PIN device and its manufacturing method, and display device

By arranging a patterned structure and an insulating pattern on the second electrode of the PIN device, the absorption and reflection of the optical signal are reduced and directly incident on the intrinsic layer, thereby solving the optical signal absorption problem of the PIN device and improving the photoelectric conversion rate and responsivity. Improved external quantum efficiency and signal-to-noise ratio.

CN114400268BActive Publication Date: 2024-10-01BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210039356.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-13
Publication Date
2024-10-01
Estimated Expiration
2042-01-13

AI Technical Summary

Technical Problem

The second electrode of the PIN device absorbs and reflects the optical signal, resulting in less light incident on the intrinsic layer and lowering the response and external quantum efficiency.

Method used

Design a PIN device with patterned electrodes, by arranging blank parts and island parts on the second electrode to reduce the absorption and reflection of optical signals, and form an insulating pattern on the side of the intrinsic layer away from the first electrode to ensure that the light The signal is directly incident on the intrinsic layer.

Benefits of technology

The photoelectric conversion rate and responsivity of the intrinsic layer are improved, and the external quantum efficiency, signal-to-noise ratio and sensitivity of the PIN device are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114400268B_ABST
    Figure CN114400268B_ABST
Patent Text Reader

Abstract

The embodiment of the present disclosure provides a PIN device and a method for preparing the same, and a display device, wherein the PIN device comprises a first electrode, a first doped layer, an intrinsic layer, a second doped layer, and a second electrode stacked in sequence on one side of the first electrode; the second electrode is a patterned electrode, and the patterned electrode comprises a plurality of blank portions, each blank portion being separated or connected by a connecting portion. The technical solution of the embodiment of the present disclosure can improve the photoelectric conversion rate and responsiveness of the intrinsic layer, and is helpful to improve the EQE and other performances of the PIN device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of display technology, and in particular to a PIN device and a manufacturing method thereof, and a display device. Background Art

[0002] At present, since part of the film layer of a PIN (a diode with a PIN structure) device absorbs light, the light incident on the intrinsic layer of the PIN device is reduced, thereby reducing the response of the intrinsic layer and the external quantum efficiency (EQE) of the PIN device. Summary of the invention

[0003] The embodiments of the present disclosure provide a PIN device and a method for manufacturing the same, and a display device to solve or alleviate one or more technical problems in the prior art.

[0004] As a first aspect of an embodiment of the present disclosure, an embodiment of the present disclosure provides a PIN device, including a first electrode, a first doped layer, an intrinsic layer, a second doped layer and a second electrode stacked in sequence on one side of the first electrode;

[0005] The second electrode is a patterned electrode, which includes a plurality of blank portions, and each blank portion is arranged separately or connected by a connecting portion.

[0006] In one embodiment, the patterned electrode also includes multiple island-shaped portions, and the orthographic projection of each island-shaped portion on the first electrode is located outside the orthographic projection of each blank portion on the first electrode, and the orthographic projection of each island-shaped portion and each blank portion on the first electrode covers the orthographic projection of the intrinsic layer on the first electrode.

[0007] In one embodiment, the second doped layer is a patterned doped layer, and the PIN device further includes an insulating pattern located on the side of the intrinsic layer facing away from the first electrode, the orthographic projection of the patterned doped layer on the first electrode overlaps with the orthographic projection of each island-shaped portion on the first electrode, and the orthographic projection of the insulating pattern on the first electrode overlaps with the orthographic projection of each blank portion on the first electrode.

[0008] In one embodiment, the orthographic projection of the connecting portion on the first electrode overlaps with the orthographic projection of the insulating pattern on the first electrode, the connecting portion is made of a transparent conductive material, and the insulating pattern is made of a transparent insulating material.

[0009] In one embodiment, the thickness of the second doping layer is in the range of

[0010] In one embodiment, the reflectivity of the first electrode is greater than the reflectivity of the aluminum-titanium alloy.

[0011] As a second aspect of the embodiments of the present disclosure, the embodiments of the present disclosure provide a PIN device, characterized in that it includes a first electrode, a first doped layer, an intrinsic layer, and a second doped layer stacked in sequence on one side of the first electrode; wherein the thickness of the second doped layer is in the range of

[0012] In one embodiment, the reflectivity of the first electrode is greater than the reflectivity of the aluminum-titanium alloy.

