Semiconductor structure preparation method and semiconductor structure
By forming a tensile stress layer in the dielectric layer, the adhesion between the contact plug and the dielectric layer is enhanced, solving the problem of CMP polishing slurry corroding the bottom metal layer and improving device yield.
Patent Information
- Application Number
- CN202411088125.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-08-09
AI Technical Summary
In the prior art, the poor adhesion between the contact plug and the dielectric layer causes the CMP polishing slurry to corrode the bottom metal layer, affecting the device yield.
A curable second dielectric layer is formed in the dielectric layer and transformed into a tensile stress layer by ultraviolet or heat treatment. The first dielectric layer is squeezed closer to the contact plug to enhance adhesion. The tensile stress layer is removed before chemical mechanical polishing to reduce the gap.
It effectively prevents CMP polishing fluid from corroding the bottom metal layer, improves device yield, enhances the adhesion between the contact plug and the dielectric layer, and reduces physical gaps.
Smart Images

Figure CN118610163B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor structure and a preparation method thereof. Background Art
[0002] The middle end of line (MEOL) is an important link in the semiconductor manufacturing process. It is located between the front end of line (FEOL) and the back end of line (BEOL) and is used to electrically connect the device layer of the FEOL to the metal interconnection layer of the BEOL.
[0003] In order to lead out the electrodes of the device layer and connect them to the upper metal interconnection layer, it is necessary to form contact holes in the interlayer dielectric layer (ILD) between the device layer and the metal interconnection layer, and fill the contact holes with conductive material to form contact plugs that electrically connect the device layer and the metal interconnection layer.
[0004] In the prior art, the adhesion between the contact plug and the dielectric layers on both sides is relatively poor, resulting in a certain gap between the plug metal and the dielectric layer. In the subsequent planarization process, the polishing liquid of the Chemical Mechanical Planarization (CMP) will pass through the gap into the substrate and corrode the metal layer of the bottom device, thereby affecting the device yield. Summary of the invention
[0005] In view of the above shortcomings of the prior art, the present invention provides a method for preparing a semiconductor structure and a semiconductor structure to improve the problem that CMP polishing liquid slides into the gap between the contact plug and the dielectric layer and corrodes the bottom metal layer.
[0006] To achieve the above object and other related objects, the present invention provides a method for preparing a semiconductor structure, comprising the following steps:
[0007] Providing a substrate, on which a metal layer and a first dielectric layer located on the metal layer are formed;
[0008] forming a second dielectric layer on the first dielectric layer;
[0009] forming contact holes in the first dielectric layer and the second dielectric layer, wherein the metal layer is exposed at the bottom of the contact holes;
[0010] Filling the contact hole with a conductive material to form an initial plug;
[0011] curing the second dielectric layer to form a tensile stress layer, wherein the tensile stress layer squeezes the first dielectric layer toward the initial plug;
[0012] The tensile stress layer and part of the conductive material are removed by chemical mechanical polishing to form a contact plug.
[0013] In an example of the present invention, the second dielectric layer is selected from silicon dioxide and / or a derivative of silicon dioxide, and the derivative of silicon dioxide is selected from one or more of silicon oxycarbide, silicon oxynitride, and silicon oxycarbonitride.
[0014] In an example of the present invention, the thickness of the second dielectric layer is 100 angstroms to 500 angstroms.
[0015] In one example of the present invention, the second dielectric layer is cured to form a tensile stress layer by an ultraviolet curing process, and the ultraviolet curing process includes: treating under ultraviolet light with a wavelength of 200 nm to 450 nm for 1 min to 5 min.
[0016] In an example of the present invention, the curing treatment of the second dielectric layer to form the tensile stress layer adopts a heat treatment process, and the heat treatment process includes: annealing treatment at a temperature of 500° C. to 1050° C. for 10 min to 30 min.
[0017] In an example of the present invention, before removing the tensile stress layer, a portion of the first dielectric layer and a portion of the conductive material by a chemical mechanical polishing process, the method further includes:
[0018] forming a barrier layer on the tensile stress layer;
[0019] A conductive film layer is formed on the barrier layer.
