OTP storage unit manufacturing method and OTP storage unit structure

By using BPSG layer overlay and thermal reflux planarization technology in OTP storage units, the problem of difficult lithography process of metal silicide barrier layer is solved, the lithography process is simplified and data protection capability is improved, and floating gate electron loss is avoided , achieving smaller device size and higher data reliability.

CN114050157BActive Publication Date: 2024-11-12SHANGHAI HUAHONG GRACE SEMICON MFG CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202111151603.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-09-29
Publication Date
2024-11-12
Estimated Expiration
2041-09-29

AI Technical Summary

Technical Problem

In the prior art, the metal silicide barrier layer lithography process of OTP memory cells has high requirements and is difficult, resulting in insufficient device data protection capabilities and high process complexity.

Method used

By forming a select gate and a floating gate on the semiconductor substrate, depositing a BPSG layer to cover the OTP region and the metal silicide barrier layer surface, and performing thermal reflux planarization and wet cleaning, reducing the lithography accuracy requirements and simplifying the process flow.

Benefits of technology

It effectively avoids the problem of floating gate electron loss caused by high-density plasma bombardment, reduces the lithography accuracy requirements of the metal silicide barrier layer, simplifies the lithography process, reduces the device size, and ensures the reliability of stored data.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114050157B_ABST
    Figure CN114050157B_ABST
Patent Text Reader

Abstract

The present application relates to the field of semiconductor integrated circuit manufacturing technology, and specifically to a method for manufacturing an OTP memory cell and an OTP memory cell structure. The method for manufacturing an OTP memory cell comprises the following steps: providing a semiconductor substrate, the semiconductor substrate comprising an OTP area and other areas, and a select gate and a floating gate are formed on the semiconductor substrate at the position of the OTP area; manufacturing a metal silicide barrier layer, and using a photolithography process to cover the metal silicide barrier layer on other areas; depositing a BPSG layer, so that the BPSG layer covers the select gate, floating gate and exposed semiconductor substrate surface of the OTP area, as well as the metal silicide barrier layer surface of other areas; using a thermal reflow process to reflow and flatten the BPSG layer; wet cleaning the reflow and flattened BPSG layer; manufacturing a TEOS layer, so that the TEOS layer covers the BPSG layer. The method for manufacturing an OTP memory cell provided in the present application can solve the problem of high requirements and difficulty in the photolithography process of the metal silicide barrier layer in the related art.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of semiconductor integrated circuit manufacturing, and in particular to a method for manufacturing an OTP storage unit and an OTP storage unit structure. Background Art

[0002] Reference Figure 1 , which shows a cross-sectional structural diagram of an OTP (One Time Programable) storage unit in the related art. Figure 1 As can be seen from FIG. 1 , the OTP memory cell 100 includes a select gate structure SG and a floating gate structure FG.

[0003] Related technology Before making the metal interconnection layer of the OTP storage unit, an interlayer dielectric layer is formed on the OTP storage unit so that the interlayer dielectric layer isolates the OTP storage unit from the metal interconnection layer. In order to protect the electrons in the floating gate FG from being lost after programming and improve the data protection capability of the device, the floating gate FG at the position of the OTP storage unit 100 needs to be covered by a metal silicide barrier layer, and there are high requirements for the size of the metal silicide barrier layer covering the floating gate FG. Then, the HDP (High Density Plasma) chemical vapor deposition layer 120 and the TEOS (Tetraethyl Orthosilicate) layer 130 of the interlayer dielectric layer are deposited in sequence.

[0004] Therefore, in the related art, the photolithography process for the metal silicide barrier layer has high requirements and is relatively difficult. Summary of the invention

[0005] The present application provides a method for manufacturing an OTP storage unit and an OTP storage unit structure, which can solve the problem in the related art that the photolithography process of the metal silicide barrier layer has high requirements and is relatively difficult.

[0006] In order to solve the technical problem described in the background technology, the first aspect of the present application provides a method for manufacturing an OTP storage unit, and the method for manufacturing the OTP storage unit comprises the following steps:

[0007] Providing a semiconductor substrate, the semiconductor substrate comprising an OTP area and other areas, and a select gate and a floating gate are formed on the semiconductor substrate at the location of the OTP area;

[0008] Making a metal silicide barrier layer, and making the metal silicide barrier layer cover the other regions through a photolithography process;

[0009] Depositing a BPSG layer so that the BPSG layer covers the select gate, the floating gate and the exposed surface of the semiconductor substrate in the OTP region, and the surface of the metal silicide barrier layer in other regions;

[0010] The BPSG layer is reflowed and planarized by a thermal reflow process;

[0011] Wet cleaning the BPSG layer after reflow and planarization;

[0012] A TEOS layer is formed so that the TEOS layer covers the BPSG layer.

