Semiconductor structure and method for manufacturing the same
By forming an upper semiconductor layer with an undoped semiconductor layer and a doped ion band in the interlayer dielectric layer in the semiconductor structure production method, the problem of GIDL current in the MOSFET is solved, the GIDL effect is reduced and the electrical performance is improved.
Patent Information
- Application Number
- CN201910456609.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-05-29
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2039-05-29
AI Technical Summary
In semiconductor structures, as the size of MOSFETs decreases, the leakage current phenomenon of static power consumption gradually appears, especially the GIDL current dominates when the device is in a waiting state, which affects the reliability of battery power technology.
In the method of producing a semiconductor structure, a contact hole is formed in the interlayer dielectric layer, and an undoped semiconductor layer is formed at the bottom, and an upper semiconductor layer with doped ions is formed on the undoped semiconductor layer, so that the The doped ions diffuse into the undoped semiconductor layer after thermal annealing, avoiding the doped ion concentration of the overlapping region of the doped region and the gate structure to reduce the GIDL effect.
The GIDL effect is effectively reduced, the electrical performance of the semiconductor structure is improved, and the conductive performance of the conductive plug is ensured through the same design as the material of the undoped semiconductor layer and the upper semiconductor layer.
Smart Images

Figure CN112018039B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor structure and a manufacturing method thereof. Background Art
[0002] With the advancement of semiconductor manufacturing technology and the increasing demand for the convenience of electronic devices, high integration and miniaturization of circuits have become the current development trend. Semiconductor structures are widely used in digital circuits and analog circuits, among which metal-oxide-semiconductor field-effect transistors (MOSFET) are the main representatives.
[0003] At present, in order to improve the performance of integrated circuits and reduce the cost of chip manufacturing, manufacturers are constantly developing smaller MOSFETs. The success of MOSFET in digital signal processing comes from the invention of CMOS logic circuits. The biggest advantage of this structure is that there is no static power loss in theory, which can greatly increase the standby time of mobile electronic devices. However, as the size of MOSFET continues to shrink, the leakage current phenomenon that causes static power consumption has gradually emerged, which mainly includes subthreshold leakage current, gate leakage current and gate-induced drain leakage (GIDL). When the device in the circuit is in a waiting state or off state, the GIDL current dominates the leakage current. Therefore, how to turn off or reduce the GIDL current of the device has become a key issue in the reliability of battery-powered technology. Summary of the invention
[0004] The embodiment of the present invention provides a semiconductor structure and a manufacturing method thereof, which can reduce the GIDL effect of the semiconductor structure.
[0005] To solve the above technical problems, an embodiment of the present invention provides a method for manufacturing a semiconductor structure, comprising: providing a substrate, wherein the substrate has a gate structure, the substrate exposing the top surface of the gate structure, and doped regions are formed in the substrate on opposite sides of the gate structure; forming an interlayer dielectric layer on the substrate, the interlayer dielectric layer covering the doped region and the gate structure; forming a contact hole in the interlayer dielectric layer, the contact hole exposing the surface of the doped region; and forming an undoped semiconductor layer at the bottom of the contact hole, the undoped semiconductor layer being in contact with the surface of the doped region.
[0006] An embodiment of the present invention also provides a semiconductor structure, comprising: a substrate, wherein a gate structure is provided therein, and wherein the substrate exposes the top surface of the gate structure; a doped region, wherein the doped region is located on two opposite sides of the gate structure; an interlayer dielectric layer, wherein the interlayer dielectric layer covers the doped region and the gate structure, wherein the interlayer dielectric layer has a contact hole, and wherein the contact hole exposes the surface of the doped region; an undoped semiconductor layer, wherein the undoped semiconductor layer is located at the bottom of the contact hole, and wherein the undoped semiconductor layer is located on the surface of the doped region; and an upper semiconductor layer, wherein the upper semiconductor layer is located in the contact hole, wherein the upper semiconductor layer is located on the undoped semiconductor layer, and wherein the upper semiconductor layer has doped ions.
