A photoresist spray coating method
By calculating the wafer heat transfer coefficient and temperature control, combined with the nozzle movement path, the problem of poor film uniformity and bubbles during the photoresist spraying process is solved, achieving uniform coating of the film on the wafer surface and reducing bubbles, ensuring the photoresist film of high quality.
Patent Information
- Application Number
- CN202210082573.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-01-24
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-01-24
AI Technical Summary
During the existing photoresist spraying process, the film uniformity on the wafer surface is poor and bubbles are easily generated, which affects subsequent photolithography and development processes.
By calculating the heat transfer coefficient K of the uncoated wafer, combined with temperature control and nozzle movement process control, uniform coating of the film and reduction of bubbles are achieved. Specific steps include calculating the temperature increase ΔT, determining the heat transfer coefficient K, fitting constant ɑ, setting the heating plate temperature and the nozzle movement path to ensure the uniformity of the film during temperature and movement.
It achieves good uniformity of the film on the wafer surface without bubble deposition, improves the surface quality of the photoresist film, and ensures the normal progress of subsequent processes.
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductor manufacturing, and more specifically, particularly relates to a photoresist spray coating method. Background Art
[0002] The semiconductor manufacturing process includes wafer manufacturing, photolithography, etching, diffusion, ion implantation, thin film deposition and other processes. Among them, the photolithography process is an important link in pattern formation. The photolithography process is a key process in semiconductor production and manufacturing. Photolithography is the process of transferring the geometric pattern on the mask to the photosensitive thin film material (commonly known as photoresist) coated on the surface of the semiconductor wafer. The main steps of pattern formation in photolithography are coating, exposure and development. Spraying has the characteristics of high material utilization, no influence of substrate morphology, good repeatability and large coating area, and is widely used in photolithography.
[0003] In the existing spray coating process, the starting point of each cycle is exactly the same, and the nozzle travel route of each cycle is the same, because the amount of photoresist deposited in each area of the wafer surface during the spray coating process is different. And the cycle is superimposed, resulting in poor uniformity of the thick film. And due to the physical and chemical properties of the photoresist chemicals themselves and the limitations of process conditions, bubbles are easily generated during the spray coating process, affecting the uniformity of the photoresist film surface. Especially for photoresist products with high viscosity. The film surface has bubbles, and the more serious consequence is that it affects the subsequent photolithography and development processes. Summary of the invention
[0004] The purpose of the present invention is to solve the shortcomings of the prior art. The method can make the wafer surface film uniform, good and bubble-free. Combined with the covering spray-type glue coating action, it can solve the problem of poor uniformity and reduce the deposition of bubbles on the surface of the photoresist film.
[0005] To achieve the above object, the present invention provides the following technical solutions:
[0006] A photoresist spray coating method includes a temperature control part based on heat transfer and a motion process control part for a nozzle, and includes the following steps:
[0007] S1. Calculate the temperature increase ΔT during the heating process and the heat transfer coefficient K of the uncoated wafer. Combined with the known content, the calculation process is as follows:
[0008] K0=dQ / (T1-T0)dS;
[0009] S2. Through experiments, the above formula can be used to calculate K total:
[0010] K 总 =dQ / (T1-T x )dS
[0011] The total reciprocal of K is the reciprocal of the heat transfer coefficient of the wafer plus the reciprocal of the heat transfer coefficient of the coated photoresist film, that is:
[0012] 1 / K 总 =1 / K0+1 / K,
[0013] The value of the heat transfer coefficient K of the photoresist film is calculated accordingly;
[0014] S3. Through experiments, the film thickness and K of the photoresist are obtained. 总 The function records the entire spraying time TIM. During the time TIM, the film thickness changes from 0 to h, and the heat transfer coefficient changes from K0 to K 总 , where K 总 is a function of time TIM, and K is defined 总 =ɑ / TIM, through the above steps, the constant ɑ can be fitted;
[0015] According to the constant ɑ and time TIM, calculate T h , and set the temperature change from T0 to T h , realized by heating plate temperature controller;
[0016] S4. Send the wafer to be processed to the designated area, define the coordinates of the center point of the wafer as (Xi, Yi), Xi = R + σ, Yi = R + σ, Xi = Yi, the radius of the wafer is R, set the range and speed of the nozzle along the X-axis; set the range and speed of the nozzle along the Y-axis; define that after the spraying process in the X-axis direction is completed, the nozzle moves a distance a in the Y-axis direction, and after the spraying process in the X-axis direction is completed, the nozzle moves a distance a in the Y-axis direction, define the starting point as (0, 0), and then start the glue coating equipment;
[0017] S5. Carry out the gluing action in the following steps:
[0018] Step 1: The starting point is (0, 0), and the coordinate is (2R+2σ, 0) along the X-axis. Step 2: The starting point is (2R+2σ, 0), and the coordinate is (2R+2σ, a) along the Y-axis. Step 3: The coordinate is (0, a) at the moment of moving in the opposite direction of the X-axis. Step 4: The coordinate is (0, 2a) at the moment of moving in the Y-axis.
