A method for purifying 3-chloropropylene containing ether impurities

By reacting with hydrogen chloride at low temperatures with the bimetallic catalyst Ni-Ce(H+)/Zr-MCM-41, the problem of difficult separation of allyl methyl ether impurities in the epoxychlorohydrin process by hydrogen peroxide method is solved, and high efficiency is achieved 3-chloropropylene purification and high-quality production of epoxypropylene products reduce process costs and energy consumption.

CN116041140BActive Publication Date: 2024-12-03WANHUA CHEM GRP CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310001802.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-01-03
Publication Date
2024-12-03
Estimated Expiration
2043-01-03

AI Technical Summary

Technical Problem

In the existing hydrogen peroxide method, it is difficult to effectively separate allyl methyl ether impurities, resulting in a decrease in hydrogen peroxide utilization rate and the purity of epoxy chlorohydrin products. The existing methods have high cost, high energy consumption, and environmental Great impact.

Method used

The solid acid catalyst Ni-Ce(H+)/Zr-MCM-41, supported by bimetals, reacts with hydrogen chloride gas at low temperatures to effectively remove allyl methyl ether impurities, improve the purification effect of 3-chloropropylene, and pass The recycling of catalysts reduces process costs.

Benefits of technology

Achieve the removal rate of allyl methyl ether by more than 95%, reduce the loss of 3-chloropropylene and methanol, improve the purity and process efficiency of epoxychlorohydrin products, and the process flow is simple, energy consumption is low, and investment is Low cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004034259470000141
    Figure BDA0004034259470000141
Patent Text Reader

Abstract

The present invention provides a method for purifying 3-chloropropylene containing ether impurities. The method uses 3-chloropropylene containing allyl methyl ether impurities as a raw material, and reacts the 3-chloropropylene with a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41 is catalyzed, and reacts with hydrogen chloride gas at low temperature to obtain a 3-chloropropylene product from which allyl methyl ether is removed. The method of the present invention can not only effectively remove allyl methyl ether, but also improve the quality of the product in the process of preparing epichlorohydrin by hydrogen peroxide, and can further increase the output of allyl chloride and methanol, thereby reducing the unit consumption of epichlorohydrin products, and has the advantages of simple process flow, mild reaction conditions, recyclable catalyst, low investment cost, and allyl methyl ether removal rate of more than 95%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of separation, purification and recovery, and in particular to a method for purifying 3-chloropropene containing ether impurities, and in particular to a method for purifying 3-chloropropene containing allyl methyl ether recovered in a production process of epichlorohydrin by a hydrogen peroxide method. Background Art

[0002] Epichlorohydrin, also known as epichlorohydrin, is a volatile, unstable, transparent, colorless liquid. It is an important organic chemical raw material and intermediate, mainly used in the synthesis of epoxy resins, as well as downstream products such as glycerin, epichlorohydrin rubber, pesticides, and plasticizers.

[0003] The main methods for industrial production of epichlorohydrin include the chlorohydrin method, the glycerin method and the hydrogen peroxide method. Among them, the chlorohydrin method has a mature production process, but has disadvantages such as high reaction temperature, many by-products, severe equipment corrosion and large discharge of three wastes; the glycerin method has a low technical threshold, but this method has high process energy consumption, low equipment utilization, and is dependent on the supply of the main raw material glycerin, and inevitably produces saponification wastewater; compared with the above two technologies, the hydrogen peroxide method produces less wastewater and is a green and environmentally friendly process for preparing epichlorohydrin, and is listed as an encouraged industry.

[0004] At present, the most commonly used hydrogen peroxide production technology is to use titanium silicon molecular sieve as a catalyst, and hydrogen peroxide and 3-chloropropylene are directly oxidized in methanol solvent to prepare epichlorohydrin. This process uses methanol as a solvent, which can effectively ensure a high conversion rate of hydrogen peroxide and a high selectivity of epichlorohydrin, and enable the molecular sieve to maintain excellent catalytic activity for a long period of time. However, this reaction system will inevitably produce allyl methyl ether impurities as a by-product. The boiling points of allyl methyl ether and 3-chloropropylene differ by 1-3°C, and it is difficult for the solvent recovery process to achieve separation requirements through ordinary distillation. If this impurity is significantly accumulated in the 3-chloropropylene reaction process, it will not only reduce the utilization rate of hydrogen peroxide, but also make it difficult for the purity of the epichlorohydrin product to meet the requirements of high-quality products.

[0005] CN112778080A reports a method for recovering 3-chloropropene without allyl methyl ether from epichlorohydrin reaction solution. The invention effectively reduces the content of allyl methyl ether in 3-chloropropene through a method consisting of multi-stage distillation and extractive distillation, and reduces the impact of recovering 3-chloropropene on catalysts and products. However, the method introduces a third component, and the separation process is relatively long, the equipment investment is large, and the process energy consumption is high.

[0006] CN111960921A discloses a method and device for recovering allyl chloride and methanol from the water layer of the epichlorohydrin process by hydrogen peroxide method. In order to effectively prevent the proliferation of allyl methyl ether in the distillation separation process, the invention adopts a washing + adsorption method to achieve the separation of allyl methyl ether and 3-chloropropene. However, organic wastewater is generated in the process of washing and separating methanol and hot water desorption and regeneration of the adsorbent, which increases the cost of three waste treatment.

