Construction method of anti-cracking bridge deck expansion joint device
By installing support components and expansion joint devices from the bottom up, combined with prestressed dispersion layers and flexible fillers, the problems of steel deformation and inaccurate installation in traditional bridge deck expansion joint construction are solved, achieving one-time pouring and efficient construction, improving It improves structural safety and construction efficiency, and reduces costs and environmental pollution.
Patent Information
- Application Number
- CN202010897496.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-08-31
- Publication Date
- 2024-10-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The traditional bridge deck expansion joint construction method has problems such as deformation of steel bars, excessive cutting debris, inaccurate installation, and the need for secondary pouring and repair, resulting in slow construction progress, high cost, large material loss, and difficulty in adapting to the expansion and contraction deformation of the bridge structure. .
Support components and expansion joint devices are installed sequentially from bottom to top, including retractable mounting seats, prestressed connectors and flexible fillers. This avoids cutting concrete and reserving steel bars at a later stage, achieving one-time pouring and forming, combining prestressed dispersion layers and Anti-slip protrusions ensure construction accuracy and safety.
It achieves time-saving and efficient construction, avoids steel bar deformation and concrete crushing damage, improves structural safety and waterproofing, reduces construction costs and environmental pollution, simplifies the process, extends equipment life, and improves construction safety .
Smart Images

Figure CN111979909B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an expansion joint, in particular to a construction method of an anti-cracking bridge deck expansion joint device, which is mainly used for the construction of bridge deck expansion joints and belongs to the technical field of bridge building construction. Background Art
[0002] As we all know, an expansion joint refers to a structural joint set at an appropriate position along the construction joint direction of a building or structure to release the internal force generated by climate temperature changes (thermal expansion and contraction) and concrete shrinkage when the plane size of the building is large, in order to prevent the building components from cracking or being damaged.
[0003] Taking the bridge deck of 10cm reinforced concrete + 10cm asphalt as an example, the general construction sequence of the expansion joint of the traditional bridge deck is: pre-embedded steel bars → pouring concrete → cutting the concrete of the expansion joint slot → installing the expansion joint device → paving asphalt. In the actual construction process, the reserved steel bars are deformed in large quantities, and there are many cutting debris, so the expansion joint device cannot be accurately installed. The concrete is cut later, which is time-consuming and laborious. In addition, due to the deformation of the reserved steel bars, the steel bars arranged throughout the length in the later stage cannot be accurately inserted and fixed. The only way is to weld or cut the reserved steel bars. At the same time, the garbage in the expansion joint slot cannot be cleaned up, and it can only be buried in it for the next step of construction.
[0004] At the same time, due to the high requirements for the pouring and installation accuracy of the expansion joint, if the pouring accuracy is not enough, it will need to be roughened or repaired during the later installation. The time interval is long, and some garbage and damage will inevitably enter, which needs to be cleaned and repaired. After the main body is capped, it is difficult to transport concrete, which increases material loss, labor, and construction period, thereby greatly increasing costs. The traditional construction method is slow and requires secondary pouring for coordination, which increases transportation costs.
[0005] Therefore, the key to solving the above technical problems is to develop a time-saving and efficient improved bridge deck expansion joint. Summary of the invention
[0006] In view of the many defects and shortcomings existing in the above-mentioned background technology, the present invention has made improvements and innovations thereto, with the aim of providing a method that can change the traditional construction sequence, achieve the goal of not needing to cut concrete later, and can be cast in one time, and does not need to reserve steel bars, thereby avoiding the problem of steel bar deformation in the later stage.
[0007] Another object of the present invention is to achieve a simple structure and convenient and quick construction, which can effectively avoid damage to various expansion joint devices caused by concrete crushing, greatly improve structural safety and reduce operating costs.
