A steel lining plastic rotational molding preparation process and rotational molding machine for the preparation
By rough processing first and then comprehensively processing in the steel-lined plastic pipe rotary molding preparation process and the design of combining rotary rotary molding mechanism with oven swing rotary molding machine, the problems of working time and energy consumption in the existing process are solved, and the problem of high power consumption in the existing process is achieved. More efficient surface treatment and energy consumption reduction.
Patent Information
- Application Number
- CN202410935637.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-07-12
AI Technical Summary
The existing rotomolding process of steel-lined plastic pipes has multiple steel pipe surface treatment processes, resulting in high working hours, wear and energy consumption, and backward molding equipment technology, low mold processing accuracy and low production efficiency.
Design a steel-lined plastic rotomolding preparation process, first roughly process the outer surface of the steel pipe, and then perform comprehensive surface treatment after the rotation molding is completed. The oven swing rotomolding machine combined with a rotary rotomolding mechanism and an intermediate frequency furnace is used to seal the cavity and seal it. Thermal insulation roller shutter door reduces energy consumption and optimizes the heating and cooling process.
Improves surface finish and appearance quality, reduces surface treatment steps, reduces energy consumption and working hours, and improves production efficiency and finished product quality.
Smart Images

Figure CN118477808B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the molding or connection of plastics and the molding of materials in a plastic state, and in particular to a steel lining plastic rotational molding preparation process and a rotational molding machine for the preparation. Background Art
[0002] Plastic-lined pipes, also known as steel-plastic composite pipes, use ordinary carbon steel pipes as the base, and are lined with thermoplastic plastic pipes with excellent chemical stability (commonly used PE, PO, PVC, PTFE), which are cold-drawn composite or rotationally molded. The most commonly used method in the market is rotational molding. Steel-lined plastic pipe rotational molding is also known as rotational molding, rotational molding, rotational casting, rotational molding, etc. First, the plastic raw material is added to the mold, and then the mold is continuously rotated along two vertical axes and heated, so that the plastic raw material in the mold is gradually and evenly coated, melted and adhered to the entire surface of the mold cavity under the action of gravity and heat energy, and formed into the required shape, and then cooled, finalized, and demolded to finally obtain the product. As a result, it has both the mechanical properties of steel pipes and the characteristics of plastic pipes such as corrosion resistance, slow scaling, and difficulty in the growth of microorganisms. It is an ideal pipeline for transporting media such as acids, alkalis, salts, and corrosive gases.
[0003] In the process of roto-molding of steel-lined plastic pipes, the surface of the steel pipe is usually treated first (usually by grinding and rust removal), then the flange is welded to the end of the steel pipe, the welding part is polished, and then the inner and outer surfaces of the entire pipe are treated (usually by sandblasting and rust removal). The steel pipe is then heated, and the plastic raw material is put into the pipe. The pipe is rotated back and forth so that the plastic powder is evenly attached to the inner wall of the pipe. The steel-lined plastic pipe is obtained after cooling. However, this method involves multiple steel pipe surface treatment processes (wear and rust removal, grinding welding parts, and sandblasting), which requires more working hours and reduces work efficiency. In addition, during roto-molding, the outer surface of the steel pipe in the early stage of surface treatment is subjected to certain wear or scratches due to rolling contact with the roto-molding drive component (usually the roller that drives the steel pipe to rotate). Therefore, there are unreasonable aspects in the existing roto-molding preparation process of steel-lined plastic pipes.
[0004] Qin Liu mentioned in the paper "Advanced Manufacturing Technology of Roto-molding of Large Plastic Products" published in "Plastics" Volume 42, Issue 4, 2013: Roto-molding is a unique process for preparing hollow plastic products, suitable for processing thermoplastic polymers, and has a history of several decades in the field of plastic processing. Its molding process mainly includes: filling polymer, heating, cooling, and demolding. The roto-molding equipment has a simple structure and is suitable for molding hollow products with complex shapes, fine surface textures, large and extra-large sizes... But it has its own defects such as backward molding equipment technology, low mold processing accuracy, long molding cycle, low production efficiency, and high energy consumption. Han Daming's paper "Research on Energy-saving Methods for Roto-molded Biogas Tank Processing" published in "Forest Engineering" Volume 28, Issue 1, January 2012, uses instruments to directly and accurately measure the temperature inside the mold to prevent overheating; uses an insulation cover to seal the mold in the swing roto-molding machine to reduce gas convection heat dissipation and radiation heat dissipation; adds an insulation layer, reduces the shaft diameter, and reduces conduction heat dissipation; uses infrared radiation temperature measurement to prevent overheating; these energy-saving methods. However, these energy-saving methods are still implemented by setting them up inside the rotomolding machine. The rotomolding machine itself is large in size because it needs to accommodate the rotation of the mold (especially the revolution and rotation of the two axes), so the energy consumption required for heating is also large. Therefore, even if these methods are adopted, the energy-saving effect is limited. Summary of the invention
[0005] The purpose of the present invention is to overcome the defects existing in the prior art and provide a steel lining plastic rotational molding preparation process, in which the entire surface treatment of the outer surface of the steel pipe is carried out only after the rotational molding is completed; this process is reasonably designed and can ensure the surface smoothness and appearance quality; and because the surface treatment process is placed after the rotational molding, the number of surface treatment passes or the workload can be appropriately reduced.
