IGBT front side temperature acquisition method and IGBT back side annealing method
By depositing a titanium film on the front of the IGBT wafer and performing laser annealing on the back, the sheet resistance of the titanium film is obtained to monitor the temperature. This solves the problem of difficulty in repairing lattice damage and activating impurity atoms with the whole-wafer annealing method, and ensures the safety of the IGBT back annealing process. sex and effectiveness.
Patent Information
- Application Number
- CN202411009022.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-07-26
AI Technical Summary
In the IGBT backside process, the whole-chip annealing method is difficult to repair the lattice damage and activate impurity atoms without damaging the frontside graphics, and it is impossible to monitor the temperature of the IGBT frontside during laser annealing in real time, which may damage the frontside graphics.
By depositing a titanium film on the front side of the IGBT wafer, grinding and etching the back side and then performing laser annealing, the square resistance of the titanium film after laser annealing is obtained to deduce the front side temperature and determine whether the energy intensity during laser annealing will damage the front side. graph, and then determine the annealing standard energy.
It is possible to monitor the IGBT front temperature under different energy intensities, avoid laser annealing damage to the front pattern, and at the same time realize lattice damage repair and impurity atom activation to ensure the safety and effectiveness of the annealing process.
Smart Images

Figure CN118538629B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of chips, and in particular to an IGBT front temperature acquisition method and an IGBT back annealing method. Background Art
[0002] In the back process of the Insulated Gate Bipolar Transistor (IGBT), ion implantation is required to implant a specific amount of ions into a specific location. During the implantation process, a large number of high-energy ions will collide with silicon atoms in the lattice, resulting in a large number of lattice defects in the implanted layer, and because a large number of impurity atoms are located in the lattice gaps, they cannot conduct electricity directly. Annealing is required to repair the lattice damage on the back of the IGBT and activate the impurity atoms.
[0003] At the same time, when the IGBT back is processed, the process of the IGBT front has been completed. The metal in the front pattern may melt under high temperature environment. For example, the melting point of the metal aluminum in the front pattern is about 660℃. If the whole IGBT is annealed, the annealing temperature needs to be limited (for example, below 660℃). However, the annealing temperature after the limit cannot reach the minimum temperature of 750℃ for activating ions. It is difficult to achieve the purpose of repairing the lattice damage on the back of the IGBT and activating the impurity atoms without damaging the front pattern.
[0004] In order to overcome the problems caused by the whole-wafer IGBT annealing method, laser annealing can be used. The irradiation surface (back side) temperature of laser annealing is as high as about 1400°C, which can achieve lattice damage and impurity atom activation, and the temperature gradually decreases with the increase of wafer thickness, thereby reducing the impact on the front side pattern. However, during laser annealing, the actual temperature of the front side of the IGBT cannot be known, and it is unclear whether it will damage the front side pattern. Therefore, it is important to monitor the front side temperature of the IGBT during laser annealing. Summary of the invention
[0005] The object of the present invention is to provide an IGBT front side temperature acquisition method and an IGBT back side annealing method, so as to at least partially improve the above-mentioned problems.
[0006] In order to achieve the above purpose, the technical solution adopted by the embodiment of the present invention is as follows:
[0007] In a first aspect, an embodiment of the present invention provides a method for obtaining the front temperature of an IGBT, the method comprising:
[0008] depositing a titanium film on the front side of the target wafer;
[0009] Perform back grinding and etching on the target wafer after deposition;
[0010] Performing backside laser annealing on the target wafer according to target energy;
[0011] Obtaining the sheet resistance of the titanium film on the front side of the target wafer after laser annealing;
[0012] The front titanium film temperature of the target wafer during laser annealing is obtained based on the titanium film square resistance.
[0013] In a second aspect, an embodiment of the present invention provides an IGBT back annealing method, the method comprising:
[0014] Determine the laser annealing standard energy according to the above-mentioned IGBT front side temperature acquisition method;
[0015] The back side laser annealing is performed on the standard product wafer according to the laser annealing standard energy.
