Optical components
By using the thickness ratio adjustment and construction of the refractive index laminate in the terahertz band optical element, the problem of manufacturing complexity is solved, the precise adjustment of the refractive index and the reflection prevention effect are achieved, and the manufacturing process is simplified.
Patent Information
- Application Number
- CN202010783557.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-08-09
- Filing Date
- 2020-08-06
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2040-08-06
AI Technical Summary
Prior Art When manufacturing terahertz band optical elements, multiple composite materials need to be made to adjust the refractive index, resulting in the problem of complex manufacturing processes.
By combining two laminates with different refractive indices from each other, the thickness ratio is adjusted to achieve refractive index adjustment of terahertz waves, the manufacturing process is simplified, and the pseudo-moth eye or monolayer reflection prevention film construction is introduced into the laminate. Implement reflection prevention of frequency bandwidth.
The accuracy of refractive index adjustment of terahertz waves is achieved and the manufacturing process is simplified, which reduces manufacturing complexity and maintains efficient reflection prevention effects.
Smart Images

Figure CN112346157B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an optical element. Background Art
[0002] In recent years, in order to realize various technologies using terahertz waves (electromagnetic waves in the terahertz band), research and development of optical elements that can be used in the terahertz band has been carried out. For example, a terahertz wave absorber is disclosed in Non-Patent Document 1 (GongjieXu, et al., "0.1-20THz ultra-broadband perfect absorber via a flat multi-layer structure" Optics Express 24, 23177 (2016)). In this Non-Patent Document 1, an example is given of a method in which a reflection prevention film whose refractive index is adjusted by nanoparticles such as titanium oxide microparticles or hollow polystyrene microspheres is provided on a highly doped silicon substrate. Summary of the invention
[0003] As optical elements, in addition to the above-mentioned absorbers, various elements such as lenses, polarizers, spectrometers, and sensors can also be cited. When constructing an optical element that can be used in the terahertz band, the adjustment of the refractive index relative to the terahertz wave becomes an important technical matter. In the above-mentioned non-patent document 1, the concentration of nanoparticles dispersed in the resin is controlled to form an arbitrary refractive index layer, and the refractive index layer with a high concentration of nanoparticles is stacked in sequence, thereby making an absorber for terahertz waves. However, in such a method, because it is necessary to make a composite material with multiple concentrations corresponding to each refractive index layer, there is a problem that the manufacturing process of the optical element is complicated.
[0004] The present invention has been made to solve the above-mentioned problems, and an object of the present invention is to provide an optical element that can be easily manufactured and in which the refractive index with respect to terahertz waves can be easily adjusted.
[0005] In order to solve the above problems, the inventors of the present application have focused on the relationship between the wavelength of light and the thickness of the layer constituting the optical element in the process of repeated in-depth research. Then, it was found that when the thickness of the layer constituting the optical element is sufficiently small relative to the wavelength of the terahertz wave, the layer does not have sensitivity to the terahertz wave. In the wavelength band of visible light, in order to make the thickness of the layer constituting the optical element sufficiently small relative to the wavelength of light, for example, the thickness of the layer needs to be set to less than 1nm, and the manufacturing method of such a layer is very limited. In addition, in the visible light region, even if the relationship between the wavelength of light and the thickness of the layer is not considered, there are many options for optical elements. On the other hand, the wavelength band of the terahertz wave is closer to the long wavelength side than the wavelength band of visible light, which can make the thickness of the layer constituting the optical element sufficiently small relative to the wavelength of light. Therefore, the inventors of the present application have obtained the insight that an optical element that is simple to manufacture and easy to adjust the refractive index relative to the terahertz wave can be realized by combining layers that do not have sensitivity to the terahertz wave, and have completed the present invention.
[0006] An optical element according to one aspect of the present invention comprises a stacked body including a first refractive index layer and a second refractive index layer having different refractive indices with respect to a terahertz wave, the stacked body having a paired layer group including a plurality of paired layers composed of the first refractive index layer and the second refractive index layer, the thickness of the first refractive index layer and the thickness of the second refractive index layer are both smaller than the wavelength of the terahertz wave, and the paired layers have a prescribed effective refractive index with respect to the terahertz wave corresponding to the ratio of the thickness of the first refractive index layer to the second refractive index layer.
[0007] In the optical element, the first refractive index layer and the second refractive index layer are both smaller than the wavelength of the terahertz wave. Therefore, the first refractive index layer and the second refractive index layer do not have sensitivity to the terahertz wave, and the effective refractive index of the paired layer composed of the first refractive index layer and the second refractive index layer corresponds to the ratio of the thickness of these layers and can take a value between the refractive index of the first refractive index layer and the refractive index of the second refractive index layer. Therefore, in the optical element, by adjusting the ratio of the thickness of the first refractive index layer and the thickness of the second refractive index layer in the paired layer, the effective refractive index relative to the terahertz wave can be adjusted to a desired value. In addition, in the optical element, since the desired refractive index is obtained by using only two refractive index layers with different refractive indices, the manufacturing becomes easier than the case of making a composite material of multiple concentrations corresponding to each refractive index layer.