[0013] As a third aspect of an embodiment of the present disclosure, an embodiment of the present disclosure provides a display device, characterized in that it includes: a PIN device of any one of the above-mentioned implementation modes.

[0014] As a fourth aspect of the embodiments of the present disclosure, the embodiments of the present disclosure provide a method for preparing a PIN device, including:

[0015] forming a first doped layer, an intrinsic layer, a second doped layer and a second electrode in sequence on one side of the first electrode;

[0016] The second electrode is a patterned electrode, which includes a plurality of blank portions, and each blank portion is arranged separately or connected by a connecting portion.

[0017] In one embodiment, sequentially forming a second doping layer and a second electrode on one side of the first electrode includes:

[0018] An insulating pattern is formed on a side of the intrinsic layer away from the first electrode; the intrinsic layer is patterned to form a second doped layer on a side of the intrinsic layer away from the first electrode; the orthographic projection of the second doped layer on the first electrode does not overlap with the orthographic projection of the insulating pattern on the first electrode, and the orthographic projections of the second doped layer and the insulating pattern on the first electrode cover the orthographic projection of the intrinsic layer on the first electrode;

[0019] A second electrode is formed on the side of the second doped layer and the insulating pattern away from the first electrode; the second electrode includes a plurality of island portions and a connecting portion connecting the blank portions; the positive projection of each island portion on the first electrode overlaps with the positive projection of the second doped layer on the first electrode.

[0020] In one embodiment, forming a second doping layer on one side of the first electrode includes:

[0021] forming a doped region on a side of the intrinsic layer away from the first electrode;

[0022] The doped region is thinned to form a second doped layer; wherein the thickness of the doped region is greater than The thickness of the second doped layer is in the range of

[0023] In one embodiment, forming a second doping layer on one side of the first electrode includes:

[0024] forming an insulating layer on a side of the intrinsic layer facing away from the first electrode;

[0025] Performing a doping process on the intrinsic layer to form a doped region on a side of the intrinsic layer away from the first electrode;

[0026] The insulating layer is removed and the doped region is used as a second doped layer.

[0027] As a fifth aspect of the embodiments of the present disclosure, the embodiments of the present disclosure provide a method for preparing a PIN device, including:

[0028] forming a first doped layer, an intrinsic layer and a doped region in sequence on one side of the first electrode;

[0029] The doped region is thinned to form a second doped layer; wherein the thickness of the doped region is greater than The thickness of the second doped layer is in the range of

[0030] As a sixth aspect of the embodiments of the present disclosure, the embodiments of the present disclosure provide a method for preparing a PIN device, including:

[0031] forming a first doped layer, an intrinsic layer and an insulating layer in sequence on one side of the first electrode;

[0032] Performing a doping process on the intrinsic layer to form a doping region on a side of the intrinsic layer away from the first electrode;

[0033] The insulating layer is removed, and the doped region is used as the second doped layer; wherein the thickness of the second doped layer is in the range of

[0034] In the disclosed embodiment, the second electrode of the PIN device is set as a patterned electrode, so that a part of the light signal can be directly incident on the intrinsic layer from the blank part of the patterned electrode without being absorbed and reflected by the blank part, thereby reducing the loss of the second electrode to the absorption and reflection of the light signal, improving the photoelectric conversion rate and responsiveness of the intrinsic layer, and helping to improve the EQE and other performance of the PIN device.

[0035] The above summary is for illustrative purposes only and is not intended to be limiting in any way. In addition to the illustrative aspects, embodiments and features described above, further aspects, embodiments and features of the present disclosure will be readily apparent by reference to the accompanying drawings and the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] In the accompanying drawings, unless otherwise specified, the same reference numerals throughout the multiple drawings represent the same or similar parts or elements. These drawings are not necessarily drawn to scale. It should be understood that these drawings only depict some embodiments disclosed in accordance with the present disclosure and should not be regarded as limiting the scope of the present disclosure.

[0037] Figure 1A A schematic structural diagram of an active pixel sensor in the related art is shown.

[0038] Figure 1B Show Figure 1A Schematic diagram of the preparation process of PIN devices.

