Retroreflective relief structures in embossing lacquers

By adjusting the plane angle of the pyramid structure in the imprint mold, the problem of loss of retroreflective characteristics due to hardening and shrinking of the imprint paint is solved, and the retroreflective characteristics of the retroreflective film is maintained, and the mold is bent and flexible Weldability.

CN115666961BActive Publication Date: 2024-11-22GIESECKE & DEVRIENT CURRENCY TECHNOLOGY GMBH
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
CN202080101342.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-06-09
Publication Date
2024-11-22
Estimated Expiration
2040-06-09

AI Technical Summary

Technical Problem

The pyramidal prism structure used in the prior art for manufacturing a retroreflective film is no longer 90° due to anisotropic volume shrinkage during the hardening of the imprint paint, thus losing the retroreflective characteristics.

Method used

Design an imprint mold with an angle between the planes of the pyramidal prism structure formed after hardening is 90°-X. By adjusting the angles of the protrusions and concaves of the mold, the shrinkage of the paint is compensated and the retroreflective characteristics are ensured. Keep after hardening.

Benefits of technology

The retroreflective properties of the retroreflective film are effectively maintained and allow the imprint mold to be bent and welded after hardening, avoiding the laser beam reflection to damage the mold.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115666961B_ABST
    Figure CN115666961B_ABST
Patent Text Reader

Abstract

The invention relates to an embossing die for producing a planar retroreflector, which has a retroreflective corner-cube prism relief structure formed in a hardenable embossing lacquer, in particular a UV lacquer, and retroreflects electromagnetic radiation incident from the incident side. Here, the embossing die has a number n of mutually adjacent recesses and / or protrusions on one side, wherein each of the n recesses and / or protrusions is formed by three planes arranged at a specific angle (α') to each other. In addition, the invention relates to a method for producing such an embossing die. According to the invention, the specific angle (α') is less than 90° by a specific value X, i.e. α'=90°-X, so that the number n of mutually adjacent protrusions and / or recesses formed into the embossing lacquer by the embossing die, after the hardening of the hardenable embossing lacquer, each consists of three planes arranged at an angle of 90° to each other. The protrusions of the embossing die correspond to the recesses in the embossing lacquer and the recesses in the embossing die correspond to the protrusions of the embossing lacquer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an embossing mold for producing a planar retroreflector having a retroreflective corner-cube relief structure formed in a hardenable embossing lacquer, in particular a UV lacquer, and retroreflecting electromagnetic radiation incident from an incident side. In this case, the embossing mold has a number n of mutually adjacent recesses and / or elevations on one side, wherein each of the n recesses and / or elevations is formed by three planes arranged at a specific angle (α') to one another. The invention also relates to a method for producing such an embossing mold. Background Art

[0002] The retroreflective structure reflects incident electromagnetic radiation, such as light, in the direction of the radiation incidence, largely independent of the incident direction and the orientation of the reflector. This is called retroreflection. On the contrary, in a plane mirror, the back radiation depends on the mirror surface orientation, which is only oriented perpendicular to the observer in exceptional cases. A planar retroreflector has a large number of single retroreflectors arranged side by side. Retroreflective film is a common implementation form of a planar retroreflector. Retroreflective film is used in various ways in traffic technology, but also in security technology, for example, as an anti-counterfeiting element for verifying valuable documents, such as banknotes, credit cards or ID cards according to US2014 / 0226212 A1. Most traffic signs and truck signs are also equipped with retroreflective structures to improve visibility at night or improve anti-counterfeiting security (see US 5656360).

