A hydrophilic and hydrophobic grid chip, preparation method and application thereof

Through the preparation method of hydrophilic grid chips, etching treatment and silane coating technology, the problems of complex chip production, high cost and low yield in existing DNA synthesis technology are solved, and the low cost of high-throughput DNA synthesis is achieved. Efficient production.

CN115138411BActive Publication Date: 2024-11-29SANGON BIOENGINEERING (SHENZHEN) CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202210908400.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-29
Publication Date
2024-11-29
Estimated Expiration
2042-07-29

AI Technical Summary

Technical Problem

In the existing DNA synthesis technology, the chip production process is complex, expensive, and low yield, which cannot meet the high throughput and low cost requirements of synthetic biology.

Method used

Using the preparation method of hydrophilic grid chips, a microstructure chip with a mesh shape is prepared through etching treatment and silane coating technology, which realizes simple production and low-cost production of the chip.

Benefits of technology

It realizes simple production and low-cost production of chips, with a yield of up to Fmol-10Pmol, and is suitable for applications such as gene splicing, mutant library and DNA synthesis, avoiding amplification steps and improving production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115138411B_ABST
    Figure CN115138411B_ABST
Patent Text Reader

Abstract

The present invention relates to a hydrophilic-hydrophobic grid chip, a preparation method and its application, wherein the preparation method of the hydrophilic-hydrophobic grid chip comprises the following steps: etching the surface of the chip to obtain a roughened microstructure chip with a grid shape; cleaning the roughened microstructure chip and drying it for standby use; coating the dried standby chip under the condition of a silane reagent to obtain the hydrophilic-hydrophobic grid chip. The preparation method of the hydrophilic-hydrophobic grid chip in the present application is simple, low in cost, and suitable for industrial production. The size and shape of the prepared chip are adjustable, and can be used for the synthesis of Fmol-10Pmol yields, and can be directly used for gene splicing, mutant libraries, capture probes and other applications without amplification. The prepared chip can be directly operated on liquid with a pipette gun or an automated pipetting workstation, and each sequence can be operated separately.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of synthetic biology, and in particular relates to a hydrophilic-hydrophobic grid chip, a preparation method and applications thereof. Background Art

[0002] In synthetic biology, DNA synthesis is one of the core upstream tools and is crucial to promoting the development of downstream platforms and applications of synthetic biology. Among the DNA synthesis technologies, column synthesis, as a first-generation synthesis technology, has developed the earliest and most mature, and has been widely used in the field of primer synthesis, but it cannot fully meet the development needs of synthetic biology. With the development of technology, the second-generation high-throughput chip synthesis has emerged. Compared with the first generation, it has an increase of 2-4 orders of magnitude in flux and a decrease of 2-4 orders of magnitude in cost, which can basically meet the requirements of synthetic biology for flux and cost. The core technology of the second-generation DNA synthesis is the chip. Among the second-generation technologies, it mainly includes photochemical, electrochemical, and inkjet chemical synthesis methods, among which the inkjet synthesis method of Agilent and Twist is the mainstream representative, but there is still no commercial inkjet synthesis equipment in China. Although the inkjet synthesis method of Agilent and Twist can reach the million level in flux, its output is only at the Fmol level, which does not have an advantage in the main application of synthetic biology-gene synthesis, and needs to be amplified to the Pmol level to achieve effective amplification. At the same time, the manufacturing process is complex and costly, requiring complex coating technology and even photolithography technology to complete. Therefore, developing a chip that is simple to make, low-cost, and easy to operate individually is critical to achieving a breakthrough in high-throughput DNA synthesis, which is an urgent problem to be solved in the industry. Summary of the invention

[0003] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the first aspect of the present invention provides a method for preparing a hydrophilic-hydrophobic grid chip, which has simple and practical steps and low cost, and is suitable for the production of large quantities of hydrophilic-hydrophobic grid chips.

[0004] A second aspect of the present invention provides a hydrophilic-hydrophobic grid chip.

[0005] The third aspect of the present invention further proposes an application of a hydrophilic-hydrophobic grid chip.

