A method for producing a magnetic thin film inductor
By preparing a layered film structure on the substrate substrate of the inductor and filling copper wires in turn, the problems of inductor magnetic circuits are solved, and the performance improvement and volume reduction of the inductor are achieved, and the radio frequency circuit is adapted to miniaturization and integration requirements.
Patent Information
- Application Number
- CN202111183284.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-11
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2041-10-11
AI Technical Summary
Existing inductors face insufficient performance in terms of high frequency, miniaturization and integration, especially the problems of non-closing of magnetic circuits and low inductance values, which are difficult to match with RF circuits and compatible with semiconductor processes.
The magnetic thin film inductor production and manufacturing method adopts a layered film structure. By preparing the lower conductor, the lower oxidation isolation layer, the magnetic film layer, the upper oxidation isolation layer and the upper conductor are successively prepared on the substrate substrate, and connecting the upper conductor through the through holes. With the lower wire, fill the copper wire to increase the inductance value.
Effectively reduce the space volume of the inductor, improve the inductor value and performance, so that the inductor can better match the circuit and be compatible with the semiconductor process.
Smart Images

Figure CN114121466B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of inductor manufacturing, and in particular to a method for producing a magnetic thin film inductor. Background Art
[0002] With the development of science and technology, integrated circuit manufacturing technology has been able to significantly reduce the size of processors, but there are still some core components such as integrated inductors and noise suppressors that face many difficulties in high frequency, miniaturization, integration, etc. Therefore, soft magnetic film materials with high magnetization intensity, high magnetic permeability, high resonance frequency and high resistivity have attracted more and more attention.
[0003] Inductors are important passive devices that realize functions such as filtering, tuning, amplification, and impedance coupling. At present, electronic components such as resistors and capacitors have been integrated, but magnetic devices including inductors have not been fully integrated. With the development of RF circuits towards miniaturization and integration, system-on-chip (SoC) has become the mainstream of RF devices, which requires inductors to continuously optimize their own performance, reduce size, reduce costs, be able to match well with circuits, and most importantly, be compatible with semiconductor processes.
[0004] Thin film inductors are divided into two categories according to the coil structure: planar coil type and three-dimensional solenoid winding type. Planar coil type inductors are spiral coil inductors with a relatively simple structure; however, since the magnetic circuit cannot be closed, the inductance value is low. Three-dimensional solenoid winding inductors are three-dimensional inductors, which are composed of coils and magnetic films wound vertically. Since the magnetic circuit is parallel to the substrate, eddy current losses can be reduced, but there are also problems such as non-closed magnetic circuits and low inductance values.
[0005] With respect to the above-mentioned related technologies, the inventors found that the performance of the related inductors was average. Summary of the invention
[0006] In order to improve the performance of an inductor, the present application provides a method for producing a magnetic thin film inductor.
[0007] The present application provides a method for manufacturing a magnetic thin film inductor using the following technical solution:
[0008] A method for manufacturing a magnetic thin film inductor comprises the following steps:
[0009] S1, selecting substrate raw materials and preparing substrate substrate;
[0010] S2, preparing a lower conductor and a lower oxide isolation layer in sequence from the inside to the outside on the base substrate;
[0011] S3, preparing a magnetic film layer on a side of the lower oxide isolation layer facing away from the base substrate;
[0012] S4, preparing an upper oxide isolation layer and an upper conductive line on the side of the magnetic film layer facing away from the base substrate, which also includes preparing a through hole connecting the upper conductive line with the lower conductive line, and filling the through hole with a copper conductive line.
[0013] By adopting the above technical scheme, step S1 is used to prepare a substrate containing a substrate, step S2 is used to plate a lower conductor on the vertical upper end of the substrate, and then a lower oxide isolation layer is plated on the vertical upper end of the lower conductor, step S3 is used to plate a magnetic film layer on the vertical upper end of the lower oxide isolation layer, step S4 is used to plate an oxide isolation layer on the vertical upper end of the magnetic film layer, and then a through hole is prepared, and an upper conductor is plated on the upper end of the upper oxide isolation layer, and the metal copper filled in the through hole is used to connect the lower conductor with the upper conductor. In the present application, a substrate is first prepared, and a lower conductor, a lower oxide isolation layer, a magnetic film layer, an upper oxide isolation layer and an upper conductor are sequentially prepared on the basis of the substrate from bottom to top. The upper conductor is connected to the lower conductor through a through hole. The magnetic thin film inductor in the present application can reduce the spatial volume of the magnetic thin film inductor by appropriately reducing the thickness of each film structure; and after the copper conductor is filled in the through hole, the upper conductor is connected to the lower conductor. After power is turned on, the current of the upper conductor is in the same direction as that of the lower conductor, and the induced current generated on the upper conductor and the lower conductor is in the same direction, thereby effectively improving the inductance value, and then improving the performance of the magnetic thin film inductor.