[0008] Another object of the present invention is not only to adapt to the telescopic deformation and small rotational deformation of various types of bridge superstructures; to make the bridge deck pavement form a continuum with better waterproof properties; to not only generate impact and vibration when vehicles pass by, but also to provide better comfort; and to facilitate and speed construction with low cost; to achieve the goal of unifying safety, economy and durability.
[0009] Another purpose of the present invention is to solve the technical problems that the traditional method of roughening or repairing during the later installation has a long time interval, and some garbage and damage will inevitably enter, which requires cleaning and repairing. It reduces the subsequent construction procedures, reduces material loss, labor, and construction period, thereby greatly reducing construction costs while also achieving environmental protection.
[0010] In order to solve the above problems and achieve the above invention objectives, a construction method of an anti-crack bridge deck expansion joint device of the present invention is achieved by adopting the following design structure and the following technical solutions:
[0011] As an improvement of the construction method of an anti-crack bridge deck expansion joint device of the present invention, it comprises a support assembly (1) installed in sequence from bottom to top and an expansion joint device (2) installed above the support assembly (1), the expansion joint device (2) comprising a telescopic mounting seat (21) and expansion joint baffles (22) symmetrically connected to both sides of the top of the telescopic mounting seat (21), an expansion joint (23) is formed between the two expansion joint baffles (22), and a plurality of prestressed connectors (24) are also provided on the two expansion joint baffles (22), and the prestressed connectors (24) are symmetrically coaxially connected to the outer walls of the two expansion joint baffles (22).
[0012] As an improvement of the above-mentioned present invention, the support assembly (1) comprises a base plate (11), a supporting weight component (12) and a cover plate (13), wherein the base plate (11), the supporting weight component (12) and the cover plate (13) are arranged and installed in sequence from bottom to top; an installation groove (14) is formed between the upper part of one end of the base plate (11) and the cover plate (13), and the shrinkage device (2) is engaged in the installation groove (14), and the installation groove (14) is filled with filler, and the top end is filled with flexible filler.
[0013] As a further improvement of the above-mentioned present invention, the base plate (11) is an L-shaped plate-like member as a whole, and a plurality of prestressed reinforcement members (15) are coaxially arranged on the vertical outer wall of the plate-like member; the cover plate (13) is a right-angled Z-shaped plate-like member as a whole, and a plurality of prestressed support members (16) are arranged on the outer wall of one side of the plate-like member, and the prestressed support members (16) and the prestressed reinforcement members (15) are symmetrically arranged with each other.
[0014] As a further improvement of the above-mentioned present invention, a lower baffle (17) is installed at the lower part of one end of the base plate (11) and the cover plate (13), one end of the lower baffle (17) is detachably connected to the base plate (11), and the other end is detachably connected to the cover plate (13); an upper baffle (18) is installed at the upper part of the other end of the base plate (11) and the cover plate (13), one end of the upper baffle (18) is detachably connected to the base plate (11), and the other end is detachably connected to the cover plate (13).
[0015] As a further improvement of the above-mentioned present invention, the cover plate (13) is further provided with a plurality of granular anti-skid protrusions (19), and the anti-skid protrusions (19) are arranged on the upper casting end surface of the cover plate (13); the lower baffle plate (17) and the upper baffle plate (18) are both arc-shaped baffle plates, and are located at the connection between the bottom plate (11) and the cover plate (13).
[0016] As a further improvement of the above-mentioned present invention, the supporting counterweight component (12) is an inverted U-shaped ridge-shaped, pier-shaped, or square-shaped component, and is located between the base plate (11) and the cover plate (13); the total number of the supporting counterweight components (12) is set to be multiple, and the multiple supporting counterweight components (12) are arranged in rows, and one end of the supporting counterweight component (12) is fixedly connected to the base plate (11), and the other end is overlapped with the cover plate (13).
