A preparation method for stacked nanosheet GAA-FET with suppressed channel leakage
By using selective GP diffusion doping of P-type and N-type doped oxides in the manufacturing process of GAA-FET, the surface damage and particle problems caused by high-energy ion implantation are solved, and the channel of GAA-FET is realized. Leakage suppression improves device performance and quality.
Patent Information
- Application Number
- CN202210809638.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-11
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-07-11
AI Technical Summary
In the manufacturing process of stacked nanosheet GAA-FET, conventional high-energy ion implantation causes surface defects and particles, which affects device characteristics. Especially in the integration process of CMOS GAA-FET, N-type and P-type ion implantation and doping are required respectively. , resulting in surface damage and particle contamination.
Through selective GP diffusion doping of P-type and N-type doped oxides, a high-concentration residual error doping distribution is formed on the surface to suppress GAA-FET sub-fin parasitic channel leakage, replace high-energy ion implantation, and reduce surface damage. and particles.
It effectively suppresses channel leakage, improves the surface quality of the device, reduces film defects in subsequent SiGe/Si stack epitaxy, and improves device performance.
Smart Images

Figure CN115295416B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductors, and in particular to a preparation method for stacked nanosheet GAA-FETs capable of suppressing channel leakage. Background Art
[0002] As transistor feature sizes continue to shrink, traditional MOSFET devices have undergone a transition from planar structures to three-dimensional structures, improving device performance while reducing the impact of short channel effects. The current mainstream three-dimensional structure transistor is FinFET. However, FinFET faces huge challenges in the technology generation below 5nm. In the latest International Roadmap for Devices and Systems (IRDS), Nanosheet-GAAFET is a key device that can effectively replace FinFET after the 3nm node, and can significantly suppress the short channel effect and improve the current driving performance of the device.
[0003] At present, the research progress of GAA stacked nanosheet FET has attracted wide attention from academia and industry. The constantly updated preparation process and key processes, as well as the optimized device structure are the hot research directions of new CMOS devices.
[0004] GAA stacked nanosheet FET is a new device developed on the basis of FinFET and Nanowire-FET, with a ring gate structure and horizontal nanosheet (NS) as a conductive channel. In terms of gate control, the ring gate structure has better gate control capability than the FinFET device structure, which can effectively suppress the short channel effect of the device; in terms of current drive, Nanosheet-GAAFET has an effective gate adjustable and vertical and horizontal stacking design, which can also significantly enhance the current drive performance of the device.
[0005] However, the current integrated manufacturing process of conventional stacked nanosheet GAA-FET is compatible with the traditional FinFET manufacturing process. There is a parasitic leakage channel at the bottom of the stacked nanosheet channel. It is usually necessary to form a heavy substrate doping by high-energy and high-dose ion implantation for Ground Plane Doping to prevent the formation of parasitic channel leakage channels in the sub-fin region. However, high-energy and high-dose implantation of the substrate followed by rapid thermal annealing can easily produce surface defects or particles on the surface of the silicon wafer, which can easily affect the quality of subsequent SiGe / Si stacked epitaxy, bring about thin film defects, and lead to device characteristic degradation. In particular, the integration of CMOS GAA-FET requires N-type and P-type ion implantation doping in the PMOS and NMOS regions respectively, and the corresponding implantation mask layer removal, which can cause more implantation damage and particle contamination on the substrate surface. Summary of the invention
[0006] In view of the above technical problems, the present invention proposes a preparation method for stacked nanosheet GAA-FET that suppresses channel leakage. In the GAA-FET integrated manufacturing process, the manufacturing method suppresses GAA-FET sub-fin parasitic channel leakage by selectively performing GP diffusion doping with P-type and N-type doped oxides. Thus, a high-concentration residual error doping distribution on the surface can be formed, and surface damage and particles caused by conventional high-energy ion implantation can be suppressed.
