A kind of synthetic method of N-ethylpiperazine

By using diethanolamine and ethylamine as raw materials and by liquid-phase catalytic synthesis reaction of modified Rainey nickel catalyst, the problems of many by-products and high cost in N-ethylpiperazine production are solved, and yield and selection are improved , promotes the development of downstream industries.

CN118530194BActive Publication Date: 2024-11-12SHANDONG DIAM CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410590188.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-13
Publication Date
2024-11-12
Estimated Expiration
2044-05-13

AI Technical Summary

Technical Problem

The existing N-ethylpiperazine production process has many by-products and high costs, which affects production efficiency and downstream industrial development.

Method used

Use diethanolamine and ethylamine as raw materials to carry out liquid-phase catalytic synthesis reaction through modified Rainey nickel catalyst to avoid the formation of by-product N,N-diethylpiperazine, reduce the content of other by-products, and increase the N-ethylpiperazine. yield and selectivity of the zine.

Benefits of technology

It effectively avoids the generation of by-products, improves the yield and selectivity of N-ethylpiperazine, reduces the cost of raw materials, and promotes the development of downstream industries.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention belongs to the technical field of organic synthesis, and in particular to a method for synthesizing N-ethylpiperazine. The present invention uses ethylamine and diethanolamine as raw materials, and modified Raney nickel as a catalyst to obtain N-ethylpiperazine by liquid phase catalytic synthesis reaction. The method can effectively avoid the generation of by-product N, N-diethylpiperazine during the reaction, and other by-product contents are relatively low, thereby improving the yield and selectivity of N-ethylpiperazine. Meanwhile, the raw material diethanolamine used in the present invention is prepared by reacting ethylene oxide with ammonia, and the raw material cost is low, and the source is extensive, which is conducive to promoting the development of N-ethylpiperazine downstream industries.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of organic synthesis, and specifically relates to a method for synthesizing N-ethylpiperazine. Background Art

[0002] N-ethylpiperazine is mainly used for the synthesis of enrofloxacin, dyes and plant protection agents, etc. It is also widely used in polymer industries such as plastics and rubber. It can also be used as a raw material for the manufacture of drugs to expel roundworms and burnworms. It is also widely used in the production of polymer products such as polyurethane foam plastics, sulfur-containing polyesters, and polyoxytetrafluoroethylene.

[0003] At present, the main raw materials for the actual production of N-ethylpiperazine in industry are piperazine and ethanol, but the activity of ethanol is relatively high. If the single-pass conversion rate of piperazine is higher than 40%, it is easy to produce byproduct N,N-diethylpiperazine, which affects the production efficiency of N-ethylpiperazine. In addition, the high price of piperazine used as a raw material to synthesize ethylpiperazine increases the cost of N-ethylpiperazine, which is not conducive to the development of the downstream industry of N-ethylpiperazine. Summary of the invention

[0004] Aiming at the problems of many by-products and high cost in the production process of N-ethylpiperazine in the prior art, the present invention provides a method for synthesizing N-ethylpiperazine, which uses diethanolamine and ethylamine as raw materials and modified Raney nickel as a catalyst, can effectively avoid the generation of by-product N,N-diethylpiperazine during the reaction process, and the content of other by-products is low, thereby improving the yield and selectivity of N-ethylpiperazine. At the same time, diethanolamine is prepared by the reaction of ethylene oxide and ammonia, the raw material cost is low, and the source is wide, which is conducive to promoting the development of the downstream industry of N-ethylpiperazine.

[0005] In order to achieve the above object, the present invention provides a method for synthesizing N-ethylpiperazine, using ethylamine and diethanolamine as raw materials, modified Raney nickel as a catalyst, and obtaining N-ethylpiperazine through a liquid phase catalytic synthesis reaction;

[0006] The preparation method of the modified Raney nickel is:

[0007] The Raney nickel is immersed in a mixed solution of sodium methoxide, ammonium metavanadate and ethylene glycol for activation. After washing and drying, the activated Raney nickel is placed downstream of the gas flow direction of a tube furnace, and sodium hypophosphite is placed upstream of the gas flow direction of the tube furnace. Then, high-temperature sintering is performed in a nitrogen atmosphere to obtain a modified Raney nickel catalyst.

[0008] Furthermore, the addition ratio of sodium methoxide, ammonium metavanadate and ethylene glycol is 1 mL: 0.1-0.15 g: 3-5 mL.

[0009] Further, the Raney nickel is immersed in a mixed solution of sodium methoxide, ammonium metavanadate and ethylene glycol for activation for 6 to 8 hours.

[0010] Furthermore, the mass ratio of activated Raney nickel to sodium hypophosphite is 1:2-3.