[0006] According to a first aspect of the present invention, there is provided a method for preparing a hydrophilic-hydrophobic grid chip, comprising the following steps: etching the surface of a chip to obtain a textured microstructure chip having a grid shape; cleaning the textured microstructure chip and drying it for standby use; coating the dried chip in the presence of a silane reagent to obtain the hydrophilic-hydrophobic grid chip.

[0007] According to the preparation method of the hydrophilic-hydrophobic grid chip of the embodiment of the present invention, at least the following beneficial effects are achieved: the preparation method of the hydrophilic-hydrophobic grid chip is simple, low in cost, and suitable for industrial production. In the traditional chip manufacturing method, the process is complicated and the cost is high. For example, the Agilent solution has a complex coating, no physical isolation is formed, and it is difficult to limit adhesion and diffusion. The Twist solution requires complex photolithography technology, which is complex to manufacture and costly. And whether it is the Agilent or Twist solution, the yield of a single DNA produced is too low, only about 0.2-1fmol, which is not suitable for direct gene splicing and library application scenarios with certain requirements for quantity, and needs to be amplified before use. In addition, the post-processing process of the chip is complicated, and complex microfluidic equipment is required to obtain DNA products of a single sequence. The technical solution of the present application, in addition to the above-mentioned simple manufacture, low cost and suitability for industrial production, also has the following characteristics: the size and shape of the prepared chip are adjustable, which can be used for the synthesis of Fmol-10Pmol yields, and can be directly used for gene splicing, mutant libraries, capture probes and other applications without amplification. The prepared chip can be used to perform liquid operations directly using a pipette or an automated pipetting workstation, and each sequence can be operated separately.

[0008] It is understandable that the above-mentioned grid chip is composed of a specific grid shape and a roughened edge. The specific grid refers to the structure formed on the chip outside the roughened area. The roughened area will produce a microstructure on the chip surface, forming a lotus leaf effect at the edge of the grid, thereby effectively limiting the diffusion and flow of droplets at the edge of the grid.

[0009] According to some embodiments of the present invention, the material of the chip may be glass, silicon, silicon oxide, quartz or plastic.

[0010] According to some embodiments of the present invention, the size and shape of the chip can be (2.5*7.5) mm, (4*4) mm, (4*6) mm, (6*6) mm or any larger rectangular, square, or circular chip. Or a conventional glass slide size can be selected. Preferably, the shape of the chip is square or circular.

[0011] According to some embodiments of the present invention, the etching process includes any one of laser etching, strong acid etching, strong alkali etching, electron beam etching or plasma etching.

[0012] It should be noted that the etching process forms a microstructure with a special morphology on the chip surface. The microstructure can be a strip, well, circle, star, diamond or other texture. It can also be pits made directly on the chip surface, including regular or irregular pits. These pits can effectively increase the surface area of ​​the chip.

[0013] It can be understood that in the above-mentioned etching process, the strong acid includes any one or more of ammonium fluoride, hydrofluoric acid, hydrofluoric acid salts, etc., and the strong base includes any one or more of sodium hydroxide, potassium hydroxide, etc.

[0014] According to some embodiments of the present invention, the grid shape includes any one or more of a triangle, a rectangle, a diamond, a cylinder, a circle, a line, a mesh or a well. Preferably, the grid shape is a square in a circle or a rectangle.

[0015] It is understood that the area occupied by the grid can be (0.1-1) mm 2 ,(1-16)mm 2 , (16-100)mm 2 , or the entire chip. The appropriate area can be selected according to the different single synthesis requirements and the types of synthesis on the same chip, according to the current synthesis method and principle, and the required minimum yield. It should be noted that different grid areas correspond to different DNA synthesis yields, for example, (0.1-100) m 2 , which can correspond to the synthesis of 1Fmol-10Pmol DNA yield. Preferably, the area occupied by the grid is 4mm 2 , or 8mm 2 .