[0019] S6. Continue to perform the gluing action in sequence according to the steps until step m-3, travel a distance a along the negative direction of the X-axis, at which time the nozzle position coordinates are (2R+2σ-a, 2R+2σ); step m-2, travel along the Y-axis direction, travel a distance a, at which time the nozzle coordinates are (0, 2R+2σ-a); step m-1, travel a along the Y-axis direction, at which time the nozzle coordinates are (0, 2R+2σ); step m, travel 2R+2σ along the X-axis direction, at which time the nozzle coordinates are (2R+2σ, 2R+2σ), so far, the first period of lateral travel ends;
[0020] Continue the longitudinal movement part of the first cycle; the nozzle position is at (2R+2σ, 2R+2σ), the first step is to move a distance 2R+2σ along the negative direction of the Y axis, the second step is to move a along the negative direction of the X axis to the coordinate (2R+2σ-a, 0), the third step is to move 2R+2σ along the Y axis to the coordinate (2R+2σ-a, 2R+2σ), the fourth step is to move a along the negative direction of the X axis to the coordinate (2R+2σ-2a, 2R+2σ), repeat the above steps, m times, at this time the nozzle coordinates return to (0, 0), and the first cycle ends longitudinally;
[0021] At this point the first cycle ends and the second cycle begins;
[0022] S7. The starting point of the second cycle is designated as (σ, σ) and the above steps are repeated. The second cycle ends and the process distance is always 2R+2σ. The starting point of the third cycle is designated as (2σ, 2σ). The steps of the first cycle are repeated. The starting point of the nth cycle is designated as ((n+1)*σ, (n+1)*σ). The steps of the first cycle are repeated. The nth cycle ends and the entire spraying process ends, where n is the specific number of cycles required in the process. In the specific spraying process, the starting point of each cycle is different.
[0023] Preferably, the surface temperature T0 of the heating plate in S1 is obtained by a temperature sensor.
[0024] Preferably, the wafer surface area dS in S1 is directly measured by the staff, and the heat output dQ of the heating plate is obtained from the design value of the heating plate.
[0025] Preferably, during the spraying process, K 总 It is known that in order to achieve the goal, T x If it remains unchanged, dQ can be calculated, that is, the heat change of the heating plate, and the temperature change can be calculated. The purpose can be achieved by controlling the relevant parameters of the heating plate.
[0026] Preferably, in S3, ɑ is different for different process condition parameters, and needs to be calculated before each process adjustment, and the process parameters and ɑ remain unchanged during operation.
[0027] Preferably, in the gluing process, the heat of the electric heating plate is Q0 to Q i , keep Qi-Q0=dQ, dQ unchanged, then the surface temperature of the wafer is always T1 during the spraying process.
[0028] Preferably, in S1, K0 is the heat transfer coefficient of the uncoated wafer, T1 is the surface temperature of the wafer, T0 is the surface temperature of the heating plate, dS is the surface area of the wafer, and dQ is the heat output of the heating plate.
[0029] Preferably, in S2, when the electric heating plate temperature is T1, the film uniformity of the wafer surface is good and there are no bubbles. At this time, the temperature of the surface of the wafer coated with glue is Tx.
[0030] Preferably, the distance from point 0 to point Xi in S4 is R+σ, σ=a / n, and the distance from point Y0 to point Yi is also R+σ, σ=a / n, where n is the number of times the spraying cycle is repeated.
[0031] Preferably, step S5 is repeated for the mth time. During step m, the nozzle moves 2R+2σ along the X-axis direction, and the nozzle coordinates are (2R+2σ, 2R+2σ).
