A cold stamping aluminum production process
By using antibacterial color-changing colloid and polyethylene oxide to form an isolation layer in the cold stamping molding process, and using the gas separation technology of the cold stamping equipment, the problem of uneven stress when the aluminum foil paper is demoulded is solved, and the finished product qualification rate is improved. And realize the recycling of aluminum foil layer.
Patent Information
- Application Number
- CN202311367517.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-21
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-10-21
AI Technical Summary
In the existing cold stamping aluminum foil paper process, the aluminum foil paper is prone to secondary deformation, wrinkles or tears due to uneven force exerted by the floating material block during demolding, resulting in a low finished product qualification rate.
A cold stamping molding process is used to crush the waste paper into powder, add antibacterial color-changing colloid and mix it with polyethylene oxide to form an isolation layer, and then coat the color-changing gelled pulp on the surface of the aluminum foil paper, and use cold stamping equipment During stripping, the aluminum foil paper and the mold are separated by gas, and the air pressure and air flow direction are controlled to evenly stress.
It improves the qualification rate of aluminum foil packaging finished products, realizes the recycling of aluminum foil layers, reduces production costs, and reduces the risk of deformation and tearing of aluminum foil through gas separation.
Smart Images

Figure CN117265915B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a cold stamping aluminum production process, belonging to the technical field of cold stamping. Background Art
[0002] With the increasing application areas and demand of aluminum foil, the domestic aluminum foil industry continues to develop, especially the aluminum foil industry for flexible packaging has developed rapidly. Aluminum foil is moisture-proof, airtight, and light-shielding. Due to its excellent quality, aluminum foil is involved in many different technical fields, including pharmaceutical products, cigarettes, beverages, food and other industries.
[0003] After searching, a Chinese patent with publication number CN219337944U discloses an aluminum foil stamping and cutting forming mold structure, and its technical key points are: it includes a lower mold forming block, a lower mold knife seat arranged on the top of the lower mold forming block, an upper mold plate, a pressing core elastically arranged inside the upper mold plate and corresponding to the lower mold forming block, and an upper mold punch arranged at the bottom of the upper mold plate and staggered and movable with the lower mold knife seat; the inner wall of the lower mold knife seat is spliced and transitionally connected with the inner wall of the arc-shaped cavity, the outer edge of the lower mold knife seat is a corrugated continuous structure along its length direction, and the inner side of the upper mold punch is correspondingly arranged along the corrugated continuous structure.
[0004] In the above scheme, the pressure core elastically arranged at the bottom of the upper template cooperates with the floating material block, which is beneficial to the demolding of the aluminum foil product when the mold is opened. However, when the aluminum foil is pushed out by the floating material block, since the aluminum foil is thin, the aluminum foil is unevenly stressed when the floating material block applies force to the aluminum foil. If the pressure of the floating material block is too great, the aluminum foil is easily deformed, wrinkled or even torn, resulting in a low qualified rate of finished products.
[0005] Therefore, a new solution needs to be proposed to solve this problem. Summary of the invention
[0006] The technical problem to be solved by the present invention is to provide a cold stamping aluminum production process, which solves the problem of low finished product qualification rate in the prior art.
[0007] The technical problem to be solved by the present invention is achieved by adopting the following technical solutions:
[0008] A cold stamping aluminum production process comprises the following steps:
[0009] S1. Grinding waste paper into powder to obtain paper powder; adding the paper powder into an antibacterial color-changing colloid, mixing and stirring to obtain color-changing gelled pulp;
[0010] S2, weighing a certain amount of polyethylene oxide, spraying it on the surface of the aluminum foil layer while it is hot after melting, and then placing the sprayed aluminum foil layer at room temperature to dry, so as to form an isolation layer on the surface of the aluminum foil layer;
[0011] S3, evenly coating the color-changing gelatinized pulp on the surface of the isolation layer, and then compounding a layer of antibacterial color-changing paper base on the surface of the isolation layer to obtain aluminum foil;
[0012] S4, cold stamping the aluminum foil by a cold stamping device, the cold stamping device includes a male die and a female die, when the aluminum foil is demolded, gas is introduced between the male die and the aluminum foil, and between the female die and the aluminum foil, and the gas is used to separate the aluminum foil from the male die and the female die, respectively, to obtain an aluminum foil packaging product;
[0013] S5. Check the surface defects of the finished aluminum foil packaging products and put the qualified products into storage.
