A mold and method for evaluating dimensional deviation of investment castings

By designing molds and measurement methods for investment casting, combined with blue light scanning and three-dimensional detection technology, the problem of difficulty in measuring the internal and external fillet dimensions and contour clarity of investment castings is solved, achieving accurate deviation assessment and improving measurement accuracy. .

CN114199176BActive Publication Date: 2024-10-29CHINA HANGFA SOUTH IND CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202111528805.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-14
Publication Date
2024-10-29
Estimated Expiration
2041-12-14

AI Technical Summary

Technical Problem

Investment casting castings are prone to dimensional deviations during the wax pattern preparation, shell preparation and alloy shrinkage processes. In particular, the internal and external fillet dimensions and contour clarity are difficult to measure and evaluate, which affects the assembly effect and aerodynamics of aerospace engines and automotive parts. Study design.

Method used

A mold is designed, including a lower mold, a forming boss, a template and an upper mold. The wax material is transported through the injection tube to form multiple internal and external fillet wax model cavities of different sizes. Combined with blue light scanning and three-dimensional detection software, the points are collected. The cloud data is fitted to the CAD model, the fillet radius size deviation rate is measured, and the contour definition deviation is evaluated.

Benefits of technology

It achieves accurate measurement and evaluation of the internal and external fillet dimensions of investment castings, improves the accuracy of contour definition deviation, solves the error problem in traditional measurement methods, and enhances the versatility and stability of the mold.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114199176B_ABST
    Figure CN114199176B_ABST
Patent Text Reader

Abstract

The invention discloses a mold for evaluating the dimensional deviation of an investment casting, wherein an upper mold and a forming boss are used to enclose a casting cavity; a wax material identical to the investment casting to be evaluated is selected to manufacture a wax mold for a rounded corner part; since the inner wall of the upper mold is provided with a plurality of inner fillets of different sizes, the outer wall of the forming boss is provided with a plurality of outer fillets of different sizes, so as to form a plurality of inner and outer fillets of different sizes on the wax mold for the rounded corner part; the forming boss, a template removal plate and the upper mold are supported by the lower mold; the wax mold for the rounded corner part is taken out by the template removal plate; in this scheme, the upper mold, the forming boss and the injection tube cooperate with each other to obtain a wax mold for the rounded corner part with multiple inner and outer fillet sizes but convenient for measurement, so as to evaluate the inner and outer fillets of the investment casting with the same fillet size but difficult to measure, the lower mold is used to ensure the stability and smoothness of the preparation process of the wax mold for the rounded corner part, the template removal plate is used to ensure the smooth removal of the wax mold for the rounded corner part, so as to ensure the dimensional accuracy of the wax mold for the rounded corner part.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of investment casting, in particular, to a mold for evaluating the dimensional deviation of investment castings. In addition, the present invention also relates to a method for evaluating the dimensional deviation of investment castings using the mold for evaluating the dimensional deviation of investment castings. Background Art

[0002] Investment casting is a net-shape process with the advantages of high molding accuracy, smooth surface, and less machining. However, the manufacturing cycle of investment casting is long and the process flow is relatively complicated, which easily leads to the accumulation and transmission of dimensional deviations, resulting in the final casting size failing to meet the dimensional accuracy requirements. This is mainly related to the three major process flows of investment casting: 1. Wax pattern preparation. During the preparation of the wax pattern, the composition and properties of the wax material, wax injection process parameters, and wax injection runner design will affect the dimensional deviation of the wax pattern; 2. Shell preparation. During the preparation of the shell, it will be subject to different thermal gradients in all directions, resulting in thermal expansion; 3. Alloy shrinkage. The process of alloy solidification and shrinkage during the pouring stage is the main reason for the out-of-tolerance casting size.

[0003] The contour clarity of a casting refers to comparing the dimensions of the manufactured casting with the dimensions of the original CAD model to obtain the deviation of the dimensions of each part relative to the original model. Since complex castings often have different fillet sizes and the contours of most castings are composed of a variety of internal and external fillets, it is difficult to measure the internal fillet dimensions of castings using traditional measurement methods and the measurement error is large, making these fillet dimensions difficult to measure and evaluate in the three major process flows of investment casting. However, in aircraft engines and automotive parts, the fillet dimensions of key parts will directly affect the overall assembly effect and aerodynamic design requirements. Summary of the invention

[0004] The invention provides a mold and a method for evaluating the dimensional deviation of an investment casting, so as to solve the technical problem that the existing investment casting dimensional transfer deviation of the inner and outer fillet and the contour clarity deviation are difficult to evaluate.