[0020] In an example of the present invention, the conductive material is selected from one or more combinations of tungsten, cobalt, copper, molybdenum, ruthenium, and titanium.
[0021] In an example of the present invention, an etching stop layer is further formed on the substrate, and the etching stop layer is formed between the substrate and the first dielectric layer.
[0022] In an example of the present invention, forming contact holes in the first dielectric layer and the second dielectric layer includes:
[0023] forming a patterned mask layer on the second dielectric layer;
[0024] Using the patterned mask layer as a mask, the second dielectric layer and the first dielectric layer are etched sequentially from top to bottom until the metal layer on the substrate is exposed.
[0025] Another aspect of the present invention provides a semiconductor structure, which is prepared by any of the above-mentioned preparation methods.
[0026] The semiconductor structure includes a substrate and a contact plug, wherein a metal layer and a first dielectric layer located on the metal layer are formed on the substrate, and the contact plug includes a contact hole and a conductive material, wherein the contact hole is arranged in the first dielectric layer and the contact hole exposes the metal layer; and the conductive material is filled in the contact hole and is connected to the metal layer.
[0027] The method for preparing a semiconductor structure of the present invention forms a processable second dielectric layer on a first dielectric layer, and the second dielectric layer can be transformed into a tensile stress layer through a curing process, which helps to achieve better adhesion between the conductive material of the contact plug and the first dielectric layer and minimizes the physical gap between the conductive material and the first dielectric layer; it can effectively prevent or minimize the possibility that the CMP polishing liquid slides down from the gap between the conductive material of the contact plug and the first dielectric layer and attacks the bottom metal, thereby improving the yield of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0029] Figure 1 A schematic diagram of CMP processing of contact plugs in the prior art;
[0030] Figure 2 A flow chart of a method for preparing a semiconductor structure according to an embodiment of the present invention;
[0031] Figure 3 A schematic diagram of the structure of a substrate in an embodiment of a method for preparing a semiconductor structure of the present invention;
[0032] Figure 4 A schematic diagram of a structure of forming a second dielectric layer in an embodiment of a method for preparing a semiconductor structure of the present invention;
[0033] Figure 5 A schematic diagram of a structure for forming a contact hole in an embodiment of a method for preparing a semiconductor structure of the present invention;
[0034] Figure 6 A schematic diagram of a method for preparing a semiconductor structure of the present invention in one embodiment of filling a contact hole with a conductive material;
[0035] Figure 7 A schematic structural diagram of a method for preparing a semiconductor structure of the present invention in one embodiment of curing a second dielectric layer to form a tensile stress layer;
[0036] Figure 8 A schematic structural diagram of forming a barrier layer and a conductive film layer on a tensile stress layer in an embodiment of a method for preparing a semiconductor structure of the present invention;
[0037] Fig. 9 FIG. 4 is a schematic structural diagram of a semiconductor structure of the present invention in one embodiment.
[0038] Component number description
[0039] 100, substrate; 110, etch stop layer; 120, first dielectric layer; 130, second dielectric layer; 131, tensile stress layer; 140, initial plug; 141, contact hole; 142, conductive material; 150, barrier layer; 160, conductive film layer. DETAILED DESCRIPTION
[0040] The following describes the embodiments of the present invention by specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the following embodiments and features in the embodiments can be combined with each other without conflict.
[0041] It should be noted that the illustrations provided in the following embodiments are only schematic illustrations of the basic concept of the present invention, and thus the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0042] In the following description, numerous details are discussed to provide a more thorough explanation of the embodiments of the present invention. However, it is obvious to those skilled in the art that the embodiments of the present invention can be implemented without these specific details. In other embodiments, well-known structures and devices are shown in the form of block diagrams rather than in detail to avoid making the embodiments of the present invention difficult to understand.
[0043] In the present invention, if the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc. appear, the orientation or position relationship indicated is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, if the terms "first" and "second" appear, they are only used for description and distinction purposes, and cannot be understood as indicating or implying relative importance.