[0007] The present invention adopts the following technical solutions:
[0008] A method for preparing a stacked nanosheet CMOS GAA-FET for suppressing channel leakage, characterized in that it comprises the following steps:
[0009] Providing a substrate; performing N-type dielectric doping and P-type dielectric doping on the upper surface of the substrate by depositing a doped film, and performing rapid thermal annealing to diffuse the doped ions to form PMOS and NMOS regions respectively;
[0010] epitaxially growing a superlattice stack of alternately stacked first semiconductors and second semiconductors on the substrate;
[0011] Etching the superlattice stack to form a plurality of fins;
[0012] forming a dummy gate on the fin and etching the fin;
[0013] Selectively etching the superlattice stack of the first semiconductor and the second semiconductor on the fin to form a nanosheet stack portion, and etching away a portion of the nanosheet formed by the first semiconductor in the superlattice stack from the outside to the inside;
[0014] Selecting an epitaxial growth process to form source and drain regions;
[0015] Dielectric deposition and planarization to expose the dummy gate;
[0016] Channel release of nanosheets is achieved, wherein the stack of nanosheets forms a plurality of conductive channels. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] By reading the detailed description of the preferred embodiment below, various other advantages and benefits will become clear to those of ordinary skill in the art. The accompanying drawings are only used for the purpose of illustrating the preferred embodiment and are not considered to be limitations of the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings.
[0018] FIG. 1(A) is a top view of the partitioned doping of a substrate according to the present invention, and FIG. 1(B) is a schematic diagram of the growth of a superlattice stack on a substrate according to the present invention.
[0019] Figure 2 The diagram is a schematic diagram of forming a first sidewall on a superlattice stack according to the present invention.
[0020] Figure 3 Schematic diagram of etching a superlattice stack to form fins according to the present invention.
[0021] Figure 4 The schematic longitudinal cross-sectional view of the present invention is a schematic diagram of removing the first sidewall to form a shallow trench isolation region along a direction perpendicular to the fin line.
[0022] Figure 5 The figure is a schematic longitudinal cross-sectional view of forming a dummy gate on a fin according to the present invention along a direction perpendicular to the fin line.
[0023] Figure 6 These are the XX and YY directions defined in the device of the present invention.
[0024] Figure 7 It is a cross-sectional schematic diagram along line XX, where a second sidewall spacer is formed on both sides of the dummy gate and source and drain etching is performed.
[0025] Figure 8 It is a cross-sectional schematic diagram of etching away a portion of the first semiconductor layer from the outside to the inside, further depositing the second sidewall, and etching the outer second sidewall along the XX line of the present invention.
[0026] Fig. 9 It is a cross-sectional schematic diagram of depositing source and drain regions, doping source and drain regions, and depositing an isolation layer according to the present invention.
[0027] Fig.10 This is a cross-sectional schematic diagram of the deposition of the present invention, removing the false gate and releasing the nanochannel along the XX line.
[0028] Fig.11 The diagram is a schematic diagram of the formation of the deposition interface oxide layer, the high-K dielectric layer, and the metal gate according to the present invention.
[0029] Fig.12 The cross-sectional schematic diagram of the present invention is to remove the redundant deposition interface oxide layer, high-K dielectric layer, metal gate, deposit to form dielectric CMP layer, contact hole photolithography and etching, and deposit hole silicide. DETAILED DESCRIPTION
[0030] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. However, it should be understood that these descriptions are exemplary only and are not intended to limit the scope of the present invention. In addition, in the following description, descriptions of known structures and technologies are omitted to avoid unnecessary confusion of the concept of the present invention.
[0031] Various structural schematic diagrams according to embodiments of the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing tolerances or technical limitations, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs.
[0032] In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element or an intervening layer / element may exist between them. In addition, if a layer / element is "on" another layer / element in one orientation, the layer / element may be "under" the other layer / element when the orientation is reversed.
[0033] In this embodiment, a method for manufacturing a semiconductor device is provided. 1-11 are schematic diagrams of a process for manufacturing a FET device of the present invention, and the process for manufacturing a FET device includes:
[0034] As shown in FIG. 1(A) which is a top view of a substrate, a substrate 101 is provided, which may be bulk silicon.