[0005] According to one aspect of the present invention, there is provided a mold for evaluating the dimensional deviation of an investment casting, and for evaluating the deviation in the dimensional transfer and contour clarity of the inner and outer fillets of the investment casting, comprising a lower mold, a molding boss connected to the lower mold, a removal mold plate sleeved on the molding boss and fitted with the upper end surface of the lower mold, and an upper mold covered on the molding boss and fitted with the upper end surface of the removal mold plate, the inner wall of the upper mold being provided with a plurality of inner fillets of different sizes, the outer wall of the molding boss being provided with a plurality of outer fillets of different sizes, the inner wall of the upper mold and the outer wall of the molding boss being enclosed to form a casting cavity for injection molding a wax mold of a filleted part having a plurality of inner fillets and outer fillets of different sizes, the mold also comprising an injection pipe connected to the casting cavity for conveying wax into the casting cavity.

[0006] Furthermore, the forming boss includes a plurality of cylinders of different diameters connected in sequence, the connection between two adjacent cylinders is set as an outer fillet, and the edge corner of the end face of the cylinder is set as an outer fillet; and / or the inner cavity of the upper mold includes a plurality of cylindrical grooves of different diameters connected in sequence, the connection between two adjacent cylindrical grooves is set as an inner fillet, and the edge corner of the bottom of the cylindrical groove is set as an inner fillet.

[0007] Furthermore, the lower end surface of the upper mold is vertically recessed with a plurality of connecting holes, and the mold also includes a supporting member fixedly connected to the connecting hole for supporting the upper mold, and the mold plate is provided with a relief groove for accommodating the supporting member and arranged corresponding to the supporting member, and the connecting holes, the supporting member and the relief groove are arranged one by one.

[0008] Furthermore, the mold also includes a moving part connected to the side wall of the lower mold and used for applying force when the lower mold or the mold moves.

[0009] Furthermore, the upper end surface of the lower mold is vertically recessed with an installation groove for installing the forming boss, the bottom of the installation groove is vertically opened with a first fixing hole, the lower end surface of the forming boss is vertically recessed with a second fixing hole arranged corresponding to the first fixing hole, and the mold also includes a fixing part that passes through the first fixing hole and is fixedly connected to the second fixing hole.

[0010] Furthermore, a first mold removal groove for removing the upper mold is vertically recessed on the edge of the upper end surface of the mold removal plate.

[0011] Furthermore, a second mold removal groove for removing the mold plate is vertically recessed on the edge of the upper end surface of the lower mold.

[0012] Furthermore, a plurality of weight-reducing grooves for reducing weight are concavely arranged in the circumferential direction of the side wall of the lower mold.

[0013] According to another aspect of the present invention, a method for evaluating the dimensional deviation of an investment casting is also provided, which is used to evaluate the dimensional transfer deviation of the inner and outer fillets of the investment casting and the deviation of the contour clarity. The above-mentioned mold for evaluating the dimensional deviation of the investment casting is used, and the method includes the following steps: a. In the wax mold preparation stage, a wax material identical to the investment casting to be evaluated is selected, and the wax material is injected into the casting cavity through an injection tube to obtain a wax mold of a rounded corner part, and then blue light scanning is used to collect point cloud data of the wax mold of the rounded corner part to obtain a point cloud model of the wax mold of the rounded corner part; b. The point cloud model of the wax mold of the rounded corner part is fitted with a CAD model of the rounded corner part by using three-dimensional detection software, and the size of each fillet of the wax mold of the rounded corner part is measured by slicing in the axial direction, and then the deviation of the radius size of the wax mold of the rounded corner part is compared to obtain the deviation rate of the radius size of the rounded corner part of the wax mold; c. In the shell preparation stage, a shell material identical to the investment casting to be evaluated is selected to prepare a shell of the rounded corner part, and industrial CT is used to collect point cloud data of the shell of the rounded corner part to obtain the shell of the rounded corner part. point cloud model; d. slice the collected point cloud model of the rounded corner mold shell in the direction of the central axis, measure the radius size of each fillet of the rounded corner mold shell, and then compare the deviation of the fillet radius size of the rounded corner mold shell to obtain the fillet radius size deviation rate of the rounded corner mold shell; e. in the alloy shrinkage stage, select the same molten metal as the investment casting to be evaluated, introduce the molten metal into the rounded corner mold shell, and then cool it to obtain the rounded corner casting, and use blue light scanning to collect the point cloud data of the rounded corner casting to obtain the fillet radius size deviation rate of the rounded corner mold shell; f. Use 3D detection software to fit the point cloud model of the rounded corner casting with the CAD model of the rounded corner casting, slice the center axis direction to measure the size of each fillet, and then compare the deviation of the fillet radius size of the rounded corner casting to obtain the fillet radius size deviation rate of the rounded corner casting; g. Evaluate the fillet radius size deviation rate of the investment casting according to the fillet radius size deviation rate of the wax mold of the rounded corner part, the fillet radius size deviation rate of the shell of the rounded corner part and the fillet radius size deviation rate of the rounded corner casting.

