Method for producing hydrochlorofluorocarbon, method for producing 1-chloro-2,3,3-trifluoropropene, method for producing 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene

By reacting hydrofluorocarbons with hydrogen chloride in the presence of a catalyst, the problem of selective substitution of HCFC in the prior art is solved, and HCFC manufacturing with high selectivity is achieved, suitable for industrial production, and expanded to 1-chloro-2, Manufacturing of 3,3-trifluoropropylene and 1-chloro-2,3,4,4,5,5-heptafluoro-1-pentene.

CN113710636BActive Publication Date: 2024-11-12AGC INC
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202080030172.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-04-25
Filing Date
2020-04-22
Publication Date
2024-11-12
Estimated Expiration
2040-04-22

AI Technical Summary

Technical Problem

The prior art is difficult to efficiently control the fluorination reaction, and there are difficulties in selectively obtaining hydrochlorofluorocarbons (HCFCs) with specific structures, especially in the absence of a high selectivity method when manufacturing HCFCs from hydrofluorocarbons in industrial use.

Method used

In the presence of a catalyst, the hydrofluorocarbon is reacted with hydrogen chloride, and the selective substitution between fluorine atoms and chlorine atoms is improved to produce HCFCs with a specific structure by adjusting the reaction conditions such as temperature and catalyst composition. The specific method includes using a metal-containing catalyst, such as metal oxides, metal halides, catalysts containing metal elements such as Cr and Al, and controlling the reaction temperature to 100-450°C, the hydrogen chloride molar ratio to 0.5-2.0, and the moisture content to 5,000 mass. Below ppm.

Benefits of technology

A high selectivity production of HCFCs can be achieved, and 1-chloro-2,3,3-trifluoropropylene and 1-chloro-2,3,4,4,5,5-heptafluoro-1-pentene can be produced , improves the efficiency of industrial production and product purity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003313009270000051
    Figure BDA0003313009270000051
  • Figure BDA0003313009270000241
    Figure BDA0003313009270000241
  • Figure BDA0003313009270000281
    Figure BDA0003313009270000281
Patent Text Reader

Abstract

The present invention provides a method for producing HCFC, which can produce HCFC with high selectivity. The method for producing hydrochlorofluorocarbons of the present invention is characterized in that a hydrofluorocarbon represented by formula (1) is reacted with hydrogen chloride in the presence of a catalyst to produce a hydrochlorofluorocarbon represented by formula (2). Formula (1) X-L-Y Formula (2) X-L-ZX represents -CH a F (3‑a) . Y represents ‑CH b F (3‑b) . Z represents ‑CH b Cl c F (3‑b‑c) .
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for producing hydrochlorofluorocarbon, a method for producing 1-chloro-2,3,3-trifluoropropene, and a method for producing 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene. Background Art

[0002] In recent years, hydrochlorofluoroolefins (HCFO) have attracted attention as compounds that have little impact on the global environment and can be used in various applications such as cleaning agents, refrigerants, working fluids, propellants, heat media, foaming agents, solvents, etc. Among HCFOs, 1-chloro-2,3,3,3-tetrafluoropropene (CF3-CF=CClH, HCFO-1224yd) and 1-chloro-2,3,3-trifluoropropene (CF2H-CF=CClH, HCFO-1233yd) are known as compounds with high non-flammability and suitable for the above-mentioned applications, and HCFOs in which a chlorine atom is bonded to the terminal carbon of the carbon-carbon double bond are known.

[0003] In addition, in this specification, the abbreviation of the compound is recorded in the brackets after the compound name for the halogenated hydrocarbon, but the abbreviation may be used instead of the compound name as needed in this specification. In addition, as an abbreviation, only the numerals and lowercase letters after the dash (-) may be used (for example, only "1233yd" is used for "HCFO-1233yd").

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: International Publication No. 1990 / 008754 Summary of the invention

[0007] Technical problem to be solved by the invention

[0008] The present inventors have found that the following specific structure (-CF2-CH b Cl c F (3-b-c) ) can efficiently synthesize HCFO in which a chlorine atom is bonded to the terminal carbon of the carbon-carbon double bond.

[0009] As a method for producing the HCFC having a specific structure, for example, Patent Document 1 describes a method for fluorinating the HCFC by reacting a HCFC having a difluoromethylene group with hydrogen fluoride. However, the production method described in Patent Document 1 is difficult to control the fluorination reaction and has difficulty in selectively obtaining the HCFC having a specific structure, and therefore a method for obtaining the HCFC with a higher selectivity is desired.

[0010] Thus, a more efficient method for producing HCFC is desired. In particular, from an industrial point of view, it is desired to produce HCFC with a high selectivity from hydrofluorocarbons that are relatively easy to synthesize.

[0011] An object of the present invention is to provide a method for producing HCFC which can produce HCFC with a high selectivity.

[0012] Another object of the present invention is to provide a method for producing 1-chloro-2,3,3-trifluoropropene and a method for producing 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene.

[0013] Technical solutions adopted to solve technical problems

[0014] In order to solve the above technical problems, the inventors have conducted in-depth research and found that the above technical problems can be solved by the following technical solutions.

[0015] (1) A method for producing a hydrochlorofluorocarbon, characterized in that a hydrofluorocarbon represented by the formula (1) described below is reacted with hydrogen chloride in the presence of a catalyst to produce a hydrochlorofluorocarbon represented by the formula (2) described below.

[0016] (2) The production method according to (1), wherein the catalyst is a metal-containing catalyst.

[0017] (3) A production method as described in (1) or (2), wherein the catalyst comprises one or more selected from metal oxides, partial halides of metal oxides and metal halides, and the metal oxides, partial halides of metal oxides and metal halides each contain at least one selected from Cr and Al.

[0018] (4) The production method according to (3), wherein the catalyst comprises a partial halide of a metal oxide.

[0019] (5) The production method as described in any one of (1) to (4), wherein L is -CF2-, -CF2CF2-, -CF2-CF2-CF2-, -CF2-CHF-CF2- or -CF2-CH2-CF2-.

[0020] (6) The production method according to any one of (1) to (5), wherein a is 1, b is 2, and c is 1.

[0021] (7) The production method according to any one of (1) to (6), wherein the hydrofluorocarbon represented by the formula (1) and hydrogen chloride are reacted in a gas phase.

[0022] (8) The production method according to any one of (1) to (7), wherein the reaction temperature is 100 to 450°C.

[0023] (9) The production method according to any one of (1) to (8), wherein the molar ratio of hydrogen chloride to the hydrofluorocarbon represented by formula (1) is 0.5 to 2.0.

[0024] (10) The production method according to any one of (1) to (9), wherein a raw material composition containing a hydrofluorocarbon represented by formula (1) is reacted with hydrogen chloride, and the water content of the raw material composition is 5000 mass ppm or less.

[0025] (11) The production method according to (10), wherein the water content is 400 mass ppm or less.

[0026] (12) The production method according to any one of (1) to (11), wherein the hydrofluorocarbon represented by formula (1) is 1,1,2,2,3-pentafluoropropane,

[0027] The hydrochlorofluorocarbon represented by formula (2) is 3-chloro-1,1,2,2-tetrafluoropropane.

[0028] (13) A method for producing 1-chloro-2,3,3-trifluoropropene, characterized in that 3-chloro-1,1,2,2-tetrafluoropropane produced by the method described in (12) is subjected to a dehydrofluorination reaction to produce 1-chloro-2,3,3-trifluoropropene.