[0006] To achieve the above object, the technical solution of the present invention is to design a steel liner plastic rotational molding preparation process, which consists of the following process steps performed in sequence:
[0007] S1: Welding: Cut the steel pipe according to the size required by the customer, and weld the flange that matches the steel pipe to the end of the steel pipe;
[0008] S2: Grinding and sandblasting to remove rust: Grind the welding part between the steel pipe and the flange; then perform partial sandblasting to remove rust: 1. Use a sandblasting gun to sandblast the inside of the steel pipe; 2. Use a sandblasting gun to sandblast and remove rust on only this part of the outer surface according to the contact position between the steel pipe and the driving wheel during rotational molding;
[0009] S3: Heating the steel pipe: Put the steel pipe into the medium frequency furnace for uniform heating;
[0010] S4: Filler: Calculate the required plastic raw materials according to the thickness of the lining and fill the plastic raw materials into the heated steel pipe;
[0011] S5: Hot rotomolding: The plastic raw material is centrifugally rolled onto the inner wall of the pipe through a rotary rotomolding mechanism; a driving wheel for driving the steel pipe to rotate is provided on the rotary rotomolding mechanism;
[0012] S6: Cooling and shaping: scrape off the excess material at both ends of the pipe; then cool and shape it to form a plastic-lined pipe; frost and remove rust on the outer surface of the steel pipe and then sandblast it;
[0013] S7: Rust removal and painting: After the pipeline has cooled, the outer pipe is rust-free and painted with anti-corrosion paint. After drying, it is the finished product.
[0014] S8: Detect the quality of steel-lined plastic pipes: Use the electric spark detection method to detect the quality of the pipe. In the S3 step, the medium frequency furnace can also be replaced by other heating furnace bodies. The steel-lined plastic rotational molding preparation process here is a preparation process for straight steel-lined plastic pipes. When the steel-lined plastic pipe is prepared by rotational molding, it is first rough-processed (grinding and rust-removing part of the outer surface of the steel pipe). It is only necessary to ensure that the rotation of the pipe is stable during rotational molding (that is, the contact point where the pipe rotates and rolls during rotational molding is flat). The entire surface treatment of the outer surface of the steel pipe is performed after rotational molding; this process is reasonably designed and can ensure surface finish and appearance quality; and because the surface treatment process is placed after rotational molding, the number of surface treatment passes or workload can be appropriately reduced.
[0015] A further technical solution is that in step S3, the temperature is heated to 300-370°C and then maintained for 2 hours; in step S6, the steel pipe is rotated during cooling.
[0016] A further technical solution is that, in step S8, a JG-373 electric spark micropore flaw detector is used and carried out at an output voltage of 5KV-30KV; the flaw detector is qualified if no penetration occurs.
[0017] A further technical solution is that the surface roughness obtained by sandblasting and rust removal in step S2 is rougher than the surface roughness obtained by sandblasting in step S6. As is well known, the larger the value of roughness ra, the rougher it is; so although step S6 sandblasts the entire outer surface of the steel pipe, the contact position between the steel pipe and the drive wheel is equivalent to a secondary sandblasting (since secondary sandblasting can make the workpiece surface smoother, that is, the roughness ra value is lower), to obtain the final required finish requirements.
[0018] The present invention also provides a technical solution, that is, a roto-molding machine for preparing steel-lined plastic roto-molding, which is composed of an oven swing roto-molding machine dedicated to roto-molding of curved steel-lined plastic pipe linings and a rotary roto-molding mechanism dedicated to roto-molding of straight steel-lined plastic pipe linings;
[0019] The rotary roto-molding mechanism comprises a closed cavity connected to the medium frequency furnace through a connecting pipe, a roller frame is arranged in the closed cavity, and the roller frame is adapted to the heated steel pipe to be roto-molded;
[0020] The intermediate frequency furnace and the closed cavity are arranged in sequence and the two are connected, and a sealed heat-insulating rolling shutter door is arranged at the connecting point;
[0021] There are multiple connecting pipes, and the connection position of each connecting pipe and the closed cavity is located at different positions in the length direction of the closed cavity to realize the introduction of heated air in the medium frequency furnace body into the closed cavity from multiple different points. The rotomolding machine includes an oven swing rotomolding machine and a steel-lined plastic pipe rotary rotomolding mechanism; it can minimize energy consumption (using an oven swing rotomolding machine alone consumes a lot of energy); the oven swing rotomolding machine is used for the rotomolding preparation of curved steel-lined plastic pipes, and can also be used for the rotomolding preparation of other steel-lined plastic products such as steel-lined plastic storage tanks (because the oven swing rotomolding machine is not limited by the volume of the hot box, the product size is larger, the price is lower, and there are more practical applications); through the improvement of the rotomolding machine itself, the original rotomolding preparation of the inner lining of straight pipes and curved pipes, which was originally all made of oven swing rotomolding machines or other rotomolding machines, is changed to the rotomolding preparation of straight pipes, and no longer uses a large-volume oven swing rotomolding machine; energy consumption is greatly reduced, and the energy-saving effect is obvious. A hinged opening and closing door is set on the closed cavity for the steel pipe to enter and exit. After the steel pipe is moved to the closed cavity, the opening and closing door is closed to ensure relative closure, and then the roller frame is started to drive the steel pipe to rotate. The feeding pipe is used to add material to the inner wall of the steel pipe. The material should be added evenly and the steel pipe should be rotated immediately after adding.
