Dielectric layer etching method on metal gate
By forming a metal oxide barrier layer on the surface of the metal gate to fill the recessed scratches and using it as an etching stop layer, the problem of acidic solution erosion during etching of the dielectric layer is solved and the integrity of the metal gate is protected.
Patent Information
- Application Number
- CN202111319340.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-09
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-11-09
AI Technical Summary
The dented scratches generated during the planarization process of the metal gate surface will cause the acidic solution to erode the metal gate during subsequent etching of the dielectric layer, causing damage.
By forming a metal oxide barrier layer on the surface of the metal gate, the recessed scratches are filled, and the oxide barrier layer is used as an etching stop layer during the dielectric layer etching process to avoid acidic solution erosion.
It effectively protects the surface of the metal gate, prevents damage caused by dent scratches during the etching process of the dielectric layer, and ensures the integrity of the metal gate.
Smart Images

Figure CN114242574B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor integrated circuit manufacturing, and in particular to a method for etching a dielectric layer on a metal gate. Background Art
[0002] In the related art, after the metal gate is manufactured, the surface of the metal gate is firstly planarized by a chemical mechanical polishing process, and then a dielectric layer is formed on the planarized metal gate.
[0003] However, particles generated during the surface planarization of the metal gate will scratch the surface of the metal gate during the subsequent grinding process, thereby forming concave scratches on the surface of the metal gate. The subsequent dielectric layer will grow along the device surface morphology, so that the dielectric layer will form a sunken morphology at the concave scratches.
[0004] In the subsequent process of etching the dielectric layer to form the contact hole, an acid solution is used, and the acid solution will corrode the metal gate downward along the recess, causing damage to the metal gate. Summary of the invention
[0005] The present application provides a method for etching a dielectric layer on a metal gate, which can solve the problem in the related art that the dielectric layer on the metal gate is corroded by an acidic solution used in the etching process due to recessed scratches in the surface layer of the metal gate.
[0006] In order to solve the technical problem described in the background technology, the present application provides a method for etching a dielectric layer on a metal gate, and the method for etching a dielectric layer on a metal gate comprises the following steps performed in sequence:
[0007] Providing a semiconductor device having a metal gate formed thereon;
[0008] Oxidizing the surface of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the concave scratches on the surface of the metal grid;
[0009] Fabricating a dielectric layer on the semiconductor device, wherein the dielectric layer at least covers the metal oxide barrier layer;
[0010] An etching pattern is defined by the photoresist layer, and the dielectric layer is etched according to the etching pattern with the metal oxide barrier layer being used as an etching stop layer.
[0011] Optionally, in the step of providing a semiconductor device having a metal gate, the metal gate of the semiconductor device is subjected to chemical mechanical polishing.
[0012] Optionally, the step of oxidizing the surface layer of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the recessed scratches on the surface of the metal grid, comprises:
[0013] In an environment of 300° C. to 500° C., oxygen is introduced for 30 seconds to 60 seconds to oxidize the surface of the metal grid to form a metal oxide barrier layer, which fills the concave scratches on the surface of the metal grid.
[0014] Optionally, the step of oxidizing the surface layer of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the recessed scratches on the surface of the metal grid, comprises:
[0015] The surface layer of the metal grid is oxidized to form a metal oxide barrier layer with a thickness ranging from 30 angstroms to 50 angstroms, and the metal oxide barrier layer fills the concave scratches on the surface of the metal grid.
[0016] Optionally, the material of the metal grid is aluminum, and the material of the metal oxide barrier layer is aluminum oxide.
[0017] Optionally, the step of manufacturing a dielectric layer on the semiconductor device, wherein the dielectric layer at least covers the metal oxide barrier layer, comprises:
[0018] Fabricating a titanium nitride dielectric layer on the semiconductor device, wherein the titanium nitride dielectric layer at least covers the metal oxide barrier layer;
[0019] A silicon nitride dielectric layer is manufactured so that the silicon nitride dielectric layer covers the titanium nitride dielectric layer.
[0020] Optionally, the step of defining an etching pattern through the photoresist layer, and etching the dielectric layer according to the etching pattern using the metal oxide barrier layer as an etching stop layer comprises:
[0021] Defining an etching pattern through the photoresist layer;
[0022] According to the etching pattern, the portion of the silicon nitride dielectric layer not covered by the photoresist layer is removed by dry etching, so that the portion of the titanium nitride dielectric layer under the portion of the silicon nitride dielectric layer is exposed;
[0023] According to the etching pattern, the exposed part of the titanium nitride dielectric layer is removed by wet etching, so that the etching stop layer is located in the metal oxide barrier layer, and the part of the metal oxide barrier layer under the part of the titanium nitride dielectric layer is exposed.
[0024] Optionally, the exposed portion of the titanium nitride dielectric layer is removed by wet etching according to the etching pattern, so that the etch stop layer is located in the metal oxide barrier layer, and in the step of exposing the portion of the metal oxide barrier layer under the titanium nitride dielectric layer, the wet etching is performed using an acidic wet etching solution.