[0007] Therefore, it is urgent to develop a method for purifying 3-chloropropene containing allyl methyl ether with good separation effect, low process cost and environmental friendliness, so as to benefit the industrial production of the process of preparing epichlorohydrin from hydrogen peroxide. Summary of the invention

[0008] In view of the above problems existing in the prior art, the present invention aims to provide a method for purifying 3-chloropropene containing ether impurities, and more specifically, to a method for purifying 3-chloropropene containing allyl methyl ether recovered in a hydrogen peroxide process for producing epichlorohydrin.

[0009] The purification method of the present invention can not only effectively remove the allyl methyl ether impurity in 3-chloropropene and improve the quality of the product in the process of preparing epichlorohydrin by hydrogen peroxide, but also can further improve the recovery rate of 3-chloropropene and methanol and reduce the unit consumption of epichlorohydrin product.

[0010] The invention has the advantages of low investment cost, mild reaction conditions, and an allyl methyl ether removal rate of more than 95%.

[0011] In order to achieve the above invention object, the technical solution provided by the present invention is as follows:

[0012] The present invention provides a method for purifying 3-chloropropylene containing ether impurities. The method uses 3-chloropropylene containing allyl methyl ether impurities as a raw material, and purifies the 3-chloropropylene in a solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41 is used as catalyst to react with hydrogen chloride gas at low temperature to obtain 3-chloropropylene product from which allyl methyl ether has been removed.

[0013] In the present invention, the 3-chloropropylene containing ether impurities is 3-chloropropylene containing allyl methyl ether impurities, which contains 3-chloropropylene, allyl methyl ether impurities, and methanol and / or water. Specifically, the 3-chloropropylene containing ether impurities suitable for the purification method of the present invention has a content of 10-98wt% of chloropropylene, a content of 0.01-10wt% of allyl methyl ether impurities, and methanol and / or water, wherein the content of methanol is 0-88wt% and the content of water is 0-0.1wt%. In the 3-chloropropylene raw material containing ether impurities of the present invention, the water content is required to be controlled below 0.1%. If it exceeds this limit, the conventional method in the art, such as using 5A molecular sieve or ZSM-5 molecular sieve, can be used to adsorb and remove water to control it below the limit.

[0014] In the present invention, the 3-chloropropylene containing ether impurities is derived from the separation process of the process of preparing epichlorohydrin by hydrogen peroxide method. This method is a known process in the prior art and is not particularly required by the present invention; specifically, the source of the 3-chloropropylene containing allyl methyl ether involved in the present invention includes but is not limited to the process of extracting oil phase distillation to recover 3-chloropropylene and the process of recovering methanol from the raffinate water phase in the process of preparing epichlorohydrin by hydrogen peroxide method. In this process, the reaction liquid is extracted and separated to obtain an extracted oil phase and a raffinate water phase, wherein the reaction liquid mainly contains 3-chloropropylene, methanol, epichlorohydrin and water; the extracted oil phase includes epichlorohydrin and 3-chloropropylene, and after ordinary distillation separation, the recovered 3-chloropropylene is obtained at the top of the tower; the raffinate water phase contains methanol, water and a small amount of chloropropylene, and after ordinary distillation separation, the recovered methanol is obtained at the top of the tower. Both the recovered 3-chloropropylene and the recovered methanol contain allyl methyl ether impurities and are suitable for the purification method of the present invention.

[0015] In the present invention, the bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, based on the total mass of the catalyst, wherein the Ni content is 1.8-3.5wt%, preferably 2.0-2.8wt%, the Ce content is 1.5-2.7wt%, preferably 1.9-2.3wt%; the Zr content in the carrier Zr-MCM-41 is 3.6-9.4wt%, preferably 5.0-6.7wt%.

[0016] In the present invention, the bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, which can be prepared by conventional supported catalyst preparation methods in the art, such as impregnation method, and the present invention has no special requirements; in some specific examples of the present invention, as a preference, the supported bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41 is prepared by the method comprising the steps of:

[0017] (1) impregnating an organic zirconium salt, MCM-41 molecular sieve, and an organic solvent, adjusting the pH to 3-4 with a composite solution of propionic acid and nitric acid under rapid stirring, and then aging, filtering, washing, drying, and calcining to obtain a carrier Zr-MCM-41;

[0018] (2) adding the carrier Zr-MCM-41 of step (1) into water, adjusting the pH of the system to 2-3 with concentrated nitric acid, then adding inorganic nickel salt and inorganic cerium salt, stirring and impregnating, and then filtering, washing, drying and roasting to obtain a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41.

[0019] In step (1) of the above preparation method, the amount of the MCM-41 molecular sieve is 10-20wt% of the mass of the organic solvent, preferably 14-18wt%;

[0020] The organic solvent is selected from one or more of methanol, ethanol, acetone and ethyl acetate.

[0021] In step (1) of the above preparation method, the amount of the organic zirconium salt is 32-85wt% of the mass of the MCM-41 molecular sieve, preferably 45-60wt%;

[0022] The organic zirconium salt is zirconium propionate.

[0023] In step (1) of the above preparation method, the immersion temperature is 10-40°C, preferably 25-30°C; and the time is 0.5-8h, preferably 4-5h.

