A production method of glass fiber powder steel pipe lubricant

By using steel pipe lubricants prepared by raw materials such as glass fiber powder, the problems of thermal conductivity and pollution in steel pipe extrusion processing are solved, high-temperature lubricants, low friction and protection effects are achieved, and the material yield and chemical stability are improved. sex.

CN117186969BActive Publication Date: 2024-11-22WUHE COUNTY WEI JIA COMPOSITE MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311171708.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-09-12
Publication Date
2024-11-22
Estimated Expiration
2043-09-12

AI Technical Summary

Technical Problem

Traditional graphite lubricants have problems such as thermal conductivity, fast mold heating, rapid wear, carbon increase, easy corrosion, and environmental pollution in steel pipe extrusion processing, which is difficult to meet the lubrication needs under high temperature and high pressure.

Method used

Using glass fiber powder, boron oxide or sodium borate, anhydrous sodium sulfate, phosphorus pentoxide, flow agent and hollow glass microbeads, etc., the glass fiber powder steel pipe lubricant is prepared through a mixing process to form a lubricating film to provide viscosity and insulation. Effect and low friction coefficient reduce the cooling effect and friction resistance of the extruder.

Benefits of technology

It improves the yield of steel pipes, reduces friction resistance, provides high-temperature lubrication, isolation and protection effects, avoids the thermal conductivity and pollution problems of traditional lubricants, and has good chemical stability and will not cause tissue defects.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a production method of a glass fiber powder steel pipe lubricant, which belongs to the technical field of glass fiber powder lubrication. Glass fiber powder is used as a main material, and has a certain viscosity and a good heat insulation effect at high temperature. When used during extrusion, the dry friction of the contact surface can be converted into boundary friction as much as possible, and the friction coefficient is small, which reduces the cooling effect of extrusion and reduces the friction resistance. Boron oxide and sodium borate play a high-temperature lubricating role on the surface of the steel pipe under high-temperature melting conditions, and quickly produce a layer of lubricating film, which is tightly attached to the surface of the blank to achieve protective effects such as lubrication, isolation and protection. The thermal conductivity is small, which can prevent the surface of the blank from cooling too quickly, can play a certain protective role, has good chemical stability, will not cause tissue defects, can be kept clean during lubrication, and has a low friction coefficient on the contact surface, thereby improving the yield rate of the steel pipe.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of glass fiber powder lubricants, and in particular relates to a production method of a glass fiber powder steel pipe lubricant. Background Art

[0002] Glass fiber powder is an inorganic non-metallic material in the shape of a long rod, composed of a variety of oxides. It is made of short chopped and sieved glass fiber strands, and is used to fill and reinforce various resins. Glass fiber powder has the advantages of high mechanical strength, excellent heat resistance, good insulation, low moisture absorption and corrosion resistance. It has been widely used in insulating materials, plastics, rubber, cement and other fields, and is often used as a car wall material to increase thermal insulation performance. Liu Siyang et al. used ultrafine glass fiber powder as the main component of composite ceramic powder to prepare a dealcoholized single-component ceramic silicone sealant. Glass fiber powder is mainly used in the FRP industry and also in asphalt concrete. In the construction industry, glass fiber powder is currently mainly used to increase strength. Metal extrusion requires high temperature and high pressure, and requires suitable lubricants. This is a prerequisite for extrusion deformation, and it also affects quality and energy consumption. Countries around the world have conducted extensive research on metal extrusion lubricants. In 1942, Frenchman J. Sejournet invented glass lubricants for extruded steel pipe manufacturing. Steel extrusion processing is characterized by high pressure, high temperature and high speed. Therefore, the lubricant used in steel extrusion processing must have the following characteristics: sufficient viscosity to ensure that it will not be squeezed out under the extrusion force, to ensure good insulation between the hot metal and the cold tool, and a low friction coefficient on the contact surface. Traditional steel extrusion production uses graphite lubricants, but the disadvantages are: poor thermal conductivity, fast mold heating, fast wear, difficulty in extruding long products, carbon increase, easy corrosion, carbon removal, increased metal consumption, and environmental pollution. It is easy to cause carbon increase in the product, and intergranular corrosion is easy to occur when extruding stainless steel. Therefore, the carburized layer must be removed after extrusion, resulting in increased metal consumption. It often pollutes the environment. Those skilled in the art are in urgent need of developing a production method for glass fiber powder steel pipe lubricants to meet the existing application market and performance requirements. Summary of the invention

[0003] In view of this, the present invention provides a method for producing a glass fiber powder steel pipe lubricant.

