A method for manufacturing a silicon carbide superjunction MOSFET
By etching technology of ion implantation of P-type columns and silicon dioxide layer on the back of the silicon carbide superjunction MOSFET, the problem of P-type column defects on the front of the epitaxial sheet is solved, the process steps are simplified and the cost is reduced, and high-quality Silicon carbide superjunction MOSFET production.
Patent Information
- Application Number
- CN202411095260.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-08-12
AI Technical Summary
In the prior art, when making silicon carbide superjunction MOSFETs, the preparation of P-type columns on the front of the epitaxial sheet is prone to defects, and the process is complex and costly, making it impossible to achieve efficient and large-scale commercial applications.
By ion implanting P-type columns on the back of the epitaxial sheet, combined with the etching of the silica layer and the mask pattern formation, the P-well, N+ and P+ source region structures were gradually obtained, the substrate layer was thinned, and the ions were activated by high-temperature annealing. Finally, front and back electrodes are prepared to simplify process steps and reduce costs.
Low-difficulty etching in silicon carbide superjunction MOSFET is achieved, avoiding the problems of filling holes and ion damage, simplifying process steps, reducing costs and improving device quality.
Smart Images

Figure CN118629871B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of semiconductor chip manufacturing technology, and in particular, relates to a method for manufacturing a silicon carbide super junction MOSFET. Background Art
[0002] Super junction MOSFET is a specially designed structure. Compared with conventional MOSFET, the difference lies in the design of its drift layer, which is composed of multiple vertically arranged PN junctions. This structure can reduce the on-resistance while maintaining the high withstand voltage of the device, making it very suitable for fast switching applications with high energy efficiency and high power density.
[0003] The drift layer of the superjunction MOSFET is composed of alternating N-type and P-type pillars, which form multiple vertical structures between the source and drain ends. Under reverse withstand voltage, they are first depleted laterally and then begin to withstand high withstand voltage vertically. Since the drift region is depleted laterally, a higher doping concentration can be used to reduce the on-resistance of the device. At present, this result has begun to mature in silicon-based products, but based on the characteristics of the material, it is still in the research and development stage in silicon carbide products. The main reason is that the diffusion coefficient of the doped ions in silicon carbide is small, the etching rate is low, and the etching morphology is rough, so that the commonly used manufacturing process in silicon cannot achieve the corresponding effect in silicon carbide products.
[0004] At present, the typical technical route for making silicon carbide super junction is:
[0005] Epitaxial growth fills the trench. This method first requires etching a deeper trench and then filling the P-type trench by epitaxy. Therefore, the etching roughness requirement is very high, otherwise the subsequent epitaxy will increase defects and there will be problems with filling voids.
[0006] Multiple epitaxial growth and ion implantation: This method also involves multiple growth of thin epitaxial layers (1-2um) on N rows of epitaxy, and then ion implantation is used to obtain a P-type region. This process is then repeated multiple times to obtain a P-type N-type column structure. This method requires multiple epitaxy, photolithography, and ion implantation, which is too costly and involves complex procedures. It cannot be commercialized on a large scale.
[0007] Multiple epitaxy and high-energy ion implantation: This method combines the epitaxy and implantation methods, increasing the ion implantation energy on the basis of multiple epitaxy, thereby reducing the number of epitaxy times. It is a variation of the second method, but the problem it brings is ion damage caused by high-energy ion implantation, and the energy is too high, which places extremely high demands on equipment; it does not have the potential for widespread application. Summary of the invention
[0008] The present application provides a method for manufacturing a silicon carbide super junction MOSFET, which solves the technical problem that defects are easily generated when preparing a P-type column on the front side of an epitaxial wafer.
[0009] In order to solve at least one of the above technical problems, the technical solution adopted in this application is:
[0010] A method for manufacturing a silicon carbide super junction MOSFET, comprising the steps of:
[0011] Obtaining a substrate having a P-well, N+ and P+ source region structure on the front side of the epitaxial wafer;
[0012] Ion implantation of P-type pillars from the back of the substrate makes the P-type pillars intersect with the P-well region to obtain a substrate having a MOSFET superjunction structure;
[0013] Activate ions in the epitaxial wafer;
[0014] Then, the front and back electrodes are fabricated in sequence.