[0014] The present invention is further configured as follows: the cold stamping equipment includes a punch, a die below the punch, and a driving member connected between the punch and the die; the punch and the die cooperate to form a cavity; a first pressure chamber is provided inside the punch and inside the die; a plurality of air holes connected to the cavity are provided on the inner wall of the first pressure chamber; a sealing member is provided on the air hole; and a control mechanism for controlling the sealing member to close or open the air hole is provided on the punch and the die.
[0015] The present invention is further configured as follows: the bottom surface of the punch is provided with an annular sealing plate arranged in an annular shape around the circumference of the cavity, the bottom surface of the punch is provided with an annular plug-in groove matching with the annular sealing plate, the annular sealing plate is slidably plugged into the annular plug-in groove, a plurality of return springs are provided between the top surface of the annular sealing plate and the top surface of the annular plug-in groove, when the bottom end of the annular sealing plate abuts against the top surface of the die, an air cavity is formed on the upper periphery of the cavity, the bottom surface of the punch and the top surface of the die corresponding to the air cavity are provided with an air inlet channel connected to the first pressure chamber, a one-way valve is provided in the air inlet channel, and the one-way valve is used to intake air into the first pressure chamber.
[0016] The present invention is further configured as follows: the bottom end surface of the annular sealing plate is provided with an annular blade circumferentially arranged around the annular sealing plate, and the top surface of the die is provided with an annular groove matching the annular blade.
[0017] The present invention is further configured as follows: the control mechanism includes a second pressure chamber opened inside the punch and the die, a pressure regulating pipe connected to the second pressure chamber and extending to the outside of the punch or the die respectively, the pressure regulating pipe is connected to a three-position three-way solenoid valve, and the three-position three-way solenoid valve is respectively connected to a boost pipe and a pressure reducing pipe, the sealing member includes a connecting hole connected between the first pressure chamber and the second pressure chamber, a piston column slidably inserted in the connecting hole, a sealing block fixedly connected to one end of the piston column located in the first pressure chamber, and a limit block fixedly connected to one end of the piston column located in the second pressure chamber, and the sealing block is slidably inserted in the air hole to close the air hole.
[0018] The present invention is further configured as follows: the air hole is truncated cone-shaped, and the diameter of the air hole close to one end of the cavity is smaller than the diameter of the air hole close to the second pressure chamber, and the sealing block is a truncated cone-shaped structure matching the air hole.
[0019] The present invention is further configured as follows: a plurality of drainage grooves are opened on the inner peripheral wall of the air hole, the drainage grooves pass through one end of the air hole close to the cavity, the drainage grooves extend along the chord tangent of the air hole, and a plurality of sealing belts matching the drainage grooves are fixedly connected to the peripheral wall of the sealing block.
[0020] The present invention is further configured as follows: the first pressure chamber on the punch is connected to a pressure relief pipe extending to the outside of the punch, the first pressure chamber on the die is connected to a pressure relief pipe extending to the outside of the die, an adjusting piece is provided at one end of the pressure relief pipe away from the first pressure chamber, the adjusting piece includes a threaded ring located in the pressure relief pipe, a plurality of support rods fixedly connected to the threaded ring and the inner wall of the pressure relief pipe, an adjusting screw threadedly connected to the threaded ring, an abutment ring fixedly connected to the inner wall of the pressure relief pipe, an adjusting block arranged at the end of the adjusting screw and abutting against the inner wall of the abutment ring, the inner side wall of the abutment ring is in the shape of a truncated cone with a gradually increasing diameter, the adjusting block is configured to be in the shape of a truncated cone matching the inner side wall of the abutment ring, and a knob is provided at one end of the adjusting screw extending out of the pressure relief pipe.
[0021] The present invention is further configured as follows: the adjusting block and the adjusting screw are elastically connected, a plug-in hole is provided on the end face of the adjusting block, the adjusting screw is slidably plugged into the plug-in hole, a supporting spring is provided between the end of the adjusting screw and the inner wall of the plug-in hole, a first limiting ring is fixedly connected to one end of the inner wall of the plug-in hole close to the opening, and a second limiting ring is fixedly connected to the peripheral wall of one end of the adjusting screw located in the plug-in hole.