[0032] Technical effects and advantages of the present invention:
[0033] 1. A photoresist spray coating method provided by the present invention calculates the heat transfer coefficient K of an uncoated wafer, and uses this to test and obtain the appropriate temperature of the electric heating plate under different conditions, and puts this into use in a specific coating process, so that the wafer surface film can be uniform, good and free of bubbles. In combination with a covering spray coating action, the problem of poor uniformity can be solved, and bubbles can be reduced from being deposited on the surface of the photoresist film;
[0034] 2. The heat of the electric heating plate used for wafer heating comes from electrical energy. The heating system includes a temperature controller. The target temperature can be input and the heater can be started. The temperature change can be set in the temperature controller. For example, during the entire spraying cycle TIM, the heater temperature needs to be increased from T0 to T h End, just need to set in the temperature controller, the overall operation is simple and easy to implement. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with specific embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0036] Example 1
[0037] A photoresist spray coating method comprises the following steps:
[0038] In the specific glue coating process, the wafer can be set to any desired shape, and the specific shape of its surface is not limited. Here, taking the circle as an example, the temperature increase ΔT during the heating process is first calculated, and the heat transfer coefficient K of the uncoated wafer is calculated. The calculation process is as follows:
[0039] K0=dQ / (T1-T0)dS
[0040] The surface temperature T0 of the heating plate is obtained through the temperature sensor, the surface area dS of the wafer is directly measured by the staff, the heat output dQ of the heating plate is obtained from the design value of the electric heating plate, K0 is the heat transfer coefficient of the uncoated wafer, T1 is the surface temperature of the wafer, T0 is the surface temperature of the heating plate, dS is the surface area of the wafer, and dQ is the heat output of the heating plate. Through experiments, it can be concluded that when the temperature of the electric heating plate is T1, the film uniformity of the wafer surface is good and there are no bubbles. The heat of the electric heating plate used for wafer heating comes from electrical energy. The heating system includes a temperature controller, and the target temperature can be input to start the heater. The temperature change can be set in the temperature controller. For example, during the entire spraying cycle TIM, the heater temperature needs to be heated from T0 to T h End, just set it in the temperature controller. For example: the spraying cycle is 10 minutes; the heating plate temperature needs to be increased from 60 degrees to 80 degrees, then 10 minutes is 600 seconds, and the temperature rises by 20 degrees within 600 seconds, then setting the temperature to rise by 1 degree within 30 seconds can meet the demand, and the overall operation is simple and easy to implement.
[0041] At this time, the temperature of the coated wafer surface is Tx; according to the above formula, Ktotal can be calculated:
[0042] K 总 =dQ / (T1-T x )dS
[0043] The total reciprocal of K is the reciprocal of the heat transfer coefficient of the wafer plus the reciprocal of the heat transfer coefficient of the coated photoresist film, that is:
[0044] 1 / K 总 =1 / K0+1 / K,
[0045] The K value of the photoresist film is calculated based on this. Through experiments, the film thickness and K of the photoresist are obtained. 总 The function records the entire spraying time TIM. During the time TIM, the film thickness changes from 0 to h, and the heat transfer coefficient changes from K0 to K 总 , where K 总 is a function of time TIM, and K is defined 总=ɑ / TIM. Through the above steps, the constant ɑ can be fitted. It should be noted that ɑ is different for different process conditions and parameters. It needs to be calculated before each process adjustment. During operation, the process parameters and ɑ remain unchanged, and then the specific glue coating work is performed:
[0046] Set the temperature of the heating plate to rise from T0 to TIM within the time period TIM. h ,Afterwards, the nozzle movement part is executed;
[0047] S1. Send the wafer to be processed to the designated area, define the coordinates of the center point of the wafer as (Xi, Yi), and Xi = Yi, the radius of the wafer is R, set the range and speed of the nozzle along the X-axis; set the range and speed of the nozzle along the Y-axis; define that after the spraying process in the X-axis direction is completed, the nozzle moves a distance a in the Y-axis direction, and the distance a in the Y-axis direction after the spraying process in the X-axis direction is completed, define the starting point as (0, 0), the distance from 0 to Xi is R+σ, σ=a / n, the distance from Y0 to Yi is also R+σ, σ=a / n, n is the number of times the spraying cycle is repeated, and then start the glue coating equipment. During the glue coating process, the heat of the electric heating plate is Q0 to Q i , keep Qi-Q0=dQ, dQ unchanged, then, the surface temperature of the wafer is always T1 during the spraying process;
