A metal-coated composite semiconductor material and its preparation method and photoelectric detection, photocatalysis and wave absorption applications
Through metal-semiconductor interaction and ultrasonic-assisted-in-situ photosynthesis, the light absorption range and charge separation efficiency of semiconductor materials are broadened, and the problems of narrow response range and poor compatibility of existing materials are solved, thus achieving the full solar spectrum and long range Effective response and efficient photocatalysis of infrared light.
Patent Information
- Application Number
- CN202211425240.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-14
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-11-14
AI Technical Summary
The existing semiconductor materials have narrow light absorption range and low photogenerated charge separation efficiency, making it difficult to meet the response needs of the full solar spectrum and medium and far infrared light. The traditional improved methods have problems such as poor compatibility and non-compatibility in line with green chemistry requirements.
Through metal-semiconductor interaction, metal elemental nanoparticles are used to coat semiconductor materials, broaden the light absorption range and improve charge separation efficiency, and ultrasonic-assisted in-situ photosynthesis method is used to introduce metal nanoparticles at the semiconductor surface interface to form composite semiconductor materials.
It realizes broad spectrum light response to far-infrared and terahertz bands, improves photoelectric detection and photocatalytic efficiency, combines green synthesis and military stealth performance, has good material compatibility, and meets green chemistry requirements.
Smart Images

Figure GDA0004870972100000081 
Figure GDA0004870972100000091 
Figure GDA0004870972100000092
Abstract
Description
Technical Field
[0001] The present application relates to a metal-coated composite semiconductor material and a preparation method thereof, as well as photoelectric detection, photocatalysis, and wave absorption applications, and belongs to the field of semiconductor materials. Background Art
[0002] Semiconductors refer to materials whose electrical conductivity is between that of conductors and insulators at room temperature. From the perspective of electronic band structure, semiconductors have a band gap that allows free carriers to be promoted to the conduction band. At present, semiconductors have spread to all aspects of people's lives. Therefore, from the perspective of science and technology or economic development, the importance of semiconductors is very huge. The photoelectric effect of semiconductors has always been the research focus in the semiconductor field. Photocatalysis and photoelectric detection are two important research directions using the photoelectric effect of semiconductors. Broadening the light response range of semiconductors and improving the charge separation efficiency of semiconductors have always been difficult problems in the semiconductor field.
[0003] With the increase of population and the development of human society and economy, more and more energy needs to be used. At present, fossil energy still accounts for the majority of global energy consumption. Fossil energy cannot be regenerated after development and utilization. If it is mined on a large scale for a long time, it will be exhausted in the near future. The use of fossil energy is bound to emit a large amount of carbon dioxide. With the emission of carbon dioxide in various countries, greenhouse gases have soared, causing a series of environmental problems such as glacier melting, sea level rise, and ocean acidification, posing a threat to the life system. Climate change is a global problem facing mankind. Therefore, it is extremely important to pursue the green utilization of greenhouse gases such as carbon dioxide and develop carbon-neutral green energy and chemical production processes. As one of the recyclable clean energy sources, sunlight has attracted widespread attention from the international community and the scientific community. Sunlight can irradiate most parts of the earth, and the energy of the sun is extremely huge. Scientists have calculated that it has a period of at least six million years. For humans, such a time is unlimited. The most used fossil energy today has the problem of waste discharge. The more energy is depleted, the more pollution is generated. Although nuclear energy is a highly efficient way of generating electricity, it has the risk of nuclear leakage, which will cause a great ecological crisis. Solar energy is non-hazardous and non-polluting. Under the principle of peaceful coexistence between humans and nature, the use of solar energy is the greenest and safest. If the equipment is used properly, the cost of the installation is very low, and it can produce at least 10 17Kilowatts of electricity. The use of sunlight for photocatalytic production of hydrogen can achieve green production of green high calorific value fuels; the use of sunlight for photocatalytic carbon dioxide reduction can realize the conversion of greenhouse gases into industrial raw materials or industrial primary products; the use of sunlight for photocatalytic carbon-hydrogen bond activation and other chemical reactions can realize chemical reactions and conversions under mild conditions, and the use of photocatalytic reactions can control the emission of carbon pollution from the source of the reaction. Therefore, the use of solar photocatalytic reactions has become one of the most promising chemical methods currently receiving much attention. In order to improve the catalytic efficiency of semiconductor photocatalysts, the commonly used strategies currently include designing new single-component semiconductor photocatalysts and improving existing semiconductor photocatalysts. Among them, the introduction of semiconductor-semiconductor heterojunctions and metal-semiconductor Schottky junctions are often used to improve the performance of existing semiconductor photocatalysts. However, the optimization methods for forming junctions often have problems such as poor compatibility between the "guest" and "host" materials, and the synthesis methods do not meet the requirements of green chemistry and are not economical. Therefore, developing composite materials of "guest" and "host" with good compatibility, which can greatly broaden the light response range of semiconductor materials and significantly improve charge separation, is of great practical significance for promoting the green industrialization of semiconductor material photocatalysis.