[0022] The present invention is further configured as follows: the circumferential wall of the male die is fixedly connected to an upper mounting plate, the circumferential wall of the female die is fixedly connected to a lower mounting plate, and the driving member comprises a hydraulic cylinder fixedly mounted on the lower mounting plate and having a piston rod connected to the upper mounting plate.
[0023] The beneficial effects of the present invention are:
[0024] 1. By adopting this process to produce aluminum foil, when recycling aluminum foil, the discarded aluminum foil packaging is placed in hot water and soaked for 20-30 minutes. Since polyethylene oxide is easily soluble in hot water, the polyethylene oxide in the isolation layer is dissolved after soaking in hot water, thereby separating the aluminum foil layer from the antibacterial color-changing paper base layer, and the aluminum foil layer can continue to be recycled, thus realizing the recycling of the aluminum foil layer, which is not only simple in recycling process, but also environmentally friendly and cost-saving;
[0025] 2. By using cold stamping equipment, when the aluminum foil is demolded after stamping, gas is sprayed on the punch and the die respectively, so that the gas fills the aluminum foil and the punch, and between the aluminum foil and the die, and the aluminum foil adhering to the inner wall of the cavity is separated from the punch and the die by the gas. In this process, due to the fluidity of the gas, the finished aluminum foil packaging product is not easy to be torn or deformed due to excessive force on a certain part, and the force on the aluminum foil is more uniform, thereby improving the yield rate of the finished aluminum foil packaging product;
[0026] 3. When the punch and the die are closed by the driving member, the annular sealing plate slidably connected to the punch closes the groove on the die, and an air cavity is formed around the punch above the cavity. In the process of the punch and the die gradually closing, the air cavity gradually shrinks, and the gas is pressed into the first pressure cavity through the one-way valve and the air inlet channel, so that the air pressure in the first pressure cavity is much greater than the air pressure in the cavity. At this time, the three-way three-way valve is controlled to connect the boosting pipe to the pressure regulating pipe, thereby increasing the air pressure in the second pressure cavity, so that the air pressure in the second pressure cavity is greater than the first pressure cavity. The air pressure in the cavity, at this time, under the action of the piston column, the sealing block is pressed against the air hole to close the air hole. When the punch and the die are opening, the three-position three-way valve is controlled to connect the pressure reducing pipe to the pressure regulating pipe to reduce the air pressure in the second pressure cavity, so that the air pressure in the second pressure cavity is less than the air pressure in the first pressure cavity. Under the action of the air pressure difference, the piston drives the sealing block away from the air hole, so that the air hole is opened, and the gas in the first pressure cavity is injected into the aluminum foil and the punch, and between the aluminum foil and the die through the air hole, so that the aluminum foil is separated from the punch and the die by air pressure;
[0027] 4. By arranging a drainage groove on the air hole, when the gas in the first pressure chamber flows into the cavity through the air hole, since the air hole is in a truncated cone shape, the drainage groove located on the inner wall of the air hole is inclined relative to the inner wall of the cavity. Under the action of the drainage groove, the flow direction of the airflow forms an acute angle with the aluminum foil in the cavity, so that when the airflow flows toward the inside of the cavity, it is not easy to blow directly on the aluminum foil, thereby reducing the air pressure on the aluminum foil and reducing the possibility of deformation of the aluminum foil;
[0028] 5. By setting a pressure relief pipe, and setting an adjusting block and an abutment ring in the pressure relief pipe, when cold stamping is performed on aluminum foil of different materials, the adjusting screw is rotated to drive the adjusting block to press against the inner wall of the abutment ring. When the air pressure in the first pressure chamber is greater than the elastic force of the supporting spring, the air pressure pushes the adjusting block away and can be ejected from the pressure relief pipe, so that the first pressure chamber can maintain a constant pressure, thereby reducing the situation where the air pressure in the first pressure chamber is too high and the pressure on the aluminum foil is too high when it is ejected from the air hole. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a schematic diagram of the overall structure of the present invention.
[0030] Figure 2 It is an overall cross-sectional view of the present invention.