[0029] (14) The production method according to any one of (1) to (11), wherein the hydrofluorocarbon represented by formula (1) is 1,1,2,2,3,3,4,4,5-nonafluoropentane,

[0030] The hydrochlorofluorocarbon represented by formula (2) is 5-chloro-1,1,2,2,3,3,4,4-octafluoropentane.

[0031] (15) A method for producing 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene, characterized in that 5-chloro-1,1,2,2,3,3,4,4-octafluoropentane produced by the method described in (14) is subjected to a dehydrofluorination reaction to produce 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene.

[0032] Effects of the Invention

[0033] According to the present invention, it is possible to provide a method for producing HCFC capable of producing HCFC with a high selectivity.

[0034] Furthermore, the present invention can also provide a method for producing 1-chloro-2,3,3-trifluoropropene and a method for producing 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 Shown is a schematic diagram of the reaction apparatus. DETAILED DESCRIPTION

[0036] The method for producing a hydrochlorofluorocarbon of the present invention (hereinafter also simply referred to as "the production method of the present invention") is a method for producing a hydrochlorofluorocarbon represented by formula (2) (hereinafter also referred to as "compound 2") by reacting a hydrofluorocarbon represented by formula (1) described below (hereinafter also referred to as "compound 1") with hydrogen chloride in the presence of a catalyst. That is, the production method of the present invention is a method for producing compound 2 by contacting compound 1 with hydrogen chloride in the presence of a catalyst.

[0037] Hereinafter, first, the components used in the production method of the present invention will be described in detail, and then the steps of the production method will be described in detail.

[0038] As a description of the components, Compound 1 and Compound 2 will be described in detail first.

[0039] Compound 1 is a compound represented by formula (1).

[0040] Formula (1) XLY

[0041] X stands for -CH a F (3-a) .

[0042] a represents 0 or 1.

[0043] Y stands for -CH b F (3-b) .

[0044] b means 1 or 2.

[0045] Here, when a is 0, b represents 1 or 2, and when a is 1, b represents 2.

[0046] That is, examples of compound 1 include CF3-L-CHF2, CF3-L-CH2F, and CHF2-L-CH2F.

[0047] L is -CF2-, -CF2CF2-, or a fluoroalkylene group having 3 to 6 carbon atoms in which at least a part of hydrogen atoms may be substituted with fluorine atoms, wherein the terminal of the fluoroalkylene group having 3 to 6 carbon atoms is -CF2-.

[0048] In addition, the terminals of the above-mentioned fluoroalkylene groups are all -CF2-, which means that -CF2- is located at both terminals of the fluoroalkylene group. For example, the above-mentioned fluoroalkylene group having 3 carbon atoms includes -CF2-CF2-CF2-, -CF2-CH2-CF2-, and -CF2-CFH-CF2-.

[0049] As L, -CF2-, -CF2CF2-, -CF2-CF2-CF2-, -CF2-CHF-CF2- and -CF2-CH2-CF2- are preferred, and -CF2-, -CF2CF2- and -CF2-CF2-- which are perfluoroalkylene groups are more preferred.

[0050] The compound produced using compound 1 as a raw material is a compound represented by formula (2).

[0051] Formula (2) XLZ

[0052] Z stands for -CH b Cl c F (3-b-c) .

[0053] b means 1 or 2.

[0054] c represents 1 or 2.

[0055] When b is 1, c represents 1 or 2, and when b is 2, c represents 1.

[0056] That is, examples of Z include -CHClF, -CHCl2, and -CH2Cl.

[0057] The relationship among a, b, and c is shown in the following Table 1. In Table 1, "X", "Y", and "Z" correspond to "X", "Y", and "Z" in the above formula (1) and formula (2).

[0058] In addition, the columns "X", "Y" and "Z" in Table 1 show the possible values ​​of a, b and c and the structure at that time. For example, "(a=0)CF3" means that when a is 0, X represents CF3.

[0059] [Table 1]

[0060]

[0061] In the production method of the present invention, the fluorine atom bonded to the carbon atom at the terminal of the compound 1 is substituted with a chlorine atom by reacting the compound 1 with hydrogen chloride in the presence of a catalyst. At this time, the fluorine atom substituted on the terminal carbon atom with the smaller number of fluorine atom substitutions at the two terminals can be selectively substituted with a chlorine atom. In the production method of the present invention, if X and Y in formula (1) are compared, the number of fluorine atom substitutions of Y is smaller, and the fluorine atom and the chlorine atom are substituted at the position of Y.

[0062] In addition, the number of substitutions from fluorine atoms to chlorine atoms can be controlled by adjusting the reaction conditions, etc. For example, as shown in Table 1, when Y is CHF2, one fluorine atom is substituted with a chlorine atom to form CHClF, or two fluorine atoms are substituted with chlorine atoms to form CHCl2.

[0063] More specifically, the relationship between a, b, and c is represented by the cases of Forms 1 to 4 in Table 1. For example, in the case of Form 4, the "X" column and the "Y" column indicate that Compound 1 is CHF2-L-CH2F, and the "X" column and the "Z" column indicate that Compound 2 is CHF2-L-CH2Cl.

[0064] That is, in the production method of the present invention, a, b, and c can take the following four forms.

[0065] (Form 1) a is 0, b is 1, and c is 1.

[0066] (Form 2) a is 0, b is 1, and c is 2.

[0067] (Form 3) a is 0, b is 2, and c is 1.

[0068] (Form 4) a is 1, b is 2, and c is 1.

[0069] The production method of the present invention can be particularly advantageously used for a reaction in which only one fluorine atom of compound 1 is replaced with a chlorine atom. For example, when 1,1,2,2,3-pentafluoropropane is used as compound 1, 3-chloro-1,1,2,2-tetrafluoropropane (HCFC-244ca) can be produced as compound 2. In addition, when 1,1,2,2,3,3,4,4,5-nonafluoropentane (HFC-449pccc) is used as compound 1, 5-chloro-1,1,2,2,3,3,4,4-octafluoropentane (HCFC-448occc) can be produced as compound 2.

[0070] In the production method of the present invention, as described above, compound 1 contributes to the reaction. As a raw material, a raw material composition containing compound 1 can be used. Compound 1 may be two or more types.

[0071] The raw material composition may contain impurities in addition to compound 1. As impurities, byproducts other than compound 1 produced when the raw material of compound 1 or compound 1 is produced, water, etc. can be cited. In addition, when the raw material composition contains the above-mentioned impurities, the byproducts produced by the impurities can be removed by known means such as distillation, extractive distillation, azeotropic distillation, membrane separation, two-layer separation, adsorption, etc. As impurities, it is preferably an inert compound under the reaction conditions of the present invention.

[0072] It is preferred to dehydrate the raw material composition before using it for the reaction from the viewpoint of obtaining a better conversion rate of compound 1. That is, it is preferred to use a raw material composition that has been subjected to a dehydration treatment for the reaction.

[0073] The water content (moisture content) of the raw material composition used in the reaction is preferably 5000 mass ppm or less, more preferably 2000 mass ppm or less, further preferably 400 mass ppm or less, particularly preferably 200 mass ppm or less. The lower limit may be 0 mass ppm.

[0074] Herein, ppm means parts per million.

[0075] The water content is measured by a Karl Fischer titrator. As the Karl Fischer titrator, a trace moisture measuring device (Mitsubishi Chemical Analytical Technology Co., Ltd., CA-200 model) is used, and a liquefied gas vaporizer (Mitsubishi Chemical Analytical Technology Co., Ltd., model: VG-200 model) is connected to the sample introduction part to vaporize a preset amount of the dehydrated raw material composition and automatically inject it into the moisture meter.