[0039] Figure 2 A schematic structural diagram of a PIN device according to a first embodiment of the present disclosure is shown.

[0040] Figure 3 A schematic structural diagram of a PIN device according to a second embodiment of the present disclosure is shown.

[0041] Figure 4 A schematic structural diagram of a PIN device according to a third embodiment of the present disclosure is shown.

[0042] Figure 5 A schematic structural diagram of a PIN device according to a fourth embodiment of the present disclosure is shown.

[0043] Figure 6 A schematic flow chart of a preparation method according to a second embodiment of the present disclosure is shown.

[0044] Figure 7 A schematic flow chart of a preparation method according to the third embodiment of the present disclosure is shown.

[0045] Figure 8 Another schematic flow chart of the preparation method according to the third embodiment of the present disclosure is shown. DETAILED DESCRIPTION

[0046] In the following, only some exemplary embodiments are briefly described. As those skilled in the art will appreciate, the described embodiments may be modified in various ways without departing from the spirit or scope of the present disclosure. Therefore, the drawings and descriptions are considered to be exemplary and non-restrictive in nature.

[0047] like Figure 1A and Figure 1BAs shown, in the related art, a PIN device 110 and a thin film transistor 120 are usually used to integrate an active pixel sensor 100 (APS) or a passive pixel sensor (PPS). In the process of preparing the PIN device 110, the first electrode 111 is connected to the gate of the thin film transistor 120 through a via hole, and a first doped layer 112, an intrinsic layer 113, a second doped layer 114 and a second electrode 115 are sequentially arranged on the side of the first electrode 111 away from the substrate. However, since the second electrode 115 of the PIN device 110 is basically arranged as a surface electrode, its orthographic projection on the first electrode 111 covers the orthographic projection of the intrinsic layer 113 on the first electrode 111, and the second electrode 115 absorbs the light signal, reduces the light signal incident on the intrinsic layer 113, reduces the photoelectric conversion rate and the responsiveness of the intrinsic layer 113, and thus reduces the performance of the PIN device 110.

[0048] In order to solve the above technical problems, an embodiment of the present disclosure provides a PIN device, and the PIN device of the embodiment of the present disclosure is described below with reference to the accompanying drawings.

[0049] Figure 2 A schematic structural diagram of a PIN device according to a first embodiment of the present disclosure is shown. Figure 3 FIG. 2 shows a schematic diagram of the structure of a PIN device according to a first embodiment of the present disclosure. Figure 2 and Figure 3 As shown, the PIN device 200 may include a first electrode 210 , a first doping layer 220 , an intrinsic layer 230 , a second doping layer 240 , and a second electrode 250 stacked in sequence on one side of the first electrode 210 .

[0050] The first doping layer 220 and the second doping layer 240 are both heavily doped layers, and the doping type of the first doping layer 220 is opposite to the doping type of the second doping layer 240. For example, the first doping layer 220 may be a P-type semiconductor layer, and the second doping layer 240 may be an N-type semiconductor layer; or, the first doping layer 220 may be an N-type semiconductor layer, and the second doping layer 240 may be a P-type semiconductor layer.

[0051] The second electrode 250 is a patterned electrode, and the patterned electrode includes a plurality of blank portions 251, and each blank portion 251 is separated or connected by a connecting portion 252. It should be noted that, in the case where the PIN device 200 of the embodiment of the present disclosure is arranged on the driving backplane in a manner perpendicular to the driving backplane, the first electrode 210 can be regarded as a bottom electrode, and the second electrode 250 can be regarded as a top electrode. Exemplarily, the plurality of blank portions 251 can be arranged in an array. When the light signal is incident on the PIN device 200, a portion of the light signal can be directly incident on the intrinsic layer 230 from the blank portion 251 without being absorbed and reflected by the blank portion 251, thereby reducing the loss of the light signal by the second electrode 250, increasing the transmittance of the light signal, and being conducive to improving the photoelectric conversion rate and responsiveness of the intrinsic layer 230, and improving the light-to-dark current ratio (i.e., the ratio of the photocurrent to the dark current) of the PIN device 200, thereby further helping to improve the external quantum efficiency (EQE), signal-to-noise ratio, sensitivity and other performance of the PIN device 200.