[0015] Further, the obtaining of a substrate having a P-well, N+ and P+ source region structure on the front side of the epitaxial wafer is specifically as follows:
[0016] A silicon dioxide layer is deposited on the front side of the epitaxial wafer, and then a P-well mask pattern is formed by etching the silicon dioxide layer;
[0017] Based on the P-well mask pattern, Al ions are implanted into the epitaxial layer on the front side of the epitaxial wafer to obtain a P-well region structure on the front side of the epitaxial layer;
[0018] The P-well mask on the front side of the epitaxial wafer is removed, a silicon dioxide layer is deposited on the front side of the epitaxial wafer, and then an N+ source region mask pattern is formed by etching the silicon dioxide layer;
[0019] Based on the N+ source region mask pattern, N ions are implanted on the P-well region on the front side of the epitaxial wafer to obtain an N+ source region structure stacked on the P-well region;
[0020] The N+ source region mask on the front side of the epitaxial wafer is removed, a silicon dioxide layer is deposited on the front side of the epitaxial wafer, and a P+ source region mask pattern is formed by etching the silicon dioxide layer;
[0021] Based on the P+ source region mask pattern, Al ions are implanted on the P-well layer on the front side of the epitaxial wafer to obtain a P+ source region structure stacked on the P-well region, and to make the P+ and N+ source regions adjacent to each other;
[0022] The P+ source region mask in the front side of the epitaxial wafer is removed, and then a substrate having a P-well, N+ and P+ source region structure is obtained.
[0023] Furthermore, when Al ions are implanted to obtain the P-well region, the temperature is 500-600°C, the energy is 10-500keV, and the dose is 1E11-1E13;
[0024] When N ions are injected to obtain the N+ source region, the temperature is 500-600°C, the energy is 10-200keV, and the dose is 1E12-1E14;
[0025] When Al ions are injected to obtain the P+ source region, the temperature is 500-600°C, the energy is 30-500keV, and the dose is 1E12-1E15.
[0026] Furthermore, before ion implantation of the P-type pillars on the back side of the substrate, the method further includes:
[0027] Bonding a temporary backing layer on the front side of the substrate;
[0028] Reducing the thickness of the back substrate layer;
[0029] Wherein, the temporary substrate material is any one of sapphire, silicon, and glass;
[0030] The back substrate layer is thinned by coarse grinding and fine grinding, so that the thickness of the thinned substrate is about 40-60um.
[0031] Furthermore, the ion implantation of the P-type column from the back side of the substrate is specifically as follows:
[0032] A layer of metal Ni is deposited on the back of the thinned substrate, and a P-type column mask pattern is formed by etching the metal layer;
[0033] Based on the P-type pillar mask pattern in the metal layer, continue etching the same etching pattern as the P-type pillar mask pattern in the substrate layer;
[0034] Based on the etching pattern in the substrate layer, Al ions are directly injected into the etching holes to form a P-type column intersecting with the P-well area on the back of the epitaxial layer, and then the metal layer is removed;
[0035] The P-type column can cut off the epitaxial layer to form a number of N-type columns parallel to the P-type column, which is the base of the MOSFET super junction structure.
[0036] Furthermore, the thickness of the metal layer is 100-800 nm;
[0037] When Al ions are injected to obtain P-type columns, the temperature is 500-600°C, the energy is 10keV-2MeV, and the dose is 1E11-1E15;
[0038] When etching the same etching pattern as the P-type column mask pattern continues in the substrate layer, the etching depth is 1-3um thick from the bottom of the substrate layer.
[0039] Furthermore, before etching the P-type column mask pattern on the metal layer, the method further includes:
[0040] coating a layer of photoresist on the metal layer;
[0041] Etching a P-type column mask pattern on the photoresist;
[0042] Based on the P-type pillar mask pattern on the photoresist, etching is performed on the metal layer by dry etching to form a metal mask layer having the P-type pillar mask pattern;
[0043] Finally, the metal layer mask is removed by using a metal etching solution.