[0044] The contact plug is an electrical connection structure used to connect the device layer and the upper metal interconnect layer in the MEOL process. The conventional process of the contact plug is to first form a contact hole in the interlayer dielectric layer, then deposit a barrier layer on the sidewall of the contact hole, and then fill the contact hole with a conductive material. The provision of the barrier layer can increase the adhesion between the interlayer dielectric layer and the conductive material of the contact plug and reduce the gap between the two. However, since the barrier layer is mostly high-resistance metal nitride, it will affect the performance of the device. If the barrier layer between the conductive material and the interlayer dielectric layer is removed, the adhesion between the conductive material and the interlayer dielectric layer will deteriorate, and a certain physical gap will appear between the two. During the subsequent planarization process, the CMP polishing liquid will pass through the gap into the substrate. Since the CMP polishing liquid is an acidic liquid, it will corrode the bottom metal layer (see Figure 1 ), affecting the yield of the device.
[0045] Based on this, the present invention provides a method for preparing a semiconductor structure and a semiconductor structure, wherein a processable second dielectric layer is formed on a first dielectric layer, and before CMP treatment, the second dielectric layer is first cured to transform it into a tensile stress layer, which can squeeze the first dielectric layer to approach the contact plug, thereby facilitating better adhesion between the contact plug and the interlayer dielectric layer and minimizing the physical gap; and effectively preventing or minimizing the CMP polishing liquid from sliding down the gap and corroding the metal layer on the substrate.
[0046] See also Figures 2 to 9 According to a first aspect of the present invention, there is provided a method for preparing a semiconductor structure, the method comprising at least the following steps:
[0047] S1, providing a substrate 100, on which a metal layer and a first dielectric layer 120 located on the metal layer are formed (see Figure 3 );
[0048] S2, forming a second dielectric layer 130 on the first dielectric layer 120 (see Figure 4 );
[0049] S3, forming a contact hole 141 in the first dielectric layer 120 and the second dielectric layer 130, wherein the bottom of the contact hole 141 exposes the metal layer on the substrate 100 (see Figure 5 );
[0050] S4, filling the contact hole 141 with a conductive material 142 to form an initial plug 140 (see Figure 6 );
[0051] S5, curing the second dielectric layer 130 to form a tensile stress layer 131, wherein the tensile stress layer 131 squeezes the first dielectric layer 120 toward the initial plug 140 (see Figure 7 );
[0052] S6, using a chemical mechanical polishing process to remove the tensile stress layer 131, a portion of the first dielectric layer 120 and a portion of the conductive material 142, to form a contact plug (see Fig. 9 ).
[0053] Combine the following Figures 3 to 9 Each step of the method for preparing a semiconductor structure in an embodiment of the present invention is described in detail.
[0054] See also Figure 2 The base 100 provided in step S1 includes a substrate (not shown in the figure) and a device layer (not shown in the figure) formed on the substrate. The substrate can be any substrate material that can meet the requirements of integrated circuits. As an example, the substrate can be single crystal silicon (Si), single crystal germanium (Ge), silicon germanium (SiGe), silicon carbide (SiC), gallium arsenide (GaAs), indium arsenide (InAs) or other III / V compound semiconductor materials. In addition, the substrate can also be a stacked substrate material such as Si / SiGe, Si / SiC, silicon on insulator (SOI), germanium on insulator (GOI) or silicon germanium on insulator (SGOI). The device layer refers to a structural layer on which a semiconductor device is formed. The semiconductor device is, for example, a MOS (Metal-Oxide-Semiconductor) device. The MOS device specifically includes a gate, a source region (source), a drain region (drain), etc. The metal layer on the substrate 100 is the electrode lead-out member of the gate, drain or source of the device. The MOS device is insulated and isolated from adjacent MOS devices through an isolation structure such as a shallow trench isolation (Shallow Trench Isolation, STI for short) structure.