[0022] When the steel pipe is heated by the medium frequency furnace, the valve on the connecting pipe is closed to avoid increased energy consumption. After the heating is completed, the steel pipe is moved into the closed cavity and the valve is opened to utilize the waste heat of the medium frequency furnace (because heat dissipation also occurs during the heating process of the medium frequency furnace, and part of the heat is lost to the air, and the heated air is passed through the connecting pipe to heat the air in the closed cavity; if it is other furnace bodies, the heated air in the furnace body can be used to heat the air in the closed cavity) to avoid poor lining effect or surface quality problems caused by cooling of the steel pipe when the steel pipe is driven to rotate by the roller frame and its inner wall is rotationally molded into an inner lining; due to the arrangement of introducing hot air into the closed cavity, combined with the closed cavity that is only slightly larger than the size of the steel pipe, the heated steel pipe can be effectively insulated, the lining effect is effectively improved, and the lining efficiency is also improved.
[0023] The medium frequency furnace and the closed cavity are arranged in sequence and the two are connected. A sealed heat-insulating rolling shutter door is arranged at the connecting point. The sealed heat-insulating rolling shutter door can be closed when the medium frequency furnace is used to heat the steel pipe to avoid increased energy consumption. When the heating is completed and the steel pipe needs to be moved to the closed cavity, the sealed heat-insulating rolling shutter door is opened to avoid the steel pipe being cooled too early due to contact with the outside air or a long transfer path when transferring the steel pipe from the medium frequency furnace as in the prior art. Since the transfer path length is shortened, the heating temperature of the medium frequency furnace can be set lower, so the energy consumption is further reduced.
[0024] A further technical solution is that the roller frame includes a pair of roller seats arranged along the length direction of the steel pipe, each roller seat is provided with two pairs of rollers arranged opposite to each other, the two pairs of rollers are located at two corners of the roller seat, and one of the four rollers is connected to the reduction motor to realize the driving of the steel pipe placed on the roller to rotate when the reduction motor is started.
[0025] The advantages and beneficial effects of the present invention are as follows: when the steel-lined plastic pipe is prepared by rotational molding, rough processing is first performed (grinding and removing rust from the outer surface of the steel pipe). It is only necessary to ensure that the pipe rotates stably during rotational molding (that is, the contact point where the pipe rotates and rolls during rotational molding is flat). The entire surface treatment of the outer surface of the steel pipe is performed after the rotational molding is completed. This process is reasonably designed and can ensure surface smoothness and appearance quality. Moreover, since the surface treatment process is placed after the rotational molding, the number of surface treatment passes or the workload can be appropriately reduced.
[0026] Although the entire outer surface of the steel pipe is sandblasted in step S6, the contact position between the steel pipe and the driving wheel is equivalent to a secondary sandblasting (since the secondary sandblasting can make the workpiece surface smoother, that is, the roughness ra value is lower), the final required smoothness requirement is obtained.
[0027] The rotomolding machine includes an oven swing rotomolding machine and a steel-lined plastic pipe rotary rotomolding mechanism; it can minimize energy consumption (using an oven swing rotomolding machine alone consumes a lot of energy); the oven swing rotomolding machine is used for the rotomolding preparation of curved steel-lined plastic pipes, and can also be used for the rotomolding preparation of other steel-lined plastic products such as steel-lined plastic storage tanks (because the oven swing rotomolding machine is not limited by the volume of the hot box, the product size is larger, the price is lower, and there are more practical applications); through the improvement of the rotomolding machine itself, the rotomolding preparation of the inner lining of straight pipes and curved pipes, which was originally all made by oven swing rotomolding machines or other rotomolding machines, is changed to the rotomolding preparation for straight pipes, and the large-volume oven swing rotomolding machine is no longer used; the energy consumption is greatly reduced, and the energy-saving effect is obvious.
[0028] When the steel pipe is heated by the medium frequency furnace, the valve on the connecting pipe is closed to avoid increased energy consumption. After the heating is completed, the steel pipe is moved into the closed cavity and the valve is opened to utilize the waste heat of the medium frequency furnace (because heat dissipation also occurs during the heating process of the medium frequency furnace, and part of the heat is lost to the air, and the heated air is passed through the connecting pipe to heat the air in the closed cavity; if it is other furnace bodies, the heated air in the furnace body can be used to heat the air in the closed cavity) to avoid poor lining effect or surface quality problems caused by cooling of the steel pipe when the steel pipe is driven to rotate by the roller frame and its inner wall is rotationally molded into an inner lining; due to the arrangement of introducing hot air into the closed cavity, combined with the closed cavity that is only slightly larger than the size of the steel pipe, the heated steel pipe can be effectively insulated, the lining effect is effectively improved, and the lining efficiency is also improved.