[0007] Compared with the prior art, the technical solution provided by the embodiment of the present invention has the following advantages:
[0008] The embodiment of the present invention provides a method for manufacturing a semiconductor structure, in which an upper semiconductor layer with doped ions is located above an undoped semiconductor layer in a contact hole in an interlayer dielectric layer, so that the doped ions in the upper semiconductor layer diffuse into the undoped semiconductor layer after being activated. The undoped semiconductor layer plays a role in blocking the diffusion of doped ions into the doped region below the contact hole, thereby avoiding the problem of increased doped ion concentration in the overlapping region of the doped region and the gate structure, that is, it is conducive to indirectly reducing the doped ion concentration in the overlapping region of the doped region and the gate structure, thereby reducing the GIDL effect and improving the electrical performance of the semiconductor structure.
[0009] In addition, the undoped semiconductor layer and the upper semiconductor layer are made of the same material, which helps to ensure that the contact resistance between the undoped semiconductor layer and the upper semiconductor layer is small, thereby improving the conductive performance of the conductive plug.
[0010] In addition, after forming the upper semiconductor layer, a thermal annealing process is performed to activate the doped ions in the upper semiconductor layer so that the doped ions diffuse into the undoped semiconductor layer. After the thermal annealing process, the doped ion concentration of the undoped semiconductor layer is greater than 1.0E20Atom / cm 3 , the resistance of the undoped semiconductor layer decreases and the conductivity of the conductive plug increases. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] One or more embodiments are exemplarily described by pictures in the corresponding drawings, and these exemplified descriptions do not constitute limitations on the embodiments. Elements with the same reference numerals in the drawings represent similar elements, and unless otherwise stated, the figures in the drawings do not constitute proportional limitations.
[0012] Figure 1 It is a schematic diagram of a cross-sectional structure of a semiconductor structure;
[0013] Figures 2 to 6 A schematic diagram of the cross-sectional structure corresponding to each step of the method for manufacturing a semiconductor structure provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0014] As can be seen from the background art, the semiconductor structure in the prior art has a GIDL effect.
[0015] Figure 1 It is a schematic diagram of a semiconductor structure. Figure 1 The semiconductor structure includes: a substrate 21, wherein the substrate 21 has a gate structure 23, and the substrate 21 exposes the top surface of the gate structure 23; a doped region 24, wherein the doped region 24 is located on opposite sides of the gate structure 23; an interlayer dielectric layer 27, wherein the interlayer dielectric layer 27 covers the doped region 24 and the gate structure 23, and wherein the interlayer dielectric layer 27 has a contact hole, and wherein the contact hole exposes the surface of the doped region 24; and a semiconductor layer 26, wherein the semiconductor layer 26 fills the contact hole, and wherein the semiconductor layer 26 is located on the surface of the doped region 24.
[0016] In the process steps of manufacturing the above semiconductor structure, there is a problem of high-concentration ions in the semiconductor layer 26 diffusing into the active area. Analysis shows that the reasons for the above problem are as follows: there is a thermal annealing process step in the process of manufacturing the semiconductor structure, and before the thermal annealing process step, in order to ensure that the manufactured semiconductor layer 26 has good conductivity, doping ions with a concentration higher than that of the doping region 24 are usually injected into the semiconductor layer 26, and the thermal annealing process step activates the doping ions in the semiconductor layer 26, and the doping ions are transferred to the doping region 24 due to the diffusion effect caused by the concentration difference, thereby increasing the doping ion concentration in the overlapping area of the doping region 24 and the gate structure 23, and enhancing the GIDL effect.
[0017] To solve the above problems, an embodiment of the present invention provides a method for manufacturing a semiconductor structure, by forming an undoped semiconductor layer at the bottom of a contact hole, and forming an upper semiconductor layer with doped ions on the undoped semiconductor layer, so that during the thermal annealing process of the semiconductor structure, the doped ions in the upper semiconductor layer diffuse into the undoped semiconductor layer without affecting the doped ion concentration in the overlapping area of the doped region and the gate structure, thereby reducing the GIDL effect.
[0018] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the embodiments of the present invention will be described in detail below with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present invention, many technical details are provided to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can be implemented.
