Crystallization purification method of crude pyromellitic acid
Through the combined treatment of cation exchanger and activated carbon, the problem of excessive impurity content in PMA products is solved, and high-purity phenylatic acid crystal refining is achieved, ensuring the quality and color requirements of downstream polyimide materials.
Patent Information
- Application Number
- CN202110445596.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-04-25
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-04-25
AI Technical Summary
In the prior art, the impurity content of phenylatic acid (PMA) products is too high, especially metal ions, which affects the colority and quality of downstream polyimides.
The combination of cation exchanger and activated carbon is used as impurity removal agents to improve the purity of PMA through different treatment sequences and conditions (such as sequence, dosage ratio, temperature and time), including first treatment of activated carbon after cation exchanger, or Both are used at the same time, and crystallization is carried out after solid-liquid separation.
The purity of PMA is significantly improved, up to 92.0 wt.%, which is better than the treatment with cation exchange resin or activated carbon alone, ensuring the quality and color requirements of downstream materials.
Smart Images

Figure BDA0003036736550000101
Abstract
Description
Technical Field
[0001] The invention relates to a crystallization purification method for crude pyromellitic acid. Background Art
[0002] Pyromellitic acid (PMA) is a promising polyacid compound widely used in industrial processes. Among them, the dehydration product of PMA, pyromellitic dianhydride (PMDA), is one of the important raw materials for the production of polyimide (PI) materials. PI is polymerized by PMDA and 4,4-diaminodiphenyl ether (ODA). It has the advantages of ultra-high heat resistance, chemical corrosion resistance, and high mechanical strength. It is widely used in aviation, aerospace, microelectronics, nano, liquid crystal, separation membranes, lasers and other fields. Therefore, as an indispensable and important precursor of PI, PMA has extremely high requirements for its quality and purity during the synthesis process.
[0003] The synthesis method of PMA mainly uses alkyl oxidation of benzene rings. The main raw materials include a series of polyalkyl aromatic hydrocarbons such as durene, 2,4,5-trimethylbenzaldehyde, 1-chloromethyl-2,4,5-trimethylbenzene and 1-methanol-2,4,5-trimethylbenzene. At present, the PMA synthesis method based on the Co-Mn-Br liquid phase oxidation catalytic system has a high yield. Compared with nitric acid oxidation, it has the advantages of high efficiency and environmental friendliness and is widely used. Although the product yield of the homogeneous oxidation process is high, impurities such as metal ions and by-products are dissolved in the solution, and the boiling point of PMA is high, so it is crucial to select a suitable purification and separation method.
[0004] Mitsubishi Gas Chemical Co., Ltd. published patent US 6579990B2 (Process for Producing Refined Pyromellitic Acid and Refined Pyromellitic Anhydride). The publication date is June 7, 2003, and discloses a method for purifying pyromellitic acid. Specifically, different types of activated carbon adsorbents are used to adsorb and purify crude PMA, and then a high-temperature sublimation process is used to dehydrate and generate uniform PMDA. Although this method can significantly improve the purity of PMA by only using one adsorption process, it lacks the process of removing trace metal ions, and metal ions have a greater impact on the color of downstream synthetic polyimide. Summary of the invention
[0005] The present invention aims to solve the problem of excessively high impurity content in PMA products in the prior art, and provides a new crystallization and purification method for crude pyromellitic acid. The PMA obtained by implementing the method has the characteristic of high purity.
[0006] In order to solve the above technical problems, the technical solution of the present invention is as follows:
[0007] The crystallization and purification method of crude pyromellitic acid comprises:
[0008] (I) treating a solution containing crude PMA with an impurity removing agent to obtain a refined PMA solution;
[0009] (II) crystallization of refined PMA solution to obtain refined PMA;
[0010] Wherein, the impurity remover comprises an impurity remover A and an impurity remover B, the impurity remover A is selected from a cation exchanger, and the impurity remover B is selected from activated carbon.
[0011] Under the condition of the same amount of impurity removal agent, the purity of refined PMA is better when cation exchange resin and activated carbon are used simultaneously than that of single cation exchange resin or single activated carbon.
[0012] In the above technical solution, the processing order of step (I) is preferably selected from any one of the following:
[0013] Processing sequence 1: first treated with impurity removal agent A, solid-liquid separation, then treated with impurity removal agent B, solid-liquid separation;
[0014] Or treatment sequence 2: first treat with impurity removal agent B, solid-liquid separation, then treat with impurity removal agent A, solid-liquid separation;
[0015] Or treatment sequence 3: using impurity removal agent A and impurity removal agent B for treatment at the same time, and separating the solid and liquid.