[0003] Two variants of retroreflectors are generally widely used: embedded highly refractive microspheres, which reflect on the bottom side, as described, for example, in US 4763985 and US 2009 / 0300953 A1. The optical principle here is based on so-called Luneburg lenses, which reflect the incident light in the direction of the radiation source. Another variant in the field to which the invention relates is based on a relief structure consisting of planes, a so-called corner-cube relief structure, which has the shape of a cube corner. Here, the incident light is deflected successively on three planes arranged at exactly 90° to each other (so-called prisms) and reflected towards the radiation source. This geometry has the highest retroreflection efficiency when the light is incident at right angles; the efficiency decreases with increasingly tilted incident light. The geometry of this structure known from the prior art is shown in FIG. Here, Figure 1aThe relief structure of a planar retroreflector is schematically shown in a side view, with a retroreflective light path. The retroreflector is designed as a film composite, which includes a carrier film 1 and a layer 2 made of embossing lacquer, wherein a reflective structure 3 is formed in the layer 2. The reflective structure 3 consists of planes that are arranged at an angle of 90° to each other, so that the incident radiation is deflected multiple times and finally retroreflected. Figure 1b The path of a retroreflection as occurs in the triangular facets of a prism is illustrated in a plan view, from which a retroreflective relief structure for a planar retroreflector can be formed by the successive arrangement of the triangular facets. Figure 1c and 1d Suitable cube-corner facets for the relief structure are shown in plan view or in perspective.

[0004] Retroreflective films for truck markings and road signs are usually produced in a hot embossing process, where the structure of the embossing mold is transferred almost intact into the thermoplastic.

[0005] For example, it is known from WO 2018 / 151959 A1, WO 2018 / 151960 A1 or WO 2018 / 151964 A1 to produce an embossing mold having a corner cube prism structure using a rotating engraving knife.

[0006] The corner-cube structures used for retroreflective films are highly demanding during embossing due to their depth, which is usually 15 μm to 80 μm. When embossing into a hardenable embossing lacquer, for example a UV lacquer that hardens after being irradiated with electromagnetic radiation in the ultraviolet (UV) wavelength range, a UV lacquer with very good fluidity is required in order to avoid the inclusion of air bubbles and to make it easier to demold the UV lacquer and the embossing mold. This UV lacquer, on the other hand, produces a relatively high volume shrinkage during its curing, which is not isotropic but more pronounced in a direction perpendicular to the film surface than in a horizontal direction, because the UV lacquer is fixed to the film in a form-fitting and friction-fitting manner. This "anisotropic" shrinkage leads to a flattening of the corner-cube structures and an increase in the corner-cube angle (depending on the lacquer viscosity, chemical composition, substrate, temperature, etc.).

[0007] However, a corner cube structure whose angle between the corresponding planes is no longer 90° but differs from 90° by more than + / - 0.5° almost completely loses its retroreflective properties. Summary of the invention

[0008] The technical problem to be solved by the present invention is to develop an embossing mold for a corner-cube prism structure of the type described in the present invention in such a way that the disadvantages of the prior art are eliminated. The technical problem to be solved by the present invention is to realize a retroreflective film having a corner-cube prism structure in an embossing lacquer, in particular a UV lacquer.

[0009] This object is achieved by an embossing tool for producing a planar retroreflector and a method for producing an embossing tool.

[0010] According to the invention, the specific angle (α') is smaller than 90° by a specific value X, i.e. α'=90°-X, so that the number n of mutually adjacent elevations and / or depressions formed (or embossed) into the embossing lacquer by the embossing die, after the curable embossing lacquer has hardened, each consists of three planes arranged at an angle of 90° to one another. The elevations of the embossing die correspond to the depressions in the embossing lacquer and the depressions in the embossing die correspond to the elevations of the embossing lacquer.

[0011] Therefore, the present invention provides a stamping die, which maintains or compensates for the shrinkage of the paint by manufacturing the stamping structure in a sharp manner. Therefore, the stamping die itself does not show retroreflective properties. This produces another special advantage of the present invention, that is, the stamping die according to the present invention can be bent into a tube or a tube segment and the adjacent edges of the tube or the adjacent edges of the adjacent tube segments can be welded to each other into an embossing roller by electromagnetic radiation, such as a laser beam. Because the laser beam reaches the structure of the stamping die that does not have retroreflectivity, the laser beam will not be reflected back to the laser in principle. On the contrary, for a stamping die with a retroreflective structure, the laser beam is reflected back to the laser in principle and may damage or destroy the laser.