[0076] The raw material composition used in the reaction contains compound 1 as a main component. The main component means that the content of compound 1 is 50% by mass or more, preferably 60% by mass or more, and more preferably 75% by mass or more relative to the total mass of the raw material composition. As an upper limit, 100% by mass can be cited.

[0077] The method for dehydrating the raw material composition is not particularly limited, and examples thereof include distillation and a method using a dehydrating agent. When a dehydrating agent is used, the dehydrating agent is brought into contact with the raw material composition to reduce the water content in the raw material composition.

[0078] Examples of the dehydrating agent include zeolite, molecular sieves, alumina, calcium chloride, magnesium sulfate, sodium sulfate, calcium sulfate, and potassium carbonate.

[0079] Hydrogen chloride is a gas at room temperature and pressure. Hydrogen chloride can be dissolved in water for use during operation.

[0080] In addition, it is preferred to use dehydrated hydrogen chloride for the reaction.

[0081] As the catalyst in the manufacturing method of the present invention, a metal-containing catalyst is preferred. As specific examples of metal-containing catalysts, metal monomers, metal oxides, partial halides of metal oxides, and metal halides can be cited. The partial halides of the above-mentioned metal oxides are compounds formed by halogenating a portion of the metal oxide (F, Cl, Br, I, etc.). The above-mentioned metal halide is a compound composed of a metal and a halogen. The partial halides of metal oxides and metal halides may contain only one halogen, or may contain two or more halogens.

[0082] As the catalyst, two or more types may be used in combination.

[0083] The partial halide of the metal oxide is preferably a partial fluoride of the metal oxide obtained by fluorinating the metal oxide. In this case, the partial fluoride of the metal oxide may further contain a halogen other than fluorine.

[0084] In addition, as the metal halide, a metal fluoride is preferable. The metal fluoride may contain a halogen other than fluorine.

[0085] From the viewpoint of improving reactivity, the metal element contained in the above-mentioned metal monomer, metal oxide and metal halide is preferably at least one selected from Li, Na, K, Cs, Mg, Ca, Sr, Ba, Al, Cr, Zr, Fe, Ni, Co, Zn, Mn, Sb, Nb and Ta, more preferably at least one selected from Al, Zn, Cr, Mg, Ca, K, Zr and Li, and further preferably at least one selected from Al, Zn, Cr, Mg and Zr.

[0086] Among them, from the viewpoint of being able to produce compound 2 with higher selectivity, the catalyst preferably contains one or more selected from metal oxides, partial halides of metal oxides, or metal halides, and the above-mentioned metal oxides, partial halides of metal oxides, and metal halides each contain at least one metal element selected from Cr and Al (hereinafter also referred to as "metal A"). That is, the catalyst preferably contains one or more selected from metal oxides containing metal A, partial halides of metal oxides containing metal A, and metal halides containing metal A. The above-mentioned metal oxides, partial halides of metal oxides, and metal halides may also contain both Cr and Al.

[0087] Among them, the catalyst more preferably contains a partial halide of a metal oxide having metal A.

[0088] As the catalyst containing metal A, from the viewpoint of increasing the conversion rate of compound 1, a metal oxide containing Cr, a partial halide of a metal oxide containing Cr, or a metal halide containing Cr is preferred.

[0089] When a metal oxide, a partial halide of a metal oxide, or a metal halide containing the metal A is used as the catalyst, the catalyst may contain a metal other than the metal A for various purposes such as improving durability.

[0090] Specific examples of other metals include Na, K, Mg, Ca, Zr, Fe, Zn, Ni, Co, and Mn. Among them, from the viewpoint of improving the physical and chemical durability of the catalyst and being able to more efficiently produce Compound 2, Na, K, Mg, Zn, or Mn is preferred, and Mg or Zn is more preferred.

[0091] In addition, when the catalyst further contains a metal other than the metal A, the conversion rate of the compound 1 is further improved. From the viewpoint of further improving the conversion rate, the other metal is preferably Na, K, Mg, Zn or Mn, and more preferably Mg or Zn.

[0092] When the catalyst contains Cr, the Cr content is preferably 1% by mass or more, more preferably 5% by mass or more, and further preferably 10% by mass or more relative to the total mass of metals contained in the catalyst (100% by mass), from the viewpoint of being able to improve the conversion rate of compound 1. The upper limit is 100% by mass.

[0093] When the catalyst contains Al, the content of Al is preferably 5% by mass or more, more preferably 20% by mass or more, and further preferably 50% by mass or more relative to the total mass of metals contained in the catalyst (100% by mass) from the viewpoint of being able to improve the conversion rate of compound 1. The upper limit is 100% by mass.

[0094] When the catalyst further contains a metal other than metal A, the content of metal A is preferably 90 to 99.9 mass %, more preferably 95 to 99 mass %, relative to the total mass of metals (100 mass %). The content of the metal other than metal A is preferably 0.1 to 10 mass %, more preferably 1 to 5 mass %, relative to the total mass of metals (100 mass %).

[0095] The water content of the catalyst provided for the reaction is preferably low. Specifically, the catalyst is arranged in a reactor, N2 is supplied to the reactor at a rate of 3.94 NmL / min per 1 g of catalyst, and the water content of the gas obtained from the reactor outlet is preferably 100 ppm by volume or less, more preferably 50 ppm by volume or less.

[0096] Specific examples of the catalyst include partially fluorinated chromium zinc composite oxides (partial fluorides of chromium zinc composite oxides), partially fluorinated chromium aluminum magnesium composite oxides (partial fluorides of chromium aluminum magnesium composite oxides), partially fluorinated aluminum oxides (partial fluorides of aluminum oxides), and partially fluorinated chromium oxides (partial fluorides of chromium oxides). Among these, partially fluorinated chromium zinc composite oxides (partial fluorides of chromium zinc composite oxides) and partially fluorinated chromium oxides (partial fluorides of chromium oxides) are preferred from the viewpoint of excellent conversion of compound 1.

[0097] In order to improve the reactivity, the catalyst may be used in the form of particles or supported on a carrier.

[0098] As the carrier, carbon materials such as activated carbon, carbon black, and carbon fiber, and oxide materials such as aluminum oxide, silicon oxide, titanium oxide, zirconium oxide, alkali metal oxides, and alkaline earth metal oxides can be cited, and activated carbon, aluminum oxide, silicon oxide, zirconium oxide, alkali metal oxides, and alkaline earth metal oxides are preferred. Among them, activated carbon, aluminum oxide, and zirconium oxide are more preferred from the perspective of large specific surface area and easy catalyst loading.

[0099] Examples of a method for forming the catalyst into particles include a method of crushing the catalyst into powder and forming the powder using a tablet press or the like.

[0100] As a granular catalyst, for example, a cylindrical one shaped as about 3.0 mm in diameter and about 4.0 mm in height can be used. In addition, as required, the catalyst can be mixed with a binder. The usage amount of the binder is preferably less than 100 mass parts relative to 100 mass parts of the catalyst, more preferably less than 50 mass parts, and further preferably less than 10 mass parts. In this case, the mixture of the catalyst and the binder can be shaped into a granular catalyst by a tabletting machine etc.

[0101] Specific examples of the binder include carbon, cellulose, aluminum oxide, and silicon oxide.

[0102] To improve reactivity, the catalyst is preferably dried in advance in an inert atmosphere (eg, nitrogen flow). From the viewpoint of simplifying the operation and improving the working efficiency, the catalyst can be dried in the same manner as described above while being stored in the reactor.