[0044] Furthermore, the activating of ions in the epitaxial wafer includes:
[0045] removing the temporary backing on the front side of the substrate;
[0046] Place the entire substrate into a high-temperature annealing furnace with a temperature of 1600-1900°C and an activation time of 10-40 minutes to activate all ions inside the epitaxial wafer.
[0047] Furthermore, the front and back electrodes are fabricated in sequence, specifically:
[0048] A temporary substrate is bonded to the back of the substrate, and a front electrode is prepared on the front of the substrate;
[0049] Remove the back temporary substrate, in the back substrate layer,
[0050] First, metal CVD is used to fill the deep holes on the back with metal W;
[0051] Then, four metal layers of Ni, Ti, Ni, and Ag are deposited on the back in sequence by sputtering or evaporation, with a thickness ranging from 50nm to 2um;
[0052] That is, the back electrode is obtained.
[0053] Furthermore, the preparation of the front electrode on the front side of the substrate comprises:
[0054] A layer of oxide is obtained on the front side of the substrate by high temperature oxidation as a gate oxide layer;
[0055] Then a layer of polysilicon is deposited by LPCVD;
[0056] By photolithography and dry etching, a gate is obtained;
[0057] Then, a silicon dioxide insulating layer is deposited outside the gate to wrap the gate, and the thickness of the insulating layer is 1 um;
[0058] The insulating layer is etched away in the source region to expose the P+ and N+ source regions;
[0059] The source metal layer is deposited on the front side of the substrate by evaporation or sputtering. From bottom to top, the corresponding metals in the metal layer are Ni, Ti, and Al, respectively, with thicknesses ranging from 10nm to 4um. The front source metal pattern is formed by photolithography, which is the front electrode.
[0060] A method for manufacturing a silicon carbide super junction MOSFET designed in the present application is used. On the basis of not affecting the device structure, thinning and etching are performed on the back side of the epitaxial layer to obtain a P-type column grinding pattern, and the P-type column is obtained by injecting Al ions on the back side, thereby obtaining a substrate with a MOSFET super junction structure. Not only is the etching difficulty low, but the various process steps are simple, safe and controllable. There are no problems of filling voids and ion damage, and the performance of the front device structure will not be affected. The manufacturing cost is low and the quality is good. BRIEF DESCRIPTION OF THE DRAWINGS
[0061] Figure 1 is a flow chart of a method for manufacturing a silicon carbide superjunction MOSFET in the present application;
[0062] Figure 2 is a schematic diagram of the structure of the substrate in this application;
[0063] Figure 3 It is a schematic diagram of the structure after front bonding and substrate thinning in this application;
[0064] Figure 4 This is a schematic diagram of the formation of a super junction structure by particle injection after etching of the back substrate in the present application;
[0065] Figure 5 is a schematic diagram of the superjunction structure after the front electrode is completed in this application;
[0066] Figure 6 It is a schematic diagram of the structure of a chip with a MOSFET super junction structure in this application.
[0067] In the figure:
[0068] 100. Chip; 10. Epitaxial layer; 11. P-well region; 12. P+ source region; 13. N+ source region; 14. P-type column; 20. Substrate layer; 30. Temporary substrate; 40. Front source; 41. Gate; 42. Insulating layer; 50. Back drain. DETAILED DESCRIPTION
[0069] The present application is described in detail below with reference to the accompanying drawings and specific embodiments.
[0070] This embodiment provides a method for manufacturing a silicon carbide super junction MOSFET. Figure 1 As shown, the steps include:
[0071] S1. Obtain a substrate having a P-well, N+ and P+ source region structure on the front side of the epitaxial wafer.
[0072] A layer of silicon dioxide is first deposited on the front side of the epitaxial wafer, and then the silicon dioxide layer is etched to form a P-well mask pattern, wherein the epitaxial wafer includes an epitaxial layer 10 and a substrate layer 20. At this time, the epitaxial layer 10 and the substrate layer 20 are both epitaxial wafers made of N-type SiC material, and because the initial thickness of the substrate layer 20 is relatively thick, about 300-500um, its base structure strength is high, and etching can be performed directly on the front side.