[0014] Furthermore, the contour definition deviation of the investment casting is evaluated according to the radius size deviation rate of the fillet part wax pattern, the radius size deviation rate of the fillet part shell and the radius size deviation rate of the fillet part casting.

[0015] The present invention has the following beneficial effects:

[0016] The mold for evaluating the dimensional deviation of an investment casting of the present invention forms a casting cavity by enclosing an upper mold and a molding boss, selects the same wax material as that in the casting process of the investment casting to be evaluated, and then conveys the wax material into the casting cavity through an injection pipe to obtain a wax mold of a rounded corner part with a simple structure and a rounded corner size that is easy to measure, and then compares and calculates the rounded corner size of the wax mold of the rounded corner part with the rounded corner size at the beginning of the design to obtain the rounded corner radius size deviation rate of the wax mold of the rounded corner part; since the inner wall of the upper mold is provided with a plurality of inner fillets of different sizes, a plurality of outer fillets of different sizes are formed on the wax mold of the rounded corner part, and since the rounded corner radius size deviation rates of these outer fillets of different sizes are easy to obtain, it can be used to evaluate the rounded corner radius size deviation rate of the outer fillets of the same fillet size but difficult to measure on the investment casting during the wax mold preparation process; since the outer wall of the molding boss is provided with a plurality of outer fillets of different sizes, a plurality of outer fillets of different sizes are formed on the wax mold of the rounded corner part Different sizes of inner fillets, since the fillet radius size deviation rate of these different sizes of inner fillets is easy to obtain, it can be used to evaluate the fillet radius size deviation rate of inner fillets with the same fillet size but difficult to measure on investment castings during the preparation of wax molds; the lower mold is used to support the forming boss, the removal template and the upper mold to ensure the stability and reliability of the wax mold forming process of the fillet part; the wax mold of the fillet part is taken out by removing the template to avoid damage to the wax mold of the fillet part due to direct removal, thereby ensuring the dimensional accuracy of the wax mold of the fillet part; this scheme uses the upper mold, the forming boss and the injection tube to cooperate with each other to obtain a wax mold of a fillet part with multiple inner and outer fillet sizes but easy to measure, so as to evaluate the inner and outer fillets with the same fillet size but difficult to measure on investment castings, ensure the stability and smoothness of the wax mold preparation process of the fillet part by the lower mold, and ensure the smooth removal of the wax mold of the fillet part by the removal template, so as to ensure the dimensional accuracy of the wax mold of the fillet part, thereby improving the accuracy of the evaluation results.

[0017] The method for evaluating the dimensional deviation of an investment casting of the present invention comprises the following steps: in the preparation of a wax pattern, the same wax material as that in the preparation process of the investment casting wax pattern to be evaluated is selected to prepare a wax pattern of a rounded corner part, and the rounded corner radius size deviation rate of the wax pattern of the rounded corner part is accurately and quickly obtained through blue light scanning and three-dimensional detection software; in the preparation of a mold shell, the same mold shell material as that in the preparation process of the investment casting mold shell to be evaluated is selected to prepare a mold shell of the rounded corner part, and the rounded corner radius size deviation rate of the mold shell of the rounded corner part is accurately and quickly obtained through industrial CT; in the shrinkage of the alloy .... During the shrinkage process of the die casting alloy, the same molten metal is introduced into the rounded corner mold shell to prepare the rounded corner casting. The fillet radius size deviation rate of the rounded corner casting is accurately and quickly obtained through blue light scanning and 3D detection software; then according to the size transfer in these three stages, the deviation rate of the contour clarity of the investment casting is obtained to solve the problems that the inner and outer fillet size transfer is difficult to measure and the measurement error is large, and the contour clarity deviation is difficult to observe in the traditional measurement method of investment casting. At the same time, the wax material, mold shell material and molten metal can be replaced as needed, with strong versatility.