[0103] Alternatively, the catalyst may be dried before being stored in the reactor.

[0104] The specific surface area of ​​a catalyst depends on the type of each catalyst, and generally, the smaller the specific surface area, the lower the conversion rate, while the larger the specific surface area, the lower the selectivity and the faster the deterioration.

[0105] For example, when the binder is not used, the specific surface area of ​​the metal oxide and the partial halide of the metal oxide is preferably 10 to 400 m 2 / g, the specific surface area of ​​the above metal halide is preferably 3 to 300m 2 / g.

[0106] When the above-mentioned binder is used, the specific surface area of ​​the binder cannot be generalized. For example, when a carbon binder with a high specific surface area is used, the specific surface area of ​​the mixture of the catalyst and the carbon binder is preferably 20 to 1200 m 2 / g or so.

[0107] In addition, in this specification, the specific surface area is a value measured by the BET method.

[0108] In addition, from the viewpoint of improving reactivity (particularly the viewpoint of improving the conversion rate of compound 1), it is preferred that the catalyst is pre-activated. As the method of activation, a method of contacting the catalyst with an activation agent under heating or non-heating can be cited. As the activation agent, a halogen-containing compound can be cited, specifically, hydrogen chloride, hydrogen fluoride, chlorocarbons, fluorocarbons, chlorofluorocarbons, hydrochlorocarbons, hydrofluorocarbons, hydrochlorofluorocarbons, chloroolefins, fluoroolefins, chlorofluoroolefins, hydrofluoroolefins, hydrochloroolefins, and hydrochlorofluoroolefins can be cited. In addition, the compound 1 as a raw material can also be used as a halogen-containing compound.

[0109] By subjecting the metal oxide to the above-mentioned activation treatment, a partial halide of the metal oxide can be generated.

[0110] Catalyst can be activated before being contained in the reactor, but considering that it is easy to operate and has good working efficiency, it is preferably activated under the state contained in the reactor. Therefore, it is preferred that the activation treatment agent is imported into the reactor containing the catalyst to carry out the activation treatment. The activation treatment agent can be directly imported into the reactor at normal temperatures, but from the viewpoint of being able to efficiently carry out the activation treatment, it is preferably carried out temperature regulation by heating etc. when importing the reactor. When importing the activation treatment agent, it can be merged with an inert gas (diluent gas) to be imported. As the specific example of diluent gas, nitrogen, carbon dioxide, helium, argon can be listed.

[0111] In addition, in order to improve the efficiency of the activation treatment, the activation treatment is preferably carried out in a heated state. At this time, the reactor temperature when the activation treatment agent is supplied is preferably 50 to 500° C., more preferably 100 to 400° C., and further preferably 150 to 350° C. The residence time of the activation treatment agent is preferably 1 to 1000 seconds, and more preferably 2 to 500 seconds.

[0112] In addition to the activation treatment before the reaction, the catalyst may be reactivated. In particular, when the activity of the catalyst decreases and the conversion rate of compound 1 decreases, the catalyst may be reactivated. In this way, the activity of the catalyst may be regenerated and the catalyst may be reused.

[0113] The reactivation treatment method is the same as the activation treatment before use, and includes a method of contacting the catalyst with a treatment agent for reactivation treatment (reactivation treatment agent) under heating or without heating. Specific examples of the reactivation treatment agent include oxygen, chlorine, hydrogen fluoride, hydrogen chloride, halogen-containing hydrocarbons, and perhalogenated carbons.

[0114] In the reactivation treatment, an inert gas such as nitrogen, carbon dioxide, a rare gas (helium, etc.), or water vapor may be used to dilute the reactivation agent from the viewpoint of suppressing side reactions and improving catalyst durability.

[0115] When the activity of the catalyst decreases to a level that cannot be reactivated, or when the manufacture of compound 2 is stopped, the operation of extracting the catalyst from the reactor and reloading the catalyst may be performed sometimes. When the catalyst is extracted, in order to remove organic matter or acid components remaining in the reactor or adhering to the catalyst, the reactor is preferably purged with an inert gas in advance. As a specific example of the inert gas used, nitrogen and helium can be cited. Air purging may form harmful substances such as hexavalent chromium in the catalyst, so it is sometimes not preferred.

[0116] From the viewpoint of being able to produce compound 2 with a higher selectivity, in the above reaction (liquid phase reaction, gas phase reaction), the molar ratio of hydrogen chloride used to compound 1 used (molar amount of hydrogen chloride / molar amount of compound 1) is preferably 0.01 to 100, more preferably 0.1 to 10, further preferably 0.3 to 5, and particularly preferably 0.5 to 2. From the viewpoint of suppressing the generation of by-products and improving the volumetric efficiency of the reactor, it is particularly preferably 0.75 to 1.5, and most preferably 0.8 to 1.2.

[0117] Among them, when the molar ratio is 0.75 or more, the conversion rate of compound 1 is more excellent.

[0118] The above reaction is carried out using a reactor.

[0119] The shape and structure of the reactor are not particularly limited. For example, in the case of a gas phase reaction described later, a cylindrical vertical reactor in which a catalyst can be filled can be cited. As a cylindrical vertical reactor, a multi-tubular reactor can be cited.

[0120] Specific examples of the material of the reactor include glass, iron, nickel, stainless steel, and alloys containing iron or nickel as a main component.

[0121] The reactor may be equipped with a heating unit such as an electric heater inside. The reactor may also have a sheath into which a thermometer for measuring the internal temperature is inserted.

[0122] When a multi-tubular reactor is used as the reactor, the pressure loss of each reaction tube is preferably within ±20%, more preferably within ±15%, and further preferably within ±10% relative to the average value of the pressure loss of all reaction tubes. By adjusting the catalyst filling amount of each reaction tube to be constant, the difference in pressure loss of each reaction tube can be reduced.

[0123] In the production method of the present invention, the reaction between Compound 1 and hydrogen chloride may be either a liquid phase reaction or a gas phase reaction.

[0124] The liquid phase reaction means that the compound 1 and hydrogen chloride are reacted while they are both in liquid state.

[0125] The gas phase reaction means that the compound 1 and hydrogen chloride are reacted while they are both in the gaseous state.

[0126] The above reaction can be carried out in batch mode, semi-continuous mode or continuous flow mode.

[0127] The liquid phase reaction is described in detail below.

[0128] Specific steps of the liquid phase reaction include, for example, continuously or discontinuously supplying hydrogen chloride into a reactor containing a mixture of the liquid compound 1 and the catalyst, and continuously or discontinuously extracting the compound 2 produced by the reaction from the reactor.

[0129] From the viewpoint of reaction yield and production efficiency, the reaction temperature of the liquid phase reaction is preferably 20°C or higher, more preferably 30°C or higher, further preferably 50°C or higher, and preferably 250°C or lower, more preferably 200°C or lower, further preferably 150°C or lower.

[0130] From the viewpoint of reaction yield and production efficiency, the reaction time of the liquid phase reaction is preferably 0.1 to 100 hours, more preferably 0.2 to 50 hours, and even more preferably 0.5 to 20 hours. The reaction time refers to the residence time of the raw materials in the reactor.

[0131] If necessary, the liquid phase reaction can also be carried out in the presence of a solvent. Specific examples of solvents include CF3 (CF2) m A linear perfluoroalkyl compound having 5 to 8 carbon atoms represented by CF3 (wherein m is an integer of 3 to 6).

[0132] Next, the gas phase reaction will be described in detail.