[0004] With the rapid development of the information age, semiconductors, as the high-tech core of this era, have an important measurement parameter in the fields of photoelectric detection and solar energy conversion. At present, the light response range of commercial materials is relatively narrow. For example, the light response range of Si-based and Ge-based semiconductors is in the visible light region, and the light response range of InGaAs-based semiconductors is in the short-wave infrared region. They cannot cover the entire solar spectrum. To achieve the photoelectric response of the entire solar spectrum, at least two semiconductor devices need to be combined to meet the detection needs, which will lead to complex equipment, difficult maintenance, and high cost. In addition, improving national defense security and military strength is an important prerequisite for consolidating a country's international status. This makes it particularly important for key equipment to be multi-band stealth and perception of enemy detection light spectra such as the full solar spectrum (about 295-2500 nanometers), even mid- and far-infrared light (about 2500 nanometers-1 mm) and radar waves (about 1 mm-100 meters). Therefore, the development of ultra-wideband absorption and response semiconductor materials has important national defense significance. Summary of the invention
[0005] According to the first aspect of the present application, a coated composite semiconductor material is provided. The composite semiconductor material utilizes metal-semiconductor interaction to solve the problem of narrow semiconductor light absorption range or low photogenerated charge separation efficiency. Metal-semiconductor interaction includes but is not limited to metal-semiconductor Schottky junction, surface plasmon resonance metal-semiconductor interaction, metal hot electron injection semiconductor interaction, etc. Compared with the traditional method of improving the light absorption range or charge separation efficiency of semiconductor materials, the coating material of the present invention is introduced into the semiconductor surface interface later through a green photosynthesis method without the introduction of other species. In addition to retaining the photoelectric response performance of the initial semiconductor, the method of introducing metal single substance nanoparticles in post-processing can improve the photoelectric response range and (or) charge separation efficiency of semiconductor materials, and can broaden the light absorption range to the far infrared and terahertz bands.
[0006] This composite semiconductor material can be used as a photoelectric detection material, and the photocurrent / dark current response of ultraviolet-visible-infrared light is greater than 10. It can also be used as a photocatalyst, a stable catalyst for reactions such as photolysis of water to produce hydrogen, carbon dioxide reduction, and carbon-hydrogen bond activation, and can achieve green photochemical synthesis. It is worth mentioning that the light absorption range of this semiconductor material is wider than that of other documents. For example, under the condition of a xenon lamp simulating AM1.5 sunlight, the zinc sulfide semiconductor material coated with elemental zinc nanoparticles has the performance of wide-spectrum absorption, and the efficiency of hydrogen production does not decrease significantly within 48 hours. The coated wide-spectrum photoelectric response semiconductor material of the present invention can be used as a wave-absorbing stealth material, and can have an absorption effect in the mid- and far-infrared and even terahertz bands.
[0007] A metal-coated composite semiconductor material, comprising metal single substance nanoparticles and a semiconductor;
[0008] The metal element nanoparticles are coated on the surface and / or inside of the semiconductor.
[0009] Optionally, the metal element nanoparticles form a metal-semiconductor interaction with the semiconductor.
[0010] Optionally, the metal-semiconductor interaction includes a metal-semiconductor Schottky junction, a surface plasmon resonance metal-semiconductor interaction, and a metal hot electron injection semiconductor interaction.