[0018] In addition to the above-described purposes, features and advantages, the present invention has other purposes, features and advantages. The present invention will be further described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The drawings constituting a part of this application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0020] Figure 1 It is a schematic structural diagram of a mold for evaluating dimensional deviation of investment castings according to a preferred embodiment of the present invention;

[0021] Figure 2 It is a schematic structural diagram of a mold for evaluating dimensional deviation of investment castings according to a preferred embodiment of the present invention.

[0022] Legend:

[0023] 1. Lower mold; 11. Moving part; 12. Mounting groove; 13. Second mold removal groove; 14. Weight reduction groove; 2. Forming boss; 3. Template removal; 31. First mold removal groove; 4. Upper mold; 41. Support part; 5. Injection tube; 6. First positioning column; 7. Second positioning column. DETAILED DESCRIPTION

[0024] The embodiments of the present invention are described in detail below with reference to the accompanying drawings. However, the present invention can be implemented in many different ways as defined and covered below.

[0025] Figure 1It is a schematic structural diagram of a mold for evaluating dimensional deviation of investment castings according to a preferred embodiment of the present invention; Figure 2 It is a schematic structural diagram of a mold for evaluating dimensional deviation of investment castings according to a preferred embodiment of the present invention.

[0026] like Figure 1 and Figure 2As shown, the mold for evaluating the dimensional deviation of investment castings in this embodiment is used to evaluate the dimensional transfer deviation of inner and outer fillets and the contour clarity deviation of investment castings, including a lower mold 1, a molding boss 2 connected to the lower mold 1, a removal template 3 sleeved on the molding boss 2 and fitted with the upper end surface of the lower mold 1, and an upper mold 4 covered on the molding boss 2 and fitted with the upper end surface of the removal template 3, the inner wall of the upper mold 4 is provided with a plurality of inner fillets of different sizes, the outer wall of the molding boss 2 is provided with a plurality of outer fillets of different sizes, the inner wall of the upper mold 4 and the outer wall of the molding boss 2 are combined to form a casting cavity for injection molding a wax mold of a filleted part with a plurality of inner and outer fillets of different sizes, and the mold also includes an injection pipe 5 connected to the casting cavity for conveying wax into the casting cavity. Specifically, the mold for evaluating the dimensional deviation of investment castings of the present invention forms a casting cavity by enclosing an upper mold 4 and a molding boss 2, selects the same wax material as that used in the casting process of the investment casting to be evaluated, and then conveys the wax material into the casting cavity through an injection pipe 5 to obtain a wax mold of a rounded corner part with a simple structure and a rounded corner size that is easy to measure, and then compares and calculates the rounded corner size of the wax mold of the rounded corner part with the rounded corner size at the beginning of the design to obtain the rounded corner radius size deviation rate of the wax mold of the rounded corner part; since the inner wall of the upper mold 4 is provided with a plurality of inner fillets of different sizes, a plurality of outer fillets of different sizes are formed on the wax mold of the rounded corner part, and since the rounded corner radius size deviation rates of these outer fillets of different sizes are easy to obtain, it can be used to evaluate the rounded corner radius size deviation rate of the outer fillets of the same fillet size but difficult to measure on the investment casting during the wax mold preparation process; since the outer wall of the molding boss 2 is provided with a plurality of outer fillets of different sizes, a plurality of Different sizes of inner fillets, since the fillet radius size deviation rate of these different sizes of inner fillets is easy to obtain, it can be used to evaluate the fillet radius size deviation rate of inner fillets with the same fillet size but difficult to measure on investment castings during the preparation of wax molds; the lower mold 1 supports the forming boss 2, the template 3 and the upper mold 4 to ensure stability and reliability during the molding process of the wax mold of the fillet part; the wax mold of the fillet part is taken out by taking out the template 3 to avoid damage to the wax mold of the fillet part due to direct removal, thereby ensuring the dimensional accuracy of the wax mold of the fillet part; in this scheme, the upper mold 4, the forming boss 2 and the injection tube 5 cooperate with each other to obtain a wax mold of a fillet part with multiple inner and outer fillet sizes but easy to measure, so as to evaluate the inner and outer fillets with the same fillet size but difficult to measure on investment castings, ensure the stability and smoothness of the preparation process of the wax mold of the fillet part by the lower mold 1, and ensure the smooth removal of the wax mold of the fillet part by taking out the template 3, so as to ensure the dimensional accuracy of the wax mold of the fillet part, thereby improving the accuracy of the evaluation results.