[0133] A specific step of the gas phase reaction is to continuously supply the raw material compound 1 heated to a gas state and hydrogen chloride into a reactor so that the catalyst filled in the reactor contacts the gaseous compound 1 and hydrogen chloride to obtain the compound 2.

[0134] In the above reaction, an inert gas (diluent gas) may be supplied to the reactor from the viewpoint of being effective in adjusting the flow rate, suppressing by-products, suppressing catalyst deactivation, etc. Specific examples of the diluent gas include nitrogen, carbon dioxide, helium, and argon.

[0135] From the viewpoint of being able to produce Compound 2 more efficiently, the reaction temperature of the gas phase reaction (temperature in the reactor) is preferably 100 to 450°C, more preferably 120 to 380°C, further preferably 140 to 360°C, particularly preferably 160 to 340°C.

[0136] When the reaction temperature is 100°C or higher (preferably 180°C or higher, more preferably 225°C or higher), the conversion rate of compound 1 increases. When the reaction temperature is 450°C or lower (preferably 360°C or lower), the selectivity of compound 2 increases.

[0137] The temperature in the reactor can be controlled by adjusting the temperature and pressure of the raw materials supplied to the reactor. If necessary, auxiliary heating can be performed on the reactor by an electric heater or a microwave generator.

[0138] The reaction time of the gas phase reaction is preferably 0.1 to 1000 seconds, more preferably 1 to 800 seconds, and further preferably 5 to 600 seconds.

[0139] The above reaction time is equivalent to the residence time of the raw material in the reactor, and can be controlled by adjusting the supply amount (flow rate) of the raw material to the reactor.

[0140] The pressure of the reaction system of the gas phase reaction (pressure in the reactor) is preferably 0 to 2.0 MPa, more preferably 0 to 1.5 MPa. It may also be a negative pressure. From the viewpoint of operability, the pressure in the reactor is more preferably 0 to 1.0 MPa. In this specification, unless otherwise specified, the pressure is expressed as a gauge pressure.

[0141] The content of the by-product in the product is preferably 10% by mass or less, more preferably 5% by mass or less relative to the total mass of the product. The lower limit of the content of the above by-product is usually 0% by mass. Herein, the product refers to the halogenated hydrocarbon generated by the reaction of compound 1 with hydrogen chloride.

[0142] When the product contains impurities, a treatment for separating the compound 2 from the obtained product may be performed. Examples of the separation treatment include known methods such as distillation.

[0143] Next, refer to Figure 1 The gas phase reaction will be described in more detail. Figure 1 The reaction apparatus 20 shown is an example of a reaction apparatus used for a gas phase reaction.

[0144] The reaction device 20 includes a reactor 1. The reactor 1 is connected to a supply line 2 for the compound 1, a supply line 3 for hydrogen chloride, and a supply line 4 for nitrogen gas as a diluent gas.

[0145] The reactor 1 preferably includes a heating unit such as an electric heater.

[0146] The supply line 2 of the compound 1 and the supply line 3 of the hydrogen chloride can be connected to the reactor 1 separately, or they can be connected in front of the reactor 1 and connected to the reactor 1. For example, Figure 1 As shown, the supply line 2 of the compound 1, the supply line 3 of hydrogen chloride and the supply line 4 of nitrogen are connected. Thereby, the mixture of the compound 1, hydrogen chloride and nitrogen is supplied to the reactor 1 via the mixture supply line 5.

[0147] Figure 1 In the reaction device 20 shown, the supply line 2 of the compound 1, the supply line 3 of the hydrogen chloride, and the supply line 4 of the nitrogen are respectively provided with preheaters 2a, 3a, and 4a having an electric heater or the like. The compound 1, hydrogen chloride, and nitrogen supplied to the reactor 1 are preferably preheated to a predetermined temperature by the preheaters 2a, 3a, and 4a, respectively, before being supplied to the reactor 1. Thereby, the temperature of the compound 1, hydrogen chloride, and nitrogen can be efficiently raised to the predetermined reaction temperature inside the reactor 1. The preheaters 2a, 3a, and 4a are not essential, but are preferably provided.

[0148] The outlet of the reactor 1 is connected to an outlet pipe 7 via a cooling unit 6 such as a heat exchanger. The outlet pipe 7 is further connected to a water vapor and acid liquid recovery tank 8, an alkali cleaning device 9, and a dehydration tower 10 in this order.

[0149] The reaction mixture extracted from the reactor 1 is treated to remove acidic substances such as hydrogen chloride and hydrogen fluoride, water vapor, and water through the outlet pipe 7. The gas thus obtained is hereinafter referred to as "outlet gas". Each component in the outlet gas is analyzed and quantified by an analysis device 11 such as a gas chromatograph (GC).

[0150] The outlet gas contains the compound 2. Examples of the compound other than the compound 2 contained in the outlet gas include the compound 1 which is an unreacted raw material, hydrogen chloride, and hydrogen fluoride.

[0151] Components other than Compound 2 contained in the outlet gas can be removed to a desired extent by known means such as distillation.

[0152] In the reaction device 20 , unreacted raw materials can be separated from the reaction mixture or outlet gas discharged from the reactor 1 by distillation or the like, and returned to the reactor as part of the raw materials. Thereby, the productivity of the compound 2 can be improved.

[0153] In the production method of the present invention, when the compound 1 is 1,1,2,2,3-pentafluoropropane (245ca), 3-chloro-1,1,2,2-tetrafluoropropane (244ca) can be obtained as the compound 2.

[0154] The case of using 245ca as a raw material is described in detail below.

[0155] 245ca can be produced by a known method, for example, by the method described in International Publication No. 1994 / 27939.

[0156] When 244ca is produced by a gas phase reaction using 245ca as a raw material, 244ca can be obtained as a component of a crude gas. The crude gas may contain, in addition to 244ca, unreacted 245ca, 2-chloro-1,3,3-trifluoropropene (1233xe), 1-chloro-2,3,3-trifluoropropene (1233yd), 1,2-dichloro-3,3-difluoropropene (1232xd), 1,3-dichloro-2,3-difluoropropene (1232yd), 2,3-dichloro-1,3-difluoropropene (1232xe), 1,2,3-trichloro-3-fluoropropene (1231xd), 2,3,3-trichloro-1-fluoropropene (1231xe), 1,3,3-trichloro-2-fluoropropene (1231yd), 1,2,3,3-tetrachloropropene (1230xd), unreacted hydrogen chloride, hydrogen fluoride, and the like.

[0157] Components other than the above-mentioned 244ca can be removed to a desired extent by known means such as distillation, extractive distillation, azeotropic distillation, membrane separation, two-layer separation, and adsorption.

[0158] In addition, in this specification, when the compound name or compound abbreviation is used without particular distinction, it means at least one selected from the Z form and the E form, and more specifically, it means the Z form or the E form, or a mixture of the Z form and the E form in any ratio. When (E) or (Z) is added after the compound name or compound abbreviation, it means the (E) form or (Z) form of the compound, respectively. For example, 1233yd(Z) means the Z form, and 1233yd(E) means the E form.

[0159] The obtained 244ca can be subjected to a dehydrofluorination reaction to produce 1233yd.

[0160] As the step of the dehydrofluorination reaction, a known method such as International Publication No. 2016 / 136744 can be mentioned.

[0161] The dehydrofluorination reaction of 244ca can be either a liquid phase reaction or a gas phase reaction. In addition, the liquid phase reaction refers to the dehydrofluorination reaction of 244ca in a liquid state or dissolved in a liquid. The gas phase reaction refers to the dehydrofluorination reaction of 244ca in a gaseous state.