[0017] As a further improvement of the above-mentioned present invention, the telescopic mounting seat (21) is an elastic inverted convex-shaped or inverted "X"-shaped component; the expansion joint baffle (22) is a plate-shaped component; a plurality of buffer members (25) are arranged at intervals in the expansion joint (23), and the buffer member (25) is a shock-absorbing spring, one end of the shock-absorbing spring is connected to one of the expansion joint baffles (22), and the other end is connected to the other expansion joint baffle (22); the expansion joint (23) is filled with a filler (231), and a flexible filler is filled inside the top end thereof; the prestressed connector (24) is connected to the prestressed dispersion layer (3).
[0018] As a further improvement of the above-mentioned present invention, the prestressed reinforcement member (15) and the prestressed support member (16) are both connected to a prestressed dispersion layer (3), and the prestressed dispersion layer (3) is an expanded mesh, a steel plate mesh, a steel wire mesh, a reinforced steel mesh, a galvanized steel wire mesh or a ribbed metal mesh or a crack-resistant and fire-proof steel mesh.
[0019] As a further improvement of the above-mentioned present invention, a construction method of an anti-crack bridge deck expansion joint device and a construction method thereof include the following construction steps:
[0020] Step 1, construction preparation, the construction personnel first measure and locate, accurately place the support assembly (1) at the expansion joint position of the bridge deck (4), and temporarily fix it;
[0021] Step 2, paving the bridge deck (4) with a prestressed dispersion layer (3), connecting the prestressed dispersion layer (3) with the prestressed reinforcement (15) and the prestressed support (16) on the side of the support assembly (1), and welding them firmly at the hook connection;
[0022] Step 3, temporarily sealing the upper opening of the support assembly (1) with an extruded board, pouring the bottom filling layer (5) of the bridge deck (4), the height of the bottom filling layer (5) of the bridge deck (4) is flush with the upper opening of the support assembly (1), and ensuring that the support assembly (1) does not move during the concrete pouring process;
[0023] Step 4, the bottom filling layer (5) of the bridge deck (4) is paved and maintained. If there is a gap between the support assembly (1) and the bottom filling layer (5) on both sides, hot asphalt is used for sealing;
[0024] Step 5, clean the extruded board, install the expansion joint device (2), and accurately insert the protrusion of the expansion joint device (2) into the recess of the support component (1);
[0025] Step 6, before paving the asphalt mixture surface layer, spray the tack coat asphalt on the outer wall of the expansion joint device (2), and install the prestressed dispersion layer (3), the prestressed dispersion layer (3) is connected to the prestressed connector (24) in the expansion joint device (2), and is firmly welded at the hook connection, and the prestressed dispersion layer (3) and the prestressed connector (24) are integrally fixed on the formed concrete bridge deck pavement;
[0026] Step 7, after installing the expansion joint device (2), fill the gap in the side wall of the expansion joint device (2) with an extruded board;
[0027] Step 8, paving the top filling layer (6) of the bridge deck, the top filling layer (6) is paved to the expansion joint baffle (22) of the expansion joint device (2), and the top filling layer (6) near the expansion joint device (2) is rolled using a small vibrating roller, and a large roller is not allowed to be used, and during the rolling process, it is ensured that the expansion joint device (2) does not move;
[0028] Step 9, clean the extruded plate inside the side wall of the expansion joint device (2), and seal it with silicone or polysulfide material, with the sealing being slightly lower than the top of the expansion joint device (2).
[0029] As a further improvement of the present invention, in step 2, the prestressed reinforcement member (15) and the prestressed support member (16) are both bent steel bars with hooks;
[0030] In step 3, the bottom filling layer (5) is a mixture of one or more of high-strength concrete, foamed concrete, ceramsite concrete, polystyrene particle foamed concrete, extruded polystyrene board, polystyrene foam board, ordinary concrete, foamed concrete, lightweight concrete, EPS particle concrete or foamed polyurethane.
[0031] In the step 8, the top filling layer (6) is asphalt concrete.