[0055] The first dielectric layer 120 is formed on the surface of the device layer to provide support for the subsequent formation of contact plugs. The material of the first dielectric layer 120 can be selected from conventional interlayer dielectric materials in the art, such as silicon oxide, silicon nitride, silicon oxynitride and insulating materials with low dielectric constants (dielectric constants less than 3), such as boron-doped silicon glass (BSG), phosphorus-doped silicon glass (PSG) or boron-phosphorus-doped silicon glass (BPSG). Subsequently, contact plugs are formed in the first dielectric layer 120 to lead out the electrodes of the MOS device (source, gate and drain). The present invention does not specifically limit the position of the contact plug, and those skilled in the art can form the contact plug on the source, drain or gate according to actual production conditions. The first dielectric layer 120 is formed by conventional processes in the art such as chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD).
[0056] In one embodiment, an etching stop layer 110 is also formed on the substrate 100. The etching stop layer 110 is arranged between the device layer and the first dielectric layer 120. The etching stop layer 110 is used as a stop layer for subsequent etching to form the contact hole 141. The etching stop layer 110 is, for example, silicon nitride, nitrogen-doped silicon carbide (NDC), etc. The etching stop layer 110 can be formed by conventional methods in the art, such as atomic layer deposition (ALD) and other processes. The setting of the etching stop layer 110 can better control the etching accuracy and prevent over-etching from damaging the substrate 100.
[0057] See also Figure 4 In step S2, a second dielectric layer 130 is formed on the first dielectric layer 120. The second dielectric layer 130 is made of a loose and porous oxide material so that a tensile stress layer 131 can be formed by subsequent curing. The tensile stress layer 131 can squeeze the first dielectric layer 120 thereunder to reduce the physical gap between the first dielectric layer 120 and the contact plug.
[0058] In one embodiment, the material of the second dielectric layer 130 is selected from silicon dioxide (SiO2) and / or a derivative of silicon dioxide. The derivative of silicon dioxide includes, but is not limited to, one or more of silicon oxycarbide (SiOC), silicon oxynitride (SiON) or silicon oxycarbonitride (SiOCN). That is, the material of the second dielectric layer 130 can be selected from any one of silicon dioxide or its derivatives, such as silicon dioxide, or can be selected from any combination of two or more of silicon dioxide and its derivatives, such as a composite layer of silicon dioxide and silicon oxycarbide, etc.
[0059] The second dielectric layer 130 can be prepared by a flowable chemical vapor deposition (FCVD) process. The FCVD process uses a silicon-containing precursor as a reactant to react with ammonia and an oxidant to form a fluid film. Taking the second dielectric layer 130 as silicon dioxide as an example, silazane is used as a reactant to react with ammonia and oxygen to form a fluid film. After the material is subsequently cured, the density and pressure in the film layer change, thereby achieving an extrusion effect. Further, the deposition thickness of the second dielectric layer 130 is 100 angstroms to 500 angstroms. For example, the deposition thickness of the second dielectric layer 130 can be 100 angstroms, 300 angstroms or 500 angstroms. The specific thickness of the second dielectric layer 130 can be set according to actual production conditions. It should be noted that if the second dielectric layer 130 is deposited too thinly, it cannot completely cover the gap between the top dielectric layer and the conductive material 142, and if the second dielectric layer 130 is deposited too thickly, it will be unfavorable for the subsequent removal process. In this embodiment, the deposition thickness of the second dielectric layer 130 is controlled to be between 100 angstroms and 500 angstroms, which can cover the gap between the first dielectric layer 120 and the top of the conductive material 142 , but is not too thick to increase the difficulty of the removal process.
[0060] See also Figure 5 In step S3, a contact hole 141 is formed in the first dielectric layer 120 and the second dielectric layer 130. The specific process is as follows:
[0061] A patterned mask layer is formed on the second dielectric layer 130 .
[0062] First, a photoresist is spin-coated on the second dielectric layer 130 to form a photoresist layer, and then the photoresist layer is exposed and developed to form one or more windows on the photoresist layer, so that the corresponding window positions of the second dielectric layer 130 are exposed. The photoresist in this embodiment can be a positive photoresist or a negative photoresist. The window on the photoresist layer is used to define the position of the contact hole 141.