[0035] The substrate 101 is a part of a semiconductor wafer suitable for forming one or more IC devices. When a bulk silicon substrate is used, the substrate 101 is first cleaned to remove surface impurities. Then, the substrate 101 is partitioned into N-type dielectric doping areas and P-type dielectric doping areas through deposition, photolithography, etching, annealing and doping processes. Through a series of processes, the N-type dielectric doping area and the P-type dielectric doping area are deposited in the bulk silicon substrate 101 by depositing N-type and P-type doped films, and then rapid thermal annealing is performed to diffuse the doped ions to form a heavily doped surface area. A specific process is as follows: depositing an N-type doped film, such as a film doped with P, As, and Sb ions, on the substrate 101, applying photoresist, and through the process of exposure and development, the subsequent doped area, such as the N-type dielectric doped area, is covered by the photoresist, and the remaining area is exposed, then the exposed doped film is selectively etched and the residual photoresist is removed, and then rapid thermal annealing is performed to diffuse the doped ions in the doped film to form an N-type surface heavily doped area; then the doped film is removed, and a P-type doped film, such as a film doped with B, In, Al, and Ga ions, is deposited, and photoresist is applied again, and through the process of exposure and development, the subsequent doped area, such as the P-type dielectric doped area, is covered by the photoresist, and the remaining area is exposed, then the residual photoresist is removed, and then rapid thermal annealing is performed to diffuse the doped ions in the doped film to form a P-type surface heavily doped area; finally, the doped film is removed to form N-type and P-type surface heavily doped areas on the substrate 101, respectively. The N-type surface heavily doped area is subsequently manufactured corresponding to the P-type FET, and the P-type surface heavily doped area is subsequently manufactured corresponding to the N-type FET.
[0036] By depositing the doped film, the N and P partitions are realized on the substrate 101. The N-type surface heavily doped area and the P-type surface heavily doped area are formed on the substrate 101. Due to the high concentration residual error distribution of the N-type surface heavily doped area and the P-type surface heavily doped area, the surface lattice is less damaged and contaminated with particles, which is beneficial to the subsequent SiGe / Si stacked epitaxy. The concentration of the doping element is 1e 16 ~5e 20 cm -3 The dielectric thickness of the formed doped region is 1nm~1um, the annealing temperature range is 600℃~1150℃, and the annealing method is rapid thermal annealing, Spike annealing, laser annealing and the like and their combination.
[0037] In the present invention, the doping order of the N-type heavily doped surface region and can also be reversed, that is, the P-type heavily doped surface region is formed first and then the N-type dielectric doped region is formed.
[0038] Silicon dioxide (SiO2) on the surface of bulk silicon substrate 101 is removed, and multiple periods of first semiconductor 201' / second semiconductor 202' superlattice structure stacks are epitaxially grown on bulk silicon substrate 101; the thickness of each semiconductor layer in the superlattice structure is less than 30 nanometers, and the final thickness will directly determine the height of the nanosheet channel and the electrostatic performance. During the superlattice stack epitaxy process, the SiGe thickness and Si thickness are regulated separately, and the Ge content is regulated to form a multi-component SiGe conductive channel.
[0039] In one way, for both P-type FET and N-type FET, the first semiconductor 201' / second semiconductor 202' superlattice is a Si / SiGe stack. In another way, for P-type FET, the first semiconductor 201' / second semiconductor 202' superlattice is a Si / SiGe stack, and for N-type FET, the first semiconductor 201' / second semiconductor 202' superlattice is a SiGe / Si stack.
[0040] like Figure 2 The self-aligned spacer transfer (SIT) process is used to form a nanoscale first spacer 301 device array, and the first spacer 301 is silicon nitride (SiN X The specific formation process is as follows: a sacrificial layer 302 is covered on the superlattice stack, and the sacrificial layer can be polysilicon (PolySi, p-si) or amorphous silicon (a-si), and a part of the sacrificial layer is etched away to deposit silicon nitride (SiN x ) layer, and then anisotropic etching is used to etch away the remaining sacrificial layer, so that only multiple periodic silicon nitride (SiN x ) first spacers 301, the silicon nitride (SiN x ) The first sidewall spacer 301 acts as a hard mask in photolithography.