[0052] In another example, the material of the connecting portion 252 can be a transparent conductive material such as indium tin oxide (ITO). Connecting the adjacent blank portions 251 through the connecting portion 252 helps to increase the conductive area of ​​the patterned electrode, thereby improving the conductive performance of the patterned electrode. In addition, connecting the adjacent blank portions 251 through the connecting portion 252 also helps to improve the firmness of the patterned electrode.

[0053] According to the PIN device 200 of the embodiment of the present disclosure, the second electrode 250 of the PIN device 200 is set as a patterned electrode, which allows a portion of the optical signal to be directly incident on the intrinsic layer 230 from the blank portion 251 of the patterned electrode without being absorbed and reflected by the blank portion 251, thereby reducing the absorption and reflection losses of the optical signal by the second electrode 250, improving the photoelectric conversion rate and responsiveness of the intrinsic layer 230, and helping to improve the EQE and other performance of the PIN device 200.

[0054] In one embodiment, if Figure 2 and Figure 3As shown, the patterned electrode further includes a plurality of island portions 253, the orthographic projection of each island portion 253 on the first electrode 210 is located outside the orthographic projection of each blank portion 251 on the first electrode 210, and the orthographic projection of each island portion 253 and each blank portion 251 on the first electrode 210 covers the orthographic projection of the intrinsic layer 230 on the first electrode 210. Such a structure can ensure that the optical signal is incident from the island portion 253 or the blank portion 251 to the intrinsic layer of the PIN device 200, and when the optical signal is incident, a part of the optical signal is directly incident from the blank portion 251 to the intrinsic layer 230 without being absorbed and reflected by the blank portion 251, and another part of the optical signal is incident on the intrinsic layer 230 through the island portion 253. In one example, the material of the island portion 253 is set to a transparent conductive material such as ITO, which can increase the transmittance of the island portion 253 and reduce the absorption and reflection loss of the light signal by the island portion 253, so that more light signals can pass through the island portion 253 and enter the intrinsic layer 230, which is beneficial to improving the photoelectric conversion rate and responsiveness of the intrinsic layer 230.

[0055] In one embodiment, if Figure 3 As shown, the PIN device 200 is different from the PIN device 200 of the first embodiment in that the second doping layer 240 is a patterned doping layer, and the PIN device 200 further includes an insulating pattern 310 located on the side of the intrinsic layer 230 away from the first electrode 210. The orthographic projection of the patterned doping layer on the first electrode 210 overlaps with the orthographic projection of each island-shaped portion 253 on the first electrode 210, so that a PIN structure is formed between each island-shaped portion 253 and the first electrode 210. The orthographic projection of the insulating pattern 310 on the first electrode 210 overlaps with the orthographic projection of each blank portion 251 on the first electrode 210.

[0056] For example, the material of the insulating pattern 310 may be silicon nitride (SiN x ) and other transparent insulating materials. By setting a transparent insulating pattern 310 on the side of the intrinsic layer 230 away from the first electrode 210, and setting the positive projection of the insulating pattern 310 on the first electrode 210 to overlap with the positive projection of each blank portion 251 on the first electrode 210, the optical signal incident on the intrinsic layer 230 through the insulating pattern 310 can avoid the patterned doped layer, reducing the absorption and reflection loss of the optical signal by the patterned doped layer, thereby helping to improve the photoelectric conversion rate and responsiveness of the intrinsic layer 230, and improving the EQE and other characteristics of the PIN device 200. In addition, setting a transparent insulating pattern 310 can also prevent the island portion 253 from being electrically connected to the intrinsic layer 230.

[0057] In one embodiment, if Figure 3As shown, the orthographic projection of the connecting portion 252 on the first electrode 210 overlaps with the orthographic projection of the insulating pattern 310 on the first electrode 210, the material of the connecting portion 252 is a transparent conductive material, and the material of the insulating pattern 310 is a transparent insulating material. Exemplarily, the connecting portion 252 and the island portion 253 are made of the same material, for example, the connecting portion 252 and the island portion 253 can both be made of a transparent conductive material such as indium tin oxide (ITO). By providing the connecting portion 252 between adjacent island portions 253, the firmness of the patterned electrode and the good electrical connection characteristics can be effectively improved.