[0031] Figure 3 yes Figure 1 A partial enlarged view of part A.
[0032] Figure 4 yes Figure 2 A partial enlarged view of part B.
[0033] Figure 5 It is a schematic diagram of the structure of the pore part in the present invention.
[0034] Figure 6 It is a structural schematic diagram of the sealing block part in the present invention.
[0035] Figure 7 yes Figure 2 A partial enlarged view of part C.
[0036] In the figure: 1, cold stamping equipment; 2, punch; 3, die; 4, cavity; 5, upper mounting plate; 6, lower mounting plate; 7, hydraulic cylinder; 8, first pressure chamber; 9, air hole; 10, annular sealing plate; 11, annular plug groove; 12, return spring; 13, air chamber; 14, air inlet channel; 15, one-way valve; 16, annular blade; 17, annular groove; 18, blocking member; 19, control mechanism; 20, second pressure chamber; 21, pressure regulating pipe; 22, three 1. three-way solenoid valve; 2. boost pipe; 2. pressure reducing pipe; 2. connecting hole; 2. piston rod; 2. sealing block; 2. limiting block; 2. drainage groove; 3. sealing belt; 3. pressure relief pipe; 3. adjusting part; 3. threaded ring; 3. support rod; 3. adjusting screw; 3. abutment ring; 3. adjusting block; 3. knob; 3. plug-in hole; 40. supporting spring; 41. first limiting ring; 42. second limiting ring. DETAILED DESCRIPTION
[0037] In order to make the technical means, creative features, objectives and effects of the present invention easier to understand, the present invention is further described below with reference to specific illustrations.
[0038] like Figure 1-Figure 7 As shown, a cold stamping aluminum production process provides a cold stamping aluminum production process, which solves the problem of low finished product qualification rate in the prior art.
[0039] The technical problem to be solved by the present invention is achieved by adopting the following technical solutions:
[0040] A cold stamping aluminum production process comprises the following steps:
[0041] S1. Grinding waste paper into powder to obtain paper powder; adding the paper powder into an antibacterial color-changing colloid, mixing and stirring to obtain color-changing gelled pulp;
[0042] S2, weighing a certain amount of polyethylene oxide, spraying it on the surface of the aluminum foil layer while it is hot after melting, and then placing the sprayed aluminum foil layer at room temperature to dry, so as to form an isolation layer on the surface of the aluminum foil layer;
[0043] S3, evenly coating the color-changing gelatinized pulp on the surface of the isolation layer, and then compounding a layer of antibacterial color-changing paper base on the surface of the isolation layer to obtain aluminum foil;
[0044] S4, cold stamping the aluminum foil by a cold stamping device 1, the cold stamping device 1 comprises a convex die 2 and a concave die 3, when the aluminum foil is demolded, gas is introduced between the convex die 2 and the aluminum foil, and between the concave die 3 and the aluminum foil, the aluminum foil is separated from the convex die 2 and the concave die 3 respectively by the gas, and after cutting, a finished aluminum foil packaging product is obtained;
[0045] S5. Check the surface defects of the finished aluminum foil packaging products and put the qualified products into storage.
[0046] In order to facilitate the passage of gas between the aluminum foil and the punch 2 and the die 3, the cold stamping equipment 1 includes a punch 2, a die 3 located below the punch 2, and a driving member connected between the punch 2 and the die 3. The punch 2 and the die 3 cooperate to form a cavity 4 when the molds are closed. The peripheral wall of the punch 2 is fixedly connected to an upper mounting plate 5, and the peripheral wall of the die 3 is fixedly connected to a lower mounting plate 6. The driving member includes a hydraulic cylinder 7 fixedly mounted on the lower mounting plate 6 and the piston rod is connected to the upper mounting plate 5.
[0047] A first pressure chamber 8 is provided inside the punch 2 and inside the die 3. The first pressure chamber 8 located in the punch 2 is layered in shape and has the same shape as the bottom of the punch 2. The first pressure chamber 8 located in the die 3 is layered in shape and has the same shape as that inside the die 3. A plurality of air holes 9 connected to the mold cavity 4 are provided on the inner wall of the first pressure chamber 8, and the air holes 9 are evenly distributed in the mold cavity 4.