[0008] It can also be the following mode: the optical element further has a main body supporting the stacked body, and in the paired layer group, the closer the paired layer is to the main body, the closer the effective refractive index of the paired layer with respect to the terahertz wave is to the refractive index of the main body with respect to the terahertz wave. In this case, the pseudo moth-eye structure can be formed in the main body. Therefore, a reflection prevention structure with a wide bandwidth for the terahertz wave can be formed in the main body. Since this structure is formed using only two refractive index layers, it is also possible to maintain ease of manufacturing.
[0009] Alternatively, the optical element may further include a main body supporting the laminate, and in the paired layer group, the effective refractive indexes of the paired layers with respect to the terahertz wave are equal to each other. In this case, the same anti-reflection structure as the single-layer anti-reflection film can be formed on the main body. Since the structure is formed using only two refractive index layers, it is also possible to maintain ease of manufacture.
[0010] Alternatively, the optical element may further include a main body supporting a stacked body, wherein a first pair of layers having a first effective refractive index with respect to terahertz waves and a second pair of layers having a second effective refractive index with respect to terahertz waves are alternately stacked. In this case, the same structure as the dielectric multilayer film can be formed in the main body. Since the structure is formed using only two refractive index layers, ease of manufacture can also be maintained.
[0011] Alternatively, in the stacked body, a plurality of paired layer groups having mutually different effective refractive indices with respect to terahertz waves are distributed along a direction intersecting the stacking direction of the paired layers. In this case, regions with different effective refractive indices can be distributed in any region in a direction intersecting the stacking direction of the paired layers. Since the refractive index distribution is formed using only two refractive index layers, ease of manufacture can also be maintained.
[0012] The thickness of the first refractive index layer and the thickness of the second refractive index layer may be less than 1 / 10 of the wavelength of the terahertz wave. In this case, the sensitivity of the first refractive index layer and the second refractive index layer to the terahertz wave can be sufficiently small. Therefore, the effective refractive index of the paired layer can be brought close to the target value with high precision.
[0013] The thickness of the first refractive index layer and the thickness of the second refractive index layer may be less than 1 / 100 of the wavelength of the terahertz wave. In this case, the sensitivity of the first refractive index layer and the second refractive index layer to the terahertz wave can be made sufficiently small. Therefore, the effective refractive index of the paired layer can be made closer to the target value with high precision.
[0014] According to the present invention, it is possible to provide an optical element that can be easily manufactured and in which the refractive index with respect to a terahertz wave can be easily adjusted. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic cross-sectional view showing the layer structure of the optical element according to the first embodiment.
[0016] Figure 2 It is a schematic cross-sectional view showing the layer structure of the optical element according to the second embodiment.
[0017] Figure 3 It is a schematic cross-sectional view showing a layer structure of an optical element according to a third embodiment.
[0018] Figure 4 It is a schematic cross-sectional view showing a layer structure of an optical element according to a fourth embodiment.
[0019] Figure 5 It is a schematic cross-sectional view showing a layer structure of an optical element according to a fifth embodiment.
[0020] Figure 6 This is a schematic cross-sectional view showing the layer structure of an optical element used for simulation.
[0021] Figure 7 A is a graph showing simulation results.
[0022] Figure 7 B is a graph showing simulation results.
[0023] Figure 8 A is a graph showing simulation results.
[0024] Figure 8 B is a graph showing simulation results.
[0025] Fig. 9 A is a graph showing simulation results.
[0026] Fig. 9 B is a graph showing simulation results.
[0027] Fig.10 A is a graph showing simulation results.
[0028] Fig.10 B is a graph showing simulation results.
[0029] Fig.11 A is a graph showing simulation results.
[0030] Fig.11 B is a graph showing simulation results. DETAILED DESCRIPTION
[0031] Hereinafter, preferred embodiments of an optical element according to one aspect of the present invention will be described in detail with reference to the accompanying drawings.
[0032] [First embodiment]
[0033] Figure 1 It is a schematic cross-sectional view showing the layer structure of the optical element involved in the first embodiment. The optical element involved in the first embodiment is an element that utilizes electromagnetic waves in the terahertz band (hereinafter referred to as "terahertz waves"). As such optical elements, for example, lenses, polarizers, spectrometers, absorbers, various sensors, etc. can be cited. In the following description, as an optical element, an element provided with an anti-reflection film is exemplified. In addition, the frequency of the terahertz wave to which the optical element is applied is, for example, 0.1THz to 10THz. The wavelength of the terahertz wave in this band is 30μm to 3000μm.