[0024] In step (1) of the above preparation method, the rapid stirring has a rotation speed of 1000-2000 rpm.

[0025] In step (1) of the preparation method, the propionic acid and nitric acid composite solution comprises, by weight percentage, 76-90wt% of propionic acid, preferably 80-85wt% of nitric acid, 5-10wt% of nitric acid, preferably 6-8wt% of nitric acid, and the remainder is water;

[0026] Preferably, the pH value of the mixture of propionic acid and nitric acid is adjusted to 3-4 for 2-5 hours, preferably 3-4 hours.

[0027] In step (1) of the above preparation method, the aging, filtering, washing, drying and calcining are conventional operations in the art and are not specifically limited in the present invention. In some specific examples, the drying is performed at a temperature of 100-150°C, preferably 120-130°C, for 2-6h, preferably 3-4h; the calcining is performed at a temperature of 450-600°C, preferably 500-550°C, for 2-8h, preferably 4-5h; and the calcining pressure is normal pressure.

[0028] In step (2) of the above preparation method, the amount of the carrier Zr-MCM-41 is 22-36wt% of the mass of water, preferably 25-30wt%.

[0029] In step (2) of the above preparation method, the amount of the inorganic nickel salt is 18-35wt% of the mass of the carrier Zr-MCM-41, preferably 20-28wt%;

[0030] The inorganic nickel salt is selected from nickel nitrate hexahydrate and / or nickel chloride hexahydrate, preferably nickel nitrate hexahydrate.

[0031] In step (2) of the above preparation method, the amount of the inorganic cerium salt is 24-42wt% of the mass of the carrier Zr-MCM-41, preferably 30-36wt%;

[0032] The inorganic cerium salt is selected from cerium nitrate hexahydrate and / or cerium sulfate tetrahydrate, preferably cerium nitrate hexahydrate.

[0033] In step (2) of the above preparation method, the immersion temperature is 15-45°C, preferably 25-35°C, and the time is 1-10h, preferably 3-5h.

[0034] In step (2) of the above preparation method, the filtering, washing, drying and calcining are conventional operations in the art and are not specifically limited in the present invention. In some specific examples, the drying temperature is 90-160°C, preferably 120-140°C, and the time is 5-20h, preferably 8-15h; the calcining temperature is 450-600°C, preferably 500-550°C, and the time is 6-9h, preferably 7-8h; and the calcining pressure is normal pressure.

[0035] Preferably, in some specific examples, the bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41 can be prepared by the following method:

[0036] The MCM-41 molecular sieve is placed in methanol, a certain amount of zirconium propionate is added, and it is immersed at 25-30°C for 4-5h. Under strong stirring, a certain amount of propionic acid and nitric acid compound solution is slowly added thereto, and the pH is adjusted to between 3-4. After aging for 5h, the precipitate is filtered, washed, and dried, and finally placed in a 500-550°C air roasting furnace for 4-5h to prepare the carrier Zr-MCM-41. The carrier is added to water, concentrated nitric acid is added to adjust the system pH to 2-3, and then a certain amount of nickel nitrate hexahydrate and cerium nitrate hexahydrate are added to the system respectively. After stirring and immersing at 25-35°C for 3-5h, it is filtered, washed and dried, and placed in an air atmosphere at 500-550°C for 7-8h to prepare a bimetallic solid acid catalyst Ni-Ce (H +) / Zr-MCM-41.

[0037] In the present invention, the bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41 is used in an amount of 5-20wt% of the mass of allyl methyl ether contained in the 3-chloropropylene raw material, preferably 6-10wt%.

[0038] In the present invention, the molar ratio of the hydrogen chloride gas ventilation volume to the allyl methyl ether contained in the 3-chloropropylene raw material is 2-10:1, preferably 4-6:1;

[0039] The ventilation time of the hydrogen chloride gas is 0.5-4h, preferably 1-2h.

[0040] In the present invention, the reaction temperature is 0-30°C, preferably 5-15°C, and the time is 5-20h, preferably 8-12h;

[0041] Preferably, when hydrogen chloride gas is introduced into the reaction, it is first replaced with an inert gas.

[0042] In some specific examples, the method for purifying 3-chloropropene containing ether impurities in the present invention comprises the following steps:

[0043] Under normal pressure, a certain amount of allyl chloride containing allyl methyl ether impurities and catalyst Ni-Ce (H + ) / Zr-MCM-41, then replace the air in the system with nitrogen, control the system to maintain a certain temperature with a heat exchange medium, and introduce hydrogen chloride gas into the reactor at a certain gas speed under stirring, and stop ventilation after a period of time. After a period of reaction under stirring, use nitrogen to discharge the residual hydrogen chloride gas in the system, and then filter out the catalyst in the reaction liquid to obtain allyl chloride with allyl methyl ether impurities removed.

[0044] In the present invention, the bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, after purification, can be recovered by solvent washing and filtering under normal pressure, the specific operation is as follows:

[0045] The catalyst after the purification reaction is replaced and rinsed with methanol 20-100 times the volume of the catalyst at 50-60°C for 30-100 minutes, and then the catalyst is taken out and filtered for recycling.

[0046] After recovery, the catalyst can be used at least 50 times, and the removal rate of allyl methyl ether can still reach more than 95%.

