Method for manufacturing circuit board, circuit board and electronic device
By using a copper-plated iron-nickel alloy plate as a metal sandwich layer in the circuit board, and forming a multi-layer structure through drilling and lamination processes, the expansion problem of the circuit board caused by differences in material properties is solved, and the strength of the circuit board is enhanced and applicable on the power supply or ground plane.
Patent Information
- Application Number
- CN202110214253.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-02-25
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-02-25
AI Technical Summary
In traditional circuit boards, stress remains due to differences in material properties during processes such as lamination, mechanical cutting, and wet treatment, causing the copper-clad board to expand, contract, or deform irregularly in the X and Y directions, affecting the use effect.
The copper-plated iron-nickel alloy plate is used as the metal sandwich layer of the high-end multi-layer board. The multi-layer circuit board is formed through drilling, laying solidified sheets and metal layers, and a lamination process to reduce expansion and enhance strength.
It effectively reduces the expansion of the circuit board in the X and Y directions, enhances the strength of the circuit board, and can be used as a power layer or ground layer to improve the stability and performance of the circuit board.
Smart Images

Figure CN114980573B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of circuit boards, and in particular to a method for manufacturing a circuit board, a circuit board, and an electronic device. Background Art
[0002] In order to realize the power layer or ground layer function of the circuit board, the traditional process is to use one of the copper clad laminates (such as the core2 below) to etch the pattern on both sides, and then laminate it with other layers in turn, and finally drill, electroplate, and pattern the outer layer. These copper clad laminates are composed of copper foil, resin, glass cloth and other materials, and their physical and chemical properties are different. During the lamination, mechanical cutting, wet treatment and other processes, due to the combined influence of pressure, temperature and humidity, residual stress will be generated, causing the copper clad laminate to expand, shrink or deform irregularly in the X and Y directions, thereby affecting the use of customer terminals. Summary of the invention
[0003] The present application provides a method for manufacturing a circuit board, a circuit board and an electronic device, which solve the problem that a copper-clad laminate composed of materials such as a metal layer, a resin, and a glass cloth has different physical and chemical properties, and that residual stress is generated during processes such as pressing, mechanical cutting, and wet treatment due to the combined influence of pressure and temperature / humidity, resulting in expansion, contraction, or irregular deformation of the copper-clad laminate in the X and Y directions.
[0004] In order to solve the above technical problems, a technical solution adopted in the present application is: to provide a method for manufacturing a circuit board, which comprises: drilling holes at preset positions of at least one copper-plated iron-nickel alloy plate; laying a first semi-cured sheet on both sides of the copper-plated iron-nickel alloy plate; laying a copper-clad laminate on the surface of the first semi-cured sheet away from the copper-plated iron-nickel alloy plate; laying a second semi-cured sheet on the surface of the copper-clad laminate away from the copper-plated iron-nickel alloy plate; laying a metal layer on the surface of the second semi-cured sheet away from the copper-clad laminate; and laminating the first semi-cured sheet, the copper-clad laminate, the second semi-cured sheet, and the metal layer on the two sides of the copper-plated iron-nickel alloy plate after drilling through a lamination process to form a multi-layer circuit board.
[0005] Wherein, after the step of drilling holes at a preset position of at least one copper-plated iron-nickel alloy plate, the method further includes: roughening the surfaces of both sides of the copper-plated iron-nickel alloy plate.
[0006] Among them, the step of laminating the first semi-cured sheet, the copper-clad laminate, the second semi-cured sheet, and the metal layer on both side surfaces of the drilled copper-plated iron-nickel alloy plate to form a multi-layer circuit board through a laminating process specifically includes: laminating the first semi-cured sheet and the copper-clad laminate on both side surfaces of the copper-plated iron-nickel alloy plate through a laminating process; laminating the metal layer and the second semi-cured sheet on the copper-clad laminate through a laminating process to add layers to form a multi-layer circuit board.