[0029] The medium frequency furnace and the closed cavity are arranged in sequence and the two are connected. A sealed heat-insulating rolling shutter door is arranged at the connecting point. The sealed heat-insulating rolling shutter door can be closed when the medium frequency furnace is used to heat the steel pipe to avoid increased energy consumption. When the heating is completed and the steel pipe needs to be moved to the closed cavity, the sealed heat-insulating rolling shutter door is opened to avoid the steel pipe being cooled too early due to contact with the outside air or a long transfer path when transferring the steel pipe from the medium frequency furnace as in the prior art. Since the transfer path length is shortened, the heating temperature of the medium frequency furnace can be set lower, so the energy consumption is further reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of a rotary rotomolding mechanism in Embodiment 1 of a rotomolding machine for preparing steel liner plastic rotomolding of the present invention;
[0031] Figure 2 yes Figure 1 Side view of
[0032] Figure 3 yes Figure 1 A side view of the middle roller seat portion;
[0033] Figure 4 is a schematic diagram of a second embodiment of the present invention;
[0034] Figure 5 yes Figure 3 A three-dimensional schematic diagram of
[0035] Figure 6 is a schematic diagram of a rotary rotomolding mechanism in Embodiment 3 of the present invention;
[0036] Figure 7 yes Figure 6 Side view of
[0037] Figure 8 is a schematic diagram of a fourth embodiment of the present invention;
[0038] Fig. 9 yes Figure 8 Schematic diagram of semi-finished steel lined plastic pipe;
[0039] Fig.10 yes Figure 8 Bottom view at the middle right end;
[0040] Fig.11 yes Figure 8 Schematic diagram of the insulation collar outside the elbow at the middle left end.
[0041] In the figure: 1. roller; 2. steel pipe; 3. medium frequency furnace; 4. roller seat; 5. reduction motor; 6. placement seat; 7. connecting pipe; 8. closed cavity; 9. sealed insulation rolling shutter door; 10. closed connecting chamber; 11. polyimide film; 12. insulation sleeve; 13. inflation nozzle; 14. metal ring; 15. insulation sleeve ring; 16. cooling water injection nozzle; 17. rubber opening and closing door. DETAILED DESCRIPTION
[0042] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and embodiments. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the present invention.
[0043] Embodiment 1: Figures 1 to 3 , Figure 5 As shown (for ease of illustration, Figure 1 The roller seat and the reduction motor are not shown). The present invention is a steel liner plastic rotational molding preparation process, and the process is as follows:
[0044] Welding: Cut the steel pipe according to the size required by the customer, and then weld the flange to the steel pipe inside and outside. In this process, the outer surface of the steel pipe is no longer frosted and rusted as in the prior art, but the frosting and rusting surface treatment process is set after rotational molding to avoid wear or scratches caused by treatment before rotational molding;
[0045] Grinding and sandblasting for rust removal: Grind the welding part between the steel pipe and the flange; then perform sandblasting for rust removal, and use a sandblasting gun to sandblast the inside of the steel pipe to make the steel pipe better integrated with the plastic; (in this process, only part of the outer surface of the steel pipe is sandblasted for rust removal and a lower sandblasting requirement is adopted, so that a roughness that is not required for the final finish is first obtained, that is, the roughness ra value after sandblasting of part of the outer surface is relatively large, because it only needs to meet the requirements that the outer surface of the steel pipe 2 that contacts the driving wheel (and the roller 1 on the roller frame) during rotational molding is flat, so the sandblasting requirements of these local parts can be relatively low at this time, which also reduces the cost of the entire process).
[0046] Heating the steel pipe: put the steel pipe 2 into the medium frequency furnace 3 and heat it evenly (to 300-370℃ for 2 hours) to reach the set temperature;
[0047] Filling part: lining thickness, calculate the required plastic raw materials, and fill the plastic raw materials into the heated steel pipe 2 pipeline;
[0048] Hot roto-molding part: The plastic raw material is centrifugally rolled onto the inner wall of the steel pipe 2 through a rotating roto-molding mechanism: the steel pipe 2 is continuously rotated along the axis, and the plastic raw material is gradually and evenly coated, melted and adhered to the entire surface of the inner cavity of the steel pipe under the action of gravity and heat energy; (the rotating roto-molding mechanism is mainly a roller rack; the heated steel pipe 2 is placed on the roller rack for roto-molding process)
[0049] Use corresponding tools to scrape off the excess material at both ends of the steel pipe 2; then cool and shape it to form a plastic-lined pipe; cool the plastic layer until the sealing surface is bright, smooth and solidified; rotate during cooling to prevent local high-temperature flow that affects use and appearance; then frost and remove rust on the outer surface of the steel pipe 2 and then sandblast it (the sandblasting at this time obtains the final required smoothness, that is, the value of the roughness ra after sandblasting is smaller, and this sandblasting is equivalent to secondary sandblasting for the outer surface of the steel pipe that contacts the drive wheel during rotational molding); it can ensure surface smoothness and appearance quality; and since the surface treatment process is placed after rotational molding, the number of surface treatment passes or workload can be appropriately reduced.
[0050] Remove rust and paint. After the pipeline has cooled down, remove rust from the outer tube of steel pipe 2 and paint it with anti-corrosion paint. After it dries, it is the finished product.
[0051] Electric spark detection of pipe quality: Use JG-373 electric spark microporous flaw detector at an output voltage of 5KV-30KV; it is qualified if it cannot be squeezed through; keep the steel pipe 2 rotating during cooling.
[0052] The surface roughness obtained by sandblasting only a portion of the outer surface of the steel pipe 2 is rougher than the surface roughness obtained by sandblasting the entire outer surface of the steel pipe.
[0053] The rotomolding machine for steel-lined plastic rotomolding preparation is composed of an oven swing rotomolding machine specially used for curved pipe steel-lined plastic rotomolding and a rotary rotomolding mechanism specially used for straight pipe steel-lined plastic rotomolding.
[0054] The roller frame includes a pair of roller seats 4 arranged along the length direction of the steel pipe 2, and each roller seat is provided with two pairs of rollers 1 arranged opposite to each other, and the two pairs of rollers are located at two corners of the roller seat 4. One of the four rollers is connected to the reduction motor 5 to realize that when the reduction motor is started, the steel pipe 2 placed on the roller 1 is driven to rotate. A reduction motor placement seat 6 is provided on one side of the roller seat.