[0016] In the comparison among the above-mentioned processing sequence 1, processing sequence 2 and processing sequence 3, the purity of refined PMA in sequence 1 is the highest.
[0017] In the above technical solution, the cation exchanger is preferably a cation exchange resin or a molecular sieve.
[0018] In the above technical solution, the purity of the crude PMA in step (I) is preferably 50.0-90.0 wt.%. For example, but not limited to, the purity of the crude PMA in step (I) is 55.0 wt.%, 60.0 wt.%, 65.0 wt.%, 70.0 wt.%, 75.0 wt.%, 80.0 wt.%, 85.0 wt.%, etc.
[0019] In the above technical solution, the mass ratio of the impurity removing agent to the crude PMA in step (I) is preferably 0.005 to 0.05. For example, but not limited to, the mass ratio of the impurity removing agent to the crude PMA in step (I) is 0.006, 0.007, 0.008, 0.009, 0.01, 0.015, 0.02, 0.025, 0.03, 0.035, 0.04, 0.045, etc., more preferably 0.02 to 0.05.
[0020] In the above technical solution, the concentration of crude PMA in the solution containing crude PMA is preferably 10-30wt%. For example, but not limited to, the concentration of crude PMA in the solution containing crude PMA is 11wt.%, 12wt.%, 13wt.%, 14wt.%, 15wt.%, 16wt.%, 17wt.%, 18wt.%, 19wt.%, 20wt.%, 21wt.%, 22wt.%, 23wt.%, 24wt.%, 25wt.%, 26wt.%, 27wt.%, 28wt.%, 29wt.%, etc. More preferably, it is 20-30wt.%.
[0021] In the above technical solution, the solvent used in the solution containing crude PMA is preferably water, acetic acid or ethanol.
[0022] In the above technical solution, the temperature of step (I) is preferably 0-100° C. For example, but not limited to, the temperature of step (I) is 5° C., 10° C., 15° C., 20° C., 25° C., 30° C., 35° C., 40° C., 45° C., 50° C., 55° C., 60° C., 65° C., 70° C., 75° C., 80° C., 85° C., 92° C., 95° C., etc. However, 50-95° C. is preferred, and 60-95° C. is more preferred.
[0023] In the above technical solution, the treatment time of step (I) is preferably 10 to 60 minutes. For example, but not limited to, the treatment time of step (I) is 12 minutes, 14 minutes, 16 minutes, 18 minutes, 20 minutes, 22 minutes, 24 minutes, 26 minutes, 28 minutes, 30 minutes, 32 minutes, 34 minutes, 36 minutes, 38 minutes, 40 minutes, 45 minutes, 50 minutes, 55 minutes, etc.
[0024] In the above technical scheme, the weight ratio of the impurity removing agent A to the impurity removing agent B in step (I) is preferably 0.1 to 10. For example, but not limited to, the weight ratio of the impurity removing agent A to the impurity removing agent B in step (I) is 0.15, 0.2, 0.25, 0.3, 0.35, 0.4, 0.45, 0.5, 0.55, 0.6, 0.65, 0.7, 0.75, 0.8, 0.85, 0.9, 0.95, 1.0, 1.5, 2, 2.5, 3, 3.5, 4, 4.5, 5, 5.5, 6, 6.5, 7, 7.5, 8, 8.5, 9, 9.5, etc. More preferably, it is 0.5 to 2.
[0025] In the above technical solution, the crystallization temperature of step (II) is preferably 0-40° C. For example, but not limited to, the crystallization temperature of step (II) is 5° C., 10° C., 15° C., 20° C., 25° C., 30° C., 35° C., etc. More preferably, it is 5-30° C.
[0026] In the above technical solution, the crystallization time of step (II) is preferably 0.5 to 2 hours. For example, but not limited to, the crystallization time of step (II) is 0.5 hours, 0.6 hours, 0.7 hours, 0.8 hours, 0.9 hours, 1.0 hours, 1.1 hours, 1.2 hours, 1.3 hours, 1.4 hours, 1.5 hours, 1.6 hours, 1.7 hours, 1.8 hours, 1.9 hours, etc.
[0027] As a non-limiting implementation of the treatment sequence 1, the mixture may be first treated with the impurity removal agent A for 10 to 30 minutes, filtered, and then treated with the impurity removal agent B for 10 to 30 minutes, and filtered.