[0162] Furthermore, in the production method of the present invention, when the compound 1 is HFC-449pccc, HCFC-448occc can be obtained as the compound 2.

[0163] The following describes in detail the case where 449 pccc is used as the raw material.

[0164] 449pccc can be produced by a known method, for example, by the method described in Russian Journal of Applied Chemistry Vol. 5 No. 7 2002 pp. 1162-1165.

[0165] When 448occc is produced by gas phase reaction using 449pccc as a raw material, 448occc can be obtained as a component of crude gas. In addition to 448occc, crude gas may also contain unreacted 449pccc and C5H2F (7-x) Cl (1+x) (x represents 0 to 7) etc.

[0166] Components other than the above 4480 cC can be removed to a desired extent by known means such as distillation, extractive distillation, azeotropic distillation, membrane separation, two-layer separation, adsorption, etc.

[0167] The obtained 448occc can be subjected to a dehydrofluorination reaction to produce 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene (HCFO-1437dycc), and particularly preferably (Z)-1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene (HCFO-1437dycc(Z)).

[0168] As the dehydrofluorination reaction step, a known method such as Zhurnal Organicheskoi Khimii, (Russia), 1988, Vol. 24, No. 8, pp. 1626-1633 can be cited.

[0169] The dehydrofluorination reaction of the above 448occc can be any one of a liquid phase reaction and a gas phase reaction. In addition, the liquid phase reaction refers to the dehydrofluorination reaction of 448occc in a liquid state or dissolved in a liquid. In addition, the gas phase reaction refers to the dehydrofluorination reaction of 448occc in a gaseous state.

[0170] Example

[0171] Hereinafter, the present invention will be described in detail by way of examples, but the present invention is not limited thereto. Examples 1 to 19 described below correspond to working examples.

[0172] <Conditions of gas chromatography>

[0173] In the production of the following various compounds, the composition of the obtained products was analyzed by gas chromatography (GC). The column used was DB-1301 (60 m long x 250 μm inner diameter x 1 μm thick, manufactured by Agilent Technologies, Inc.).

[0174] <Catalyst preparation>

[0175] The catalyst used in the reaction described below was prepared as follows.

[0176] Use and based on Figure 1 The same reaction apparatus as the reaction apparatus 20 described above was used as the reaction apparatus used in each preparation example. As the reactor 1, a tubular reactor made of SUS304 having an inner diameter of 16.1 mm and a length of 15 cm was used.

[0177] (Catalyst Preparation Example 1)

[0178] The reactor was filled with 38.1 g of chromium-zinc composite oxide (PRICAT62-3M, Johnson Matthey Co., Ltd.), and the temperature in the reactor was raised to 300°C while nitrogen (N2) was passed at 150 Nml / min. The reactor was maintained at atmospheric pressure, and the filled catalyst was dried until the water content in the gas obtained from the reactor outlet reached 5 volume ppm or less. After that, the reactor was heated to 350°C, trifluoromethane (HFC-23) was supplied at a flow rate of 21.9 Nml / min, and N2 was supplied at a flow rate of 43.7 NmL / min for 16 hours, and a partially fluorinated chromium-zinc composite oxide was prepared in the reactor. The obtained catalyst is equivalent to a partial fluoride of a metal oxide.

[0179] In addition, the Cr content in the chromium-zinc composite oxide (PRICAT62-3M) was 97.0% by mass and the Zn content was 2.9% by mass relative to the total mass of the metals contained in the catalyst.

[0180] (Catalyst Preparation Example 2)

[0181] A partially fluorinated chromium-aluminum-magnesium composite oxide was obtained by the same procedure as in (Catalyst Preparation Example 1), except that the chromium-zinc composite oxide (PRICAT62-3M, manufactured by Johnson Matthey Co., Ltd.) was replaced with 33.6 g of chromium-aluminum-magnesium composite oxide (N401AG, manufactured by Nikko Catalysts & Chemicals Co., Ltd.). The obtained catalyst corresponds to a partial fluoride of a metal oxide.

[0182] In addition, the Cr content in the above-mentioned chromium-aluminum-magnesium composite oxide (N401AG) is 20.3 mass % relative to the total mass of metals contained in the catalyst, the Al content is 76.6 mass % relative to the total mass of metals contained in the catalyst, and the Mg content is 3.0 mass % relative to the total mass of metals contained in the catalyst.

[0183] (Catalyst Preparation Example 3)

[0184] The fluorination treatment was carried out in the same manner as in (Catalyst Preparation Example 1) except that the chromium-zinc composite oxide (PRICAT62-3M, manufactured by Johnson Matthey Co., Ltd.) was replaced with 25.5 g of alumina (N612N, manufactured by JGC Catalysts & Chemicals Co., Ltd.) The partially fluorinated alumina was obtained. The obtained catalyst is equivalent to a partial fluoride of a metal oxide.

[0185] (Catalyst Preparation Example 4)

[0186] A partially fluorinated chromium-zinc composite oxide was prepared by following the same procedure as in (Catalyst Preparation Example 1) except that the temperature of the reactor was changed from 350°C to 320°C.

[0187] (Catalyst Preparation Example 5)

[0188] 1100g of Cr(NO3)3·9H2O was dissolved in 2.5 liters of water, and 2000g of 28% by mass aqueous ammonium hydroxide solution was added. While stirring the heated 4L of water, the aqueous solution obtained in the above manner was added to the water to obtain a hydroxide precipitate. After that, the precipitate was filtered, the obtained solid component was washed with pure water, dried, and the obtained product was crushed to obtain an oxide powder. 3% by mass of graphite was mixed with the obtained oxide powder, and it was formed into a cylindrical shape with a diameter of 5mm and a height of 5mm using a tablet forming machine, and calcined at 420°C for 5 hours in nitrogen to produce chromium oxide.

[0189] A partially fluorinated chromium oxide was obtained by the same procedure as in (Catalyst Preparation Example 1) except that the chromium-zinc composite oxide (PRICAT62-3M, manufactured by Johnson Matthey Co., Ltd.) was replaced with 36.6 g of the chromium oxide obtained in the above manner.

[0190] (Catalyst Preparation Example 6)

[0191] The reactor was filled with 38.1 g of chromium-zinc composite oxide (PRICAT62-3M, Johnson Matthey Co., Ltd.), and the temperature in the reactor was raised to 300° C. while nitrogen (N2) was passed at 150 Nml / min. The reactor was maintained at atmospheric pressure, and the filled catalyst was dried until the water content in the gas obtained from the reactor outlet was 5 ppm by volume or less.

[0192] <Example 1>

[0193] N2 was made to flow through the reactor containing the catalyst prepared in Catalyst Preparation Example 1 at a flow rate of 15.6NmL / min, and the reactor temperature was set to 250°C. After the reactor temperature stabilized, 245ca was supplied to the reactor at a flow rate of 0.047g / min and hydrogen chloride was supplied to the reactor at a flow rate of 0.013g / min. The crude gas at the reactor outlet was washed with water and passed through an alkali cleaning unit and a molecular sieve 4A to remove the acid component and obtain a dry product. In addition, the components of the crude gas at the reactor outlet were analyzed by gas chromatography. The analysis results of the crude gas 10 hours after the supply of 245ca and hydrogen chloride were shown in Table 2.