[0048] S2. Carry out the gluing action in the following steps:
[0049] Step 1: The starting point is (0, 0), and the nozzle moves along the X-axis to point A1, with coordinates (2R+2σ, 0); Step 2: The starting point is (2R+2σ, 0), and the nozzle moves along the Y-axis for a, and the coordinates are (2R+2σ, a); Step 3: The nozzle moves in the opposite direction of the X-axis, with a distance of R+2σ, and the coordinates are (0, a); Step 4: The nozzle moves along the Y-axis for a, and the coordinates are (0, 2a); If the steps are repeated for the mth time, in step m, the nozzle moves along the X-axis for 2R+2σ, and the nozzle coordinates are (2R+2σ, 2R+2σ);
[0050] S3. Continue to perform the gluing action in sequence according to the steps until step m-3, travel a distance a along the negative direction of the X-axis, at which time the nozzle position coordinates are (2R+2σ-a, 2R+2σ); step m-2, travel along the Y-axis direction, travel a distance a, at which time the nozzle coordinates are (0, 2R+2σ-a); step m-1, travel a along the Y-axis direction, at which time the nozzle coordinates are (0, 2R+2σ); step m, travel 2R+2σ along the X-axis direction, at which time the nozzle coordinates are (2R+2σ, 2R+2σ), so far, the first period of lateral travel ends;
[0051] Continue the longitudinal movement part of the first cycle; the nozzle position is at (2R+2σ, 2R+2σ), the first step is to move a distance 2R+2σ along the negative direction of the Y axis, the second step is to move a along the negative direction of the X axis to the coordinate (2R+2σ-a, 0), the third step is to move 2R+2σ along the Y axis to the coordinate (2R+2σ-a, 2R+2σ), the fourth step is to move a along the negative direction of the X axis to the coordinate (2R+2σ-2a, 2R+2σ), repeat the above steps, m times, at this time the nozzle coordinates return to (0, 0), and the first cycle ends longitudinally;
[0052] The first cycle ends and the second cycle begins
[0053] S4. The starting point of the second cycle is designated as (σ, σ) and the above steps are repeated. When the second cycle ends, the process distance is always 2R+2σ. The starting point of the third cycle is designated as (2σ, 2σ). Repeat the steps of the first cycle and continue working. For example, the process needs to be cycled 5 times, that is, it needs to be sprayed 5 times, a total of 5 cycles, then σ=a / 5, if a=1cm, then σ=0.2cm.
[0054] Finally, it should be noted that the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A photoresist spray coating method, characterized in that: It includes a temperature control part based on heat transfer and a motion process control part for the nozzle, including the following steps: S1. Calculate the temperature increase ΔT during the heating process and the heat transfer coefficient K of the uncoated wafer. Combined with the known content, the calculation process is as follows: K0=dQ / (T1-T0)dS; S2. Through experiments, the above formula can be used to calculate K 总 : K 总 =dQ / (T1-T x )dS K 总 The reciprocal is the reciprocal of the heat transfer coefficient of the wafer plus the reciprocal of the heat transfer coefficient of the photoresist film, that is: 1 / K 总 =1 / K0+1 / K, The value of the heat transfer coefficient K of the photoresist film is calculated accordingly; S3. Through experiments, the film thickness and K of the photoresist are obtained. 总 The function records the entire spraying time TIM. During the time TIM, the film thickness changes from 0 to h, and the heat transfer coefficient changes from K0 to K 总 , where K 总 is a function of time TIM, and K is defined 总 =ɑ / TIM, through the above steps, the constant ɑ can be fitted; According to the constant ɑ and time TIM, calculate T h , and set the temperature change from T0 to T h , realized by heating plate temperature controller; S4. Send the wafer to be processed to the designated area, define the coordinates of the center point of the wafer as (Xi, Yi), Xi = R + σ, Yi = R + σ, Xi = Yi, the radius of the wafer is R, set the range and speed of the nozzle along the X-axis; set the range and speed of the nozzle along the Y-axis; define that after the spraying process in the X-axis direction is completed, the nozzle moves a distance a in the Y-axis direction, and after the spraying process in the X-axis direction is completed, the nozzle moves a distance a in the Y-axis direction, define the starting point as (0, 0), and then start the glue coating equipment; S5. Carry out the