[0007] Among them, after the step of laminating the first semi-cured sheet, the copper-clad board, the second semi-cured sheet, and the metal layer on the two side surfaces of the drilled copper-iron-nickel alloy plate to form a multi-layer circuit board through a lamination process, it also includes: drilling the multi-layer circuit board to form via holes at corresponding preset positions of the multi-layer circuit board; electroplating the multi-layer circuit board with the via holes to metallize the via holes.
[0008] The step of electroplating the multilayer circuit board with the via holes to metallize the via holes also includes: making outer layer circuits on the metal layer of the multilayer circuit board.
[0009] Among them, there are two copper-iron-nickel alloy plates, and the metal layer includes a first metal layer and a second metal layer; the step of drilling holes at the preset position of at least one copper-iron-nickel alloy plate includes: drilling holes at the preset positions of the two copper-iron-nickel alloy plates respectively; the step of laminating the first semi-cured sheet, the copper-clad plate, the second semi-cured sheet, and the metal layer on the two side surfaces of the copper-iron-nickel alloy plates after drilling through a laminating process to form a multi-layer circuit board includes: laminating the first semi-cured sheet, the first metal layer, the second semi-cured sheet, and the copper-iron-nickel alloy plate on the two side surfaces of the copper-clad plate respectively through a laminating process; laminating the second metal layer and the second semi-cured sheet on the surface of the copper-iron-nickel alloy plate away from the copper-clad plate to add layers to form a multi-layer circuit board.
[0010] Among them, after the step of laminating the first semi-cured sheet, the copper-clad board, the second semi-cured sheet, and the metal layer on the two side surfaces of the drilled copper-iron-nickel alloy plate to form a multi-layer circuit board through a lamination process, it also includes: drilling the multi-layer circuit board to form via holes at corresponding preset positions of the multi-layer circuit board; electroplating the multi-layer circuit board with the via holes to metallize the via holes.
[0011] Among them, circuit patterns are etched on both sides of the copper clad board.
[0012] In order to solve the above technical problems, another technical solution adopted in the present application is: to provide a circuit board, which adopts any of the circuit board manufacturing methods as described above.
[0013] In order to solve the above technical problem, another technical solution adopted by the present application is: to provide an electronic device, which includes the circuit board as mentioned above.
[0014] The beneficial effects of the present application are as follows: Different from the prior art, the present application provides a method for manufacturing a circuit board, the manufacturing method comprising: drilling holes at a preset position of at least one copper-iron-nickel alloy plate; laying a first prepreg on both sides of the copper-iron-nickel alloy plate; laying a copper-clad plate on the surface of the first prepreg away from the copper-iron-nickel alloy plate; laying a second prepreg on the surface of the copper-clad plate away from the copper-iron-nickel alloy plate; laying a metal layer on the surface of the second prepreg away from the copper-clad plate; laminating the first prepreg, the copper-clad plate, the second prepreg, and the metal layer on both sides of the copper-iron-nickel alloy plate after drilling through a lamination process to form a multi-layer circuit board. The present application uses a copper-iron-nickel alloy plate as a metal sandwich layer of a high-order multi-layer board to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as a power layer or ground layer of the circuit board. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those of ordinary skill in the art, other drawings can be obtained based on these drawings without creative work, among which:
[0016] Figure 1 It is a flow chart of a first embodiment of a method for manufacturing a circuit board provided by the present application;
[0017] Figure 2 is a flow chart of a second embodiment of a method for manufacturing a circuit board provided by the present application;
[0018] Figure 3 is a structural schematic diagram of a first embodiment of a circuit board provided by the present application;
[0019] Figure 4 It is a schematic structural diagram of the second embodiment of the circuit board provided in this application. DETAILED DESCRIPTION
[0020] In order to make the technical problems solved by the present application, the technical solutions adopted and the technical effects achieved more clearly, the technical solutions of the embodiments of the present application will be further described in detail below with reference to the accompanying drawings.
[0021] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0022] See also Figure 1 , Figure 1 It is a flow chart of the first embodiment of the method for manufacturing a circuit board provided in the present application.