[0012] According to the invention, a hardenable embossing lacquer is an embossing lacquer which is applied to a substrate as a carrier in a plastically deformable state and into which an embossed structure is formed by an embossing die. Such an embossing die is, for example, an embossing punch or an embossing cylinder. The embossing lacquer is then hardened, for example by means of UV radiation or thermal radiation, so that the embossing lacquer is no longer plastically deformable and the embossed structure can no longer be changed.

[0013] As radiation-hardening embossing lacquers, for example free-radical or cationically hardening lacquers are used, which can be used on a large number of substrates, such as PET, PVC, PE, PP, PMMA or PC. In order to stably fix the UV lacquer on the substrate, an adhesion-increasing intermediate layer can be used.

[0014] The embossing die according to the invention has a number n of mutually adjacent recesses. The geometry and dimensions of the number n of mutually adjacent protrusions formed in the hardenable embossing lacquer by this embossing die correspond to the corresponding recesses of the embossing die before the embossing lacquer is hardened. After the embossing lacquer is hardened, the geometry and dimensions of the protrusions in the embossing lacquer no longer correspond to the corresponding recesses of the embossing die. Due to the shrinkage during hardening, the protrusions are flattened, so that the angle between three planes arranged respectively to one another increases. According to the invention, the protrusions are flattened by a specific value X due to the shrinkage during hardening, so that the angle between three planes arranged respectively to one another is 90° and the protrusions exhibit retroreflective properties.

[0015] The specific angle (α') is less than 90° by the value of X, and during the curing process the embossing lacquer shrinks by the value of X, the value of X depending on the curable embossing lacquer used, the substrate to which the embossing lacquer is applied and the curing conditions, and the value of X is different for different curable embossing lacquers. If the value X is not known for the specific curable embossing lacquer in combination with the substrate to be used, the value X must be determined by preliminary tests. Here, a protrusion is formed in the embossing lacquer by a test embossing mold including a recess at a first angle α', and the angle α of the side of the resulting protrusion is measured after the embossing lacquer has hardened. The difference between the measured angle α and 90° results in a correction value, by which the angle α' must be corrected in the following process. This process is repeated as necessary until the angle α is equal to 90°.

[0016] For commercially available hardenable embossing lacquers, the specific value X usually has a value less than or equal to 3.5°, preferably 0.3° to 3.5°, so that the specific angle (α') is greater than or equal to 86.5°, preferably 86.5° to 89.7°. An embossing lacquer known from the prior art is, for example, a UV-hardenable hybrid polymer for micro-optical systems from the company "micro resist technology GmbH" under the model Ormocer. For example (as of July 2015), an embossing lacquer Or the relative volume shrinkage of "InkOrmo" is 5% to 7%, 4% to 6% for "OrmoCore" and "OrmoClad" 2% to 5%, 3% to 5% 10" is <2% and " 30” is <<2%.

[0017] X is therefore the value of the shrinkage of the embossing lacquer after hardening, which is usually 0.3° to 3.5°. For example, after UV embossing through an embossing mold with a recess with an opening angle α' of 90°, the structure in a specific UV lacquer shows an opening angle of 92.5° due to the shrinkage of the lacquer, i.e. X=2.5°. In order to reserve this shrinkage or this angle difference X in the next mold, the structure in the embossing mold is produced with a corner cube angle of 90°-2.5°=87.5°.

[0018] The design of the embossing mold depends on the structure of the retroreflective film, in particular on whether the observer views the cube-corner structure through the UV lacquer or through a layer that complementarily flattens the UV lacquer. In the first case, the mold will have recesses in the form of cube-corners, the opening angle of which is changed according to the invention with respect to the expected shrinkage of the lacquer. In the second case, the embossing mold will have projections of modified cube-corner shape, which leave corresponding recesses in the UV lacquer.

[0019] The invention also relates to a method for producing an embossing mold according to the invention. The embossing mold consists of a substrate, wherein a recess is introduced into one side of the substrate by means of a chisel, wherein the chisel has an angle of 70.52°-X at its tip. For example, such a chisel is made of diamond, solid carbide, HSS-Co, SiC, TiC, tungsten or TiCN.