[0014] Preferably, the step S1 includes step S11, selecting an N-type silicon wafer as a substrate, boiling it with concentrated sulfuric acid and hydrogen peroxide at 120-130 degrees Celsius for 20-25 minutes; S12, passing oxygen to oxidize the substrate to obtain a substrate substrate.
[0015] By adopting the above technical solution, in step S11, the N-type silicon wafer is first put into concentrated sulfuric acid and hydrogen peroxide and boiled to clean and remove impurities. In step S12, the silicon is oxidized to obtain silicon dioxide as an insulating layer and as a substrate.
[0016] Preferably, in step S12, the method of oxygen-oxidizing the substrate is: introducing dry oxygen, wet oxygen, and dry oxygen into the substrate in sequence.
[0017] By adopting the above technical solution, dry oxygen is used in the front and back to ensure the quality of the oxidation layer, and wet oxygen is used in the middle to increase the oxidation rate, thereby solving the contradiction between the oxidation quality and rate.
[0018] Preferably, the step S2 includes step S21, coating the base substrate with glue and photolithography to form the shape of the lower conductor on the base substrate; S22, electroplating metal titanium and copper, and soaking the metal-plated base substrate in acetone for 5-8 minutes; S23, electroplating copper to prepare copper conductors, and the copper conductors are used as the lower conductors; S24, bonding a lower oxide isolation layer on the lower conductors.
[0019] By adopting the above technical solution, step S21 is used to make a mold of metal titanium and copper, so that the spacing and other dimensions of the lower conductor meet the design standards. Step S22 is used to sputter metal titanium and metal copper to the lower conductor pattern. Metal titanium has the function of increasing the adhesion between metal copper and the substrate, and metal copper is used as a seed during electroplating. Metal copper has a low resistivity, which is convenient for reducing the transmission loss of passive devices, thereby improving the quality factor value of the inductor, and the quality factor value determines the energy storage and conversion efficiency of the inductor. The lower oxide isolation layer is used to isolate the lower conductor. The non-metallic property of the lower oxide isolation layer can isolate the contact between most metal ions, and the resistance to the movement of electrons is increased, thereby achieving isolation of the lower conductor.
[0020] Preferably, in step S22, the thickness of the metal titanium during electrodeposition is smaller than the thickness of the metal copper.
[0021] By adopting the above technical solution, the thickness of metal titanium is smaller than that of metal copper, so that during electroplating, the contact area between the copper seed layer and the electroplating solution is large, which facilitates the copper ions in the electroplating solution to precipitate on the copper seed layer after obtaining electrons.
[0022] Preferably, in the step S2, the lower oxide isolation layer is a silicon dioxide dielectric layer, and in the step S4, the upper oxide isolation layer is also a silicon dioxide dielectric layer, and the thickness of the lower oxide isolation layer is equal to that of the upper oxide isolation layer.
[0023] By adopting the above technical solution, the non-metallic property of silicon dioxide can isolate the contact between most metal ions, thereby isolating the current and allowing the current to be transmitted only along the lower wire or the upper wire. The upper oxide isolation layer and the lower oxide isolation layer separate the upper wire from the lower wire, and the thickness of the upper oxide isolation layer and the lower oxide isolation layer are equal, which is convenient for further suppressing the skin effect of current transmission.
[0024] Preferably, in step S3, the magnetic film layer is FeCo-Si Nanoparticle film.
[0025] By adopting the above technical solution, FeCo-Si The nanoparticle film has a high resistivity, which is convenient for reducing eddy current losses, and also has a high magnetization intensity.
[0026] Preferably, in step S23, before copper electroplating, the base substrate is first soaked in dilute sulfuric acid.
[0027] By adopting the above technical solution, copper is easily oxidized in the air, and the oxide formed by oxidation adheres to the surface of the copper seed layer, so that during the electroplating operation, the copper ions in the electroplating solution are not easy to contact with the copper in the copper seed layer after obtaining electrons, thereby affecting the electroplating operation.