[0041] The epitaxially grown superlattice stack is made into multiple periodically distributed fins by etching. The first sidewall 301 is used as a mask for etching to form a fin with a superlattice stack structure. The upper part of the fin is a conductive channel area formed by the superlattice stack, and the lower part is a substrate, forming a Figure 3 The fin shown. The fin includes not only a superlattice stacked structure, but also a single crystal silicon structure that penetrates into the substrate. The etching process is dry etching or wet etching, and in one embodiment, reactive ion etching (RIE) can be used. The fin will be used to form one or more horizontal nanosheets of n-type field effect transistors and / or p-type field effect transistors. Although Figure 3 One fin is shown, and it should be understood that any suitable number and configuration of fins may be used. The height of the fin is about 10 nm-400 nm, and the width is about 1-100 nm.
[0042] like Figure 4 As shown, a shallow trench isolation (STI) region 103 is formed between two adjacent fins. First, a dielectric insulating material is deposited and then planarized, for example, using a CMP process, and then the dielectric insulating material is selectively etched back to expose a three-dimensional fin structure, thereby forming a shallow trench isolation region 103 adjacent to the fin. The upper surface of the shallow trench isolation region 103 is generally flush with the interface between the superlattice stacked structure in the fin and the substrate single crystal silicon, and may be higher or lower than the interface level. The shallow trench isolation region 103 can be formed of a suitable dielectric material, such as silicon dioxide (SiO2), silicon nitride (SiN x ) etc. The shallow trench isolation region 103 is used to separate transistors on adjacent fins. The shallow trench isolation region 103 exposes the bottommost first semiconductor layer 201' of the superlattice stack.
[0043] like Figure 5 As shown, a dummy gate stack is formed on the exposed fin in a direction perpendicular to the fin line (i.e., the YY direction). The dummy gate stack is a multi-layer structure, including a gate insulating dielectric (not shown), a dummy gate layer 106 and a hard mask layer 108. The dummy gate stack structure can be formed by processes such as thermal oxidation, chemical vapor deposition, and sputtering. The dummy gate stack structure spans the superlattice stack on the top of the fin, and multiple dummy gates are periodically distributed along the fin line direction. The material used for the dummy gate layer 106 can be polysilicon (PolySi, p-si) or amorphous silicon (a-si). The material used for the hard mask layer 108 can be oxide, carbide, carbide, organic matter, etc.
[0044] like Figure 6 The direction is defined in Figure 6 Two dotted lines XX and YY are set in the figure. The XX line is the center line of the fin along the fin line direction, and the YY line is the center line of the fin perpendicular to the fin line direction. The subsequent drawings are all cross-sectional schematic diagrams based on the XX and YY lines.
[0045] Figure 7 As shown, silicon nitride (SiN) is disposed on both sides of the dummy gate stack and along the fin line direction (ie, XX direction). x ) The second spacers 107 are formed on both sides of the fin, and the second spacers 107 have the same thickness. Then, the dummy gate layer 106, the hard mask 108, and the second spacers 107 are used as masks to perform source and drain etching on the fins through an etching process.
[0046] Then, if Figure 8 As shown, pull-back etching is performed to etch away a portion of the first semiconductor layer 201' from the source and drain regions toward the center. Then, silicon nitride (SiN) is deposited on the periphery of the fin.x ) The third sidewall spacer 107' is etched until it is flush with the second semiconductor layer 202' in the vertical direction. The missing portion of the first semiconductor layer 201' caused by the pull-back etching is replaced by the silicon nitride (SiN) of the third sidewall spacer 107'. x )Fill up.
[0047] like Fig. 9 As shown, for a P-type FET, the source and drain region material is boron (B) doped SiGe (SiGe:B), and for an N-type FET, the source and drain region material is phosphorus (P) doped silicon (Si) (Si:P), and finally the source and drain region 110 is formed.