[0047] Compared with the prior art, the present invention has at least the following positive effects:

[0048] (1) The method for purifying 3-chloropropylene containing allyl methyl ether provided by the present invention can achieve an allyl methyl ether removal rate of more than 95%, and has the advantages of simple process flow, low process energy consumption, less three wastes, and low investment cost;

[0049] (2) The catalyst Ni-Ce (H + ) / Zr-MCM-41 has the advantages of high reaction activity, mild reaction conditions and easy catalyst recovery.

[0050] (3) The allyl methyl ether impurity contained in 3-chloropropylene in the present invention will be + ) / Zr-MCM-41 catalyzes the reaction with hydrogen chloride gas to generate 3-chloropropene and methanol, thereby reducing the loss of 3-chloropropene and methanol and reducing the unit consumption of epichlorohydrin product.

[0051] (4) In the present invention, the 3-chloropropylene after the removal of allyl methyl ether can be directly returned to the extraction unit or the oxidation reaction system as a reusable raw material / solvent mixture, without the need to separate the 3-chloropropylene and methanol separately. Specific implementation methods

[0052] The following embodiments are not intended to limit the scope of implementation of the present invention. Any modification or equivalent substitution of the present invention without departing from the spirit and scope of the present invention shall be included in the protection scope of the claims of the present invention.

[0053] 1. Information on the sources of the main raw materials in the following examples:

[0054] The raw materials used in the examples are all conventional raw materials in the art, and the purity specifications used are analytically pure or chemically pure. Unless otherwise specified, they are all commercially available;

[0055] MCM-41 molecular sieve, zirconium propionate, concentrated nitric acid, propionic acid, lanthanum nitrate hexahydrate, zinc nitrate hexahydrate, ethanol, acetone, ethyl acetate, 5A molecular sieve, and ZSM-5 molecular sieve were all of analytical grade purity and purchased from Shanghai Aladdin Biochemical Technology Co., Ltd.;

[0056] Hydrogen chloride gas, purity 99.9%, purchased from Yantai Mingju Gas Co., Ltd.;

[0057] 3-Chloropropene containing ether impurities comes from the separation process of the process of producing epichlorohydrin from hydrogen peroxide.

[0058] Second, the following test methods are used in each example of the present invention:

[0059] Allyl chloride, methanol and allyl methyl ether were analyzed by GC-7890 chromatograph under the following chromatographic conditions: initial temperature 80°C, maintained for 2 min, programmed temperature increase to 150°C at a rate of 10°C / min, maintained for 5 min; vaporization chamber temperature 200°C, detection chamber temperature 200°C; FID detection; injection volume 0.2 μL.

[0060] Preparation Example 1

[0061] Preparation of bimetallic solid acid catalyst Ni-Ce(H + ) / Zr-MCM-41(Catalyst A):

[0062] (1) Add 100g of methanol to a beaker, add 10g of MCM-41 molecular sieve, then add 3.2g of zirconium propionate while stirring, transfer the beaker to a 10°C constant temperature water bath, and stir and immerse for 0.5h. After the immersion, slowly drop an aqueous solution containing 76wt% propionic acid and 10wt% nitric acid at a stirring speed of 1000rpm for 2h, adjust the pH to between 3-4, filter and wash the precipitate after aging for 5h, dry it in a 100°C constant temperature drying oven for 6h, and finally calcine it in a 450°C air calcining furnace for 8h, thereby preparing the carrier Zr-MCM-41.

[0063] (2) 11 g of carrier Zr-MCM-41 was added to 50 g of water, and concentrated nitric acid was slowly added to adjust the pH of the system to 2-3. Then 3.85 g of nickel nitrate hexahydrate and 2.64 g of cerium nitrate hexahydrate were added to the system respectively, and stirred until completely dissolved. After being immersed at 15°C for 10 h, the system was filtered and washed. The solid was then dried in a constant temperature drying oven at 90°C for 20 h, and calcined in an air atmosphere at 450°C for 9 h to prepare a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, named as catalyst A.

[0064] Based on the total mass of catalyst A, the Ni content is 3.5wt%, the Ce content is 1.5wt%; and the Zr content in the carrier Zr-MCM-41 is 3.6wt%.

[0065] Preparation Example 2

[0066] Preparation of bimetallic solid acid catalyst Ni-Ce(H + ) / Zr-MCM-41(Catalyst B):

[0067] (1) Add 100g of acetone to a beaker, add 20g of MCM-41 molecular sieve, then add 17g of zirconium propionate while stirring, transfer the beaker to a 40°C constant temperature water bath, and stir and impregnate for 8h. After the impregnation, slowly add an aqueous solution containing 90wt% propionic acid and 5wt% nitric acid at a stirring speed of 2000rpm for 5h, adjust the pH to between 3-4, filter and wash the precipitate after aging for 5h, dry it in a 150°C constant temperature drying oven for 2h, and finally calcine it in a 600°C air calcining furnace for 2h, thereby preparing the carrier Zr-MCM-41.

[0068] (2) 18 g of carrier Zr-MCM-41 was added to 50 g of water, and concentrated nitric acid was slowly added to adjust the pH of the system to 2-3. Then 3.24 g of nickel chloride hexahydrate and 7.56 g of cerium sulfate tetrahydrate were added to the system respectively, and stirred until completely dissolved. After immersion at 45°C for 1 hour, the system was filtered and washed. The solid was then dried in a 160°C constant temperature drying oven for 5 hours, and calcined in an air atmosphere at 600°C for 6 hours to prepare a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, named as catalyst B.