[0073] The silicon dioxide layer is a common deposition layer, which is convenient for photolithography masking on the front side. Then a layer of photoresist with a P-well mask pattern is coated on the surface of the silicon dioxide layer, the purpose of which is to perform photolithography on this silicon dioxide layer to form a P-well mask pattern. After the P-well mask pattern is formed on the silicon dioxide layer, the photoresist is removed. At this time, there are three layers on the epitaxial wafer, the epitaxial layer 10 located on the front side, the silicon dioxide layer with a P-well mask pattern on the front side (omitted in the figure), and the substrate layer 20 located on the back side.
[0074] Based on the P-well mask pattern on the silicon dioxide layer, Al ions are first implanted into the epitaxial layer 10 on the front side of the epitaxial wafer to obtain the P-well region 11 structure on the front side of the epitaxial layer 10. The temperature when Al ions are implanted is 500-600°C, the energy is 10-500keV, and the dose is 1E11-1E13, thereby obtaining an epitaxial wafer having the P-well region 11 structure on the front side of the epitaxial layer 10.
[0075] Hydrofluoric acid is used to remove the silicon dioxide P-well mask layer deposited for the first time on the front side of the epitaxial wafer.
[0076] A silicon dioxide layer is deposited on the front of the epitaxial wafer for the second time, and a photoresist having a mask pattern of the N+ source region 13 is coated on the surface of the silicon dioxide layer. Based on the photoresist, the mask pattern of the N+ source region 13 is etched on the silicon dioxide layer. After the mask pattern of the N+ source region 13 is formed on the silicon dioxide layer, the photoresist is removed.
[0077] Based on the mask pattern of the N+ source region 13 of the silicon dioxide layer, N ions are implanted on the P-well region 11 in the epitaxial layer 10 on the front side of the epitaxial wafer to obtain an N+ source region 13 structure stacked on the P-well region 11. The temperature when the N ions are implanted is 500-600°C, the energy is 10-200keV, and the dose is 1E12-1E14, thereby obtaining an epitaxial wafer having an N+ source region 13 structure stacked on the P-well region 11 in the epitaxial layer 10.
[0078] The mask layer of silicon dioxide N+ source region 13 deposited for the second time on the front side of the epitaxial wafer is removed by using hydrofluoric acid.
[0079] A silicon dioxide layer is deposited on the front of the epitaxial wafer for the third time, and a photoresist having a mask pattern of the P+ source region 12 is coated on the surface of the silicon dioxide layer. Based on the photoresist, the mask pattern of the P+ source region 12 is etched on the silicon dioxide layer. After the mask pattern of the P+ source region 12 is formed on the silicon dioxide layer, the photoresist is removed.
[0080] Based on the mask pattern of the P+ source region 12 of the silicon dioxide layer, Al ions are implanted on the P-well region 11 in the epitaxial layer 10 on the front side of the epitaxial wafer to obtain a P+ source region 12 structure stacked on the P-well region 11, and the P+ and N+ source regions 13 are adjacent. The temperature when Al ions are implanted to obtain the P+ source region 12 is 500-600°C, the energy is 30-500keV, and the dose is 1E12-1E15, thereby obtaining an epitaxial wafer having a P+ source region 12 structure stacked on the P-well region 11 in the epitaxial layer 10, and the P+ and N+ source regions 13 are adjacent, for ohmic contact.
[0081] Hydrofluoric acid is used to remove the third deposited silicon dioxide P+ source region 12 mask layer on the front side of the epitaxial wafer, and then the following is obtained: Figure 2 The substrate shown has a P-well, N+ and P+ source region 12 structure.
[0082] S2. Ion implantation of P-type columns from the back of the substrate makes the P-type columns intersect with the P-well region 11 to obtain a substrate having a MOSFET super junction structure.