[0048] Then, an isolation layer 111 is deposited on the upper surface of the dummy gate and the source and drain regions 110 to prevent interconnection short circuit between the dummy gate layer 106 and the source and drain regions 110 in subsequent steps, and the isolation layer 111 is chemically mechanically polished to make it flat, and the hard mask layer 108 is removed to expose the dummy gate layer 106.
[0049] Then, if Fig.10 As shown, the dummy gate layer 106 formed of the aforementioned polysilicon (PolySi, p-si) or amorphous silicon (a-si) is etched or corroded by a selective etching or corrosion process, that is, the dummy gate layer 106 is removed.
[0050] Subsequently, the sacrificial layer in the superlattice stack is selectively etched to release the nanosheet channel. The conductive channel region exposed by the fin is processed to remove each first semiconductor layer 201', which is the sacrificial layer, and release the nanosheet 202 formed by the second semiconductor. The nanosheet 202 has a width range of 1-100nm, a thickness range of 1-30nm, and a spacing range of 3-30nm between each nanosheet 202.
[0051] In one embodiment, for both P-type and N-type FETs, the sacrificial layer is a GeSi layer, the GeSi layer is selectively removed, and the Si layer is retained to form a Si horizontal stack nano stack device. In the selective removal process, an etchant that selectively etches SiGe at a faster rate than Si can be used. In one embodiment, a conventional wet process is used to isotropically etch the sacrificial layer to release the nano channel, thereby forming a nano sheet conductive channel.
[0052] In another embodiment, channel release is performed separately for P-type and N-type FETs.
[0053] For a P-type FET, the sacrificial layer is a Si layer, the Si layer is selectively removed, and the SiGe layer is retained to form a SiGe horizontal stack nano stack device. In the selective removal process, an etchant that selectively etches Si at a faster rate than SiGe can be used. In one embodiment, a conventional wet process is used to isotropically etch the sacrificial layer to release the nano channel, thereby forming a nanosheet conductive channel.
[0054] For N-type FET, the sacrificial layer is a SiGe layer, the SiGe layer is selectively removed, and the Si layer is retained to form a Si horizontal stacked nano stack device. In the selective removal process, an etchant that selectively etches SiGe at a faster rate than Si can be used. In one embodiment, a conventional wet process is used to isotropically etch the sacrificial layer to release the nano channel, thereby forming a nano sheet conductive channel. The second semiconductor nano layer sheet 202 is stacked to form a nano stack portion.
[0055] Then, if Fig.11 As shown, an interfacial oxide layer (IL) 115-1 is deposited or grown, and then a high-K dielectric layer 115-2 is deposited, so that the high-K dielectric layer surrounds the surface of the nano stack portion. The high-K dielectric layer may have a dielectric constant higher than about 6.0, and the material of the high-k dielectric layer may be HfO2, HfSiO x 、HfON、HfSiON、HfAlO x 、Al2O3、ZrO2、ZrSiO x , Ta2O5 or La2O3 or a combination of them.
[0056] Next, a metal gate is deposited outside the space formed by the dummy gate 106 and the high-K dielectric layer to form a multi-layer high-K / metal gate structure. The metal gate includes a capping layer, a barrier layer, a work function layer, and a filling layer. Film structures with different effective work functions can be formed by selective photolithography and etching to adjust the device threshold. Generally, chemical vapor deposition, physical vapor deposition and other processes are used to form a metal gate. The metal gate material is TaC, TiN, TaTbN, TaErN, TaYbN, TaSiN, HfSiN, MoSiN, RuTa x 、NiTa x ,MoN x , TiSiN, TiCN, TaAlC, TiAlN, TaN, PtSi x , Ni3Si, Pt, Ru, Ir, Mo, Ti, Al, Cr, Au, Cu, Ag, HfRu or RuO x One or a combination of Fig.11As shown in FIG. 1 , the metal gate fills the space after the dummy gate layer 106 is removed. Then, the multi-layer high-K / metal gate structure is chemically mechanically polished to make it flat, and the excess multi-layer high-K / metal gate material exposed on the surface of the dielectric layer outside the dummy gate space is removed to form a high-K dielectric layer and a metal gate 113, wherein the two are filled in the space of the original first semiconductor layer 201 to form a ring gate structure.