[0011] Furthermore, the high temperature sintering temperature is 500-550°C, the time is 4-6h, and the heating rate is 5°C / min.

[0012] Furthermore, the molar ratio of ethylamine to diethanolamine is 1.1-2.

[0013] Furthermore, the added amount of modified Raney nickel is 10% to 15% of the mass of ethylamine and diethanolamine.

[0014] Furthermore, ethylamine, diethanolamine and modified Raney nickel are added to a high-pressure reactor, and nitrogen is used to replace the oxygen in the high-pressure reactor to ensure that the oxygen content is below 0.01%. The system is then replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%. The pressure of the reactor is then increased to 1-8 MPa with hydrogen to carry out a liquid-phase catalytic synthesis reaction.

[0015] Furthermore, the liquid phase catalytic synthesis reaction temperature is 180°C to 210°C, and the reaction time is 5 to 6 hours.

[0016] Furthermore, the reaction is carried out in a high-pressure reactor with high-speed stirring, and the stirring speed during the reaction is 400-500 r / min.

[0017] The beneficial effects achieved by one or more technical solutions of the present invention are as follows:

[0018] 1. The method for synthesizing N-ethylpiperazine provided by the present invention adopts diethanolamine and ethylamine as raw materials, and further modifies the Raney nickel catalyst, thereby improving the compatibility of the catalyst and the raw material system, and can effectively avoid the formation of the by-product N,N-diethylpiperazine during the reaction process, and the content of other by-products is low, thereby improving the yield and selectivity of N-ethylpiperazine.

[0019] 2. The raw material diethanolamine used in the present invention is prepared by the reaction of ethylene oxide and ammonia, and the raw material cost is low and the source is wide, which is conducive to promoting the development of the downstream industry of N-ethylpiperazine. DETAILED DESCRIPTION

[0020] In order to enable those skilled in the art to more clearly understand the technical solution of the present invention, the technical solution of the present invention will be described in detail below in combination with specific embodiments and comparative examples.

[0021] Example 1

[0022] This embodiment provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are:

[0023] (1) Preparation of modified Raney nickel: Raney nickel was immersed in a mixed solution of 10 mL of sodium methoxide, 1 g of ammonium metavanadate and 30 mL of ethylene glycol for activation for 6 h. After washing and drying, the activated Raney nickel was placed downstream of the gas flow direction of a tube furnace, and sodium hypophosphite was placed upstream of the gas flow direction of the tube furnace (the mass ratio of activated Raney nickel to sodium hypophosphite was 1:2). Then, high-temperature sintering was carried out at 500°C for 6 h in a nitrogen atmosphere with a heating rate of 5°C / min to obtain a modified Raney nickel catalyst.

[0024] (2) Ethylamine, diethanolamine and modified Raney nickel are added to a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine is 1.1, and the amount of modified Raney nickel added is 10% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave is replaced with nitrogen to ensure that the oxygen content is below 0.01%, and then the system is replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%, and then the pressure of the autoclave is increased to 1 MPa with hydrogen, and the stirring speed is set to 500 r / min, and a liquid-phase catalytic synthesis reaction is carried out at a reaction temperature of 180° C. and a reaction time of 6 h.

[0025] Example 2

[0026] This embodiment provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are:

[0027] (1) Preparation of modified Raney nickel: Raney nickel was immersed in a mixed solution of 10 mL of sodium methoxide, 1.5 g of ammonium metavanadate and 30 mL of ethylene glycol for activation for 6 h. After washing and drying, the activated Raney nickel was placed downstream of the gas flow direction of a tube furnace, and sodium hypophosphite was placed upstream of the gas flow direction of the tube furnace (the mass ratio of activated Raney nickel to sodium hypophosphite was 1:2). Then, high-temperature sintering was carried out at 550°C for 4 h in a nitrogen atmosphere with a heating rate of 5°C / min to obtain a modified Raney nickel catalyst.

[0028] (2) Ethylamine, diethanolamine and modified Raney nickel are added to a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine is 1.5, and the amount of modified Raney nickel added is 10% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave is replaced with nitrogen to ensure that the oxygen content is below 0.01%, and then the system is replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%, and then the pressure of the reactor is increased to 4MPa with hydrogen, and the stirring speed is set to 400r / min, and a liquid-phase catalytic synthesis reaction is carried out at a reaction temperature of 210°C and a reaction time of 5h.

[0029] Example 3

[0030] This embodiment provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are:

[0031] (1) Preparation of modified Raney nickel: Raney nickel was immersed in a mixed solution of 10 mL of sodium methoxide, 1.5 g of ammonium metavanadate and 50 mL of ethylene glycol for activation for 8 h. After washing and drying, the activated Raney nickel was placed downstream of the gas flow direction of a tubular furnace, and sodium hypophosphite was placed upstream of the gas flow direction of the tubular furnace (the mass ratio of activated Raney nickel to sodium hypophosphite was 1:3). Then, high-temperature sintering was carried out at 500°C for 5 h in a nitrogen atmosphere with a heating rate of 5°C / min to obtain a modified Raney nickel catalyst.