[0027] like Figure 2As shown, in this embodiment, the forming boss 2 includes a plurality of cylinders of different diameters connected in sequence, the connection between two adjacent cylinders is set as an outer fillet, and the edge corner of the end face of the cylinder is set as an outer fillet; and / or the inner cavity of the upper mold 4 includes a plurality of cylindrical grooves of different diameters connected in sequence, the connection between two cylindrical grooves is set as an inner fillet, and the edge corner of the bottom of the cylindrical groove is set as an inner fillet. Specifically, the forming boss 2 is composed of a plurality of cylinders of different diameters connected in sequence, and the connection between the two cylinders is set as an outer fillet, and the edge corner of the end face of the cylinder is set as an outer fillet, so that when the wax mold of the filleted part is cast, the wax mold of the filleted part has multiple inner fillets on cylinders of different diameters, so as to evaluate the fillet radius size deviation rate of the inner fillets with the same diameter and the same fillet radius on the investment casting but difficult to measure during the wax mold preparation process; specifically, the inner cavity of the upper membrane is composed of a plurality of cylindrical grooves of different diameters connected in sequence, and the connection between the two cylindrical grooves is set as an inner fillet, and the edge corner of the bottom of the cylindrical groove is set as an inner fillet, so that when the wax mold of the filleted part is cast, the wax mold of the filleted part has multiple outer fillets on cylinders of different diameters, so as to evaluate the fillet radius size deviation rate of the outer fillets with the same diameter and the same fillet radius on the investment casting but difficult to measure during the wax mold preparation process.

[0028] like Figure 2 As shown, in this embodiment, the lower end face of the upper mold 4 is vertically recessed with a plurality of connection holes, and the mold also includes a support member 41 fixedly connected to the connection hole for supporting the upper mold 4, and the template 3 is provided with a clearance groove arranged corresponding to the support member 41 for accommodating the support member 41, and the connection hole, the support member 41, and the clearance groove are arranged one by one. Specifically, when the upper mold 4 is installed on the template 3, the support member 41 is plugged into the clearance groove; when the upper mold 4 is taken out, the support member 41 supports the upper mold 4 to avoid the lower end face of the upper mold 4 from contacting with the wax injection machine table and being damaged, thereby ensuring the assembly accuracy when the upper mold 4 is assembled with the template 3. Optionally, the support member 41 is fixedly connected with the connection hole by thread, and the connection is reliable and easy to disassemble and assemble. Optionally, the upper end face of the upper mold 4 is vertically recessed with a weight-reducing hole to reduce the weight of the upper mold 4, which is convenient for movement, while saving manufacturing materials and reducing costs. Optionally, a plurality of weight-reducing cavities are concavely formed in the circumferential direction of the side wall of the upper mold 4 to reduce the weight of the upper mold 4, facilitate movement, save manufacturing materials, and reduce costs. Optionally, a vent hole is formed in the middle of the molding boss 2, and an exhaust hole for exhaust connected to the vent hole is formed in the middle of the upper end surface of the upper mold 4.

[0029] like Figure 2As shown, in this embodiment, the mold further includes a moving member 11 connected to the side wall of the lower mold 1 for applying force when the lower mold 1 or the mold moves. Specifically, by applying force to the moving member 11, the lower mold 1 is moved, and when the lower mold 1 is assembled with the take-off plate 3, the molding boss 2 and the upper mold 4, it is convenient to move the entire mold. Optionally, the moving member 11 includes a U-shaped handle, and the two ends of the U-shaped handle are fixedly connected to the lower mold 1 by connecting pins, and the connection is reliable and easy to disassemble and assemble.

[0030] like Figure 2 As shown, in this embodiment, the upper end surface of the lower mold 1 is vertically recessed with a mounting groove 12 for mounting the molding boss 2, the bottom of the mounting groove 12 is vertically provided with a first fixing hole, the lower end surface of the molding boss 2 is vertically recessed with a second fixing hole arranged corresponding to the first fixing hole, and the mold further includes a fixing member that is penetrated through the first fixing hole and fixedly connected to the second fixing hole. Specifically, the fixing member is penetrated through the first fixing hole and fixedly connected to the second fixing hole to ensure reliable assembly between the lower mold 1 and the molding boss 2. Optionally, the bottom of the mounting groove 12 is circumferentially spaced with a plurality of first fixing holes, the fixing member, the second fixing hole and the first fixing hole are arranged one by one, the first fixing hole, the second fixing hole and the fixing member constitute a connection structure between the lower mold 1 and the molding boss 2, and reliable assembly between the lower mold 1 and the molding boss 2 is ensured by a plurality of connection structures. Optionally, the fixing member is threadedly fixedly connected to the second fixing hole, the connection is reliable, and the assembly and disassembly are convenient.