[0034] like Figure 1 As shown, the optical element 1A includes a main body 2 and an anti-reflection film 3 provided on the surface of the main body 2. The main body 2 has a main surface 2a located on the side of the anti-reflection film 3 in the thickness direction. The main surface 2a serves as an incident surface for incident terahertz waves in the optical element 1A. The main body 2 may be a component that transmits terahertz waves or a component that converts terahertz waves into electrical signals. In the case where the main body 2 is a sensor for detecting terahertz waves, in addition to a light receiving portion for terahertz waves, the main body 2 is provided with an amplifier circuit for amplifying the electrical signal output from the light receiving portion, various wirings, and connection terminals for external devices.
[0035] In this embodiment, the main body 2 is a component that transmits terahertz waves. Specifically, the main body 2 is a single crystal silicon substrate that has excellent transmittance to terahertz waves. Impurities may also be doped in at least a portion of the silicon substrate. At least a portion of the main surface 2a is made of silicon. The main surface 2a is not limited to being formed only of silicon, and may also include a metal surface that functions as a part of wiring, etc.
[0036] The anti-reflection film 3 is a film that prevents or suppresses reflection of the terahertz wave on the surface of the main body 2. Figure 1 As shown, the antireflection film 3 is composed of a laminate P including a first refractive index layer 4 and a second refractive index layer 5 having different refractive indices with respect to terahertz waves. The laminate P has a paired layer group 7 including a plurality of paired layers 6 composed of the first refractive index layer 4 and the second refractive index layer 5 stacked together.
[0037] The first refractive index layer 4 and the second refractive index layer 5 are, for example, layers formed by making an organic resin contain inorganic particles. The organic resin is, for example, a resin consisting only of a cycloolefin polymer, or a resin with a cycloolefin polymer as the main component. In the present embodiment, the organic resin is a resin with a cycloolefin polymer as the main component, and may contain a high molecular organic compound, a low molecular organic compound, etc. other than the cycloolefin polymer. The organic resin may also contain a crosslinking agent, a polymerization initiator, etc. In addition, the organic resin may also contain an inorganic substance other than the inorganic particles.
[0038] The inorganic particles are particles for adjusting the refractive index of the anti-reflection film 3, and are dispersed in the organic resin. The inorganic particles are composed of, for example, a substance having permeability to terahertz waves. In addition, the inorganic particles are composed of a substance having a higher refractive index to terahertz waves than the organic resin. Therefore, the higher the concentration of the inorganic particles dispersed in the organic resin, the higher the refractive index to terahertz waves, and the lower the concentration of the inorganic particles dispersed in the organic resin, the lower the refractive index to terahertz waves.
[0039] Examples of inorganic particles include silicon particles, titanium oxide particles, and diamond particles. Silicon particles may also be high-resistance silicon particles. For example, high-resistance silicon particles have a particle size of 1×10 3 The average diameter of the inorganic particles is, for example, 5 nm to 3000 nm. The upper limit of the average diameter of the inorganic particles can be 1 μm, 200 nm, or 20 nm. In addition, the lower limit of the average diameter of the inorganic particles can be 200 nm, 20 nm, or 1 nm. The average diameter of the inorganic particles can be measured, for example, by laser diffraction and scattering method, dynamic light scattering method, photon correlation method, etc.
[0040] In the present embodiment, the concentration of inorganic particles dispersed in the organic resin in the first refractive index layer 4 is higher than the concentration of inorganic particles dispersed in the organic resin in the second refractive index layer 5. That is, in the present embodiment, the first refractive index layer 4 is a high refractive index layer having a higher refractive index with respect to the terahertz wave than the second refractive index layer 5, and the second refractive index layer 5 is a low refractive index layer having a lower refractive index with respect to the terahertz wave than the first refractive index layer 4. In addition, the second refractive index layer 5 as a low refractive index layer may not be dispersed with inorganic particles but may be composed only of an organic resin.
[0041] In the paired layer 6 composed of the first refractive index layer 4 and the second refractive index layer 5, the first refractive index layer 4 and the second refractive index layer 5 are stacked at a predetermined thickness ratio. The thickness of the first refractive index layer 4 and the second refractive index layer 5 is smaller than the wavelength of the terahertz wave incident on the optical element 1A. The thickness of the first refractive index layer 4 and the second refractive index layer 5 is, for example, 1 / 10 or less of the wavelength of the terahertz wave, preferably 1 / 100 or less.