[0016] It is understandable that the number of grids can be 1-24, 24-192, 192-1536, 1536-115360, or 15360-1536000, matching the area of ​​a single grid and the entire chip. The number of grids on this chip is ultimately determined by the selected adaptation area, that is, the area of ​​a single grid and the size of the entire chip must match, and the size of the chip and the area of ​​a single grid determine the number of grids. For example, one grid corresponds to a DNA synthesized on a chip, and 1-1536000 grids correspond to the high-throughput synthesis of 1-1536000 DNAs.

[0017] According to some embodiments of the present invention, the silane includes one or more of 3-aminopropyltrimethoxysilane, (3-aminopropyl)triethoxysilane, N-(3-triethoxysilylpropyl)-4-hydroxybutyramide silane, 11-acetoxyundecanyltriethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, γ(2,3-epoxypropoxy)propyltrimethoxysilane, octylchlorosilane, (tridecafluoro-1,1,2,2-tetrahydrooctyl)trichlorosilane, perfluorooctyltrichlorosilane, perfluorooctyltriethoxysilane, perfluorooctyltrimethoxychlorosilane, n-octyltrimethoxysilane, n-decyltriethoxysilane, C4-C18 alkylsilane or C4-C18 alkyl substituted silane.

[0018] It is understood that the silane can be selected as a single silane, or a mixed silane containing two kinds. Among them, in some embodiments, if a mixed silane is selected, the first silane can be aminosilane, hydroxysilane or epoxysilane, etc., and the second silane can be C4-C18 alkylsilane, perfluorinated or partially fluorinated C4-C18 alkylsilane, or C4-C18 alkylsilane substituted by other groups. The silicon methoxy group (or silicon ethoxy group) in the silane is chemically bonded to the surface of the chip, including the grid and the grid edge of the chip. The silane can be one or more of trichlorosilane, dichlorosilane, monochlorosilane, trimethoxysilane, triethoxysilane, etc. Chlorosilane reacts chemically with the OH on the surface, loses one or more HCL molecules, and forms an O-Si chemical bond with the surface, thereby firmly connecting to the surface.

[0019] The first type of silane is a functional silane (e.g., N-(3-triethoxysilylpropyl)-4-hydroxybutyramide), which mainly provides a synthesis site for subsequent DNA synthesis and links the first base.

[0020] The second type of silane is an auxiliary silane (eg, perfluorooctyltriethoxysilane), which is mainly used to improve the hydrophobicity of the chip surface.

[0021] According to some embodiments of the present invention, the coating process includes any one of solution coating, physical vacuum coating or CVD vapor coating.

[0022] According to some embodiments of the present invention, the width of the roughened edge is (0.1-100) mm. It is understood that the width of the roughened edge can be selected in the range of (0.1-1) mm, (1-10) mm or (10-100) mm. The edge width can be selected according to the surface tension of the reagents of the surface reaction. The wider the width, the better the barrier effect will be, but it will also occupy more effective chip area. Therefore, the preferred width is related to the chip size and the amount of DNA used.

[0023] According to some embodiments of the present invention, the cleaning includes first washing with a strong alkali or plasma, and then washing alternately with water and an organic agent.

[0024] A second aspect of the present invention provides a hydrophilic-hydrophobic grid chip, comprising the hydrophilic-hydrophobic grid chip prepared by the above-mentioned method for preparing the hydrophilic-hydrophobic grid chip.

[0025] According to the hydrophilic-hydrophobic grid chip of the embodiment of the present invention, the roughness range of the microstructure on the grid of the chip is (0.1-100) μm.

[0026] According to some embodiments of the present invention, the roughness value Ra of the texturing treatment ranges from (0.1-6.3) μm, or (6.3-100) μm. The larger the Ra value, the higher the roughness, but too much roughness will also affect the hydrophilic and hydrophobic effects of texturing and non-texturing. Preferably, Ra=25um.