[0032] Compared with the prior art, the present invention has the following beneficial effects:
[0033] 1. The present invention changes the traditional construction sequence, realizes that there is no need to cut concrete later, can be cast in one time, and does not need to reserve steel bars, thus avoiding the problem of steel bar deformation in the later stage;
[0034] 2. The present invention effectively avoids damage to various expansion joint devices caused by concrete crushing, greatly improves structural safety and reduces operating costs;
[0035] 3. The present invention can not only adapt to the telescopic deformation and small rotation deformation of various bridge superstructures, but also make the bridge deck pavement form a continuum with good waterproof performance. It does not produce impact and vibration when vehicles pass by, and has good comfort. It is also convenient and fast to construct with low cost, and achieves the purpose of unifying safety, economy and durability.
[0036] 4. The present invention solves the technical problems that the traditional method of roughening or repairing during the later installation, which has a long time interval and inevitably causes some garbage and damage, and requires cleaning and repair, reduces the subsequent construction procedures, reduces material loss, labor, and construction period, thereby greatly reducing the construction cost and achieving environmental protection;
[0037] 5. The exterior of the present invention is coated with an anti-rust layer and a waterproof layer, so it can prevent rust and extend the service life of the entire device, achieving environmental protection while saving resources. At the same time, the exterior of the device is coated with a self-luminous fluorescent material, which can clearly mark the position of the wire-laying device at night or in a dark room and underground construction environment, and can effectively serve as a safety reminder, improve the conspicuousness, and be easy for people to identify, thereby increasing the safety of construction and life;
[0038] 6. The present invention simplifies the construction process, avoids secondary construction work, shortens construction time, reduces environmental pollution, reduces transportation costs, speeds up construction progress, fills the middle of the expansion joint with asphalt hemp, and after installation, it is cast into shape with concrete at one time. Compared with sealing the expansion joint when making the floor leveling layer after the structural construction is completed, the construction quality is easy to control, saves a lot of materials and labor, reduces construction costs, and can greatly reduce construction waste. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] The specific embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings, wherein:
[0040] Figure 1 It is one of the overall structural schematic diagrams of the present invention;
[0041] Figure 2 This is the second schematic diagram of the overall structure of the present invention;
[0042] Figure 3 is a top view of the present invention;
[0043] Figure 4 yes Figure 3 A schematic diagram of the local enlarged structure of position A shown;
[0044] Figure 5 It is one of the schematic diagrams of the use state of the present invention;
[0045] Figure 6 This is the second schematic diagram of the use state of the present invention;
[0046] Figure 7 This is the third schematic diagram of the use state of the present invention;
[0047] Figure 8 yes Figure 7 A schematic diagram of the local enlarged structure of position B shown;
[0048] Fig. 9 This is the fourth schematic diagram of the use state of the present invention;
[0049] Fig.10 It is a schematic diagram of the use and installation of the present invention;
[0050] Fig.11 It is a schematic diagram of the use state of another design structure of the present invention;
[0051] Among them, the numbers in the figure are: 1-support assembly, 11-bottom plate, 12-support counterweight member, 13-cover plate, 14-installation groove, 15-prestressed reinforcement member, 16-prestressed support member, 17-lower baffle plate, 18-upper baffle plate, 19-anti-slip protrusion;
[0052] 2—expansion joint device, 21—retractable mounting seat, 22—expansion joint baffle, 23—expansion joint, 231—filler, 24—prestressed connector, 25—buffer;
[0053] 3—Prestressed dispersion layer;
[0054] 4—bridge abutment;
[0055] 5—bottom filling layer;
[0056] 6—Top filling layer. DETAILED DESCRIPTION
[0057] In order to make the technical means, creative features, objectives and effects of the present invention easy to understand, the technical solution of the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. It should be noted that the embodiments and features in the embodiments of the present application can be combined with each other without conflict. The present invention will be described in detail below with reference to the accompanying drawings and in conjunction with the embodiments.