[0042] Since the thickness of the first refractive index layer 4 and the second refractive index layer 5 is sufficiently small relative to the wavelength of the terahertz wave, the first refractive index layer 4 and the second refractive index layer 5 are in a state of not having sensitivity relative to the terahertz wave. In this case, the first refractive index layer 4 and the second refractive index layer 5 do not constitute two independent refractive index layers relative to the terahertz wave, and the refractive index of the paired layer 6 composed of the first refractive index layer 4 and the second refractive index layer 5 relative to the terahertz wave (hereinafter referred to as "effective refractive index") can take a value between the refractive index of the first refractive index layer 4 and the refractive index of the second refractive index layer 5 according to the ratio of the thicknesses of these layers.
[0043] In this embodiment, if Figure 1 As shown, the pairing layer 6A, the pairing layer 6B, the pairing layer 6C, the pairing layer 6D, and the pairing layer 6E are stacked in order from the side close to the main body 2. The thickness ratio of the first refractive index layer 4 and the second refractive index layer 5 is 3:1 in the pairing layer 6A, 2:1 in the pairing layer 6B, 1:1 in the pairing layer 6C, 1:2 in the pairing layer 6D, and 1:3 in the pairing layer 6E. That is, in the pairing layer group 7, the closer the pairing layer 6 is to the main body 2, the higher the ratio of the high refractive index layer to the low refractive index layer. With such a structure, in the pairing layer group 7, the closer the pairing layer 6 is to the main body 2, the more the effective refractive index of the pairing layer 6 with respect to the terahertz wave gradually approaches the refractive index of the main body 2 with respect to the terahertz wave.
[0044] The thickness adjustment of the first refractive index layer 4 and the second refractive index layer 5 in each pairing layer 6 can be implemented, for example, by using a spray gun to form the first refractive index layer 4 and the second refractive index layer 5 by coating. When a spray gun is used, for example, the spray gun is moved in one direction within the plane of the main surface 2a in the main body 2 at a specified speed to apply a thin film of resin material. By repeatedly applying the film, the refractive index layer can be formed to any thickness. For example, when the thickness of the film formed by one coating performed by the spray gun is 100nm, a refractive index layer of 15μm thickness can be formed by repeating the coating of the film 150 times. In addition, the thickness adjustment of the refractive index layer can also be controlled by the moving speed of the spray gun. For example, when forming a thick refractive index layer, the speed of the spray gun can be reduced, and when forming a thin refractive index layer, the speed of the spray gun can be increased.
[0045] As described above, in the optical element 1A, the first refractive index layer 4 and the second refractive index layer 5 are both smaller than the wavelength of the terahertz wave. Therefore, the first refractive index layer 4 and the second refractive index layer 5 do not have sensitivity to the terahertz wave, and the effective refractive index of the paired layer 6 composed of the first refractive index layer 4 and the second refractive index layer 5 can take a value between the refractive index of the first refractive index layer 4 and the refractive index of the second refractive index layer 5 corresponding to the ratio of the thickness of these layers. Therefore, in the optical element 1A, by adjusting the ratio of the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 in the paired layer 6, the effective refractive index with respect to the terahertz wave can be easily adjusted to a desired value. In addition, in the optical element 1A, since the desired refractive index is obtained by using only two refractive index layers having different refractive indices, the manufacturing becomes easier than the case where a composite material having multiple concentrations corresponding to each refractive index layer is prepared.
[0046] In addition, the optical element 1A is a mode in which the main body 2 is provided with the supporting laminate P, and the effective refractive index of the pairing layer 6 with respect to the terahertz wave gradually approaches the refractive index of the main body 2 with respect to the terahertz wave as the pairing layer 6 is closer to the main body 2 in the pairing layer group 7. Thus, the pseudo moth-eye structure can be formed in the main body 2. Therefore, the reflection prevention structure with a wide frequency band for the terahertz wave can be formed in the main body 2. Since the structure is formed using only two refractive index layers as described above, the ease of manufacturing can also be maintained.
[0047] In addition, in the optical element 1A, the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 are both 1 / 10 or less, preferably 1 / 100 or less, of the wavelength of the terahertz wave. Thus, the sensitivity of the first refractive index layer 4 and the second refractive index layer 5 to the terahertz wave can be made sufficiently small. Therefore, the effective refractive index of the pairing layer 6 can be made close to the target value with high accuracy.
[0048] The pairing layer 6 is preferably formed using only two refractive index layers, the first refractive index layer 4 and the second refractive index layer 5 , but may include one or more other refractive index layers within a range that allows adjustment of the effective refractive index of the pairing layer 6 with respect to the terahertz wave.
[0049] [Second Embodiment]
[0050] Figure 2 1 is a schematic cross-sectional view showing the layer structure of the optical element according to the second embodiment. In the optical element 1B according to the second embodiment, the layer structure of the laminate constituting the anti-reflection film 3 is different from that of the optical element 1A according to the first embodiment. Specifically, in the optical element 1B, Figure 2As shown, in all the paired layers 6 constituting the paired layer group 7, the ratio of the thickness of the first refractive index layer 4 to the second refractive index layer 5 is 1:1. That is, in the optical element 1B, in the paired layer group 7, the effective refractive indexes of the paired layers 6 with respect to the terahertz wave are equal to each other. The thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 are both 1 / 10 or less, preferably 1 / 100 or less, of the wavelength of the terahertz wave, which is the same as the first embodiment.