[0069] Based on the total mass of catalyst B, the Ni content is 1.8wt%, the Ce content is 2.7wt%; and the Zr content in the carrier Zr-MCM-41 is 9.4wt%.

[0070] Preparation Example 3

[0071] Preparation of bimetallic solid acid catalyst Ni-Ce(H + ) / Zr-MCM-41(Catalyst C):

[0072] (1) Add 100g of ethanol to a beaker, add 14g of MCM-41 molecular sieve, then add 8.4g of zirconium propionate while stirring, transfer the beaker to a 30°C constant temperature water bath, and stir and impregnate for 4h. After the impregnation, slowly drop an aqueous solution containing 80wt% propionic acid and 8wt% nitric acid at a stirring speed of 2000rpm for 3h, adjust the pH to between 3-4, filter and wash the precipitate after aging for 5h, dry it in a 130°C constant temperature drying oven for 3h, and finally place it in a 500°C air calcining furnace for 5h, thereby preparing the carrier Zr-MCM-41.

[0073] (2) 12.5 g of carrier Zr-MCM-41 was added to 50 g of water, and concentrated nitric acid was slowly added to adjust the pH of the system to 2-3. Then 2.5 g of nickel nitrate hexahydrate and 4.5 g of cerium nitrate hexahydrate were added to the system respectively, and stirred until completely dissolved. After immersion at 25°C for 5 h, the mixture was filtered and washed. The solid was then dried in a 120°C constant temperature drying oven for 15 h, and calcined in an air atmosphere at 500°C for 8 h to prepare a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, named as catalyst C.

[0074] Based on the total mass of catalyst C, the Ni content is 2.0 wt%, the Ce content is 2.3 wt%, and the Zr content in the carrier Zr-MCM-41 is 5.0 wt%.

[0075] Preparation Example 4

[0076] Preparation of bimetallic solid acid catalyst Ni-Ce(H + ) / Zr-MCM-41 (catalyst D):

[0077] (1) Add 100g of methanol to a beaker, add 18g of MCM-41 molecular sieve, then add 8.1g of zirconium propionate while stirring, transfer the beaker to a 25°C constant temperature water bath, and stir and impregnate for 5h. After the impregnation, slowly drop an aqueous solution containing 85wt% propionic acid and 6wt% nitric acid at a stirring speed of 1500rpm for 4h, adjust the pH to between 3-4, filter and wash the precipitate after aging for 5h, dry it in a 120°C constant temperature drying oven for 4h, and finally place it in a 550°C air calcining furnace for 4h, thereby preparing the carrier Zr-MCM-41.

[0078] (2) 15 g of carrier Zr-MCM-41 was added to 50 g of water, and concentrated nitric acid was slowly added to adjust the pH of the system to 2-3. Then 4.2 g of nickel nitrate hexahydrate and 4.5 g of cerium nitrate hexahydrate were added to the system respectively, and stirred until completely dissolved. After immersion at 35°C for 3 h, the mixture was filtered and washed. The solid was then dried in a 140°C constant temperature drying oven for 8 h, and calcined in an air atmosphere at 550°C for 7 h to prepare a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, named as catalyst D.

[0079] Based on the total mass of catalyst D, the Ni content is 2.8wt%, the Ce content is 1.9wt%; and the Zr content in the carrier Zr-MCM-41 is 6.7wt%.

[0080] Preparation Example 5

[0081] Preparation of bimetallic solid acid catalyst Ni-Ce(H + ) / Zr-MCM-41(Catalyst E):

[0082] (1) Add 100g of methanol to a beaker, add 16g of MCM-41 molecular sieve, then add 8g of zirconium propionate while stirring, transfer the beaker to a 27°C constant temperature water bath, and stir and impregnate for 4.5h. After the impregnation, slowly drop an aqueous solution containing 82wt% propionic acid and 7wt% nitric acid at a stirring speed of 2000rpm for 3.5h, adjust the pH to between 3-4, filter and wash the precipitate after aging for 5h, dry it in a 125°C constant temperature drying oven for 3.5h, and finally place it in a 520°C air calcining furnace for 4.5h, thereby preparing the carrier Zr-MCM-41.

[0083] (2) 13 g of carrier Zr-MCM-41 was added to 50 g of water, and concentrated nitric acid was slowly added to adjust the pH of the system to 2-3. Then 3.25 g of nickel nitrate hexahydrate and 4.16 g of cerium nitrate hexahydrate were added to the system respectively, and stirred until completely dissolved. After immersion at 30°C for 4 h, the mixture was filtered and washed. The solid was then dried in a 130°C constant temperature drying oven for 10 h, and calcined in an air atmosphere at 540°C for 7.2 h to prepare a bimetallic solid acid catalyst Ni-Ce (H + ) / Zr-MCM-41, named as catalyst E.

[0084] Based on the total mass of catalyst E, the Ni content is 2.5wt%, the Ce content is 2.0wt%; and the Zr content in the carrier Zr-MCM-41 is 6.1wt%.