[0016] Compared with the prior art, the embodiment of the present invention provides an IGBT front temperature acquisition method and an IGBT back annealing method, including: depositing a titanium film on the front of a target wafer; performing back grinding and etching on the target wafer after deposition; performing back laser annealing on the target wafer according to the target energy; obtaining the titanium film block resistance on the front of the target wafer after laser annealing; and obtaining the titanium film temperature on the front of the target wafer during laser annealing based on the titanium film block resistance. The relationship between laser annealing and the titanium film temperature on the front of the target wafer is derived using the titanium film block resistance as an intermediary. The temperature of the front of the wafer when the back of the wafer is laser annealed at different energy intensities can be known, thereby determining whether the front pattern will be damaged at the energy intensity.
[0017] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0019] Figure 1 This is a flow chart of a method for obtaining the front temperature of an IGBT provided in an embodiment of the present invention.
[0020] Figure 2 A schematic diagram of a resistance-temperature fitting line provided in an embodiment of the present invention.
[0021] Figure 3The second flowchart of the method for obtaining the front temperature of an IGBT provided in an embodiment of the present invention.
[0022] Figure 4 The third flowchart of the method for obtaining the front temperature of an IGBT provided in an embodiment of the present invention.
[0023] Figure 5 The fourth flowchart of the method for obtaining the front temperature of an IGBT provided in an embodiment of the present invention.
[0024] Figure 6 The fifth flowchart of the method for obtaining the front temperature of an IGBT provided in an embodiment of the present invention.
[0025] Figure 7 A schematic flow chart of an IGBT back side annealing method provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0026] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0027] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in the subsequent drawings. At the same time, in the description of the present invention, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.
[0029] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0030] In the description of the present invention, it should be noted that the terms "upper", "lower", "inside", "outside", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are directions or positional relationships in which the product of the invention is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.
[0031] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "disposed" and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0032] Some embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.
[0033] By laser annealing the back of the IGBT, lattice damage and impurity atom activation can be achieved, and the temperature gradually decreases as the wafer thickness increases, thereby reducing the impact on the front pattern. However, when performing laser annealing, the actual temperature of the front of the IGBT cannot be known, and it is unclear whether it will damage the front pattern. In order to avoid laser annealing damaging the front pattern, an embodiment of the present invention provides an IGBT front temperature acquisition method, which can know the temperature of the front of the wafer when the back of the wafer is laser annealed at different energy intensities, thereby determining whether the front pattern will be damaged at this energy intensity.
[0034] Please refer to Figure 1 , Figure 1This is a flow chart of a method for obtaining the front temperature of an IGBT provided by an embodiment of the present invention. The method for obtaining the front temperature of an IGBT comprises: S101, S102, S103, S104 and S105, which are described in detail as follows.
[0035] S101, depositing a titanium film on the front side of the target wafer.
[0036] Optionally, a titanium film (also called a Ti film) is deposited on the front side of the target wafer at room temperature by magnetron sputtering. The thickness of the titanium film on the target wafer is the same as the thickness of the titanium film on the standard product wafer, which can be but is not limited to 100 nm.
[0037] S102, performing back grinding and etching on the target wafer after the deposition is completed.
[0038] The back side of the target wafer after deposition is ground and etched. Optionally, the thickness of the target wafer after grinding and etching is the same as the thickness of the standard product wafer. After grinding and etching, the thickness of the target wafer can be but is not limited to 130 μm.
[0039] After S102, the room temperature titanium film sheet resistance on the front side of the target wafer may also be obtained by, but is not limited to, a four-probe test method.
[0040] S103, performing back laser annealing on the target wafer according to the target energy.
[0041] The target energy may be, but is not limited to, 4.4 J.
[0042] S104, obtaining the sheet resistance of the titanium film on the front side of the target wafer after laser annealing.
[0043] Optionally, the titanium film on the front side of the target wafer is tested by a four-probe method to obtain the sheet resistance of the titanium film on the front side of the target wafer.
[0044] S105, obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance.
[0045] In the IGBT front temperature acquisition method provided by the embodiment of the present invention, the relationship between laser annealing and the front titanium film temperature of the target wafer is derived with the titanium film block resistance as the medium. The temperature of the front side of the wafer when the back side of the wafer is laser annealed at different energy intensities can be obtained, thereby determining whether the front pattern will be damaged at the energy intensity.