[0031] like Figure 2 As shown, in this embodiment, the edge of the upper end surface of the removal template 3 is vertically recessed with a first mold removal groove 31 for removing the upper mold 4. Specifically, the first mold removal groove 31 increases the mold removal force point to facilitate the removal of the upper mold 4, while also reducing the weight of the removal template 3, saving manufacturing materials, and reducing costs. Optionally, the upper end surface of the removal template 3 is circumferentially spaced with a plurality of first mold removal grooves 31 to increase a plurality of mold removal force points and reduce the difficulty of disassembly.

[0032] like Figure 2 As shown, in this embodiment, the edge of the upper end surface of the lower mold 1 is vertically recessed with a second mold removal groove 13 for removing the mold removal plate 3. Specifically, the second mold removal groove 13 increases the mold removal force point, so as to facilitate the removal of the mold removal plate 3, and at the same time, it can also reduce the weight of the lower mold 1, save manufacturing materials, and reduce costs. Optionally, a plurality of second mold removal grooves 13 are arranged at intervals in the circumferential direction on the upper end surface of the mold removal plate 3 to increase multiple mold removal force points and reduce the difficulty of disassembly.

[0033] like Figure 2 As shown, in this embodiment, the side wall of the lower mold 1 is circumferentially concave with a plurality of weight-reducing grooves 14 for reducing weight. Specifically, the weight of the lower mold 1 is reduced by the plurality of weight-reducing grooves 14, which is convenient for movement, while saving manufacturing materials and reducing costs.

[0034] like Figure 2 As shown, in this embodiment, the upper end surface of the lower mold 1 is vertically recessed with a first positioning groove, the mold further includes a first positioning column 6 installed in the first positioning groove, and the removal template 3 is penetrated with a first positioning hole arranged corresponding to the first positioning groove. Specifically, the first positioning groove, the first positioning column 6 and the first positioning hole cooperate with each other to position the removal template 3 on the lower mold 1.

[0035] like Figure 2 As shown, in this embodiment, the upper end surface of the lower mold 1 is vertically recessed with a second positioning groove, the mold further includes a second positioning column 7 installed in the second positioning groove, the removal template 3 is penetrated with the second positioning column 7 arranged corresponding to the second positioning groove, and the lower end surface of the upper mold 4 is vertically recessed with a limiting hole arranged corresponding to the second positioning hole. Specifically, the upper mold 4 is positioned on the removal template 3 through the mutual cooperation of the second positioning groove, the second positioning column 7, the second positioning column 7 and the limiting hole.