[0027] The third aspect of the present invention provides an application of a hydrophilic-hydrophobic grid chip, which includes the synthesis of a hybridization chip, a drug screening chip, a DNA synthesis chip or a polypeptide chip, and is particularly effective in the field of DNA synthesis chips. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] The present invention will be further described below with reference to the accompanying drawings and embodiments, wherein:

[0029] Figure 1 A frosted glass chip having grid patterns of different shapes in one embodiment of the present invention;

[0030] Figure 2 96 small rectangular grids arranged on a (75*25) mm glass in one embodiment of the present invention;

[0031] Figure 3 A (2*2) mm diamond grid arranged on a (75*25) mm glass in one embodiment of the present invention;

[0032] Figure 4 A circular grid with R=2 mm arranged on a (75*25) mm glass in one embodiment of the present invention;

[0033] Figure 5 A square grid with L=2 mm arranged on a (75*25) mm glass in one embodiment of the present invention;

[0034] Figure 6 This is a schematic diagram showing the comparison of the contact angles of pure water at the edge of a grid and in the middle of a grid in one embodiment of the present invention;

[0035] Figure 7 Schematic diagram of the application of the hydrophilic-hydrophobic grid chip in DNA synthesis according to one embodiment of the present invention. DETAILED DESCRIPTION

[0036] The following will be combined with the embodiments to clearly and completely describe the concept of the present invention and the technical effects produced, so as to fully understand the purpose, characteristics and effects of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, other embodiments obtained by those skilled in the art without creative work are all within the scope of protection of the present invention.

[0037] In the description of the present invention, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0038] The specific embodiments of the present invention are described in detail below.

[0039] Example 1

[0040] Fabrication of a microstructured chip with a textured surface in a grid shape

[0041] First, a specific area of ​​the glass is plasma etched by a picosecond laser to obtain a grid-shaped roughened glass chip. The roughened shape can be processed into any pattern and size according to the requirements, such as the following. Figure 1 The grid shapes shown in the figure are triangles, circles, rectangles, and diamonds. Figure 2 The grid shown contains 96 small rectangular grids, which are arranged on the (75*25) mm glass, or processed as shown in the attached Figure 3 The grid specifications shown are (2*2) mm diamonds. These grids are arranged on (75*25) mm glass, or processed as shown in the attached Figure 4 The grid specifications shown are circles with R = 2 mm. These grids are arranged on (75*25) mm glass, or processed as shown in the attached Figure 5 The grid size shown is L=2 mm square, and these grids are arranged on a (75*25) mm glass.

[0042] Example 2

[0043] Fabrication of hydrophilic and hydrophobic grid chips with single silane coating

[0044] Take the glass prepared in Example 1 and arrange 96 (2*3) mm small rectangular grids on the (75*25) mm glass, with a grid area of ​​6 mm 2 The roughened chip is put aside and placed in a special cleaning fixture. It is first ultrasonically cleaned for 30 minutes with a 0.1 mol / L NaOH solution and a 1% liquid cleaning agent solution by volume, and then ultrasonically cleaned with pure water for 3 times, each time for 5 minutes. After cleaning, it is blown dry with nitrogen and immediately cleaned with plasma for 2 minutes at a power of 200W.

[0045] Then, the CVD chemical vapor deposition method was used for coating. The plasma-treated chip was immediately placed in a solution containing 100ul of monohydroxysilane (N-(3-triethoxysilylpropyl)-4-hydroxybutyramide), and then the silane solution was placed in a vacuum drying oven with a cavity volume of 30L for vacuum treatment to make the pressure in the cavity less than 10mbar, and then the system was kept at 60°C for 15 hours, and then cured at 110°C for 1 hour. After completion, the chip was taken out, ultrasonically cleaned with anhydrous ethanol and water for 1 minute each, and then dried with nitrogen to obtain a single silane-coated hydrophilic and hydrophobic grid chip.

[0046] Quality control analysis: randomly select 1% (at least 2) of the coated chips for water drop method contact angle test, test the contact angles of two areas with different roughness multiple times, and take the average value. Among the qualified chips, the CA values ​​between the two differ by more than 10°.