[0004] A production method of a glass fiber powder steel pipe lubricant comprises the following steps: a first step, weighing the following raw materials in parts by weight: 68-73 parts of glass fiber powder, 15-18 parts of boric oxide or sodium borate, 9-12 parts of anhydrous sodium sulfate, 5-10 parts of phosphorus pentoxide, 4-6 parts of flow agent, and 5-10 parts of hollow glass microspheres; a second step, mixing the above raw materials uniformly in a mixer to obtain the glass fiber powder steel pipe lubricant, wherein the glass fiber powder steel pipe lubricant forms a lubricating film and is used as a steel pipe external powder coating lubricant, a steel pipe hole expansion internal powder coating lubricant, and a steel pipe extrusion internal powder coating lubricant.

[0005] Furthermore, the flowable agent in the first step is one of sodium stearate, zinc stearate or calcium stearate.

[0006] The introduction of stearate can achieve good dispersion and stability after stearate treatment, and can improve the formability of glass fiber powder steel pipe lubricant. The fluidity of glass fiber powder is improved, the properties are stable, and good fluidity is conducive to high-temperature lubrication. At the same time, stearate not only plays a role in fluidity, but also provides a certain lubricity in the initial stage of lubrication. At the same time, after decomposition, it provides oxides such as sodium oxide and zinc oxide, which participate in the high-temperature lubrication of the enamel layer.

[0007] Furthermore, the glass fiber powder in the first step is alkali-free glass fiber powder obtained by chopped, ground and sieved continuous glass fiber strands, with a mesh size of 80 to 150 meshes and a diameter of 11 to 17 μm.

[0008] Furthermore, the hollow glass microspheres in the first step have a particle size of 50 to 100 μm, a bulk density of 0.11 to 0.14 g / cm3, and a true density of 0.2 to 0.25 g / cm 3 .

[0009] Hollow glass microspheres can still maintain their excellent properties under high temperature and high pressure conditions, and when used with glass fiber powder, no new substances are introduced, which promotes lubrication.

[0010] Furthermore, the mixing process of the second step is as follows: the mixing temperature is 70-80° C., the rotation speed is 10-20 r / min, and the time is 20-30 min.

[0011] Furthermore, the thickness of the lubricating film in the second step is 20 to 50 μm.

[0012] Beneficial effects of the present invention:

[0013] Compared with the prior art, the present invention has the following advantages:

[0014] The production method of the glass fiber powder steel pipe lubricant disclosed in the present invention adopts glass fiber powder as the main material, has a certain viscosity and good insulation effect at high temperature, and can transform the dry friction of the contact surface into boundary friction as much as possible when used during extrusion, with a small friction coefficient, reducing the cooling effect of the extruder and reducing the friction resistance. Boric oxide and sodium borate affect the network structure with the flake structure of boron oxygen triangle under high-temperature melting conditions, thereby reducing the viscosity of the glass. Sodium borate also plays the role of a solvent, providing boric oxide and sodium oxide, supplemented by phosphorus pentoxide, to generate a glass enamel layer when the glass fiber powder is melted. The glass enamel layer plays a high-temperature lubricating role on the surface of the steel pipe, quickly generates a lubricating film, and is tightly attached to the surface of the blank, thereby achieving protective effects such as lubrication, isolation, and protection.

[0015] Compared with the existing graphite lubricant, the production method of the glass fiber powder steel pipe lubricant disclosed in the present invention has a small thermal conductivity, can prevent the surface of the blank from cooling too quickly, can play a certain protective role, has good chemical stability, will not cause structural defects, can be kept clean during lubrication, can be used as a powder lubricant for the outside of steel pipes, a powder lubricant for the inside of steel pipe expansion, and a powder lubricant for the inside of steel pipe extrusion, has a low friction coefficient on the contact surface, and thus improves the yield rate of steel pipes. DETAILED DESCRIPTION Example 1

[0016] The alkali-free WJ-FS alkali-free glass fiber powder is made of 150 mesh and 11μm diameter. The particle size of HGS20 hollow glass microbeads is 50μm and the bulk density is 0.11g / cm 3 , True density 0.2g / cm 3 ; Hongyuan Chemical Zinc Stearate.