[0085] Example 1

[0086] Under normal pressure, 1000 g of reaction raw materials (composition: 89.98% 3-chloropropylene, no methanol detected, 10.0% allyl methyl ether, 0.02% water) were added to a 2L reactor, and 5.0 g of catalyst Ni-Ce (H + ) / Zr-MCM-41, and then replace the air in the system with nitrogen, and then start stirring, use the reactor interlayer circulation bath to control the temperature in the reactor to 0°C, and introduce hydrogen chloride gas into the bottom of the reactor at a rate of 0.42g / min. The ventilation time is 4h. After reacting for 20h under stirring, the residual hydrogen chloride gas in the system is discharged with nitrogen, and then the catalyst in the reaction liquid is filtered out, and the reaction liquid is sampled. The gas chromatography analysis results are shown in Table 1:

[0087] Table 1

[0088] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 95.726% 4.212% 0.028% 99.7% B 95.660% 4.164% 0.143% 98.5% C 95.671% 4.172% 0.124% 98.7% D 95.699% 4.192% 0.077% 99.2% E 95.726% 4.212% 0.029% 99.7%

[0089] The catalyst filtered out in the above step is recovered by washing with a solvent and filtering under normal pressure. The specific operation is as follows:

[0090] The above 5.0g catalyst was filled into the fixed bed, and 20 times the volume of methanol was transported to the heat exchanger, heated to 50°C, and then passed through the catalyst bed from bottom to top. After replacement and flushing for 30 minutes, the fixed bed was disassembled, the catalyst was taken out and filtered to obtain the recovered catalyst.

[0091] Taking the recovered catalyst A as an example, it was reused in the purification method of 3-chloropropylene containing ether impurities according to the above operation steps. The gas chromatography analysis results of the samples are shown in Table 2 below:

[0092] Table 2

[0093] Number of applications 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate 1 95.726% 4.209% 0.0287% 99.7% 10 95.722% 4.208% 0.0380% 99.6% 20 95.694% 4.188% 0.0855% 99.1% 50 95.682% 4.181% 0.1050% 98.9%

[0094] Example 2

[0095] Purification method of 3-chloropropylene containing ether impurities:

[0096] Under normal pressure, 1000 g of 3-chloropropylene raw material containing allyl methyl ether impurity (composition: 3-chloropropylene 11.901%, methanol 88.0%, allyl methyl ether 0.01%, water 0.089%) was added into a 2L reactor, and 0.02 g of catalyst Ni-Ce (H + ) / Zr-MCM-41, and then replace the air in the system with nitrogen, and then start stirring, control the temperature in the reactor to 30°C with a reactor interlayer circulating bath, introduce hydrogen chloride gas into the bottom of the reactor at a rate of 0.017g / min, and the ventilation time is 0.5h. After reacting for 5h under stirring, use nitrogen to discharge the residual hydrogen chloride gas in the system, and then filter out the catalyst in the reaction solution to obtain 3-chloropropylene with allyl methyl ether impurity removed. The sampling gas chromatography analysis results are shown in Table 3 below:

[0097] Table 3

[0098]

[0099]

[0100] Example 3

[0101] Under normal pressure, 1000 g of reaction raw materials (composition: 10.0% 3-chloropropylene, 79.9% methanol, 10.0% allyl methyl ether, 0.1% water) were added to a 2L reactor, and 6.0 g of catalyst Ni-Ce (H +) / Zr-MCM-41, and then replace the air in the system with nitrogen, and then start stirring, use the reactor interlayer circulation bath to control the temperature in the reactor to 5°C, and introduce hydrogen chloride gas into the bottom of the reactor at a rate of 1.69g / min. The ventilation time is 2h. After reacting for 12h under stirring, the residual hydrogen chloride gas in the system is discharged with nitrogen, and then the catalyst in the reaction liquid is filtered out. The reaction liquid is sampled, and the gas chromatography analysis results are as follows:

[0102] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 19.597% 80.274% 0.0190% 99.8% B 19.565% 80.272% 0.0574% 99.4% C 19.552% 80.274% 0.0675% 99.3% D 19.506% 80.270% 0.1140% 98.8% E 19.594% 80.276% 0.0192% 99.8%

[0103] Example 4

[0104] Under normal pressure, 1000 g of reaction raw materials (composition: 3-chloropropylene 98.0%, methanol 0.95%, allyl methyl ether 1.0%, water 0.05%) were added to a 2L reactor, and 1.0 g of catalyst Ni-Ce (H + ) / Zr-MCM-41, and then replace the air in the system with nitrogen, and then start stirring, use the reactor interlayer circulation bath to control the temperature in the reactor to 15°C, and introduce hydrogen chloride gas into the bottom of the reactor at a rate of 0.51g / min. The ventilation time is 1h. After reacting for 8h under stirring, the residual hydrogen chloride gas in the system is discharged with nitrogen, and then the catalyst in the reaction liquid is filtered out, and the reaction liquid is sampled. The gas chromatography analysis results are as follows:

[0105] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 98.536% 1.367% 0.0458% 95.4% B 98.545% 1.373% 0.0318% 96.8% C 98.546% 1.375% 0.0279% 97.2% D 98.550% 1.378% 0.0189% 98.1% E 98.552% 1.381% 0.0149% 98.5%

