A type I & II composite fatigue fracture test device and method suitable for a variety of specimens

By designing an I&II composite fatigue fracture test device suitable for a variety of specimens, the problems of complex design and high cost of test devices in the existing technology have been solved, the standardization and diversified adaptation of test devices have been achieved, material consumption has been reduced, and material consumption has been improved. improve test efficiency.

CN117491128BActive Publication Date: 2024-10-22TIANJIN UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311380358.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-10-24
Publication Date
2024-10-22
Estimated Expiration
2043-10-24

AI Technical Summary

Technical Problem

The existing technology has failed to develop unified test standards for type I & II composite mode fracture and fatigue crack growth, resulting in complex and high-cost test device design. Different specimen forms and geometric sizes require separate fixture design, which lacks adaptability.

Method used

A test device including a U-shaped hook, sector clamp, auxiliary clamp block and positioning bolt is designed. Through the modular design and the open structure of the sector clamp, it is suitable for a variety of specimen forms and geometric sizes, and uses different auxiliary clamp blocks. and loading methods to achieve type I&II composite fatigue fracture tests.

Benefits of technology

It realizes the standardization and diversified adaptation of test equipment, reduces test costs, reduces material consumption, improves the economy and efficiency of the test process, and can conduct type I&II composite fatigue crack growth and fracture tests.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117491128B_ABST
    Figure CN117491128B_ABST
Patent Text Reader

Abstract

The present invention relates to a type I & II composite fatigue fracture test device and method suitable for a variety of specimens, including a U-shaped hook, a fan-shaped clamp, an auxiliary clamp block and a positioning bolt. The tail of the U-shaped hook is provided with a clamping section, the head of the U-shaped hook is connected to the fan-shaped clamp by a loading pin passing through a through hole, the auxiliary clamp block is fixedly installed in the fan-shaped clamp by a positioning bolt, and the specimen is clamped between a pair of fan-shaped clamps. The present invention adopts a modular design, and by replacing different auxiliary clamp blocks, a set of test devices can be adapted to specimens of different forms, while providing convenience for the development and use of other non-standard specimens; the open design of the fan-shaped clamp slot is adopted, which is convenient for replacing specimens of different thicknesses to study the influence of out-of-plane constraints on fracture behavior and fatigue crack growth behavior. At the same time, the main body of the test device is the same, which reduces the introduction of errors between different tests; the present invention can meet the various needs of type I & II composite fatigue crack growth tests and type I & II composite fracture tests.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of material mechanics test and testing, and in particular relates to a type I & II composite fatigue fracture test device and method suitable for a variety of specimens. Background Art

[0002] Fracture or fatigue crack propagation is the most common failure mode of materials during application. There are inevitably original defects such as microcracks, holes, inclusions, etc. in engineering components or mechanical parts. These defects are often randomly oriented, and the surrounding stress field may have both type I and type II stress states under uniaxial or multiaxial external forces and boundary constraints, facing the risk of composite mode fracture or fatigue failure. Therefore, studying the fracture behavior and fatigue crack propagation behavior of materials in the composite mode of type I&II is an important part of structural integrity analysis and damage tolerance assessment.

[0003] Researchers have been committed to reproducing these material behavior processes in the laboratory and have developed a series of different specimens and fixtures, including compact tensile shear (CTS), enhanced CTS, improved CTS (MCTS), Arcan, etc. These devices can achieve quantitative changes in the proportion of the combined mode I and II at the crack tip of the specimen; by applying quasi-static loads to carry out fracture tests, the initiation fracture toughness and resistance curves in the I&II composite mode can be determined; by applying cyclic loads to carry out fatigue crack growth tests, the threshold value ΔKth and the extension rate da / dN-ΔK curve in the I&II composite mode can be determined.

[0004] However, due to the diversity and complexity of factors such as test materials, specimen forms and geometric dimensions, the research conclusions obtained by the above test methods are not unified, and a unified I&II composite mode fracture and fatigue crack growth test standard has not yet been developed. The development of the device is the primary prerequisite for achieving standardization of the test process. Usually in the test device, different specimen forms often require separate design of matching fixtures; even if the form is the same, in order to study the influence of the constraint effect, the specimen is processed into different geometric dimensions, and the corresponding fixtures also need to be processed, which greatly increases the test cost; and considering that the force required to carry out quasi-static fracture tests is often several times that of fatigue crack growth tests, the specimens and fixtures need to be further strengthened to withstand high-amplitude loads, which means that changes in the test plan will also put forward different requirements for the design of the fixture.