[0032] (2) Ethylamine, diethanolamine and modified Raney nickel are added to a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine is 2, and the amount of modified Raney nickel added is 15% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave is replaced with nitrogen to ensure that the oxygen content is below 0.01%, and then the system is replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%, and then the pressure of the reactor is increased to 8MPa with hydrogen, and the stirring speed is set to 500r / min, and a liquid-phase catalytic synthesis reaction is carried out at a reaction temperature of 200°C and a reaction time of 5h.

[0033] Example 4

[0034] This embodiment provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are:

[0035] (1) Preparation of modified Raney nickel: Raney nickel was immersed in a mixed solution of 10 mL of sodium methoxide, 1.5 g of ammonium metavanadate and 30 mL of ethylene glycol for activation for 8 h. After washing and drying, the activated Raney nickel was placed downstream of the gas flow direction of a tube furnace, and sodium hypophosphite was placed upstream of the gas flow direction of the tube furnace (the mass ratio of activated Raney nickel to sodium hypophosphite was 1:2.5). Then, high-temperature sintering was carried out at 550°C for 6 h in a nitrogen atmosphere at a heating rate of 5°C / min to obtain a modified Raney nickel catalyst.

[0036] (2) Ethylamine, diethanolamine and modified Raney nickel are added to a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine is 1.8, and the amount of modified Raney nickel added is 12% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave is replaced with nitrogen to ensure that the oxygen content is below 0.01%, and then the system is replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%, and then the pressure of the reactor is increased to 6MPa with hydrogen, and the stirring speed is set to 500r / min, and a liquid-phase catalytic synthesis reaction is carried out at a reaction temperature of 210°C and a reaction time of 5h.

[0037] Example 5

[0038] This embodiment provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are:

[0039] (1) Preparation of modified Raney nickel: Raney nickel was immersed in a mixed solution of 10 mL of sodium methoxide, 1 g of ammonium metavanadate and 30 mL of ethylene glycol for activation for 6 h. After washing and drying, the activated Raney nickel was placed downstream of the gas flow direction of a tubular furnace, and sodium hypophosphite was placed upstream of the gas flow direction of the tubular furnace (the mass ratio of activated Raney nickel to sodium hypophosphite was 1:2). Then, the catalyst was sintered at 550 °C for 4 h in a nitrogen atmosphere at a heating rate of 5 °C / min to obtain a modified Raney nickel catalyst.

[0040] (2) Ethylamine, diethanolamine and modified Raney nickel are added to a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine is 1.5, and the amount of modified Raney nickel added is 15% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave is replaced with nitrogen to ensure that the oxygen content is below 0.01%, and then the system is replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%, and then the pressure of the reactor is increased to 5MPa with hydrogen, and the stirring speed is set to 500r / min, and a liquid-phase catalytic synthesis reaction is carried out at a reaction temperature of 180°C and a reaction time of 6h.

[0041] Comparative Example 1

[0042] This comparative example provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are as follows:

[0043] Ethylamine, diethanolamine and Raney nickel were added into a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine was 1.1, and the amount of Raney nickel added was 10% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave was replaced with nitrogen to ensure that the oxygen content was below 0.01%, and then the system was replaced with hydrogen to ensure that the hydrogen content in the system was above 99.5%, and then the pressure of the reactor was increased to 1MPa with hydrogen, and the stirring speed was set to 500r / min, and a liquid-phase catalytic synthesis reaction was carried out at a reaction temperature of 180°C and a reaction time of 6h.

[0044] Comparative Example 2

[0045] This comparative example provides a method for synthesizing N-ethylpiperazine, and the specific preparation steps are as follows:

[0046] (1) Preparation of modified Raney nickel: Raney nickel is placed downstream of the gas flow direction of a tubular furnace, and sodium hypophosphite is placed upstream of the gas flow direction of the tubular furnace (the mass ratio of Raney nickel to sodium hypophosphite is 1:2). Then, high-temperature sintering is performed at 500°C for 6 hours in a nitrogen atmosphere with a heating rate of 5°C / min to obtain a modified Raney nickel catalyst.