[0058] In one embodiment, if Figure 2 As shown, the thickness range of the second doping layer 240 is For example, the thickness of the second doping layer 240 may be For example, the thickness of the second doping layer 240 can be Any value in .

[0059] like Figure 1A and Figure 1B As shown, in the related art, due to the limitation of the minimum ion implantation energy, the thickness of the second doping layer 114 is usually more than As a result, the second doping layer 114 absorbs a large amount of optical signals, especially a large amount of short-wave optical signals, thereby reducing the optical signals incident on the intrinsic layer 113. It can effectively reduce its absorption of light signals, improve the photoelectric conversion rate and responsiveness of the intrinsic layer 230, and thus improve the EQE, signal-to-noise ratio, sensitivity and other characteristics of the PIN device 200. In addition, when the PIN device 200 is used to integrate a photosensitive component (such as a fingerprint recognition sensor) with an amplifying thin film transistor, it also helps to increase the gain of the photosensitive component.

[0060] In one embodiment, if Figure 2 and Figure 3 As shown, the reflectivity of the first electrode 210 is greater than that of the titanium aluminum alloy. Exemplarily, the material of the first electrode 210 can be ITO / Ag / ITO composite conductive material, or other types of materials. The present disclosure does not limit the material of the first electrode 210.

[0061] like Figure 1A and Figure 1BAs shown, in the related art, the material of the first electrode 111 is usually selected from materials with low reflectivity such as titanium aluminum alloy, such as Ti / Al / Ti composite conductive material. When the light signal passes through the intrinsic layer 113 and is incident on the first electrode 111, the first electrode 111 absorbs part of the light signal, reducing the light signal reflected into the intrinsic layer 113, and reducing the photoelectric conversion rate of the intrinsic layer 113. The above scheme of the embodiment of the present disclosure selects a material with a reflectivity greater than that of titanium aluminum alloy as the material of the first electrode 210, so that the first electrode 210 can reflect more light signals toward the intrinsic layer 230, which is beneficial to improve the photoelectric conversion rate and responsiveness of the intrinsic layer 230, improve the light-to-dark current ratio of the PIN device 200, and thus improve the EQE, signal-to-noise ratio, sensitivity and other performances of the PIN device 200.

[0062] like Figure 1A and Figure 1B As shown, in the related art, due to the minimum ion implantation energy limitation, for example, the minimum ion implantation energy is 8Kev, the thickness of the second doping layer 114 is usually greater than The second doped layer 114 has a large thickness and will absorb a large amount of optical signals. Especially when the second doped layer 114 is a P-type layer, the second doped layer 114 will absorb a large amount of short-wave optical signals, reducing the optical signals incident on the intrinsic layer 113, and reducing the photoelectric conversion rate and responsiveness of the intrinsic layer 113, resulting in low EQE, signal-to-noise ratio and sensitivity of the PIN device 100.

[0063] In order to solve the above technical problems, the embodiments of the present disclosure also provide another PIN device.

[0064] Figure 4 FIG. 2 shows a schematic diagram of the structure of a PIN device according to a third embodiment of the present disclosure. Figure 4 As shown, the PIN device 200 may include: a first electrode 210, a first doping layer 220, an intrinsic layer 230 and a second doping layer 240 stacked in sequence on one side of the first electrode 210; wherein the thickness of the second doping layer 240 is in the range of

[0065] For example, the thickness of the second doping layer 240 may be For example, the thickness of the second doping layer 240 can be Any value in .

[0066] The above solution sets the thickness range of the second doping layer 240 to It can effectively reduce its absorption of light signals, improve the photoelectric conversion rate and responsiveness of the intrinsic layer 230, and thus improve the EQE, signal-to-noise ratio, sensitivity and other characteristics of the PIN device 200. In addition, when the PIN device 200 is used to integrate a photosensitive component with an amplifying thin film transistor, it also helps to increase the gain of the photosensitive component.

