A selenite-coordinated organic tin oxide cluster compound and its preparation method and application
The preparation method of organotin oxygen clusters coordinated by selenite groups solves the problem of synthesizing cyclic organotin oxygen clusters with inorganic acid ligands, and achieves a high-yield, low-cost, and environmentally friendly process, which is suitable for a variety of applications. High performance applications.
Patent Information
- Application Number
- CN202310452944.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-25
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2043-04-25
AI Technical Summary
It is difficult to synthesize cyclic organotin-oxygen clusters with novel structures and excellent properties through inorganic acid radical ligands with the existing technology, and the synthesis method is complex, costly, polluting and has low yield.
A method for preparing organotin-oxygen clusters coordinated by selenite is adopted, by performing a solvothermal reaction of organotin metal salts, selenite and transition metal salts in a mixed solvent of organic amines and alcohols or amides, followed by After separation and cleaning, a zero-dimensional cyclic organotin-oxygen cluster is obtained. This method has simple process, low cost, little pollution, and the yield can reach more than 40%.
A zero-dimensional cyclic organotin-oxygen cluster coordinated by selenite is obtained, which is suitable for the fields of organic catalysis, photoelectrocatalysis, photoresist and nonlinear optics. The process meets the requirements of green environmental protection and has low raw material purity requirements, making it suitable for large-scale applications. scale production.
Smart Images

Figure CN116478205B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of crystal materials, and in particular relates to a selenite-coordinated organic tin oxide cluster compound and a preparation method and application thereof. Background Art
[0002] Organotin oxy-cluster compounds not only have rich structures, but also have broad application prospects in catalysis, optoelectronics, semiconductor materials, etc. This type of material has attracted people's attention in the research of optoelectronic materials due to its unique semiconductor properties. Organotin oxy-cluster materials also cleverly connect basic disciplines and technical fields such as cluster chemistry, coordination chemistry and nanostructured materials. They have precise known structures and multi-component adjustable characteristics, which are convenient for exploring the structure-activity relationship between their structure and performance. They are very suitable as matrix materials to study and expand their rich optical, electrical and other properties. In fact, the use of different oxygen-containing ligands to synthesize organotin oxy-cluster compounds not only makes the structure of organotin oxy-cluster compounds richer, but also gives them new chemical properties. However, compared with organic oxygen-containing ligands, inorganic acid radical ligands have trigonal pyramidal configurations, such as selenite, which can induce the synthesis of cyclic organotin oxy-cluster compounds. Therefore, it is necessary to explore an effective synthesis method to use inorganic acid radical coordinated organotin oxy-cluster compounds to obtain organotin oxy-cluster compounds with more novel structures and better performance. Summary of the invention
[0003] In order to solve the above problems, the present invention provides a selenite-coordinated organic tin oxy-cluster compound and a preparation method and application thereof. The selenite-coordinated organic tin oxy-cluster compound is a zero-dimensional cyclic organic tin oxy-cluster compound coordinated by selenite, and the organic tin of the selenite-coordinated organic tin oxy-cluster compound is located at the outer ring position of the ring; the preparation method of the selenite-coordinated organic tin oxy-cluster compound has simple process, low cost, low pollution, and the yield can reach more than 40%; in addition, the selenite-coordinated organic tin oxy-cluster compound can be used in organic catalysis, photoelectrocatalysis, photoresist, nonlinear optics and other fields.
[0004] The present invention adopts the following technical solutions:
[0005] A method for preparing a selenite-coordinated organic tin oxide cluster comprises the following steps:
[0006] S1, mixing an organic tin metal salt, a selenite and a transition metal salt in a mixed solvent of an organic amine and an alcohol or an amide or water to perform a solvothermal reaction;
[0007] S2. Separating the mixture after the solvent thermal reaction, and then washing and drying the separated solid phase with alcohol or ketone until a pure phase crystal is obtained, that is, an organic tin oxide cluster coordinated by selenite is obtained.
[0008] Preferably, the specific process of step S1 is: mixing an organic tin metal salt, a selenite and a transition metal salt in a mixed solvent of an organic amine and an alcohol or an amide, stirring evenly, and placing in a glass bottle or a polytetrafluoroethylene reactor, reacting at a constant temperature, and naturally cooling to room temperature, wherein the molar ratio of the added organic tin metal salt, the selenite and the transition metal salt is (0.2-0.8):(1-2):(0.1-0.2).
[0009] Preferably, the organic tin metal salt in step S1 is one of methyltin, ethyltin, propyltin, butyltin, pentyltin, hexyltin, butyltin or phenyltin.
[0010] Preferably, the selenite in step S1 is one of selenium dioxide, selenious acid or sodium selenite.
[0011] Preferably, the transition metal salt in step S1 is one or more of nitrates, acetates, chlorides, sulfates or carbonates of transition metals.