[0051] The anti-reflection film 3 is the same as the anti-reflection film 3 of the first embodiment in that it has an anti-reflection function with respect to terahertz waves, but the principle of anti-reflection is different. The anti-reflection film 3 of the first embodiment realizes a wide-band anti-reflection structure by a pseudo-moth-eye structure. On the other hand, the anti-reflection film 3 of the second embodiment realizes a narrow-band anti-reflection structure, which is the same as the so-called single-layer anti-reflection film. The anti-reflection film 3 is established when the effective refractive index of each pairing layer 6 is √n when the refractive index of the main body 2 with respect to the terahertz wave is set to n, and the thickness of the stacking direction of the stack P (pairing layer group 7) is 1 / 4 of the wavelength of the terahertz wave. In this case, because the reflection component reflected by the interface of the stack P and the air and the reflection component reflected by the interface of the stack P and the main body 2 cancel each other, it is possible to accurately (pinpoint) prevent the reflection of the terahertz wave of the wavelength determined by the thickness of the stack P in the stacking direction.
[0052] In such an optical element 1B, the effective refractive index with respect to the terahertz wave can also be easily adjusted to a desired value by adjusting the ratio of the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 in the pairing layer 6. In addition, in the optical element 1B, since the desired refractive index is obtained by using only two refractive index layers having different refractive indices, the manufacturing is also easier than in the case of preparing a composite material having multiple concentrations corresponding to each refractive index layer.
[0053] In the optical element 1B, the effective refractive indexes of the paired layers 6 with respect to terahertz waves in the paired layer group 7 are equal to each other. Thus, the same antireflection structure as a single-layer antireflection film can be formed on the main body 2. Since this structure is formed using only two refractive index layers, it is also possible to maintain ease of manufacture.
[0054] In addition, in the optical element 1B, the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 are both 1 / 10 or less, preferably 1 / 100 or less, of the wavelength of the terahertz wave. Thus, the sensitivity of the first refractive index layer 4 and the second refractive index layer 5 to the terahertz wave can be made sufficiently small. Therefore, the effective refractive index of the pairing layer 6 can be made close to the target value with high precision.
[0055] [Third Embodiment]
[0056] Figure 3 : is a schematic cross-sectional view showing the layer structure of the optical element involved in the third embodiment. Figure 3 In the optical element 1C shown, the stacked body P has a first paired layer group 7A and a second paired layer group 7B. The first paired layer group 7A has a first effective refractive index with respect to the terahertz wave. The second paired layer group 7B has a second effective refractive index with respect to the terahertz wave. Figure 3 In the example of FIG. 7 , the first paired layer group 7A and the second paired layer group 7B are stacked in this order from the side close to the main body 2 .
[0057] In the first paired layer group 7A, the thickness ratio of the first refractive index layer 4 and the second refractive index layer 5 constituting the paired layer 6 is 2:1. In the second paired layer group 7B, the thickness ratio of the first refractive index layer 4 and the second refractive index layer 5 constituting the paired layer 6 is 1:1. Therefore, in the optical element 1C, the high refractive index layer formed by the first paired layer group is located on the side close to the main body 2, and the low refractive index layer formed by the second paired layer group 7B is located on the side away from the main body 2. In this optical element 1C, a wider frequency band antireflection structure can be realized compared with the above-mentioned second embodiment.
[0058] In such an optical element 1C, the effective refractive index with respect to the terahertz wave can also be easily adjusted to a desired value by adjusting the ratio of the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 in the pairing layer 6. In addition, in the optical element 1C, since the desired refractive index is obtained by using only two refractive index layers having different refractive indices, the manufacturing is also easier than in the case of preparing a composite material having multiple concentrations corresponding to each refractive index layer.
[0059] In addition, in the optical element 1C, the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 are both less than 1 / 10 of the wavelength of the terahertz wave, preferably less than 1 / 100. Thus, the sensitivity of the first refractive index layer 4 and the second refractive index layer 5 to the terahertz wave can be made sufficiently small. Therefore, the effective refractive index of the pairing layer 6 can be made close to the target value with high precision.
[0060] In addition, in this embodiment, the laminate P is composed of two paired layer groups having different effective refractive indices, but it is also possible to constitute the laminate P with three or more paired layer groups having different effective refractive indices. In the case where the laminate P is composed of three or more paired layer groups having different effective refractive indices, the paired layer groups may be arranged so that the refractive index of the paired layer groups closer to the main body 2 gradually approaches that of the main body 2.