[0019] The method for manufacturing a semiconductor structure provided by an embodiment of the present invention will be described in detail below with reference to the accompanying drawings.
[0020] Figures 2 to 6 A schematic cross-sectional structure diagram corresponding to each step of a method for manufacturing a semiconductor structure provided by an embodiment of the present invention.
[0021] Reference Figure 2 A substrate 11 is provided, wherein the substrate 11 has a gate structure 13, the substrate 11 exposes the top surface of the gate structure 13, and doped regions 14 are formed in the substrate 11 on opposite sides of the gate structure 13.
[0022] In this embodiment, an isolation structure 12 is further formed in the substrate 11 , and the material of the isolation structure may be silicon oxide or silicon nitride.
[0023] In this embodiment, two gate structures 13 are formed in the substrate. In other embodiments, the number of gate structures can be one, three, or any positive natural number, which can be set according to actual needs. The gate structure 13 includes a gate dielectric layer 101, a gate 102, and a passivation layer 103.
[0024] The process steps for forming the gate structure 13 are as follows:
[0025] A patterned photoresist is formed on the substrate 11, and the patterned photoresist is used to define the pattern of the gate structure 13 to be formed. An etching process is performed to remove the substrate at the position where the gate structure 13 is to be formed, and a groove to be filled with the gate structure 13 is formed. Among them, the etching method is preferably dry silicon etching. After the etching process, a gate dielectric layer 101 is formed by a high-temperature oxidation process, and the temperature of the high-temperature oxidation process is, for example, 900°C to 1200°C. The high-temperature oxidation process will form an oxide layer on the surface of the groove in the substrate 11, and the oxide layer will serve as the gate dielectric layer 101. The high-temperature oxidation process will also form an intermediate oxide layer (not shown) on the top surface of the substrate. In this embodiment, the oxide layer formed on the top surface of the substrate 11 is retained. In other embodiments, the intermediate oxide layer located on the top surface of the substrate can be removed.
[0026] The gate 102 is formed by depositing materials on the gate dielectric layer 101 and etching back through a dry etching process so that the gate 102 covers a portion of the surface of the gate dielectric layer 101. After the gate 102 is formed, deposition or filling is performed again to form a passivation layer 103. After deposition or filling, the passivation layer 103 also needs to be etched back or planarized, and non-limiting examples of the planarization process include a mechanical planarization method and a chemical mechanical polishing planarization method.
[0027] In this embodiment, the top surface of the passivation layer 103 is flush with the surface of the intermediate oxide layer. In other embodiments, the top surface of the passivation layer 103 is flush with the top surface of the substrate 11.
[0028] The doped region 14 can be formed by ion implantation and diffusion process. In this embodiment, the ion implantation and diffusion process is performed after the high temperature oxidation process. Since the high temperature oxidation process will form an intermediate oxide layer on the top surface of the substrate 11, and the intermediate oxide layer can effectively alleviate the problem of damage to the substrate 11 caused by the bombardment of high energy ions during the ion implantation process, and the presence of the intermediate oxide layer can save the step of forming an ion implantation protection layer. In other embodiments, the ion implantation process can also be performed before the high temperature oxidation process.
[0029] After performing the ion implantation process to form the doping region, a thermal annealing process can be performed to further activate the doping ions in the doping region 14 and diffuse the doping ions to form a source / drain region (S / D) with a more uniform particle distribution. In addition, the thermal annealing process can further drive ion migration, so that the doping ion concentration in the doping region 14 is distributed decreasingly in the direction away from the top surface. The advantage of this concentration gradient with the maximum doping ion concentration located in the top region of the doping region is that, without increasing the total amount of doping ions in the doping region 14, the concentration difference between the top region of the doping region 14 and other regions in contact with the top of the doping region is reduced, so that in the subsequent thermal annealing process, the ion diffusion of high-concentration doping ions to the low-doping ion concentration region caused by activation can be reduced, avoiding the problem of increasing the doping ion concentration in the overlapping region of the doping region and the gate structure, indirectly reducing the doping ion concentration in the overlapping region of the doping region and the gate structure, thereby reducing the GIDL effect and improving the electrical performance of the semiconductor structure. The temperature of the thermal annealing process is, for example, 900°C-1100°C.