[0028] In the present invention, the purity of PMA is measured by high performance liquid chromatography for quantitative analysis, column temperature: 35°C; mobile phase: acetonitrile with a pH of 1.9-0.1% Phosphoric acid solution (volume ratio 25:75) was mixed at 1.0 mL min -1 Isocratic elution at flow rate; wavelength: 237nm.
[0029] The present invention is described in detail below through specific implementation modes and examples. DETAILED DESCRIPTION
[0030] Comparative Example 1
[0031] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water to dissolve, and then 4 g of activated carbon was added and the temperature was raised to 80°C and stirred for 30 min, and the mixture was filtered while keeping warm. When the filtrate was cooled to 70°C, 2 g of pure PMA seed crystals were added, and the temperature was further lowered to 10°C. Crystallization was carried out at 10°C for 1 hour, and the mixture was filtered. The filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 92.0 wt.%.
[0032] For the convenience of comparison, the experimental results are listed in Table 1.
[0033] Comparative Example 2
[0034] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, followed by adding 4 g of cation exchange resin (Amberlite IR-110, sodium type) and heating to 80°C with stirring for 30 min, followed by filtration at a temperature of 70°C, and adding 2 g of pure PMA seed crystals when the filtrate was cooled to 10°C, and then the temperature was further cooled to 10°C, and crystallized at 10°C for 1 hour, filtered, and the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 89.1 wt.%.
[0035] For the convenience of comparison, the experimental results are listed in Table 1.
[0036] Example 1
[0037] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 2 g of cation exchange resin (Amberlite IR-110, sodium type) was added and the temperature was raised to 80°C and stirred for 15 min, the mixture was filtered while keeping warm, 2 g of activated carbon was added and stirred for 15 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of >99.0 wt.%.
[0038] For the convenience of comparison, the experimental results are listed in Table 1.
[0039] Example 2
[0040] The difference from Example 1 is that this example is first treated with activated carbon and then treated with a cation exchange resin, as follows:
[0041] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water to dissolve, 2 g of activated carbon was added, the temperature was raised to 80°C and stirred for 15 min, the mixture was filtered while keeping warm, 2 g of cation exchange resin (Amberlite IR-110, sodium type) was added, the mixture was stirred for 15 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, the filter cake was dried at 100°C for 6 hours, and a refined PMA product with a purity of 97.5 wt.% was obtained.
[0042] For the convenience of comparison, the experimental results are listed in Table 1.
[0043] Example 3
[0044] The difference from Example 1 is that activated carbon and cation exchange resin are used for treatment at the same time, specifically:
[0045] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 2 g of activated carbon and 2 g of cation exchange resin (Amberlite IR-110, sodium type) were added, the temperature was raised to 80°C and stirred for 30 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 96.8 wt.%.
[0046] For the convenience of comparison, the experimental results are listed in Table 1.
[0047] Example 4
[0048] The difference from Example 1 is that the ratio of activated carbon to cation exchange resin is different, specifically:
[0049] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 3 g of cation exchange resin (Amberlite IR-110, sodium type) was added and the temperature was raised to 80°C and stirred for 15 min, the mixture was filtered while keeping warm, 1 g of activated carbon was added, the mixture was stirred for 15 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 98.2 wt.%.
[0050] For the convenience of comparison, the experimental results are listed in Table 1.
[0051] Example 5
[0052] The difference from Example 1 is that the ratio of activated carbon to cation exchange resin is different, specifically:
[0053] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 1 g of cation exchange resin (Amberlite IR-110, sodium type) was added and the temperature was raised to 80°C and stirred for 15 min, the mixture was filtered while keeping warm, 3 g of activated carbon was added, the mixture was stirred for 15 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 98.6 wt.%.
[0054] For the convenience of comparison, the experimental results are listed in Table 1.
[0055] Example 6
[0056] The difference from Example 3 is that the ratio of activated carbon to cation exchange resin is different, specifically:
[0057] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 3 g of activated carbon and 1 g of cation exchange resin (Amberlite IR-110, sodium type) were added, the temperature was raised to 80°C and stirred for 30 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 97.3 wt.%.
[0058] For the convenience of comparison, the experimental results are listed in Table 1.
[0059] Example 7
[0060] The difference from Example 3 is that the ratio of activated carbon to cation exchange resin is different, specifically:
[0061] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 1 g of activated carbon and 3 g of cation exchange resin (Amberlite IR-110, sodium type) were added, the temperature was raised to 80°C and stirred for 30 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 95.6 wt.%.