[0055] The rotary roto-molding mechanism comprises a closed cavity 8 connected to the medium frequency furnace 3 via a connecting pipe 7, a roller frame is arranged in the closed cavity 8, and the roller frame is adapted to the heated steel pipe 2 to be roto-molded;
[0056] The intermediate frequency furnace 3 and the closed cavity 8 are arranged in sequence and are connected, and a sealed heat-insulating rolling shutter door 9 is arranged at the connection point. The intermediate frequency furnace and the closed cavity are arranged in sequence and are connected, and a sealed heat-insulating rolling shutter door is arranged at the connection point. When the intermediate frequency furnace is used to heat the steel pipe, the sealed heat-insulating rolling shutter door can be closed to avoid increased energy consumption. When the steel pipe needs to be moved to the closed cavity after heating, the sealed heat-insulating rolling shutter door is opened to avoid the steel pipe being cooled too early due to contact with the outside air or a long transfer path when transferring the steel pipe from the intermediate frequency furnace as in the prior art. Since the transfer path length is shortened, the heating temperature of the intermediate frequency furnace can be set lower, so the energy consumption is further reduced.
[0057] The connection between the medium frequency furnace and the closed cavity is a closed connecting chamber 10, which is provided with an opening and closing door for workers to enter; the length of the closed connecting chamber is sufficient for workers to easily take out the heated steel pipes in the medium frequency furnace after the furnace door is opened; the furnace door is closed immediately after taking them out to prevent too much high-temperature air from overflowing from the furnace body of the medium frequency furnace. After the medium frequency furnace is finished working, the sealed heat-insulating rolling shutter door between the medium frequency furnace and the closed cavity is not opened to achieve heat exchange; to prevent the air temperature in the medium frequency furnace from being too high; on the other hand, after such a setting, multiple connecting pipes 7 can be set, and the connection position of each connecting pipe 7 with the closed cavity is located at different positions in the length direction of the closed cavity to realize the introduction of heated air in the furnace body of the medium frequency furnace into the closed cavity from multiple different points, ensuring that the closed cavity reaches a uniform cavity temperature faster, ensuring a better insulation effect, and thus ensuring the rotational molding effect.
[0058] When the steel pipe is heated by the medium frequency furnace, the valve on the connecting pipe is closed to avoid increased energy consumption. After the heating is completed, the steel pipe is moved into the closed cavity and the valve is opened to utilize the waste heat of the medium frequency furnace (because heat dissipation also occurs during the heating process of the medium frequency furnace, and part of the heat is lost to the air, and the heated air is passed through the connecting pipe to heat the air in the closed cavity; if it is other furnace bodies, the heated air in the furnace body can be used to heat the air in the closed cavity) to avoid poor lining effect or surface quality problems caused by cooling of the steel pipe when the steel pipe is driven to rotate by the roller frame and its inner wall is rotationally molded into an inner lining; due to the arrangement of introducing hot air into the closed cavity, combined with the closed cavity that is only slightly larger than the size of the steel pipe, the heated steel pipe can be effectively insulated, the lining effect is effectively improved, and the lining efficiency is also improved.
[0059] Embodiment 2: The difference from Embodiment 1 is that Figure 4 As shown, a polyimide film 11 is arranged in the closed cavity 8 on one side of the sealed heat-insulating rolling shutter door 9, and the polyimide film 11 has a layer, and the edge of the polyimide film is fixedly connected to the inner wall of the closed cavity 8; a layer of polyimide film 11 is also fixedly arranged on the inner wall of the furnace cavity on the inner side of the furnace door of the intermediate frequency furnace 3;
[0060] The long-term use temperature of polyimide can reach 200~380℃. Use polyimide film to seal the two pipe openings of the heated steel pipe (because the steel pipe is first fed into the medium frequency furnace 3, a layer of polyimide film 11 is set on the inner side of the furnace door of the medium frequency furnace, and one pipe opening of the steel pipe is sealed by the polyimide film 11 when the steel pipe is fed into the medium frequency furnace 3; then the other pipe opening is sealed in the process of transferring to the closed cavity 8; after the steel pipe is fed into the medium frequency furnace 3, it can be slightly rotated along the rotation axis of the steel pipe by a certain angle so that the polyimide film 11 is wrapped around the pipe opening of the steel pipe; before each heating of the medium frequency furnace 3 begins, a layer of polyimide film 11 is fixed on the inner wall of the furnace, and a layer of polyimide film 11 is also fixed on the inner wall of the closed cavity 8; in addition, since the medium frequency furnace 3 is connected to the closed cavity 8, Therefore, in the first step of sending the steel pipe into the medium frequency furnace, the steel pipe is first sent into the closed cavity through one end of the closed cavity 8, and then sent into the medium frequency furnace 3, and then the furnace door is closed. Then the worker fixes a layer of polyimide film 11 in the closed cavity 8, and then closes the sealed insulation rolling door 9. The worker walks out of the closed connecting chamber 10 and closes the opening and closing door of the closed connecting chamber; after heating, first open the valves on each connecting pipe 7 to allow the heated air in the furnace body of the medium frequency furnace 3 to flow to the closed cavity 8; then the worker enters the closed connecting chamber 10 and opens the sealed insulation rolling door 9, opens the furnace door and turns the steel pipe to the closed cavity), and then feeds the steel pipe through the feeding pipe passing through the polyimide film, and rotates it immediately after feeding.