[0023] Step S101: drilling holes at preset positions of at least one copper-plated iron-nickel alloy plate.
[0024] In this embodiment, the copper-iron-nickel alloy plate (Copper Invar Copper, CIC) includes several layers, wherein the middle layer Invar is an alloy containing 36% nickel, 63.8% iron, and other elements such as carbon and manganese, and its thermal expansion coefficient is extremely low at -200℃~+200℃, and its expansion coefficient is <1.0ppm / ℃ under the manufacturing process environment of the circuit board.
[0025] In this embodiment, a through hole is opened at a preset position of at least one copper-iron-nickel alloy plate. Furthermore, the circuit layers on both sides of the copper-iron-nickel alloy plate can be connected through the through hole, so that the copper-iron-nickel alloy plate can be used as a ground layer or a power layer.
[0026] Step S102: laying a first prepreg on both sides of the copper-iron-nickel alloy plate.
[0027] In this embodiment, a first semi-cured sheet is laid on both sides of the copper-iron-nickel alloy plate after drilling, wherein through holes are opened at preset positions of the copper-iron-nickel alloy plate. The first semi-cured sheet will soften under heating and pressure to fill the through holes at preset positions of the copper-iron-nickel alloy plate.
[0028] Step S103: Laying the copper clad laminate on the surface of the first prepreg away from the copper-iron-nickel alloy plate.
[0029] In this embodiment, after the first prepreg is laid on both sides of the copper-plated iron-nickel alloy plate, the copper-clad laminate is laid on the side surface of the first prepreg away from the copper-plated iron-nickel alloy plate, and the copper-clad laminate and the copper-plated iron-nickel alloy plate are combined together by the first prepreg. The copper-clad laminate includes a core plate and a copper layer pressed on both sides of the core plate. Optionally, before pressing, the copper-clad laminate is exposed, developed and etched to form a circuit pattern on the copper layer on both sides of the core plate of the copper-clad laminate, so that the copper layer is made into a circuit layer, so that the copper layer on both sides of the copper-clad laminate plays the role of a power layer and a signal layer.
[0030] Optionally, the copper clad laminate and the first prepreg are pressed onto both side surfaces of the copper-plated iron-nickel alloy plate by a pressing process. During the pressing process, the first prepreg will soften and fill the through holes at preset positions of the copper-plated iron-nickel alloy plate.
[0031] Step S104: laying a second prepreg on the surface of the copper clad laminate away from the copper-iron-nickel alloy plate.
[0032] In this embodiment, a second prepreg is laid on the surface of the copper clad laminate away from the copper-iron-nickel alloy plate, so that a build-up layer is performed through the second prepreg.
[0033] Step S105: Laying a metal layer on the surface of the second prepreg away from the copper clad laminate.
[0034] In this embodiment, a metal layer is laid on the surface of the second prepreg away from the copper clad laminate, and the metal layer and the copper clad laminate are combined together through the second prepreg to achieve a build-up layer arrangement. The metal layer can be used as a signal layer of a multilayer board.
[0035] Step S106: laminating the first prepreg, the copper-clad laminate, the second prepreg and the metal layer on both sides of the drilled copper-iron-nickel alloy plate through a lamination process to form a multi-layer circuit board.
[0036] In this embodiment, a first prepreg, a copper-clad laminate, a second prepreg and a metal layer are laminated on both sides of the copper-plated iron-nickel alloy plate after drilling to form a multilayer circuit board through a lamination process. The copper-clad laminate includes a core board and copper layers laminated on both sides of the core board. Optionally, before lamination, the copper-clad laminate is exposed, developed and etched to form a circuit pattern on the copper layers on both sides of the core board of the copper-clad laminate.
[0037] Optionally, a second semi-cured sheet is laid on the surface of the copper clad laminate away from the copper-plated iron-nickel alloy plate, and a metal layer is laid on the surface of the second semi-cured sheet away from the copper clad laminate, and then the second semi-cured sheet and the metal layer are laminated on the surface of the copper clad laminate away from the copper-plated iron-nickel alloy plate through a lamination process to form a multi-layer circuit board.