[0020] In the prior art, the corresponding stamping molds are produced by diamond cutting. A diamond engraving tool with an angle of 70.52° at the tip is used here, which cuts a grid of parallel grooves in the base of the stamping mold. Next, two other grids are cut, which are twisted by 60° or 120° relative to the first grid. Thus, when using a diamond engraving tool with an angle of 70.52°, corner cubes with an opening angle α' of 90° will remain in the stamping mold.

[0021] The substrate of the stamping mold preferably consists of brass (an alloy of copper and zinc), copper, nickel, nickel phosphorus, nickel vanadium, nickel white copper (an alloy of nickel, copper and zinc) or cobalt. Softer carrier substrates are also often used, on the surface of which hard coatings such as Cr, CrN, Ti, TiN, carbides, W, DLC (diamond-like carbon) are deposited.

[0022] In order to produce an embossing mold according to the invention with a sharper opening angle of 90°-X, a correspondingly sharper diamond engraving tool is used, which has an angle of 70.52°-X at the tip. For example, for a paint shrinkage value of X=2.5°, a diamond engraving tool with an opening angle of 70.52°-2.5°=68.02° is required.

[0023] It goes without saying that the features mentioned above and those yet to be explained below can be used not only in the combination indicated but also in other combinations without departing from the scope of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The advantages of the present invention are described according to the following examples and the accompanying drawings. These examples represent preferred embodiments, but the present invention is by no means limited to these embodiments. In addition, for a better understanding, the views in the accompanying drawings are highly schematic and do not reflect the actual situation. In particular, the proportions shown in the accompanying drawings do not conform to the relationship existing in reality and are only used to improve intuitiveness. In addition, for a better understanding, the embodiments described in the following examples are simplified to basic core information. In actual implementation, much more complicated patterns or images can be applied.

[0025] In the accompanying drawings, schematically shown in detail:

[0026] FIG. 1 shows a planar retroreflector known from the prior art, in which Figure 1a The retroreflector is shown in a side view in FIG. Figure 1b The reverse reflection path occurring on the triangular face of the prism is shown in a top view in FIG. Figure 1c and 1d , suitable cube corner faces for the relief structure are shown in plan view or in perspective,

[0027] Figure 2 A first exemplary embodiment of a retro reflector produced by means of an embossing tool according to the invention is shown in a side view,

[0028] Figure 3 A first embodiment of an embossing tool according to the invention is shown in a side view,

[0029] Figure 4 shows that Figure 3 The hardenable embossing lacquer embossed by the embossing mold in the Figure 4a The middle is before the embossing varnish hardens. Figure 4b The middle is after the embossing paint has hardened.

[0030] Figure 5 A second exemplary embodiment of a retroreflector produced by means of an embossing tool according to the invention is shown in a side view,

[0031] Figure 6 A second embodiment of the embossing tool according to the invention is shown in a side view,

[0032] Figure 7 shows that Figure 6 The hardenable embossing lacquer embossed by the embossing mold in the Figure 7a The middle is before the embossing varnish hardens. Figure 7b The middle is after the embossing varnish has hardened. DETAILED DESCRIPTION

[0033] Figure 2 Schematically, as viewed from above, Figure 1a The side view, correspondingly looking at the top side of the embossing lacquer 2, shows a first embodiment of a retroreflector produced by means of an embossing tool according to the invention. The embossing lacquer 2 is shown as a dashed line before its hardening and as a solid line after its hardening. Before hardening, the side faces 3' of the embossed structure in the "valleys" of the embossed structure have an angle α' with one another. During the hardening process, the height of the embossed structure shrinks, so that after hardening, its side faces 3 in its "valleys" have an angle α=90° with one another.

[0034] Figure 3 A first embodiment of an embossing mold 4 is schematically shown in a side view, in which two recesses 5 are formed in one side of the embossing mold. The recesses 5 have side surfaces which are oriented at an angle α' to one another. FIG. 4 shows a curable embossing lacquer 2 embossed by such an embossing mold 4. Before the embossing lacquer 2 is cured, the embossing lacquer 2 is formed according to the Figure 4a , the geometry and size of the protrusions 3 'match the recesses 5 of the embossing mold 4. After the embossing lacquer 2 has hardened, according to Figure 4b , the height of the embossed structure shrinks so that its side faces 3 after hardening have an angle of α=90° with one another in their “valleys”.