[0013] Optionally, the step of manufacturing the SAB layer so that the SAB layer covers the other regions by a photolithography process includes:

[0014] forming a dielectric layer on the device;

[0015] forming a photosensitive layer on the dielectric layer;

[0016] By using an I-line photolithography machine, the photosensitive layer is defined into an etching pattern, wherein the etching pattern includes a light-transmitting area and a protection area, the OTP area is located in the light-transmitting area, and the other areas are located in the protection area;

[0017] Based on the etching pattern, etching the dielectric layer, so that the etching pattern is transferred into the dielectric layer, and the remaining dielectric layer forms a metal silicide barrier layer covering the other regions;

[0018] The photosensitive layer is removed.

[0019] Optionally, the dielectric layer is made of silicon dioxide.

[0020] Optionally, the step of reflowing and planarizing the BPSG layer by a thermal reflow process includes:

[0021] A thermal reflow process is performed in an environment with a temperature range of 800° C. to 1000° C. for 20 min to 40 min, so that the BPSG layer is reflowed and planarized.

[0022] Optionally, the BPSG layer has a thickness of 1000 Å to 2000 Å.

[0023] Optionally, the TEOS layer has a thickness of 3000 Å to 4000 Å.

[0024] Optionally, after the step of making the metal silicide barrier layer and making the metal silicide barrier layer cover the other regions by photolithography is completed, and before the step of depositing the BPSG layer so that the BPSG layer covers the select gate, the floating gate and the exposed semiconductor substrate surface of the OTP region and the metal silicide barrier layer surface of the other regions is performed, the method further comprises:

[0025] Depositing a silicon nitride layer so that the silicon nitride layer covers the select gate, the floating gate and the exposed surface of the semiconductor substrate in the OTP region, and the surface of the metal silicide barrier layer in other regions;

[0026] The step of depositing the BPSG layer so that the BPSG layer covers the select gate, the floating gate and the exposed surface of the semiconductor substrate in the OTP region, and the surface of the metal silicide barrier layer in other regions comprises:

[0027] A BPSG layer is deposited on the silicon nitride layer.

[0028] In order to solve the technical problem described in the background technology, the second aspect of the present application provides an OTP storage unit structure, and the OTP storage unit is manufactured by the manufacturing method of the OTP storage unit described in the first aspect of the present application.

[0029] The technical solution of the present application includes at least the following advantages: by using a BPSG layer to cover the device, it is possible to avoid high-density plasma bombardment on the floating gate in the OTP area, so that the floating gate in the OTP area is not covered with a metal silicide barrier layer, and there will be no problem of gate oxide damage leading to electron loss after OTP programming. In addition, the lithography accuracy of the metal silicide barrier layer can be reduced while ensuring the reliability of the stored data, thereby simplifying the lithography process and reducing the device size. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0031] Figure 1 A cross-sectional structural diagram of an OTP (One Time Programable) storage unit in the related art is shown;

[0032] Figure 2 A flow chart of a method for manufacturing an OTP storage unit provided in an embodiment of the present application is shown;

[0033] Figure 2a A schematic diagram of a cross-sectional structure of a device after step S21 is completed according to an embodiment of the present application is shown;

[0034] Figure 2b A schematic diagram of a cross-sectional structure of the device after step S22 is completed is shown;

[0035] Figure 2c A schematic diagram of a cross-sectional structure of the device after step S23 is completed is shown;

[0036] Figure 2d FIG. 1 shows a schematic diagram of a cross-sectional structure of the device after step S26 is completed. DETAILED DESCRIPTION

[0037] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0038] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0039] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0040] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.

[0041] Figure 2 A flow chart of a method for manufacturing an OTP storage unit provided in an embodiment of the present application is shown. Figure 2It can be seen that the method for manufacturing the OTP storage unit includes the following steps performed in sequence:

[0042] Step S21: providing a semiconductor substrate, wherein the semiconductor substrate includes an OTP region and other regions, and a select gate and a floating gate are formed on the semiconductor substrate at the location of the OTP region.

[0043] Reference Figure 2a , which shows a schematic diagram of a cross-sectional structure of a device after step S21 is completed according to an embodiment of the present application, Figure 2a As can be seen from the figure, the semiconductor substrate 200 includes an OTP region 210 and other regions 220 . A select gate SG and a floating gate FG are formed on the semiconductor substrate 200 where the OTP region 210 is located.