[0012] Preferably, the organic amine in step S1 is one or more of methylpiperidine, methylpiperazine, hydroxymethylpiperazine, hydroxyethylpiperazine, methylamine aqueous solution, propylenediamine, ethylenediamine, butylenediamine, diethylamine, dipropylamine, dibutylamine or dipentylamine; the alcohol in step S1 is one of methanol, ethanol, isopropanol, n-propanol, n-butanol, ethylene glycol, 1,3-propylene glycol, 1,2-propylene glycol; the amide in step S1 is one of N,N-dimethylformamide, N,N-dimethylacetamide, N,N-diethylformamide, N,N-diethylacetamide, dimethyl sulfoxide, N-methylformamide, acetonitrile.
[0013] Preferably, the reaction temperature of the solvothermal reaction in step S1 is 60-180° C.; and the reaction time of the solvothermal reaction is 72-480 hours.
[0014] Preferably, the alcohol in step S2 is one or more of methanol, ethanol, propanol, isopropanol, ethylene glycol, 1,2-propylene glycol, 1,2-butanediol, 2,3-butanediol, 1,2-pentanediol, 2,3-pentanediol, and 1,2-hexanediol; the ketone in step S2 is one of acetone, butanone, or propiophenone.
[0015] The invention discloses a selenite-coordinated organic tin oxygen cluster compound, which is prepared by the preparation method of the selenite-coordinated organic tin oxygen cluster compound.
[0016] The invention discloses an application of a selenite-coordinated organic tin oxygen cluster compound, wherein the selenite-coordinated organic tin oxygen cluster compound is applied to organic catalysis, photoelectric catalysis, photoresist or nonlinear optics.
[0017] After adopting the above technical scheme, the present invention has the following advantages compared with the background technology: the prepared selenite-coordinated organic tin oxygen cluster compound is a selenite-coordinated zero-dimensional cyclic organic tin oxygen cluster compound with a diameter of about 1.2-2nm, and the organic tin of the selenite-coordinated organic tin oxygen cluster compound is located at the outer ring position of the ring; the preparation method of the selenite-coordinated organic tin oxygen cluster compound is simple in process, low in cost, and less in pollution, and at the same time, the purity requirement of the raw materials is low, the raw materials are easy to obtain and the price is low, the raw materials used can be directly purchased as chemically pure reagents, no further purification is required, and large-scale production is convenient, the yield can reach more than 40%, and the requirements of green environmental protection are met; in addition, the selenite-coordinated organic tin oxygen cluster compound can be used in organic catalysis, photoelectric catalysis, photoresist, nonlinear optics and other fields. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 Schematic diagram of the crystal structure of the crystalline product prepared in Example 1 of the present invention;
[0019] Figure 2 : is the X-ray powder diffraction pattern of the crystalline product prepared in Example 1 of the present invention, wherein the lower line is the powder diffraction value of the crystal placed in air, and the upper line is the simulated powder diffraction value;
[0020] Figure 3 This is the infrared spectrum of the crystalline product prepared in Example 1 of the present invention. DETAILED DESCRIPTION
[0021] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0022] See also Figures 1 to 3 As shown, the radiation source used in the X-ray powder diffraction pattern is Cu-Kα radiation.
[0023] Example 1
[0024] A mixture of selenium dioxide (1 mmol), manganese carbonate (0.1 mmol), methylamine aqueous solution (1.0 mL), dimethyl sulfoxide (1.75 mL) and n-butyltin trichloride (35 μL) was stirred in a 23 mL glass bottle for 30 minutes, the container was sealed, and heated at 65° C. for 7 days. Then it was naturally cooled to room temperature, washed with ethanol, and dried to obtain colorless crystals. The chemical formula of the selenite-coordinated organic tin oxygen cluster obtained in Example 1 is [(n-BuSn)8(SeO3) 16 ], whose molecular formula without guest molecules is C 44 H 72 N2O48 Se 16 Sn8.
[0025] Example 2
[0026] A mixture of selenium dioxide (2 mmol), nickel nitrate hexahydrate (0.1 mmol), methylamine aqueous solution (1.25 mL), N,N-dimethylacetamide (1.0 mL) and n-butyltin trichloride (35 μL) was stirred in a 23 mL glass bottle for 30 minutes, the container was sealed, and heated at 65° C. for 7 days. Then it was naturally cooled to room temperature, washed with ethanol, and dried to obtain colorless crystals. The chemical formula of the selenite-coordinated organic tin oxygen cluster prepared in Example 2 is [(n-BuSnO) 12 (μ2-O)4(SeO3)8], whose molecular formula without guest molecules is C 96 H 81 N 17 O 40 8S 12 .