[0035] Figure 5 A second embodiment of a retroreflector produced by means of an embossing tool according to the invention is shown schematically in a side view from below, i.e. through the embossing lacquer 2 onto the opposite side. In this case, the substrate 6 and the embossing lacquer 2 must be transparent, so that they allow the incident light to pass through with little attenuation and little scattering. In this case, the incident light is not as Figure 1a or Figure 2 or Figure 4b Instead of being reflected directly on the reflective upper side of the embossing lacquer as in the example above, the light is reflected only after passing through the transparent substrate 6 and the transparent embossing lacquer 2. Although the reflecting surface is the same in both cases, the opposite side of this surface reflects light.

[0036] according to Figure 2 , the embossing lacquer 2 is shown by dashed lines before curing and by solid lines after curing. Before curing, the side faces 3' of the embossed structure have an angle α' with each other at their tips. During the curing process, the height of the embossed structure shrinks, so that after curing, the side faces 3 have an angle α=90° with each other at their tips.

[0037] Figure 6A second embodiment of an embossing tool 4 is schematically shown in a side view, on one side of which three projections 8 are applied. The projections 8 have side surfaces which are oriented at an angle α' to one another. FIG. 7 shows a curable embossing lacquer 2 embossed by such an embossing tool. Before the embossing lacquer 2 is cured, the embossing lacquer 2 is formed according to the Figure 7a , the geometry and size of the recess 3 'matches the projection 8 of the embossing mold 7. After the embossing lacquer 2 has hardened, according to Figure 7b The height of the embossed structure shrinks so that after hardening its side faces 3 have an angle of α=90° with one another at their tips.

[0038] Figure 2 The illustrations up to FIG. 7 are not drawn to scale. For better clarity, the depth of the recesses 5 or the height of the protrusions 8 of the respective embossing mold 4 or 7 and the height of the protrusions before the embossing lacquer 2 hardens are shown in particular in a greatly exaggerated manner. Therefore, the angle α' is of course also shown to be sharper than in reality. On the contrary, the angle α is shown almost to scale as a 90° angle.

Claims

1. An embossing tool for producing a planar retroreflector having a retroreflective corner-cube relief structure formed in a hardenable embossing lacquer and retroreflecting electromagnetic radiation incident from an incident side, wherein: The embossing mold has a number n of mutually adjacent recesses and / or protrusions on one side, wherein each of the n recesses and / or protrusions is formed by three planes arranged at a specific angle (α') to each other, characterized in that the specific angle (α') is smaller than 90° by a specific value X, so that the n recesses and / or protrusions molded into the hardenable embossing lacquer by the embossing mold are respectively composed of three planes arranged at an angle of 90° to each other after the embossing lacquer is hardened.

2. The embossing mold according to claim 1, characterized in that The value of X depends on the curable embossing lacquer used, the curing conditions and the substrate to which the embossing lacquer is applied and is different for different curable embossing lacquers.

3. The embossing mold according to claim 2, characterized in that The specific value X has a value less than or equal to 3.5°, so the specific angle (α′) is greater than or equal to 86.5°.

4. The embossing mold according to claim 1, characterized in that The embossing lacquer is a UV lacquer.

5. The embossing mold according to claim 3, characterized in that The specific value X has a value of 0.3° to 3.5°, so the specific angle (α′) is 86.5° to 89.7°.

6. A method for producing an embossing mold according to one of the preceding claims, characterized in that The embossing mold consists of a substrate, wherein recesses and / or elevations are introduced into one side of the substrate by means of an engraving tool, wherein the engraving tool has an angle of 70.52°-X at its tip.

Citation Information

Patent Citations

  • Semi-transparent retroreflective sheet and use thereof to make a backlit license plate

    US20090300953A1

  • Security devices

    US20140226212A1

  • Retroreflective sheet with enhancer brightness

    US4763985A

  • Article with holographic and retroreflective features

    US5656360A

  • End milling methods for making microstructures, especially CUBE corner elements and articles comprising such microstructures

    WO2018151959A1