[0036] The method for evaluating the dimensional deviation of an investment casting of the present embodiment is used to evaluate the dimensional transfer deviation of the inner and outer fillets of the investment casting and the contour clarity deviation. The above-mentioned mold for evaluating the dimensional deviation of an investment casting is used, and the method comprises the following steps: a. In the wax mold preparation stage, a wax material identical to the investment casting to be evaluated is selected, and the wax material is injected into the casting cavity through the injection pipe 5 to obtain a wax mold of a rounded corner part, and then the point cloud data of the wax mold of the rounded corner part is collected by blue light scanning to obtain a point cloud model of the wax mold of the rounded corner part; b. The point cloud model of the wax mold of the rounded corner part is fitted with the CAD model of the rounded corner part by using three-dimensional detection software, and the size of each fillet of the wax mold of the rounded corner part is measured by slicing in the axial direction, and then the deviation of the radius size of the wax mold of the rounded corner part is compared to obtain the deviation rate of the radius size of the wax mold of the rounded corner part; c. In the shell preparation stage, a shell material identical to the investment casting to be evaluated is selected to prepare a shell of the rounded corner part, and the point cloud data of the shell of the rounded corner part is collected by industrial CT to obtain a point cloud model of the shell of the rounded corner part; d. Slice the collected point cloud model of the rounded corner mold shell in the direction of the central axis, measure the radius size of each fillet of the rounded corner mold shell, and then compare the deviation of the fillet radius size of the rounded corner mold shell to obtain the fillet radius size deviation rate of the rounded corner mold shell; e. In the alloy shrinkage stage, select the same molten metal as the investment casting to be evaluated, introduce the molten metal into the rounded corner mold shell, and then cool it to obtain the rounded corner casting, and use blue light scanning to collect the point cloud data of the rounded corner casting to obtain the rounded corner casting. f. Use 3D detection software to fit the point cloud model of the rounded corner casting with the CAD model of the rounded corner casting, slice the center axis direction to measure the size of each fillet, and then compare the deviation of the fillet radius size of the rounded corner casting to obtain the fillet radius size deviation rate of the rounded corner casting; g. Evaluate the fillet radius size deviation rate of the investment casting according to the fillet radius size deviation rate of the wax mold of the rounded corner part, the fillet radius size deviation rate of the shell of the rounded corner part and the fillet radius size deviation rate of the rounded corner casting.Specifically, in the preparation of the wax pattern, the same wax material as that used in the preparation process of the wax pattern of the investment casting to be evaluated is selected to prepare the wax pattern of the rounded corner part, and the fillet radius size deviation rate of the wax pattern of the rounded corner part is accurately and quickly obtained through blue light scanning and three-dimensional detection software; in the preparation of the shell, the same shell material as that used in the preparation process of the shell of the investment casting to be evaluated is selected to prepare the shell of the rounded corner part, and the fillet radius size deviation rate of the shell of the rounded corner part is accurately and quickly obtained through industrial CT; in the alloy shrinkage, the same molten metal as that used in the alloy shrinkage process of the investment casting to be evaluated is selected and introduced into the shell of the rounded corner part to prepare the rounded corner part casting, and the fillet radius size deviation rate of the rounded corner part casting is accurately and quickly obtained through blue light scanning and three-dimensional detection software; then, based on the dimensional transfer in these three stages, the deviation rate of the contour clarity of the investment casting is obtained to solve the problem that the internal and external fillet size transfer is difficult to measure and the measurement error is large, and the contour clarity deviation is difficult to observe in the traditional measurement method of investment casting. At the same time, the wax material, shell material and molten metal can be replaced as needed, with strong versatility. Optionally, after the shell material is determined, the rounded corner shell can be obtained by sequentially adopting the steps of slurry dipping, sanding, air drying, dewaxing, etc. Optionally, the molten metal is cooled by air cooling to obtain the rounded corner casting. Optionally, the 3D detection software includes Geomagiccontrol.

[0037] In this embodiment, the contour clarity deviation of the investment casting is evaluated according to the fillet radius size deviation rate of the fillet part wax pattern, the fillet radius size deviation rate of the fillet part shell, and the fillet radius size deviation rate of the fillet part casting. Specifically, after obtaining the fillet radius size deviation rate of the inner and outer fillets of the casting in the three stages of investment casting, the contour clarity of the investment casting can be clearly known, thereby ensuring that the evaluation result of the contour clarity deviation of the investment casting is highly accurate.

[0038] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A mold for evaluating the dimensional deviation of investment castings, used for evaluating the transfer deviation of the inner and outer fillet dimensions and the contour clarity deviation of investment castings, characterized in that: The invention comprises a lower mold (1), a molding boss (2) connected to the lower mold (1), a removal mold plate (3) sleeved on the molding boss (2) and fitted with the upper end surface of the lower mold (1), and an upper mold (4) covered on the molding boss (2) and fitted with the upper end surface of the removal mold plate (3); the inner wall of the upper mold (4) is provided with a plurality of inner fillets of different sizes, the outer wall of the molding boss (2) is provided with a plurality of outer fillets of different sizes, the inner wall of the upper mold (4) and the outer wall of the molding boss (2) are combined to form a casting cavity for injection molding a wax mold of a filleted part having a plurality of inner fillets and outer fillets of different sizes, and the mold further comprises an injection pipe (5) connected to the casting cavity and used for conveying wax material into the casting cavity; The lower end surface of the upper mold (4) is vertically recessed with a plurality of connection holes, the mold further comprises a support member (41) fixedly connected to the connection hole and used to support the upper mold (4), the template (3) is provided with a clearance groove arranged corresponding to the support member (41) and used to accommodate the support member (41), and the connection holes, the support member (41) and the clearance groove are arranged one by one; The mold further comprises a moving part (11) connected to the side wall of the lower mold (1) and used for applying force when the lower mold (1) or the mold moves; The upper end surface of the lower mold (1) is vertically recessed with a mounting groove (12) for mounting the molding boss (2); the bottom of the mounting groove (12) is vertically provided with a first fixing hole; the lower end surface of the molding boss (2) is vertically recessed with a second fixing hole arranged corresponding to the first fixing hole; the mold further comprises a fixing member penetrating the first fixing hole and fixedly connected to the second fixing hole; A first mold removal groove (31) for removing the upper mold (4) is vertically recessed on the edge of the upper end surface of the removal mold plate (3); A second mold removal groove (13) for removing the mold plate (3) is vertically recessed on the edge of the upper end surface of the lower mold (1); The upper end surface of the lower mold (1) is vertically recessed with a first positioning groove, the mold further comprises a first positioning column (6) installed in the first positioning groove, and the template (3) is penetrated with a first positioning hole arranged corresponding to the first positioning groove; The upper end surface of the lower mold (1) is vertically recessed with a second positioning groove, the mold further comprises a second positioning column (7) installed in the second positioning groove, the template (3) is penetrated with a second positioning column (7) arranged corresponding to the second positioning groove, and the lower end surface of the upper mold (4) is vertically recessed with a limiting hole arranged corresponding to the second positioning hole.

