of groove structures (prismatic structures) are spaced apart around the side wall at the rear end of the shaping portion 33 to ensure uniform distribution of the groove microstructure formed on the inner wall of the produced pipe.
[0046] Optionally, combined Figure 1 , Figure 2 , Figure 4 , Figure 5 and Figure 7 As shown, the empty knife 25 includes a first empty knife 251 and a second empty knife 252 which are connected. The end of the first empty knife 251 away from the second empty knife 252 is connected to the working belt 24, and the end of the second empty knife 252 away from the first empty knife 251 passes through the mold pad 22 and is connected to the outside; and the cross-sectional area of the first empty knife 251 is larger than the cross-sectional area of the working belt 24, and smaller than the cross-sectional area of the second empty knife 252.
[0047] In this embodiment, when the empty knife 25 is only arranged on the die pad 22, the empty knife 25 penetrates the die pad 22, and the rear end of the working belt 24 (that is, the working belt 24 is located at Figure 1The end in the opposite direction of the middle X-axis) passes through the side of the rear mold body 21 away from the front mold 1 and is connected to the front end of the empty knife 25; when the empty knife 25 is set on the rear mold body 21 and the mold pad 22 at the same time, the front end of the empty knife 25 extends to the rear mold body 21 and is connected to the rear end of the working belt 24.
[0048] The empty knife 25 includes a first empty knife 251 and a second empty knife 252 connected to each other. The second empty knife 252 is arranged on the die pad 22. The front end of the first empty knife 251 (that is, the first empty knife 251 is located at Figure 7 The end in the positive direction of the middle X-axis) passes through the rear mold body 21 and is connected to the end of the working belt 24 away from the welding chamber 23. The rear end of the first empty knife 251 (that is, the first empty knife 251 is located at Figure 7 The end in the opposite direction of the middle Z axis) is connected to the end of the second empty knife 252 facing the front mold 1; moreover, the cross-sectional area of the first empty knife 251 (that is, the area of the surface exposed when the first empty knife 251 is cut by a plane perpendicular to the axis of the first empty knife 251) is larger than the cross-sectional area of the working belt 24 (that is, the area of the surface exposed when the working belt 24 is cut by a plane perpendicular to the axis of the working belt 24), so that the extruded product extruded between the working belt 24 and the rear end of the mold core 3 does not need to contact the inner wall of the first empty knife 251 when it is demolded, so as to avoid the inner wall of the first empty knife 251 from hindering the demolding of the extruded product to a large extent, reduce the friction force on the extruded product when it is demolded, and ensure the smooth demolding of the extruded product. The cross-sectional area of the first empty knife 251 is smaller than the cross-sectional area of the second empty knife 252 (i.e., the area of the surface exposed when the second empty knife 252 is cut by a plane perpendicular to the axis of the second empty knife 252), so as to further ensure the smooth demolding of the extruded product, and when there are multiple mold cores 3, the working belt 24 and the first empty knife 251 are also provided with multiple, at this time, only one second empty knife 252 with a larger cross-sectional area can be provided, and one second empty knife 252 is connected with multiple first empty knives 251, so that multiple extruded products can be demolded from one second empty knife 252. It is worth noting that there can also be multiple second empty knives 252.
[0049] Optionally, combined Figure 1 , Figure 4 , Figure 5 and Figure 7 As shown, the welding chamber 23 is arranged on the side of the rear mold body 21 facing the front mold 1. The welding chamber 23 is arranged on the side of the rear mold body 21 facing the front mold 1.
[0050] In this embodiment, the welding chamber 23 is preferably arranged on the rear mold body 21. Specifically, the welding chamber 23 is arranged on the side of the rear mold body 21 facing the front mold 1. On the one hand, since the rear mold body 21 and the mold pad 22 of the rear mold 2 are easy to manufacture and form, the welding chamber 23 is arranged on the rear mold body 21, which reduces the difficulty of forming the welding chamber 23. On the other hand, the front mold 1 can maintain a larger thickness to ensure that the front mold 1 has a larger contact area with the mold core 3, thereby ensuring the stability of the front mold 1 and the mold core 3 when they are connected.
[0051] Optionally, combined Figure 1 , Figure 3 As shown, the front mold 1 is provided with a plurality of diverter holes 12 penetrating the front mold 1 . The plurality of diverter holes 12 are all connected to the welding chamber 23 and are arranged at intervals around the mounting hole 11 .