[0048] The bottom surface of the punch 2 is provided with an annular sealing plate 10 arranged in an annular shape around the cavity 4. The bottom surface of the punch 2 is provided with an annular plug-in groove 11 matched with the annular sealing plate 10. The annular sealing plate 10 is slidably plugged into the annular plug-in groove 11. A plurality of return springs 12 are provided between the top surface of the annular sealing plate 10 and the top surface of the annular plug-in groove 11. When the bottom end of the annular sealing plate 10 abuts against the top surface of the die 3, an air cavity 13 is formed on the upper circumference of the cavity 4. The bottom surface of the punch 2 and the top surface of the die 3 corresponding to the air cavity 13 are provided with an air inlet channel 14 connected to the first pressure cavity 8. A one-way valve 15 is provided in the air inlet channel 14. The one-way valve 15 is used to inlet air into the first pressure cavity 8. In the process of the gradual closing of the punch 2 and the die 3, the air cavity 13 is gradually reduced, and the gas is pressed into the first pressure cavity 8 through the one-way valve 15 and the air inlet channel 14, so that the air pressure in the first pressure cavity 8 is much greater than the air pressure in the cavity 4.
[0049] The bottom end surface of the annular sealing plate 10 is provided with an annular blade 16 circumferentially arranged around the annular sealing plate 10, and the top surface of the die 3 is provided with an annular groove 17 matching with the annular blade 16. When the punch 2 and the die 3 are closed, the annular sealing plate 10 is abutted against the die 3, and the annular blade 16 is inserted into the annular groove 17, so as to cut the aluminum foil.
[0050] In order to facilitate the control of the opening and closing state of the pore 9, a plugging piece 18 is provided on the pore 9, and a control mechanism 19 for controlling the plugging piece 18 to close or open the pore 9 is provided on both the punch 2 and the die 3. The control mechanism 19 includes a second pressure chamber 20 opened inside the punch 2 and the die 3, and a pressure regulating pipe 21 connected to the second pressure chamber 20 and extending to the outside of the punch 2 or the die 3 respectively. The second pressure chamber 20 is a layered cavity structure located on the side of the first pressure chamber 8 away from the cavity 4.
[0051] Among them, the pressure regulating pipe 21 is connected to a three-position three-way solenoid valve 22, and the three-position three-way solenoid valve 22 is respectively connected to a boost pipe 23 and a pressure reducing pipe 24. The pressure medium in the second pressure chamber 20 can be gas or liquid. Correspondingly, the boost pipe 23 is an oil inlet pipe or an air inlet pipe, and the pressure reducing pipe 24 is an oil outlet pipe or an air outlet pipe.
[0052] In the process of the punch 2 and the die 3 gradually closing the mold, the air cavity 13 gradually shrinks, and the gas is pressed into the first pressure chamber 8 through the one-way valve 15 and the air inlet channel 14, so that the air pressure in the first pressure chamber 8 is much greater than the air pressure in the cavity 4. At this time, the three-position three-way valve is controlled to connect the boost pipe 23 to the pressure regulating pipe 21, thereby increasing the air pressure in the second pressure chamber 20, so that the air pressure in the second pressure chamber 20 is greater than the air pressure in the first pressure chamber 8. At this time, under the action of the piston column 26, the sealing block 27 is pressed against the air hole 9 to close the air hole 9. When the punch 2 and the die 3 are opening the mold, the three-position three-way valve is controlled to connect the pressure reducing pipe 24 to the pressure regulating pipe 21, reduce the air pressure in the second pressure chamber 20, and make the air pressure in the second pressure chamber 20 less than the air pressure in the first pressure chamber 8. Under the action of the air pressure difference, the piston drives the sealing block 27 away from the air hole 9, so that the air hole 9 opens.
[0053] The sealing member 18 includes a connecting hole 25 connected between the first pressure chamber 8 and the second pressure chamber 20, a piston column 26 slidably inserted in the connecting hole 25, a sealing block 27 fixedly connected to one end of the piston column 26 located in the first pressure chamber 8, and a limit block 28 fixedly connected to one end of the piston column 26 located in the second pressure chamber 20. The sealing block 27 is slidably inserted in the air hole 9 to close the air hole 9.