2. The mold for evaluating dimensional deviation of investment castings according to claim 1, characterized in that: The forming boss (2) comprises a plurality of cylinders of different diameters connected in sequence, the connection between two adjacent cylinders is set as an outer rounded corner, and the edge corners of the end faces of the cylinders are set as outer rounded corners; and / or The inner cavity of the upper die (4) comprises a plurality of cylindrical grooves of different diameters which are connected in sequence, the connection between two adjacent cylindrical grooves is set as an inner fillet, and the groove bottom edge corner of the cylindrical groove is set as an inner fillet.

3. The mold for evaluating dimensional deviation of investment castings according to any one of claims 1 to 2, characterized in that: A plurality of weight-reducing grooves (14) for reducing weight are concavely arranged in the circumferential direction of the side wall of the lower mold (1).

4. A method for evaluating the dimensional deviation of an investment casting, for evaluating the transfer deviation of the inner and outer fillet dimensions and the contour definition deviation of an investment casting, characterized in that: The mold for evaluating the dimensional deviation of an investment casting according to any one of claims 1 to 3 comprises the following steps: a. In the wax model preparation stage, a wax material identical to the investment casting to be evaluated is selected, and the wax material is injected into the casting cavity through an injection pipe (5) to obtain a rounded corner part wax model, and then point cloud data of the rounded corner part wax model is collected by blue light scanning to obtain a point cloud model of the rounded corner part wax model; b. Use 3D detection software to fit the point cloud model of the wax mold of the rounded corner part with the CAD model of the rounded corner part, slice the wax mold in the central axial direction to measure the size of each fillet of the wax mold of the rounded corner part, and then compare the deviation of the radius size of the wax mold of the rounded corner part to obtain the deviation rate of the radius size of the rounded corner of the wax mold of the rounded corner part; c. In the shell preparation stage, the same shell material as the investment casting to be evaluated is selected to prepare the rounded corner shell, and the point cloud data of the rounded corner shell is collected by industrial CT to obtain the point cloud model of the rounded corner shell; d. Slice the collected point cloud model of the rounded corner mold shell in the direction of the center axis, measure the radius size of each rounded corner of the rounded corner mold shell, and then compare the deviation of the rounded corner radius size of the rounded corner mold shell to obtain the rounded corner radius size deviation rate of the rounded corner mold shell; e. In the alloy shrinkage stage, select the same molten metal as the investment casting to be evaluated, introduce the molten metal into the rounded corner part shell, and then cool it to obtain the rounded corner part casting, and use blue light scanning to collect point cloud data of the rounded corner part casting to obtain a point cloud model of the rounded corner part casting; f. Use 3D detection software to fit the point cloud model of the fillet casting with the fillet CAD model, slice along the central axis to measure the size of each fillet, and then compare the deviation of the fillet radius size of the fillet casting to obtain the fillet radius size deviation rate of the fillet casting; g. Evaluate the radius size deviation rate of investment castings based on the radius size deviation rate of the wax mold of the fillet part, the radius size deviation rate of the shell of the fillet part, and the radius size deviation rate of the casting of the fillet part.

5. The method for evaluating dimensional deviation of an investment casting according to claim 4, characterized in that: The contour definition deviation of investment castings was evaluated based on the radius deviation rate of the fillet of the wax pattern, the radius deviation rate of the shell and the radius deviation rate of the casting.

Citation Information

Patent Citations

  • Investment casting wax mold and deformation control method of investment casting wax mold

    CN108907081A