[0030] Reference Figure 3 , an interlayer dielectric layer 17 is formed on the substrate 11 , and the interlayer dielectric layer 17 covers the doped region 14 and the gate structure 13 .
[0031] In the present embodiment, the interlayer dielectric layer 17 is deposited and planarized, and non-limiting examples of the planarization process include a mechanical planarization method and a chemical mechanical polishing planarization method.
[0032] The interlayer dielectric layer 17 is usually made of oxide or nitride.
[0033] Reference Figure 4 , a contact hole 18 is formed in the interlayer dielectric layer 17 , and the contact hole 18 exposes the surface of the doped region 14 .
[0034] In this embodiment, the process steps for forming the contact hole include: first, forming a patterned photoresist layer on the surface of the interlayer dielectric layer 17, the photoresist layer setting the position and size of the contact hole 18 to be formed, and then etching the interlayer dielectric layer 17 using the patterned photoresist as a mask, stopping at the surface of the doped region 14 to form the contact hole 18, the contact hole 18 penetrates the interlayer dielectric layer 17 and the intermediate oxide layer (not shown) located on the top surface of the substrate.
[0035] After etching is completed, the patterned photoresist layer is removed, and an ashing method or other suitable methods may be used.
[0036] Reference Figure 5 An undoped semiconductor layer 15 is formed at the bottom of the contact hole 18 , and the undoped semiconductor layer 15 is in contact with the surface of the doped region 14 .
[0037] The undoped semiconductor layer 15 is located on the top surface of the doped region 14 and is not doped with N-type ions or P-type ions, thereby preventing the doped ions at other locations in the contact hole 18 from diffusing into the doped region 14 below the contact hole 18 due to ion activation in the subsequent thermal annealing process. Since the doped ions will diffuse into the undoped semiconductor layer 15, the problem of increased doping concentration in the overlapping area of the doped region 14 and the gate structure 13 can be avoided.
[0038] The doping ion concentration in the doping region 14 in contact with the undoped semiconductor layer 15 is distributed decreasingly in the direction away from the undoped semiconductor layer. This decreasing distribution can reduce the ion diffusion from the high-concentration doping ion region to the low-concentration doping ion region due to ion activation without increasing the total amount of doping ions in the doping region 14, avoids the problem of increased doping ion concentration in the overlapping area of the doping region and the gate structure, indirectly reduces the doping ion concentration in the overlapping area of the doping region and the gate structure, thereby reducing the GIDL effect and improving the electrical performance of the semiconductor structure.
[0039] In this embodiment, before the deposition of the undoped semiconductor layer 15, a pre-cleaning step is performed to remove the natural oxide layer and reduce the contact resistance between the undoped semiconductor layer 15 and the doped region 14. The pre-cleaning may be performed using any suitable method known to those skilled in the art, such as using a cleaning solution including hydrofluoric acid. In other embodiments, when there is no oxide layer, this step may not be performed.
[0040] The undoped semiconductor layer 15 may be formed by chemical vapor deposition or physical vapor deposition, and the thickness of the undoped semiconductor layer 15 may be controlled by adjusting process parameters such as the deposition time.
[0041] In this embodiment, the method for forming the undoped semiconductor layer 15 includes: forming a sacrificial semiconductor layer that fills the contact hole 18; removing a portion of the sacrificial semiconductor layer, and the remaining sacrificial semiconductor layer serves as the undoped semiconductor layer 15. The material of the undoped semiconductor layer 15 includes polycrystalline silicon, polycrystalline germanium, or polycrystalline silicon germanium.
[0042] In this embodiment, the thickness of the undoped semiconductor layer 15 is 10-20 nm. The thickness of the undoped semiconductor layer is related to the subsequent thermal annealing process. The higher the temperature and the longer the thermal treatment time in the thermal annealing process, the thicker the thickness of the undoped semiconductor layer 15. In this embodiment, when the thickness is 10-20 nm, the diffusion effect caused by ion activation can be blocked. In other embodiments, when the temperature environment or the thermal treatment time of the thermal annealing process changes, the thickness of the undoped semiconductor layer is not limited to 10-20 nm.