[0011] Optionally, the metal element nanoparticles are derived from the semiconductor.
[0012] Optionally, the mass of the metal element nanoparticles accounts for 0.1% to 10% of the total mass of the composite semiconductor material.
[0013] Optionally, the mass of the metal element nanoparticles accounts for 0.5% to 5% of the total mass of the composite semiconductor material.
[0014] Optionally, the mass proportion of the metal element nanoparticles is independently selected from any value among 0.1%, 0.5%, 1.0%, 2%, 3%, 4%, 5%, 6%, 7%, 8%, 9%, 10% or any range between two values.
[0015] Optionally, the semiconductor is micrometer-scale and / or nanometer-scale.
[0016] Optionally, the size of the semiconductor is 50 nm to 10 μm.
[0017] Optionally, the size of the semiconductor is 50nm to 200nm.
[0018] Optionally, the semiconductor is selected from chalcogenide semiconductors.
[0019] Optionally, the semiconductor is selected from at least one of ZnO, CdO, ZnS, CdS, Ag2S, AgGaS2, and In2Se3.
[0020] Optionally, the size of the semiconductor is independently selected from any value among 50nm, 100nm, 200nm, 300nm, 400nm, 500nm, 600nm, 700nm, 800nm, 900nm, 1μm, 2μm, 3μm, 4μm, 5μm, 6μm, 7μm, 8μm, 9μm, 10μm or any range therebetween.
[0021] Optionally, the metal element nanoparticles are selected from at least one of Zn, Cd, Ag and In.
[0022] Optionally, the average particle size of the metal element nanoparticles is 10 nm to 100 nm.
[0023] Optionally, the average particle size of the metal element nanoparticles is 30 nm to 60 nm.
[0024] Optionally, the average particle size of the metal element nanoparticles is independently selected from any value among 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm, 100 nm, or any range value between two thereof.
[0025] According to the second aspect of the present application, a method for preparing a composite semiconductor material is provided. The method adopts ultrasound-assisted in-situ photosynthesis to prepare a coated semiconductor material. Traditional methods for improving the photoelectric response range of semiconductors and (or) the efficiency of photogenerated charge separation require a lot of effort to improve the compatibility of the "guest" material and the "host" semiconductor. Compared with other traditional methods, the in-situ photosynthesis method of the present invention is more compatible with each other in the "guest" material and the "host" of the synthesized material. In addition, this in-situ photosynthesis method meets the requirements of green chemistry and does not require the introduction of other species. The initial semiconductor material is irradiated with ultraviolet light while being ultrasonicated, and metal nanoparticles can be generated in situ by utilizing the photochromic phenomenon or photocorrosion phenomenon of the initial semiconductor.
[0026] The method for preparing the composite semiconductor material comprises the following steps:
[0027] The mixture containing semiconductor is placed in a container, and ultrasonic and ultraviolet light are applied to obtain the composite semiconductor material.
[0028] Optionally, the ultrasonication time is 10 min to 30 min.
[0029] Optionally, the ultrasonication time is 20 min to 30 min.
[0030] Optionally, the ultrasound time is independently selected from any value of 10 min, 12 min, 14 min, 16 min, 18 min, 20 min, 22 min, 24 min, 26 min, 28 min, 30 min, or any range between two thereof.
[0031] Optionally, the light source of ultraviolet light is selected from any one of a high-pressure mercury lamp, an ultraviolet LED lamp, a xenon lamp containing an ultraviolet band, and an ultraviolet band laser.
[0032] Optionally, the ultraviolet irradiation time is 1 h to 12 h.
[0033] Optionally, the ultraviolet irradiation time is 4h to 6h.
[0034] Optionally, the time of ultraviolet irradiation is independently selected from any value of 1 h, 2 h, 4 h, 6 h, 8 h, 10 h, 12 h, or any range between two of them.
[0035] Optionally, the following steps are included:
[0036] The semiconductor is placed in a container and irradiated with ultrasound and ultraviolet light to obtain the composite semiconductor material.
[0037] Optionally, ultrasound and ultraviolet light irradiation are performed simultaneously.
[0038] According to a third aspect of the present application, an application of a composite semiconductor material is provided.