[0038] Different from the prior art, the present application provides a method for manufacturing a circuit board, which includes: drilling holes at a preset position of at least one copper-iron-nickel alloy plate; laying a first prepreg on both sides of the copper-iron-nickel alloy plate; laying a copper-clad plate on the surface of the first prepreg away from the copper-iron-nickel alloy plate; laying a second prepreg on the surface of the copper-clad plate away from the copper-iron-nickel alloy plate; laying a metal layer on the surface of the second prepreg away from the copper-clad plate; laminating the first prepreg, the copper-clad plate, the second prepreg, and the metal layer on both sides of the copper-iron-nickel alloy plate after drilling through a lamination process to form a multi-layer circuit board. The present application uses a copper-iron-nickel alloy plate as a metal sandwich layer of a high-order multi-layer board to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as a power layer or ground layer of the circuit board.
[0039] See also Figure 2 , Figure 2 It is a flow chart of a second embodiment of a method for manufacturing a circuit board provided in the present application.
[0040] Step S201: drilling holes at preset positions of at least one copper-plated iron-nickel alloy plate.
[0041] Step S201 is the same as the above-mentioned step S101 and will not be described again here.
[0042] Step S202: roughening the surfaces of both sides of the copper-iron-nickel alloy plate.
[0043] In this embodiment, after a through hole is formed at a preset position of the copper-plated iron-nickel alloy plate by a drilling process, the surfaces on both sides of the copper-plated iron-nickel alloy plate are roughened. Through the roughening treatment, pollutants on the surface of the copper-plated iron-nickel alloy plate are removed, and the surface roughness of the copper-plated iron-nickel alloy plate is increased, thereby facilitating the combination of the copper-plated iron-nickel alloy plate and the semi-cured sheet in the subsequent pressing process.
[0044] Step S203: Laminating the first prepreg and the copper-clad laminate on both side surfaces of the copper-plated iron-nickel alloy plate through a laminating process.
[0045] In this embodiment, the first prepreg and the copper clad laminate are laid on both side surfaces of the copper-plated iron-nickel alloy plate after roughening treatment, and the first prepreg and the copper clad laminate are pressed on both side surfaces of the copper-plated iron-nickel alloy plate by a pressing process. Wherein, the first prepreg is first laid on both side surfaces of the copper-plated iron-nickel alloy plate, and then the copper clad laminate is laid on one side surface of the first prepreg away from the copper-plated iron-nickel alloy plate, and then the first prepreg and the copper clad laminate are pressed on both side surfaces of the copper-plated iron-nickel alloy plate by a pressing process. Wherein, the copper clad laminate includes a core plate and a copper layer pressed on both sides of the core plate. Optionally, before pressing, the copper clad laminate is exposed, developed and etched to form a circuit pattern on the copper layer on both sides of the core plate of the copper clad laminate, so as to make the copper layer into a circuit layer, so that the copper layer on both sides of the copper clad laminate plays the role of a power layer and a signal layer.
[0046] Step S204: Laminating the metal layer and the second prepreg on the copper clad laminate through a lamination process to build up layers and form a multi-layer circuit board.
[0047] In this embodiment, after the first prepreg and the copper clad laminate are pressed on both sides of the copper-plated iron-nickel alloy plate, the second prepreg is laid on the side of the copper clad laminate away from the copper-plated iron-nickel alloy plate, and the metal layer is laid on the surface of the second prepreg away from the copper clad laminate, and then the metal layer and the second prepreg are pressed on the copper clad laminate by a pressing process to add layers to form a multi-layer circuit board. The metal layer can be used as a signal layer of the multi-layer board.
[0048] Step S205: making outer layer circuits on the metal layer of the multi-layer circuit board.