[0043] Reference Figure 6 An upper semiconductor layer 16 filling up the contact holes (not shown) is formed on the surface of the undoped semiconductor layer 15 , and the upper semiconductor layer 15 has doped ions.
[0044] In the present embodiment, in the process step of forming the upper semiconductor layer 16 on the undoped semiconductor layer 15, the upper semiconductor layer 16 is doped with doping ions of the same type as the doping ions in the doping region 14, and the types of doping ions include N-type ions and P-type ions. The doping ion concentration of the upper semiconductor layer 16 is greater than the doping ion concentration of the top region of the doping region 14, and the top region of the doping region 14 is the region of the doping region 14 close to the undoped semiconductor layer 15.
[0045] It should be noted that, in other embodiments, after the process step of forming the upper semiconductor layer 16, the upper semiconductor layer 16 may be doped with doping ions of the same type as the doping ions in the doping region 14. If there is material remaining on the surface of the interlayer dielectric layer 17 after the upper semiconductor layer 16 is formed, it is necessary to perform back etching or CMP to remove the excess residual material.
[0046] It should be noted that, in other embodiments, the method of forming an undoped semiconductor layer and an upper semiconductor layer may also include: forming an undoped semiconductor layer at the bottom and sidewalls of the contact hole; forming an upper semiconductor layer on the surface of the undoped semiconductor layer, and doping doped ions in the upper semiconductor layer during or after the process step of forming the upper semiconductor layer.
[0047] The undoped semiconductor layer 15 blocks the doping ions in the upper semiconductor layer 16 from diffusing into the doping region 14 below the contact hole, thereby avoiding the problem of an increase in the doping ion concentration in the overlapping region of the doping region 14 and the gate structure 13. In addition, the doping region below the undoped semiconductor layer 15 has a doping ion concentration that decreases in a direction away from the undoped semiconductor layer. This gradient distribution can reduce the effect of the doping ions in the upper semiconductor layer 16 diffusing into the doping region 14 without increasing the total amount of doping ions in the doping region 14, and cooperates with the blocking of the undoped semiconductor layer 15.
[0048] In this embodiment, in order to ensure that the conductive medium in the contact hole has good conductive properties, the material of the upper semiconductor layer 16 is the same as the material of the undoped semiconductor layer 15, so that the contact resistance between the undoped semiconductor layer 15 and the upper semiconductor layer 16 is small, and the undoped semiconductor layer 15 and the upper semiconductor layer 16 together fill the contact hole and form a conductive plug.
[0049] After executing the above-mentioned method for manufacturing the semiconductor structure, a thermal annealing step can also be performed. The purpose of the thermal annealing is to activate the doped ions in the upper semiconductor layer 16. The thermal annealing can use any suitable annealing method, such as furnace tube annealing, peak annealing, laser annealing, pulsed electron beam rapid annealing, ion beam rapid annealing, continuous wave laser rapid annealing, and incoherent broadband light source (such as halogen lamp, arc lamp, graphite heating) rapid annealing.
[0050] During the thermal annealing process, the doped ions in the upper semiconductor layer 16 are activated, and the formation of the undoped semiconductor layer 15 allows the doped ions that were originally diffused to the doped region 14 below the contact hole to enter the undoped semiconductor layer 15, thereby avoiding the problem of increased doped ion concentration in the overlapping area of the doped region 14 and the gate structure 13. At the same time, the undoped semiconductor layer 15 plays the role of receiving the doped ions diffused after activation, that is, the doped ions in the upper semiconductor layer 16 are diffused and transferred to the undoped semiconductor layer 15, so that the undoped semiconductor layer 15 has good conductive properties. Finally, the upper semiconductor layer 16 and the undoped semiconductor layer 15 of the contact hole have similar doped ion concentrations. It should be noted that before the thermal annealing process, the doped ion concentration in the upper semiconductor layer 16 is 1.0E21~1.0E22Atom / cm 3 After the annealing process, the doping ion concentration in the undoped semiconductor layer 15 is greater than 1.0E20Atom / cm 3 .