[0054] In order to reduce the impact force of the air hole 9 on the aluminum foil when the air is ejected, the air hole 9 is truncated cone-shaped, and the diameter of the air hole 9 near the mold cavity 4 is smaller than the diameter of the air hole 9 near the second pressure chamber 20. The sealing block 27 is a truncated cone structure that matches the air hole 9. The inner peripheral wall of the air hole 9 is provided with a plurality of drainage grooves 29, which penetrate the end of the air hole 9 near the mold cavity 4 and extend along the chord tangent of the air hole 9. The peripheral wall of the sealing block 27 is fixedly connected with a plurality of sealing belts 30 that match the drainage grooves 29.
[0055] When the gas in the first pressure chamber 8 flows into the cavity 4 through the air hole 9, since the air hole 9 is in a truncated cone shape, the drainage groove 29 located on the inner wall of the air hole 9 is inclined relative to the inner wall of the cavity 4. Under the action of the drainage groove 29, the flow direction of the air flow forms an acute angle with the aluminum foil located in the cavity 4, so that when the air flow flows toward the inside of the cavity 4, it is not easy to blow directly on the aluminum foil, thereby reducing the air pressure on the aluminum foil and reducing the possibility of deformation of the aluminum foil.
[0056] The first pressure chamber 8 is connected to a pressure relief pipe 31 extending to the outside of the punch 2 or the outside of the die 3. An adjusting member 32 is provided at one end of the pressure relief pipe 31 away from the first pressure chamber 8. The adjusting member 32 includes a threaded ring 33 located in the pressure relief pipe 31, a plurality of support rods 34 fixedly connected to the threaded ring 33 and the inner wall of the pressure relief pipe 31, an adjusting screw 35 threadedly connected to the threaded ring 33, an abutment ring 36 fixedly connected to the inner wall of the pressure relief pipe 31, and an adjusting block 37 arranged at the end of the adjusting screw 35 and abutting against the inner wall of the abutment ring 36. The inner side wall of the abutment ring 36 is in a frustum shape with a gradually increasing diameter. The adjusting block 37 is arranged in a frustum shape matching the inner side wall of the abutment ring 36. A knob 38 is provided at one end of the adjusting screw 35 extending out of the pressure relief pipe 31.
[0057] The adjusting block 37 is elastically connected to the adjusting screw 35. An inserting hole 39 is provided on the end face of the adjusting block 37. The adjusting screw 35 is slidably inserted into the inserting hole 39. A supporting spring 40 is provided between the end of the adjusting screw 35 and the inner wall of the inserting hole 39. A first limiting ring 41 is fixedly connected to one end of the inner wall of the inserting hole 39 close to the opening, and a second limiting ring 42 is fixedly connected to the peripheral wall of one end of the adjusting screw 35 located in the inserting hole 39.
[0058] By setting a pressure relief pipe 31, and setting an adjusting block 37 and an abutment ring 36 in the pressure relief pipe 31, when cold stamping is performed on aluminum foil of different materials, the adjusting screw 35 is rotated to drive the adjusting block 37 to press against the inner wall of the abutment ring 36. When the air pressure in the first pressure chamber 8 is greater than the elastic force of the supporting spring 40, the air pressure pushes the adjusting block 37 away and can be ejected from the pressure relief pipe 31, so that the first pressure chamber 8 can maintain a constant pressure, thereby reducing the situation where the air pressure in the first pressure chamber 8 is too high, resulting in excessive pressure on the aluminum foil when ejected from the air hole 9.