[0028] In summary, the present application includes at least one of the following beneficial technical effects: in the present application, a substrate is first prepared, and a lower conductor, a lower oxide isolation layer, a magnetic film layer, an upper oxide isolation layer and an upper conductor are sequentially prepared from bottom to top on the basis of the substrate. The upper conductor is connected to the lower conductor through a through hole, and a layered film structure is adopted to reduce the size of the inductor; and the upper conductor and the lower conductor are connected by metal copper in the through hole, so that the current direction in the upper conductor and the lower conductor is consistent, so that the direction of the induced current generated by the upper conductor and the lower conductor is consistent, thereby increasing the inductance value and effectively improving the inductor performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a flow chart of a method for producing a magnetic thin film inductor according to an embodiment of the present application.
[0030] Figure 2 It is a detailed step flow chart of an embodiment of the present application.
[0031] Figure 3 is a cross-sectional view of a magnetic thin film inductor in an embodiment of the present application.
[0032] Figure 4 is a top view of the magnetic thin film inductor in an embodiment of the present application.
[0033] Explanation of the reference numerals: 1. substrate; 11. substrate substrate; 2. lower conductor; 3. lower oxide isolation layer; 4. magnetic film layer; 5. upper oxide isolation layer; 6. upper conductor; 7. through hole. DETAILED DESCRIPTION
[0034] The following is combined with Figure 1-4 This application is described in further detail.
[0035] The present application discloses a method for manufacturing a magnetic thin film inductor. Figure 1 and Figure 2 The manufacturing method of the magnetic thin film inductor mainly includes four major steps: step S1, selecting raw materials and preparing a base substrate 11; step S2, preparing a lower conductor 2 and a lower oxide isolation layer 3 at the vertical upper end of the base substrate 11; step S3, preparing a magnetic film layer 4 at the vertical upper end of the oxide isolation layer 3; step S4, preparing an upper oxide isolation layer 5 and an upper conductor 6 at the vertical upper end of the magnetic film layer 4, which also includes photolithography to open a through hole 7 connecting the upper conductor 6 and the lower conductor 2, and filling the through hole 7 with a copper conductor.
[0036] Reference Figure 2 and Figure 3That is, in the manufacturing process of the magnetic thin film inductor, a base substrate 11 is prepared first, and then a lower conductor 2, a lower oxide isolation layer 3, a magnetic film layer 4, an upper oxide isolation layer 5 and an upper conductor 6 are prepared in sequence from bottom to top on the basis of the base substrate 11, and the upper conductor 6 is connected to the lower conductor 2 through a through hole 7. The magnetic thin film inductor in the present application adopts a layered film structure. Compared with the mainstream three-dimensional solenoid wound inductor, the thickness of each film layer can be controlled according to demand, and the minimum thickness of the three-dimensional solenoid wound inductor is the diameter of the solenoid, that is, the thickness of the three-dimensional solenoid wound inductor is fixed. The magnetic thin film inductor in the present application can reduce the spatial volume of the magnetic thin film inductor by appropriately reducing the thickness of each film structure; and after the copper wire is filled in the through hole 7, the upper wire 6 is connected to the lower wire 2. After power is turned on, the current in the upper wire 6 and the lower wire 2 are in the same direction, and the induced current generated on the upper wire 6 and the lower wire 2 are in the same direction, thereby effectively improving the inductance value, and then improving the performance of the magnetic thin film inductor.
[0037] Reference Figure 2 and Figure 3 Step S1, selecting raw materials and preparing the substrate 11, is divided into two small steps: Step S11, select N-type silicon wafer as substrate 1, boil it with concentrated sulfuric acid and hydrogen peroxide at 125 degrees Celsius for 22 minutes. Piranha solution is prepared by mixing concentrated sulfuric acid and hydrogen peroxide, and the N-type silicon wafer is put into the piranha solution and boiled for a period of time to facilitate the removal of impurities on the N-type silicon wafer. Step S12, dry oxygen is passed in sequence for 25 minutes, wet oxygen for 50 minutes, and dry oxygen for 25 minutes, thereby oxidizing.