[0049] In this embodiment, after a multi-layer circuit board is formed by adding layers, an outer layer circuit is made on the metal layer of the multi-layer circuit board. Specifically, a layer of anti-etching dry film is first laid on the outer metal layer of the multi-layer circuit board, and then the pattern on the anti-etching dry film is transferred to the outer metal layer by exposure, development and etching to form the outer layer circuit.
[0050] Step S206: drilling the multi-layer circuit board to form via holes at corresponding preset positions of the multi-layer circuit board.
[0051] In this embodiment, the metal layers on both sides of the multi-layer circuit board are processed to form outer layer circuits, and the multi-layer circuit board is drilled to form a via hole at a preset position of the multi-layer circuit board corresponding to the copper-iron-nickel alloy plate. The via hole runs through the entire multi-layer circuit board, and the diameter of the via hole is smaller than the diameter of the through hole at the preset position of the copper-iron-nickel alloy plate.
[0052] Step S207: electroplating the multilayer circuit board with the via holes formed therein to metallize the via holes.
[0053] In this embodiment, the multilayer circuit board with the via hole is electroplated to make the via hole metallized, and the metallized via hole can conduct the copper-clad plates and the outer layer circuit on both sides of the copper-iron-nickel alloy plate. Among them, since the diameter of the via hole is smaller than the diameter of the through hole at the preset position of the copper-iron-nickel alloy plate, and the through hole of the copper-iron-nickel alloy plate is filled with the first prepreg, the metallized via hole is not connected to the copper-iron-nickel alloy plate, thereby avoiding the problem of short circuit in the process of opening the via hole.
[0054] Different from the prior art, the present application provides a method for manufacturing a circuit board, which includes: drilling holes at a preset position of at least one copper-iron-nickel alloy plate; laying a first prepreg on both sides of the copper-iron-nickel alloy plate; laying a copper-clad plate on the surface of the first prepreg away from the copper-iron-nickel alloy plate; laying a second prepreg on the surface of the copper-clad plate away from the copper-iron-nickel alloy plate; laying a metal layer on the surface of the second prepreg away from the copper-clad plate; laminating the first prepreg, the copper-clad plate, the second prepreg, and the metal layer on both sides of the copper-iron-nickel alloy plate after drilling through a lamination process to form a multi-layer circuit board. The present application uses a copper-iron-nickel alloy plate as a metal sandwich layer of a high-order multi-layer board to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as a power layer or ground layer of the circuit board.
[0055] See also Figure 3 , Figure 3 The circuit board 30 of the present application comprises a copper-plated iron-nickel alloy layer 301 , a first semi-cured layer 302 , a copper-clad laminate 303 , a second semi-cured layer 304 and a metal layer 305 .
[0056] In this embodiment, the copper-iron-nickel alloy layer 301 can be used as the ground layer of the circuit board 30, and can dissipate heat for the circuit board 30 during the operation of the circuit board 30. A through hole 306 is provided at a preset position of the copper-iron-nickel alloy layer 301, and the through hole 306 is filled with a semi-cured material.
[0057] In this embodiment, the first prepreg layer 302 is disposed on both sides of the copper-iron-nickel alloy layer 301. Specifically, the prepreg can be pressed on both sides of the copper-iron-nickel alloy layer 301 to form the first plate solidified layer 302. The prepreg will fill the through hole 306 during the pressing process.
[0058] In this embodiment, a copper clad laminate 303 is arranged on a surface of a side of the first semi-cured layer 302 away from the copper-plated iron-nickel alloy layer 301. The copper clad laminate 303 includes a core board 3031 and a copper layer 3032 pressed on both sides of the core board. Optionally, before pressing, the copper clad laminate 303 is exposed, developed and etched to form a circuit pattern on the copper layer 3032 on both sides of the core board 3031 of the copper clad laminate to make the copper layer 3032 into a circuit layer.
[0059] In this embodiment, the second semi-cured layer 304 is disposed on a side surface of the copper clad laminate 303 away from the copper-iron-nickel alloy layer 301, and the metal layer 305 is disposed on a side surface of the second semi-cured layer 304 away from the copper clad laminate 303. The metal layer 305 and the second semi-cured layer 304 are pressed on the surface of the copper clad laminate 303 through a pressing process, and the metal layer 305 is exposed, developed, and etched to form an outer layer circuit.