[0047] Example 3

[0048] Hybrid silane-coated hydrophilic and hydrophobic grid chip

[0049] Take the glass prepared in Example 1 and arrange 96 (2*3) mm small rectangular grids on the (75*25) mm glass, with a grid area of ​​6 mm 2 The roughened chip is put aside and placed in a special cleaning fixture. It is first ultrasonically cleaned for 30 minutes with a 0.1 mol / L NaOH solution and a 1% liquid cleaning agent solution by volume, and then ultrasonically cleaned with pure water for 3 times, each time for 5 minutes. After cleaning, it is blown dry with nitrogen and immediately cleaned with plasma for 2 minutes at a power of 200W.

[0050] Then, the CVD chemical vapor deposition method was used for coating. The plasma-treated chip was immediately placed in a monohydroxysilane solution containing 200ul (N-(3-triethoxysilylpropyl)-4-hydroxybutyramide) and 40ul perfluoroalkylsilane (perfluorooctyltriethoxysilane), and then the silane solutions were placed in a vacuum drying oven with a cavity volume of 30L, and vacuumized to make the pressure in the cavity less than 10mbar, and then the system was kept at 60°C for 15 hours, and then cured at 110°C for 1 hour. After completion, the chip was taken out, ultrasonically cleaned with ethanol and water for 1 minute each, and then dried with nitrogen to obtain a hydrophilic and hydrophobic grid chip with mixed silane coating.

[0051] Quality control analysis: randomly select 1% (at least 2) of the coated chips for water drop method contact angle test, test the contact angles of two areas with different roughness multiple times, and take the average value. Among the qualified chips, the CA values ​​between the two differ by more than 10°.

[0052] Attached Figure 6 In Example 3, 96 (2*3) mm small rectangular grids are arranged on the (75*25) mm glass, and the grid area is 6 mm 2 The contact angle of pure water at the edge and the middle of the same grid after the roughened chip is mixed with silane coating. Among them, the hydrophilic and hydrophobic grid chip is due to the selectivity of different roughness surfaces for the amount and type of coating silane, resulting in a higher contact angle on the roughened grid of the present application, while the contact angle is lower in the non-roughened area, that is, inside the grid, thereby achieving the production of a hydrophilic and hydrophobic surface in one step.

[0053] The hydrophilic and hydrophobic grid chip prepared in Example 3 was used to take different reagents in small amounts and multiple times with a pipette to test the barrier effect. The volume of reagents that can be accommodated by the grid of the same area is shown in the following table, where the barrier effect of the chip is pure water>mixed liquid>propylene carbonate>acetonitrile. This shows that the hydrophilic and hydrophobic grid chip has a significant barrier effect, and the same surface has obvious differences in the barrier effect for reagents with different surface tensions, among which the barrier effect for pure water is the best.

[0054]

[0055] Example 4

[0056] Application of hydrophilic-hydrophobic grid chip in DNA synthesis

[0057] Take the hydrophilic and hydrophobic grid chip made in Example 3 for standby use. It should be noted that on the ul-level inkjet device, the reagent can be used to complete the spotting and liquid addition respectively through an independent nozzle and a fluid device, and the synthesis of DNA is carried out by a phosphoramidite reaction. The surface of the chip after coating carries a large number of active hydroxyl groups, which provides a synthesis site for the synthesis of DNA on the surface. The specific process of synthesis is as follows: 1. Activation. Before the reaction starts, a deprotection reagent is printed in each mesh to activate the hydroxyl groups on the surface; 2. Coupling the first base, printing the first modified base with DMT and the catalyst in different grids respectively, and the bases printed in different grids can be any one of A, G, C, and T, and then printing the capping reagent, oxidant, and deprotection reagent in sequence to complete the synthesis of the first base; 3. Coupling the second base: Repeat the process of the first base, the only difference is that the second base printed in different grids is preset, which can also be any one of A, G, C, and T. 4. Couple the third to the Nth base, and repeat the above 3 steps. The third or Nth base in different grids is preset and can be any one of A, G, C, and T. In this way, 96 different base sequences of a specified length (such as 90nt) can be synthesized in different grids on the chip, thereby achieving high-throughput synthesis of DNA. The synthesis process is shown in the following table (Note: There is an acetonitrile cleaning and nitrogen drying process after each step of the reaction, which is omitted here):