[0061] Embodiment 3: The difference from Embodiment 1 is that Figure 6 , Figure 7 As shown, a heat-insulating layer structure adapted to the steel pipe for covering the outer surface of the steel pipe 2 is provided, the heat-insulating layer structure is a heat-insulating sleeve 12 made of a high-temperature resistant silicone airbag, the heat-insulating sleeve 12 is in a circular ring shape for covering the outer surface of the steel pipe 2, and an air-inflating nozzle 13 is provided on the side end surface (i.e., the plane on one side thereof); the outer surface of the heat-insulating sleeve 12 located outside the straight pipe is fixedly connected with a metal ring 14 to facilitate the driving rotation of the roller frame, and the inner surface of the heat-insulating sleeve 12 is fixedly connected with a heat-insulating sleeve ring 15 made of a heat-insulating material (such as rock wool) (in order to avoid the flange at the end of the steel pipe blocking the air-inflating nozzle, the thickness of the heat-insulating sleeve 12 or the thickness of the heat-insulating sleeve ring 15 ensures that the air-inflating nozzle is not blocked by the flange at the end of the steel pipe. The nozzle is located outside the edge of the flange); the insulation collar 15 is adapted to the outer surface of the steel pipe 2 and the insulation collar 15 is split, and the insulation collar 15 is composed of two half rings for easy installation on the outer surface of the steel pipe; a temperature sensor is provided in the medium frequency furnace 3. After the medium frequency furnace is heated, the heat is transferred to the closed cavity 8 through the connecting pipe 7 for a period of time until the temperature in the medium frequency furnace 3 is lower than 200°C. The worker enters the closed connecting chamber 10 and opens the sealed insulation rolling shutter door 9. The furnace door is opened to first cover the uninflated insulation layer structure on the outer surface of the steel pipe 2, and then the insulation sleeve 12 is inflated. After the inflation, wait for a while for the insulation sleeve 12 to expand, and then transfer the steel pipe 2 to the closed cavity 8.
[0062] This method can further improve the steel-lined plastic rotational molding preparation process. There is no need to sandblast the outer surface of the steel pipe before heating the steel pipe; only after removing the insulation layer structure finally, sandblast the entire outer surface of the steel pipe, which further optimizes and streamlines the process flow. Since the insulation sleeve can withstand the temperature in the furnace below 200°C, at this time, the insulation layer structure is sleeved on the outer surface of the steel pipe, and then inflated. After a while, the insulation sleeve expands to enable the insulation layer structure to tightly abut against the outer surface of the steel pipe, realizing the tight installation of the insulation layer and the steel pipe by using the preheating in the furnace, improving the insulation effect during the rotational molding process; it is also possible to better insulate by closing the two ends of the steel pipe with plastic film before adding materials to the inner wall of the steel pipe after transferring it to the closed cavity, ensuring a better rotational molding and lining effect (or referring to the method of Embodiment 2 to close the two ends of the steel pipe after transferring the steel pipe to the closed cavity).
[0063] Embodiment 4: The difference from Embodiment 3 is that, as Figures 8 to 11 shown, a metal ring 14 (the length of the metal ring 14 is the same as the length of the straight steel pipe) is fixedly sleeved and connected to the outer surface of the insulation sleeve 12 located outside the straight pipe to facilitate the driving and rotation of the roller rack. The insulation sleeve 12 is in a circular ring shape for covering the outer surface of the steel pipe 2 (and the flange at the end of the steel pipe 2); a cooling water injection nozzle 16 is provided on the side end surface (that is, one side plane) of the insulation sleeve 12 on the side of the inflation nozzle 13; on the other side end surface of the insulation sleeve 12 (that is, the opposite side end surface of the side end surface where the inflation nozzle 13 is provided), a rubber opening and closing door 17 integrally provided with the insulation sleeve 12 is provided (the rubber opening and closing door can be made of the same material as the insulation sleeve 12, that is, the high-temperature resistant silicone airbag). The rubber opening and closing door 17 can be formed by opening a "凵"-shaped opening on the high-temperature resistant silicone airbag, and a rubber strip is provided at the "凵"-shaped edge of the rubber opening and closing door for sealing the high-temperature resistant silicone airbag.
[0064] After the rotational molding is completed, the worker enters the closed communication room and opens the sealed insulation rolling shutter door, then opens the inflation nozzle 13 to release the insulation air of the insulation sleeve 12, and repeatedly opens and closes the rubber opening and closing door 17 on one side of the insulation sleeve, using the "bellows" principle to quickly dissipate the high-temperature gas in the insulation sleeve 12 and quickly cool it down. Then close the rubber opening and closing door, and then inject cooling water into the insulation sleeve 12 through the cooling water injection nozzle 16 to accelerate the cooling of the rotationally molded steel pipe. After a period of time (the inflation nozzle is blocked for a period of time in order to discharge the heated cooling water from the inflation nozzle, so that the insulation sleeve 12 is always filled with new cooling water with a lower temperature to ensure the cooling effect), the inflation nozzle is blocked. After cooling, the inflation nozzle 13 is opened to squeeze out the water in the insulation sleeve, and the insulation layer structure is taken out from the end of the steel pipe (specifically, the insulation sleeve 12 and the metal ring 14 are first taken out to form an annular whole; then the two semi-annular insulation sleeve rings 15 are removed and taken out), and the insulation layer structure is naturally dried or blown dry by a fan and then used again (of course, since this embodiment is a semi-finished steel lined plastic pipe (that is, one section is a straight pipe and the other section is a curved pipe, or the middle section is a straight pipe and the two ends are curved pipes), the two semi-annular insulation sleeve rings and the semi-finished steel The plastic-lined pipe is shaped like the insulation sleeve and the insulation sleeve consists of six parts, which are three pairs of semi-annular insulation sleeves 15; the end of the insulation sleeve is also shaped like the flange so that the insulation sleeve can cover the steel pipe and the flange to achieve better insulation effect; the outer surface of the insulation sleeve 12 is still fixedly connected with a metal ring 14; and the driven rotation of the roller frame is for the straight pipe section, and the inner surface of the insulation sleeve 12 is still fixedly connected with an insulation sleeve 15 made of insulation material (such as rock wool) to achieve full wrapping insulation of the outer surface of the semi-finished steel plastic-lined pipe).