gluing action in the following steps: Step 1: The starting point is (0, 0), and the coordinate is (2R+2σ, 0) along the X-axis. Step 2: The starting point is (2R+2σ, 0), and the coordinate is (2R+2σ, a) along the Y-axis. Step 3: The coordinate is (0, a) at the moment of moving in the opposite direction of the X-axis. Step 4: The coordinate is (0, 2a) at the moment of moving in the Y-axis. S6. Continue to perform the gluing action in sequence according to the steps until step m-3, travel a distance along the Y-axis direction, at which time the nozzle position coordinates are (2R+2σ-a, 2R+2σ); step m-2, travel along the X-axis direction, the travel distance is 2R+2σ, at which time the nozzle coordinates are (0, 2R+2σ-a); step m-1, travel a along the Y-axis direction, at which time the nozzle coordinates are (0, 2R+2σ); step m, travel 2R+2σ along the X-axis direction, at which time the nozzle coordinates are (2R+2σ, 2R+2σ), so far, the first period of lateral travel ends; Continue the longitudinal movement part of the first cycle; the nozzle position is at (2R+2σ, 2R+2σ), the first step is to move a distance 2R+2σ along the negative direction of the Y axis, the second step is to move a along the negative direction of the X axis to the coordinate (2R+2σ-a, 0), the third step is to move 2R+2σ along the Y axis to the coordinate (2R+2σ-a, 2R+2σ), the fourth step is to move a along the negative direction of the X axis to the coordinate (2R+2σ-2a, 2R+2σ), repeat the above steps, m times, at this time the nozzle coordinates return to (0, 0), and the first cycle ends longitudinally; At this point the first cycle ends and the second cycle begins; S7. The starting point of the second cycle is designated as (σ, σ) and the above steps are repeated. The second cycle ends and the process distance is always 2R+2σ. The starting point of the third cycle is designated as (2σ, 2σ). The steps of the first cycle are repeated. The starting point of the nth cycle is designated as ((n+1)*σ, (n+1)*σ). The steps of the first cycle are repeated. The nth cycle ends and the entire spraying process ends, where n is the specific number of cycles required in the process. In the specific spraying process, the starting point of each cycle is different.
2. A photoresist spray coating method according to claim 1, characterized in that: The surface temperature T0 of the heating plate in S1 is obtained by a temperature sensor.
3. A photoresist spray coating method according to claim 1, characterized in that: The wafer surface area dS in S1 is directly measured by the staff, and the heat output dQ of the heating plate is obtained from the design value of the heating plate.
4. A photoresist spray coating method according to claim 1, characterized in that: During the spraying process, K 总 It is known that in order to achieve the goal, T x If it remains unchanged, dQ can be calculated, that is, the heat change of the heating plate, and the temperature change can be calculated. The purpose can be achieved by controlling the relevant parameters of the heating plate.
5. A photoresist spray coating method according to claim 1, characterized in that: In S3, ɑ is different for different process condition parameters and needs to be calculated before each process adjustment. During operation, the process parameters and ɑ remain unchanged.
6. A photoresist spray coating method according to claim 1, characterized in that: In the gluing process, the heat of the electric heating plate is set to Q0 to Q i , keep Qi-Q0=dQ, dQ unchanged, then the surface temperature of the wafer is always T1 during the spraying process.
7. A photoresist spray coating method according to claim 1, characterized in that: In S1, K0 is the heat transfer coefficient of the uncoated wafer, T1 is the surface temperature of the wafer, T0 is the surface temperature of the heating plate, dS is the surface area of the wafer, and dQ is the heat output of the heating plate.
8. A photoresist spray coating method according to claim 1, characterized in that: It is obtained in S2 that when the temperature of the electric heating plate is T1, the film uniformity of the wafer surface is good and there are no bubbles. At this time, the temperature of the surface of the wafer coated with glue is Tx.
9. A photoresist spray coating method according to claim 1, characterized in that: The distance from point 0 to point Xi in S4 is R+σ, σ=a / n, and the distance from point Y0 to point Yi is also R+σ, σ=a / n, where n is the number of times the spraying cycle is repeated.
10. A photoresist spray coating method according to claim 1, characterized in that: The step S5 is repeated for the mth time. During the step m, the nozzle moves 2R+2σ along the X-axis direction. At this time, the nozzle coordinates are (2R+2σ, 2R+2σ).
Citation Information
Patent Citations
Spraying method and system of gluing machine
CN110209015A
Spraying method and spraying system of gluing machine
CN112619933A