[0017] The production method of glass fiber powder steel pipe lubricant comprises the following steps: a first step, weighing the following raw materials in parts by weight: 73 parts of glass fiber powder, 18 parts of sodium borate, 9 parts of anhydrous sodium sulfate; 5 parts of phosphorus pentoxide, 4 parts of flow agent zinc stearate, and 10 parts of hollow glass microspheres; a second step, mixing the above raw materials evenly in a mixer, wherein the mixing temperature is 80°C, the rotation speed is 20r / min, and the time is 30min, thereby preparing the glass fiber powder steel pipe lubricant, the lubricating film thickness is 50μm, and the glass fiber powder steel pipe lubricant forms a lubricating film for use as a steel pipe external coating powder lubricant.

[0018] Product: Dry powder fluidity 28 seconds (DIN standard 6# cup), friction coefficient 0.054 at 1200 degrees Celsius. Example

[0019] Raw materials: WJ-FS alkali-free glass fiber powder is made of 80 mesh and 17μm diameter. The particle size of HGS25 hollow glass microbeads is 100μm and the bulk density is 0.14g / cm 3 , True density 0.25g / cm 3 ; Kexiang Chemical Calcium Stearate.

[0020] The production method of glass fiber powder steel pipe lubricant comprises the following steps: the first step is to weigh the following raw materials in parts by weight: 68 parts of glass fiber powder, 15 parts of boron oxide, 12 parts of anhydrous sodium sulfate, 5 parts of phosphorus pentoxide, 6 parts of flow agent calcium stearate, and 5 parts of hollow glass microspheres; the second step is to evenly mix the above raw materials in a mixer, wherein the mixing temperature is 70°C, the rotation speed is 10r / min, and the time is 20min, thereby preparing the glass fiber powder steel pipe lubricant, the lubricating film thickness is 20μm, and the glass fiber powder steel pipe lubricant forms a lubricating film for use as a powder coating lubricant for steel pipe expansion.

[0021] Product: Dry powder fluidity: 28 seconds (DIN standard 6# cup), friction coefficient 0.059 at 1210 degrees Celsius. Example 2

[0022] The alkali-free WJ-FS alkali-free glass fiber powder is made of 80 mesh and 11μm diameter. The particle size of HGS20 hollow glass microbeads is 50μm and the bulk density is 0.11g / cm 3 , True density 0.2g / cm 3 ; Xinxin Chemical Sodium Stearate.

[0023] The production method of glass fiber powder steel pipe lubricant comprises the following steps: the first step is to weigh the following raw materials in parts by weight: 70 parts of glass fiber powder, 17 parts of sodium borate, 11 parts of anhydrous sodium sulfate, 8 parts of phosphorus pentoxide, 5 parts of sodium stearate as a flow agent, and 8 parts of hollow glass microspheres; the second step is to evenly mix the above raw materials in a mixer, wherein the process is a mixing temperature of 75°C, a rotation speed of 15 r / min, and a time of 25 min, thereby preparing the glass fiber powder steel pipe lubricant, the lubricating film thickness of which is 35 μm, and the glass fiber powder steel pipe lubricant forms a lubricating film for use as a steel pipe extrusion internal coating powder lubricant.

[0024] Dry powder fluidity: 25 seconds (DIN standard 6# cup), friction coefficient is 0.051 at 1240 degrees Celsius.

[0025] Note: The friction coefficient test reference (Zhou Xudong, Wang Shijun, Wang Pingping, et al. Experimental study on lubricants for hot-rolled steel pipes [J]. Steel Pipe, 1994(04):27-29.).

Claims

1. A method for producing a glass fiber powder steel pipe lubricant, It is characterized in that The invention comprises the following steps: first, weighing the following raw materials in parts by weight: 68-73 parts of glass fiber powder, 15-18 parts of boron oxide or sodium borate, 9-12 parts of anhydrous sodium sulfate, 5-10 parts of phosphorus pentoxide, 4-6 parts of flow agent, and 5-10 parts of hollow glass microspheres, wherein the flow agent is one of sodium stearate, zinc stearate or calcium stearate, the glass fiber powder is alkali-free glass fiber powder obtained by chopped, ground and sieved continuous glass fiber raw yarn, the mesh number is 80-150 meshes, the diameter is 11-17 μm, the hollow glass microspheres have a particle size of 50-100 μm, and a bulk density of 0.11-0.14 g / cm 3 , True density 0.2~0.25g / cm 3 ; The second step is to mix the above raw materials evenly in a mixer, the mixing temperature is 70-80°C, the rotation speed is 10-20r / min, and the time is 20-30min; thereby obtaining a glass fiber powder steel pipe lubricant, the glass fiber powder steel pipe lubricant forms a lubricating film used as a steel pipe external powder lubricant, a steel pipe hole expansion internal powder lubricant, and a steel pipe extrusion internal powder lubricant, and the lubricating film thickness is 20-50μm.