[0058] A construction method for a crack-proof bridge deck expansion joint device as shown in the accompanying drawings of the specification comprises a support assembly 1 installed in sequence from bottom to top and an expansion joint device 2 installed above the support assembly 1, wherein the expansion joint device 2 comprises a telescopic mounting seat 21 and expansion joint baffles 22 symmetrically connected to both sides of the top of the telescopic mounting seat 21, an expansion joint 23 is formed between the two expansion joint baffles 22, and a plurality of prestressed connectors 24 are also provided on the two expansion joint baffles 22, and the prestressed connectors 24 are symmetrically and coaxially connected to the outer walls of the two expansion joint baffles 22.
[0059] Furthermore, the support assembly 1 includes a base plate 11, a supporting weight member 12, and a cover plate 13, wherein the base plate 11, the supporting weight member 12, and the cover plate 13 are arranged and installed in sequence from bottom to top; an installation groove 14 is formed between the base plate 11 and the upper part of one end of the cover plate 13, and the shrinkage device 2 is engaged in the installation groove 14, and the installation groove 14 is filled with filler, and the top end is filled with flexible filler.
[0060] Specifically, the base plate 11 is an L-shaped plate-like member as a whole, and a plurality of prestressed reinforcement members 15 are coaxially arranged on the vertical outer wall of the plate-like member; the cover plate 13 is a right-angled Z-shaped plate-like member as a whole, and a plurality of prestressed support members 16 are arranged on the outer wall of one side of the plate-like member, and the prestressed support members 16 and the prestressed reinforcement members 15 are symmetrically arranged with each other.
[0061] Specifically, a lower baffle 17 is installed at the lower part of one end of the bottom plate 11 and the cover plate 13, one end of the lower baffle 17 is detachably connected to the bottom plate 11, and the other end is detachably connected to the cover plate 13; an upper baffle 18 is installed at the upper part of the other end of the bottom plate 11 and the cover plate 13, one end of the upper baffle 18 is detachably connected to the bottom plate 11, and the other end is detachably connected to the cover plate 13.
[0062] More specifically, the cover plate 13 is also provided with a plurality of granular anti-skid protrusions 19, which are arranged on the upper casting end surface of the cover plate 13; the lower baffle plate 17 and the upper baffle plate 18 are both arc-shaped baffle plates, and are located at the connection between the bottom plate 11 and the cover plate 13.
[0063] Furthermore, the supporting counterweight component 12 is an inverted U-shaped ridge, a pier or a square-shaped component, and is located between the base plate 11 and the cover plate 13; the total number of the supporting counterweight components 12 is set to multiple, and the multiple supporting counterweight components 12 are arranged in several rows, and one end of the supporting counterweight component 12 is fixedly connected to the base plate 11, and the other end is overlapped with the cover plate 13.
[0064] Furthermore, the telescopic mounting seat 21 is an elastic inverted convex-shaped or inverted "X"-shaped component; the expansion joint baffle 22 is a plate-shaped component; a plurality of buffer members 25 are arranged at intervals in the expansion joint 23, and the buffer member 25 is a shock-absorbing spring, one end of the shock-absorbing spring is connected to one of the expansion joint baffles 22, and the other end is connected to the other expansion joint baffle 22; the expansion joint 23 is filled with a filler 231, and a flexible filler is filled inside its top end; the prestressed connector 24 is connected to the prestressed dispersion layer 3.
[0065] Specifically, the prestressed reinforcement 15 and the prestressed support 16 are both connected to the prestressed dispersion layer 3, and the prestressed dispersion layer 3 is an expanded mesh, a steel plate mesh, a steel wire mesh, a reinforced steel mesh, a galvanized steel wire mesh or a ribbed metal mesh or a crack-resistant and fire-proof steel mesh.