[0063] Using the patterned mask layer as a mask, the second dielectric layer 130 and the first dielectric layer 120 are etched sequentially from top to bottom until the metal layer on the substrate 100 is exposed.
[0064] In this embodiment, the second dielectric layer 130 is first etched by an etching process using a patterned photoresist layer as a mask until the second dielectric layer 130 is penetrated, and a first through hole is formed in the second dielectric layer 130; then the first dielectric layer 120 is etched downward until a second through hole is formed in the first dielectric layer 120, and the second through hole exposes the metal layer on the substrate 100 (the electrode lead-out area of the source, drain, and gate of the device), and the first through hole and the second through hole together form a contact hole 141. In other embodiments, if an etching stop layer 110 is further provided under the first dielectric layer 120, etching is continued until the etching stop layer 110 is penetrated to expose the metal layer on the substrate 100. The etching process of the contact hole 141 includes, but is not limited to, dry etching, wet etching, or a combination of dry etching and wet etching.
[0065] See also Figure 6 In step S4 , a conductive material 142 is filled in the contact hole 141 to form an initial plug 140 .
[0066] In one embodiment, the conductive material 142 is filled by a selective chemical deposition process, and the conductive material 142 is sequentially deposited from the bottom of the contact hole 141 from bottom to top until it is flush with the upper surface of the second dielectric layer 130. The selective chemical deposition process can realize that a conductive film is formed on the surface of the metal layer at the bottom of the contact hole 141, while it is not easy to form a conductive film on the surface of the second dielectric layer 130, which is conducive to preventing the deposited conductive material 142 from closing prematurely at the top of the contact hole 141, thereby avoiding the formation of voids inside the formed conductive material 142, so that the performance of the formed semiconductor structure is better.
[0067] The conductive material 142 in step S4 can be selected from conventional materials with good conductivity in the art. In some embodiments, the conductive material 142 includes one or more combinations of tungsten (W), cobalt (Co), copper (Cu), molybdenum (Mo), ruthenium (Ru), and titanium (Ti). That is, the conductive material 142 can be selected from any one of the materials listed above, such as tungsten or cobalt, etc.; or any combination of two or more of the materials listed above can be selected, such as tungsten-cobalt alloy, or tungsten-titanium alloy, etc. In this embodiment, the conductive material 142 is selected from tungsten.
[0068] See also Figure 7 In step S5 , the second dielectric layer 130 is cured to transform it into a tensile stress layer 131 .
[0069] The curing treatment includes but is not limited to ultraviolet curing or heat treatment. Since the material of the second dielectric layer 130 is a thin film material of silicon dioxide and / or its derivatives with a certain degree of looseness, after the curing treatment, the chemical bonds such as Si-OH in the film layer of the second dielectric layer 130 will be broken and reorganized, and the second dielectric layer 130 film will become denser, and squeeze the first dielectric layer 120 to make it close to the conductive material 142 in the contact hole 141, so as to reduce the gap between the first dielectric layer 120 and the conductive material 142.
[0070] In one embodiment, the curing treatment adopts an ultraviolet curing process. The ultraviolet curing treatment is carried out under the irradiation condition of ultraviolet light, specifically, the treatment is carried out under ultraviolet light with a wavelength of 200 nm to 450 nm for 1 min to 5 min. As an example, the ultraviolet light can be ultraviolet light with a wavelength of 200nm, 300nm, 400nm or 450nm, etc.; the irradiation time of the ultraviolet light can be 1min, 3min or 5min, etc. The shorter the wavelength of the ultraviolet light, the higher its energy, so the irradiation time can be shortened accordingly. After the ultraviolet light treatment, the gap in the second dielectric layer 130 is reduced, and the loose oxide layer is transformed into a dense tensile stress layer 131, thereby generating stress in the film layer. Since the contact hole 141 penetrates the second dielectric layer 130, the second dielectric layer 130 uses the contact hole as a stress release area under the action of internal stress, thereby squeezing close to the edge of the contact hole, thereby reducing or even blocking the gap between the first dielectric layer 120 and the conductive material 142.