[0065] As described in the patent with publication number CN214872135U: the existing roto-molding machine mainly cools down the material naturally after molding, and the finished product can only be taken out when the temperature drops to a certain value, which is very inefficient. Although the rotary roto-molding mechanism cools faster than the oven swing roto-molding machine, there is still a technical trend that the cooling efficiency needs to be improved. Therefore, this embodiment solves the problem of the need to improve the cooling efficiency after such a setting, and achieves the effect of rapid cooling, improving cooling efficiency, reducing working hours and improving work efficiency.
[0066] Combined with the method of covering the two ends of the steel pipe with plastic film, the curved steel-lined plastic pipe is connected to the straight steel-lined plastic pipe through the flange at the end of the straight steel-lined plastic pipe, and then the combined semi-finished steel-lined plastic pipe (one section is a straight pipe and the other section is a curved pipe) is roto-molded through a rotating roto-molding mechanism; after this arrangement, the oven swing roto-molding machine can be eliminated; the specific process steps are as follows:
[0067] After the intermediate frequency furnace is heated, the heat is transferred to the closed cavity through the connecting pipe for a period of time until the temperature in the intermediate frequency furnace is lower than 200°C. The worker enters the closed connecting room and opens the sealed insulation shutter door. After opening the furnace door, the uninflated insulation layer structure is first set on the outer surface of the steel pipe 2, and then the insulation sleeve 12 is inflated. After the inflation, wait for a while until the insulation sleeve 12 expands, take out the steel pipe 2 (that is, take it out of the intermediate frequency furnace), and then cover the pipe openings at both ends of the semi-finished steel lined plastic pipe (that is, one section is a straight pipe and the other section is a curved pipe, or the middle section is a straight pipe and the two ends are curved pipes) with plastic film (or refer to the method of Example 2 to achieve the closure of the pipe openings at both ends of the steel pipe after transferring the steel pipe to the closed cavity); then transfer to the closed cavity (that is, in this case, a slightly larger closed cavity is required to allow the rotation space of the end of the semi-finished steel lined plastic pipe, that is, the curved pipe part). This process ensures that the heated steel pipe is cooled more slowly, and has a better insulation effect to ensure a better rotational molding effect.
[0068] Therefore, the rotomolding machine for preparing the steel liner plastic rotomolding corresponding to the preparation process of this embodiment can be realized by only a rotary rotomolding mechanism as structured in the first embodiment.
[0069] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A rotomolding machine for preparing steel liner rotomolding, characterized in that: It is composed of an oven swing rotational molding machine dedicated to rotational molding of plastic-lined elbow steel pipes and a rotary rotational molding mechanism dedicated to rotational molding of plastic-lined straight steel pipes; The rotary rotational molding mechanism includes a closed cavity connected to an intermediate frequency furnace through a connecting pipe. A roller rack is arranged in the closed cavity, and the roller rack is adapted to the steel pipe to be rotationally molded after heating; The intermediate frequency furnace and the closed cavity are arranged in sequence and communicated with each other, and a sealed heat-insulating rolling curtain door is arranged at the communication part; There are multiple connecting pipes, and the connection position of each connecting pipe with the closed cavity is located at different positions in the length direction of the closed cavity to realize introducing the heated air in the intermediate frequency furnace body into the closed cavity from multiple different points; The communication part between the intermediate frequency furnace and the closed cavity is a section of closed communication chamber; A heat-insulating layer structure adapted to the steel pipe for covering the outer surface of the steel pipe is provided. The heat-insulating layer structure is a heat-insulating sleeve made of a high-temperature resistant silica gel airbag; A metal ring with the same length as the straight steel pipe is fixedly sleeved on the outer surface of the heat-insulating sleeve located outside the straight pipe to facilitate the driving rotation of the roller rack. The heat-insulating sleeve is circular to cover the outer surfaces of the steel pipe and the flange at the end of the steel pipe; An air inflation nozzle is arranged on the flat surface of one side of the heat-insulating sleeve, and a cooling water injection nozzle is arranged on the side end surface of the heat-insulating sleeve on one side of the air inflation nozzle; A rubber opening and closing door integrated with the heat-insulating sleeve is arranged on the opposite side end surface of the side end surface of the heat-insulating sleeve where the air inflation nozzle is arranged. The rubber opening and closing door is made of the same material as the heat-insulating sleeve, that is, a high-temperature resistant silica gel airbag. The rubber opening and closing door is formed by opening a "凵"-shaped opening on the high-temperature resistant silica gel airbag, and a rubber strip is arranged on the "凵"-shaped edge of the rubber opening and closing door to seal the high-temperature resistant silica gel airbag; A heat-insulating sleeve ring made of rock wool is fixedly connected to the inner surface of the heat-insulating sleeve; The heat-insulating sleeve ring is composed of two semi-rings to facilitate installation and sleeving on the outer surface of the steel pipe; The two semi-circular