[0005] In summary, it is urgent to propose a set of complete test equipment and methods to meet the requirements of different test schemes (fracture test and fatigue crack growth test), suitable for different specimen forms (CTS, reinforced CTS, MCTS and Arcan, etc.) and geometric dimensions (such as different specimen thicknesses), and provide a new solution and idea for the standardization of type I&II composite mode test process. Summary of the invention

[0006] The purpose of the present invention is to overcome the deficiencies of the prior art and to provide a type I & II composite fatigue fracture test device and method suitable for a variety of specimens.

[0007] The present invention solves the technical problem by the following technical solutions:

[0008] A type I & II composite fatigue fracture test device suitable for a variety of specimens, characterized in that it comprises a pair of U-shaped hooks, a pair of fan-shaped clamps, an auxiliary clamp block and a positioning bolt, the tail of the U-shaped hook is provided with a clamping section, the clamping section cooperates with the chuck of the testing machine, the head of the U-shaped hook is connected to the fan-shaped clamp via a loading pin passing through a through hole, the auxiliary clamp block is fixedly installed in the fan-shaped clamp via a positioning bolt, and the pair of fan-shaped clamps clamp the specimen via the auxiliary clamp block;

[0009] The fan-shaped clamp is integrally arranged and divided into a first thickness section, a second thickness section and a transition section. Five regular through holes are opened on the first thickness section, three pairs of special through holes are opened on the second thickness section, and one special through hole is opened on the transition section. The diameters of the regular through holes, the special through holes and the special through holes are the same and their center points are distributed on the same circumference. The angular interval between each of the regular through holes, the special through holes and the special through holes is 15°. A COD gauge slot is set on the second thickness section, and a COD gauge is placed in the COD gauge slot. A sample slot is set below the first thickness section of the fan-shaped clamp, and a positioning threaded hole is set in the sample slot. An auxiliary clamp block is installed in the positioning threaded hole through a positioning bolt.

[0010] Moreover, the U-shaped hook includes a narrow-pitch U-shaped hook and a wide-pitch U-shaped hook. The tail of the narrow-pitch U-shaped hook is provided with a narrow-pitch clamping section, and the head of the narrow-pitch U-shaped hook is connected to the fan-shaped clamp via a narrow-pitch loading pin passing through a through hole; the tail of the wide-pitch U-shaped hook is provided with a wide-pitch clamping section, and the head of the wide-pitch U-shaped hook is connected to the fan-shaped clamp via a wide-pitch loading pin passing through a through hole.

[0011] Moreover, the specimens include CTS specimens, reinforced CTS specimens, MCTS specimens and Arcan specimens. The CTS specimens, reinforced CTS specimens, MCTS specimens and Arcan specimens are all provided with a single-sided notch that penetrates the thickness in the middle, and a trapezoidal built-in knife edge is provided at the outer end of the single-sided notch for setting up the COD gauge; three connecting pin holes are provided in a row at both ends of the CTS specimen; two reinforced pin holes are added to the outer sides of both ends of the reinforced CTS specimen on the basis of the CTS specimen, and the thickness around the pin holes is thickened; the MCTS specimen is widened at both ends, and the three connecting pin holes at each end are arranged in a triangle; the width of the Arcan specimen is gradually contracted in the middle of the specimen, and the overall shape is butterfly-shaped, with three connecting pin holes in a row at both ends.

[0012] Moreover, the auxiliary clamps include CTS auxiliary clamps, MCTS auxiliary clamps and Arcan auxiliary clamps. The CTS auxiliary clamps, MCTS auxiliary clamps and Arcan auxiliary clamps have the same outline size. The CTS auxiliary clamps are used in combination with CTS specimens through CTS connecting bolts, or in combination with reinforced CTS specimens through CTS connecting bolts and reinforcing bolts; the MCTS auxiliary clamps are used in combination with MCTS specimens through MCTS connecting bolts; and the Arcan auxiliary clamps are used in combination with Arcan specimens through Arcan connecting bolts.