[0061] [Fourth Embodiment]
[0062] Figure 4 : is a schematic cross-sectional view showing the layer structure of the optical element involved in the fourth embodiment. Figure 4 The optical element 1D shown is different from the third embodiment in that the first paired layer group 7A and the second paired layer group 7B are alternately stacked in the stacked body P. That is, in the optical element 1D, the first paired layer group as the high refractive index layer and the second paired layer group 7B as the low refractive index layer are alternately located in the stacking direction of the stacked body P.
[0063] In such an optical element 1D, the effective refractive index with respect to the terahertz wave can also be easily adjusted to a desired value by adjusting the ratio of the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 in the pairing layer 6. In addition, in the optical element 1D, since the desired refractive index is obtained by using only two refractive index layers having different refractive indices, the manufacturing is also easier than in the case of preparing a composite material having multiple concentrations corresponding to each refractive index layer.
[0064] In the optical element 1D, the first paired layer group 7A having a first effective refractive index with respect to the terahertz wave and the second paired layer group 7B having a second effective refractive index with respect to the terahertz wave are alternately stacked in the stacked body P. Thus, the same structure as a dielectric multilayer film in which high refractive index layers and low refractive index layers are alternately stacked can be formed in the main body 2. Since this structure is formed using only two refractive index layers, it is also possible to maintain ease of manufacture.
[0065] In addition, in the optical element 1D, the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 are both less than 1 / 10 of the wavelength of the terahertz wave, preferably less than 1 / 100. Thus, the sensitivity of the first refractive index layer 4 and the second refractive index layer 5 to the terahertz wave can be made sufficiently small. Therefore, the effective refractive index of the pairing layer 6 can be made close to the target value with high accuracy.
[0066] In this embodiment, the stacked body P is formed by alternately stacking two paired layer groups with different effective refractive indices, but the stacked body P may be formed by repeatedly stacking three or more paired layer groups with different effective refractive indices in the order of increasing effective refractive index.
[0067] [Fifth Embodiment]
[0068] Figure 5 1 is a schematic cross-sectional view showing the layer structure of the optical element according to the fifth embodiment. In the optical element 1E according to the fifth embodiment, in the stacked body P, a plurality of paired layer groups 7 having mutually different effective refractive indexes with respect to terahertz waves are distributed in a direction intersecting with the stacking direction of the paired layers 6. Figure 5In the example of FIG. 1 , the optical element 1E does not include the main body 2, but is composed only of the laminate P. The laminate P is formed into a circular shape as a whole in a plan view. A first paired layer group 7A having a circular shape in a plan view is arranged in the central portion of the laminate P, and a second paired layer group 7B having a ring shape in a plan view is arranged in the outer edge portion of the laminate P so as to surround the first paired layer group 7A.
[0069] In the first paired layer group 7A, the thickness ratio of the first refractive index layer 4 and the second refractive index layer 5 constituting the paired layer 6 is 1:1. In the second paired layer group 7B, the thickness ratio of the first refractive index layer 4 and the second refractive index layer 5 constituting the paired layer 6 is 1:2. Therefore, in the optical element 1E, the circular high refractive index layer formed by the first paired layer group 7A is located in the central part of the laminated body P, and the low refractive index layer formed by the second paired layer group 7B is located in a ring shape around the high refractive index layer.
[0070] In such an optical element 1E, the effective refractive index with respect to the terahertz wave can also be easily adjusted to a desired value by adjusting the ratio of the thickness of the first refractive index layer 4 and the thickness of the second refractive index layer 5 in the pairing layer 6. In addition, in the optical element 1E, since the desired refractive index is obtained by using only two refractive index layers having different refractive indices, the manufacturing is also easier than in the case of preparing a composite material having multiple concentrations corresponding to each refractive index layer.
[0071] In the optical element 1E, in the stacked body P, a plurality of paired layer groups 7 having mutually different effective refractive indexes with respect to the terahertz wave are distributed in a direction intersecting the stacking direction of the paired layer 6. Thus, regions with different effective refractive indexes can be distributed in arbitrary regions in a direction intersecting the stacking direction of the paired layers. In the present embodiment, the effective refractive index of the peripheral portion is lower than that of the central portion of the stacked body P. Therefore, in the present embodiment, for example, a refractive index distribution lens that refracts the terahertz wave in a parabolic shape in the stacked body P can be constructed. Since the refractive index distribution is formed using only two refractive index layers, it is also possible to maintain ease of manufacturing.