[0046] exist Figure 1 Based on the content in S105, the embodiment of the present invention also provides an optional implementation method, please refer to the following. S105, the step of obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film square resistance, includes: S105-1, which is specifically described as follows.
[0047] S105-1, calculating based on the titanium film block resistance and the resistance temperature fitting line to obtain the front titanium film temperature of the target wafer during laser annealing.
[0048] Among them, the resistance-temperature fitting line represents the mapping relationship between the titanium film block resistance and the front titanium film temperature.
[0049] Please refer to Figure 2 , Figure 2 Schematic diagram of the resistance temperature fitting line provided by an embodiment of the present invention. RS in the figure represents the square resistance of the titanium film. Figure 2 The figure shows that the sheet resistance of the titanium film at 25°C, 150°C, 250°C, 300°C and 350°C is 6.502, 6.114, 5.568, 5.481 and 5.424 respectively. Based on the above array, a resistance temperature fitting line can be constructed. It should be noted that the resistance temperature fitting line can also be other array relationships, not limited to Figure 2 The values shown.
[0050] Similarly, the four-probe test shows that the square resistance of the titanium film on the front side of the target wafer after 4.4J laser annealing is 6.062Ω / □, where □ represents square and Ω / □ is equivalent to Ω / sq. Figure 2 The annealing temperature was found to be between 150 and 250°C.
[0051] Based on the above, regarding how to obtain the resistance temperature fitting line, the embodiment of the present invention also provides an optional implementation method, please refer to Figure 3 The IGBT front temperature acquisition method further includes: S201, S203, S204, S205 and S206, which are described in detail as follows.
[0052] S201, grinding and etching N sample wafers.
[0053] Wherein, N is an integer greater than or equal to 1. It should be noted that, in order to ensure the accuracy of the resistance-temperature fitting line, as many titanium film block resistances at different annealing temperatures as possible can be collected, for example, N is greater than or equal to 5.
[0054] In order to ensure the consistency of heat transfer effect, the thickness of the sample wafer after grinding and etching and the thickness of the target wafer after grinding and etching can be made the same as the thickness of the standard product wafer, and the thickness can be but is not limited to 130 μm.
[0055] S203, depositing a titanium film on the front side of the sample wafer.
[0056] Optionally, magnetron sputtering is used to deposit titanium films on the front sides of the N sample wafers. The thickness of the titanium films on the sample wafers is the same as the thickness of the titanium films on the standard product wafers, which may be but is not limited to 100 nm.
[0057] S204, annealing the i-th sample wafer at the i-th temperature, 1≤i≤N.
[0058] In an optional implementation, as the value of i increases, the i-th temperature gradually increases, and the difference between two adjacent temperatures is a fixed difference (which may be but is not limited to 5° C.).
[0059] In an optional manner, the N temperatures may not be distributed equidistantly, for example Figure 2 As shown, the five temperatures are 25°C, 150°C, 250°C, 300°C and 350°C.
[0060] Optionally, the step of annealing the i-th sample wafer at the i-th temperature includes: annealing the i-th sample wafer at the i-th temperature by using an annealing furnace.
[0061] S205, after the annealing is completed, the titanium film sheet resistance on the front side of the i-th sample wafer is obtained.
[0062] Optionally, the step of obtaining the titanium film sheet resistance on the front side of the i-th sample wafer includes: testing the titanium film on the front side of the i-th sample wafer by a four-probe method to obtain the titanium film sheet resistance on the front side of the i-th sample wafer.
[0063] Sheet resistance of titanium film at different annealing temperatures Figure 2 As shown, it can be seen from the figure that as the annealing temperature increases, the square resistance of the titanium film gradually decreases.
[0064] S206, constructing a resistance-temperature fitting line based on the titanium film sheet resistance on the front side of each sample wafer and the corresponding annealing temperature.
[0065] In order to eliminate interference and ensure the accuracy of the resistance temperature fitting line, the embodiment of the present invention also provides an optional implementation method, please refer to Figure 4 , in S203, before depositing a titanium film on the front side of the sample wafer, the IGBT front side temperature acquisition method further includes: S202, which is described in detail as follows.
[0066] S202, using hydrofluoric acid to clean the oxide layer on the polished surface of the sample wafer.