[0013] A type I & II composite fatigue fracture test method applicable to a variety of specimens, characterized in that the method comprises the following steps:

[0014] S1, perform assembly of the specimen components:

[0015] Align all through holes on the auxiliary clamps with the connecting pin holes at both ends of the specimen. Two auxiliary clamps are allocated at each end of the specimen, so that the auxiliary clamps are closely attached to the front and rear surfaces of the specimen. Then, the auxiliary clamps and the specimen are fastened by six connecting bolts to form a specimen assembly.

[0016] S2. assemble and align the sample assembly and the fan-shaped fixture: fill the two ends of the sample assembly into the sample slots of a pair of fan-shaped fixtures respectively, each sample slot holds the two auxiliary clamps at one end of the sample assembly, and the sample assembly and the pair of fan-shaped fixtures form a roughly circular disk as a whole; screw a positioning bolt into each of the pair of positioning threaded holes on both sides of the sample slot, tighten one end of the sample assembly in the sample slot, so that it is fixed with the fan-shaped fixture at the same end, and the other end is operated in the same way; by adjusting the screw-in length of each of the four positioning bolts, the thickness midplane of the sample assembly and the thickness midplane of the two fan-shaped fixtures are made coplanar, thereby completing the centering operation;

[0017] S3. Overall assembly of the test device and the universal testing machine:

[0018] ① Carry out I&II type composite fracture and fatigue crack growth tests at loading angles of 45°, 60°, 75° or 90°: First, operate the upper and lower clamps of the testing machine to clamp the narrow-pitch clamping sections of the tail of a pair of narrow-pitch U-shaped hooks respectively, and control the operation process so that the central axes of the through holes of the two narrow-pitch U-shaped hook heads are parallel to each other; then, connect the entire component assembled in S2 to the upper and lower narrow-pitch U-shaped hooks through a pair of narrow-pitch loading pins, so that the crack behavior of the specimen is pure I type (90°) or I&II type composite (45°, 60° and 75°);

[0019] ② Carry out I&II type composite fracture and fatigue crack growth tests at loading angles of 30°, 15° or 0°: First, operate the upper and lower clamps of the testing machine to clamp the wide-spacing clamping sections of the tail of a pair of wide-spacing U-shaped hooks respectively, and control the central axes of the through holes of the two wide-spacing U-shaped hook heads to be parallel to each other; then, connect the entire component assembled in S2 to the upper and lower wide-spacing U-shaped hooks through a pair of wide-spacing loading pins, so that the crack behavior of the specimen is pure II type (0°) or I&II type composite (15° and 30°);

[0020] S4. The COD gauge foot is matched with the built-in blade of the specimen. The tail of the COD gauge and the signal line are placed in the space of the COD gauge slot. The testing machine applies a quasi-static load to the test device to carry out a fracture test, which can determine the crack initiation toughness and JR curve under the I&II composite mode; the fatigue crack growth test is carried out by applying a cyclic load to determine the threshold value ΔK under the I&II composite mode. th And the expansion rate da / dN-ΔK curve.

[0021] The advantages and beneficial effects of the present invention are:

[0022] 1. The I&II composite fatigue fracture test device of the present invention is applicable to a variety of specimens, has an ingenious structural design, and is quick and efficient in assembly operation.

[0023] 2. The present invention adopts a modular design. By replacing different auxiliary clamps, a set of test equipment can be adapted to different types of specimens. In addition to the four types of specimens involved in this patent, the present invention also facilitates the development and use of other non-standard specimens.

[0024] 3. The present invention adopts an open design of the fan-shaped fixture slot, which is convenient for replacing samples of different thicknesses to study the influence of out-of-plane constraints on fracture behavior and fatigue crack growth behavior. At the same time, the main body of the test device is the same, which reduces the error introduced between different tests.

[0025] 4. The present invention overcomes the drawback of having to replace the test device in order to carry out different tests in the conventional process, which is beneficial to reducing material consumption and improving economy.