[0072] In addition, in this embodiment, three or more paired layer groups with different effective refractive indexes can also be distributed in any area in the direction intersecting the stacking direction of the paired layer 6. In addition, the distribution method is not limited to a circular shape or a ring shape, and other methods such as a rectangular shape, a grid shape, and a radial shape can be adopted. The propagation of terahertz waves in the stacked body can be controlled by the distribution method of the paired layer group. Therefore, in addition to the above-mentioned refractive index distribution lens, it can also be applied to waveguides, optical camouflage materials, super lenses, etc.
[0073] [Modifications]
[0074] In the above embodiment, a single crystal silicon substrate is exemplified as the main body 2, but the material forming the main body 2 is not limited thereto. The main body 2 may also be formed of an optical material such as germanium or diamond. In addition, the main body 2 may also be formed of an optical crystal such as zinc telluride (ZnTe), lithium niobate (LiNbO3), DAST (4-dimethylamino-N-methyl-4-stilbazolium tosylate), etc.
[0075] [Study on the relationship between the wavelength of terahertz waves and the thickness of the refractive index layer]
[0076] The relationship between the wavelength of the terahertz wave and the thickness of the refractive index layer is examined below. Here, the condition that the first refractive index layer and the second refractive index layer have no sensitivity to the terahertz wave is examined. That is, the effective refractive index of the paired layer is a value between the refractive index of the first refractive index layer and the refractive index of the second refractive index layer, and the condition that the paired layer functions as an intermediate refractive index layer between the first refractive index layer and the second refractive index layer is described.
[0077] Figure 6 is a schematic cross-sectional view showing the layer structure of the optical element used for simulation. Figure 6 As shown, in this simulation, the anti-reflection film 103 formed on the silicon substrate, that is, the main body 102 is used as a model. The anti-reflection film 103 is formed by a pairing layer group 107 in which a pairing layer 106 composed of a first refractive index layer 104 and a second refractive index layer 105 is stacked. Three patterns are prepared for the refractive index n1 of the first refractive index layer 104 and the refractive index n2 of the second refractive index layer 105. In pattern 1, n1=1.5 and n2=2.5 are set. In pattern 2, n1=1.8 and n2=2.2 are set. In pattern 3, n1=2.0 and n2=2.0 are set. In pattern 1, the refractive index difference between the first refractive index layer 104 and the second refractive index layer 105 becomes larger than that in pattern 2. In pattern 3, n1 and n2 are equal. This pattern 3 is equivalent to an anti-reflection film formed by a single refractive index layer and is a reference for this simulation.
[0078] The frequency of the terahertz wave is set to a range of 0.1THz to 100THz. If this range is converted into a wavelength, it is 30μm to 3000μm. The variables of the simulation, namely the layer thickness of the first refractive index layer 104 and the second refractive index layer 105, are set to four 100nm, 250nm, 500nm, and 1000nm. In order to make the reflection prevention characteristics consistent, regardless of the layer thickness of the first refractive index layer 104 and the second refractive index layer 105, the thickness of the paired layer group 107 is set to 20μm in any case. Therefore, the number of layers of the paired layer 106 constituting the paired layer group 107 is different from each other according to the layer thickness of the first refractive index layer 104 and the second refractive index layer 105.
[0079] Figure 7 to Figure 10 is a graph showing the simulation results. Figure 7 and Figure 8 In each of the figures, the horizontal axis represents frequency and the vertical axis represents transmittance (amplitude). Fig. 9 and Fig.10 The graph is extracted Figure 7 and Figure 8 The peak points of the vibration of each graph are connected. Figure 7 (A) and Fig. 9 As shown in (A), when the layer thickness is 100nm, both pattern 1 and pattern 2 are the same as pattern 3, and the transmittance vibrates in the range of 0.7 to 1 over the entire frequency range. From this result, it can be seen that the first refractive index layer 104 and the second refractive index layer 105 with a layer thickness of 100nm do not have sensitivity to the terahertz wave with a frequency of 0.1THz to 100THz, and these paired layers 106 function as intermediate refractive index layers. In addition, the layer thickness of 100nm can be said to be a thickness that is sufficiently small relative to the wavelength of the terahertz wave with a frequency of 0.1THz to 100THz.
[0080] like Figure 7 (B)( Fig. 9 (B))、 Figure 8 (A)( Fig.10 (A)) and Figure 8 (B)( Fig.10 As shown in Figure (B), as the layer thickness increases to 250nm, 500nm, and 1000nm, the deviation of the patterns 1 and 2 relative to the pattern 3 becomes larger. When the layer thickness is 500nm and 1000nm, a significant drop in transmittance occurs in the patterns 1 and 2. In addition, regarding the degree of deviation of the graph, the pattern 1 having a large refractive index difference between the first refractive index layer 104 and the second refractive index layer 105 is larger than the pattern 2 having a small refractive index difference between the first refractive index layer 104 and the second refractive index layer 105. From this result, it can be seen that as the layer thickness increases, the first refractive index layer 104 and the second refractive index layer 105 have sensitivity to terahertz waves with a frequency of 0.1THz to 100THz, and the first refractive index layer 104 and the second refractive index layer 105 act as two independent layers and contribute to the reflection of terahertz waves.