[0071] In another embodiment, the curing treatment adopts a heat treatment process. The heat treatment process adopts, for example, a water vapor thermal annealing process. By exposing the second dielectric layer 130 to a water vapor environment at a high temperature, physical or chemical changes in the second dielectric layer 130 film are achieved. The treatment temperature of the water vapor thermal annealing process is 500°C to 1050°C, for example, 500°C, 700°C, 900°C or 1050°C, etc.; the annealing treatment time is 10min to 30min, for example, 10min, 20min or 30min, etc. The temperature and treatment time of the heat treatment process can be selected within the above range according to the thickness and material of the second dielectric layer 130 in actual production.
[0072] See also Figure 8 and Fig. 9 In step S6, the tensile stress layer 131, a portion of the first dielectric layer 120 and a portion of the conductive material 142 are removed to form a final contact plug.
[0073] In one embodiment, before executing step S6, a barrier layer 150 is formed on the tensile stress layer 131, and a conductive film layer 160 is formed on the barrier layer 150. The barrier layer 150 can further prevent the polishing liquid from corroding the bottom metal layer through the gap between the conductive material 142 in the contact hole 141 and the first dielectric layer 120 during the subsequent CMP process. The material of the barrier layer 150 can be selected from titanium nitride or tantalum nitride, etc., and its formation method includes chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD), etc. The conductive film layer 160 can also be used as a protective layer to reduce the damage of CMP to the material in the hole, and can also improve the polishing performance during the CMP process, for example, by controlling the polishing rate and improving the uniformity of polishing. The material of the conductive film layer 160 includes, but is not limited to, one or more combinations of tungsten (W), cobalt (Co), copper (Cu), molybdenum (Mo), ruthenium (Ru), and titanium (Ti). The conductive film layer 160 may be the same as the conductive material 142 filled in the contact hole 141, for example, both the conductive film layer 160 and the conductive material 142 may be tungsten; or it may be different from the conductive material 142, for example, the conductive material 142 may be tungsten, and the material of the conductive film layer 160 may be copper. Furthermore, the material of the conductive film layer 160 is the same as the conductive material 142.
[0074] Please continue reading Fig. 9 , perform step S6, use chemical mechanical polishing (CMP) to remove the tensile stress layer 131, a portion of the first dielectric layer 120 and a portion of the conductive material 142, thereby exposing the first dielectric layer 120 and the contact plug formed in the first dielectric layer 120 to facilitate the execution of subsequent processes.
[0075] It should be noted that, due to the compression of the first dielectric layer 120 below it by the tensile stress layer 131, the first dielectric layer 120 is moved closer to the conductive material 142 in the contact hole 141, greatly reducing or even completely covering the gap between the first dielectric layer 120 and the conductive material 142. During the CMP process, the CMP polishing liquid can be effectively prevented from entering the metal layer at the bottom of the contact hole 141 from the gap at the top between the first dielectric layer 120 and the conductive material 142, thereby reducing the corrosion of the bottom metal layer. In addition, the tensile stress layer 131, the barrier layer 150 and the conductive film layer 160 located above the first dielectric layer 120 will further block the entry of the CMP slurry, thereby improving the reliability of the semiconductor structure.
[0076] After the chemical mechanical polishing process, the top conductive film layer 160, the barrier layer 150 and the tensile stress layer 131 are removed, and the conductive material 142 formed in the second dielectric layer 130 is also removed simultaneously in the chemical mechanical polishing process. Therefore, the second through hole and the conductive material 142 remaining in the first dielectric layer 120 form the final contact plug.