[0067] In one embodiment, the reflectivity of the first electrode 210 is greater than the reflectivity of the titanium aluminum alloy. Exemplarily, the material of the first electrode 210 can be an ITO / Ag / ITO composite conductive material, or other types of materials. The present embodiment does not limit the material of the first electrode 210. In the related art, the material of the first electrode 210 is usually selected from materials with low reflectivity such as titanium aluminum alloy, such as Ti / Al / Ti composite conductive material. When the light signal passes through the intrinsic layer 230 and is incident on the first electrode 210, the first electrode 210 absorbs part of the light signal, reduces the light signal reflected into the intrinsic layer 230, and reduces the photoelectric conversion rate of the intrinsic layer 230. The above scheme of the embodiment of the present disclosure selects a material with a reflectivity greater than that of the titanium aluminum alloy as the material of the first electrode 210, so that the first electrode 210 can reflect more light signals toward the intrinsic layer 230, which is conducive to improving the photoelectric conversion rate and responsiveness of the intrinsic layer 230, improving the light-to-dark current ratio of the PIN device 200, and thus improving the EQE, signal-to-noise ratio, sensitivity and other performances of the PIN device 200.

[0068] It should be noted that the third embodiment of the present disclosure does not limit the second electrode disposed on the side of the second doping layer 240 away from the first electrode 210 in the PIN device 200, and it can be a surface electrode or a patterned electrode. Figure 5 The structure in which the second electrode 250 is a surface electrode is shown.

[0069] The present disclosure also provides a display device, including: the PIN device 200 of any of the above embodiments. Exemplarily, the display device can be a display panel, or a display product with a display panel, such as a smart phone, a tablet computer, a display screen, a smart wearable device, an electronic photo frame, etc.

[0070] The present disclosure also provides a method for preparing a PIN device, please refer to Figure 2 , the preparation method may include:

[0071] Step S610, forming a first doping layer 220 and an intrinsic layer 230 in sequence on one side of the first electrode 210;

[0072] Step S620, heavily doping the intrinsic layer 230 by implanting ions to form a second doping layer 240;

[0073] Step S630, forming a second electrode 250 on a side of the second doping layer 240 away from the first electrode 210. Exemplarily, step S630 may include: forming a conductive film on a side of the second doping layer 240 away from the first electrode 210 by a coating process; performing patterning treatments such as coating, exposing, developing, and etching on the conductive film to form the second electrode 250; wherein the second electrode 250 is a patterned electrode, and the patterned electrode includes a plurality of blank portions 251, and each blank portion 251 is separately arranged or connected by a connecting portion 252.

[0074] In one implementation, please refer to Figure 6 and Figure 3 , step S620 may include:

[0075] Step S621, forming an insulating pattern 310 on the side of the intrinsic layer 230 away from the first electrode 210. For example, step S621 may include: forming an insulating film on the side of the intrinsic layer 230 away from the first electrode 210 by using a coating process; performing patterning treatments such as coating, exposing, developing, and etching on the insulating film to form an insulating pattern 310, wherein the insulating pattern 310 includes a plurality of hollow portions (not marked in the figure).

[0076] Step S622: patterning the intrinsic layer 230 to form a second doped layer 240 on the side of the intrinsic layer 230 away from the first electrode 210; the orthographic projection of the second doped layer 240 on the first electrode 210 overlaps with the orthographic projection of each island portion 253 on the first electrode 210. For example, Figure 6 As shown, step S622 may include: coating a photoresist 610 on a side of the insulating pattern 310 away from the first electrode 210, so that the intrinsic layer 230 is exposed from a plurality of hollowed-out portions; heavily doping the intrinsic layer 230 by implanting ions and removing the photoresist 610, to form a patterned second doping layer 240, i.e., a patterned doping layer. The orthographic projections of the insulating pattern 310 on the first electrode 210 do not overlap, and the orthographic projections of the second doping layer 240 and the insulating pattern 310 on the first electrode 210 cover the orthographic projection of the intrinsic layer 230 on the first electrode 210.

[0077] Correspondingly, such as Figure 3 As shown, step S630 may include: forming a second electrode 250 on the side of the second doping layer 240 away from the first electrode 210 using a coating process; the second electrode 250 includes a connecting portion 252 connecting the blank portion 251 and a plurality of island portions 253, and the orthographic projection of each island portion 253 on the first electrode 210 overlaps with the orthographic projection of the second doping layer 240 on the first electrode 210.