[0067] By cleaning the oxide layer, the interference of impurities is further eliminated to ensure the accuracy of the resistance temperature fitting line. The oxide layer can be but is not limited to silicon oxide.
[0068] In order to achieve both the effects of lattice damage repair and impurity atom activation while avoiding laser annealing damage to the front pattern, the embodiment of the present invention also provides an optional implementation method, please refer to Figure 5 When the initial value of the target energy is the minimum energy of the laser annealing equipment, after obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance, the IGBT front temperature acquisition method further includes: S106, S107, S108 and S109, which are specifically described as follows.
[0069] S106, determining whether the temperature of the front titanium film is less than a temperature threshold. If so, executing S107; if not, executing S109.
[0070] If the front titanium film temperature is less than the temperature threshold, it means that the front pattern will not be damaged at this energy, and the energy corresponding to the front titanium film temperature is added to the effective energy record. The corresponding energy boundary has not been explored, so S108 needs to be executed after S107.
[0071] S107, adding the energy corresponding to the temperature of the front titanium film to the effective energy record.
[0072] S108, increasing the target energy by a preset amplitude and determining a new target wafer.
[0073] After S108, repeat Figure 1 The steps in are repeated, a titanium film is deposited on the front side of the target wafer, the back side of the target wafer is ground and etched after the deposition, the back side of the target wafer is laser annealed according to the target energy, the titanium film block resistance on the front side of the target wafer after the laser annealing is obtained, and the titanium film temperature on the front side of the target wafer during the laser annealing is obtained based on the titanium film block resistance, until the front side titanium film temperature is greater than or equal to the temperature threshold.
[0074] When the temperature of the front titanium film is greater than or equal to the temperature threshold, it means that the front pattern will be damaged at this energy and the corresponding energy boundary has been explored.
[0075] S109, screening out laser annealing standard energy from the effective energy records.
[0076] It should be understood that there may be a variety of energy intensities for effective energy records, from which one (which may be but is not limited to the best) that can meet the standards for lattice damage repair and impurity atom activation is selected as the laser annealing standard energy.
[0077] In order to achieve both the effects of lattice damage repair and impurity atom activation while avoiding laser annealing damage to the front pattern, the embodiment of the present invention also provides an optional implementation method, please refer to Figure 6When the initial value of the target energy is the maximum energy of the laser annealing equipment, after obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance, the IGBT front temperature acquisition method further includes: S106, S110 and S111, which are specifically described as follows.
[0078] S106, determining whether the temperature of the front titanium film is less than a temperature threshold. If not, executing S110; if yes, executing S111.
[0079] S110, reducing the target energy by a preset amplitude and determining a new target wafer.
[0080] After S110, repeat Figure 1 The steps in are repeated, a titanium film is deposited on the front side of the target wafer, the back side of the target wafer is ground and etched after the deposition, the back side of the target wafer is laser annealed according to the target energy, the titanium film block resistance on the front side of the target wafer after the laser annealing is obtained, and the titanium film temperature on the front side of the target wafer during the laser annealing is obtained based on the titanium film block resistance, until the titanium film temperature on the front side is less than the temperature threshold.
[0081] S111, taking the energy corresponding to the temperature of the front titanium film as the laser annealing standard energy.
[0082] The embodiment of the present invention also provides an IGBT back annealing method, please refer to Figure 7 The IGBT back side annealing method includes: S301 and S302, which are described in detail as follows.
[0083] S301, determining laser annealing standard energy according to an IGBT front side temperature acquisition method.
[0084] S302, performing back laser annealing on the standard product wafer according to the laser annealing standard energy.
[0085] In summary, an IGBT front temperature acquisition method and an IGBT back annealing method provided by an embodiment of the present invention include: depositing a titanium film on the front of a target wafer; performing back grinding and etching on the target wafer after deposition; performing back laser annealing on the target wafer according to the target energy; obtaining the titanium film block resistance on the front of the target wafer after laser annealing; and obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance. The relationship between laser annealing and the front titanium film temperature of the target wafer is derived using the titanium film block resistance as an intermediary. The temperature of the front of the wafer when the back laser annealing is performed on the wafer at different energy intensities can be known, thereby determining whether the front pattern will be damaged at the energy intensity.