[0038] Both dry oxygen and wet oxygen are used to oxidize the N-type silicon wafer. Since the oxidation rate of dry oxygen is slow but the quality of the oxide layer is good, and the oxidation rate of wet oxygen is fast but the quality of the oxide layer is poor, the steps of dry oxygen-wet oxygen-dry oxygen are used to solve the contradiction between the oxidation quality and rate. Dry oxygen is used before and after to ensure the quality of the oxide layer, and wet oxygen is used in the middle to increase the oxidation rate. Thus, the surface layer of the N-type silicon is oxidized to obtain a silicon dioxide layer, and the silicon dioxide layer is used as the base substrate 11.
[0039] Reference Figure 2 and Figure 3 Step S2 of preparing the lower conductor 2 and the lower oxide isolation layer 3 is divided into two small steps: Step S21, coating and photolithography are performed to form the pattern of the lower conductor 2. In the embodiment of the present application, the photoresist used is AZ5214, and the process of coating and photolithography to form the pattern of the lower conductor 2 is as follows:
[0040] (1) Cleaning the substrate 11 with acetone and alcohol, and then drying it with nitrogen gas;
[0041] (2) Spin AZ5214 photoresist onto the substrate 11 at a speed of 3000 r / min for 30 seconds to ensure uniformity of the film;
[0042] (3) Baking the base substrate 11 on a hot plate at 100 degrees Celsius for 1 minute to fully volatilize the organic solvent in the photoresist. After baking, the base substrate 11 is exposed for the first time using a UV exposure machine. The photoresist AZ5214 exposed by the UV exposure machine deteriorates, and the area covered by the deteriorated part is the shape of the lower conductor 2.
[0043] (4) placing the first exposed substrate 11 on a hot plate for flip baking at a temperature of 120 degrees Celsius for 100 seconds;
[0044] (5) Flipping the substrate 11 for exposure, with an exposure time of 45 seconds;
[0045] (6) Use positive photoresist to develop for 40 seconds to dissolve the deteriorated part of the photoresist AZ5214, and expose the pattern used for plating the lower layer conductor 2 in process (3) on the base substrate 11.
[0046] Reference Figure 2 and Figure 3 In step S22, metal titanium and metal copper are electro-deposited on the substrate 11, and the substrate 1 plated with metal titanium and metal copper is placed in acetone. After soaking for five minutes, the undegraded part of the AZ5214 photoresist is separated, and a titanium bonding layer and a copper seed layer are obtained on the substrate 11 from the inside to the outside.
[0047] Reference Figure 2 and Figure 3 , step S23, electroplating copper, new copper forms copper wire on the copper seed layer, and the copper wire serves as the lower wire 2. In the embodiment of the present application, because metal copper has low resistivity, it is convenient to reduce the transmission loss of passive devices, thereby improving the quality factor value of the inductor (the quality factor value determines the energy storage and conversion efficiency of the inductor), and metal copper is affordable and cost-effective, so metal copper is selected as the wire material. The above process of manufacturing the lower wire 2 is as follows:
[0048] (1) Using an electroplating method, titanium and copper are plated on a substrate 11 from the inside to the outside in sequence, wherein the thickness of the titanium is less than that of the copper. The titanium plating is to increase the adhesion between the copper and the substrate 11, and the copper layer is used as a seed layer for electroplating, thereby obtaining a titanium bonding layer and a copper seed layer on the substrate 11.
[0049] (2) Use thick glue AZ4620 to form a plating mold with a thickness of about 5 microns. Thick glue AZ4620 has high stability in the plating solution and is not easy to decompose or undergo chemical changes in the plating solution, thereby reducing the pollution to the plating solution.
[0050] (3) Since copper is easily oxidized in the air, before copper electroplating, the substrate 11 is first soaked in dilute sulfuric acid for fifteen minutes to remove the oxide, and then electroplating is performed. The main components of the plating solution are copper sulfate and sulfuric acid. Copper sulfate provides copper ions for electroplating, and the role of sulfuric acid is to prevent the hydrolysis of copper salts and to facilitate the improvement of the conductivity of the plating solution. The electroplating temperature is 24 degrees Celsius, the current density is 18 milliamperes per square centimeter, and the time is 12 minutes. Finally, a copper wire with a thickness of 2 microns is obtained, which is the lower layer wire 2.