[0026] 5. The present invention can be used to carry out type I & II composite fatigue crack growth tests; by strengthening the design of the auxiliary clamps and the specimens, it is also suitable for carrying out type I & II composite fracture tests at high load levels. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 Schematic diagram of the structure of the narrow-distance U-shaped hook at three different viewing angles;

[0028] Figure 2 Schematic diagram of the structure of the wide-spacing U-shaped hook at two different viewing angles;

[0029] Figure 3 The schematic diagrams of the fan-shaped fixture at three different viewing angles;

[0030] Figure 4 The schematic diagrams are the structural diagrams of four different types of specimens (from top to bottom: CTS specimen, enhanced CTS specimen, MCTS specimen and Arcan specimen);

[0031] Figure 5 The following is a schematic diagram of the structures of three different auxiliary clamps (from top to bottom: CTS auxiliary clamp, MCTS auxiliary clamp and Arcan auxiliary clamp);

[0032] Figure 6 The schematic diagrams are the structural diagrams of four different sample assemblies (from top to bottom: CTS sample assembly, enhanced CTS sample assembly, MCTS sample assembly and Arcan sample assembly);

[0033] Figure 7 This is a schematic diagram of the appearance of the COD gauge;

[0034] Figure 8 Schematic diagram of the test device assembly with the reinforced CTS specimen assembly installed at three different viewing angles (45° loading);

[0035] Fig. 9 Schematic diagram of the test device assembly for the reinforced CTS specimen assembly at two different viewing angles (0° loading);

[0036] Fig.10 Schematic diagram of the replacement of different sample components. DETAILED DESCRIPTION

[0037] The present invention is further described in detail below through specific examples. The following examples are only illustrative and not restrictive, and the protection scope of the present invention cannot be limited thereto.

[0038] The purpose of the present invention is to address the defects and shortcomings of the current I&II type composite fracture and fatigue crack growth tests, such as poor versatility and poor economy, and to propose a new test device and method of use that is suitable for specimens of various forms and sizes. In the implementation of this embodiment, the use of reinforced CTS specimens to carry out composite loading at 45° and 0° angles is used as the main case, and the specific device structure and application process are explained in detail:

[0039] This embodiment of Figures 1 to 10 The component numbers involved are as follows:

[0040]

[0041]

[0042] For the 45° loading mode I&II combined fracture and fatigue crack growth tests, the required device components include: a pair of narrow-pitch U-shaped hooks

[10] , a pair of narrow-pitch loading pins

[12] , a pair of fan-shaped clamps

[30] , a reinforced CTS specimen

[50] , four CTS auxiliary clamps

[41] , four positioning bolts

[80] , and six CTS connecting bolts

[42] and four reinforcing bolts

[51] .

[0043] Figure 1 The schematic diagram of the structure of a single narrow-pitch U-shaped hook

[10] is given, and sub-figures (a), (b), and (c) represent three different viewing angles of the same part; a through hole is opened at the head and a narrow-pitch clamping section is provided at the tail

[11] .

[0044] Figure 3 The schematic diagram of the structure of the fan-shaped fixture

[30] is given, and sub-figures (a), (b), and (c) represent three different viewing angles of the same part. As the main component of the test device, the fan-shaped fixture

[30] is a fan-shaped plate with a transitional change in thickness. It is provided with five regular through holes

[31] , one special-shaped through hole

[32] , and three pairs of special through holes

[33] . The three types of through holes have the same diameter and their center points are distributed on the same circumference. The indication meanings of the 0°, 15°, 30°, 45°, 60°, 75°, and 90° marks are as follows: When testing the load angle, the corresponding through holes on the fan-shaped fixture

[30] need to be used, where 0° represents pure type II loading, 90° represents pure type I loading, and the others represent composite loading with different proportions of type I and type II. In particular, the 45° loading test requires the use of the regular through holes

[31] corresponding to the 45° mark. A COD gauge slot

[36] is provided to leave enough space for the placement of the COD gauge

[90] . A sample slot

[35] is provided, and a pair of positioning threaded holes

[34] are provided on its edge, projecting as two-thirds of a circle.

[0045] Figure 4The structural schematic diagrams of four different types of specimens are given. In this example, a reinforced CTS specimen

[50] is required, in which a single-sided notch that penetrates the thickness is provided in the middle, and a trapezoidal built-in knife edge is provided at the outer end of the notch for setting up the COD gauge

[90] . Two reinforcing pin holes are added to the outer sides of the two ends on the basis of the CTS specimen

[40] . The thickness around the pin holes is thickened to prevent tearing under high-amplitude loading, which is suitable for carrying out fracture tests. In order to study the influence of the out-of-plane constraint effect, its thickness can be varied within a certain range. The current test equipment can be adaptively adjusted according to the respective situations.