[0052] In this embodiment, a plurality of diverter holes 12 are provided on the front mold 1, and the plurality of diverter holes 12 are spaced apart around the mounting hole 11, that is, the plurality of diverter holes 12 are spaced apart around the mold core 3 to ensure that the billet extruded on the side of the front mold 1 away from the rear mold body 21 can flow plastically uniformly through the plurality of diverter holes 12 to the edge of the welding chamber 23, and gather toward the middle of the welding chamber 23, so as to facilitate the billet in the welding chamber 23 to be extruded along the side wall of the shaping portion 33 also located in the middle of the welding chamber 23 to the working belt 24 for forming, and demolded from the empty knife 25 to complete the production of the extruded product.
[0053] Optionally, combined Figure 1 , Figure 2 , Figure 4 and Figure 7 As shown, the front mold 1 and the rear mold body 21 are respectively provided with a positioning groove 26 and one of the positioning platforms 13 , and the positioning platform 13 is plugged and matched with the positioning groove 26 .
[0054] In this embodiment, a positioning platform 13 may be provided on the side of the front mold 1 facing the rear mold body 21, and a positioning groove 26 may be provided on the side of the rear mold body 21 facing the front mold 1; or a positioning groove 26 may be provided on the side of the front mold 1 facing the rear mold body 21, and a positioning platform 13 may be provided on the side of the rear mold body 21 facing the front mold 1; the positioning platform 13 is plugged into and matched with the positioning groove 26, so that the front mold 1 and the rear mold body 21 are limited to each other in a direction perpendicular to the axis of the front mold 1 (rear mold body 21), thereby further improving the stability of the connection between the front mold 1 and the rear mold body 21.
[0055] Furthermore, the positioning platform 13 is a boss-shaped structure, and the shape of the positioning groove 26 is adapted to the shape of the positioning platform 13 .
[0056] Optionally, combined Figure 1-Figure 3 , Figure 6 and Figure 7As shown, the micro-grooved heat pipe extrusion die also includes a positioning member 4, which is suitable for being assembled in a die base of an extruder. The positioning member 4 is arranged on the outer side wall of the rear die body 21, and / or, on the outer side wall of the die pad 22, and is used to limit the micro-grooved heat pipe extrusion die from rotating around the axis of the micro-grooved heat pipe extrusion die in the die base.
[0057] The micro-grooved heat pipe extrusion die is assembled on the die base of the extruder to ensure the stability of the micro-grooved heat pipe extrusion die during operation; the extruder is used to extrude the blank on the side of the front die 1 away from the rear die body 21, so as to extrude the blank from the diverter hole 12 into the micro-grooved heat pipe extrusion die. The positioning member 4 is preferably arranged on the outer side wall of the rear die body 21, and / or, arranged on the outer side wall of the die pad 22, so as to avoid affecting the installation and replacement of the core 3 when the positioning member 4 is arranged on the outer side wall of the front die 1. The positioning member 4 can be a structure convexly arranged on the outer side wall of the rear die body 21 (die pad 22), or the positioning member 4 can be detachably connected to the rear die body 21 (die pad 22). In this embodiment, the positioning member 4 is preferably detachably connected to the rear mold body 21 (mold pad 22) to reduce the difficulty and cost of manufacturing the rear mold body 21 (mold pad 22). Specifically, the positioning member 4 includes fasteners such as pins and bolts, which are connected to the outer side wall of the rear mold body 21 (mold pad 22). One end of the positioning member 4 is detachably connected to the rear mold body 21 (mold pad 22) to ensure the stability of the positioning member 4 when connected to the rear mold body 21 (mold pad 22) and the convenience of disassembly. The other end of the positioning member 4 faces away from the rear mold body 21 (mold pad 22). The mold body 21 (mold pad 22) extends in the direction of the mold body 21 (mold pad 22), and the axis of the positioning member 4 is perpendicular to the axis of the rear mold body 21 (mold pad 22) to ensure that the positioning member 4 can stably cooperate with the corresponding structure on the mold base of the extruder to limit the rear mold body 21 (mold pad 22) from rotating around the axis of the rear mold body 21 (mold pad 22) in the mold base of the extruder, thereby limiting the rotation of the micro-grooved heat pipe extrusion mold around the axis of the micro-grooved heat pipe extrusion mold in the mold base to ensure the stability of the micro-grooved heat pipe extrusion mold during operation.