[0027] Example 3
[0028] A mixture of selenium dioxide (1 mmol), nickel acetate tetrahydrate (0.1 mmol), hydrated gallium nitrate (0.1 mmol), 3,5-dimethylpiperidine (2.0 mL), water (1.0 mL) and n-butyltin trichloride (67 μL) was stirred in a 23 mL glass bottle for 30 minutes, the container was sealed, and heated at 80° C. for 7 days. Then it was naturally cooled to room temperature, washed with ethanol, and dried to obtain colorless crystals. The chemical formula of the selenite-coordinated organic tin oxygen cluster obtained in Example 3 is [(n-BuSnO) 12 (ClO4)(SeO3)8], whose molecular formula without guest molecules is C 94 H 81 ClN8O 40 8S 12 .
[0029] Example 4
[0030] A mixture of selenium dioxide (1 mmol), anhydrous ferric chloride (0.1 mmol), pentamethyldiethylenetriamine (0.5 mL), ethylene glycol (1.5 mL) and n-butyltin trichloride (67 μL) was stirred in a 23 mL glass bottle for 30 minutes, the container was sealed, and heated at 80°C for 5 days. Then it was cooled naturally to room temperature. It was washed with acetone to obtain orange-yellow crystals. The chemical formula of the selenite-coordinated organic tin oxygen cluster obtained in Example 4 is (n-BuSn) 12 Fe 18 (EG) 24 (μ4-O)6(SeO3)18 ], whose molecular formula without guest molecules is C 64 H 148 Fe 18 O 108 Se 18 Sn 12 .
[0031] The crystal parameters of the selenite-coordinated organotin oxide clusters prepared in Examples 1 to 4 are shown in Table 1.
[0032] Table 1 shows the crystal parameters of the selenite-coordinated organotin oxide clusters prepared in Examples 1 to 4.
[0033]
[0034] The above is only a preferred specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A method for preparing a selenite-coordinated organic tin oxide cluster, It is characterized in that The following steps are involved: S1, mixing an organic tin metal salt, selenium dioxide and a transition metal salt in a mixed solvent to perform a solvothermal reaction; The specific process of step S1 is: after mixing the organic tin metal salt, selenium dioxide and transition metal salt in a mixed solvent, stirring evenly, placing in a glass bottle or a polytetrafluoroethylene reactor, reacting at a constant temperature, and naturally cooling to room temperature, wherein the molar ratio of the added organic tin metal salt, selenium dioxide and transition metal salt is (0.2-0.8): (1-2): (0.1-0.2); the mixed solvent is obtained by mixing an organic amine and an alcohol, or the mixed solvent is obtained by mixing an organic amine and an amide, or the mixed solvent is obtained by mixing an organic amine and water; The organotin metal salt in step S1 is one of methyltin, ethyltin, propyltin, butyltin, pentyltin, hexyltin, butyltin or phenyltin; S2. Separating the mixture after the solvent thermal reaction, and then washing and drying the separated solid phase with alcohol or ketone until a pure phase crystal is obtained, that is, an organic tin oxide cluster coordinated by selenite is obtained.
2. The method for preparing the selenite-coordinated organotin oxide cluster compound according to claim 1, Features: The transition metal salt in step S1 is one or more of nitrate, acetate, chloride, sulfate or carbonate of a transition metal.
3. The method for preparing the selenite-coordinated organotin oxide cluster compound according to claim 1, Features: The organic amine described in step S1 is one or more of methyl piperidine, methyl piperazine, hydroxymethyl piperazine, hydroxyethyl piperazine, methylamine aqueous solution, propylene diamine, ethylene diamine, butylene diamine, diethylamine, dipropylamine, dibutylamine or dipentylamine; the alcohol described in step S1 is one of methanol, ethanol, isopropanol, n-propanol, n-butanol, ethylene glycol, 1,3-propylene glycol, and 1,2-propylene glycol; the amide described in step S1 is one of N,N-dimethylformamide, N,N-dimethylacetamide, N,N-diethylformamide, N,N-diethylacetamide, dimethyl sulfoxide, N-methylformamide, and acetonitrile.
4. The method for preparing the selenite-coordinated organotin oxide cluster compound according to claim 1, Features: The reaction temperature of the solvent thermal reaction in step S1 is 60-180° C.; the reaction time of the solvent thermal reaction is 72-480 hours.
5. The method for preparing the selenite-coordinated organotin-oxygen cluster compound according to claim 1, Features: The alcohol in step S2 is one or more of methanol, ethanol, propanol, isopropanol, ethylene glycol, 1,2-propylene glycol, 1,2-butanediol, 2,3-butanediol, 1,2-pentanediol, 2,3-pentanediol, and 1,2-hexanediol; the ketone in step S2 is one of acetone, butanone, or propiophenone.
6. A selenite-coordinated organotin-oxygen cluster, Features: The selenite-coordinated organotin-oxygen cluster compound is prepared by the preparation method of the selenite-coordinated organotin-oxygen cluster compound according to any one of claims 1 to 5.
7. Use of the selenite-coordinated organic tin oxide cluster compound as claimed in claim 6, Features: The selenite-coordinated organic tin oxygen cluster is applied to organic catalysis, photoelectric catalysis, photoresist or nonlinear optics.