[0081] Fig.11 (A) Enlarged display Fig.10 (B) is the area enclosed by the dotted line in the figure. Fig.11 In (A), the dotted line indicates the frequency (=3 THz) of the terahertz wave having a wavelength of 100 μm. Fig.11As shown in (A), when the layer thickness is 1000nm, in the region where the wavelength of the terahertz wave is greater than 100μm (the frequency is 3THz or less), the deviation of the graphs of pattern 1 and pattern 2 relative to the graph of pattern 3 is small. In particular, in pattern 2 where the refractive index difference between the first refractive index layer 104 and the second refractive index layer 105 is small, it is substantially the same value as that of the reference, i.e., pattern 3. It can be seen from this that when the thickness of the first refractive index layer 104 and the thickness of the second refractive index layer 105 are both less than 1 / 100 of the wavelength of the terahertz wave, the sensitivity of the first refractive index layer 104 and the second refractive index layer 105 to the terahertz wave becomes sufficiently small.
[0082] in addition, Fig.11 (B) shows again Fig.10 (A) Figure. Fig.11 In (B), the dotted line indicates the frequency (= 60 THz) of the terahertz wave having a wavelength of 5 μm. Fig.11 As shown in (B), when the layer thickness is 500nm, in the region where the wavelength of the terahertz wave is greater than 5μm (the frequency is below 60THz), there is no significant drop in transmittance, and the deviation of the graphs of pattern 1 and pattern 2 relative to the graph of pattern 3 becomes smaller. It can be seen that when the thickness of the first refractive index layer 104 and the thickness of the second refractive index layer 105 are both less than 1 / 10 of the wavelength of the terahertz wave, the sensitivity of the first refractive index layer and the second refractive index layer to the terahertz wave becomes sufficiently small.
[0083] 1A to 1E ... optical element, 2 ... main body, 4 ... first refractive index layer, 5 ... second refractive index layer, 6 ... paired layer, 7 ... paired layer group, 7A ... first paired layer group, 7B ... second paired layer group, P ... laminated body.
Claims
1. An optical element, wherein: A laminated body including a first refractive index layer and a second refractive index layer having different refractive indices with respect to terahertz waves, The laminated body includes a paired layer group including a plurality of paired layers composed of the first refractive index layer and the second refractive index layer. The thickness of the first refractive index layer and the thickness of the second refractive index layer are both smaller than the wavelength of the terahertz wave. The paired layers have a predetermined effective refractive index with respect to the terahertz wave corresponding to a thickness ratio of the first refractive index layer and the second refractive index layer, respectively. The thickness of the first refractive index layer and the thickness of the second refractive index layer are both less than 1 / 10 of the wavelength of the terahertz wave incident on the optical element. The paired layer group includes a plurality of paired layers in which the ratio of the thickness of the first refractive index layer to the thickness of the second refractive index layer is equal.
2. The optical element according to claim 1, wherein It also has a main body portion supporting the stacked body, In the paired layer group, the closer the paired layer is to the main body, the closer the effective refractive index of the paired layer with respect to the terahertz wave is to the refractive index of the main body with respect to the terahertz wave.
3. An optical element, wherein: A laminated body including a first refractive index layer and a second refractive index layer having different refractive indices with respect to terahertz waves, The laminated body includes a paired layer group including a plurality of paired layers composed of the first refractive index layer and the second refractive index layer. The thickness of the first refractive index layer and the thickness of the second refractive index layer are both smaller than the wavelength of the terahertz wave. The paired layers have a predetermined effective refractive index with respect to the terahertz wave corresponding to a thickness ratio of the first refractive index layer and the second refractive index layer, respectively. The thickness of the first refractive index layer and the thickness of the second refractive index layer are both less than 1 / 10 of the wavelength of the terahertz wave incident on the optical element. It also has a main body portion supporting the stacked body, In the paired layer group, effective refractive indexes of the paired layers with respect to the terahertz wave are equal to each other.
4. The optical element according to claim 1, wherein It also has a main body portion supporting the stacked body, In the stacked body, a first paired layer group having a first effective refractive index with respect to the terahertz wave and a second paired layer group having a second effective refractive index with respect to the terahertz wave are alternately stacked.
5. The optical element according to claim 1, wherein In the stacked body, a plurality of paired layer groups having mutually different effective refractive indexes with respect to the terahertz wave are distributed in a direction intersecting with a stacking direction of the paired layers.
6. The optical element according to any one of claims 1 to 5, wherein The thickness of the first refractive index layer and the thickness of the second refractive index layer are both less than 1 / 100 of the wavelength of the terahertz wave.