[0066] Furthermore, a construction method of an anti-crack bridge deck expansion joint device and a construction method thereof include the following construction steps:
[0067] Step 1, construction preparation, the construction personnel first measure and locate, accurately place the support assembly 1 at the expansion joint position of the bridge deck 4, and temporarily fix it;
[0068] Step 2: The bridge deck 4 is paved with a prestressed dispersion layer 3, and the prestressed dispersion layer 3 is connected to the prestressed reinforcement 15 and the prestressed support 16 on the side of the support assembly 1, and the prestressed dispersion layer 3 is welded firmly at the hook connection;
[0069] Step 3, temporarily seal the upper opening of the support assembly 1 with an extruded board, pour the bridge deck 4 and pave the bottom filling layer 5, the height of the bridge deck 4 pavement bottom filling layer 5 is flush with the upper opening of the support assembly 1, and ensure that the support assembly 1 does not move during the concrete pouring process;
[0070] Step 4: The bottom filling layer 5 of the bridge deck 4 is paved and maintained. If there is a gap between the support assembly 1 and the bottom filling layer 5 on both sides, hot asphalt is used for sealing;
[0071] Step 5, clean the extruded board, install the expansion joint device 2, and accurately insert the protrusion of the expansion joint device 2 into the recess of the support component 1;
[0072] Step 6, before paving the asphalt mixture surface layer, spray the tack coat asphalt on the outer wall of the expansion joint device 2, and install the prestressed dispersion layer 3, the prestressed dispersion layer 3 is connected to the prestressed connector 24 in the expansion joint device 2, and is firmly welded at the hook connection, and the prestressed dispersion layer 3 and the prestressed connector 24 are integrally fixed on the formed concrete bridge deck pavement;
[0073] Step 7, after installing the expansion joint device 2, fill the gap in the side wall of the expansion joint device 2 with an extruded board;
[0074] Step 8, paving the top filling layer 6 of the bridge deck, the top filling layer 6 is paved to the expansion joint baffle 22 of the expansion joint device 2, and the top filling layer 6 near the expansion joint device 2 is rolled using a small vibrating roller, and a large roller is not allowed to be used, and during the rolling process, it is ensured that the expansion joint device 2 does not move;
[0075] Step 9, clean the extruded plate inside the side wall of the expansion joint device 2, and seal it with silicone or polysulfide material, with the seal slightly lower than the top of the expansion joint device 2.
[0076] Specifically, in step 2, the prestressed reinforcement member 15 and the prestressed support member 16 are both bent steel bars with hooks;
[0077] In step 3, the bottom filling layer 5 is a mixture of one or more of high-strength concrete, foamed concrete, ceramsite concrete, polystyrene particle foamed concrete, extruded polystyrene board, polystyrene foam board, ordinary concrete, foamed concrete, lightweight concrete, EPS particle concrete or foamed polyurethane.
[0078] In the step 8, the top filling layer 6 is asphalt concrete.
[0079] In the present invention, the bottom filling layer 5 is a high-strength lightweight polystyrene particle concrete; a cement-based thermal insulation and sound-absorbing layer, a metal plate layer, a rock wool plate layer, a shock-absorbing layer, a waterproof layer and a stress dispersion layer are arranged in the high-strength lightweight polystyrene particle concrete, and the cement-based thermal insulation and sound-absorbing layer, the metal plate layer, the rock wool plate layer, the waterproof layer and the stress dispersion layer are stacked or mixed together in sequence.
[0080] The outer surfaces of the support assembly 1, the expansion joint device 2 and the prestressed dispersion layer 3 are sprayed with an injection molding layer, an anti-rust layer, a waterproof layer and a warning layer in sequence from the inside to the outside, and the warning layer is coated with fluorescent powder.