[0057] Next, an ILD dielectric is deposited on the top to form a dielectric CMP layer 112 , contact hole photolithography and etching are performed on the dielectric CMP layer 112 , hole silicide 114 is deposited, and contact electrodes are drawn out.
[0058] Subsequently, multi-layer back-end interconnection and passivation protection processes are completed.
[0059] The above is the process flow for preparing a complete semiconductor device, forming a Fig.12 FET device shown.
[0060] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0061] The present invention proposes a preparation method for stacked nanosheet GAA-FETs that suppress channel leakage. In the GAA-FET integrated manufacturing process, the manufacturing method suppresses GAA-FET sub-fin parasitic channel leakage by selectively performing GP diffusion doping with P-type and N-type doped oxides. Thus, a high-concentration residual error doping distribution on the surface can be formed, and surface damage and particles caused by conventional high-energy ion implantation can be suppressed.
[0062] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.
[0063] The embodiments of the present invention are described above. However, these embodiments are only for illustrative purposes and are not intended to limit the scope of the present invention. The scope of the present invention is defined by the appended claims and their equivalents. Without departing from the scope of the present invention, those skilled in the art may make various substitutions and modifications, which should all fall within the scope of the present invention.
Claims
1. A method for preparing a stacked nanosheet CMOS GAA-FET for suppressing channel leakage, characterized in that: The steps include: Providing a substrate; performing N-type dielectric doping and P-type dielectric doping on the upper surface of the substrate by depositing a doped film, and performing rapid thermal annealing to diffuse the doped ions to form PMOS and NMOS regions respectively; epitaxially growing a superlattice stack of alternately stacked first semiconductors and second semiconductors on the substrate; Etching the superlattice stack to form a plurality of fins; forming a dummy gate on the fin and etching the fin; Selectively etching the superlattice stack of the first semiconductor and the second semiconductor on the fin to form a nanosheet stack portion, and etching away a portion of the nanosheet formed by the first semiconductor in the superlattice stack from the outside to the inside; Selecting an epitaxial growth process to form source and drain regions; Dielectric deposition and planarization to expose the dummy gate; Achieving channel release of nanosheets, wherein the stack of nanosheets forms a plurality of conductive channels; The step of forming a plurality of fins is specifically as follows: providing a first sidewall on the superlattice stack; etching the superlattice stack using the first sidewall as a mask to form the plurality of fins; The method further includes forming a shallow trench isolation region, specifically: generating a shallow trench isolation region between adjacent fins, so that the plurality of conductive channels are located above the shallow trench isolation region; The method also includes forming source and drain regions, specifically, etching away the fin structure between adjacent dummy gates to form a source and drain growth space; epitaxially growing the source and drain regions in the growth space, and depositing an isolation layer on the source and drain regions; After the source and drain regions are formed, the dummy gate is removed by selective etching. After the nanosheet channel is released, a gate is deposited at the original dummy gate position.
2. The method according to claim 1, characterized in that: The doping elements of the N-type dielectric doping region are P, As or Sb respectively; the doping elements of the P-type dielectric doping region are B, In, Al or Ga.
3. The method according to claim 2, characterized in that: The concentration of the doping element is 1e 16 ~5e 20 cm -3 The dielectric thickness of the formed doped region is 1 nm to 1 μm.
4. The method according to claim 1, characterized in that: The gate comprises an interface oxide layer, a high-K dielectric layer and a metal gate in sequence from the outside to the inside.
5. The method according to claim 1, characterized in that: The annealing temperature ranges from 600°C to 1150°C.
6. The method according to claim 1, characterized in that: The annealing method includes rapid thermal annealing, spike annealing, laser annealing and a combination thereof.