[0051] Reference Figure 2 and Figure 3 After the electroplating is completed, the seed layer needs to be etched away. In the embodiment of the present application, the copper seed layer is etched with a mixture of sulfuric acid and hydrogen peroxide. The hydrogen peroxide first oxidizes the copper, and then the sulfuric acid dissolves the copper oxide. Since the copper wire is exposed to the corrosive solution at the same time, the line is plated thicker during electroplating. For the titanium seed layer, a hydrofluoric acid solution is used, and the etching time is controlled at the same time to prevent the hydrofluoric acid from corroding the silicon dioxide under the lower conductor 2.
[0052] Reference Figure 2 and Figure 3 , step S24, bonding a lower oxide isolation layer 3 on the copper wire. Specifically, a silicon dioxide dielectric layer with a thickness of 500 nanometers is disposed on the copper wire, and the silicon dioxide dielectric layer is the lower oxide isolation layer 3.
[0053] Reference Figure 2 and Figure 3 Step S3, preparing the magnetic film layer 4. In the embodiment of the present application, the magnetic film layer is prepared by magnetron sputtering, that is, a 99% pure Alloy as target material, in high purity A certain number of silicon dioxide flakes are placed on the surface of the alloy, and the silicon dioxide flakes are symmetrically placed at the etching track position of the target material, and sputtering is performed in a pure argon environment. Argon is a gas element composed of single atomic molecules, and argon is the most abundant rare gas in the air, which is suitable for ionization.
[0054] In the magnetron sputtering instrument, due to the effect of the electric field, the electrons collide with argon atoms in the process of heading to substrate 1, and the argon atoms are ionized to produce argon positive ions. The argon positive ions are accelerated in the electric field of the magnetron sputtering instrument, and the argon positive ions change direction in the magnetic field of the magnetron sputtering instrument. After acceleration and deflection, the argon positive ions finally collide with the silicon dioxide flakes on the target material. The argon positive ions transfer part of the momentum to the silicon dioxide molecules, and the silicon dioxide molecules collide with other silicon dioxide molecules, forming a cascade process. After sputtering, the silicon dioxide molecules enter alloy, thereby obtaining a magnetic film layer 4 with a thickness of 500 nanometers.
[0055] Step S4 is divided into step S41, bonding a 500 nanometer thick silicon dioxide dielectric layer on the magnetic film layer 4, where the silicon dioxide dielectric layer is the upper oxide isolation layer 5, and the preparation process is the same as step S24; step S42, photolithography through hole 7, two through holes 7 are opened, and the two through holes 7 are diagonally distributed on the substrate 1, and the lower end of the through hole 7 is connected to the lower conductor 2, and the through hole 7 is plated with metal copper; step S43, electroplating metal titanium and metal copper on the upper oxide isolation layer 5, metal titanium as the titanium adhesion layer for electroplating the upper conductor 6, and metal copper as the copper seed layer for the upper conductor 6; electroplating the upper conductor 6 on the copper seed layer to obtain a copper conductor with a thickness of 2 microns, where the copper conductor is the upper conductor 6, and the preparation process is the same as step S22 and step S23. The magnetic thin film inductor finally obtained is as follows Figure 4 shown.
[0056] The working principle of a method for producing a magnetic thin film inductor in an embodiment of the present application is as follows: the magnetic thin film inductor is connected to the circuit, that is, one end of the lower wire 2 is coupled to the positive electrode, and the other end of the lower wire 2 is coupled to the negative electrode. The current enters the magnetic thin film inductor along the positive input end of the lower wire 2, and then the current is split, with part of the current being transmitted along the lower wire 2; the other part of the current is transmitted along the upper wire 6 through the copper wire in the through hole. After this part of the current reaches the end of the upper wire 6, this part of the current continues to converge to the lower wire 2 along the copper wire in another through hole, and then is connected to the circuit from the negative output end of the lower wire 2.
[0057] When the current is transmitted between the upper conductor 6 and the lower conductor 2, the current transmission directions of the two parts are from one end of the substrate 11 to the other end of the substrate 11. The directions of the two parts of the current are consistent. The direction of the electromotive force in the law of electromagnetic induction can be determined by Lenz's law or the right-hand rule, that is, the direction of the induced current generated by the electromagnetic induction phenomenon in the upper conductor 6 and the lower conductor 2 is consistent, thereby improving the inductance performance.
[0058] The above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit the protection scope of the present application. Obviously, the described embodiments are only some embodiments of the present application, rather than all embodiments. Although the present application is described in detail with reference to the above embodiments, ordinary technicians in this field can still combine, add, delete or make other adjustments to the features in the embodiments of the present application according to the circumstances without conflict and without making creative efforts, so as to obtain different other technical solutions that do not deviate from the concept of the present application in essence, and these technical solutions also belong to the scope to be protected by the present application.