[0047] (2) Ethylamine, diethanolamine and modified Raney nickel are added to a high-speed stirring autoclave (the molar ratio of ethylamine to diethanolamine is 1.1, and the amount of modified Raney nickel added is 10% of the mass of ethylamine and diethanolamine), and the oxygen in the autoclave is replaced with nitrogen to ensure that the oxygen content is below 0.01%, and then the system is replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%, and then the pressure of the autoclave is increased to 1 MPa with hydrogen, and the stirring speed is set to 500 r / min, and a liquid-phase catalytic synthesis reaction is carried out at a reaction temperature of 180° C. and a reaction time of 6 h.

[0048] Chromatographic analysis was performed on the materials after the reaction in Examples 1 to 5 and Comparative Examples 1 and 2. Table 1 shows the contents of diethylamine, piperazine, N-ethylpiperazine, ethylamine and diethanolamine in the materials after the reaction (except water). The remaining components are other impurities, and the other impurities do not exceed 0.1%.

[0049] Table 1

[0050] sample Ethylamine(%) Diethylamine(%) Piperazine(%) N-Ethylpiperazine(%) Diethanolamine(%) Example 1 1.25 2.77 2.37 90.52 3.07 Example 2 1.17 2.48 2.15 91.47 2.68 Example 3 1.69 3.05 2.41 89.61 3.16 Example 4 1.26 2.55 2.19 90.94 3.02 Example 5 1.18 2.50 2.25 91.23 2.77 Comparative Example 1 4.74 5.51 4.83 78.91 5.95 Comparative Example 2 2.66 4.19 3.12 85.63 4.31

[0051] As shown in Table 1, the synthetic method of N-ethylpiperazine provided by the present invention has a high yield of N-ethylpiperazine, excellent selectivity, and a low proportion of by-products. The excellent effect achieved by the present invention is derived from the selection of reactants on the one hand, using diethanolamine and ethylamine as raw materials, which can avoid the generation of by-product N, N-diethylpiperazine; on the other hand, it is attributed to the modification of Raney nickel catalyst, by first synergistically activating Raney nickel in sodium methoxide, ammonium metavanadate, and ethylene glycol solution, and then performing a high-temperature phosphating process, which can significantly enhance the catalytic activity, reduce the content of other by-products, and improve the selectivity of N-ethylpiperazine.

Claims

1. A method for synthesizing N-ethylpiperazine, Features: Using ethylamine and diethanolamine as raw materials and modified Raney nickel as catalyst, N-ethylpiperazine is obtained through liquid phase catalytic synthesis reaction. The preparation method of the modified Raney nickel is: The Raney nickel is immersed in a mixed solution of sodium methoxide, ammonium metavanadate and ethylene glycol for activation. After washing and drying, the activated Raney nickel is placed downstream of the gas flow direction of a tube furnace, and sodium hypophosphite is placed upstream of the gas flow direction of the tube furnace. Then, high-temperature sintering is performed in a nitrogen atmosphere to obtain a modified Raney nickel catalyst.

2. The synthetic method of N-ethylpiperazine as claimed in claim 1, Features: The addition ratio of sodium methoxide, ammonium metavanadate and ethylene glycol is 1 mL: 0.1-0.15 g: 3-5 mL.

3. The synthetic method of N-ethylpiperazine as claimed in claim 1, Features: Raney nickel is activated by immersing in a mixed solution of sodium methoxide, ammonium metavanadate and ethylene glycol for 6 to 8 hours.

4. The synthetic method of N-ethylpiperazine as claimed in claim 1, Features: The mass ratio of activated Raney nickel to sodium hypophosphite is 1:2-3.

5. The method for synthesizing N-ethylpiperazine according to claim 1, Features: The high temperature sintering temperature is 500-550°C, the time is 4-6h, and the heating rate is 5°C / min.

6. The method for synthesizing N-ethylpiperazine according to claim 1, Features: The molar ratio of ethylamine to diethanolamine is 1.1-2.

7. The method for synthesizing N-ethylpiperazine according to claim 1, Features: The added amount of the modified Raney nickel is 10% to 15% of the mass of ethylamine and diethanolamine.

8. The method for synthesizing N-ethylpiperazine according to claim 1, Features: Ethylamine, diethanolamine and modified Raney nickel are added into a high-pressure reactor, and nitrogen is used to replace the oxygen in the high-pressure reactor to ensure that the oxygen content is below 0.01%. The system is then replaced with hydrogen to ensure that the hydrogen content in the system is above 99.5%. The pressure of the reactor is then increased to 1-8 MPa with hydrogen to carry out a liquid-phase catalytic synthesis reaction.

9. The method for synthesizing N-ethylpiperazine according to claim 8, Features: The reaction temperature of liquid phase catalytic synthesis is 180°C to 210°C, and the reaction time is 5 to 6 hours.

10. The method for synthesizing N-ethylpiperazine according to claim 8, Features: The reaction is carried out in a high-pressure reactor with high-speed stirring, and the stirring speed during the reaction is 400-500 r / min.