[0060] In this embodiment, the circuit board 30 further includes a via hole 307, which is disposed at a position of the circuit board 30 corresponding to the through hole 306, and the diameter of the via hole 307 is smaller than the diameter of the through hole 306. The via hole 307 is electroplated to form a metallized via hole 307, thereby connecting the copper clad board 303 and the metal layer 305. Since the diameter of the via hole 307 is smaller than the diameter of the through hole 306, and the through hole 306 is filled with a semi-cured material, the problem of short circuit during the manufacturing process of the via hole 307 is avoided.
[0061] Different from the prior art, the present application provides a circuit board, which uses a copper-plated iron-nickel alloy plate as a metal sandwich layer of a high-order multilayer board to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as a power layer or ground layer of the circuit board.
[0062] See also Figure 4 , Figure 4The circuit board 40 of the present application comprises a copper clad plate 401 , a first semi-cured layer 402 , a first metal layer 403 , a second semi-cured layer 404 , a copper-plated iron-nickel alloy plate 405 and a second metal layer 406 .
[0063] In this embodiment, a first semi-cured layer 402 is disposed on both sides of the copper clad laminate 401, a first metal layer 403 is disposed on a surface of the first semi-cured layer 402 away from the copper clad laminate 401, and the first metal layer 403 and the first semi-cured layer 402 are pressed on both sides of the copper clad laminate 401 through a lamination process. The copper clad laminate 401 includes a core board 4011 and a copper layer 4012 pressed on both sides of the core board, and the copper layers 4012 on both sides of the copper clad laminate 401 are used as ground layers in the circuit board to play a role in heat dissipation.
[0064] In this embodiment, a through hole 407 is opened at a preset position of the copper-iron-nickel alloy plate 405, and a semi-cured material is filled in the through hole 407. The second semi-cured layer 404 is arranged on both sides of the copper-iron-nickel alloy plate 405, and the second metal layer 406 is arranged on the side of the copper-iron-nickel alloy plate 405 away from the copper-clad laminate 401. The second semi-cured layer 404, the copper-iron-nickel alloy plate 405 and the second metal layer 406 are pressed on the side of the first metal layer 403 away from the copper-clad laminate 401 through a pressing process.
[0065] In this embodiment, the circuit board 40 further includes a via hole 408, which is disposed at a position of the circuit board 40 corresponding to the through hole 408, and the diameter of the via hole 408 is smaller than the diameter of the through hole 407. The via hole 408 is electroplated to form a metallized via hole 408, thereby connecting the copper clad board 401, the first metal layer 402, and the second metal layer 406. Among them, since the diameter of the via hole 408 is smaller than the diameter of the through hole 407, and the through hole 407 is filled with a semi-cured material, the problem of short circuit during the production process of the via hole 408 is avoided.
[0066] Different from the prior art, the present application provides a circuit board, which uses a copper-plated iron-nickel alloy plate as a metal sandwich layer of a high-order multilayer board to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as a power layer or ground layer of the circuit board.
[0067] Furthermore, the present application also provides a circuit board, which adopts any of the above-mentioned manufacturing methods. In the circuit board manufactured by this method, the copper-plated iron-nickel alloy plate is used as the metal sandwich layer of the high-order multilayer board during the board forming process to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as the power layer or ground layer of the circuit board.
[0068] Furthermore, the present application also provides an electronic device, the circuit board includes the above circuit board. The electronic device uses the above circuit board, and uses the copper-plated iron-nickel alloy plate as the metal sandwich layer of the high-order multilayer board to reduce the expansion of the circuit board in the X and Y directions and enhance the strength of the circuit board, and can also be used as the power layer or ground layer of the circuit board.