[0046] Figure 5 The structural schematic diagrams of three different auxiliary clamps are given. In this example, four CTS auxiliary clamps

[41] are required, which are combined with the reinforced CTS specimen

[50] through six CTS connecting bolts

[42] and four reinforcing bolts

[51] to form a reinforced CTS specimen assembly. The specific assembly process is: first, align all the through holes on the four CTS auxiliary clamps

[41] with the connecting pin holes at both ends of the reinforced CTS specimen

[50] ; allocate two CTS auxiliary clamps

[41] at each end of the reinforced CTS specimen

[50] , so that the latter are respectively close to the front and rear surfaces of the specimen, and then fasten the above five parts together through six CTS connecting bolts

[42] and four reinforcing bolts

[51] to form a reinforced CTS specimen assembly. The combination effect is as follows: Figure 6 shown.

[0047] Figure 8 The overall assembly diagram of the test device under 45° loading is given. Sub-figures (a), (b), and (c) represent three different viewing angles of the assembly. The reinforced CTS specimen assembly ( Figure 6) Each end is fixed in the sample slot

[35] of the fan-shaped fixture

[30] by two positioning bolts

[80] and the positioning threaded holes

[34] ; each end is matched with a fan-shaped fixture

[30] , and the whole forms a roughly circular disk; by adjusting the screw-in length of each of the four positioning bolts

[80] , the thickness midplane of the sample and the thickness midplane of the two fan-shaped fixtures

[30] are made coplanar; the upper and lower clamps of the test machine are operated to clamp the narrow-pitch clamping sections

[11] at the tail ends of a pair of narrow-pitch U-shaped hooks

[10] respectively. In order to achieve a good centering effect, the operation process must be controlled so that the center axes of the through holes of the heads of the two narrow-pitch U-shaped hooks

[10] are mutually aligned. Parallel; then the above-assembled disk component is connected to the upper and lower narrow-pitch U-shaped hooks

[10] through a pair of narrow-pitch loading pins

[12] , respectively. Taking 45° loading as an example, the 45° conventional through hole

[31] on the fan-shaped fixture

[30] is inserted into the inner groove of the narrow-pitch U-shaped hook

[10] to be flush with its through hole, and the narrow-pitch loading pin

[12] is inserted so that these holes are connected in series; it is particularly important to note that the upper and lower narrow-pitch U-shaped hooks

[10] should be matched with the 45° conventional through holes

[31] on the two fan-shaped fixtures

[30] at the same time to achieve 45° loading, and mismatching must be avoided; if a COD gauge

[90] (approximate appearance is shown in FIG. 1 ) is required to be installed Figure 7 (Schematic diagram) To measure COD data during the test, the clamping foot of the COD gauge

[90] can be matched with the built-in knife edge of the reinforced CTS specimen

[50] , and the tail of the COD gauge

[90] and the signal line (not shown) are placed in the space of the COD gauge slot

[36] .

[0048] Then the formal test plan was carried out. The test machine applied quasi-static load to the test device to carry out fracture test, which can determine the crack initiation toughness and JR curve under the I&II composite mode; cyclic load was applied to carry out fatigue crack growth test, which can determine the threshold value ΔK under the I&II composite mode. th And expansion rate da / dN-ΔK curve, etc.

[0049] For the I&II type combined fracture and fatigue crack growth tests with 0° loading, the required device components include: a pair of wide-pitch U-shaped hooks

[20] , a pair of wide-pitch loading pins

[22] , a pair of fan-shaped clamps

[30] , a reinforced CTS specimen

[50] , four CTS auxiliary clamps

[41] , four positioning bolts

[80] , and six CTS connecting bolts

[42] and four reinforcing bolts

[51] . The only difference from the components required for 0° loading is that the narrow-pitch U-shaped hooks

[10] and narrow-pitch loading pins

[12] are replaced with wide-pitch U-shaped hooks

[20] and wide-pitch loading pins

[22] .