[0081] Specifically, a polymer wear-resistant material is injection molded on the injection layer; the anti-rust layer includes an epoxy zinc-rich primer and a chlorinated rubber topcoat and an epoxy micaceous iron intermediate paint between the epoxy zinc-rich primer and the chlorinated rubber topcoat; the waterproof layer is a polyurethane waterproof coating; the warning layer is a yellow or black reflective warning tape or a reflective color film or a reflective paint
[0082] At the same time, in the present invention, the connections referred to are all fixed connections, movable connections, or detachable connections, wherein the fixed connection is a welding connection or is directly processed into an integrally formed structure; the movable connection or detachable connection is a hinged connection, a threaded connection, a bayonet connection, a plug-in connection, or a bolt assembly connection or a screw connection.
[0083] Finally, it should be noted that the above has been combined with the embodiments and drawings to clearly and completely describe the concept, specific structure and technical effects of the present invention, so as to fully understand the purpose, characteristics and effects of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, other embodiments obtained by technicians in this field without creative work are within the scope of protection of the present invention. In addition, all the connections and connection relationships mentioned in the text do not refer to the direct connection of components, but refer to the formation of a better connection structure by adding or reducing connection accessories according to the specific implementation situation. The various technical features in the invention can be combined interchangeably without conflicting with each other.
Claims
1. A construction method for an anti-crack bridge deck expansion joint device, characterized in that: The construction steps include: Step 1, construction preparation, the construction personnel first measure and locate, accurately place the support assembly (1) at the expansion joint position of the bridge deck (4), and temporarily fix it; Step 2, paving the bridge deck (4) with a prestressed dispersion layer (3), connecting the prestressed dispersion layer (3) with the prestressed reinforcement (15) and the prestressed support (16) on the side of the support assembly (1), and welding them firmly at the hook connection; Step 3, temporarily sealing the upper opening of the support assembly (1) with an extruded board, pouring the bottom filling layer (5) of the bridge deck (4), the height of the bottom filling layer (5) of the bridge deck (4) is flush with the upper opening of the support assembly (1), and ensuring that the support assembly (1) does not move during the concrete pouring process; Step 4, the bottom filling layer (5) of the bridge deck (4) is paved and maintained. If there is a gap between the support assembly (1) and the bottom filling layer (5) on both sides, hot asphalt is used for sealing; Step 5, clean the extruded board, install the expansion joint device (2), and accurately insert the protrusion of the expansion joint device (2) into the recess of the support component (1); Step 6, before paving the asphalt mixture surface layer, spray the tack coat asphalt on the outer wall of the expansion joint device (2), and install the prestressed dispersion layer (3), the prestressed dispersion layer (3) is connected to the prestressed connector (24) in the expansion joint device (2), and is firmly welded at the hook connection, and the prestressed dispersion layer (3) and the prestressed connector (24) are integrally fixed on the formed concrete bridge deck pavement; Step 7, after installing the expansion joint device (2), fill the gap in the side wall of the expansion joint device (2) with an extruded board; Step 8, paving the top filling layer (6) of the bridge deck, the top filling layer (6) is paved to the expansion joint baffle (22) of the expansion joint device (2), and the top filling layer (6) near the expansion joint device (2) is rolled using a small vibrating roller, and a large roller is not allowed to be used, and during the rolling process, it is ensured that the expansion joint device (2) does not move; Step 9, cleaning the extruded plate inside the side wall of the expansion joint device (2), and sealing it with silicone or polysulfide materials, with the sealing being slightly lower than the top of the expansion joint device (2); wherein: The support assembly (1) and the expansion joint device (2) installed above the support assembly (1) are installed in sequence from bottom to top; The contraction joint device (2) comprises a telescopic mounting seat (21) and expansion joint baffles (22) symmetrically connected to both sides of the top of the telescopic mounting seat (21); an expansion joint (23) is formed between the two