[0069] The above descriptions are merely embodiments of the present application and are not intended to limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A method for manufacturing a circuit board, characterized in that: The production method comprises: Drilling holes at predetermined positions of at least one copper-plated iron-nickel alloy plate; The copper-plated iron-nickel alloy plate is an alloy comprising nickel, iron, carbon and manganese elements; The first prepreg is laid on both sides of the copper-iron-nickel alloy plate; Laying the copper clad laminate on the surface of the first prepreg away from the copper-plated iron-nickel alloy plate; Laying a second prepreg on the surface of the copper-clad laminate away from the copper-plated iron-nickel alloy plate; Laying a metal layer on the surface of the second prepreg away from the copper clad laminate; The first prepreg, the copper-clad laminate, the second prepreg and the metal layer are laminated on both sides of the drilled copper-iron-nickel alloy plate to form a multilayer circuit board; The step of laminating the first prepreg, the copper-clad laminate, the second prepreg and the metal layer on both sides of the drilled copper-iron-nickel alloy plate to form a multilayer circuit board specifically includes: laminating the first prepreg and the copper-clad laminate on both sides of the copper-iron-nickel alloy plate by a laminating process; the first prepreg will soften and fill the through hole at the preset position of the copper-iron-nickel alloy plate; The metal layer and the second prepreg are pressed onto the copper clad laminate through a pressing process to build up layers, thereby forming the multi-layer circuit board.
2. The method for manufacturing a circuit board according to claim 1, characterized in that: After the step of drilling holes at a preset position of at least one copper-plated iron-nickel alloy plate, the method further comprises: The surfaces of both sides of the copper-plated iron-nickel alloy plate are roughened.
3. The method for manufacturing a circuit board according to claim 1, characterized in that: After the step of laminating the first prepreg, the copper-clad laminate, the second prepreg and the metal layer on both sides of the drilled copper-iron-nickel alloy plate to form a multi-layer circuit board by a lamination process, the following steps are further included: Drilling the multi-layer circuit board to form a via hole at a position on the multi-layer circuit board corresponding to the preset position; The multilayer circuit board with the via holes is electroplated to metallize the via holes.
4. The method for manufacturing a circuit board according to claim 3, characterized in that: The step of electroplating the multilayer circuit board with the via holes so as to metallize the via holes further includes: An outer layer circuit is manufactured on the metal layer of the multi-layer circuit board.
5. The method for manufacturing a circuit board according to claim 1, characterized in that: The copper-iron-nickel alloy plate is two sheets, and the metal layer includes a first metal layer and a second metal layer; The step of drilling holes at a preset position of at least one copper-plated iron-nickel alloy plate comprises: Drilling holes at preset positions of the two copper-plated iron-nickel alloy plates respectively; The step of laminating the first prepreg, the copper-clad laminate, the second prepreg and the metal layer on both sides of the drilled copper-iron-nickel alloy plate to form a multilayer circuit board comprises: The first prepreg, the first metal layer, the second prepreg and the copper-plated iron-nickel alloy plate are respectively pressed onto the two side surfaces of the copper-clad laminate by a pressing process; The second metal layer and the second prepreg are pressed together on the surface of the copper-plated iron-nickel alloy plate away from the copper-clad plate to build up layers, so as to form the multi-layer circuit board.
6. The method for manufacturing a circuit board according to claim 1, characterized in that: After the step of laminating the first prepreg, the copper-clad laminate, the second prepreg and the metal layer on both sides of the drilled copper-iron-nickel alloy plate to form a multi-layer circuit board by a lamination process, the following steps are further included: Drilling the multi-layer circuit board to form a via hole at a position on the multi-layer circuit board corresponding to the preset position; The multilayer circuit board with the via holes is electroplated to metallize the via holes.
7. The method for manufacturing a circuit board according to claim 1, characterized in that: Circuit patterns are etched on both sides of the copper clad board.
8. A circuit board, characterized in that: The circuit board adopts the circuit board manufacturing method as described in any one of claims 1 to 7.
9. An electronic device, characterized in that: The electronic device comprises the circuit board as claimed in claim 8.