[0059] The implementation principle of the present invention is:
[0060] In the process of the punch 2 and the die 3 gradually closing, the air cavity 13 gradually shrinks, and the gas is pressed into the first pressure chamber 8 through the one-way valve 15 and the air inlet channel 14, so that the air pressure in the first pressure chamber 8 is much greater than the air pressure in the cavity 4. At this time, the three-position three-way valve is controlled to connect the boosting pipe 23 to the pressure regulating pipe 21, thereby increasing the air pressure in the second pressure chamber 20, so that the air pressure in the second pressure chamber 20 is greater than the air pressure in the first pressure chamber 8. At this time, under the action of the piston column 26, the sealing block 27 is pressed against the air hole 9 to close the air hole 9. When the punch 2 and the die 3 are opening, the three-position three-way valve is controlled to connect the pressure reducing pipe 24 to the pressure regulating pipe 21, so as to reduce the air pressure in the second pressure chamber 20. The air pressure in the second pressure chamber 20 is lower than the air pressure in the first pressure chamber 8. Under the action of the air pressure difference, the piston drives the sealing block 27 away from the air hole 9, so that the air hole 9 is opened, and the gas in the first pressure chamber 8 is injected into the space between the aluminum foil and the punch 2, and the aluminum foil and the die 3 through the air hole 9, so that the gas is filled between the aluminum foil and the punch 2, and the aluminum foil and the die 3. The aluminum foil adhered to the inner wall of the cavity 4 is separated from the punch 2 and the die 3 by the gas. In this process, due to the fluidity of the gas, the finished aluminum foil packaging product is not easy to be torn or deformed due to excessive force on a certain part, and the force on the aluminum foil is more uniform, thereby improving the yield rate of the finished aluminum foil packaging product.
[0061] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of the present invention is defined by the attached claims and their equivalents.
Claims
1. A cold stamping aluminum production process, characterized in that: The following steps are involved: S1. Grinding waste paper into powder to obtain paper powder; adding the paper powder into an antibacterial color-changing colloid, mixing and stirring to obtain color-changing gelled pulp; S2, weighing a certain amount of polyethylene oxide, spraying it on the surface of the aluminum foil layer while it is hot after melting, and then placing the sprayed aluminum foil layer at room temperature to dry, so as to form an isolation layer on the surface of the aluminum foil layer; S3, evenly coating the color-changing gelatinized pulp on the surface of the isolation layer, and then compounding a layer of antibacterial color-changing paper base on the surface of the isolation layer to obtain aluminum foil; S4, cold stamping the aluminum foil using a cold stamping device (1), the cold stamping device (1) comprising a male die (2) and a female die (3), when the aluminum foil is demolded, gas is introduced between the male die (2) and the aluminum foil, and between the female die (3) and the aluminum foil, and the gas separates the aluminum foil from the male die (2) and the female die (3), respectively, and after cutting, a finished aluminum foil packaging product is obtained; S5. Check the surface defects of the finished aluminum foil packaging products and put the qualified products into storage; The cold stamping equipment (1) comprises a punch (2), a die (3) located below the punch (2), and a driving member connected between the punch (2) and the die (3); the punch (2) and the die (3) cooperate to form a cavity (4); a first pressure cavity (8) is provided inside the punch (2) and inside the die (3); a plurality of air holes (9) connected to the cavity (4) are provided on the inner wall of the first pressure cavity (8); a blocking member (18) is provided on the air hole (9); and a control mechanism (19) for controlling the blocking member (18) to close or open the air hole (9) is provided on the punch (2) and the die (3); The bottom surface of the punch (2) is provided with an annular sealing plate (10) which is arranged in an annular shape around the circumference of the cavity (4); the bottom surface of the punch (2) is provided with an annular plug-in groove (11) which matches the annular sealing plate (10); the annular sealing plate (10) is slidably plugged into the annular plug-in groove (11); a plurality of return springs (12) are provided between the top surface of the annular sealing plate (10) and the top surface of the annular plug-in groove (11); when the bottom end of the annular sealing plate (10) abuts against the top surface of the die (3), an air cavity (13) is formed on the upper circumference of the cavity (4); the bottom surface of the punch (2) and the top surface of the die (3) corresponding to the air cavity (13) are provided with an air inlet channel (14) which is connected to the first pressure chamber (8); a one-way valve (15) is provided in the air inlet channel (14); the one-way valve (15) is used to allow air to enter the first pressure chamber (8); The control mechanism (19) comprises a second pressure chamber (20) opened inside the male mold (2) and the female mold (3), a pressure regulating pipe (21) connected to the second pressure chamber (20) and extending to the outside of the male mold (2) or the female mold (3), the pressure regulating pipe (21) being connected to a three-position three-way solenoid valve (22), the three-position three-way solenoid valve (22) being connected to a pressure increasing pipe (23) and a pressure reducing pipe (24), the blocking member (18) comprising a pressure regulating pipe (21) connected to the second pressure chamber (20) and extending to the outside of the male mold (2) or the female mold (3), the pressure regulating pipe (21) being connected to a three-position three-way solenoid valve (22), the pressure regulating pipe (21 ... three-position three-way solenoid valve (22), the pressure regulating pipe (21) being connected to a pressure increasing pipe (23) and a pressure reducing pipe (24), the blocking member (18) comprising a pressure regulating pipe (21) connected to the second pressure chamber (20) and extending to the outside of the male mold (2) or the female mold (3), the pressure regulating pipe (21) being connected to the third pressure A connecting hole (25) between the first pressure chamber (8) and the second pressure chamber (20), a piston column (26) slidably inserted in the connecting hole (25), a sealing block (27) fixedly connected to one end of the piston column (26) located in the first pressure chamber (8), and a limiting block (28) fixedly connected to one end of the piston column (26) located in the second pressure chamber (20), wherein the sealing block (27) is slidably inserted in the air hole (9) to close the air hole (9).