[0039] Application of the composite semiconductor material described above and / or the composite semiconductor material obtained by the preparation method described above in photocatalysis, wide-spectrum photoelectric detection, and intelligent wave-absorbing stealth.
[0040] Optionally, the composite semiconductor material converts light with a wavelength greater than 300 nanometers into an electrical signal at a voltage of -20V to 20V.
[0041] Optionally, the composite semiconductor material has a photocurrent / dark current response greater than 10 to ultraviolet-visible-infrared light.
[0042] Optionally, the composite semiconductor material absorbs light greater than 2500 nanometers.
[0043] Optionally, the composite semiconductor material has an absorption effect on the terahertz band spectrum.
[0044] Optionally, the hydrogen production efficiency of the composite semiconductor material remains unchanged within 48 hours under irradiation of a 300W AM1.5 sunlight simulated xenon lamp.
[0045] According to one embodiment of the present application, ultrasound-assisted in-situ photosynthesis is used for preparation. The preparation steps are as follows:
[0046] (1) placing the initial semiconductor in a quartz container and ultrasonically coating the bottom of the quartz container with the initial semiconductor;
[0047] (2) During the ultrasonic process, under the irradiation of ultraviolet light, a coated semiconductor material is obtained.
[0048] The initial semiconductor described in step (1) can be any one or more of common chalcogenide compound semiconductors (such as ZnO, CdO, ZnS, CdS, Ag2S, AgGaS2, In2Se3, etc.), preferably a metal compound containing Zn.
[0049] The ultrasonic time in step (1) is cumulatively 10-30 minutes, preferably 30 minutes.
[0050] The ultraviolet lamp described in step (2) can be any one of a high pressure mercury lamp, an ultraviolet LED lamp, a xenon lamp containing an ultraviolet band, and an ultraviolet band laser, preferably a xenon lamp containing an ultraviolet band.
[0051] The illumination time in step (2) is 1-12 hours in total, preferably 6 hours.
[0052] The purpose of the present invention is to be used for photocatalysis and realize green photochemical synthesis. A photocatalytic reactor is used to disperse the coated semiconductor material as a photocatalyst in a reactant environment, and the target product is obtained under the irradiation of a xenon lamp.
[0053] The invention is used for wide-spectrum photoelectric detection, and can realize wide-spectrum photoelectric detection of a single semiconductor material. A semiconductor tester is used to prepare a coated semiconductor into a photoelectric detection device, and at a voltage of -20V-20V, the light with a wavelength greater than 300 nanometers is converted into an electrical signal by using a photoelectric response to realize photoelectric detection.
[0054] The purpose of the present invention is to absorb and sense the light waves of military detection, and realize the intelligent stealth of military equipment. The coated semiconductor has an absorption effect on light greater than 2500 nanometers, and even on the terahertz band spectrum. Combined with the wide-spectrum photoelectric detection performance, it can realize the electrical response to the radar band, sense being detected, and realize intelligent stealth.
[0055] The beneficial effects of this application include:
[0056] 1) A composite semiconductor material provided by the present application, compared with the initial semiconductor, the coated semiconductor material of the present invention introduces metal nanoparticles in situ into the surface and (or) the interior of the initial semiconductor. The light response range of the semiconductor material is broadened and the charge separation efficiency is improved through metal-semiconductor interaction, wherein the metal-semiconductor interaction includes but is not limited to metal-semiconductor Schottky junction, surface plasmon resonance metal-semiconductor interaction, metal hot electron injection semiconductor interaction, etc.; it can be used as a stable and efficient photocatalyst for photocatalysis, a wide-spectrum photoelectric detection semiconductor material, and a military intelligent wave absorbing material. It has practical significance for realizing green synthesis of photocatalysis, wide-spectrum photoelectric detection of a single semiconductor material, and intelligent stealth of military equipment. The coated semiconductor material has the performance of a wide light response range and high charge separation. Zn-coated ZnS, under the irradiation of 300W AM1.5 sunlight simulated xenon lamp, the hydrogen production efficiency remains basically unchanged within 48 hours; it can realize photoelectric detection of 300W xenon lamp with an output wavelength greater than 420 nanometers; the absorption range can reach the terahertz band.