[0051] In this embodiment, the undoped semiconductor layer 15 and the upper semiconductor layer 16 with doped ions fill the contact hole and together form a conductive plug. In the subsequent thermal annealing process step, since the undoped semiconductor layer 15 blocks the doped ions in the upper semiconductor layer 16 from diffusing to the doped region 14 below the contact hole, the doped ions diffuse into the undoped semiconductor layer 15, so that the undoped semiconductor layer 15 has good conductivity. The doped region below the undoped semiconductor layer 15 has a doped ion concentration that decreases in the direction away from the undoped semiconductor layer. This gradient distribution method can reduce the effect of the doped ions in the upper semiconductor layer 16 diffusing into the doped region 14 without increasing the total amount of doped ions in the doped region 14, and cooperates with the blocking effect of the undoped semiconductor layer 15. In addition, since the undoped semiconductor layer 15 and the upper semiconductor layer 16 are made of the same material, the contact resistance between the two is small. Therefore, this embodiment avoids the problem of increased doping ion concentration in the overlapping area of the doping region and the gate structure without affecting the conductive performance of the conductive plug, indirectly reduces the doping ion concentration in the overlapping area of the doping region and the gate structure, thereby reducing the GIDL effect and improving the electrical performance of the semiconductor structure.
[0052] Correspondingly, an embodiment of the present invention further provides a semiconductor structure.
[0053] refer to Figure 6 The semiconductor structure includes: a substrate 11, a gate structure 13 is provided in the substrate 11, and the substrate 11 exposes the top surface of the gate structure 13; a doped region 14, and the doped region 14 is located on two opposite sides of the gate structure 13; an interlayer dielectric layer 17, the interlayer dielectric layer 17 covers the doped region 14 and the gate structure 13, and the interlayer dielectric layer 17 has a contact hole, and the contact hole exposes the surface of the doped region 14; an undoped semiconductor layer 15, the undoped semiconductor layer 15 is located at the bottom of the contact hole, and the undoped semiconductor layer 15 is located on the surface of the doped region 14; an upper semiconductor 16, the upper semiconductor layer 16 is located in the contact hole, the upper semiconductor layer 16 is located on the undoped semiconductor layer 15, and the upper semiconductor layer 16 has doped ions.
[0054] The semiconductor structure provided by this embodiment will be described in detail below with reference to the accompanying drawings.
[0055] In this embodiment, the gate structure 13 is located inside the substrate 11 , which can make the overall structure more compact; the substrate 11 exposes the top surface of the gate structure 13 , which is convenient for subsequent electrical connection.
[0056] In this embodiment, the gate structure 13 includes a gate dielectric layer 101, a gate 102 and a passivation layer 103. There is also an intermediate oxide layer (not shown) between the substrate 11 and the interlayer dielectric layer 17, and the intermediate oxide layer and the gate dielectric layer 101 are formed in the same high-temperature oxidation process step. In other embodiments, the interlayer dielectric layer 17 covers the top surface of the substrate 11 and contacts the substrate 11.
[0057] The gate dielectric layer 101 may be made of commonly used oxides, such as silicon dioxide. The gate 102 material may be made of commonly used semiconductor materials in the art, such as polysilicon, etc., but is not limited to a certain type and will not be listed here one by one.
[0058] The passivation layer 103 plays a role in protecting the gate, and its material is usually oxide or nitride.
[0059] The doping regions 14 located on both sides of the gate structure 13 are heavily doped source / drain. The doping ions in the doping region 14 can be either P-type ions or N-type ions. The P-type doping ions include but are not limited to boron ions, indium ions, or a combination thereof, and the N-type doping ions include but are not limited to phosphorus ions, arsenic ions, or a combination thereof.