2. A cold stamping aluminum production process according to claim 1, characterized in that: The bottom end surface of the annular sealing plate (10) is provided with an annular blade (16) circumferentially arranged around the annular sealing plate (10), and the top surface of the die (3) is provided with an annular groove (17) matching with the annular blade (16).
3. A cold stamping aluminum production process according to claim 1, characterized in that: The air hole (9) is truncated cone-shaped, and the diameter of the air hole (9) at one end close to the mold cavity (4) is smaller than the diameter of the air hole (9) close to the second pressure chamber (20), and the sealing block (27) is a truncated cone-shaped structure matching the air hole (9).
4. A cold stamping aluminum production process according to claim 3, characterized in that: The inner wall of the air hole (9) is provided with a plurality of drainage grooves (29), the drainage grooves (29) penetrate through one end of the air hole (9) close to the mold cavity (4), the drainage grooves (29) extend along the chord tangent of the air hole (9), and the peripheral wall of the sealing block (27) is fixedly connected with a plurality of sealing belts (30) matching with the drainage grooves (29).
5. A cold stamping aluminum production process according to claim 1, characterized in that: The first pressure chamber (8) on the male mold is connected to a pressure relief pipe (31) extending to the outside of the male mold (2), and the first pressure chamber (8) on the female mold is connected to a pressure relief pipe (31) extending to the outside of the female mold (3). An adjusting member (32) is provided at one end of the pressure relief pipe (31) away from the first pressure chamber (8). The adjusting member (32) includes a threaded ring (33) located inside the pressure relief pipe (31), and a plurality of support rods (34) fixedly connected to the threaded ring (33) and the inner wall of the pressure relief pipe (31). , an adjusting screw (35) threadedly connected to the threaded ring (33), an abutting ring (36) fixedly connected to the inner wall of the pressure relief pipe (31), and an adjusting block (37) arranged at the end of the adjusting screw (35) and abutting against the inner wall of the abutting ring (36), the inner wall of the abutting ring (36) being in the shape of a truncated cone with a gradually increasing diameter, the adjusting block (37) being arranged in the shape of a truncated cone matching the inner wall of the abutting ring (36), and a knob (38) being arranged at one end of the adjusting screw (35) extending out of the pressure relief pipe (31).
6. A cold stamping aluminum production process according to claim 5, characterized in that: The adjusting block (37) and the adjusting screw (35) are elastically connected, and an inserting hole (39) is provided on the end surface of the adjusting block (37). The adjusting screw (35) is slidably inserted into the inserting hole (39). A supporting spring (40) is provided between the end of the adjusting screw (35) and the inner wall of the inserting hole (39). A first limiting ring (41) is fixedly connected to one end of the inner wall of the inserting hole (39) close to the opening, and a second limiting ring (42) is fixedly connected to the peripheral wall of one end of the adjusting screw (35) located in the inserting hole (39).
7. A cold stamping aluminum production process according to claim 1, characterized in that: The circumferential wall of the male die (2) is fixedly connected to an upper mounting plate (5), the circumferential wall of the female die (3) is fixedly connected to a lower mounting plate (6), and the driving member comprises a hydraulic cylinder (7) fixedly mounted on the lower mounting plate (6) and having a piston rod connected to the upper mounting plate (5).