[0058] Although the disclosure is disclosed as above, the protection scope of the disclosure is not limited thereto. Those skilled in the art may make various changes and modifications without departing from the spirit and scope of the disclosure, and these changes and modifications will fall within the protection scope of the present invention.
Claims
1. A miniature groove heat pipe extrusion die, characterized in that: The invention comprises a mold core (3), and a front mold (1), a rear mold body (21), and a mold pad (22) which are detachably connected in sequence; a welding chamber (23) is provided at the connection between the rear mold body (21) and the front mold (1); a working belt (24) which is in communication with the welding chamber (23) is provided on the rear mold body (21); a hollow knife (25) is provided at the connection between the rear mold body (21) and the mold pad (22); an end of the working belt (24) which is away from the welding chamber (23) is in contact with the hollow knife The front mold (1) is provided with a mounting hole (11) which penetrates the front mold (1), and the mounting hole (11) is connected to the welding chamber (23); the mold core (3) is suitable for being inserted into the mounting hole (11) and being detachably connected to the mounting hole (11), and one end of the mold core (3) facing the mold pad (22) extends through the welding chamber (23) into the working belt (24); The mold core (3) comprises a positioning portion (31), a connecting portion (32) and a shaping portion (33), wherein the positioning portion (31), the connecting portion (32) and the shaping portion (33) are sequentially connected in a direction from the front mold (1) to the rear mold body (21); the mounting hole (11) comprises a first accommodating hole (111) suitable for accommodating the positioning portion (31) and a second accommodating hole (112) suitable for accommodating the connecting portion (32), and a hole wall of the first accommodating hole (111) is suitable for limiting the rotation of the positioning portion (31) around the axis of the positioning portion (31); a connection point between the connecting portion (32) and the shaping portion (33) is located in the welding chamber (23), and an end of the shaping portion (33) away from the connecting portion (32) extends into the working belt (24); The welding chamber (23) is arranged on a side of the rear mold body (21) facing the front mold (1); The front mold (1) and the rear mold body (21) are respectively provided with a positioning groove (26) and one of the positioning platforms (13), and the positioning platform (13) is plug-fitted into the positioning groove (26).
2. The micro-grooved heat pipe extrusion die according to claim 1, characterized in that: The shaping portion (33) is coaxially arranged with the working belt (24), and an annular gap is provided between a side wall of one end of the shaping portion (33) extending into the working belt (24) and an inner wall of the working belt (24).
3. The micro-grooved heat pipe extrusion die according to claim 2, characterized in that: The positioning portion (31), the connecting portion (32) and the shaping portion (33) are all coaxially arranged, and the cross-sectional area of the connecting portion (32) is larger than the cross-sectional area of the shaping portion (33) and smaller than the cross-sectional area of the positioning portion (31).
4. The micro-grooved heat pipe extrusion die according to any one of claims 1 to 3, characterized in that: A prism-shaped structure and / or a groove structure is provided on a side wall of one end of the shaped portion (33) extending into the working belt (24), and the extending direction of the prism-shaped structure and / or the groove structure is parallel to the axis of the shaped portion (33).
5. The micro-grooved heat pipe extrusion die according to any one of claims 1 to 3, characterized in that: The empty knife (25) comprises a first empty knife (251) and a second empty knife (252) which are connected to each other; an end of the first empty knife (251) away from the second empty knife (252) is connected to the working belt (24); an end of the second empty knife (252) away from the first empty knife (251) passes through the die pad (22) and is connected to the outside; and a cross-sectional area of the first empty knife (251) is larger than a cross-sectional area of the working belt (24) and smaller than a cross-sectional area of the second empty knife (252).
6. The micro-grooved heat pipe extrusion die according to any one of claims 1 to 3, characterized in that: The front mold (1) is provided with a plurality of flow diversion holes (12) penetrating the front mold (1); the plurality of flow diversion holes (12) are all connected to the welding chamber (23) and are arranged at intervals around the mounting hole (11).
7. The micro-grooved heat pipe extrusion die according to any one of claims 1 to 3, characterized in that: The micro-miniature groove heat pipe extrusion die also includes a positioning member (4), the micro-miniature groove heat pipe extrusion die is suitable for being assembled in a die base of an extruder, the positioning member (4) is arranged on the outer side wall of the rear die body (21), and / or, is arranged on the outer side wall of the die pad (22), and is used to limit the micro-miniature groove heat pipe extrusion die from rotating around the axis of the micro-miniature groove heat pipe extrusion die in the die base.