[0060] In this embodiment, the doping ion concentration in the doping region 14 decreases in the direction away from the interlayer dielectric layer 17, and the maximum doping ion concentration in the doping region 14 is in the top region of the doping region 14, and the top region of the doping region 14 is a region close to the undoped semiconductor layer 15. The advantage of such a concentration gradient with the maximum doping ion concentration located in the top region of the doping region is that, without increasing the total amount of doping ions in the doping region 14, the concentration difference between the doping ion concentration in the top region of the doping region 14 and the doping ion concentration in the upper semiconductor layer 16 is reduced, so that in the subsequent thermal annealing process, the ion diffusion of the doping ions in the upper semiconductor layer 16 to the low ion concentration region due to activation can be reduced, thereby reducing the GIDL effect.
[0061] In this embodiment, there are two gate structures 13, and the doped regions 14 are located at opposite sides of the gate structures 13. Two adjacent gate structures 13 share the doped region 14 located in the middle thereof. In other embodiments, the number of gate structures can be any positive natural number.
[0062] The number of contact holes in the interlayer dielectric layer 17 is the same as the number of doped regions 14, and the contact holes expose the top surfaces of the doped regions 14. When there is an intermediate oxide layer, the contact holes also need to penetrate the intermediate oxide layer.
[0063] In this embodiment, the undoped semiconductor layer 15 is located at the bottom of the contact hole and on the surface of the doped region 14. The material of the undoped semiconductor layer 15 includes polysilicon, polycrystalline germanium and polycrystalline germanium silicon. No N-type or P-type ions are doped in the undoped semiconductor layer 15. In other embodiments, the undoped semiconductor layer is also located on the sidewall of the contact hole.
[0064] In this embodiment, the thickness of the undoped semiconductor layer 15 is 10-20 nm.
[0065] The upper semiconductor layer 16 is located in the contact hole and above the undoped semiconductor layer 15, and fills the contact hole. In this embodiment, the doping ion concentration of the upper semiconductor layer 16 is 1.0E21-1.0E22 Atom / cm 3 , which is greater than the doping ion concentration in the doping region 14. The doping ion type in the upper semiconductor layer 16 is the same as the doping ion type in the doping region 14, which can be either N-type ions or P-type ions.
[0066] In this embodiment, the material of the upper semiconductor layer 16 is the same as that of the undoped semiconductor layer 15, and the contact resistance between the two is small. The material of the upper semiconductor layer 16 includes polysilicon, polycrystalline germanium or polycrystalline silicon germanium.
[0067] In this embodiment, the undoped semiconductor layer 15 and the upper semiconductor layer 16 with doped ions fill the contact hole and together form a conductive plug. The undoped semiconductor layer 15 blocks the doped ions in the upper semiconductor layer 16 from diffusing to the doped region 14 below the contact hole. The doped ions diffused downward enter the undoped semiconductor layer 15, so that the undoped semiconductor layer 15 has good conductivity. The doped region below the undoped semiconductor layer 15 has a doped ion concentration that decreases in the direction away from the undoped semiconductor layer 15. This gradient distribution can reduce the effect of the doped ions in the upper semiconductor layer 16 diffusing into the doped region 14 without increasing the total amount of doped ions in the doped region 14, which cooperates with the blocking effect of the undoped semiconductor layer 15. In addition, since the undoped semiconductor layer 15 and the upper semiconductor layer 16 are made of the same material, the contact resistance between the two is small. Therefore, this embodiment avoids the problem of increased doping ion concentration in the overlapping area of the doping region and the gate structure without affecting the conductive performance of the conductive plug, indirectly reduces the doping ion concentration in the overlapping area of the doping region and the gate structure, thereby reducing the GIDL effect and improving the electrical performance of the semiconductor structure.
[0068] Those skilled in the art will appreciate that the above embodiments are specific examples of the present invention, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present invention. Any person skilled in the art may make changes and modifications without departing from the spirit and scope of the present invention, and therefore the scope of protection of the present invention shall be subject to the scope defined in the claims.
Claims
1. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate, wherein the substrate has a gate structure, the substrate exposes a top surface of the gate structure, and doped regions are formed in the substrate on opposite sides of the gate structure; forming an interlayer dielectric layer on the substrate, wherein the interlayer dielectric layer covers the doped region and the gate structure; forming a contact hole in the interlayer dielectric layer, wherein the contact hole exposes the surface of the doped region; forming an undoped semiconductor layer at the bottom of the contact hole, wherein the undoped semiconductor layer is in contact with the surface of the doped region; An upper semiconductor layer filling the contact hole is formed on the surface of the undoped semiconductor layer, and the upper semiconductor layer has doping ions.
2. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The undoped semiconductor layer is made of the same material as the upper semiconductor layer.
3. The method for manufacturing a semiconductor structure according to claim 2, characterized in that: The material of the undoped semiconductor layer includes polycrystalline silicon, polycrystalline germanium or polycrystalline germanium silicon.
4. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The thickness of the undoped semiconductor layer is 10-20 nm.
5. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The type of doping ions in the upper semiconductor layer is the same as the type of doping ions in the doping region.
6. The method for manufacturing a semiconductor structure according to claim 5, characterized in that: The doping ion types in the upper semiconductor layer include P-type ions or N-type ions.
7. The method for manufacturing a semiconductor structure according to claim 5, characterized in that: The doping ion concentration of the upper semiconductor layer is greater than the doping ion concentration of the top region of the doping region, and the top region is a region of the doping region close to the undoped semiconductor layer.
8. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The method for forming the undoped semiconductor layer and the upper semiconductor layer comprises: forming a sacrificial semiconductor layer that fills the contact hole; removing a portion of the thickness of the sacrificial semiconductor layer, and using the remaining sacrificial semiconductor layer as the undoped semiconductor layer; forming the upper semiconductor layer on the surface of the undoped semiconductor layer, and doping the doping ions in the upper semiconductor layer during or after the process step of forming the upper semiconductor layer.
9. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The method for forming the undoped semiconductor layer and the upper semiconductor layer comprises: forming the undoped semiconductor layer at the bottom and sidewall of the contact hole; forming the upper semiconductor layer on the surface of the undoped semiconductor layer, and doping the doping ions in the upper semiconductor layer during or after the process step of forming the upper semiconductor layer.
10. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: After forming the upper semiconductor layer, a thermal annealing process is performed.
11. The method for manufacturing a semiconductor structure according to claim 10, characterized in that: Before the thermal annealing process, the doping ion concentration in the upper semiconductor layer is 1.0E21~1.0E22Atom / cm 3 .
12. A semiconductor structure, characterized in that: include: A substrate, wherein the substrate has a gate structure therein, and the substrate exposes a top surface of the gate structure; doped regions, the doped regions being located at opposite sides of the gate structure; an interlayer dielectric layer, the interlayer dielectric layer covers the doped region and the gate structure, the interlayer dielectric layer has a contact hole, and the contact hole exposes the surface of the doped region; An undoped semiconductor layer, wherein the undoped semiconductor layer is located at the bottom of the contact hole and the undoped semiconductor layer is located on the surface of the doped region; an upper semiconductor layer, wherein the upper semiconductor layer is located in the contact hole, the upper semiconductor layer is located on the undoped semiconductor layer, and the upper semiconductor layer has doped ions; Wherein, the material of the undoped semiconductor layer includes polycrystalline silicon, polycrystalline germanium or polycrystalline germanium silicon.
13. The semiconductor structure according to claim 12, characterized in that: The undoped semiconductor layer is made of the same material as the upper semiconductor layer.
14. The semiconductor structure according to claim 12, characterized in that: The thickness of the undoped semiconductor layer is 10-20 nm.
15. The semiconductor structure according to claim 12, characterized in that: The undoped semiconductor layer is located on the sidewall surface of the contact hole.
16. The semiconductor structure according to claim 12, characterized in that The type of doping ions in the upper semiconductor layer is the same as the type of doping ions in the doping region.
17. The semiconductor structure according to claim 16, characterized in that: The doping ion type in the upper semiconductor layer includes P type or N type.
18. The semiconductor structure according to claim 16, characterized in that The doping ion concentration of the upper semiconductor layer is greater than the doping ion concentration of the contact surface of the doping region with the undoped semiconductor layer.
19. The semiconductor structure according to claim 12, characterized in that The doping ion concentration of the doping region decreases in a direction away from the interlayer dielectric layer.