[0194] In addition, as the above-mentioned 245ca, a dehydrated one was used. Specifically, in a sealed container filled with a raw material composition 1 containing 245ca (the content of 245ca in the raw material composition 1: 99.9 mass % or more) (1 kg), 100 g of molecular sieve 4A (manufactured by Junsei Chemical Co., Ltd. (Junsei Chemical Co., Ltd.) as a dehydrating agent was added, and the mixture was allowed to stand for 3 days to be dehydrated, and the dehydrated raw material composition 2 was used as the above-mentioned 245ca.

[0195] The water content of the raw material composition 2 was 20 mass ppm.

[0196] The water content was measured using a Karl Fischer titrator. As the Karl Fischer titrator, a trace moisture measuring device (manufactured by Mitsubishi Chemical Analysis Tech Co., Ltd., CA-200 model) was used, and a liquefied gas vaporizer (manufactured by the same company, model: VG-200 model) was connected to the sample introduction portion to vaporize a preset amount of the raw material composition 2 and automatically inject it into the moisture meter.

[0197] <Example 2>

[0198] As shown in Table 2, the product was obtained by following the same steps as in Example 1 except that the supply amounts of hydrogen chloride and N2 were changed.

[0199] <Example 3>

[0200] As shown in Table 2, the product was obtained by following the same procedure as Example 1 except that the type of catalyst was changed.

[0201] <Example 8>

[0202] As shown in Table 2, the product was obtained by following the same steps as in Example 1 except that the supply amounts of hydrogen chloride and N2 were changed.

[0203] <Example 9>

[0204] As shown in Table 2, the product was obtained by following the same steps as in Example 1 except that the reaction temperature and the supply amounts of 245ca, hydrogen chloride and N2 were changed.

[0205] <Example 10>

[0206] As shown in Table 2, the product was obtained by following the same steps as in Example 1 except that the reaction temperature and the supply amounts of 245ca, hydrogen chloride and N2 were changed.

[0207] <Example 11>

[0208] As shown in Table 2, the product was obtained by following the same steps as in Example 1 except that the supply amounts of 245ca, hydrogen chloride and N2 were changed.

[0209] <Example 12>

[0210] N2 was made to flow through the reactor containing the catalyst prepared in Catalyst Preparation Example 4 at a flow rate of 81.5NmL / min, and the reactor temperature was set to 330°C. After the reactor temperature stabilized, 245ca was supplied to the reactor at a flow rate of 0.244g / min and hydrogen chloride was supplied to the reactor at a flow rate of 0.066g / min. The crude gas at the reactor outlet was washed with water and passed through an alkali cleaning unit and a molecular sieve 4A to remove the acid component and obtain a dry product. In addition, the components of the crude gas at the reactor outlet were analyzed by gas chromatography. The analysis results of the crude gas 10 hours after the start of the supply of 245ca and hydrogen chloride are shown in Table 2.

[0211] In addition, as the above-mentioned 245ca, one subjected to the same dehydration treatment as in Example 1 was used.

[0212] <Example 13>

[0213] As shown in Table 2, the product was obtained by following the same steps as in Example 12 except that the reaction temperature and the supply amounts of 245ca, hydrogen chloride and N2 were changed.

[0214] <Example 14>

[0215] As shown in Table 2, the product was obtained by following the same steps as in Example 12 except that the reaction temperature and the supply amounts of 245ca, hydrogen chloride and N2 were changed.

[0216] <Example 15>

[0217] The product was obtained by following the same steps as in Example 1 except that the catalyst was changed to the catalyst prepared in (Catalyst Preparation Example 5).

[0218] <Example 16>

[0219] N2 was made to flow through the reactor containing the catalyst prepared in Catalyst Preparation Example 6 at a flow rate of 85.7NmL / min, and the reactor temperature was set to 300°C. After the reactor temperature stabilized, 245ca was supplied to the reactor at a flow rate of 0.256g / min and hydrogen chloride was supplied to the reactor at a flow rate of 0.070g / min. The crude gas at the reactor outlet was washed with water and passed through an alkali cleaning unit and a molecular sieve 4A to remove the acid component and obtain a dry product. In addition, the components of the crude gas at the reactor outlet were analyzed by gas chromatography. The analysis results of the crude gas 5 hours after the supply of 245ca and hydrogen chloride were shown in Table 2.

[0220] <Example 17>

[0221] As shown in Table 2, the product was obtained by following the same steps as in Example 16 except for changing the reaction temperature and the supply amounts of 245ca, hydrogen chloride and N2.

[0222] In Table 2, the conversion rate indicates the ratio (unit: %) of the molar amount of 245ca consumed in the reaction to the molar amount of 245ca used in the reaction.

[0223] The 244ca selectivity indicates the ratio (unit: %) of the molar amount of 244ca in the product to the molar amount of 245ca consumed in the reaction.

[0224] The 1233yd(Z) selectivity indicates the ratio (unit: %) of the molar amount of 1233yd(Z) in the product to the molar amount of 245ca consumed in the reaction.

[0225] The other selectivities represent the ratio (unit: %) of the molar amount of components other than the above components in the product to the molar amount of 245ca consumed in the reaction.

[0226] In addition, in Examples 1 to 3, 8 to 10, and 14 to 15, the reaction pressure (pressure in the reactor) was 0 MPaG, and the residence time was 30 seconds. In Examples 11 to 13, and 16 to 17, the reaction pressure (pressure in the reactor) was 0 MPaG, and the residence time was 5 seconds. In addition, in Example 4 described later, the reaction pressure (pressure in the reactor) was 0 MPaG, and the residence time was 30 seconds.

[0227] [Table 2]

[0228]

[0229] As shown in Table 2, according to the production method of the present invention, HCFC can be produced with a high selectivity.

[0230] In addition, when the catalyst obtained in Catalyst Preparation Example 3 was used instead of the catalyst obtained in Catalyst Preparation Example 1, although the specified HCFC (Example 4) could be obtained, the conversion rate was lower than that in Example 3, and the selectivity was only about 70%, which was slightly poor.

[0231] By comparing Examples 1 to 4, it was confirmed that the effect was greater when the catalyst contained Cr.

[0232] By comparing Example 1 with Example 8, it can be confirmed that when the molar ratio of hydrogen chloride to compound 1 is 0.75 or more, the conversion rate is better.

[0233] By comparing Example 1 with Examples 9 to 10, it can be confirmed that the conversion rate is better when the reaction temperature is 180° C. (preferably 225° C.) or higher.

[0234] Comparison of Examples 11 to 14 showed that the selectivity was better when the reaction temperature was 360° C. or lower.

[0235] By comparing Example 12 with Examples 16 to 17, it was confirmed that the conversion rate was better when the activation treatment was performed (in other words, when the partial halide of the metal oxide was used).

[0236] <Example 5>

[0237] N2 is allowed to flow through a reactor containing the catalyst prepared in Catalyst Preparation Example 1 at a flow rate of 15.6NmL / min, and the reactor temperature is set to 250°C. After the reactor temperature stabilizes, 449pccc is supplied to the reactor at a flow rate of 0.082g / min and hydrogen chloride is supplied to the reactor at a flow rate of 0.013g / min. The crude gas at the outlet of the reactor is washed with water and passed through an alkali cleaning section and a molecular sieve 4A to remove the acid component and obtain a dry product. In addition, the components of the crude gas at the outlet of the reactor are analyzed by gas chromatography. The results of analyzing the crude gas 10 hours after the start of the supply of 449pccc and hydrogen chloride showed that the conversion rate of 449pccc was 63.4%, the selectivity of 448occc was 94.8%, and the selectivity of 1437dycc (Z) was 0.1%.