[0106] Example 5

[0107] Under normal pressure, 1000 g of reaction raw materials (composition: 10.0% 3-chloropropylene, 85.0% methanol, 5.0% allyl methyl ether, no water detected) were added to a 2L reactor, and 4.0 g of catalyst Ni-Ce (H + ) / Zr-MCM-41, and then replace the air in the system with nitrogen, and then start stirring, use the reactor interlayer circulation bath to control the temperature in the reactor to 12°C, and introduce hydrogen chloride gas into the bottom of the reactor at a rate of 1.41g / min. The ventilation time is 1.5h. After reacting for 10h under stirring, the residual hydrogen chloride gas in the system is discharged with nitrogen, and then the catalyst in the reaction liquid is filtered out. The reaction liquid is sampled, and the gas chromatography analysis results are as follows:

[0108] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 14.859% 85.063% 0.0683% 98.6% B 14.875% 85.065% 0.0537% 98.9% C 14.880% 85.068% 0.0488% 99.0% D 14.826% 85.065% 0.1025% 97.9% E 14.916% 85.066% 0.0098% 99.8%

[0109] Comparative Example 1

[0110] Referring to Preparation Example 1-5, the only difference is that only the inorganic nickel salt is not added, and other parameters and operations remain unchanged. Referring to the method in Example 1, the results of gas chromatography analysis of the samples are as follows:

[0111] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 94.436% 3.264% 2.273% 76.4% B 94.575% 3.367% 2.029% 78.9% C 94.062% 2.992% 2.918% 69.8% D 93.944% 2.906% 3.123% 67.7% E 94.276% 3.149% 2.545% 73.6%

[0112] Comparative Example 2

[0113] Referring to Preparation Example 1-5, the only difference is that only the inorganic cerium salt is not added, and other parameters and operations remain unchanged. Referring to the method in Example 1, the results of gas chromatography analysis of the samples are as follows:

[0114] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 92.904% 2.143% 4.927% 49.5% B 93.180% 2.346% 4.448% 54.3% C 93.610% 2.659% 3.704% 61.8% D 93.632% 2.684% 3.646% 62.4% E 92.447% 1.809% 5.720% 41.6%

[0115] Comparative Example 3

[0116] Referring to Preparation Example 1-5, the only difference is that only the inorganic nickel salt is replaced with ferric nitrate, and other parameters and operations remain unchanged. Referring to the method in Example 1, the results of gas chromatography analysis of the samples are as follows:

[0117] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 93.466% 2.558% 3.951% 59.3% B 92.802% 2.067% 5.107% 47.7% C 93.368% 2.481% 4.121% 57.6% D 93.157% 2.328% 4.488% 53.9% E 94.025% 2.963% 2.986% 69.1%

[0118] Comparative Example 4

[0119] Referring to Preparation Example 1-5, the only difference is that only the inorganic cerium salt is replaced with lanthanum nitrate, and other parameters and operations remain unchanged. Referring to the method in Example 1, the results of gas chromatography analysis of the samples are as follows:

[0120] Catalyst name 3-Chloropropene Methanol Allyl methyl ether Allyl methyl ether removal rate A 92.336% 1.727% 5.914% 39.7% B 93.445% 2.538% 3.991% 58.9% C 92.563% 1.893% 5.519% 43.6% D 91.917% 1.419% 6.641% 32.5% E 92.696% 1.991% 5.287% 45.9%

Claims

1. A method for purifying 3-chloropropylene containing ether impurities, characterized in that: The method uses 3-chloropropylene containing allyl methyl ether impurities as a raw material, and reacts with hydrogen chloride gas at low temperature under the catalytic action of a bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 to obtain a 3-chloropropylene product from which allyl methyl ether has been removed. The 3-chloropropene containing ether impurities is 3-chloropropene containing allyl methyl ether impurities, wherein the content of allyl chloride is 10-98wt%, the content of allyl methyl ether impurities is 0.01-10wt%, and methanol and / or water, wherein the content of methanol is 0-88wt% and the content of water is 0-0.1wt%.

2. The purification method according to claim 1, characterized in that The bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 has a Ni content of 1.8-3.5wt% and a Ce content of 1.5-2.7wt% based on the total mass of the catalyst; and the Zr content in the carrier Zr-MCM-41 is 3.6-9.4wt%.

3. The purification method according to claim 2, characterized in that The bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 has a Ni content of 2.0-2.8wt% and a Ce content of 1.9-2.3wt% based on the total mass of the catalyst; and the Zr content in the carrier Zr-MCM-41 is 5.0-6.7wt%.

4. The purification method according to claim 1, characterized in that The preparation method of the bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 comprises the following steps: (1) impregnating an organic zirconium salt, MCM-41 molecular sieve, and an organic solvent, adjusting the pH to 3-4 with a composite solution of propionic acid and nitric acid under rapid stirring, and then aging, filtering, washing, drying, and calcining to obtain a carrier Zr-MCM-41; (2) Add the carrier Zr-MCM-41 of step (1) into water, adjust the pH of the system to 2-3 with concentrated nitric acid, then add inorganic nickel salt and inorganic cerium salt, stir and impregnate, and then filter, wash, dry and calcine to obtain a bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41.