[0044] Step S22: manufacturing a metal silicide barrier layer, and making the metal silicide barrier layer cover the other regions through a photolithography process.

[0045] Reference Figure 2b , which shows a schematic diagram of the cross-sectional structure of the device after step S22 is completed, from Figure 2b As can be seen in the figure, the semiconductor substrate 200 at other regions 220 except the OTP region 210 is covered with a metal silicide blocking layer (Salicide block, SAB). The metal silicide blocking layer 221 is used to block the formation of metal silicide, thereby improving the resistance and withstand voltage of the device at other regions 220.

[0046] Optionally, the metal silicide barrier layer 221 may be a silicon dioxide layer, which is first formed on the surface of the device, and then a photosensitive layer is formed on the silicon dioxide layer.

[0047] Then, the photosensitive layer is defined as an etching pattern by an I-line photolithography machine, and the etching pattern includes a light-transmitting area and a protection area, the OTP area 210 is located in the light-transmitting area, and the other area 220 is located in the protection area. The step of defining the etching pattern by the I-line photolithography machine can expose the photosensitive layer to an exposure light source with a wavelength of 350nm to 500nm, so that the photosensitive layer defines the etching pattern, and the etching pattern is revealed after development.

[0048] Next, based on the etching pattern, the silicon dioxide layer is etched so that the etching pattern is transferred into the silicon dioxide layer, and the remaining silicon dioxide layer forms a metal silicide barrier layer 221 covering the other region 220 .

[0049] Finally the photosensitive layer is removed.

[0050] However, in the related art, in order to protect the electrons in the floating gate FG from being lost and improve the data protection capability of the device, the floating gate FG at the position of the OTP area 210 needs to be covered by the metal silicide barrier layer 221, and there are high requirements for the size of the metal silicide barrier layer 221 covering the floating gate FG. Therefore, in the related art, the photolithography process of the metal silicide barrier layer 221 is required to be high. Generally, after the silicon dioxide layer is made, the related art also forms a silicon oxynitride layer on the silicon dioxide layer as a hard mask, and then exposes the photosensitive layer through an exposure light source with a wavelength of 240nm to 350nm, so that the photosensitive layer defines the etching pattern, and the etching pattern is revealed after development. Then, based on the etching pattern, the silicon oxynitride layer and the silicon dioxide layer are etched, so that the etching pattern is transferred to the silicon oxynitride layer and the silicon dioxide layer, and the remaining silicon oxynitride layer and the silicon dioxide layer form a metal silicide barrier layer 221 covering the other area 220 and the floating gate FG.

[0051] Finally the photosensitive layer is removed.

[0052] Generally speaking, the shorter the wavelength of the exposure light source, the higher the resolution of the lithography. Since the lithography process of the metal silicide barrier layer 221 in the related art has higher requirements, a shorter wavelength exposure light source can be used for lithography, such as a KRF Scan lithography machine, but the lithography process is more complicated and costly. The present application does not need to set a metal silicide barrier layer 221 in the OTP area, thereby allowing the use of longer wavelength light such as I-line as the exposure light source, thereby simplifying the process and reducing the process cost.

[0053] Step S23: depositing a BPSG (Boro Phospho Silicate Glass) layer so that the BPSG layer covers the select gate, the floating gate and the exposed semiconductor substrate surface of the OTP region, and the metal silicide barrier layer surface of the other regions.

[0054] Reference Figure 2c , which shows a schematic diagram of the cross-sectional structure of the device after step S23 is completed, from Figure 2c It can be seen from the figure that the deposited BPSG layer 230 covers the select gate SG, the floating gate FG and the exposed surface of the semiconductor substrate 200 in the OTP region 210 , and the surface of the metal silicide barrier layer 221 in the other region 220 .

[0055] Optionally, before depositing the BPSG layer, a silicon nitride layer may be deposited so that the silicon nitride layer covers the select gate, floating gate and exposed semiconductor substrate surface of the OTP region, as well as the surface of the metal silicide barrier layer in other regions. The BPSG layer deposited subsequently covers the silicon nitride layer.

[0056] Optionally, the BPSG layer 230 has a thickness of 1000 Å to 2000 Å.

[0057] Step S24: performing a thermal reflow process to reflow and planarize the BPSG layer.

[0058] A thermal reflow process may be performed in an environment with a temperature range of 800° C. to 1000° C. for 20 min to 40 min to reflow and planarize the BPSG layer.

[0059] Step S25: wet cleaning the BPSG layer after reflow and planarization.

[0060] Step S26: forming a TEOS (Tetraethyl Orthosilicate) layer, so that the TEOS layer covers the BPSG layer.