expansion joint baffles (22); a plurality of prestressed connectors (24) are provided on the two expansion joint baffles (22); the prestressed connectors (24) are symmetrically and coaxially connected to the outer walls of the two expansion joint baffles (22); The support assembly (1) comprises a base plate (11), a supporting weight component (12) and a cover plate (13), wherein the base plate (11), the supporting weight component (12) and the cover plate (13) are arranged and installed in sequence from bottom to top; an installation groove (14) is formed between the base plate (11) and the upper part of one end of the cover plate (13), the shrinkage device (2) is engaged in the installation groove (14), the installation groove (14) is filled with filler, and the top end is filled with flexible filler; The bottom plate (11) is an L-shaped plate-like member as a whole, and a plurality of prestressed reinforcement members (15) are coaxially arranged on the vertical outer wall of the plate-like member; the cover plate (13) is a right-angled Z-shaped plate-like member as a whole, and a plurality of prestressed support members (16) are arranged on the outer wall of one side of the plate-like member, and the prestressed support members (16) and the prestressed reinforcement members (15) are symmetrically arranged with each other; A lower baffle (17) is installed at the lower part of one end of the bottom plate (11) and the cover plate (13); one end of the lower baffle (17) is detachably connected to the bottom plate (11), and the other end is detachably connected to the cover plate (13); an upper baffle (18) is installed at the upper part of the other end of the bottom plate (11) and the cover plate (13); one end of the upper baffle (18) is detachably connected to the bottom plate (11), and the other end is detachably connected to the cover plate (13).
2. The construction method of a crack-proof bridge deck expansion joint device according to claim 1, characterized in that: The cover plate (13) is also provided with a plurality of granular anti-skid protrusions (19), and the anti-skid protrusions (19) are arranged on the upper casting end surface of the cover plate (13); the lower baffle plate (17) and the upper baffle plate (18) are both arc-shaped baffle plates, and are located at the connection between the bottom plate (11) and the cover plate (13).
3. The construction method of a crack-proof bridge deck expansion joint device according to claim 1, characterized in that: The supporting counterweight component (12) is an inverted U-shaped ridge, a pier or a square-shaped component, and is located between the base plate (11) and the cover plate (13); the total number of the supporting counterweight components (12) is set to be multiple, and the multiple supporting counterweight components (12) are arranged in rows, and one end of the supporting counterweight component (12) is fixedly connected to the base plate (11), and the other end is overlapped with the cover plate (13).
4. The construction method of a crack-proof bridge deck expansion joint device according to claim 1, characterized in that: The telescopic mounting seat (21) is an elastic inverted convex-shaped or inverted "X"-shaped component; the expansion joint baffle (22) is a plate-shaped component; a plurality of buffers (25) are arranged at intervals in the expansion joint (23); the buffers (25) are shock-absorbing springs, one end of the shock-absorbing spring is connected to one of the expansion joint baffles (22), and the other end is connected to the other expansion joint baffle (22); the expansion joint (23) is filled with a filler (231), and a flexible filler is filled inside the top end thereof; the prestressed connector (24) is connected to the prestressed dispersion layer (3).
5. The construction method of a crack-proof bridge deck expansion joint device according to claim 1, characterized in that: The prestressed reinforcement member (15) and the prestressed support member (16) are both connected to a prestressed dispersion layer (3), and the prestressed dispersion layer (3) is an expanded mesh, a steel plate mesh, a steel wire mesh, a reinforced steel mesh, a galvanized steel wire mesh or a ribbed metal mesh or a crack-resistant and fire-proof steel mesh.
6. The construction method of a crack-proof bridge deck expansion joint device according to claim 1, characterized in that: In step 2, the prestressed reinforcement member (15) and the prestressed support member (16) are both bent steel bars with hooks; In step 3, the bottom filling layer (5) is a mixture of one or more of high-strength concrete, foamed concrete, ceramsite concrete, polystyrene particle foamed concrete, extruded polystyrene board, polystyrene foam board, ordinary concrete, foamed concrete, lightweight concrete, EPS particle concrete or foamed polyurethane. In the step 8, the top filling layer (6) is asphalt concrete.