[0083] Since it is difficult to directly etch on the back side of the substrate and it is difficult to control the etching morphology, a temporary bonding device is used to bond a temporary substrate 30 on the front side of the substrate. The material used for the temporary substrate 30 can be any one of sapphire, silicon, glass and other materials.
[0084] like Figure 3 As shown, before ion implantation of the P-type pillars 14 is performed on the back side of the substrate, a temporary substrate 30 needs to be bonded on the front side of the substrate using a temporary bonding device.
[0085] Then, the thickness of the back substrate layer 20 of the substrate can be thinned by rough grinding and fine grinding, so that the thickness of the back substrate is about 40-60um; Figure 3 The substrate layer in is the thickness of the substrate after thinning.
[0086] like Figure 4 As shown, preparations are made to ion-implant the P-type column 14 from the back side of the substrate, specifically:
[0087] A layer of metal Ni is deposited on the back of the thinned substrate, that is, a metal layer (omitted in the drawing) is deposited on the substrate layer 20, and the thickness of the metal layer is 100-800nm.
[0088] A layer of photoresist is then coated on the metal layer, and a mask pattern having a P-type column 14 structure is first photoetched on the photoresist to form a photoresist mask layer.
[0089] Based on the mask pattern of the P-type pillar 14 on the photoresist, the metal layer is etched by dry etching to form a metal mask layer with the mask pattern of the P-type pillar 14. After the mask pattern on the metal layer is formed, the photoresist mask layer on the metal layer is removed by a stripping liquid, thereby forming a mask pattern with the P-type pillar 14 on the metal layer.
[0090] Based on the mask pattern of the P-type column 14 in the metal layer, etching is continued in the substrate layer to form an etching pattern identical to the mask pattern of the P-type column 14. However, during this etching process, when etching the same etching pattern as the mask pattern of the P-type column 14 in the substrate layer, the depth of the hole is 1-3um thick from the bottom of the substrate layer. That is, when etching a hole in the substrate layer 20, the depth of the hole cannot completely penetrate the substrate, and a thickness of 1-3um needs to be retained.
[0091] Then, in the etched substrate layer 20, based on the etching pattern thereon, high-energy Al ions are directly injected into the etching holes to form a P-type column 14 intersecting with the P-well region 11 on the back of the epitaxial layer 10; for silicon carbide, Al particles are selected as the doping element for P-type doping. When Al ions are injected to obtain the P-type column 14, the temperature is 500-600°C, the energy is 10keV-2MeV, and the dose is 1E11-1E15.
[0092] After the mask pattern in the substrate layer 20 is prepared, a metal etching solution is used to remove the metal layer mask. The metal solution may be aqua regia to remove the metal layer.
[0093] The P-type column 14 obtained in the epitaxial layer 10 can cut off the epitaxial layer 10 to form a plurality of N-type columns parallel to the P-type column 14. This structure with the P-type column 14 and the N-type column in parallel is the substrate of the MOSFET super junction structure.
[0094] S3. Activate the ions in the epitaxial wafer.
[0095] First, remove the temporary substrate 30 on the front side of the substrate; then put the entire substrate into a high-temperature annealing furnace with a temperature of 1600-1900° C. and an activation time of 10-40 minutes to activate all ions inside the epitaxial wafer.
[0096] S4. Then, the front and back electrodes are fabricated in sequence.
[0097] like Figure 5 As shown, a temporary substrate 30 is first bonded on the back of the substrate, and then a front source is prepared on the front of the substrate; then the back temporary substrate 30 is removed, and then a back drain 50 is prepared on the back of the substrate to make a Figure 6 Chip 100 is shown.
[0098] A front electrode is prepared on the front side of the substrate, including:
[0099] A layer of oxide is deposited on the front side of the substrate by high-temperature oxidation as a gate oxide layer; a layer of polysilicon is then deposited by LPCVD; the gate pattern is then produced by photolithography, and the oxide layer and polysilicon outside the gate 41 are etched away by dry etching, and the photoresist is then removed; thus, the middle gate 41 is formed.