[0061] Reference Figure 2d , which shows a schematic diagram of the cross-sectional structure of the device after step S26 is completed, from Figure 2d As can be seen in FIG. 2 , the formed TEOS layer 240 covers the BPSG layer 230 .

[0062] Optionally, the TEOS layer has a thickness of 3000 Å to 4000 Å.

[0063] In this embodiment, by using a BPSG layer to cover the device, high-density plasma bombardment to the floating gate in the OTP area can be avoided, so that the floating gate in the OTP area is not covered with a metal silicide barrier layer, and there will be no problem of gate oxide damage leading to electron loss after OTP programming. In addition, the lithography accuracy of the metal silicide barrier layer can be reduced while ensuring the reliability of the stored data, thereby simplifying the lithography process and reducing the device size.

[0064] The present application also provides an OTP storage unit structure, wherein the OTP storage unit is composed of Figure 2 as well as Figure 2a to Figure 2d The OTP storage unit is manufactured by the manufacturing method shown in FIG. Figure 2d shown.

[0065] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.

Claims

1. A method for manufacturing an OTP storage unit, characterized in that: The method for making the OTP storage unit comprises the following steps: Providing a semiconductor substrate, the semiconductor substrate comprising an OTP area and other areas, and a select gate and a floating gate are formed on the semiconductor substrate at the location of the OTP area; Making a metal silicide barrier layer, and making the metal silicide barrier layer cover the other regions through a photolithography process; Depositing a BPSG layer so that the BPSG layer covers the select gate, the floating gate and the exposed surface of the semiconductor substrate in the OTP region, and the surface of the metal silicide barrier layer in other regions; The BPSG layer is reflowed and planarized by a thermal reflow process; Wet cleaning the BPSG layer after reflow and planarization; A TEOS layer is formed so that the TEOS layer covers the BPSG layer.

2. The method for making an OTP storage unit as claimed in claim 1, wherein: The step of manufacturing the SAB layer and making the SAB layer cover the other regions by a photolithography process comprises: forming a dielectric layer on the device; forming a photosensitive layer on the dielectric layer; By using an I-line photolithography machine, the photosensitive layer is defined into an etching pattern, wherein the etching pattern includes a light-transmitting area and a protection area, the OTP area is located in the light-transmitting area, and the other areas are located in the protection area; Based on the etching pattern, etching the dielectric layer, so that the etching pattern is transferred into the dielectric layer, and the remaining dielectric layer forms a metal silicide barrier layer covering the other regions; The photosensitive layer is removed.

3. The method for making an OTP storage unit as claimed in claim 2, characterized in that: The material of the dielectric layer is silicon dioxide.

4. The method for making an OTP storage unit as claimed in claim 1, wherein: The step of reflowing and planarizing the BPSG layer by a thermal reflow process comprises: A thermal reflow process is performed in an environment with a temperature range of 800° C. to 1000° C. for 20 min to 40 min, so that the BPSG layer is reflowed and planarized.

5. The method for making an OTP storage unit according to claim 1, wherein: The thickness of the BPSG layer is 1000 Å to 2000 Å.

6. The method for making an OTP storage unit according to claim 1, wherein: The thickness of the TEOS layer is 3000 Å to 4000 Å.

7. The method for making an OTP storage unit according to claim 1, wherein: The method further comprises the following steps after the step of making a metal silicide barrier layer and making the metal silicide barrier layer cover the other regions by a photolithography process and before the step of depositing a BPSG layer so that the BPSG layer covers the select gate, the floating gate and the exposed semiconductor substrate surface of the OTP region and the metal silicide barrier layer surface of the other regions: Depositing a silicon nitride layer so that the silicon nitride layer covers the select gate, the floating gate and the exposed surface of the semiconductor substrate in the OTP region, and the surface of the metal silicide barrier layer in other regions; The step of depositing the BPSG layer so that the BPSG layer covers the select gate, the floating gate and the exposed surface of the semiconductor substrate in the OTP region, and the surface of the metal silicide barrier layer in other regions comprises: A BPSG layer is deposited on the silicon nitride layer.

8. An OTP storage cell structure, characterized in that: The OTP storage unit is manufactured by the manufacturing method of the OTP storage unit according to any one of claims 1 to 7.

Citation Information

Patent Citations

  • OTP device structure and manufacturing method

    CN104538362A

  • OTP memory device and manufacture method thereof and electronic device

    CN110416214A

  • Unit structure of multi-time programmable memory and manufacturing method of unit structure

    CN111430452A

  • Manufacture of semiconductor device

    JP2001007046A