[0062] For the convenience of comparison, the experimental results are listed in Table 1.
[0063] Example 8
[0064] The difference from Example 1 is that no additional PMA seed crystals are added, and the crystallization is directly performed by cooling, specifically:
[0065] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 2 g of cation exchange resin (Amberlite IR-110, sodium type) was added and the temperature was raised to 80°C and stirred for 15 min, the mixture was filtered while keeping warm, 2 g of activated carbon was added, the mixture was stirred for 15 min, the mixture was filtered while keeping warm, the temperature was lowered to 10°C, crystallized for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 98.0 wt.%.
[0066] For the convenience of comparison, the experimental results are listed in Table 1.
[0067] Example 9
[0068] The difference from Example 1 is that the crystallization temperature is different, specifically:
[0069] 100 g of crude PMA with a purity of 85.1 wt.% was added to 400 g of pure water for dissolution, 2 g of cation exchange resin (Amberlite IR-110, sodium type) was added and the temperature was raised to 80°C and stirred for 15 min, the mixture was filtered while keeping warm, 2 g of activated carbon was added, the mixture was stirred for 15 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 30°C, crystallized at 30°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 98.6 wt.%.
[0070] For the convenience of comparison, the experimental results are listed in Table 1.
[0071] Example 10
[0072] The difference from Example 1 is that the ratio of crude PMA to water is different, specifically:
[0073] 100 g of crude PMA with a purity of 85.1 wt.% was added to 200 g of pure water for dissolution, 2 g of cation exchange resin (Amberlite IR-110, sodium type) was added and the temperature was raised to 80°C and stirred for 30 min, the mixture was filtered while keeping warm, 2 g of activated carbon was added, the mixture was stirred for 30 min, the mixture was filtered while keeping warm, 2 g of pure PMA seed crystals were added when the filtrate was cooled to 70°C, the temperature was further lowered to 10°C, crystallized at 10°C for 1 hour, filtered, the filter cake was rinsed with an equal amount of pure water, and the filter cake was dried at 100°C for 6 hours to obtain a refined PMA product with a purity of 98.0 wt.%.
[0074] For the convenience of comparison, the experimental results are listed in Table 1.
[0075] Table 1
[0076]
[0077] In the table:
[0078] A represents an impurity removal agent A, i.e., a cation exchanger;
[0079] B represents impurity removal agent B, i.e. activated carbon;
[0080] Processing sequence 1: firstly treated with impurity removal agent A, solid-liquid separation, then treated with impurity removal agent B, solid-liquid separation;
[0081] Processing sequence 2: firstly treated with impurity removal agent B, solid-liquid separation, then treated with impurity removal agent A, solid-liquid separation;
[0082] Processing sequence 3---Use impurity removal agent A and impurity removal agent B for treatment at the same time, and separate the solid and liquid.
Claims
1. A method for crystallizing and refining crude pyromellitic acid, comprising: (I) treating a solution containing crude PMA with an impurity-removing agent to obtain a refined PMA solution; (II) Refined PMA solution is crystallized to obtain refined PMA; Wherein, the impurity removing agent is an impurity removing agent A and an impurity removing agent B, the impurity removing agent A is selected from a cation exchanger, and the impurity removing agent B is selected from activated carbon; In step (I), the mass ratio of the impurity removing agent to the crude PMA is 0.005 to 0.05; The weight ratio of the impurity removing agent A to the impurity removing agent B is 0.1 to 10; The order of treatment in step (I) is: firstly treated with impurity removal agent A, solid-liquid separation, then treated with impurity removal agent B, solid-liquid separation; The cation exchanger is a cation exchange resin; The purity of the crude PMA in step (I) is 50.0-90.0 wt %.
2. The purification method according to claim 1, characterized in that The concentration of crude PMA in the solution containing crude PMA is 10-30wt%.
3. The purification method according to claim 1, characterized in that The solvent used for the solution containing crude PMA is water, acetic acid or ethanol.
4. The purification method according to claim 1, characterized in that The treatment temperature is 0-100°C.
5. The purification method according to claim 1, characterized in that The processing time is 10~60 min.
6. The purification method according to claim 1, characterized in that The crystallization temperature in step (II) is 0-40°C.
7. The purification method according to claim 1, characterized in that The crystallization time of step (II) is 0.5 to 2 hours.