[0025] The technical solution of the present application has at least the following advantages: the present application forms a metal oxide barrier layer by oxidizing the surface of the metal gate, and the metal oxide barrier layer fills the concave scratch on the surface of the metal gate; a dielectric layer is made on the semiconductor device, and the dielectric layer at least covers the metal oxide barrier layer; an etching pattern is defined by the photoresist layer, and the dielectric layer is etched according to the etching pattern with the metal oxide barrier layer as an etching stop layer. Since the metal oxide barrier layer fills the concave scratch, the concave scratch 111 is protected by the metal oxide barrier layer, thereby preventing the metal oxide barrier layer from being damaged by the concave scratch during the etching of the dielectric layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0027] Figure 1 A flow chart of a dielectric layer etching method on a metal gate provided in an embodiment of the present application is shown;
[0028] Figure 1a A schematic diagram of a partial cross-sectional structure of a semiconductor device provided in step S11 is shown;
[0029] Figure 2 Shown in Figure 1 Based on the semiconductor device structure shown, a schematic cross-sectional structure diagram of the semiconductor device after completing step S12;
[0030] Figure 3 Shown in Figure 2 Based on the structure shown, a schematic diagram of a cross-sectional structure of a semiconductor device after completing step S13 is shown. DETAILED DESCRIPTION
[0031] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0032] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0033] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0034] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0035] Figure 1 A flow chart of a dielectric layer etching method on a metal gate provided in an embodiment of the present application is shown. Figure 1 It can be seen that the method for etching the dielectric layer on the metal gate provided in this embodiment includes the following steps performed in sequence:
[0036] Step S11: providing a semiconductor device with a metal gate formed thereon.
[0037] Reference Figure 1a , which shows a partial cross-sectional structural schematic diagram of the semiconductor device provided in step S11.
[0038] from Figure 1a As can be seen, the semiconductor device 100 includes a base layer 101, a metal gate 110 is formed on the base layer 101, sidewall structures 102 are respectively formed on the left and right side walls of the metal gate 110, and a source 103 and a drain 104 are respectively formed in the base layer 101 located on both sides of the metal gate 110.
[0039] It should be noted that Figure 1aThe metal gate 110 of the semiconductor device 100 shown in the figure is subjected to chemical mechanical polishing. The particles generated during the chemical mechanical polishing and flattening process of the metal gate 110 surface will scratch the surface of the metal gate 110 during the subsequent polishing process. Figure 1 The metal grid 110 shown has recessed scratches 111 formed on its surface.
[0040] Step S12: oxidizing the surface layer of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the recessed scratches on the surface of the metal grid.
[0041] Reference Figure 2 , which shows that in Figure 1 Based on the semiconductor device structure shown, a schematic diagram of a cross-sectional structure of the semiconductor device after completing step S12 is shown.
[0042] from Figure 2 It can be seen that the surface layer of the metal gate 110 is oxidized to form a metal oxide barrier layer 120 , and the formed metal oxide barrier layer 120 fills the recessed scratch 111 .
[0043] Optionally, oxygen is introduced in an environment of 300°C to 500°C for 30 seconds to 60 seconds to oxidize the surface of the metal grid to form a metal oxide barrier layer with a thickness ranging from 30 angstroms to 50 angstroms, and the metal oxide barrier layer fills the recessed scratches on the surface of the metal grid.
[0044] The material of the metal gate 110 is aluminum, and the material of the metal oxide barrier layer 120 is aluminum oxide.
[0045] Step S13: manufacturing a dielectric layer on the semiconductor device, wherein the dielectric layer at least covers the metal oxide barrier layer.
[0046] Reference Figure 3 , which shows that in Figure 2 Based on the structure shown, a schematic diagram of a cross-sectional structure of a semiconductor device after completing step S13 is shown.
[0047] from Figure 3 It can be seen that the metal oxide barrier layer 120 is covered with a dielectric layer 130.
[0048] Optionally, the dielectric layer 130 may be a composite structure stacked up and down, including a titanium nitride dielectric layer located at the bottom and covering the metal oxide barrier layer 120 , and a silicon nitride dielectric layer covering the titanium nitride dielectric layer.
[0049] The method for manufacturing the dielectric layer 130 of the composite structure includes:
[0050] First, a titanium nitride dielectric layer is formed on the semiconductor device, and the titanium nitride dielectric layer at least covers the metal oxide barrier layer.
[0051] A silicon nitride dielectric layer is then manufactured so that the silicon nitride dielectric layer covers the titanium nitride dielectric layer.
[0052] Step S14: defining an etching pattern through the photoresist layer, and etching the dielectric layer according to the etching pattern with the metal oxide barrier layer as an etching stop layer.
[0053] After the dielectric layer 130 is etched based on the etching pattern of the photoresist layer, the etching stop layer is located in the metal oxide barrier layer 120. Since the metal oxide barrier layer 120 fills the recessed scratch 111, the recessed scratch 111 is protected by the metal oxide barrier layer 120, thereby preventing the metal oxide barrier layer 120 from being damaged by the recessed scratch 111 during the etching of the dielectric layer 130.