[0100] Then, a silicon dioxide insulating layer 42 is deposited outside the gate 41 to completely cover the gate 41, and the thickness of the insulating layer 42 is 1 um. Then, photolithography and etching are performed to etch away the insulating layer 42 corresponding to the source region, and the source regions of P+ and N+ are exposed. Then, the resist is removed; only the insulating layer 42 that wraps the gate 41 is retained.
[0101] The front source electrode 40 metal layer is deposited on the front of the substrate by evaporation or sputtering. From bottom to top, the corresponding metals in the metal layer are Ni, Ti, and Al, respectively, with a thickness of 10nm-4um. Then, the front source electrode 40 metal pattern is formed by photolithography, which is the front electrode.
[0102] In the back substrate layer, metal CVD is first used to fill the deep holes on the back with metal W. Then, four layers of metal, Ni, Ti, Ni, and Ag, are deposited on the back in sequence by sputtering or evaporation, with a thickness ranging from 50nm to 2um, to obtain a back drain 50, i.e., a back electrode.
[0103] A method for manufacturing a silicon carbide super junction MOSFET designed in the present application is used. On the basis of not affecting the device structure, thinning and etching are performed on the back side of the epitaxial layer to obtain a P-type column grinding pattern, and the P-type column is obtained by injecting Al ions on the back side, thereby obtaining a substrate with a MOSFET super junction structure. Not only is the etching difficulty low, but the various process steps are simple, safe and controllable. There are no problems of filling voids and ion damage, and the performance of the front device structure will not be affected. The manufacturing cost is low and the quality is good.
[0104] The above detailed description of the embodiments of the present application is only a preferred embodiment of the present application and cannot be considered to limit the scope of implementation of the present application. All equivalent changes and improvements made within the scope of the present application should still fall within the scope of the patent coverage of the present application.
Claims
1. A method for manufacturing a silicon carbide super junction MOSFET, It is characterized in that the steps include: Obtaining a substrate having a P-well, N+ and P+ source region structure on the front side of the epitaxial wafer; Ion implantation of P-type pillars from the back of the substrate makes the P-type pillars intersect with the P-well region to obtain a substrate having a MOSFET superjunction structure; Activate ions in the epitaxial wafer; Then, the front and back electrodes are fabricated in sequence; Before ion implantation of the P-type column on the back side of the substrate, the method further includes: Bonding a temporary backing layer on the front side of the substrate; Reducing the thickness of the back substrate layer; The ion implantation of the P-type column from the back side of the substrate is specifically as follows: Depositing a metal layer on the back of the thinned substrate, and etching the metal layer to form a P-type column mask pattern; Based on the P-type pillar mask pattern in the metal layer, continue etching the same etching pattern as the P-type pillar mask pattern in the substrate layer; Based on the etching pattern in the substrate layer, Al ions are directly injected into the etching holes to form a P-type column intersecting with the P-well area on the back of the epitaxial layer, and then the metal layer is removed; The P-type column cuts off the epitaxial layer to form a number of N-type columns parallel to the P-type column, which is the base of the MOSFET super junction structure.
2. A method for manufacturing a silicon carbide super junction MOSFET according to claim 1, It is characterized in that The step of obtaining a substrate having a P-well, N+ and P+ source region structure on the front side of the epitaxial wafer is specifically as follows: A silicon dioxide layer is deposited on the front side of the epitaxial wafer, and then a P-well mask pattern is formed by etching the silicon dioxide layer; Based on the P-well mask pattern, Al ions are implanted into the epitaxial layer on the front side of the epitaxial wafer to obtain a P-well region structure on the front side of the epitaxial layer; The P-well mask on the front side of the epitaxial wafer is removed, a silicon dioxide layer is deposited on the front side of the epitaxial wafer, and then an N+ source region mask pattern is formed by etching the silicon dioxide layer; Based on the N+ source region mask pattern, N ions are implanted on the P-well region on the front side of the epitaxial wafer to obtain an N+ source region structure stacked on the P-well region; The N+ source region mask on the front side of the epitaxial wafer is removed, a silicon dioxide layer is deposited on the front side of the epitaxial wafer, and a P+ source region mask pattern is formed by etching the silicon dioxide layer; Based on the P+ source region mask pattern, Al ions are implanted into the P-well region on the front side of the epitaxial wafer to obtain a P+ source region structure stacked on the P-well region, and to make the P+ and N+ source regions adjacent to each other; The P+ source region mask in the front side of the epitaxial wafer is removed, and then a substrate having a P-well, N+ and P+ source region structure is obtained.