[0050] Figure 2The schematic diagram of the structure of a single wide-pitch U-shaped hook

[20] is given, and sub-figures (a) and (b) show two different perspectives of the same part; a through hole is opened at the head and a narrow-pitch clamping section is provided at the tail

[21] . The structures of the fan-shaped fixture

[30] , the reinforced CTS specimen

[50] , the CTS auxiliary clamp

[41] and the reinforced CTS specimen assembly are shown in Fig. Figure 3 , Figure 4 , Figure 5 and Figure 6 ; The combination or assembly method between them is also the same as that of the embodiment of 45° compound loading. The only difference is that during the specific operation, the upper and lower clamps of the testing machine should respectively clamp the wide-spacing clamping sections

[21] at the tail ends of a pair of wide-spacing U-shaped hooks

[20] ; in order to achieve a good centering effect, the operation process must be controlled so that the central axes of the through holes at the heads of the two wide-spacing U-shaped hooks

[20] are parallel to each other; then the assembled disk component (including a pair of fan-shaped clamps

[30] , a reinforced CTS specimen assembly and four positioning bolts

[80] ) is connected to the upper and lower wide-spacing U-shaped hooks

[20] through a pair of wide-spacing loading pins

[22] ; it is particularly important that the upper and lower wide-spacing U-shaped hooks

[20] should be matched with the special through holes

[33] corresponding to 0° on the two fan-shaped clamps

[30] at the same time to achieve 0° loading.

[0051] The test device proposed in the present invention has simple and exquisite components and is easy and efficient to use. It adopts a modular design and can adapt a set of test devices to different types of specimens by replacing different auxiliary clamps. In addition to the reinforced CTS specimens involved in the embodiment

[50] , Fig.10 As shown, the device can also be used to test CTS specimens

[40] , MCTS specimens

[60] and Arcan specimens

[70] , and provide convenience for the development and use of other non-standard specimens; the open design of the fan-shaped fixture slot is adopted to facilitate the replacement of specimens of different thicknesses to study the influence of out-of-plane constraints on fracture behavior and fatigue crack growth behavior. At the same time, the main body of the test device is the same, which reduces the introduction of errors between different tests; the device can meet the various needs of type I & II composite fatigue crack growth tests and type I & II composite fracture tests; the present invention overcomes the disadvantage of having to replace the test device in the conventional process to carry out different tests, which is beneficial to reducing material consumption and improving economy.

[0052] Although the embodiments and drawings of the present invention are disclosed for illustrative purposes, those skilled in the art will appreciate that various substitutions, changes and modifications are possible without departing from the spirit and scope of the present invention and the appended claims. Therefore, the scope of the present invention is not limited to the contents disclosed in the embodiments and drawings.