[0057] 2) The present application provides a method for preparing a composite semiconductor material. Compared with the traditional semiconductor optimization method, the coated semiconductor material of the present invention is introduced through a later in-situ photoreaction, retaining the basic properties of the initial semiconductor, and this optimization method can solve the problem of poor compatibility between the "guest" material and the "host" semiconductor, and this photochemical synthesis method meets the requirements of green chemistry without the introduction of other species. BRIEF DESCRIPTION OF THE DRAWINGS
[0058] Figure 1This is the absorption spectrum of the encapsulated semiconductor material to ultraviolet-visible-infrared light in Example 1. This figure shows that the encapsulated semiconductor material has an ultra-wide spectral absorption range.
[0059] Figure 2 This is a reflection loss diagram of the clad semiconductor material in the terahertz band in Example 2. This diagram shows that the clad semiconductor material has absorption in the terahertz band.
[0060] Figure 3 The photoelectric response diagram of the coated semiconductor material in Example 8 and Example GG to 300W xenon lamp light with a wavelength greater than 800 nanometers is shown in the figure. The figure shows that the coated semiconductor material can achieve photoelectric detection of visible light-infrared light.
[0061] Figure 4 This is a time-space yield diagram of the coated semiconductor material in Example 2 in the sunlight-simulated photolysis of water to produce hydrogen. The catalyst evaluation conditions are shown in Example A. This diagram shows that the coated semiconductor material has good hydrogen production performance and stability. DETAILED DESCRIPTION
[0062] The present application is described in detail below with reference to embodiments, but the present application is not limited to these embodiments.
[0063] Unless otherwise specified, the raw materials in the examples of this application were purchased through commercial channels.
[0064] Example: Preparation of coated semiconductor materials using ultrasound-assisted in-situ photosynthesis
[0065] A certain amount of initial semiconductor was placed in a 50 mL quartz beaker. Ultrasound was used to make the initial semiconductor evenly cover the bottom of the quartz beaker. Ultrasound was used to irradiate with ultraviolet light to obtain a coated semiconductor material. The specific experimental parameters of the 8 catalyst preparation examples are shown in Table 1.
[0066] Table 1. Experimental parameters for the preparation of coated semiconductors
[0067]
[0068] Evaluation of Hydrogen Production by Solar-Simulated Water Decomposition
[0069] A certain amount of coated semiconductor material photocatalyst was placed in a photocatalytic reactor, 100 mL of sacrificial agent solution was added, and argon was bubbled for 0.5-2 hours to remove all oxygen in the reactor. The reactor was irradiated with sunlight to simulate the xenon lamp, and argon with a flow rate of 1-5 mL / min was used as a carrier gas to detect the hydrogen evolution efficiency online. The specific test conditions of the 7 catalyst evaluation examples are shown in Table 2.
[0070] Table 2. Experimental parameters for catalyst evaluation
[0071]
[0072]
[0073] The photocatalyst hydrogen production efficiency is calculated using the following formula:
[0074] Space Time Yield (STY) = (p·α·A·v Flow ) / (R·T·m)
[0075] p-pressure (N·m -2 ), α-chromatographic calibration factor (1.73×10 -8 ), A-chromatographic integrated peak area, v Flow -Gas flow rate at the end of the reaction device (m 3 ·h -1 ), R-universal gas constant (8.3145N·m·mol -1 ·K -1 ), T-room temperature (298K), m-catalyst mass (g)
[0076] Evaluation of broadband photoelectric detection performance
[0077] A certain amount of coated semiconductor material is prepared into a photoelectric detection device, and the photoelectric performance is tested using a semiconductor tester or an electrochemical workstation. The photoelectric detection is tested under a bias voltage of -20V-20V. The specific test conditions of the 8 photoelectric detection device evaluation embodiments are shown in Table 3.
[0078] Table 3 Experimental parameters for semiconductor photodetection evaluation
[0079]
[0080]
[0081] The above are only a few embodiments of the present application and do not constitute any form of limitation to the present application. Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases and fall within the scope of the technical solution.