3. A method for manufacturing a silicon carbide super junction MOSFET according to claim 2, It is characterized in that When Al ions are injected to obtain the P-well region, the temperature is 500-600°C, the energy is 10-500keV, and the dose is 1E11-1E13 ion / cm 2 ; When N ions are injected to obtain the N+ source region, the temperature is 500-600°C, the energy is 10-200keV, and the dose is 1E12-1E14ion / cm 2 ; When Al ions are injected to obtain the P+ source region, the temperature is 500-600°C, the energy is 30-500keV, and the dose is 1E12-1E15ion / cm 2 .
4. A method for manufacturing a silicon carbide super junction MOSFET according to any one of claims 1 to 3, It is characterized in that The temporary substrate material is any one of sapphire, silicon, and glass; The back substrate layer is thinned by coarse grinding and fine grinding to make the thickness of the thinned substrate 40-60um.
5. The method for manufacturing a silicon carbide super junction MOSFET according to claim 1, It is characterized in that The thickness of the metal layer is 100-800nm; When Al ions are injected to obtain P-type columns, the temperature is 500-600°C, the energy is 10keV-2MeV, and the dose is 1E11-1E15ion / cm 2 ; When etching the same etching pattern as the P-type column mask pattern continues in the substrate layer, the etching depth is 1-3um thick from the bottom of the substrate layer.
6. The method for manufacturing a silicon carbide super junction MOSFET according to claim 5, It is characterized in that Before etching the P-type column mask pattern on the metal layer, the method further includes: coating a layer of photoresist on the metal layer; Etching a P-type column mask pattern on the photoresist; Based on the P-type pillar mask pattern on the photoresist, etching is performed on the metal layer by dry etching to form a metal mask layer having the P-type pillar mask pattern; Finally, the metal mask layer is removed by using a metal etching solution.
7. The method for manufacturing a silicon carbide super junction MOSFET according to claim 1, It is characterized in that The activating of ions in the epitaxial wafer comprises: removing the temporary backing on the front side of the substrate; Place the entire substrate into a high-temperature annealing furnace with a temperature of 1600-1900°C and an activation time of 10-40 minutes to activate all ions inside the epitaxial wafer.
8. A method for manufacturing a silicon carbide super junction MOSFET according to any one of claims 1-3 and 5-7, It is characterized in that Then make the front and back electrodes in turn, specifically: A temporary substrate is bonded to the back of the substrate, and a front electrode is prepared on the front of the substrate; Remove the back temporary substrate, in the back substrate layer, First, metal CVD is used to fill the deep holes on the back with metal W; Then, four metal layers of Ni, Ti, Ni, and Ag are deposited on the back in sequence by sputtering or evaporation, with a thickness ranging from 50nm to 2um; That is, the back electrode is obtained.
9. The method for manufacturing a silicon carbide super junction MOSFET according to claim 8, It is characterized in that The method of preparing a front electrode on the front side of the substrate comprises: A layer of oxide is obtained on the front side of the substrate by high temperature oxidation as a gate oxide layer; Then a layer of polysilicon is deposited by LPCVD; By photolithography and dry etching, a gate is obtained; Then, a silicon dioxide insulating layer is deposited outside the gate to wrap the gate, and the thickness of the insulating layer is 1 um; The insulating layer is etched away in the source region to expose the P+ and N+ source regions; The source metal layer is deposited on the front side of the substrate by evaporation or sputtering. From bottom to top, the corresponding metals in the metal layer are Ni, Ti, and Al, respectively, with thicknesses ranging from 10nm to 4um. The front source metal pattern is formed by photolithography, which is the front electrode.