[0054] Optionally, when the dielectric layer 130 may be a composite structure stacked up and down, including a titanium nitride dielectric layer located at the bottom layer and covering the metal oxide barrier layer 120, and a silicon nitride dielectric layer covering the titanium nitride dielectric layer, the etching pattern is defined by the photoresist layer, and according to the etching pattern, the step of etching the dielectric layer with the metal oxide barrier layer as an etching stop layer includes the following steps performed in sequence:
[0055] Step S141: defining an etching pattern through the photoresist layer;
[0056] Step S142: removing the portion of the silicon nitride dielectric layer not covered by the photoresist layer by dry etching according to the etching pattern, so that the portion of the titanium nitride dielectric layer under the portion of the silicon nitride dielectric layer is exposed;
[0057] Step S143: removing the exposed portion of the titanium nitride dielectric layer by wet etching according to the etching pattern, so that the etching stop layer is located in the metal oxide barrier layer, and the portion of the metal oxide barrier layer under the portion of the titanium nitride dielectric layer is exposed.
[0058] Among them, according to the etching pattern, the exposed part of the titanium nitride dielectric layer is removed by wet etching, so that the etching stop layer is located in the metal oxide barrier layer, and in the step of exposing the part of the metal oxide barrier layer under the titanium nitride dielectric layer, the wet etching is performed using an acidic wet etching solution.
[0059] After the dielectric layer 130 is etched, the remaining photoresist layer may be removed.
[0060] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.
Claims
1. A method for etching a dielectric layer on a metal gate, characterized in that: The method for etching the dielectric layer on the metal gate comprises the following steps performed in sequence: Providing a semiconductor device having a metal gate formed thereon; Oxidizing the surface of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the concave scratches on the surface of the metal grid; Fabricating a dielectric layer on the semiconductor device, wherein the dielectric layer at least covers the metal oxide barrier layer; An etching pattern is defined by the photoresist layer, and the dielectric layer is etched according to the etching pattern with the metal oxide barrier layer being used as an etching stop layer.
2. The method for etching a dielectric layer on a metal gate according to claim 1, characterized in that: In the step of providing a semiconductor device having a metal gate, the metal gate of the semiconductor device is subjected to chemical mechanical polishing.
3. The method for etching a dielectric layer on a metal gate according to claim 1, characterized in that: The step of oxidizing the surface layer of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the concave scratches on the surface of the metal grid, comprises: In an environment of 300° C. to 500° C., oxygen is introduced for 30 seconds to 60 seconds to oxidize the surface of the metal grid to form a metal oxide barrier layer, which fills the concave scratches on the surface of the metal grid.
4. The method for etching a dielectric layer on a metal gate according to claim 1, wherein: The step of oxidizing the surface layer of the metal grid to form a metal oxide barrier layer, wherein the metal oxide barrier layer fills the concave scratches on the surface of the metal grid, comprises: The surface layer of the metal grid is oxidized to form a metal oxide barrier layer with a thickness ranging from 30 angstroms to 50 angstroms, and the metal oxide barrier layer fills the concave scratches on the surface of the metal grid.
5. The method for etching a dielectric layer on a metal gate according to claim 1, wherein: The material of the metal grid is aluminum, and the material of the metal oxide barrier layer is aluminum oxide.
6. The method for etching a dielectric layer on a metal gate according to claim 1, characterized in that: The step of manufacturing a dielectric layer on the semiconductor device, wherein the dielectric layer at least covers the metal oxide barrier layer, comprises: Fabricating a titanium nitride dielectric layer on the semiconductor device, wherein the titanium nitride dielectric layer at least covers the metal oxide barrier layer; A silicon nitride dielectric layer is manufactured so that the silicon nitride dielectric layer covers the titanium nitride dielectric layer.
7. The method for etching a dielectric layer on a metal gate according to claim 6, characterized in that: The step of defining an etching pattern through the photoresist layer and etching the dielectric layer according to the etching pattern using the metal oxide barrier layer as an etching stop layer comprises: Defining an etching pattern through the photoresist layer; According to the etching pattern, the portion of the silicon nitride dielectric layer not covered by the photoresist layer is removed by dry etching, so that the portion of the titanium nitride dielectric layer under the portion of the silicon nitride dielectric layer is exposed; According to the etching pattern, the exposed part of the titanium nitride dielectric layer is removed by wet etching, so that the etching stop layer is located in the metal oxide barrier layer, and the part of the metal oxide barrier layer under the part of the titanium nitride dielectric layer is exposed.
8. The method for etching a dielectric layer on a metal gate according to claim 7, wherein: According to the etching pattern, the exposed part of the titanium nitride dielectric layer is removed by wet etching, so that the etching stop layer is located in the metal oxide barrier layer. In the step of exposing the part of the metal oxide barrier layer under the titanium nitride dielectric layer, the wet etching is performed using an acidic wet etching solution.
Citation Information
Patent Citations
Method for fabricating semiconductor device
CN104025268A
Method for manufacturing zeroth interlayer film
CN110148552A