[0238] The above conversion rate indicates the ratio (unit: %) of the molar amount of 449 pccc consumed in the reaction relative to the molar amount of 449 pccc used in the reaction.

[0239] The 448occc selectivity represents the ratio of the molar amount of 448occc in the product to the molar amount of 449pccc consumed in the reaction (unit: %).

[0240] The 1437dycc(Z) selectivity represents the ratio (unit: %) of the molar amount of 1437dycc(Z) in the product to the molar amount of 449pccc consumed in the reaction.

[0241] <Example 6>

[0242] In a 2-liter four-necked flask equipped with a stirrer and a Dimro condenser, 251.31 g of 244ca obtained in Example 1 and 2.51 g of tetra-n-butylammonium chloride (TBAC) were added, and the flask was heated to 50°C. The reaction temperature was maintained at 50°C, and 631.55 g of a 34% by mass potassium hydroxide (KOH) aqueous solution was added dropwise over 5 minutes. After that, stirring was continued for 30 hours, and the organic layer was recovered. After the organic layer recovered in the above manner was washed with water, it was distilled to obtain refined 1233yd containing 1233yd (E) and 1233yd (Z). The selectivity of 1233yd (E) was 8.9%, and the selectivity of 1233yd (Z) was 91.0%.

[0243] <Example 7>

[0244] In a 0.2-liter four-necked flask equipped with a stirrer and a Dimrod condenser, 100.7 g of 448 occc obtained in Example 7 and 1.0 g of tetra-n-butylammonium bromide (TBAB) as a phase transfer catalyst were added, and the flask was cooled to 10°C. The reaction temperature was maintained at 10°C, and 153.9 g of a 34% by mass potassium hydroxide (KOH) aqueous solution was added dropwise over 30 minutes. Thereafter, stirring was continued for 38 hours. The obtained reaction solution was separated into an organic phase and an aqueous phase, and the organic phase was recovered. The recovered organic phase was purified to obtain 78.6 g of an isomeric mixture of 1437dycc (Z) and 1437dycc (E) with a purity of 99.5%. In addition, the mass ratio of 1437dycc (Z) to 1437dycc (E) in the isomeric mixture (1437dycc (Z) / 1437dycc (E)) was 99 / 1.

[0245] <Example 17>

[0246] As shown in Table 3, a product was obtained by following the same procedure as in Example 1 except that the water content of the raw material composition 2 was 198 mass ppm.

[0247] <Example 18>

[0248] As shown in Table 3, a product was obtained by following the same procedure as in Example 1 except that the water content of the raw material composition 2 was 395 mass ppm.

[0249] <Example 19>

[0250] As shown in Table 3, a product was obtained by following the same procedure as in Example 1 except that the water content of the raw material composition 2 was 1995 mass ppm.

[0251] In Table 3, the column “Water content [mass ppm]” shows the water content of the raw material composition 2.

[0252] [Table 3]

[0253]

[0254] As shown in Table 3, it was confirmed that the production method of the present invention is excellent when the water content of the raw material composition 2 is 2000 mass ppm or less (preferably 400 mass ppm or less, more preferably 200 mass ppm or less).

[0255] The entire contents of the specification, claims, abstract, and drawings of Japanese Patent Application No. 2019-084111 filed on April 25, 2019 are cited here as a disclosure of the present invention.

[0256] Explanation of symbols

[0257] 1: Reactor

[0258] 2: Supply line for compound 1

[0259] 2a: Preheater

[0260] 3: Hydrogen chloride supply pipeline

[0261] 3a: Preheater

[0262] 4: Nitrogen supply pipeline

[0263] 4a: Preheater

[0264] 5: Mixture supply pipeline

[0265] 6: Cooling section

[0266] 7: Export pipeline

[0267] 8: Recovery tank for water vapor and acidic liquid

[0268] 9: Alkaline cleaning device

[0269] 10: Dehydration Tower

[0270] 11: Analytical device

[0271] 20: Reaction device

Claims

1. A method for producing hydrochlorofluorocarbons, characterized in that: In the presence of a catalyst, a raw material composition containing the hydrofluorocarbon represented by the formula (1) is reacted with hydrogen chloride to produce a hydrochlorofluorocarbon represented by the formula (2): Formula (1) XLY Formula (2) XLZ X stands for -CH a F (3-a) , Y stands for -CH b F (3-b) , Z stands for -CH b Cl c F (3-b-c) , L is -CF2-, -CF2CF2-, or a fluoroalkylene group having 3 to 6 carbon atoms in which at least a portion of hydrogen atoms may be substituted with fluorine atoms, wherein the terminal of the fluoroalkylene group having 3 to 6 carbon atoms is -CF2-, a represents 0 or 1, b means 1 or 2, c means 1 or 2, When a is 0, b is 1 or 2, and when a is 1, b is 2. In addition, when b is 1, c represents 1 or 2, and when b is 2, c represents 1. The catalyst is a partial fluoride of a metal oxide containing Cr and other metals, or a metal fluoride, wherein the other metal is selected from Na, K, Mg, Zn and Mn, The water content of the raw material composition is 400 mass ppm or less.

2. The manufacturing method according to claim 1, wherein: The L is -CF2-, -CF2CF2-, -CF2-CF2-CF2-, -CF2-CHF-CF2- or -CF2-CH2-CF2-.

3. The manufacturing method according to claim 1, wherein: a is 1, b is 2, and c is 1.

4. The manufacturing method according to claim 1, wherein: The hydrofluorocarbon represented by the formula (1) is reacted with the hydrogen chloride in a gas phase.

5. The manufacturing method according to claim 1, wherein: The reaction temperature is 180-360°C.

6. The manufacturing method according to claim 1, wherein: The molar ratio of the hydrogen chloride to the hydrofluorocarbon represented by the formula (1) is 0.75 to 2.

0.

7. The manufacturing method according to claim 1, wherein: The hydrofluorocarbon represented by the formula (1) is 1,1,2,2,3-pentafluoropropane, The hydrochlorofluorocarbon represented by the formula (2) is 3-chloro-1,1,2,2-tetrafluoropropane.

8. The manufacturing method according to claim 1, wherein: The hydrofluorocarbon represented by the formula (1) is 1,1,2,2,3,3,4,4,5-nonafluoropentane, The hydrochlorofluorocarbon represented by the formula (2) is 5-chloro-1,1,2,2,3,3,4,4-octafluoropentane.

9. A method for producing 1-chloro-2,3,3-trifluoropropene, wherein The following steps are involved: 3-Chloro-1,1,2,2-tetrafluoropropane is prepared according to the method of claim 7; 3-Chloro-1,1,2,2-tetrafluoropropane is subjected to a dehydrofluorination reaction to produce 1-chloro-2,3,3-trifluoropropene.

10. A method for producing 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene, comprising the following steps: 5-Chloro-1,1,2,2,3,3,4,4-octafluoropentane is prepared according to the method of claim 8; 5-Chloro-1,1,2,2,3,3,4,4-octafluoropentane is subjected to dehydrofluorination to produce 1-chloro-2,3,3,4,4,5,5-heptafluoro-1-pentene.

Citation Information

Patent Citations

  • Process for producing a 2,2-difluoropropane

    WO1990008754A2

  • Process for the manfuacture of linear hydrofluorocarbons containing end group hydrogen substituents and azeotropes thereof

    WO1994027939A1

  • Method and apparatus for the treatment of fibrillation

    WO2000044440A1

  • Method for producing 1-chloro-2,3,3-trifluoropropene

    WO2016136744A1

  • Method for producing 1-chloro-2,3,3-trifluoropropene

    CN107848917A