heat-insulating sleeve rings are arranged in a shape similar to that of the semi-finished plastic-lined steel pipe, and the heat-insulating sleeve ring is composed of six parts, namely three pairs of semi-circular heat-insulating sleeve rings; The end of the heat-insulating sleeve ring is also shaped similar to the flange so that the heat-insulating sleeve ring can cover the steel pipe and the flange, achieving a better heat-insulating effect; The technological steps to improve the cooling efficiency by adopting the foregoing structure are as follows: After rotational molding is completed, the worker enters the closed communication chamber and opens the sealed heat-insulating rolling curtain door, then opens the air inflation nozzle to release the heat-insulating air in the heat-insulating sleeve. At the same time, repeatedly open and close the rubber opening and closing door on one side of the heat-insulating sleeve, and use the "bellows" principle to quickly disperse the high-temperature gas in the heat-insulating sleeve and rapidly cool down; Then close the rubber opening and closing door, and then inject cooling water into the heat-insulating sleeve through the cooling water injection nozzle to accelerate the cooling of the steel pipe after rotational molding; After a period of time, block the air inflation nozzle to discharge the heated cooling water from the air inflation nozzle, so that the heat-insulating sleeve is always filled with new and cooler cooling water to ensure the cooling effect; After cooling is completed, open the air inflation nozzle again to squeeze out the water in the heat-insulating sleeve, and take out the heat-insulating layer structure from the end of the steel pipe; The technological steps to take out the heat-insulating layer structure are as follows: First, take out a circular integral body composed of the heat-insulating sleeve and the metal ring; Then remove and take out the two semi-circular heat-insulating sleeve rings. The heat-insulating layer structure is used again after being naturally dried or dried by a fan; Plastic film is covered on both ends of the steel pipe, and then the bent steel-lined plastic pipe is connected to the straight steel-lined plastic pipe through the flange at the end of the straight steel-lined plastic pipe, and then the semi-finished steel-lined plastic pipe with one section of straight pipe and one section of bent pipe is roto-molded through a rotary roto-molding mechanism to eliminate the oven swing roto-molding machine; wherein, the driving rotation of the roller frame in the rotary roto-molding mechanism is only for the straight pipe section; the specific process steps are as follows: After the intermediate frequency furnace is heated, the heat is transferred to the closed cavity through the connecting pipe for a period of time until the temperature in the intermediate frequency furnace is lower than 200℃. The worker enters the closed connecting room and opens the sealed insulation shutter door. After opening the furnace door, the uninflated insulation layer structure is first set on the outer surface of the steel pipe, and then the insulation sleeve is inflated. After the inflation, wait for a while until the insulation sleeve expands, take the steel pipe out of the intermediate frequency furnace and cover the plastic film at both ends of the semi-finished steel lined plastic pipe; the semi-finished steel lined plastic pipe is composed of a straight pipe and a curved pipe, or a straight pipe in the middle and curved pipes at both ends; then it is transferred to the closed cavity to achieve a slower cooling of the heated steel pipe, which has a better insulation effect to ensure a better rotational molding effect; The preparation process of the steel-lined plastic pipe produced by rotational molding of this rotational molding machine is as follows: It consists of the following process steps performed in sequence: S1: Welding: Cut the steel pipe according to the size required by the customer, and weld the flange that matches the steel pipe to the end of the steel pipe; S2: Insulation layer structure covering the outer surface of the installed steel pipe; S3: Heating the steel pipe: Put the steel pipe into the medium frequency furnace for uniform heating; S4: Filler: Calculate the required plastic raw materials according to the thickness of the lining and fill the plastic raw materials into the heated steel pipe; S5: Hot rotomolding: The plastic raw material is centrifugally rolled onto the inner wall of the pipe through a rotary rotomolding mechanism; a driving wheel for driving the steel pipe to rotate is provided on the rotary rotomolding mechanism; S6: Cooling and shaping: scrape off the excess material at both ends of the pipe; then cool and shape it to form a plastic-lined pipe; frost and remove rust on the outer surface of the steel pipe and then sandblast it; S7: Rust removal and painting: After the pipeline has cooled, the outer pipe is rust-free and painted with anti-corrosion paint. After drying, it is the finished product. S8: Check the quality of steel-lined plastic pipes: Use the electric spark detection method to check the quality of the pipes; The oven swing type rotational molding machine specially used for rotational molding of curved pipes and steel lined plastic pipes and the rotational molding mechanism specially used for rotational molding of straight pipes and steel lined plastic pipes are the same rotational molding mechanism mentioned above.
2. The rotomolding machine for preparing steel-lined plastic rotomolding according to claim 1, characterized in that: The roller frame includes a pair of roller seats arranged along the length direction of the steel pipe, each roller seat is provided with two pairs of rollers arranged opposite to each other, the two pairs of rollers are located at two corners of the roller seat, and one of the four rollers is connected to the reduction motor to realize driving the steel pipe placed on the roller to rotate when the reduction motor is started.