[0077] The method for preparing the semiconductor structure of the present invention forms a curable second dielectric layer 130 on the first dielectric layer 120, and before the chemical mechanical polishing process, first cures the second dielectric layer 130 to transform it into a tensile stress layer 131, and the tensile stress layer 131 applies pressure to the first dielectric layer 120 to make it close to the conductive material 142 in the contact hole 141, reducing the gap between the two, and effectively preventing the polishing liquid from corroding the bottom metal layer during the chemical mechanical polishing process; and because the tensile stress layer 131 will not eventually remain on the substrate 100, even when the contact hole 141 is formed, etching the second dielectric layer 130 may cause etching damage to the surface of the second dielectric layer 130 due to the thin thickness of the photoresist, but it will not affect the formation of the contact plug. Further, etching the first dielectric layer 120 using the second dielectric layer 130 as a hard mask can ensure that the surface of the first dielectric layer 120 will not be damaged by etching, and at the same time, the morphology of the contact hole 141 in the first dielectric layer 120 can be ensured.
[0078] See also Fig. 9 On the other hand, the present invention further provides a semiconductor structure, which is prepared by the preparation method described above. The semiconductor structure includes a substrate 100, a first dielectric layer 120, a contact hole 141 and a conductive material 142.
[0079] The base 100 includes a substrate (not shown in the figure) and a device layer (not shown in the figure) formed on the substrate. Among them, the substrate can be any substrate material that can meet the requirements of the integrated circuit. As an example, the substrate can be selected from single crystal silicon (Si), single crystal germanium (Ge), silicon germanium (SiGe), silicon carbide (SiC), gallium arsenide (GaAs), indium arsenide (InAs) or other III / V compound semiconductor materials. In addition, the substrate can also be a stacked substrate material such as Si / SiGe, Si / SiC, silicon on insulator (SOI), germanium on insulator (GOI) or silicon germanium on insulator (SGOI). The device layer represents a structural layer formed with a semiconductor device, such as a MOS (Metal-Oxide-Semiconductor) device, and the MOS device specifically includes a gate, a source region (source), a drain region (drain), etc., and an isolation structure such as a shallow trench isolation (Shallow Trench Isolation, referred to as STI) structure is used to insulate and isolate adjacent MOS devices.
[0080] The first dielectric layer 120 is formed on the surface of the device layer to provide support for the subsequent formation of contact plugs. The material of the first dielectric layer 120 can be selected from conventional interlayer dielectric materials in the art, such as silicon oxide, silicon nitride, silicon oxynitride, and insulating materials with low dielectric constants (dielectric constants less than 3), such as boron-doped silicon glass (BSG), phosphorus-doped silicon glass (PSG), or boron-phosphorus-doped silicon glass (BPSG). Subsequently, contact plugs are formed in the first dielectric layer 120 to lead out the electrodes of the MOS device (source, gate, and drain). The present invention does not specifically limit the position of the contact plug, and those skilled in the art can form the contact plug on the source, drain, or gate according to actual production conditions.
[0081] In one embodiment, an etching stop layer 110 is further provided between the first dielectric layer 120 and the substrate 100. The etching stop layer 110 is used as a stop layer for subsequent etching to form the contact hole 141. The etching stop layer 110 is, for example, silicon nitride, nitrogen-doped silicon carbide (NDC for short), or the like.
[0082] The contact hole 141 is disposed in the first dielectric layer 120, and the bottom of the contact hole 141 exposes the metal layer on the substrate 100. In the present invention, before forming the contact hole 141, the second dielectric layer 130 is first formed on the first dielectric layer 120, and the second dielectric layer 130 is an oxide material with a certain degree of looseness, for example, one or more of silicon dioxide (SiO2) and / or silicon dioxide derivatives. The silicon dioxide derivatives include but are not limited to one or more of silicon oxycarbide (SiOC), silicon oxynitride (SiON) or silicon oxycarbonitride (SiOCN). Subsequently, the second dielectric layer 130 is cured to form a tensile stress layer 131, which can squeeze the first dielectric layer 120 to reduce the physical gap between the first dielectric layer 120 and the contact plug. The contact hole 141 is formed in the first dielectric layer 120 and the second dielectric layer 130. The second dielectric layer 130 can not only reduce the gap between the first dielectric layer 120 and the conductive material 142 , but also protect the surface of the first dielectric layer 120 from being damaged by etching when the contact hole 141 is formed by etching, thereby ensuring the morphology of the contact hole 141 .