Claims
1. A method for producing a magnetic thin film inductor, characterized in that: The following steps are involved: S1, selecting a substrate (1) raw material and preparing a substrate (11): S11, select an N-type silicon wafer as a substrate (1), and boil it with concentrated sulfuric acid and hydrogen peroxide at 120-130 degrees Celsius for 20-25 minutes; S12, oxygen is passed through the substrate (1), and dry oxygen, wet oxygen, and dry oxygen are passed through the substrate (1) in sequence to obtain a silicon dioxide layer on the surface of the N-type silicon through oxidation, and the silicon dioxide layer is used as a substrate (11); S2, preparing a lower conductor (2) and a lower oxide isolation layer (3) in sequence from the inside to the outside on a base substrate (11); S21, using acetone and alcohol to clean the substrate (11), and then drying it with nitrogen; applying AZ5214 photoresist to the substrate (11) by rotation at a speed of 3000 r / min for 30 seconds to ensure the uniformity of the film; placing the substrate (11) on a hot plate at 100 degrees Celsius for 1 minute to fully volatilize the organic solvent in the photoresist, and after the baking is completed, using a UV exposure machine to perform a first exposure on the substrate (11); The photoresist AZ5214 exposed by the UV exposure machine is deteriorated, and the area covered by the deteriorated part is the shape of the lower conductor (2); the base substrate (11) exposed for the first time is placed on a hot plate for flip baking, the baking temperature is 120 degrees Celsius, and the time is 100 seconds; the base substrate (11) is flipped for exposure, and the exposure time is 45 seconds; positive photoresist is used for 40 seconds to develop, and the deteriorated part of the photoresist AZ5214 is dissolved, and the pattern for plating the lower conductor (2) is exposed on the base substrate (11); S22, using an electroplating method to electroplating metal titanium and metal copper on the base substrate (11) obtained in step S21, soaking the base substrate (11) plated with metal titanium and metal copper in acetone for 5-8 minutes, and then separating the undegraded part of the AZ5214 photoresist, wherein the titanium plating is to increase the adhesion between the copper and the base substrate (11), and the copper layer is used as a seed layer for electroplating, thereby obtaining a titanium bonding layer and a copper seed layer on the base substrate (11) from the inside to the outside in sequence; during the electroplating, the thickness of the metal titanium is less than the thickness of the metal copper; S23, soaking the base substrate (11) obtained in step S21 in dilute sulfuric acid for fifteen minutes to remove oxides, and then electroplating copper, new copper forms copper wires on the copper seed layer, and the copper wires serve as the lower layer wires (2); the main components of the plating solution are copper sulfate and sulfuric acid; the electroplating temperature is 24 degrees Celsius, the current density is 18 milliamperes per square centimeter, and the time is 12 minutes, and finally a copper wire with a thickness of 2 microns is obtained, and the copper wire is the lower layer wire (2); after the electroplating is completed, the copper seed layer is etched away, and the etching of the copper seed layer is selected from a mixed solution of sulfuric acid and hydrogen peroxide, the hydrogen peroxide first oxidizes the copper, and then the sulfuric acid dissolves the copper oxide; S24, bonding a lower oxide isolation layer (3) onto the lower conductor (2); S3, forming a magnetic film layer (4) on the side of the lower oxide isolation layer (3) facing away from the base substrate (11); S4, preparing an upper oxide isolation layer (5) and an upper conductor (6) on the side of the magnetic film layer (4) facing away from the base substrate (11), which also includes preparing a through hole (7) connecting the upper conductor (6) and the lower conductor (2), and filling the through hole (7) with a copper conductor.
2. The method for manufacturing a magnetic thin film inductor according to claim 1, characterized in that: In step S2, the lower oxide isolation layer (3) is a silicon dioxide dielectric layer; In step S4, the upper oxide isolation layer (5) is a silicon dioxide dielectric layer, and the thickness of the lower oxide isolation layer (3) is equal to that of the upper oxide isolation layer (5).
3. The method for manufacturing a magnetic thin film inductor according to claim 1, characterized in that: In step S3, the magnetic film layer (4) is a FeCo-SiO2 nanoparticle film layer.