[0058] process Reagents Reaction time activation Deprotection reagents 30s Coupling first base DMT modified base / catalyst 60s Capping reagents 30s Oxidation reagents 30s Deprotection reagents 60s Coupling the second base DMT modified base / catalyst 60s Capping reagents 30s Oxidation reagents 30s Deprotection reagents 60s Coupling the third to Nth base DMT modified base / catalyst 60s Capping reagents 30s Oxidation reagents 30s Deprotection reagents 60s

[0059] After DNA synthesis is completed, the chip is placed in an ultra-clean bench through gas phase aminolysis, and 20ul NF water is added to each grid in turn to dissolve the DNA in a specific grid, and then concentrated and purified to obtain several single DNA products. Through identification, the synthesized products are all 90nt, and the single DNA yield fluctuates between 1-1.2Pmol. The synthesis process is shown in the attached figure. Figure 7 As shown. The chip produced by the present application can be directly operated on it with a pipette gun or an automated pipetting workstation. Each sequence corresponds to a grid, which can be operated individually or with a mixture of specified sequences. Compared with the solutions of Agilent or Twist, the processing process of the present application is simple, and DNA products of a single sequence can be obtained without the use of complex microfluidic equipment.

[0060] The embodiments of the present invention are described in detail above in conjunction with specific implementation methods, but the present invention is not limited to the above embodiments. Various changes can be made within the knowledge of ordinary technicians in the relevant technical field without departing from the purpose of the present invention. In addition, the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.

Claims

1. A method for preparing a hydrophilic-hydrophobic grid chip, characterized in that: It consists of the following steps: The specific area of ​​the glass is subjected to plasma etching by picosecond laser to obtain a roughened microstructure chip with a specific grid shape. The texturing microstructure chip is cleaned in the following specific steps: first, ultrasonic cleaning is performed for 30 minutes using a NaOH solution with a concentration of 0.1 mol / L and a Liquid cleaning agent solution with a volume ratio of 1%, then ultrasonic cleaning is performed for 3 times using pure water, each time for 5 minutes, and after cleaning, drying is performed using nitrogen gas, and plasma cleaning is immediately performed for 2 minutes at a power of 200 W; The cleaned chip is subjected to a coating treatment in a mixed silane solution to obtain the hydrophilic and hydrophobic grid chip. The coating treatment process specifically includes: placing the chip after plasma treatment immediately in a mixed silane solution containing 200ul of N-(3-triethoxysilylpropyl)-4-hydroxybutyramide and 40ul of perfluorooctyltriethoxysilane, and then placing the mixed silane solution in a vacuum drying oven with a cavity volume of 30L for vacuum treatment to make the pressure in the cavity less than 10mbar, and then keeping the system at 60°C for reaction for 15 hours, and then curing at 110°C for 1 hour. After completion, the chip is taken out, ultrasonically cleaned with ethanol and water for 1min each, and then blown dry with nitrogen to obtain a hydrophilic and hydrophobic grid chip coated with mixed silane; The hydrophilic-hydrophobic grid chip is composed of a specific grid and a roughened edge. The specific grid refers to a structure formed on the chip other than the roughened edge. The roughened edge will produce a microstructure on the chip surface.

2. The preparation method according to claim 1, characterized in that: The shape of the specific grid includes any one or more of a triangle, a rectangle, a diamond, a circle, and a line.

3. The preparation method according to any one of claims 1 to 2, characterized in that: The width of the roughened edge is 0.1-100mm.

4. A hydrophilic and hydrophobic grid chip, characterized in that: The chip is prepared by the preparation method according to any one of claims 1 to 3.

5. The hydrophilic-hydrophobic grid chip according to claim 4, characterized in that: The roughness of the microstructure is in the range of 0.1-100 μm.

6. An application of the hydrophilic-hydrophobic grid chip as claimed in claim 5, characterized in that: The application includes the synthesis of hybridization chips, drug screening chips or DNA synthesis chips.

Citation Information

Patent Citations

  • Reaction device for biological / chemical reaction system, preparation method and application thereof

    CN106111220A