[0083] The conductive material 142 is filled in the contact hole 141. The conductive material 142 includes one or more combinations of tungsten (W), cobalt (Co), copper (Cu), molybdenum (Mo), ruthenium (Ru), and titanium (Ti). The redundant tensile stress layer 131 and part of the conductive material 142 on the top are removed by the CMP process, and the conductive material 142 remaining in the first dielectric layer 120 and the contact hole 141 form a final contact plug, which is electrically connected to the metal layer on the substrate 100.
[0084] The method for preparing the semiconductor structure of the present invention forms a curable dielectric layer on the first dielectric layer, and the dielectric layer can be transformed into a tensile stress layer through curing, which helps the conductive material of the contact plug to have better adhesion with the first dielectric layer and minimizes the physical gap between the conductive material and the first dielectric layer; it can effectively prevent or minimize the possibility of CMP slurry sliding down from the gap between the conductive material of the contact plug and the first dielectric layer, and then attacking the bottom metal layer, thereby improving the yield of the device. Therefore, the present invention effectively overcomes some practical problems in the prior art and has high utilization value and use significance.
[0085] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for preparing a semiconductor structure, It is characterized in that include: Providing a substrate, on which a metal layer and a first dielectric layer located on the metal layer are formed; forming a second dielectric layer on the first dielectric layer; forming contact holes in the first dielectric layer and the second dielectric layer, wherein the metal layer is exposed at the bottom of the contact holes; Filling the contact hole with a conductive material to form an initial plug; curing the second dielectric layer to form a tensile stress layer, wherein the tensile stress layer squeezes the first dielectric layer toward the initial plug; The tensile stress layer, a portion of the first dielectric layer and a portion of the conductive material are removed by a chemical mechanical polishing process to form a contact plug.
2. The preparation method according to claim 1, It is characterized in that The second dielectric layer is selected from silicon dioxide and / or a derivative of silicon dioxide, and the derivative of silicon dioxide is selected from one or more of silicon oxycarbide, silicon oxynitride, and silicon oxycarbonitride.
3. The preparation method according to claim 1, It is characterized in that The thickness of the second dielectric layer is 100 angstroms to 500 angstroms.
4. The preparation method according to claim 1, It is characterized in that The curing treatment of the second dielectric layer to form the tensile stress layer adopts an ultraviolet curing treatment process, and the ultraviolet curing treatment process includes: treating under ultraviolet light with a wavelength of 200 nm to 450 nm for 1 min to 5 min.
5. The preparation method according to claim 1, It is characterized in that The second dielectric layer is cured to form a tensile stress layer by a heat treatment process, wherein the heat treatment process includes: annealing at a temperature of 500° C. to 1050° C. for 10 min to 30 min.
6. The preparation method according to claim 1, It is characterized in that Before removing the tensile stress layer, part of the first dielectric layer and part of the conductive material by a chemical mechanical polishing process, the method further includes: forming a barrier layer on the tensile stress layer; A conductive film layer is formed on the barrier layer.
7. The preparation method according to claim 1, It is characterized in that The conductive material is selected from one or more combinations of tungsten, cobalt, copper, molybdenum, ruthenium and titanium.
8. The preparation method according to claim 1, It is characterized in that An etch stop layer is also formed on the substrate, and the etch stop layer is formed between the substrate and the first dielectric layer.
9. The preparation method according to claim 1, It is characterized in that Forming contact holes in the first dielectric layer and the second dielectric layer, comprising: forming a patterned mask layer on the second dielectric layer; Using the patterned mask layer as a mask, the second dielectric layer and the first dielectric layer are etched sequentially from top to bottom until the metal layer on the substrate is exposed.
10. A semiconductor structure, It is characterized in that Prepared by the preparation method according to any one of claims 1 to 9, the semiconductor structure comprises: A substrate, on which a metal layer and a first dielectric layer located on the metal layer are formed; A contact plug, wherein the contact plug comprises a contact hole and a conductive material, wherein the contact hole is arranged in the first dielectric layer and the contact hole exposes the metal layer; and the conductive material is filled in the contact hole and communicated with the metal layer.