[0086] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
[0087] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.
Claims
1. A method for obtaining the front temperature of an IGBT, characterized in that: The method comprises: depositing a titanium film on the front side of the target wafer; Perform back grinding and etching on the target wafer after deposition; Performing backside laser annealing on the target wafer according to target energy; Obtaining the sheet resistance of the titanium film on the front side of the target wafer after laser annealing; Acquiring the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance; The initial value of the target energy is the lowest energy of the laser annealing equipment. After obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance, the method further includes: determining whether the front titanium film temperature is less than a temperature threshold; if the front titanium film temperature is less than the temperature threshold, adding the energy corresponding to the front titanium film temperature to the effective energy record; increasing the target energy by a preset amplitude, and determining a new target wafer; repeatedly depositing a titanium film on the front side of the target wafer, back grinding and etching the target wafer after deposition, performing back laser annealing on the target wafer according to the target energy, obtaining the titanium film block resistance on the front side of the target wafer after laser annealing, and obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance, until the front titanium film temperature is greater than or equal to the temperature threshold; filtering out the laser annealing standard energy from the effective energy record; Alternatively, the initial value of the target energy is the maximum energy of the laser annealing equipment. After obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance, the method further includes: determining whether the front titanium film temperature is less than a temperature threshold; if the front titanium film temperature is less than the temperature threshold, using the energy corresponding to the front titanium film temperature as the laser annealing standard energy; if the front titanium film temperature is greater than the temperature threshold, reducing the target energy by a preset amplitude and determining a new target wafer; repeatedly depositing a titanium film on the front side of the target wafer, back grinding and etching the target wafer after deposition, performing back laser annealing on the target wafer according to the target energy, obtaining the titanium film block resistance on the front side of the target wafer after laser annealing, and obtaining the front titanium film temperature of the target wafer during laser annealing based on the titanium film block resistance until the front titanium film temperature is less than the temperature threshold; The laser annealing standard energy is used as a standard for back-side laser annealing of standard product wafers.
2. The IGBT front temperature acquisition method according to claim 1, characterized in that: The step of obtaining the temperature of the front titanium film of the target wafer during laser annealing based on the titanium film square resistance includes: Calculating based on the titanium film block resistance and the resistance temperature fitting line to obtain the front titanium film temperature of the target wafer during laser annealing; Among them, the resistance-temperature fitting line represents the mapping relationship between the titanium film block resistance and the front titanium film temperature.
3. The IGBT front surface temperature acquisition method according to claim 2, characterized in that: The IGBT front temperature acquisition method also includes: Grinding and etching N sample wafers; depositing a titanium film on the front side of the sample wafer; Annealing the i-th sample wafer at the i-th temperature, 1≤i≤N; After the annealing is completed, obtaining the sheet resistance of the titanium film on the front side of the i-th sample wafer; The resistance-temperature fitting line is constructed based on the square resistance of the titanium film on the front side of each sample wafer and the corresponding annealing temperature.
4. The IGBT front temperature acquisition method according to claim 3, characterized in that: The step of obtaining the titanium film sheet resistance on the front side of the i-th sample wafer comprises: The titanium film on the front side of the i-th sample wafer is tested by a four-probe method to obtain the square resistance of the titanium film on the front side of the i-th sample wafer.
5. The IGBT front surface temperature acquisition method according to claim 3, characterized in that: The thickness of the sample wafer after grinding and etching, the thickness of the target wafer after grinding and etching are the same as the thickness of the standard product wafer.
6. The IGBT front surface temperature acquisition method according to claim 3, characterized in that: Before depositing the titanium film on the front side of the sample wafer, the method further comprises: The oxide layer on the polished surface of the sample wafer is cleaned with hydrofluoric acid.
7. The IGBT front surface temperature acquisition method according to claim 3, characterized in that: The step of annealing the i-th sample wafer at the i-th temperature comprises: The i-th sample wafer is annealed at the i-th temperature in an annealing furnace.
8. An IGBT back annealing method, characterized in that: The method comprises: Determine the laser annealing standard energy according to the IGBT front side temperature acquisition method of claim 1; The back side laser annealing is performed on the standard product wafer according to the laser annealing standard energy.