[0078] In an optional implementation, please refer to Figure 7 and Figure 4 Step S620 may include: heavily doping the intrinsic layer 230 with ions to form a doping region 710 on a side of the intrinsic layer 230 away from the first electrode 210; etching the side of the doping region 710 away from the first electrode 210 with HF acid to reduce the thickness of the doping region 710 to form a second doping layer 240; wherein the thickness of the doping region 710 is greater than The thickness of the second doping layer 240 is in the range of It should be noted that other thinning processes commonly used in the art may also be used to thin the doped region 710 , such as other types of etching processes, polishing, etc. The embodiment of the present disclosure does not limit the thinning process of the doped region 710 .

[0079] In another optional implementation, please refer to Figure 8 and Figure 4 Step S620 may include: forming an insulating layer 810 on a side of the intrinsic layer 230 away from the first electrode 210 by using a coating process. The insulating layer 810 may be made of silicon nitride (SiN x ) or other transparent materials that are easy to etch; perform ion implantation and heavy doping on the intrinsic layer 230 to form a doping region 710 on the side of the intrinsic layer 230 that is away from the first electrode 210; use HF acid to etch away the insulating layer 810, and use the remaining doping region 710 as the second doping layer 240. In this embodiment, by forming the insulating layer 810 on the side of the intrinsic layer 230 that is away from the first electrode 210, and then performing ion implantation and heavy doping on the intrinsic layer 230, the insulating layer 810 can be used to buffer the ion implantation energy, reduce the doping depth of the ion implantation and heavy doping in the intrinsic layer 230, and thus form a second doping layer 240 with a relatively thin thickness on the intrinsic layer 230. In addition, by providing the insulating layer 810, it is more helpful to flexibly control the doping depth in the intrinsic layer 230, and because silicon nitride is easy to be etched and removed, it is also beneficial to improve the preparation efficiency.

[0080] The present disclosure also provides another method for preparing a PIN device. Figure 7 and Figure 4 , the preparation method may include:

[0081] Step S710: using a coating process to sequentially form a first doped layer 220, an intrinsic layer 230 and a doped region 710 on one side of the first electrode 210. The formation of the intrinsic layer 230 and the doped region 710 can refer to the above embodiments and will not be described in detail here.

[0082] Step S720: Thinning the doped region 710 to form a second doped layer 240; wherein the thickness of the doped region 710 is greater than The thickness of the second doping layer 240 is in the range of It should be noted that step S720 may also refer to the above embodiments and will not be described in detail here.

[0083] like Figure 1A and Figure 1B As shown, the related art is limited by the minimum ion implantation energy, and the thickness of the second doping layer 114 formed directly is usually greater than The second doping layer 114 absorbs a large amount of light signals, causing light signal loss and reducing the light signals incident to the intrinsic layer 113. In the above scheme, the second doping layer 240 is formed by first forming the doping region 710 and then thinning the doping region 710. The second doping layer 240 formed in this way is thinner, which reduces the absorption loss of the light signal and helps to increase the light signal incident to the intrinsic layer 230, thereby improving the photoelectric conversion rate and responsiveness of the intrinsic layer 230. In addition, the above scheme first forms the doping region 710 and then directly thins the doping region 710, which simplifies the preparation process.

[0084] The present disclosure also provides another method for preparing a PIN device. Figure 8 and Figure 4 , the preparation method may include:

[0085] Step S810: forming a first doped layer 220, an intrinsic layer 230 and an insulating layer 810 in sequence on one side of the first electrode 210; wherein the insulating layer 810 may be made of silicon nitride (SiN x ) and other transparent insulating materials.

[0086] Step S820 , performing a doping process on the intrinsic layer 230 , and forming a doped region 710 on a side of the intrinsic layer 230 away from the first electrode 210 .

[0087] Step S830, removing the insulating layer 810, and using the doped region 710 as the second doped layer 240; wherein the thickness of the second doped layer 240 is in the range of

[0088] It can be understood that step S820 and step S830 can refer to the previous embodiments and will not be described in detail here.

[0089] In the above solution, by forming an insulating layer 810 on the side of the intrinsic layer 230 away from the first electrode 210, and then performing ion implantation heavy doping treatment on the intrinsic layer 230, the insulating layer 810 can be used to buffer the ion implantation energy, reduce the ion implantation depth in the intrinsic layer 230, and thus form a thinner second doping layer 240 on the intrinsic layer 230. In addition, since silicon nitride is easy to be etched and removed, it helps to improve the preparation efficiency.