Claims

1. A type I & II composite fatigue fracture test method applicable to a variety of specimens, characterized by: The test device adopted by the method includes a pair of U-shaped hooks, a pair of fan-shaped clamps, an auxiliary clamp block and a positioning bolt. The tail of the U-shaped hook is provided with a clamping section, and the clamping section cooperates with the clamp of the testing machine. The head of the U-shaped hook is connected to the fan-shaped clamp through a loading pin passing through a through hole. The auxiliary clamp block is fixedly installed in the fan-shaped clamp by a positioning bolt, and the auxiliary clamp block is used to clamp the sample between the pair of fan-shaped clamps. The fan-shaped fixture is integrally arranged and divided into a first thickness section, a second thickness section and a transition section. The first thickness section is provided with five regular through holes, the second thickness section is provided with three pairs of special through holes, and the transition section is provided with a special-shaped through hole. The diameters of the regular through holes, the special-shaped through holes and the special through holes are the same and their center points are distributed on the same circumference. The angle interval between the regular through holes, the special-shaped through holes and the special through holes is 15°. The second thickness section is provided with a COD gauge slot, in which a COD gauge is placed. A sample card slot is provided below the first thickness section of the fan-shaped fixture, and a positioning threaded hole is provided at the edge of the sample card slot. An auxiliary clamp block is installed in the positioning threaded hole through a positioning bolt. The U-shaped hook includes a narrow-pitch U-shaped hook and a wide-pitch U-shaped hook, the tail of the narrow-pitch U-shaped hook is provided with a narrow-pitch clamping section, and the head of the narrow-pitch U-shaped hook is connected to the fan-shaped clamp through a narrow-pitch loading pin passing through a through hole; the tail of the wide-pitch U-shaped hook is provided with a wide-pitch clamping section, and the head of the wide-pitch U-shaped hook is connected to the fan-shaped clamp through a wide-pitch loading pin passing through a through hole; The samples include CTS samples, reinforced CTS samples, MCTS samples and Arcan samples. The middle of the CTS samples, reinforced CTS samples, MCTS samples and Arcan samples are all provided with a single-sided notch that penetrates the thickness, and the outer end of the single-sided notch is provided with a trapezoidal built-in knife edge for setting up the COD gauge; three connecting pin holes are arranged in a row at both ends of the CTS sample; two reinforced pin holes are added to the outer sides of both ends of the reinforced CTS sample on the basis of the CTS sample, and the thickness around the pin holes is thickened; the MCTS sample is widened at both ends, and the three connecting pin holes at each end are arranged in a triangle; the width of the Arcan sample is gradually contracted in the middle of the sample, and the overall shape is similar to a butterfly, and the connecting pin holes at both ends are three in a row; The auxiliary clamps include CTS auxiliary clamps, MCTS auxiliary clamps and Arcan auxiliary clamps. The CTS auxiliary clamps, MCTS auxiliary clamps and Arcan auxiliary clamps have the same outline size. The CTS auxiliary clamps are used in combination with CTS specimens through CTS connecting bolts, or in combination with reinforced CTS specimens through CTS connecting bolts and reinforcing bolts; the MCTS auxiliary clamps are used in combination with MCTS specimens through MCTS connecting bolts; and the Arcan auxiliary clamps are used in combination with Arcan specimens through Arcan connecting bolts. The steps of the method are: S1, perform assembly of the specimen components: Align all through holes on the auxiliary clamps with the connecting pin holes at both ends of the specimen. Two auxiliary clamps are allocated at each end of the specimen, so that the auxiliary clamps are closely attached to the front and rear surfaces of the specimen. Then, the auxiliary clamps and the specimen are fastened by six connecting bolts to form a specimen assembly. S2. Assemble and align the sample assembly and the fan-shaped fixture: fill the two ends of the sample assembly into the sample slots of a pair of fan-shaped fixtures respectively, each sample slot holds the two auxiliary clamps at one end of the sample assembly, and the sample assembly and the pair of fan-shaped fixtures form a disc as a whole; screw a positioning bolt into each of the pair of positioning threaded holes on both sides of the sample slot, tighten one end of the sample assembly in the sample slot, so that it is fixed with the fan-shaped fixture at the same end, and the other end is operated in the same way; by adjusting the screw-in length of each of the four positioning bolts, the thickness midplane of the sample assembly and the thickness midplane of the two fan-shaped fixtures are made coplanar, thereby completing the centering operation; S3. Overall assembly of the test device and the universal testing machine: ① Carry out I&II type composite fracture and fatigue crack growth tests at loading angles of 45°, 60°, 75° or 90°: First, operate the upper and lower clamps of the testing machine to clamp the narrow-pitch clamping sections of the tail of a pair of narrow-pitch U-shaped hooks respectively, and control the operation process so that the central axes of the through holes of the two narrow-pitch U-shaped hook heads are parallel to each other; then, connect the entire component assembled in S2 to the upper and lower narrow-pitch U-shaped hooks through a pair of narrow-pitch loading pins, so that the crack behavior of the specimen is pure I type or I&II type composite; ② Carry out I&II type composite fracture and fatigue crack growth tests at loading angles of 30°, 15° or 0°: First, operate the upper and lower clamps of the testing machine to clamp the wide-spacing clamping sections of the tail of a pair of wide-spacing U-shaped hooks respectively, and control the central axes of the through holes of the two wide-spacing U-shaped hook heads to be parallel to each other; then, connect the entire component assembled in S2 to the upper and lower wide-spacing U-shaped hooks through a pair of wide-spacing loading pins, so that the crack behavior of the specimen is pure II type or I&II type composite; S4. The COD gauge foot is matched with the built-in blade of the sample. The tail of the COD gauge and the signal line are placed in the space of the COD gauge slot. The testing machine applies a quasi-static load to the test device to carry out a fracture test to determine the crack initiation toughness and J -R curve; fatigue crack growth test was carried out by applying cyclic load to determine the threshold value ∆ in the combined mode of I & II K th and expansion rate d a / d N -∆ K curve.