Claims
1. A metal-clad composite semiconductor material, It is characterized in that The composite semiconductor material includes metal single substance nanoparticles and semiconductor; The metal element nanoparticles are coated on the surface and / or inside of the semiconductor; The metal-coated composite semiconductor material is prepared by an in-situ photosynthesis method without introducing other species; The method for preparing the composite semiconductor material comprises the following steps: Placing a mixture containing a semiconductor in a container, and subjecting it to ultrasound and ultraviolet light to obtain the composite semiconductor material; The semiconductor is selected from chalcogenide semiconductors; The metal element nanoparticles are from the semiconductor; The semiconductor is selected from ZnO, CdO, ZnS, CdS, Ag 2 S, AgGaS 2 、In 2 Se 3 At least one of .
2. The composite semiconductor material according to claim 1, It is characterized in that The metal element nanoparticles and the semiconductor form a metal-semiconductor interaction.
3. The composite semiconductor material according to claim 1, It is characterized in that The metal-semiconductor interaction includes metal-semiconductor Schottky junction, surface plasmon resonance metal-semiconductor interaction, and metal hot electron injection semiconductor interaction.
4. The composite semiconductor material according to claim 1, It is characterized in that The mass of the metal single substance nanoparticles accounts for 0.1% to 10% of the total mass of the composite semiconductor material.
5. The composite semiconductor material according to claim 1, It is characterized in that The mass of the metal single substance nanoparticles accounts for 0.5% to 5% of the total mass of the composite semiconductor material.
6. The composite semiconductor material according to claim 1, It is characterized in that The semiconductor is of micrometer scale and / or nanometer scale.
7. The composite semiconductor material according to claim 1, It is characterized in that The size of the semiconductor is 50nm-10μm.
8. The composite semiconductor material according to claim 1, It is characterized in that The metal single substance nanoparticles are selected from at least one of Zn, Cd, Ag and In.
9. The composite semiconductor material according to claim 1, It is characterized in that The average particle size of the metal single substance nanoparticles is 10nm to 100nm.
10. The composite semiconductor material according to claim 1, It is characterized in that The average particle size of the metal single substance nanoparticles is 30nm to 60nm.
11. A method for preparing the composite semiconductor material according to any one of claims 1 to 10, It is characterized in that The following steps are involved: The mixture containing semiconductor is placed in a container, and ultrasonic and ultraviolet light are applied to obtain the composite semiconductor material.
12. The preparation method according to claim 11, It is characterized in that The ultrasonic time is 10min to 30min.
13. The preparation method according to claim 11, It is characterized in that The ultrasound time is 20min to 30min.
14. The preparation method according to claim 11, It is characterized in that The light source of ultraviolet light is selected from any one of a high pressure mercury lamp, an ultraviolet LED lamp, an ultraviolet xenon lamp, and an ultraviolet laser.
15. The preparation method according to claim 11, It is characterized in that The UV exposure time is 1h to 12h.
16. The preparation method according to claim 11, It is characterized in that The UV exposure time is 4h to 6h.
17. The preparation method according to claim 11, It is characterized in that The following steps are involved: The semiconductor is placed in a container and irradiated with ultrasound and ultraviolet light to obtain the composite semiconductor material.
18. The preparation method according to claim 11, It is characterized in that Ultrasound and ultraviolet light are carried out simultaneously.
19. Application of the composite semiconductor material according to any one of claims 1 to 10 and / or the composite semiconductor material obtained by the preparation method according to any one of claims 11 to 18 in photocatalysis, wide-spectrum photoelectric detection, and intelligent wave-absorbing stealth.
20. The use according to claim 19, It is characterized in that The composite semiconductor material converts light with a wavelength greater than 300 nanometers into an electrical signal under a voltage of -20V to 20V.
21. The use according to claim 19, It is characterized in that The composite semiconductor material has a photocurrent / dark current response greater than 10 to ultraviolet-visible-infrared light.
22. The use according to claim 19, It is characterized in that The composite semiconductor material has an absorption effect on light with a wavelength greater than 2500 nanometers.
23. The use according to claim 19, It is characterized in that The composite semiconductor material has an absorption effect on the terahertz band spectrum.
24. The use according to claim 19, It is characterized in that The hydrogen production efficiency of the composite semiconductor material remains unchanged within 48 hours under irradiation of a 300W AM1.5 sunlight simulated xenon lamp.