[0090] In the description of this specification, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present disclosure.

[0091] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present disclosure, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0092] In the present disclosure, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to specific circumstances.

[0093] In the present disclosure, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being “above”, “above”, and “above” a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being “below”, “below”, and “below” a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0094] The disclosure above provides many different embodiments or examples to realize different structures of the present disclosure. In order to simplify the disclosure of the present disclosure, the components and settings of specific examples are described above. Of course, they are only examples, and the purpose is not to limit the present disclosure. In addition, the present disclosure can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, and does not itself indicate the relationship between the various embodiments and / or settings discussed.

[0095] The above is only a specific implementation of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any technician familiar with the technical field can easily think of various changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure. Therefore, the protection scope of the present disclosure should be based on the protection scope of the claims.

Claims

1. A PIN device, characterized in that: It comprises a first electrode, a first doped layer, an intrinsic layer, a second doped layer and a second electrode which are sequentially stacked on one side of the first electrode; Among them, the second electrode is a patterned electrode, and the patterned electrode includes a plurality of blank parts, each of which is separated or connected by a connecting part; the patterned electrode also includes a plurality of island parts, and the orthogonal projection of each of the island parts on the first electrode is located outside the orthogonal projection of each of the blank parts on the first electrode, and the orthogonal projection of each of the island parts and each of the blank parts on the first electrode covers the orthogonal projection of the intrinsic layer on the first electrode; the second doped layer is a patterned doped layer, and the PIN device also includes an insulating pattern located on the side of the intrinsic layer away from the first electrode, the orthogonal projection of the patterned doped layer on the first electrode overlaps with the orthogonal projection of each of the island parts on the first electrode, and the orthogonal projection of the insulating pattern on the first electrode overlaps with the orthogonal projection of each of the blank parts on the first electrode; the thickness range of the second doped layer is 2. The PIN device according to claim 1, characterized in that: The orthographic projection of the connecting portion on the first electrode overlaps with the orthographic projection of the insulating pattern on the first electrode. The connecting portion is made of a transparent conductive material, and the insulating pattern is made of a transparent insulating material.

3. The PIN device according to claim 1, characterized in that: The reflectivity of the first electrode is greater than the reflectivity of the aluminum-titanium alloy.

4. A display device, characterized in that: include: The PIN device according to any one of claims 1 to 3.

5. A method for preparing a PIN device, characterized in that: include: forming a first doped layer, an intrinsic layer, a second doped layer and a second electrode in sequence on one side of the first electrode; Wherein, the second electrode is a patterned electrode, and the patterned electrode includes a plurality of blank portions, and each of the blank portions is separately arranged or connected by a connecting portion; Sequentially forming a second doped layer and a second electrode on one side of the first electrode comprises: forming an insulating pattern on a side of the intrinsic layer away from the first electrode; patterning the intrinsic layer to form a second doped layer on a side of the intrinsic layer away from the first electrode; an orthographic projection of the second doped layer on the first electrode does not overlap with an orthographic projection of the insulating pattern on the first electrode, and the orthographic projections of the second doped layer and the insulating pattern on the first electrode cover the orthographic projection of the intrinsic layer on the first electrode; forming a second electrode on a side of the second doped layer and the insulating pattern away from the first electrode; the second electrode comprises a plurality of island-shaped portions and the connecting portion connecting the blank portions; an orthographic projection of each of the island-shaped portions on the first electrode overlaps with an orthographic projection of the second doped layer on the first electrode; The second doping layer is formed on one side of the first electrode, comprising: forming a doping region on a side of the intrinsic layer away from the first electrode, thinning the doping region to form the second doping layer, wherein the thickness of the doping region is greater than The thickness of the second doping layer is in the range of Alternatively, the second doped layer is formed on one side of the first electrode, including: forming an insulating layer on the side of the intrinsic layer away from the first electrode; performing doping treatment on the intrinsic layer to form a doped region on the side of the intrinsic layer away from the first electrode; removing the insulating layer and using the doped region as the second doped layer.