5. The purification method according to claim 4, characterized in that In step (1), the amount of MCM-41 molecular sieve used is 10-20wt% of the mass of the organic solvent; The organic solvent is selected from one or more of methanol, ethanol, acetone and ethyl acetate; In step (1), the amount of the organic zirconium salt is 32-85wt% of the mass of the MCM-41 molecular sieve; The organic zirconium salt is zirconium propionate; In step (1), the immersion temperature is 10-40° C. and the time is 0.5-8 h; In step (1), the rapid stirring has a rotation speed of 1000-2000 rpm; In step (1), the propionic acid and nitric acid composite solution comprises, by weight percentage, 76-90wt% propionic acid, 5-10wt% nitric acid, and the remainder water; In step (1), the drying temperature is 100-150°C and the time is 2-6 hours; the calcination temperature is 450-600°C and the time is 2-8 hours; and the calcination pressure is normal pressure.

6. The purification method according to claim 5, characterized in that The amount of the MCM-41 molecular sieve used is 14-18 wt % of the mass of the organic solvent.

7. The purification method according to claim 5, characterized in that The amount of the organic zirconium salt is 45-60wt% of the mass of the MCM-41 molecular sieve.

8. The purification method according to claim 5, characterized in that The immersion temperature is 25-30°C and the time is 4-5 hours.

9. The purification method according to claim 5, characterized in that The propionic acid and nitric acid composite solution comprises, in weight percentage, 80-85wt% of propionic acid, 6-8wt% of nitric acid, and the remainder of water.

10. The purification method according to claim 5, characterized in that The drying temperature is 120-130° C. and the time is 3-4 hours.

11. The purification method according to claim 5, characterized in that The calcination temperature is 500-550°C and the calcination time is 4-5h.

12. The purification method according to claim 4, characterized in that In step (1), the pH value of the solution of propionic acid and nitric acid is adjusted to 3-4 for 2-5 hours.

13. The purification method according to claim 12, characterized in that: The adjustment time is 3-4h.

14. The purification method according to claim 4, characterized in that: In step (2), the amount of the carrier Zr-MCM-41 is 22-36wt% of the mass of water; In step (2), the amount of the inorganic nickel salt is 18-35wt% of the mass of the carrier Zr-MCM-41; The inorganic nickel salt is selected from nickel nitrate hexahydrate and / or nickel chloride hexahydrate; In step (2), the amount of the inorganic cerium salt is 24-42 wt% of the mass of the carrier Zr-MCM-41; The inorganic cerium salt is selected from cerium nitrate hexahydrate and / or cerium sulfate tetrahydrate; In step (2), the immersion temperature is 15-45° C. and the time is 1-10 h; In step (2), the drying temperature is 90-160° C. and the time is 5-20 h; the calcination temperature is 450-600° C. and the time is 6-9 h; and the calcination pressure is normal pressure.

15. The purification method according to claim 14, characterized in that: The amount of the carrier Zr-MCM-41 is 25-30 wt % of the mass of water.

16. The purification method according to claim 14, characterized in that: The amount of the inorganic nickel salt is 20-28 wt % of the mass of the carrier Zr-MCM-41.

17. The purification method according to claim 14, characterized in that: The amount of the inorganic cerium salt is 30-36 wt % of the mass of the carrier Zr-MCM-41.

18. The purification method according to claim 14, characterized in that: The immersion temperature is 25-35°C and the time is 3-5h.

19. The purification method according to claim 14, characterized in that: The drying temperature is 120-140° C. and the drying time is 8-15 hours.

20. The purification method according to claim 14, characterized in that: The calcination temperature is 500-550°C and the calcination time is 7-8h.

21. The purification method according to claim 1, characterized in that The amount of the bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 is 5-20wt% of the mass of allyl methyl ether contained in the 3-chloropropylene raw material.

22. The purification method according to claim 21, characterized in that The amount of the bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 is 6-10wt% of the mass of allyl methyl ether contained in the 3-chloropropylene raw material.

23. The purification method according to claim 1, characterized in that The molar ratio of the hydrogen chloride gas ventilation volume to the allyl methyl ether contained in the 3-chloropropylene raw material is 2-10:1; The ventilation time of the hydrogen chloride gas is 0.5-4h.

24. The purification method according to claim 23, characterized in that The molar ratio of the hydrogen chloride gas ventilation volume to the allyl methyl ether contained in the 3-chloropropylene raw material is 4-6:

1.

25. The purification method according to claim 23, characterized in that The ventilation time of the hydrogen chloride gas is 1-2h.

26. The purification method according to claim 1, characterized in that The reaction temperature is 0-30°C and the reaction time is 5-20h.

27. The purification method according to claim 26, characterized in that The reaction temperature is 5-15°C and the reaction time is 8-12h.

28. The purification method according to claim 1, characterized in that When hydrogen chloride gas is introduced into the reaction, it is first replaced with an inert gas.

29. The purification method according to claim 1, characterized in that The bimetallic solid acid catalyst Ni-Ce(H+) / Zr-MCM-41 can be recovered after purification, and the specific operation is as follows: The catalyst after the purification reaction is replaced and rinsed with methanol 20-100 times the volume equivalent of the catalyst at 50-60°C for 30-100 minutes, and then filtered, and then it can be recycled.

Citation Information

Patent Citations

  • Method and device for recovering chloropropene and methanol from hydrogen peroxide method epoxy chloropropane process water layer

    CN111960921A

  • Method for recovering 3-chloropropene from solution containing 3-chloropropene and methanol

    CN112778080A